Wide bandgap MOSFET device and manufacturing method thereof

By designing the tilt protection layer in a wide bandgap MOSFET device, the problem of insufficient voltage resistance is solved and higher voltage resistance is achieved.

CN119008694APending Publication Date: 2024-11-22BEIJING SMARTCHIP MICROELECTRONICS TECHNOLOGY CO LTD +3
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411007660.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing wide bandgap MOSFET devices lack voltage resistance under extremely harsh conditions, making it difficult to overcome the disadvantages of traditional semiconductors.

Method used

A wide bandgap MOSFET device is designed, which includes a silicon carbide substrate, a drift region, a channel region, a source region, a gate structure and an inclined protective layer. The inclined portion of the inclined protective layer forms an obtuse angle with the horizontal portion to enhance the device's Voltage resistance.

Benefits of technology

Through the design of the inclined protective layer, the boundaries of the device are smoother, reducing electric field concentration, improving lateral depletion capacity, and significantly improving the voltage withstand performance of MOSFET devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008694A_ABST
    Figure CN119008694A_ABST
Patent Text Reader

Abstract

The invention relates to the field of semiconductors, and provides a wide bandgap MOSFET device and a manufacturing method thereof. The wide bandgap MOSFET device comprises a silicon carbide substrate, a silicon carbide drift region, a channel region, a source region, a gate structure, a drain electrode and a first protection layer, the silicon carbide drift region is formed on the surface of the silicon carbide substrate, and the channel region and the source region are formed on the surface of the silicon carbide drift region; the first protection layer comprises two inclined structures, and the two inclined structures are located on the two sides of the silicon carbide drift region respectively; the inclined structure comprises an inclined part and a horizontal part, the inclined part is connected with the side walls of the source region and the silicon carbide drift region, the horizontal part extends to the bottom of the silicon carbide drift region, and the inclined angle of the inclined part relative to the horizontal part is an obtuse angle. The first protection region is in an oblique angle form, the boundary of the protection region is smoother and smoother, transverse depletion in the silicon carbide drift region is easier to realize, the silicon carbide drift region is not easy to break down, and the voltage resistance of the device can be improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductors, and in particular to a wide bandgap MOSFET device and a manufacturing method thereof. Background Art

[0002] Wide bandgap semiconductor materials generally refer to materials such as gallium nitride (GaN), silicon carbide (SiC), aluminum nitride (AlN), and diamond. They have the characteristics of large bandgap width, strong radiation resistance, good breakdown electric field strength, and high temperature resistance. They can overcome the disadvantages of traditional semiconductors and enable semiconductor devices to work normally under extremely harsh conditions.

[0003] MOSFET devices made of wide bandgap semiconductor materials (such as SiC) are wide bandgap power devices with a wide range of applications. How to improve the voltage withstand capability of wide bandgap MOSFET devices is a further problem to be solved. Summary of the invention

[0004] The present invention provides a wide bandgap MOSFET device and a manufacturing method, which can improve the voltage resistance of the device.

[0005] On one hand, the present invention provides a wide bandgap MOSFET device, comprising: a silicon carbide substrate, a silicon carbide drift region, a channel region, a source region, a gate structure, a drain and a first protective layer, wherein the silicon carbide drift region is formed on the surface of the silicon carbide substrate, the channel region and the source region are formed on the surface of the silicon carbide drift region, and the gate structure is formed above the silicon carbide drift region, the channel region and the source region;

[0006] The first protective layer includes two inclined structures, and the two inclined structures are respectively located on both sides of the silicon carbide drift region;

[0007] The inclined structure includes an inclined portion and a horizontal portion, the inclined portion is connected to the side walls of the source region and the silicon carbide drift region, the horizontal portion extends to the bottom of the silicon carbide drift region, and the inclined portion is inclined at an obtuse angle compared to the horizontal portion.

[0008] In an embodiment of the present invention, the wide bandgap MOSFET device also includes two second protective layers, one end of the two second protective layers are respectively connected to the two inclined structures of the first protective layer, and the other end of the two second protective layers are connected to the silicon carbide drift region; the upper surface of the second protective layer is connected to the source region and the channel region.

[0009] In an embodiment of the present invention, the gate structure includes a gate oxide layer and a gate electrode contact, the gate oxide layer is formed on the surfaces of the silicon carbide drift region, the channel region and the source region, and the gate electrode contact is formed on the surface of the gate oxide layer.

[0010] In an embodiment of the present invention, a passivation layer is further included, and the passivation layer is formed on a surface contacting the gate electrode.

[0011] In an embodiment of the present invention, a source metal contact is further included, and the source metal contact is formed on the surface of the passivation layer and the first protective layer.

[0012] In the embodiment of the present invention, the inclined portion of the first protective layer has an inclination angle of 120°-150° compared to the horizontal portion.

[0013] In the embodiment of the present invention, a preset spacing distance exists between the horizontal portion of the first protection layer and the bottom of the silicon carbide drift region.

[0014] Another aspect of the present invention provides a method for manufacturing a wide bandgap MOSFET device, comprising:

[0015] preparing a silicon carbide substrate;

[0016] epitaxially growing silicon carbide material on the surface of the silicon carbide substrate to form an epitaxial layer;

[0017] Etching the epitaxial layer to form a silicon carbide drift region;

[0018] A first protective layer with an inclined structure is formed on both sides of the silicon carbide drift region, wherein the inclined structure of the first protective layer includes an inclined portion and a horizontal portion, wherein the inclined portion is connected to the side wall of the silicon carbide drift region, and the horizontal portion extends to the bottom of the silicon carbide drift region, and the inclined angle of the inclined portion relative to the horizontal portion is an obtuse angle;

[0019] forming a second protection layer, a channel region, and a source region;

[0020] A gate, a source, and a drain are formed.

[0021] In an embodiment of the present invention, the step of preparing a silicon carbide substrate includes:

[0022] Standard cleaning of silicon carbide substrates;

[0023] The silicon carbide substrate after standard cleaning is cleaned for a second time using concentrated sulfuric acid and hydrogen peroxide solution;

[0024] The silicon carbide substrate after the second cleaning is cleaned for the third time using deionized water or a mixture of ammonia water, hydrogen peroxide and deionized water.

[0025] In an embodiment of the present invention, the silicon carbide substrate after the second cleaning is cleaned for a third time, comprising:

[0026] The silicon carbide substrate after the second cleaning is rinsed with deionized water;

[0027] Boil the rinsed silicon carbide substrate in a mixture of ammonia, hydrogen peroxide and deionized water for at least 10 minutes;

[0028] The silicon carbide substrate is placed in a mixture of hydrochloric acid, hydrogen peroxide and deionized water and boiled for at least 10 minutes;

[0029] The silicon carbide substrate is immersed in a hydrofluoric acid solution for at least 2 minutes.

[0030] In an embodiment of the present invention, the step of epitaxially growing an epitaxial layer on the surface of a silicon carbide substrate comprises:

[0031] The silicon carbide material is epitaxially grown on the surface of the silicon carbide substrate to form an epitaxial layer, wherein the N-type ion doping concentration of the epitaxial layer is 1.0×10 15 cm -3 -1.0×10 16 cm -3 , thickness is 2-10μm.

[0032] In an embodiment of the present invention, etching the epitaxial layer to form a silicon carbide drift region includes:

[0033] Depositing a dielectric material on the surface of the epitaxial layer to form a first barrier layer;

[0034] The first barrier layer is used as a mask to perform dry etching on the epitaxial layer to remove the silicon carbide material on both sides of the epitaxial layer, and the etched epitaxial layer is used as a silicon carbide drift region.

[0035] In an embodiment of the present invention, the first protective layer of the inclined structure is formed on both sides of the silicon carbide drift region, including: using a dry oblique angle etching method to etch out the inclination angle corresponding to the inclined structure on both sides of the silicon carbide drift region; and injecting P-type ions on both sides of the silicon carbide drift region to form the first protective layer of the inclined structure.

[0036] In an embodiment of the present invention, the dry oblique angle etching method is used to etch the inclined angles corresponding to the inclined structure on both sides of the silicon carbide drift region, including:

[0037] Depositing dielectric material on both sides of the silicon carbide drift region to form a second barrier layer;

[0038] Using the second barrier layer as a mask, dry oblique-angle etching is performed on both sides of the silicon carbide drift region to form an inclination angle corresponding to the inclination portion of the inclination structure;

[0039] removing the second barrier layer, and depositing dielectric material in the inclined angle regions on both sides of the silicon carbide drift region to form a third barrier layer;

[0040] Using the third barrier layer as a mask, dry etching is performed on both sides of the silicon carbide drift region to form a horizontal portion corresponding to the inclined structure.

[0041] In an embodiment of the present invention, the step of implanting P-type ions on both sides of the silicon carbide drift region to form a first protective layer with an inclined structure includes:

[0042] removing the first barrier layer and the third barrier layer, and forming an implantation mask layer by photolithography pattern transfer;

[0043] By utilizing the blocking effect of the implantation mask layer, P-type ions are implanted into the side walls with an inclined angle on both sides of the silicon carbide drift region to form a first protective layer with an inclined structure.

[0044] In an embodiment of the present invention, the forming of the second protection layer, the channel region, and the source region includes:

[0045] Using photolithography pattern transfer to form an implantation mask layer, three P-type ion implantations are performed to form a second protective layer and a channel region;

[0046] An implantation mask layer is formed by photolithography pattern transfer, and three N-type ion implantations are performed to form a source region.

[0047] In an embodiment of the present invention, a method for forming a gate includes:

[0048] forming an oxide layer on the surfaces of the first protective layer, the second protective layer, the channel region and the source region;

[0049] Depositing polysilicon or silicide on the surface of the oxide layer and etching it to form a gate electrode contact;

[0050] A passivation layer is formed on the gate electrode contact.

[0051] In an embodiment of the present invention, a method for forming a source and a drain includes:

[0052] Removing the oxide layer on the surface of the source region and the surface of the first protective layer, and depositing metal on the surface of the source region and the surface of the first protective layer by a thin film deposition method to form a source metal contact;

[0053] Depositing a metal layer on the back side of the silicon carbide substrate as a drain metal contact;

[0054] The source metal contact and the drain metal contact are annealed to form ohmic contacts.

[0055] The present invention sets the first protection zone as an oblique angle shape. The first protection layer of the inclined structure includes an inclined portion and a horizontal portion. The inclination angle of the inclined portion is an obtuse angle compared to the horizontal portion. The boundary of the protection zone is flatter and smoother, and it is easier to achieve lateral depletion in the silicon carbide drift zone, making it less likely to be broken down, thereby improving the voltage resistance performance of the MOSFET device.

[0056] Other features and advantages of the technical solution of the present invention will be described in detail in the specific implementation section below. BRIEF DESCRIPTION OF THE DRAWINGS

[0057] The drawings described herein are used to provide a further understanding of the present invention and constitute a part of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute an improper limitation of the present invention. In the drawings:

[0058] Figure 1 is a schematic structural diagram of a wide bandgap MOSFET device provided by an embodiment of the present invention;

[0059] Figure 2 is a flow chart of a method for manufacturing a wide bandgap MOSFET device provided by an embodiment of the present invention;

[0060] Figure 3a is a schematic diagram of an epitaxial layer formed in the manufacturing method provided in an embodiment of the present invention;

[0061] Figure 3b is a schematic diagram of a silicon carbide drift region formed by etching an epitaxial layer in a manufacturing method provided in an embodiment of the present invention;

[0062] Figure 3c It is a schematic diagram of a structure formed by dry oblique-angle etching of a silicon carbide drift region in a manufacturing method provided in an embodiment of the present invention;

[0063] Figure 3d is a schematic diagram of a horizontal portion formed by dry etching a silicon carbide drift region in a manufacturing method provided by an embodiment of the present invention;

[0064] Figure 3e is a schematic diagram of a first protective layer formed in a manufacturing method provided in an embodiment of the present invention;

[0065] Figure 3f is a schematic diagram of a second protective layer and a channel region formed in a manufacturing method provided in an embodiment of the present invention;

[0066] Figure 3g is a schematic diagram of a gate oxide layer formed in a manufacturing method provided in an embodiment of the present invention;

[0067] Figure 3h is a schematic diagram of a gate electrode contact formed in a manufacturing method provided in an embodiment of the present invention;

[0068] Figure 3i is a schematic diagram of a passivation layer formed in a manufacturing method provided in an embodiment of the present invention;

[0069] Figure 3j It is a schematic diagram of a source metal contact and a drain metal contact formed in a manufacturing method provided in an embodiment of the present invention.

[0070] Description of Reference Numerals

[0071] 101 - silicon carbide substrate, 102 - silicon carbide drift region, 103 - first protective layer, 103a - inclined portion,

[0072] 103b-horizontal portion, 104-second protection layer, 105-channel region, 106-source region, 107-gate oxide layer,

[0073] 108 - gate electrode contact, 109 - passivation layer, 110 - source metal contact, 111 - drain metal contact, 102a - epitaxial layer, 201 - first barrier layer, 202 - second barrier layer, 203 - third barrier layer,

[0074] 204-implantation mask layer. DETAILED DESCRIPTION

[0075] In order to make the technical solutions and advantages of the embodiments of the present invention more clearly understood, the exemplary embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than an exhaustive list of all the embodiments. It should be noted that the embodiments of the present invention and the features in the embodiments can be combined with each other without conflict.

[0076] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used only for descriptive purposes, and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features.

[0077] In the present invention, unless otherwise clearly specified and limited, the terms such as "connected", "connected", "connected" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0078] Figure 1Schematic diagram of the structure of a wide bandgap MOSFET device provided by an embodiment of the present invention. Figure 1 As shown, the wide bandgap MOSFET device provided in this embodiment includes: a silicon carbide substrate 101, a silicon carbide drift region 102, a channel region 105, a source region 106, a first protective layer 103, a gate structure and a drain structure. The silicon carbide drift region 102 is formed on the upper surface of the silicon carbide substrate 101, the channel region 105 and the source region 106 are formed on the surface of the silicon carbide drift region 102, and the gate structure is formed above the silicon carbide drift region 102, the channel region 105 and the source region 106. The first protective layer 103 includes two inclined structures, which are respectively located on both sides of the silicon carbide drift region 102. The inclined structures include an inclined portion 103a and a horizontal portion 103b. The inclined portion 103a is connected to the sidewalls of the source region 106 and the silicon carbide drift region, and the horizontal portion 103b extends to the bottom of the silicon carbide drift region. The inclined angle of the inclined portion 103a compared to the horizontal portion 103b is an obtuse angle. The gate structure includes a gate oxide layer 107 and a gate electrode contact 108 . The gate oxide layer 107 is formed on the surface of the silicon carbide drift region 102 , the channel region 105 and the source region 106 . The gate electrode contact 108 is formed on the surface of the gate oxide layer 107 .

[0079] In this embodiment, the wide bandgap MOSFET device further includes two second protective layers 104, one end of the two second protective layers 104 is respectively connected to the two inclined structures of the first protective layer 103, the other end of the two second protective layers 104 is connected to the silicon carbide drift region 102, and the upper surface of the second protective layer 104 is connected to the source region 106 and the channel region 105. The thickness of the second protective layer 104 is 0.2-1 μm, and the distance between the bottom of the second protective layer 104 and the bottom of the silicon carbide drift region 102 is 2-8 μm. The horizontal length of the channel region 5 is 0.2-1 μm, and the horizontal length of the source region 6 is 0.2-1 μm.

[0080] In this embodiment, the surface of the gate electrode contact 108 and the surface of the gate oxide layer 107 have a passivation layer 109. The surface of the passivation layer 109 and the surface of the first protection layer 103 are source metal contacts 110. The back side of the silicon carbide substrate 101 has a drain metal contact 111.

[0081] In this embodiment, the horizontal portion 103b of the first protective layer has a preset spacing distance from the bottom of the silicon carbide drift region 102, and the spacing distance is 0.6-2 μm. The inclined portion 103a of the first protective layer is preferably inclined at an angle of 120°-150° compared to the horizontal portion 103b. The thickness of the horizontal portion 103b is 0.2-2 μm, the thickness of the inclined portion 103a is 0.2-2 μm, and the angle between the inclined portion 103a and the horizontal plane is 30°-60°.

[0082] Since silicon carbide (SiC) is a wide bandgap material, SiC MOSFET devices usually need to set up protection zones to achieve better voltage resistance. Traditional protection zones have sharp corners and are very steep and sharp-angle structures. The electric field is easily concentrated in the corner area, the electric field intensity is high, and the corners are easily broken down. The diffusion coefficient of wide bandgap semiconductors is relatively low, and SiC is difficult to diffuse. It is difficult to form a protection zone with smooth corners through processes such as heat treatment.

[0083] In an embodiment of the present invention, the first protection zone is set to an oblique angle shape. The first protection layer of the inclined structure includes an inclined portion and a horizontal portion. The inclination angle of the inclined portion is an obtuse angle compared to the horizontal portion. The boundary of the protection zone is flatter and smoother, and it is easier to achieve lateral depletion in the silicon carbide drift zone, making it less likely to be broken down, thereby improving the voltage resistance performance of the MOSFET device.

[0084] Figure 2 FIG. 1 is a flow chart of a method for manufacturing a wide bandgap MOSFET device provided by an embodiment of the present invention. Figure 2 As shown, the manufacturing method of the wide bandgap MOSFET device provided in this embodiment includes the following steps:

[0085] S210, preparing a silicon carbide substrate;

[0086] S220, epitaxially growing silicon carbide material on the surface of the silicon carbide substrate to form an epitaxial layer;

[0087] S230, etching the epitaxial layer to form a silicon carbide drift region;

[0088] S240, forming a first protective layer with an inclined structure on both sides of the silicon carbide drift region, wherein the inclined structure of the first protective layer includes an inclined portion and a horizontal portion, wherein the inclined portion is connected to the side wall of the silicon carbide drift region, and the horizontal portion extends to the bottom of the silicon carbide drift region, and the inclined portion is inclined at an obtuse angle compared to the horizontal portion;

[0089] S250, forming a second protection layer, a channel region, and a source region;

[0090] S260 , forming a gate, a source, and a drain.

[0091] In the above step S210, a silicon carbide substrate with a corresponding crystal structure (different crystal structures correspond to different bandgap widths) is selected, with a standard thickness of 350-1000 μm, or the silicon carbide substrate is thinned, ground, polished, cleaned, etc. by mechanical processing and chemical reaction methods to achieve the required thickness and flatness on its surface. Specifically, the method comprises the following steps: (1) performing standard cleaning (RCA) on the silicon carbide substrate, ultrasonically cleaning with acetone and ethanol in turn, with a power of 40-60W, for more than 10 minutes respectively, and then rinsing with deionized water; (2) performing a second cleaning on the silicon carbide substrate after standard cleaning, boiling the silicon carbide substrate after organic ultrasonic cleaning in concentrated sulfuric acid and hydrogen peroxide solution for more than 10 minutes; (3) performing a third cleaning on the silicon carbide substrate after the second cleaning, rinsing the silicon carbide substrate boiled in concentrated sulfuric acid with deionized water, boiling it with a mixture of ammonia, hydrogen peroxide and deionized water for more than 10 minutes, rinsing it with deionized water, boiling it with a mixture of hydrochloric acid, hydrogen peroxide and deionized water for more than 10 minutes, and then rinsing it with deionized water, blowing it dry with nitrogen, and soaking the silicon carbide substrate in hydrofluoric acid for at least 2 minutes to remove the surface oxide layer.

[0092] In the above step S220, a silicon carbide material is epitaxially grown on the surface of the silicon carbide substrate 101 to form a silicon carbide substrate 101. Figure 3a The epitaxial layer 102a is shown. The doping concentration of the epitaxial layer is 1.0×10 15 cm -3 to 1.0×10 16 cm -3 , thickness is 2-10μm, the source of epitaxial growth is silane / trichlorosilane, ethylene / propane, and the temperature of epitaxial growth is 1500-1700℃. The source of epitaxial growth is silane or trichlorosilane, ethylene or propane, etc., and the doping source used is ammonia and other gas sources.

[0093] In the above step S230, dielectric materials such as silicon dioxide, polysilicon or metal are deposited on the surface of the epitaxial layer 102a by physical and chemical vapor deposition or other thin film deposition methods, patterned by photolithography, and dry-etched to form a first barrier layer 201; the first barrier layer 201 is used as a mask to dry-etch the epitaxial layer to remove the silicon carbide material on both sides of the epitaxial layer, so as to form a first barrier layer 201; Figure 3bIn the structure shown, the etched epitaxial layer serves as the silicon carbide drift region 102 of the device. If the material of the first barrier layer 201 is silicon dioxide, the thickness is 2μm-5μm, and it needs to be annealed and densified under O2 conditions at above 1000°C; if the material of the first barrier layer 201 is a metal such as Al, Ni, etc., the thickness is about 1μm. The dry etching gas can be C4F8, CHF3, Cl2 and other gases. Using the first barrier layer 201 as a mask, etching is performed by physical, chemical and other etching methods, such as reactive ion etching (RIE) or inductively coupled plasma (ICP), dry etching of the SiC substrate, and the etching gas can be a gas combination of SF6 / O2, NF3 / Ar, CF4, CHF3 / O2, C4F8 / O2 and the like. As an example, using SF6 / O2 / HBr etching gas, ICP power is 600-1000W, bias power is 100-300W, temperature is 20°C, and etching depth is 1-3μm.

[0094] In the above step S240, a dry oblique angle etching method is used to etch the inclined angles corresponding to the inclined structure on both sides of the silicon carbide drift region, and P-type ions are implanted on both sides of the silicon carbide drift region to form a first protective layer of the inclined structure.

[0095] like Figure 3c As shown, dielectric materials such as silicon dioxide, polysilicon or metal are deposited on both sides of the silicon carbide drift region 102 by physical and chemical vapor deposition or other thin film deposition methods, patterned by photolithography, and dry-etched to form a second barrier layer 202. If the material of the second barrier layer 202 is silicon dioxide, the thickness is 2μm-5μm, and it needs to be annealed and densified under O2 conditions at above 1000°C; if the material of the second barrier layer 202 is metal such as Al, Ni, the thickness is about 1μm. The dry etching gas can be C4F8, CHF3, Cl2 and other gases. Using the second barrier layer 202 as a mask, physical, chemical and other dry etching methods, such as reactive ion etching (RIE) or inductively coupled plasma (ICP), are used to perform dry oblique angle etching on both sides of the silicon carbide drift region 102 to form the required tilt angle. The etching gas can be a gas combination of SF6 / O2, NF3 / Ar, CF4, CHF3 / O2, C4F8 / O2, etc. For example, SF6 / O2 / HBr etching gas is used, the ICP power is 600-1000W, the bias power is 100-300W, the temperature is 20°C, and the etching depth is 0.5-2μm.

[0096] like Figure 3d As shown, the second barrier layer 202 is removed, and dielectric materials such as silicon dioxide, polysilicon or metal are deposited on the inclined angle regions on both sides of the silicon carbide drift region 102 by physical and chemical vapor deposition or other thin film deposition methods, and patterned by photolithography and dry etching are performed to form a Figure 3dThe third barrier layer 203 is shown. If the material of the third barrier layer 203 is silicon dioxide, the thickness is 2μm-5μm, and it needs to be annealed and densified under O2 conditions at above 1000°C; if the material of the third barrier layer 203 is metal such as Al, Ni, etc., the thickness is about 1μm. The dry etching gas can be C4F8, CHF3, Cl2 and other gases. Using the third barrier layer 203 as a mask, physical, chemical and other dry etching methods, such as reactive ion etching (RIE) or inductively coupled plasma (ICP), are used to perform dry etching on both sides of the silicon carbide drift region 102 to form a horizontal region corresponding to the inclined structure. The etching gas can be a gas combination of SF6 / O2, NF3 / Ar, CF4, CHF3 / O2, C4F8 / O2, etc. For example, SF6 / O2 / HBr etching gas is used, the ICP power is 600-1000W, the bias power is 100-300W, the temperature is 20°C, and the etching depth is 1-3μm.

[0097] like Figure 3e As shown, the first barrier layer 201 and the third barrier layer 203 are removed, and an implantation mask layer 204 is formed by photolithography pattern transfer. Using the blocking effect of the implantation mask layer 204, P-type ions are implanted into the sidewalls with inclined angles on both sides of the silicon carbide drift region 102 to form a first protective layer 103 having an inclined portion 103a and a horizontal portion 103b. In the process of P-type ion implantation, the implantation energy is 28keV and the implantation dose is 2.36×10 13 cm -2 The implantation energy is 60 keV and the implantation dose is 4.6×10 13 cm -2 The implantation energy is 100 keV and the implantation dose is 6.3×10 13 cm -2 The three times Al atoms (or B atoms) are implanted to form a doping concentration of about 1.0×10 19 cm -3 The p+ protection zone (ie, the first protection layer 103) has a depth of 0.2-2 μm.

[0098] In the above step S250, if Figure 3f As shown in FIG. 1 , a mask layer is formed by photolithography pattern transfer, and three P-type ion implantations are performed. The three ion (Al atom or B atom) implantations are respectively implanted with an energy of 28 keV and an implantation dose of 2.36×10 13 cm -2 , injection energy 60keV, injection dose 4.6×10 13 cm -2 , injection energy 100keV, injection dose 6.3×10 13 cm -2, forming a doping concentration of about 1.0×10 19 cm -3 The second protective layer 104 and the lower doped channel region 105 are formed with a total depth of 0.2-1 μm. The implantation mask layer of the source region is formed by photolithography pattern transfer, and three N-type ion implantations are performed. The three ion (such as phosphorus atoms) implantations are respectively implanted with an energy of 28 keV and an implantation dose of 2.36×10 13 cm -2 , injection energy 60keV, injection dose 4.6×10 13 cm -2 , injection energy 100keV, injection dose 6.3×10 13 cm -2 , forming a doping concentration of about 1.0×10 19 cm -3 The n+ source region 106 has a depth of 0.2-0.5 μm.

[0099] The next step is to perform annealing after ion implantation: remove the implantation mask layer, clean the surface, and use carbon film, AlN film covering, silane suppression and other methods. Anneal for about half an hour at a high temperature of 1600°C and a pressure of 600-700Torr to activate the ion implantation doping in the previous steps, and then remove the carbon film, AlN film, etc. covering the surface after annealing.

[0100] Next, make the terminal. Use physical and chemical vapor deposition or other thin film deposition methods to deposit a certain thickness of silicon dioxide, polysilicon or metal dielectric to form a barrier layer, photolithography patterning, and dry etching the barrier layer; use the barrier layer to dry etch the SiC substrate by physical, chemical and other etching methods, such as reactive ion etching or inductively coupled plasma, to form a terminal structure. After the terminal structure is etched, remove the corresponding barrier layer.

[0101] In the above step S260, a first protective layer, a second protective layer, a channel region, and a source region are formed on the surface of the first protective layer, the second protective layer, the channel region, and the source region by using physical or chemical vapor deposition, high temperature thermal oxidation and post-oxidation annealing, atomic layer deposition (ALD), and the like. Figure 3gThe gate oxide layer 107 shown. Specifically, the SiC substrate is ultrasonically cleaned with acetone and ethanol in turn, and then rinsed with deionized water; the SiC substrate after organic ultrasonic treatment is boiled in concentrated sulfuric acid and hydrogen peroxide solution for at least 10 minutes; the SiC substrate boiled in concentrated sulfuric acid is boiled in liquid No. 1 and liquid No. 2 for more than 10 minutes respectively, then rinsed with deionized water and blown dry with nitrogen for standby use. Liquid No. 1 is a mixture of ammonia, hydrogen peroxide and deionized water, and liquid No. 2 is a mixture of hydrochloric acid, hydrogen peroxide and deionized water. The rinsed SiC substrate is immersed in hydrofluoric acid for at least 1 minute to remove the surface oxide layer. The SiC substrate that has been cleaned by standard cleaning needs to be oxidized in a wet oxygen environment at about 1100°C for about half an hour to form a sacrificial oxide layer, and the sacrificial oxide layer is removed by diluted HF ultrasonic rinsing. Oxidation is performed at 1100-1300°C for about half an hour, and annealing is performed at 1200-1300°C in a NO atmosphere for 1-3 hours. The annealing atmosphere may also be POCl3, H2, N2O, P2O5, Sb+NO, etc.

[0102] Polysilicon or silicide is deposited on the surface of the gate oxide layer 107, and then etched and planarized to form a Figure 3h The gate electrode contact 108 is shown. Specifically, the gate oxide layer 107 is filled with a gate electrode contact by an isotropic deposition technique. The filling material may be doped polysilicon or silicide with high conductivity. The deposited gate electrode contact is etched back by dry etching, wet etching, etc., and deposited again and etched back until it is flattened and only the gate electrode contact 108 on the gate oxide layer 107 is retained.

[0103] A SiO2 / Si3N4 passivation dielectric layer of about 1 μm is deposited on the gate electrode contact 108 by physical or chemical vapor deposition, patterned by photolithography, and the passivation dielectric layer is dry-etched by selective etching gas to form a Figure 3i A passivation layer 109 is shown.

[0104] like Figure 3j As shown, the oxide layer on the surface of the source region and the surface of the first protective layer is removed, and metal is deposited on the surface of the source region and the surface of the first protective layer using a thin film deposition method to form a source metal contact 110; a metal layer is deposited on the back side of the silicon carbide substrate as a drain metal contact 111.

[0105] The specific method of making the source metal contact 110 is: photolithography patterning, and using diluted HF to remove part of the oxide layer on the n+ source region and the p+ protection region, using thin film deposition methods such as electron beam evaporation or sputtering to deposit 50-100nm Ni, 10-40nm Ti, 50-100nm Al multi-layer metals in sequence, and peeling to form a source metal contact. The source metal contact needs to cover the surface of the n+ source region and the p+ protection region at the same time. The source metal contact can be a combination of other metals such as AlTi, Ni, TiW, etc.

[0106] The specific method of making the drain metal contact 111 is: apply glue to protect the front source metal contact, and use diluted HF to remove the oxide layer on the back of the substrate, and use thin film deposition methods such as electron beam evaporation or sputtering to deposit 20nm thick AlTi and 200-400nm Ni metal layer on the back as the drain metal contact. The drain metal contact can be AlTi, Ni, TiW, AlTi and other metal combinations.

[0107] Finally, the source metal contact 110 and the drain metal contact 111 are annealed to form ohmic contacts, wherein rapid thermal annealing is performed at 900-1100° C. in an Ar or N2 environment for 1-2 minutes.

[0108] In an embodiment of the present invention, the first protection zone is set to an oblique angle shape. The first protection layer of the inclined structure includes an inclined portion and a horizontal portion. The oblique angle protection zone is realized by performing oblique angle etching through three etching mask layers. The boundary of the protection zone with the oblique angle morphology is smoother and the corners are rounder, which makes it easier to realize lateral depletion in the silicon carbide drift zone, making it less likely to be broken down, thereby improving the voltage resistance performance of the MOSFET device.

[0109] The embodiment of the present invention further provides a chip, which includes the above-mentioned wide bandgap MOSFET device. The chip can be a power chip or an isolation driver chip.

[0110] The optional implementation modes of the present invention are described in detail above in conjunction with the accompanying drawings. However, the implementation modes of the present invention are not limited to the specific details in the above implementation modes. Within the technical concept of the implementation modes of the present invention, a variety of simple modifications can be made to the technical solutions of the implementation modes of the present invention, and these simple modifications all belong to the protection scope of the implementation modes of the present invention. It should also be noted that the various specific technical features described in the above specific implementation modes can be combined in any suitable manner without contradiction, and as long as the combination does not violate the concept of the implementation modes of the present invention, it should also be regarded as the content disclosed in the implementation modes of the present invention.

Claims

1. A wide bandgap MOSFET device, characterized in that: The invention comprises: a silicon carbide substrate, a silicon carbide drift region, a channel region, a source region, a gate structure, a drain and a first protective layer, wherein the silicon carbide drift region is formed on the surface of the silicon carbide substrate, the channel region and the source region are formed on the surface of the silicon carbide drift region, and the gate structure is formed above the silicon carbide drift region, the channel region and the source region; The first protective layer includes two inclined structures, and the two inclined structures are respectively located on both sides of the silicon carbide drift region; The inclined structure includes an inclined portion and a horizontal portion, the inclined portion is connected to the side walls of the source region and the silicon carbide drift region, the horizontal portion extends to the bottom of the silicon carbide drift region, and the inclined portion is inclined at an obtuse angle compared to the horizontal portion.

2. The wide bandgap MOSFET device according to claim 1, characterized in that: It also includes two second protective layers, one end of the two second protective layers is connected to the two inclined structures of the first protective layer respectively, and the other end of the two second protective layers is connected to the silicon carbide drift region; The upper surface of the second protection layer is connected to the source region and the channel region.

3. The wide bandgap MOSFET device according to claim 1, characterized in that: The gate structure comprises a gate oxide layer and a gate electrode contact. The gate oxide layer is formed on the surfaces of the silicon carbide drift region, the channel region and the source region. The gate electrode contact is formed on the surface of the gate oxide layer.

4. The wide bandgap MOSFET device according to claim 3, characterized in that: The invention also includes a passivation layer formed on a surface contacting the gate electrode.

5. The wide bandgap MOSFET device according to claim 4, characterized in that: The invention also includes a source metal contact, wherein the source metal contact is formed on the surface of the passivation layer and the first protection layer.

6. The wide bandgap MOSFET device according to claim 1, characterized in that: The inclined portion of the first protective layer has an inclination angle of 120°-150° compared to the horizontal portion.

7. The wide bandgap MOSFET device according to claim 1, characterized in that: A preset spacing distance exists between the horizontal portion of the first protection layer and the bottom of the silicon carbide drift region.

8. A method for manufacturing a wide bandgap MOSFET device, characterized in that: include: preparing a silicon carbide substrate; epitaxially growing silicon carbide material on the surface of the silicon carbide substrate to form an epitaxial layer; Etching the epitaxial layer to form a silicon carbide drift region; A first protective layer with an inclined structure is formed on both sides of the silicon carbide drift region, wherein the inclined structure of the first protective layer includes an inclined portion and a horizontal portion, wherein the inclined portion is connected to the side wall of the silicon carbide drift region, and the horizontal portion extends to the bottom of the silicon carbide drift region, and the inclined angle of the inclined portion relative to the horizontal portion is an obtuse angle; forming a second protection layer, a channel region, and a source region; A gate, a source, and a drain are formed.

9. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: The step of preparing a silicon carbide substrate comprises: Standard cleaning of silicon carbide substrates; The silicon carbide substrate after standard cleaning is cleaned for a second time using concentrated sulfuric acid and hydrogen peroxide solution; The silicon carbide substrate after the second cleaning is cleaned for the third time using deionized water or a mixture of ammonia water, hydrogen peroxide and deionized water.

10. The method for manufacturing a wide bandgap MOSFET device according to claim 9, characterized in that: The silicon carbide substrate after the second cleaning is cleaned for the third time, including: The silicon carbide substrate after the second cleaning is rinsed with deionized water; Boil the rinsed silicon carbide substrate in a mixture of ammonia, hydrogen peroxide and deionized water for at least 10 minutes; The silicon carbide substrate is placed in a mixture of hydrochloric acid, hydrogen peroxide and deionized water and boiled for at least 10 minutes; The silicon carbide substrate is immersed in a hydrofluoric acid solution for at least 2 minutes.

11. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: The epitaxially growing an epitaxial layer on the surface of the silicon carbide substrate comprises: The silicon carbide material is epitaxially grown on the surface of the silicon carbide substrate to form an epitaxial layer, wherein the N-type ion doping concentration of the epitaxial layer is 1.0×10 15 cm -3 ~1.0×10 16 cm -3 , thickness is 2μm~10μm.

12. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: The step of etching the epitaxial layer to form a silicon carbide drift region comprises: Depositing a dielectric material on the surface of the epitaxial layer to form a first barrier layer; The first barrier layer is used as a mask to perform dry etching on the epitaxial layer to remove the silicon carbide material on both sides of the epitaxial layer, and the etched epitaxial layer is used as a silicon carbide drift region.

13. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: The first protective layer with an inclined structure formed on both sides of the silicon carbide drift region includes: Using a dry oblique-angle etching method, etching an inclination angle corresponding to the inclination structure on both sides of the silicon carbide drift region; P-type ions are implanted on both sides of the silicon carbide drift region to form a first protective layer with an inclined structure.

14. The method for manufacturing a wide bandgap MOSFET device according to claim 13, characterized in that: The dry oblique angle etching method is used to etch the inclined angles corresponding to the inclined structure on both sides of the silicon carbide drift region, including: Depositing dielectric material on both sides of the silicon carbide drift region to form a second barrier layer; Using the second barrier layer as a mask, dry oblique-angle etching is performed on both sides of the silicon carbide drift region to form an inclination angle corresponding to the inclination portion of the inclination structure; removing the second barrier layer, and depositing dielectric material in the inclined angle regions on both sides of the silicon carbide drift region to form a third barrier layer; Using the third barrier layer as a mask, dry etching is performed on both sides of the silicon carbide drift region to form a horizontal portion corresponding to the inclined structure.

15. The method for manufacturing a wide bandgap MOSFET device according to claim 14, characterized in that: The step of implanting P-type ions on both sides of the silicon carbide drift region to form a first protective layer with an inclined structure includes: removing the first barrier layer and the third barrier layer, and forming an implantation mask layer by photolithography pattern transfer; By utilizing the blocking effect of the implantation mask layer, P-type ions are implanted into the side walls with an inclined angle on both sides of the silicon carbide drift region to form a first protective layer with an inclined structure.

16. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: The forming of the second protection layer, the channel region, and the source region includes: Using photolithography pattern transfer to form an implantation mask layer, three P-type ion implantations are performed to form a second protective layer and a channel region; An implantation mask layer is formed by photolithography pattern transfer, and three N-type ion implantations are performed to form a source region.

17. The method for manufacturing a wide bandgap MOSFET device according to claim 8, characterized in that: A method for forming a gate, comprising: forming an oxide layer on the surfaces of the first protective layer, the second protective layer, the channel region and the source region; Depositing polysilicon or silicide on the surface of the oxide layer and etching it to form a gate electrode contact; A passivation layer is formed on the gate electrode contact.

18. The method for manufacturing a wide bandgap MOSFET device according to claim 17, characterized in that: A method for forming a source and a drain, comprising: Removing the oxide layer on the surface of the source region and the surface of the first protective layer, and depositing metal on the surface of the source region and the surface of the first protective layer by a thin film deposition method to form a source metal contact; Depositing a metal layer on the back side of the silicon carbide substrate as a drain metal contact; The source metal contact and the drain metal contact are annealed to form ohmic contacts.

19. A chip, characterized in that: The chip comprises the wide bandgap MOSFET device according to any one of claims 1 to 7.