Large ampere meter pasting type fuse and manufacturing method thereof
Through molding and finite element simulation design, combined with composite arc extinguishing filler of inorganic flame retardant and organic bonding materials, the packaging reliability of melt and arc extinguishing materials in high-current surface-mount fuses is solved, and the arc extinguishing performance is improved and environmental adaptability, achieving higher breakage capabilities and reliability.
Patent Information
- Application Number
- CN202411373499.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-29
AI Technical Summary
In the existing high-current surface-mount fuses, in the ceramic tube perforated packaging or the slotted ceramic tube integrated molding packaging, the packaging reliability of melt and arc extinguishing materials is insufficient, resulting in serious arc diffusion, material corrosion and mechanical strength, which affects the Product breakdown capability and reliability.
Using molding technology, the molding of the arc extinguishing filler and melt is molded by granulation and compaction, and the melt is designed in combination with finite element simulation, and composite arc extinguishing filler is made using inorganic flame retardant and organic bonding materials, and polymerizes it with polymerization. It can be used to form a product by encapsulating the arc extinguishing performance and environmental adaptability.
It improves the arc extinguishing performance and breaking ability of the fuse, avoids arc diffusion and material corrosion, enhances the mechanical strength and environmental adaptability of the product, and achieves higher reliability and performance advantages.
Smart Images

Figure CN119049940A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of fuses, and further relates to the field of surface-mount fuses, and in particular, to a high-current surface-mount fuse and a manufacturing method thereof. Background Art
[0002] As the widespread use of smartphones has made high-performance ion batteries more widely used, there is an increasing need in the market for low-cost SMD fuses assembled on PCBs for current overcurrent protection to manage higher and higher currents. Energy-intensive electric vehicles also rely on this technology. The higher the current flowing through the SMD fuse on the PCB, the more power must be converted and consumed. For such applications, reliable high-current fuses that can cut off the circuit in time in the event of current overload or short circuit are particularly important for circuit protection.
[0003] At present, there are two types of high-current surface-mount fuses in the industry. One type is a type of fuse that inserts a round or sheet-shaped fuse into a ceramic tube, welds the fuse to a copper cap with solder, and fills the tube with arc-extinguishing material. This type of surface-mount fuse is only suitable for short-circuit high-current protection when in use. When the fault current in the line is low, usually 2 to 3 times the rated current of the fuse product, the product (referring to the fuse, the same below) will take too long to melt, I 2If the t value is too large, the solder at the end will melt and the end cap will fall off the product body. If the solder at the end melts, the product will be at risk of being broken down by an electric arc. In addition, since solder is used for welding, and solder is a low-melting-point metal material, when the power is turned on at high temperature, the solder is prone to aging, resulting in a larger contact resistance at the end, and the fuse is prone to open circuit failure, which has limited use. In addition, due to the presence of solder, there are more metal particles involved in the reaction when the product melts, so its breaking capacity will be reduced. Another type of high-current surface-mount fuse uses an integrally molded melt, which is placed in a ceramic square tube with one side open, and the tube is filled with sealant or inorganic arc-extinguishing materials. This type of fuse avoids the shortcomings of the first type of fuse because the melt is integrally molded, and its rated breaking capacity is usually higher. However, when this type of fuse is filled with sealant, the arc extinguishing effect of the sealant has certain limitations, and the rated voltage value is usually not high. At present, the rated breaking capacity of the 7358 size is only 1500A@48VDC; the part using inorganic matter as the arc extinguishing material usually adopts the filling method to fill the arc extinguishing material into the ceramic tube. The filling density of the arc extinguishing material is usually low. When the product is broken, the arc generated inside diffuses more seriously. After the melt is melted, the external electrode is easy to fall out from the inside and separate from the body. This filling method exposes the arc extinguishing filler to the outside. In long-term use, the arc extinguishing material may be corroded by organic matter or corrosive gas in the environment, resulting in poor performance, thereby making the arc extinguishing performance of the arc extinguishing filler worse. In addition, since the mechanical strength of the arc extinguishing material after filling is inferior to that of the ceramic shell, there is a possibility that it cannot withstand the pressure shock generated in the tube body when the fuse is melted, so that the arc extinguishing filler is sprayed out from the side of the body that is not the ceramic, and the product structure is destroyed.
[0004] In view of this, the present invention is proposed. Summary of the invention
[0005] The technical problem to be solved by the present invention is to solve the reliability problem of the packaging of the melt and the arc extinguishing material existing in the existing high current surface mount fuse ceramic tube perforated packaging or slotted ceramic tube integrated packaging technology.
[0006] The inventive concept of the present invention is: adopt compression molding, prepare the internal arc-extinguishing filler, granulate the arc-extinguishing filler, study the arc-extinguishing filler compaction process, mold the arc-extinguishing filler and the internal melt, and then use the shell to encapsulate the semi-finished product after molding, so as to solve the arc-extinguishing problem of the product and the environmental adaptability of the product, thereby improving the reliability of the product. The integrated molding inductor production process technology is adopted, the melt is designed by using finite element simulation, the product fusing characteristic matching design is completed, the designed melt is manufactured, the arc-extinguishing material granulated by using inorganic flame retardant and organic adhesive phase is molded with the melt, and then the polymer is made into a product shell to encapsulate the product to form the final product.
[0007] For this purpose, a high current surface mount fuse is provided, such as Figure 1 As shown, it includes a shell 1, a melt 2, an arc suppressor 3, a nickel layer 4, a tin-lead layer 5, and an L-shaped pin 6.
[0008] The housing 1 is square.
[0009] The melt 2 and the L-shaped pin 6 are made in one piece. The L-shaped pin 6 is led out from two ends of the bottom of the shell 1 and is located at the bottom and sides of the two ends of the shell 1.
[0010] The melt 2 is located in the arc suppression body 3 , and the melt 2 and the arc suppression body are located in the shell 1 .
[0011] The surface of the L-shaped pin 6 is sequentially formed from the inside to the outside with a transition layer 4 and a welding layer 5. The transition layer 4 or the welding layer 5 is a single layer or a composite layer.
[0012] The method for manufacturing a high current surface mount fuse comprises the following method: 1. Melt graphics simulation design and production Use finite element simulation software to design and simulate the melt pattern, determine the size and thickness of the non-melting area and the melting area of the one-piece melt, and determine the melt cold resistance, the temperature rise of the melt under the rated current, the melt material and other parameters according to the set current specifications. After the melt design parameters are determined, the melt material is processed and manufactured according to the design drawings to form a melt.
[0013] 2. Preparation of arc extinguishing filler Arc-extinguishing fillers are made of inorganic SiO2 and other inorganic flame-retardant system materials. The inorganic system materials are mixed with organic polymer materials for mixing, granulation and molding to make composite arc-extinguishing fillers. Compared with the arc-extinguishing materials of existing products, this kind of arc-extinguishing material can absorb arc energy more effectively, promote arc extinction, and effectively improve the arc-extinguishing performance of large current surface-mount fuses to meet the set breaking capacity requirements.
[0014] 3. Molding of melt and arc-extinguishing filler The melt and arc-extinguishing filler are molded into an integral structure using a molding device to make an internal semi-finished product of a set shape and size. The arc-extinguishing filler is compacted by the molding process to make the arc-extinguishing material structure compact, which can effectively prevent the arc from spreading. When the arc burns, it is in close contact with the arc-extinguishing filler, so that the arc-extinguishing material can react with the arc quickly and effectively, causing the arc to extinguish.
[0015] 4. Product packaging The product shell is made of high molecular polymer, and the mold is designed according to the product shell packaging size, and the semi-finished product after the melt and arc extinguishing material are molded is packaged. After the melt is encapsulated by the high molecular polymer, it can effectively prevent the problem of the melt falling off from the body after melting. In addition, the high molecular polymer used as the shell material can resist the corrosion of corrosive substances such as salt spray, acid, alkali, and organic solvents, and prevent the internal arc extinguishing filler from being corroded by the above substances, thereby reducing the product performance.
[0016] 5. External electrode plating treatment The external electrodes of the packaged product are electroplated with nickel layer and tin-lead layer in sequence to form the final product.
[0017] The high-current surface-mount fuse produced by the above method not only has a simple structure, simple production process and high production efficiency. On the one hand, it solves the problem of product electrical performance, and on the other hand, it solves the problem of product environmental adaptability. It is superior to traditional surface-mount fuses in the production of high-current specifications of fuse products, and superior to existing similar products in performance. This production process can make surface-mount fuses develop towards miniaturization, high power and high reliability. Under this design and process, high-reliability and high-current surface-mount fuses of different sizes can be produced. It can also be used in the development of low-voltage power system protection fuses to meet the use requirements of high-current surface-mount fuses under different needs.
[0018] The present invention can be widely applied to the technical field of surface-mount fuses. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a schematic diagram of the structure of the surface-mount fuse of the present invention.
[0020] Figure 2 The figure is a schematic diagram of the appearance structure of the surface mount fuse of the present invention.
[0021] Figure 2 a Main view, Figure 2 b is the top view, Figure 2 c is a side view.
[0022] In the figure: 1 is the shell, 2 is the melt, 3 is the arc suppression body, 4 is the transition layer, 5 is the welding layer, and 6 is the L-shaped pin. DETAILED DESCRIPTION
[0023] like Figure 1 As shown, the high current surface mount fuse and its manufacturing method, taking a surface mount fuse with a breaking capacity of 1500A@85VDC and a temperature rise of the fuse under rated current of less than 125°C as an example, the specific implementation method is as follows: The housing 1 is a cuboid.
[0024] The transition layer is a nickel layer, and the welding layer is a tin-lead layer.
[0025] The molten material is gold, silver, copper, etc., and the shape is a ribbon structure.
[0026] The organic polymer material is epoxy resin, melamine formaldehyde resin, silicone resin and the like.
[0027] The high molecular polymer is epoxy resin, PPS resin or polyurethane.
[0028] The arc extinguishing filler formula is: Main material: inorganic SiO2, mass ratio 70%~85%.
[0029] Other inorganic flame retardant materials: such as AlO3, MgO, Mg(OH)2, CaO, etc., with a mass ratio of 15%~30%.
[0030] The components of the granulation are: Inorganic system materials: mass ratio 60%~80%.
[0031] Organic polymer materials: mass ratio is 20%~40%.
[0032] The specific production method is: 1. Melt graphics simulation design and production The finite element simulation software is used to design and simulate the melt pattern, determine the melt pattern (the size of the non-melting area of the one-piece melt and the size and thickness of the melting area, etc.), the cold resistance of the melt (the cold resistance value is determined according to the set current specification), the temperature rise of the melt at the rated current <125°C, the melt material and other parameters. After the melt design parameters are determined, the metal strip (whose material can be gold, silver, copper, etc.) is processed and manufactured into the melt by stamping according to the melt processing drawings.
[0033] 2. Preparation of arc extinguishing filler The mass ratio of inorganic SiO2 is 70%~85%, and the mass ratio of other inorganic flame retardants (AlO3, MgO, Mg(OH)2, CaO, etc.) is 15%~30%. The inorganic system materials are mixed with organic polymer materials such as epoxy resin, melamine formaldehyde resin, silicone resin, etc. for mixing, granulation and molding to make composite arc-extinguishing fillers, of which the mass ratio of inorganic system materials is 60%~80%, and the mass ratio of organic polymer materials is 20%~40%. This can meet the breaking capacity requirements of 1000A@85VDC.
[0034] 3. Molding of melt and arc-extinguishing filler The melt and the arc-extinguishing filler are molded into an integral structure using a molding device to produce an internal semi-finished product with a size of 6.3 mm×4.8 mm×3.3 mm.
[0035] 4. Product packaging The product shell uses high molecular polymers such as epoxy resin, PPS resin, and polyurethane, and the mold is designed according to the product shell packaging size of 7.3mm×5.8mm×4.3mm. The semi-finished product after the melt and arc extinguishing material are molded is packaged, and the high molecular polymer is used as the product packaging shell to package the melt and arc extinguishing filler.
[0036] 5. External electrode plating treatment The thickness of the nickel-plated transition layer is 2 microns to 4 microns, the thickness of the tin-lead soldering layer is 4 microns to 12 microns, and the lead content is 3% to 20%.
[0037] The high-current surface-mount fuse manufactured by the present invention has high internal filling density, and the internal filling uses a polymer adhesive phase to connect the arc-extinguishing filling and the melt together to form a full-solid structure. At the same time, a polymer is used to manufacture a product shell, and the internal semi-finished product is encapsulated to form a full-solid structure as a whole. The manufactured product has strong impact and vibration resistance, excellent arc extinguishing performance, resistance to organic solvents, resistance to moisture and heat, etc., and its breaking capacity can reach 1500A@85VDC. The production method is convenient and efficient.
[0038] Finally, it should be noted that the above embodiments are merely examples for the purpose of clear explanation. The present invention includes but is not limited to the above embodiments. It is not necessary and impossible to list all implementation methods exhaustively. For ordinary technicians in the relevant field, other different forms of changes or modifications can be made based on the above description. All implementation methods that meet the requirements of the present invention belong to the protection scope of the present invention.
Claims
1. A high current surface mount fuse, characterized in that: Including shell, melt, arc suppression body, transition layer, welding layer, L-shaped pin; The shell is in a square shape; The melt and the L-shaped pin are made in one piece, and the L-shaped pin is led out from the two ends of the bottom of the shell and is located at the two ends of the bottom and the two ends of the side of the shell; The melt is located in the arc suppression body, and the melt and the arc suppression body are located in the shell; The surfaces of the L-shaped pin are a transition layer and a welding layer from the inside to the outside.
2. A high current surface mount fuse as claimed in claim 1, characterized in that: The material of the melt is gold, silver or copper, and the shape of the melt is a ribbon structure.
3. A high current surface mount fuse as claimed in claim 1, characterized in that: The material high molecular polymer of the shell is epoxy resin, PPS resin or polyurethane.
4. A high current surface mount fuse as claimed in claim 1, characterized in that: The arc extinguishing material formula of the arc suppression body is: Inorganic SiO2, mass ratio 70%~85%; Inorganic flame retardant materials other than inorganic SiO2, mass ratio is 15%~30%.
5. A high current surface mount fuse as claimed in claim 1, characterized in that: The components of the granulation of the arc-suppressing body are: Inorganic materials: mass ratio 60%~80%; Organic polymer materials: mass ratio is 20%~40%.
6. A high current surface mount fuse as claimed in claim 5, characterized in that: The organic polymer material is epoxy resin, melamine formaldehyde resin or silicone resin.
7. A high current surface mount fuse as claimed in claim 1, characterized in that: The transition layer is a nickel layer, and the welding layer is a tin-lead layer.
8. The method for manufacturing a high current surface mount fuse according to claim 1, characterized in that , including the following methods: (1) Melt pattern simulation design and production Use finite element simulation software to design and simulate the melt pattern, determine the size and thickness of the non-melting area and the melting area of the one-piece melt, determine the cold resistance of the melt, the temperature rise of the melt under the rated current, and the melt material parameters according to the set current specifications, and after the melt design parameters are determined, process and manufacture the melt material according to the design drawings to form a melt; (2) Preparation of arc-extinguishing filler Arc-extinguishing fillers are prepared by selecting inorganic SiO2 and inorganic flame retardant system materials other than inorganic SiO2, and the inorganic system materials are mixed into organic polymer materials for mixing, granulation and molding to make composite arc-extinguishing fillers; (3) Molding of melt and arc-extinguishing filler The melt and the arc-extinguishing filler are molded into an integral structure using a molding device to produce an internal semi-finished product of a set shape and size; (4) Product packaging The shell is made of high molecular polymer, and the mold is designed according to the shell packaging size, and the semi-finished products after the melt and arc extinguishing material are molded are packaged; (5) External electrode plating treatment The external electrodes of the packaged product are electroplated with a transition layer and a welding layer in sequence to form the final product.
9. The method for manufacturing a high current surface mount fuse according to claim 8, characterized in that: The specific production method is: (1) Melt pattern simulation design and production The temperature rise of the melt at rated current is less than 125℃; (2) Preparation of arc-extinguishing filler The mass ratio of inorganic SiO2 is 70% to 85%, and the mass ratio of flame retardant AlO3, MgO, Mg(OH)2 or CaO is 15% to 30%. The inorganic system material is mixed with the organic polymer material epoxy resin, melamine formaldehyde resin or silicone resin for mixing, granulation and molding to make the composite arc-extinguishing filler. The mass ratio of the inorganic system material is 60% to 80%, and the mass ratio of the organic polymer material is 20% to 40%. (3) Molding of melt and arc-extinguishing filler The melt and the arc-extinguishing filler are molded into an integral structure using a molding device to produce an internal semi-finished product with a size of 6.3 mm×4.8 mm×3.3 mm; (4) Product packaging The shell is made of high molecular polymer epoxy resin, PPS resin or polyurethane. The mold is designed according to the shell packaging size of 7.3mm×5.8mm×4.3mm. The semi-finished product after the melt and arc extinguishing material are molded is packaged. The high molecular polymer is used as the product packaging shell to package the melt and arc extinguishing filler; (5) External electrode plating treatment The thickness of the nickel-plated transition layer is 2 microns to 4 microns, the thickness of the tin-lead soldering layer is 4 microns to 12 microns, and the lead content of the tin-lead soldering layer is 3% to 20%.
10. The method for manufacturing a high current surface mount fuse according to claim 1, characterized in that: The transition layer or welding layer is a single layer or a composite layer.