Fin-shaped electron channel semiconductor device and fin-shaped complementary semiconductor device

By forming a stepped structure and a nitride semiconductor layer on the substrate, combining the compound semiconductor layer and buried layer, the problems of low integration and normally open per unit area of ​​existing semiconductor devices are solved, and high integration density and safe and reliable fins are achieved electronic channel semiconductor device.

CN119050152APending Publication Date: 2024-11-29GUANGDONG ZHINENG TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411185387.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2019-04-12
Filing Date
2020-04-13
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The structural design of existing semiconductor devices results in low integration per unit area, and normally open devices are not suitable in many applications, affecting energy conservation and safety.

Method used

Using the method of manufacturing a fin-shaped electron-channel semiconductor device, by forming a step-like structure on the substrate, vertically growing a nitride semiconductor layer, and forming a compound semiconductor layer thereon to form a two-dimensional hole gas and electron gas, combined with P The type buried layer and gate dielectric layer realize the normal off state and high integration density of the device.

Benefits of technology

It realizes high threshold voltage, low on-resistance, safe and reliable semiconductor devices, and is simple in process and low in cost, which can achieve higher channel density and integrated density per unit area.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119050152A_ABST
    Figure CN119050152A_ABST
Patent Text Reader

Abstract

The invention provides a fin-shaped electron channel semiconductor device and a fin-shaped complementary type semiconductor device. The semiconductor device includes a group III nitride device of a plurality of hole channels and a group III nitride device of a plurality of electron channels. Wherein the III-group nitride device of the hole channel and the III-group nitride device of the electron channel are correspondingly arranged. The III-nitride device of the electron channel is provided with a fin-shaped channel, and two-dimensional hole gas and / or two-dimensional electron gas can be formed at the interface of the compound semiconductor layer and the nitride semiconductor layer at the same time. The present disclosure provides a normally closed electron and / or hole channel group III nitride transistor having high performance, safety, and energy saving, having a simple process, low cost, achieving higher channel density per unit area, having high withstand voltage, high power, and low on-resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the semiconductor field, and more specifically, to a fin-shaped electronic channel semiconductor device and a fin-shaped complementary semiconductor device. Background Art

[0002] Group III nitride semiconductors are an important new type of semiconductor material, mainly including AlN, GaN, InN and compounds of these materials such as AlGaN, InGaN, AlInGaN, etc. Group III nitride semiconductors have great prospects in the fields of power semiconductors and wireless communications by utilizing the advantages of direct band gap, wide bandgap, high breakdown electric field strength, etc. through the optimization design of device structure and process.

[0003] In addition, the structural design of existing semiconductor devices is mostly lateral devices, and the integration per unit area is not high enough; and the existing III-nitride semiconductor devices are normally-on devices, that is, when there is no bias on the third electrode, the device is in the on state. However, in many applications, semiconductor devices must be normally-off devices, which is also not conducive to energy conservation and application safety.

[0004] Based on this, the present disclosure provides a fin-shaped electron channel semiconductor device and a fin-shaped complementary semiconductor device, aiming to overcome the above-mentioned defects and provide a high-performance, safe and energy-saving semiconductor device with simple process, low cost, higher channel density per unit area, simultaneous electron channel and hole channel, high withstand voltage, high power and low on-resistance. Summary of the invention

[0005] A brief overview of the present disclosure will be given below in order to provide a basic understanding of certain aspects of the present disclosure. It should be understood that this overview is not an exhaustive overview of the present disclosure. It is not intended to identify key or important parts of the present disclosure, nor is it intended to limit the scope of the present disclosure. Its purpose is simply to give certain concepts in a simplified form as a prelude to a more detailed description discussed later.

[0006] According to one aspect of the present disclosure, a method for manufacturing a fin-shaped electronic channel semiconductor device is provided, comprising:

[0007] A substrate is provided, and a step-like structure is etched on the upper surface of the substrate, wherein the step-like structure has a first plane and a second plane that are substantially parallel, and a third surface that connects the first plane and the second plane respectively, and the lattice of the third surface has hexagonal symmetry;

[0008] Taking the third surface as the core and limited by the second plane, epitaxially growing a fin-shaped nitride semiconductor layer upward and perpendicular to the second plane;

[0009] A first compound semiconductor layer (130) is formed on the nitride semiconductor layer, thereby simultaneously forming a two-dimensional hole gas and an immovable background negative charge; and / or a two-dimensional electron gas and an immovable background positive charge at an interface between the first compound semiconductor layer (130) and the nitride semiconductor layer.

[0010] Furthermore, the substrate is selected from Al2O3, 4H-SiC, (110)-faced silicon or (112)-faced silicon.

[0011] Furthermore, the third surface is selected from the (0001) surface of Al2O3, the (0001) surface of 4H-SiC and the (111) surface of silicon.

[0012] Furthermore, a first insulating layer is formed on other surfaces of the substrate except the third surface.

[0013] Furthermore, the method for forming the first insulating layer includes coplanarly depositing SiN on the substrate, retaining only the SiN on the third surface through a vertically oriented etching technique, and then forming a silicon dioxide layer on other surfaces except the third surface, and then removing the SiN on the side wall through wet etching, retaining the silicon dioxide layer on the other surfaces.

[0014] Furthermore, it also includes forming a seed layer at the third surface, wherein the seed layer is formed on a portion of the third surface; or the seed layer is formed on the entire surface of the third surface.

[0015] Furthermore, the polycrystalline or amorphous layer formed by the seed layer material is removed or retained on the first insulating layer.

[0016] Furthermore, when the substrate is a silicon substrate, it must have the seed layer.

[0017] Furthermore, the method further comprises epitaxially growing a buffer layer laterally with the seed crystal layer as the core.

[0018] Furthermore, the method further comprises the step of epitaxially growing a first nitride semiconductor layer (110) with the seed layer or the buffer layer as the core.

[0019] Furthermore, the method further comprises the step of epitaxially growing a P-type buried layer with the first nitride semiconductor layer (110) as the core.

[0020] Furthermore, the buried layer can deplete 95-100% of the two-dimensional electron gas.

[0021] Furthermore, the P-type buried layer and the two-dimensional electron gas can form a body diode, thereby protecting the device.

[0022] Furthermore, the method further comprises continuing to laterally epitaxially grow a second nitride semiconductor layer (120) with the first nitride semiconductor layer (110) or the buried layer as a core.

[0023] Furthermore, the materials of the first nitride semiconductor layer (110) and the second nitride semiconductor layer (120) are the same or different.

[0024] Furthermore, the first nitride semiconductor layer (110) is N-type GaN or P-type GaN, and the second nitride semiconductor layer (120) is intrinsic GaN or N-type GaN.

[0025] Furthermore, it also includes exposing the (0001) surface of the first trench layer; or exposing the (0001) and noodle.

[0026] Furthermore, it also includes removing the first nitride semiconductor layer direction of the first compound semiconductor layer.

[0027] Furthermore, in the first nitride semiconductor layer A fourth insulating layer is formed in the direction.

[0028] Furthermore, when the second nitride semiconductor layer is N-type GaN, the P-type buried layer and the second nitride semiconductor layer form a PN structure.

[0029] Furthermore, the method further comprises depositing a second compound semiconductor layer (160) before depositing the first compound semiconductor layer (130).

[0030] Furthermore, the second compound semiconductor layer (160) is unintentionally doped or intrinsic GaN; or the compound semiconductor layer 160 is selected from AlN, InGaN, AlInN or AlInGaN.

[0031] Furthermore, it also includes forming a first electrode, a second electrode and a third electrode of the device.

[0032] Furthermore, the first electrode and the second electrode are in physical contact with the nitride semiconductor layer of the device and in ohmic contact with the two-dimensional electron gas; or the first electrode and the second electrode are in physical contact with the compound semiconductor layer to form ohmic contact.

[0033] Furthermore, the third electrode forms a Schottky contact or an insulating contact with the first compound semiconductor layer.

[0034] Furthermore, the insulating contact is a gate dielectric layer formed on the first compound semiconductor layer at a position corresponding to the third electrode.

[0035] Furthermore, the gate dielectric layer is formed by forming the first compound semiconductor layer (130) by MOCVD and then growing the gate dielectric layer in-situ; or the gate dielectric layer is grown separately in a growth device different from that of the first compound semiconductor layer (130).

[0036] Furthermore, the first electrode, the third electrode and the second electrode are arranged in sequence in a direction substantially perpendicular to the first plane of the substrate, and the positions of the first electrode and the second electrode can be interchanged.

[0037] Furthermore, the method also includes forming a body electrode connected to the buried layer.

[0038] Further, the body electrode is formed by physically contacting the buried layer.

[0039] Furthermore, the body electrode is formed by ohmic contact with the two-dimensional hole gas, and the body electrode is electrically connected to the buried layer through the two-dimensional hole gas.

[0040] Furthermore, the body electrode depletes all or part of the two-dimensional hole gas between the second and third electrodes when the device is turned off, leaving only the background negative charge, thereby offsetting the electric field generated by the background positive charge depleted when the device is turned off, making the electric field distribution more uniform.

[0041] Furthermore, the method for forming the second electrode further comprises forming a first metal layer on the first plane of the substrate, and isotropically etching away a small amount of the first metal layer deposited on the first compound semiconductor layer (0001) surface of the device.

[0042] Furthermore, the gate formation method further includes coplanarly depositing a second insulating layer on the first metal layer, the second insulating layer exposing the compound semiconductor layer 130 or the gate dielectric layer, and then forming a second metal layer on the second insulating layer, and isotropically etching to remove a small amount of the second metal layer deposited on the first compound semiconductor layer (0001) surface of the device.

[0043] Furthermore, the method for forming the first electrode further comprises coplanarly depositing a third insulating layer on the second metal layer, and then forming a third metal layer on the third insulating layer, and then forming the first electrode by photolithography and etching.

[0044] According to another aspect of the present disclosure, there is provided a fin-shaped electron channel semiconductor device, comprising:

[0045] A substrate having a stepped structure formed thereon, wherein the stepped structure has a first plane and a second plane that are substantially parallel to each other, and a third surface connecting the first plane and the second plane, respectively, and a lattice of the third surface has hexagonal symmetry;

[0046] A fin-shaped nitride semiconductor layer is epitaxially grown upward and perpendicular to the second plane with the third surface as the core and restricted by the second plane;

[0047] The first compound semiconductor layer (130) is formed on the nitride semiconductor layer, thereby simultaneously forming a two-dimensional electron gas and / or the two-dimensional hole gas at an interface between the first compound semiconductor layer and the nitride semiconductor layer.

[0048] Furthermore, the substrate is selected from Al2O3, intrinsic GaN, 4H-SiC, and (110)-plane silicon or (112)-plane silicon.

[0049] Furthermore, the nitride semiconductor layer includes a first nitride semiconductor layer and a second nitride semiconductor layer.

[0050] Furthermore, the third surface is selected from the (0001) surface of Al2O3, the (0001) surface of 4H-SiC and the (111) surface of silicon.

[0051] Furthermore, a first insulating layer is provided on other surfaces of the substrate except the third surface.

[0052] Furthermore, a seed layer is provided on the third surface of the substrate.

[0053] Furthermore, a polycrystalline or amorphous layer formed of the seed layer material is provided on the first insulating layer.

[0054] Furthermore, a buffer layer is provided outside the seed crystal layer, and the buffer layer has a single-layer or multi-layer structure.

[0055] Furthermore, the first nitride semiconductor layer (110) is provided outside the seed crystal layer.

[0056] Furthermore, the first nitride semiconductor layer (110) is provided outside the buffer layer.

[0057] Furthermore, a P-type buried layer is provided on the nitride semiconductor layer 110 , and the P-type buried layer and the two-dimensional electron gas form a body diode structure.

[0058] Furthermore, the second nitride semiconductor layer is formed on the first nitride semiconductor layer or the buried layer.

[0059] Furthermore, the materials of the first nitride semiconductor layer and the second nitride semiconductor layer are the same or different.

[0060] Furthermore, the first nitride semiconductor layer is N- or P-type GaN, and the second nitride semiconductor layer is intrinsic GaN or N-type GaN.

[0061] Furthermore, it also comprises a second compound semiconductor layer (160), wherein the second compound semiconductor layer (160) is unintentionally doped GaN, InGaN, AlN, AlInGaN.

[0062] Furthermore, in the first nitride semiconductor layer The first compound semiconductor layer is not provided in the direction.

[0063] Furthermore, a fourth insulating layer is provided in the <0001> direction of the first nitride semiconductor layer.

[0064] Furthermore, when the second nitride semiconductor layer is N-type GaN, the second nitride semiconductor layer and the buried layer form a body diode structure.

[0065] Furthermore, it also comprises a first electrode, a second electrode and a third electrode.

[0066] Furthermore, the first electrode / second electrode is in physical contact with the nitride semiconductor layer of the device and in ohmic contact with the two-dimensional electron gas; or the first electrode / second electrode is in physical contact with the first compound semiconductor layer to form an ohmic contact.

[0067] Furthermore, the third electrode forms a Schottky contact or an insulating contact with the first compound semiconductor layer.

[0068] Furthermore, the insulating contact has a gate dielectric layer between the third electrode and the compound semiconductor layer 130 .

[0069] Furthermore, the first, third and fourth electrodes are arranged in sequence in a direction substantially perpendicular to the first plane of the substrate; and the positions of the first and second electrodes can be interchanged.

[0070] Furthermore, it also has an integral electrode, and the body electrode is electrically connected to the buried layer. Through the setting of the body electrode, the body diode formed by the buried layer and the two-dimensional electron gas conducts a current in the opposite direction to the channel current of the transistor while stabilizing the threshold voltage; or through the connection of the body electrode, the circuit application of the body diode formed by the buried layer and the second nitride semiconductor layer composed of N-type GaN is realized.

[0071] Furthermore, the body electrode is physically connected to the buried layer, or the body electrode is in ohmic contact with the two-dimensional hole gas.

[0072] Furthermore, the first nitride semiconductor layer (110) is N-type doped in a region corresponding to the second electrode, and the second nitride semiconductor layer (120) is N-type doped in a region corresponding to the first electrode.

[0073] According to another aspect of the present disclosure, there is provided a fin-shaped electron channel semiconductor device, comprising:

[0074] a substrate, epitaxially growing a fin-shaped nitride semiconductor layer on an upper surface vertical to the substrate;

[0075] The nitride semiconductor layer includes first and second nitride semiconductor layers;

[0076] A first compound semiconductor layer (130) is formed on the nitride semiconductor layer, thereby simultaneously forming a two-dimensional hole gas and / or the two-dimensional electron gas at an interface between the first compound semiconductor layer (130) and the nitride semiconductor layer.

[0077] Furthermore, the substrate is selected from Al2O3, intrinsic GaN, 4H-SiC, and (110)-plane silicon or (112)-plane silicon.

[0078] Furthermore, a first insulating layer is provided on the upper surface of the substrate.

[0079] Furthermore, there is a seed crystal layer on the substrate.

[0080] Furthermore, a buffer layer is provided outside the seed crystal layer, and the buffer layer has a single-layer or multi-layer structure.

[0081] Furthermore, the first and second nitride semiconductor layers are stacked one above the other parallel to the upper surface of the substrate.

[0082] Furthermore, a P-type buried layer is sandwiched between the first and second nitride semiconductor layers.

[0083] Furthermore, the P-type buried layer and the two-dimensional electron gas form a body diode structure.

[0084] Furthermore, the materials of the first nitride semiconductor layer and the second nitride semiconductor layer are the same or different.

[0085] Furthermore, the first nitride semiconductor layer is N- or P-type GaN, and the second nitride semiconductor layer is intrinsic GaN or N-type GaN.

[0086] Furthermore, it also comprises a second compound semiconductor layer (160), wherein the second compound semiconductor layer (160) is unintentionally doped GaN, InGaN, AlN or AlInGaN.

[0087] Furthermore, the first compound semiconductor layer is not provided in the <000-1> direction of the first nitride semiconductor layer.

[0088] Furthermore, a fourth insulating layer is provided in the <000-1> direction of the first nitride semiconductor layer.

[0089] Furthermore, when the second nitride semiconductor layer is N-type GaN, the second nitride semiconductor layer and the buried layer form a body diode structure.

[0090] Furthermore, it also comprises a first electrode, a second electrode and a third electrode.

[0091] Furthermore, the first electrode / second electrode is in physical contact with the nitride semiconductor layer of the device and in ohmic contact with the two-dimensional electron gas; or the first electrode / second electrode is in physical contact with the first compound semiconductor layer to form an ohmic contact.

[0092] Furthermore, the third electrode forms a Schottky contact or an insulating contact with the first compound semiconductor layer.

[0093] Furthermore, the insulating contact has a gate dielectric layer between the third electrode and the first compound semiconductor layer.

[0094] Furthermore, the first, third and fourth electrodes are arranged in sequence in a direction substantially perpendicular to the first plane of the substrate; and the positions of the first and second electrodes can be interchanged.

[0095] Furthermore, there is an integral electrode, which is electrically connected to the buried layer.

[0096] Furthermore, the body electrode is physically connected to the buried layer, or the body electrode is in ohmic contact with the two-dimensional hole gas.

[0097] According to another aspect of the present disclosure, there is provided a fin-shaped complementary semiconductor device, comprising:

[0098] An electron channel semiconductor device as described above, and

[0099] A plurality of hole channel semiconductor devices, wherein the hole channel semiconductor devices are arranged opposite to the electron channel semiconductor device structure.

[0100] Further, wherein: the hole channel device has fourth, fifth and sixth electrodes.

[0101] Furthermore, the hole channel device and the electron channel semiconductor device forming the fourth to sixth electrodes can be symmetrically arranged.

[0102] Furthermore, the hole channel device has an N-type buried layer at the first nitride semiconductor layer corresponding to the sixth electrode.

[0103] Furthermore, the hole channel device has P-type doping in the corresponding nitride semiconductor layer corresponding to the fourth and fifth electrodes.

[0104] Furthermore, the hole channel device and the electron channel device have both N-type and P-type buried layers.

[0105] According to another aspect of the present disclosure, a radio frequency device is provided, comprising any device as described above.

[0106] According to another aspect of the present disclosure, an electric power device is provided, comprising any one of the devices described above.

[0107] The solution of the present disclosure can at least help achieve one of the following effects: the semiconductor device structure can reduce gate leakage current, has high threshold voltage, high power, and high reliability, can achieve low on-resistance and a normally-off state of the device, and can provide a stable threshold voltage, so that the semiconductor device has good switching characteristics and is safer in use.

[0108] The solution of the present disclosure can also help achieve one of the following effects: a higher channel density can be achieved per unit area; the integration density of the device is improved; the structure and preparation process of the device are relatively simple, which can effectively reduce production costs. BRIEF DESCRIPTION OF THE DRAWINGS

[0109] The following is a description of the specific contents of the present disclosure with reference to the accompanying drawings, which will help to more easily understand the above and other purposes, features and advantages of the present disclosure. The accompanying drawings are only for the purpose of illustrating the principles of the present disclosure. The sizes and relative positions of the units in the accompanying drawings are not necessarily drawn to scale. In the accompanying drawings:

[0110] Figure 1 -12 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to the first embodiment;

[0111] Fig.13 -15 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to the second embodiment;

[0112] Fig.16 -17 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to a third embodiment;

[0113] Fig.18 A schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to a fourth embodiment;

[0114] Fig.19 -21 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to a fifth embodiment;

[0115] Fig. 22 -25 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to a sixth embodiment;

[0116] Fig.26 -32 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to the seventh embodiment;

[0117] Fig.33 -34 is a schematic diagram showing a semiconductor device structure and a method for manufacturing the same according to an eighth embodiment;

[0118] Fig.35 -36 shows a schematic diagram of a semiconductor device structure and a method for manufacturing the same according to the eighth embodiment. DETAILED DESCRIPTION

[0119] Exemplary disclosures of the present disclosure are described below in conjunction with the accompanying drawings. For the sake of clarity and conciseness, not all features of implementing the present disclosure are described in the specification. However, it should be understood that many decisions specific to the present disclosure may be made in the process of developing any such implementation of the present disclosure in order to achieve the developer's specific goals, and these decisions may vary from one disclosure to another.

[0120] It should also be noted here that in order to avoid obscuring the contents of the present disclosure due to unnecessary details, only device structures closely related to the solutions according to the contents of the present disclosure are shown in the drawings, while other details that are not closely related to the contents of the present disclosure are omitted.

[0121] It should be understood that the present disclosure is not limited to the described implementation forms due to the following description with reference to the accompanying drawings. In the present disclosure, features between different embodiments may be replaced or borrowed, and one or more features may be omitted in one embodiment, where feasible.

[0122] In the following specific embodiments, reference may be made to the accompanying drawings, which form a part of the present disclosure and illustrate exemplary embodiments. In addition, it will be understood that other embodiments may be utilized and structural and / or logical changes may be made without departing from the scope of the claimed subject matter. It should also be noted that directions and references (e.g., up, down, top, bottom, etc.) are only used to assist in the description of features in the accompanying drawings and are not intended to be limited to the following specific embodiments.

[0123] As used in the specification of the present disclosure and the appended claims, the singular forms "a", "an", and "the" include the plural forms as well, unless the context clearly indicates otherwise. It will also be understood that the term "and / or" as used herein refers to and includes any and all possible combinations of one or more of the associated listed items.

[0124] There are two main crystal structures of III-nitride semiconductors: wurtzite and zinc-blende. Due to the advantages of stability and the ease of obtaining high crystal quality, the III-nitride semiconductors used in practical applications usually have a wurtzite structure.

[0125] Therefore, in particular, the semiconductor device structure of the present disclosure includes a Group III nitride device using a wurtzite crystal structure. Further, the Group III nitride device is a normally-off nitride semiconductor device.

[0126] First embodiment

[0127] Reference Figure 1 -12 to describe the fin-shaped semiconductor device and the method for manufacturing the same according to the first embodiment.

[0128] like Figure 1As shown in Figure 3, in the first embodiment, the semiconductor device includes a substrate 100, and the substrate 100 can be made of independent or bulk gallium nitride materials. Since the preparation of gallium nitride bulk materials is very expensive, a feasible way is to epitaxially grow the gallium nitride semiconductor layer on a foreign substrate and make the device. The foreign substrate materials mainly include sapphire (Al2O3), Si and SiC. Among them, the (0001) plane of sapphire, the (0001) plane of SiC and the (111) plane of Si all have a hexagonal symmetrical lattice structure, which is suitable as a substrate for heterogeneous growth. The gallium nitride semiconductor layer nucleates and grows thereon, which is most conducive to obtaining higher quality GaN or AlN crystals.

[0129] Furthermore, sapphire substrates are widely used due to their low cost and the lattice matching between the gallium nitride epitaxial layer and the sapphire substrate. Taking heat dissipation into consideration, more and more gallium nitride semiconductor layers are prepared using silicon substrates, but the use of silicon substrates requires consideration of leakage current and withstand voltage issues. The process flow disclosed in the present invention is carefully designed to avoid the impact of silicon substrate materials on device performance, and is significantly helpful in improving withstand voltage and reducing dark current.

[0130] In summary, the material of the heterogeneous substrate can be selected according to actual needs, and the present disclosure does not limit the specific material of the substrate, as long as the substrate material can satisfy the lattice structure with hexagonal symmetry on the side surface of the vertical groove formed on its surface plane and perpendicular to its surface plane. In the present disclosure, the substrate material can be sapphire (Al2O3), SiC, silicon, and independent or bulk intrinsic gallium nitride materials, etc.

[0131] In this disclosure Figure 1 As shown, a substrate 100 includes a first plane 1001, and a structure including a third surface perpendicular to the first plane of the substrate is formed on the substrate 100 by etching. Exemplarily, the structure may be a stepped structure, which consists of the first plane 1001 of the substrate 100, a second plane 1002 parallel to the first plane, and a third surface 1003 respectively connecting the first plane 1001 and the second plane 1002, and the third surface has hexagonal symmetry. Exemplarily, the step height of the step is about 5 microns.

[0132] A seed layer 101 is formed on the third surface, and the seed layer 101 can be on a part of the third surface, or on the entire surface of the third surface. For silicon materials, due to the influence of the Ga atom melt-back effect, semiconductor layers such as gallium nitride cannot be grown directly on the substrate. It is usually necessary to grow structures such as AlN and gallium nitride seed layers on the substrate to further grow gallium nitride epitaxial layers. The gallium nitride layer can be directly nucleated and grown on Al2O3 (sapphire), SiC, or intrinsic GaN, but from the perspective of crystal control quality, it is also preferred to introduce the seed layer 101 during the process.

[0133] With the seed layer 101 as the core, and limited by the second plane 1002 of the substrate 100, the nitride semiconductor layer 110 is epitaxially grown vertically to the second plane, and then the nitride semiconductor layer 120 is epitaxially grown laterally. The materials of the nitride semiconductor layer 110 and the nitride semiconductor layer 120 can be the same or different. Exemplarily, the nitride semiconductor layer 110 is an N-type doped GaN layer or a P-type doped GaN layer; the nitride semiconductor layer 120 is an intrinsic GaN layer or an N-type doped GaN layer. Exemplarily, the doping concentration of the N- or P-type can be 1E17-1E20 / cm3. It can be understood that the seed layer and the nitride semiconductor layer can be formed on the upper surface of the substrate 100 without forming a stepped structure, but the directionality of the growth should be met.

[0134] Optional, such as Figure 2 As shown, a semiconductor layer 140 can also be provided between the seed layer 101 and the nitride semiconductor layer 110. The semiconductor layer is used as a buffer layer. The semiconductor layer can have a single-layer or multi-layer structure. The material of the semiconductor layer can be, for example, one or more of AlN, GaN, AlGaN, InGaN, AlInN and AlGaInN.

[0135] Preferably, corresponding N-type doping is performed in the partial regions of the nitride semiconductor layer 110 and the nitride semiconductor layer 120 corresponding to the source / drain of the device; the doping can effectively reduce the contact resistance of the source / drain region, and the N-type doping concentration can be 1E17-1E20 / cm3.

[0136] The nitride semiconductor layer 120 covering and perpendicular to the nitride semiconductor layer 110 is removed to expose the nitride semiconductor layer 110. A compound semiconductor layer 130 is formed on the nitride semiconductor layer 110 and the nitride semiconductor layer 120, such as AlGaN.

[0137] If the nitride semiconductor layer 110, the nitride semiconductor layer 120 and the compound semiconductor layer 130 are made of group III nitride semiconductors, since group III nitride semiconductors have polarity, fixed polarization charges may exist on the surface of the polar semiconductor or at the interface between two different polar semiconductors. The presence of these fixed polarization charges attracts movable holes and electrons to form two-dimensional hole gas 2DHG and two-dimensional electron gas 2DEG. The generation of these two-dimensional hole gas 2DHG and two-dimensional electron gas 2DEG does not require an additional electric field, nor does it rely on the doping effect in the semiconductor. They are spontaneously generated. Since doping is not required, the two-dimensional carrier gas (two-dimensional hole gas and two-dimensional electron gas) is greatly reduced by ion scattering, and therefore has a higher carrier mobility.

[0138] Remove the covering perpendicular to the nitride semiconductor layer 110 The nitride semiconductor layer 120 in the direction of <0001> is exposed to expose the nitride semiconductor layer 110. A compound semiconductor layer 130, such as AlGaN, is formed on the nitride semiconductor layer 110 and the nitride semiconductor layer 120. A two-dimensional hole gas 2DHG is formed at the interface between the nitride semiconductor layer 110 and the nitride semiconductor layer 120 in the <0001> direction and the compound semiconductor layer 130, and a two-dimensional electron gas 2DEG is formed at the interface between the nitride semiconductor layer 110 and the nitride semiconductor layer 120 in the <0001> direction and the compound semiconductor layer 130.

[0139] A first electrode 200, a second electrode 210 and a third electrode 220 of a HEMT device are formed. The positions of the first electrode 200 to the third electrode 220 are not specifically limited, wherein the first electrode may be the source of the device, the second electrode may be the drain of the device, and the third electrode may be the gate of the device; the first and second electrodes may be in physical contact with the channel layer (110 / 120) of the device and in ohmic contact with the two-dimensional electron carrier gas (2DEG), or the first and second electrodes may be in physical contact directly with the compound semiconductor layer 130 and form ohmic contact. And the third electrode 220 can form an insulating contact or a Schottky contact with the compound semiconductor layer 130 on the compound semiconductor layer 130, wherein the insulating layer contact refers to forming a gate dielectric layer 300 between the third electrode and the compound semiconductor layer 130, and the gate dielectric layer can be SiO2, SiN, high-K dielectric material, etc. The gate dielectric layer 300 can play a role in passivating the surface of the compound semiconductor layer 130, which plays a very important role in reducing the gate leakage current of the device and the application of the device in the field of power electronics.

[0140] When the gate is directly made on the compound semiconductor layer 130, it has a larger gate leakage current. At this time, the compound semiconductor layer 130 also plays the role of a dielectric layer while maintaining a sufficiently high bandgap width. However, the devices made in this way are mostly used in the radio frequency (RF) field.

[0141] For example, Figure 3 As shown, the first electrode 200, the second electrode 210 and the third electrode 220 can be arranged in a direction perpendicular to the first plane of the substrate 100. The second electrode 210 is closer to the first plane 1001 of the substrate 100. It can be understood that the first electrode can also be closer to the first plane 1001 of the substrate 100.

[0142] Now refer to Figure 4 -12 will be described in detail the manufacturing method for manufacturing the semiconductor device of the first embodiment.

[0143] Step 1, such as Figure 4 As shown, a substrate 100 is provided, a photolithography pattern is formed on the substrate 100, and then a step-like structure is formed by etching the upper surface thereof, and illustratively, the etching depth is about 5 microns. The step-like structure is composed of a first plane 1001 of the substrate 100, a second plane 1002 parallel to the first plane 1001, and a third surface 1003 respectively connecting the first plane 1001 and the second plane 1002, wherein the third surface has a hexagonal symmetrical lattice structure, and the third surface with a hexagonal symmetrical lattice structure is easy for the nucleation and growth of nitride semiconductors, while other surfaces are not easy for the nucleation and growth of nitride semiconductors.

[0144] Step 2: If Figure 5 As shown, a seed layer 101 is formed on the third surface, and the seed layer 101 can be formed on a portion of the third surface, or on the entire surface of the third surface. The seed layer material is exemplified by GaN, ALN, etc.

[0145] For silicon materials, due to the influence of the Ga atom melt-back effect, GaN cannot be grown directly on the substrate. Usually, structures such as a seed layer need to be grown on the substrate before further growing the GaN epitaxial layer.

[0146] Step 3: If Figure 6 As shown in the figure, with the seed layer 101 as the core, and limited by the second plane 1002 of the substrate 100, a buffer layer 140 is epitaxially grown upward along the third surface of the substrate and sideways along the second plane of the substrate, and then a nitride semiconductor layer 110 is epitaxially grown laterally; it can be understood that the buffer layer is not necessary, so it can be as shown in Figure 7As shown, a nitride semiconductor layer 110 is epitaxially grown with the seed crystal layer as the core.

[0147] Step 4: Figure 8 As shown, the nitride semiconductor layer 110 is taken as the core, and then the nitride semiconductor layer 120 is grown laterally epitaxially. The materials of the nitride semiconductor layer 110 and the nitride semiconductor layer 120 may be the same or different. For example, N-type doping or P-type doping may be performed during the lateral epitaxial growth of the nitride semiconductor layer 110. It is understood that here, the subsequent formation of the drain electrode on the nitride semiconductor layer 110 is taken as an example. If the subsequent source electrode is formed at the nitride semiconductor layer 110, N-type doping or P-type doping is performed during the lateral epitaxial growth of the nitride semiconductor layer 120.

[0148] Furthermore, corresponding N-doping may be performed in the nitride semiconductor layer 120 at the locations where first and second electrode regions (ie, drain / source regions) are subsequently formed corresponding to the device, and the corresponding doping may effectively reduce the contact resistance of the corresponding regions.

[0149] Step 5: Fig. 9 As shown, while removing the covering layer perpendicular to the nitride semiconductor layer The nitride semiconductor layer 120 in the direction of the nitride semiconductor layer 110 is exposed. The (0001) surface of the nitride semiconductor layer 110 is exposed. Fig.10 As shown, a compound semiconductor layer 130, such as AlGaN, is formed on the nitride semiconductor layer 110 and the nitride semiconductor layer 120. 2DHG and immovable background negative charges are formed at the interface between the nitride semiconductor layer 110 and the nitride semiconductor layer 120 and the compound semiconductor layer 130 in the <0001> direction; 2DEG and immovable background positive charges are formed at the interface between the nitride semiconductor layer 110 and the nitride semiconductor layer 120 and the compound semiconductor layer 130 in the <0001> direction.

[0150] Step 6: Fig.11As shown, the first electrode to the third electrode of the device are formed on the nitride semiconductor layer in the <0001> direction; the positions of the first electrode 200 (source), the second electrode 210 (drain) and the third electrode 220 (gate) are not specifically limited, and the first and second electrodes can be in physical contact with the channel layer (110 / 120) of the device and in ohmic contact with the two-dimensional electron gas (2DEG), or the first electrode and the second electrode are directly in physical contact with the compound semiconductor layer 130 to form an ohmic contact, and the third electrode on the compound semiconductor layer 130 can form an insulating contact or a Schottky contact with the compound semiconductor layer 130.

[0151] wherein the insulating layer contacts Fig.12 The figure shows that a gate dielectric layer 300 is formed between the third electrode and the compound semiconductor layer 130. The gate dielectric layer 300 can be formed by in-situ growth after the compound semiconductor layer 130 is formed in an MOCVD chamber. The gate dielectric layer 300 can also be grown separately in a growth device different from the compound semiconductor layer 130. However, it should be noted that the quality of the gate dielectric layer grown in-situ is better, so it is preferred to grow the insulating layer in-situ.

[0152] The gate dielectric layer can be silicon dioxide, SiN, high-K dielectric material, etc. The gate dielectric layer 300 can play a role in passivating the surface of the compound semiconductor layer 130, which plays a very important role in reducing the gate leakage current of the device and the application of the device in power electronics. If the third electrode is directly made on the compound semiconductor layer 130, the device made in this way is more used in radio frequency (RF) devices, because compared with the device with a gate dielectric layer, it has a larger gate leakage current.

[0153] Exemplarily, the first electrode to the third electrode may be arranged in a direction perpendicular to the first plane of the substrate 100. The second electrode is closer to the first plane 1001 of the substrate 100. The third electrode is located between the second electrode and the first electrode.

[0154] Preferably, when N-type doping exists in the source region and the drain region of the N channel in the nitride semiconductor layer 110 and the nitride semiconductor layer 120, the first electrode and the second electrode are in physical contact with the channel layer of the device, which is more conducive to reducing the ohmic contact resistance.

[0155] This embodiment greatly improves the integration of the device by growing a fin-shaped III-nitride HEMT device with an irregular cross section on the third surface, can effectively reduce gate leakage current, and has a simple preparation process.

[0156] Second embodiment

[0157] Reference Fig.13 -15 to describe a Group III nitride device and a method for manufacturing the same according to the second embodiment.

[0158] The difference between the structure and method of the second embodiment and the first embodiment is that: Fig.13 As shown, a P-type buried layer 150 is provided between the nitride semiconductor layer 110 and the nitride semiconductor layer 120 .

[0159] The specific manufacturing method is as follows Fig.14 As shown, in step 4, with the AlN seed layer as the core, restricted by the second plane 1002 of the substrate 100, after the nitride semiconductor layer 110 is epitaxially grown laterally, before the nitride semiconductor layer 120 is epitaxially grown laterally, a P-type buried layer is first formed by lateral epitaxy, and the P-type buried layer is exemplarily a P-type GaN layer. Then, the nitride semiconductor layer 120 is epitaxially grown laterally with the buried layer as the core. The doping concentration covering the P-type buried layer is exemplarily 1E17-1E20 / cm3, and more preferably 1E+18 / cm3-5E+19 / cm3. The P-type GaN layer can deplete the two-dimensional electron gas in the channel layer, thereby causing the device to have a normally closed state; it is understandable that the doping can be gradual, which will not be repeated here. Further, the projection of the P-type buried layer in the <0001> direction falls within the projection range of the third electrode in the direction, or has a partial overlapping range with the projection of the third electrode in the direction. The configuration of the P-type buried layer, such as its doping concentration, size parameters, etc., can be set through device parameters to exhaust 95%-100% of the two-dimensional electron gas above it. The higher the concentration of the two-dimensional electron gas, the higher the corresponding doping concentration can be.

[0160] Then as Fig.15 As shown, the nitride semiconductor layer 120 and the buried layer covering the direction perpendicular to the nitride semiconductor layer 110 <0001> are removed at the same time, exposing the (0001) surface of the nitride semiconductor layer 110 and removing the nitride semiconductor layer covering the direction perpendicular to the nitride semiconductor layer 110. The nitride semiconductor layer 120 and the buried layer in the direction of the nitride semiconductor layer 110 are exposed. noodle.

[0161] It can be understood that when the P-type GaN layer is formed, the P-type GaN layer and the two-dimensional electron gas channel also realize the structure of a body diode at the same time.

[0162] Furthermore, the P-type GaN layer forms a natural PN structure integrated with the two-dimensional electron gas channel in the device structure while causing the device to have a normally closed state, wherein the two-dimensional electron gas constitutes the "N" part of the PN structure. This natural PN structure can be used in various circuit applications through the connection of electrodes. Exemplarily, in circuit applications, the PN structure can conduct current in the opposite direction to the HEMT current direction, enriching the design and function of the circuit.

[0163] Third embodiment

[0164] Reference Fig.16 -17 to describe a Group III nitride device and a method for manufacturing the same according to a third embodiment.

[0165] The third embodiment differs from the first / second embodiment only in that it further comprises an integral electrode 230, which is connected to the P-type buried layer. Fig.16 As shown, the body electrode 230 can be formed by etching the non-polar or semi-polar surface of the compound semiconductor layer 130 and the nitride semiconductor layer 120 to form a through hole reaching the P-type buried layer and then further filling it with metal.

[0166] It is understood that the method for forming the body electrode also includes: Fig.17 As shown, completely or partially removing the covering layer perpendicular to the nitride semiconductor layer The compound semiconductor layer 130 in the direction of the N-type buried layer is exposed to expose the P-type buried layer, and then the body electrode 230 is formed on the exposed N-type buried layer.

[0167] It should be noted that when the body electrode 230 is not present, the potential of the P-type semiconductor buried layer is floating, which is not conducive to stably controlling the threshold voltage of the device.

[0168] In addition, a PN structure is naturally formed between the P-type buried layer and the N-type GaN semiconductor layer 120 . The PN structure can enrich the design and function of the circuit by adjusting the voltage of the second electrode (source electrode) and the body electrode.

[0169] Fourth Implementation Method

[0170] Reference Fig.18 A Group III nitride device and a method for manufacturing the same according to a fourth embodiment will be described.

[0171] The fourth embodiment differs from the first / second embodiment only in that it further comprises an integral electrode 230, and the integral electrode 230 is in contact with the two-dimensional hole gas. It is understandable that the integral electrode 230 only needs to be in contact with the two-dimensional hole gas, and no further limitation is imposed on its specific position. The compound semiconductor layer 130 on the surface exposes the The nitride semiconductor layer 120 is formed on the surface of the nitride semiconductor layer 120, and the body electrode 230 is formed on the nitride semiconductor layer 120. Two-dimensional hole gas (2DHG) is formed at the interface of the nitride semiconductor layer 110 and the compound semiconductor layer 130 in the nitride semiconductor layer 120 based on spontaneous and piezoelectric effects. The body electrode is electrically connected to the P-type nitride semiconductor buried layer through the two-dimensional hole gas and controls its potential.

[0172] It should be noted that when the body electrode 230 is not present, the potential of the P-type semiconductor buried layer is floating, which is not conducive to stably controlling the threshold voltage of the device. At this time, the two-dimensional hole gas spontaneously formed in the nitride semiconductor layer is used, and the two-dimensional hole gas is indirectly electrically connected to the P-type semiconductor buried layer to control the potential of the P-type buried layer, thereby making the setting of the body electrode more flexible. It can be further understood that the PN structure in the above-mentioned embodiment 2 and embodiment 3 can also be applied to the circuit through the connection method between the body electrode and the two-dimensional hole gas in this embodiment. For example, the PN structure can conduct the current in the opposite direction relative to the HEMT current direction, enriching the design and function of the circuit.

[0173] Furthermore, since there are immovable background negative charges in the nitride semiconductor layer when the two-dimensional hole gas is spontaneously formed, the background negative charges attract the two-dimensional hole gas, so that the body electrode is at a high voltage during the device shutdown process, and the 2DEG is depleted, leaving the background positive charge. The connection between the body electrode and 2DHG will also deplete all or part of the 2DHG between the gate and drain electrodes due to the electric field and expose the background negative charges. The background negative charges can partially offset the distribution of the electric field generated by the background positive charges and increase the voltage resistance of the device.

[0174] Fifth Implementation Method

[0175] Reference Fig.19 -21 to describe a Group III nitride device and a method for manufacturing the same according to a fifth embodiment.

[0176] The difference between the fifth embodiment and the second to fourth embodiments is that before forming the compound semiconductor layer 130 on the nitride semiconductor layer 110, the buried layer and the nitride semiconductor layer 120, a compound semiconductor layer 160 is further provided. As shown in the figure, the manufacturing method thereof may be that before depositing the compound semiconductor layer 130 in step 5 of the first embodiment, a compound semiconductor layer 160 is first deposited. The compound semiconductor layer 160 may be low-doped or unintentionally doped GaN. When the buried layer 130 depletes 95-100% of the 2DEG at the corresponding channel, due to ion scattering and other effects, the resistance of the device when it is turned on will be greatly increased. When the compound semiconductor layer 160 is low-doped or unintentionally doped GaN, the provision of the compound semiconductor layer 160 can significantly reduce the ion scattering effect caused by the P-type semiconductor buried layer, thereby reducing the on-resistance of the device.

[0177] In addition, by selecting the bandgap widths of the compound semiconductor layer 160 and the nitride semiconductor layer 110 and the nitride semiconductor layer 120, the compound semiconductor layer 160 has a further effect on the electron carrier velocity, and a greater difference in the bandgap width with the compound semiconductor layer 130 is obtained, and the compound semiconductor layer 160 is formed before the compound semiconductor layer 130 is grown, which has little change to the process flow. Exemplarily, the compound semiconductor layer 160 can be InGaN, AlInGaN, AlInN or AlN.

[0178] Sixth Implementation Method

[0179] Reference Fig. 22 -25 to describe a III-nitride device and a method for manufacturing the same according to a sixth embodiment.

[0180] The sixth embodiment is different from the first to fifth embodiments in that: on the other surfaces of the substrate except the third surface 1003, a Fig. 22 An insulating layer 310 is shown. Preferably, the insulating layer completely covers the other surfaces.

[0181] It should be noted that when the substrate is a Si substrate, due to the (111) surface of the Si substrate and There is no difference in properties between the surfaces, so the third surface 1003 of the substrate can be the (111) surface of the Si substrate or The Si substrate may be a Si substrate with a (110) or (112) surface. The insulating layer may prevent Ga atoms from melting back the Si substrate during growth. In addition, since the seed layer, for example, the selective growth of AlN is very difficult, that is, in addition to growing single crystal AlN on the third surface of silicon, amorphous or polycrystalline AlN is also easily generated on the insulating layer 310. These amorphous or polycrystalline AlN may have adverse effects on the structure and function of the device, so the amorphous or polycrystalline AlN layer on the insulating layer 310 is removed by etching the amorphous or polycrystalline part, or introducing a Cl-containing corrosive gas, such as Cl2 or HCL gas, during growth, and utilizing the etching selectivity between the gas and the single crystal AlN and the polycrystalline / amorphous AlN, and the single crystal AlN layer on the third surface 1003 is retained. Furthermore, since the nitride semiconductor containing Ga material is difficult to directly nucleate and grow on the insulating layer, the nitride semiconductor can be selectively grown only on the single crystal AlN layer formed on the third surface.

[0182] It is understandable that, since the polycrystalline or amorphous AlN layer is essentially an insulating layer, it is difficult for the nitride semiconductor containing Ga material to nucleate and grow on the polycrystalline or amorphous AlN layer, so the polycrystalline or amorphous AlN layer on the insulating layer 310 may also be retained. It is preferred to remove the polycrystalline or amorphous AlN layer.

[0183] It is understandable that when using Al2O3 or SiC substrate, the above-mentioned insulating layer may not be needed. This is mainly because Ga atoms are compatible with Al2O3 or SiC and there is no melting back phenomenon. Nitride semiconductors are more likely to nucleate and grow on the third surface with a hexagonal symmetrical lattice structure, so the third surface naturally has the ability of selective growth.

[0184] It is further understood that when an Al2O3 or SiC substrate is used, the insulating layer makes the process window of nucleation and growth on the third surface larger and more controllable. Therefore, when an Al2O3 or SiC substrate is used, an insulating layer 310 is preferably formed on other surfaces except the third surface 1003.

[0185] An exemplary method of forming an insulating layer 310 on other surfaces except the third surface 1003 is as follows.

[0186] like Fig.23As shown in FIG. 25, a boss shape is etched on the substrate, and the boss has two opposite third surfaces. Exemplarily, when the substrate is silicon, the third surface is the (111) surface of silicon. Then, SiN is grown on the third surface by using LPCVD or other techniques, and only the SiN on the side wall is retained by an etching technique with a vertical orientation. Then, SiO2 is grown by oxidation technology. Since the third surface is protected by SiN, no SiO2 grows, and a SiO2 layer is formed on the other surfaces of the silicon wafer. Next, by using the etching selectivity of SiN and SiO2, a wet etching process such as hot phosphoric acid is used to etch away the SiN on the third surface and retain most of the silicon dioxide on the other surfaces.

[0187] The design of the insulating layer can effectively prevent the substrate material from affecting the device performance, and has a significant effect on improving the withstand voltage and reducing the dark current.

[0188] Seventh Implementation Plan

[0189] Reference Fig.26 -32 to describe a III-nitride device and a method for manufacturing the same according to the seventh embodiment.

[0190] The method for manufacturing the source, drain and gate is exemplarily described as follows.

[0191] After forming the HEMT device, a relatively thick first metal layer 210 is formed on the first insulating layer 310 formed on the first plane of the substrate by deposition and stripping or deposition and laser positioning etching. In addition to being deposited on the first insulating layer, the first metal layer is also deposited in small amounts on the (0001) surface of the device compound semiconductor layer 130. Then, the metal layer on the (0001) surface of the device compound semiconductor layer 130 is removed by isotropic etching. Then, a second insulating layer 320 is coplanarly deposited on the first metal layer. By CMP combined with back etching or precise control of the growth thickness of the second insulating layer 320, the height of the second insulating layer is set at the gate region of the device, exposing the compound semiconductor layer 130 or the gate dielectric layer at the gate region. Then, similar to the method for forming the first metal layer, a second metal layer 220 is formed on the second insulating layer. Similarly, in addition to being deposited on the second insulating layer, the second metal layer is also deposited in small amounts on the (0001) surface of the device compound semiconductor layer 130. Then, the metal layer on the (0001) surface of the device compound semiconductor layer 130 is removed by isotropic etching. Next, a third insulating layer 330 is deposited coplanarly on the second metal layer. By back-etching or precisely controlling the growth thickness of the third insulating layer, the height of the third insulating layer is set at the source region of the device, exposing the compound semiconductor layer 130 or the nitride semiconductor layer 120 at the source region. Then, similarly, a third metal layer 200 is formed on the third insulating layer, and then the first electrode 200 is formed by photolithography and etching. Thus, as shown in the figure, a gate, a source, and a drain are formed between the two devices at the same time.

[0192] It is understandable that the positions of the first electrode and the second electrode can be interchanged, and the first electrode and the second electrode can form an ohmic contact with the two-dimensional electron gas through steps such as annealing. The third electrode forms a Schottky contact with the compound semiconductor layer 130 or is insulated and separated from the compound semiconductor layer 130 by a gate dielectric.

[0193] Eighth Implementation Method

[0194] Reference Fig.33 -34 to describe a III-nitride device and a method for manufacturing the same according to the eighth embodiment.

[0195] As mentioned above, a III-nitride semiconductor channel layer and a compound semiconductor layer 130 are grown on the above-mentioned specific surface of the above-mentioned substrate, for example, a GaN material or an AlGaN material whose surface is a (0001) plane or When the surface is, it has gallium polarity or nitrogen polarity, that is, it has <0001> or Thus, there is 2DEG near the interface between the channel layer and the compound semiconductor layer 130 in the channel layer in the <0001> direction, and there is 2DHG near the interface between the channel layer and the compound semiconductor layer 130 in the channel layer in the <000-1> direction.

[0196] The eighth embodiment is different from the other embodiments except the fourth embodiment in that: Fig.33 As shown in FIG. 1 , the compound semiconductor layer 130 is removed in the <000-1> direction, so that it is no longer possible to The two-dimensional electron gas 2DHG is formed in the direction. Fig.34 As shown in the III-nitride semiconductor channel layer A fourth insulating layer 340 is formed on the surface to protect the channel layer. It can be understood that the fourth insulating layer 340 as a protective insulating layer can extend to the non-polar surface of the III-nitride semiconductor channel layer parallel to the first and second planes of the substrate.

[0197] The presence of the two-dimensional electron gas 2DHG will respond to the potential changes of the source, drain and gate, thereby increasing parasitic capacitance and leakage channels.

[0198] Ninth Implementation Plan

[0199] Reference Fig.35 A Group III nitride device and a method for manufacturing the same according to a ninth embodiment will be described.

[0200] The III-nitride device described in the ninth embodiment includes the III-nitride device with multiple electron channels as in the previous embodiment, and also includes a III-nitride device with multiple hole channels, wherein the III-nitride device with hole channels is arranged correspondingly to the III-nitride device with electron channels.

[0201] It can be understood that, corresponding to the III-nitride device of the electronic channel, The nitride semiconductor layer 110 and the nitride semiconductor layer 120 in the direction form a fourth electrode 240, a fifth electrode 250 and a sixth electrode 260. The positions of the fourth to sixth electrodes are not specifically limited. Thus, the fourth electrode can be the source of the hole channel device, the fifth electrode can be the drain of the hole channel device, and the sixth electrode can be the gate of the hole channel device. The fourth and fifth electrodes can be physically contacted with the channel layer (110 / 120) of the device, respectively, and ohmically contacted with the two-dimensional hole gas, or the fourth and fifth electrodes can be directly physically contacted with the compound semiconductor layer 130 to form ohmic contact. And the sixth electrode 260 forms an insulating contact or a Schottky contact with the compound semiconductor layer 130 on the compound semiconductor layer 130, respectively, wherein the insulating layer contact refers to forming a gate dielectric layer 300 between the sixth electrode 260 and the compound semiconductor layer 130, and the gate dielectric layer can be SiO2, a high-K dielectric material, etc. The gate dielectric layer 300 can play a role in passivating the surface of the compound semiconductor layer 130, which plays a very important role in reducing the gate leakage current of the device and the application of the device in the field of power electronics. If the gate dielectric layer is directly made on the compound semiconductor layer 130, it has a larger gate leakage current, and the devices made in this way are mostly used in the radio frequency (RF) field.

[0202] Exemplarily, the fourth to sixth electrodes may be arranged in a direction perpendicular to the first plane of the substrate 100. The fifth electrode is closer to the first plane 1001 of the substrate 100. It is understood that the fourth electrode may also be closer to the first plane 1001 of the substrate 100. The sixth electrode is located between the fifth electrode and the fourth electrode.

[0203] It can be understood that, corresponding to the electron channel III-nitride device, the hole channel III-nitride device is subjected to corresponding P-type doping in the source / drain regions corresponding to the device in the nitride semiconductor layer 110 and the nitride semiconductor layer 120. This is more conducive to reducing the ohmic contact resistance;

[0204] It is understandable that, corresponding to the III-nitride device of the electron channel, the hole channel has an N-type buried layer. It is further understandable that, through corresponding design, one of the P-type doping can be made to coincide with the buried layer of the III-nitride device of the electron channel; or the III-nitride device of the electron channel can be made to coincide with the N-type buried layer of the III-nitride device of the hole channel by performing corresponding N-type doping in the source / drain regions corresponding to the device in the nitride semiconductor layer 110 and the nitride semiconductor layer 120.

[0205] Understandable, such as Fig.36 As shown, a P-type buried layer and an N-type buried layer can be simultaneously provided in the nitride semiconductor layer. When a III-nitride device of the electron channel is to be formed, a gate is formed at the P-type buried layer; when a III-nitride device of the hole channel is to be formed, a gate is formed at the N-type buried layer.

[0206] The structures of the rest of the electron channel III-nitride device are similar to those of the hole channel III-nitride device, and are not described in detail here.

[0207] In this embodiment, by setting the electrodes on the corresponding polarization planes of the fin-shaped III-nitride device with an irregular cross-section, the HHMT and HEMT devices can be formed simultaneously, which greatly improves the integration of the devices, can effectively reduce the gate leakage current, and has a simple preparation process. Furthermore, a complementary device is formed by the HHMT and HEMT devices.

[0208] Tenth Implementation Plan

[0209] A radio frequency electronic device, such as a personal computer, a mobile phone, a digital camera or other electronic devices, comprises any one of the devices in the above embodiments.

[0210] Eleventh Embodiment

[0211] A power electronic device, which can be used for a power amplifier in the fields of mobile phone base stations, optical communication systems, etc., or can be a power supply device. The power electronic device can include any one of the devices in the above embodiments.

[0212] The present disclosure is described above in conjunction with specific implementation schemes, but it should be clear to those skilled in the art that these descriptions are exemplary and are not intended to limit the scope of protection of the present disclosure. Those skilled in the art can make various modifications and variations to the present disclosure based on the spirit and principles of the present disclosure, and these modifications and variations are also within the scope of the present disclosure.

Claims

1. A fin-shaped electronic channel semiconductor device, characterized in that: include: a substrate, epitaxially growing a fin-shaped nitride semiconductor layer on an upper surface vertical to the substrate; The nitride semiconductor layer includes first and second nitride semiconductor layers; forming a first compound semiconductor layer (130) on the nitride semiconductor layer, thereby simultaneously forming a two-dimensional hole gas and / or a two-dimensional electron gas at the interface between the first compound semiconductor layer (130) and the nitride semiconductor layer; Wherein, a P-type buried layer is sandwiched between the first and second nitride semiconductor layers.

2. The device according to claim 1, characterized in that A first insulating layer is provided on the upper surface of the substrate.

3. The device according to claim 2, characterized in that A seed layer is provided on the substrate.

4. The device according to claim 3, characterized in that A buffer layer is also provided outside the seed crystal layer, and the buffer layer has a single-layer or multi-layer structure.

5. The device according to claim 1, characterized in that The invention also comprises a second compound semiconductor layer (160), wherein the second compound semiconductor layer (160) is GaN, InGaN, AlN or AlInGaN which is not intentionally doped.

6. The device according to claim 1, characterized in that It also has a first electrode, a second electrode and a third electrode.

7. The device according to claim 1, characterized in that An integral electrode is also provided, and the integral electrode is electrically connected to the P-type buried layer.

8. A fin-shaped complementary semiconductor device, characterized in that: include: An electron channel semiconductor device as claimed in any one of claims 1 to 7, and A plurality of hole channel semiconductor devices, wherein the hole channel semiconductor devices are arranged opposite to the electron channel semiconductor device structure.

9. A radio frequency device, characterized in that: The invention comprises the fin-shaped electron channel semiconductor device according to any one of claims 1 to 7, or the fin-shaped complementary semiconductor device according to claim 8.

10. An electric power device, characterized in that: The invention comprises the fin-shaped electron channel semiconductor device according to any one of claims 1 to 7, or the fin-shaped complementary semiconductor device according to claim 8.