Hull structure fillet welding seam filling process and hull

Through the automatic welding of the robotic arm and the use of preset parameters, the problem that traditional welding robots are difficult to perceive the change of the bevel is solved, and the welding speed and quality are improved, ensuring the stability and uniformity of the weld.

CN119057186AActive Publication Date: 2024-12-03SHANGHAI WAIGAOQIAO SHIP BUILDING CO LTD

Patent Information

Application Number
CN202411408815.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-10
Publication Date
2024-12-03
Estimated Expiration
2044-10-10

AI Technical Summary

Technical Problem

Traditional welding robots find it difficult to dynamically perceive the change of bevel, resulting in rigid welding parameters and difficulty in ensuring the consistency of welding quality, which often leads to welding defects such as unfusion, undercuts and uneven welds.

Method used

Automatic welding of the robotic arm is adopted, and the welding gun operates according to preset arc starting, welding and arc extinguishing parameters. The preset oscillation parameters form a T-shaped joint with a welding foot height of 7mm. The 'Z-shaped' oscillation is used to cover the bevel to ensure welding. Stable seam quality.

Benefits of technology

The welding speed is achieved by more than 20% higher than manual welding, and the stability and uniformity of the weld quality are reduced, welding defects are improved, and welding strength and stability are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057186A_ABST
    Figure CN119057186A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of ships, and discloses a ship body structure fillet welding seam filling technology and a ship body. The ship body structure fillet welding seam process comprises the following steps that S1, a welding gun conducts arcing welding according to preset arcing parameters; s2, a welding gun conducts standard welding according to preset welding parameters; s3, the welding gun conducts arc quenching welding according to preset arc quenching parameters; in the step S1, the step S2 and the step S3, the welding gun swings according to preset swinging parameters so as to form a weld leg with the weld leg height of 7 mm; when flat fillet welding is adopted, the preset swing parameters comprise the following parameters that the swing form is in a Z shape, the swing frequency is 1.5 Hz, the swing amplitude is 2 mm, and the stop time of the swing limiting position is 0; when vertical fillet welding is adopted, the preset swing parameters comprise the following parameters that the swing form is in a Z shape, the swing frequency is 1 Hz, the swing amplitude is 7 mm, and the standing time of the swing limiting position is 0.4 s.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of ships, and in particular to a fillet welding process for a hull structure and a hull. Background Art

[0002] In modern manufacturing, robotic welding is widely used for its high efficiency and precision. However, a significant limitation is that these robotic systems often lack the adaptive capabilities of welders. Groove changes are a key variable in the welding process. Traditional welding robots weld along a straight line and cannot dynamically perceive the specific shape and size changes of the groove, which leads to rigidity and mismatch of welding parameters and makes it difficult to ensure the consistency of welding quality. Faced with the complex factors of groove changes in the welding process, traditional robots find it difficult to perceive in real time and adjust welding parameters accordingly, which frequently causes welding defects such as lack of fusion, undercut and uneven welds.

[0003] Based on this, a hull structure fillet welding process and a hull are urgently needed to solve the above-mentioned problems. Summary of the invention

[0004] Based on the above, the purpose of the present invention is to provide a hull structure fillet weld process and a hull, which realizes the automatic welding of T-joints with a weld leg height of 7 mm by a robotic arm, ensures stable weld quality, and increases the welding speed by more than 20% compared with manual welding.

[0005] To achieve the above object, the present invention adopts the following technical solutions:

[0006] On the one hand, a hull structure fillet weld process is provided, wherein a welding gun is arranged on a mechanical arm, and the welding gun adopts the hull structure fillet weld process to be applied to a T-joint with a weld leg height of 7 mm, and the hull structure fillet weld process comprises the following steps:

[0007] S1, the welding gun starts arc welding according to the preset arc starting parameters;

[0008] When flat fillet welding is used, the preset arc starting parameters include the following parameters: arc starting current is 260A, arc starting voltage is 23.8V, and arc starting wire feeding speed is 11000mm / min;

[0009] When vertical fillet welding is adopted, the preset arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, arc starting wire feeding speed is 5000mm / min;

[0010] S2, the welding gun performs standard welding according to the preset welding parameters;

[0011] S3, the welding gun performs arc extinguishing welding according to the preset arc extinguishing parameters;

[0012] In step S1, step S2 and step S3, the welding gun is swung according to preset swung parameters to form a weld foot with a weld foot height of 7 mm.

[0013] As a preferred technical solution for the fillet welding process of a hull structure, in step S2, when flat fillet welding is adopted, the preset welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 9.7mm / s, and wire feeding speed is 12000mm / min;

[0014] When vertical fillet welding is adopted, the preset welding parameters include the following parameters: welding current is 180A, welding voltage is 23.5V, welding speed is 7mm / s, and wire feeding speed is 6400mm / min.

[0015] As a preferred technical solution for the fillet welding process of a hull structure, when flat fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0;

[0016] When vertical fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 2 Hz, the swing amplitude is 2.7 mm, and the swing limit position dwell time is 0.6 s.

[0017] As a preferred technical solution for a fillet weld process of a hull structure, when flat fillet welding is adopted, the preset swing parameters also include that the angle between the axis of the welding gun and the horizontal plane is 45°, and the axis of the welding gun is perpendicular to the weld;

[0018] When vertical fillet welding is adopted, the preset swing parameters also include that the posture of the welding gun is push welding, the angle between the axis of the welding gun and the horizontal plane is 15°, and the axis of the welding gun is located on the bisector of the angle between the two welding plates.

[0019] As a preferred technical solution for the fillet welding process of a hull structure, in step S3, when flat fillet welding is adopted, the preset arc extinction parameters include the following parameters: arc extinction current is 220A, arc extinction voltage is 22V, arc extinction wire feeding speed is 8000mm / min;

[0020] When vertical fillet welding is adopted, the preset arc extinguishing parameters include the following parameters: arc extinguishing current is 155A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.

[0021] As a preferred technical solution for a fillet weld process of a hull structure, in steps S1, S2 and S3, a shielding gas is sprayed on the welding part, and the flow rate of the shielding gas is 15L / min-25L / min.

[0022] As an optimal technical solution for a fillet weld process of a hull structure, the start time of supplying the shielding gas is 1 second before arc starting welding, and the end time of supplying the shielding gas is 1.5 seconds after arc extinguishing welding.

[0023] As an optimal technical solution for a fillet weld process of a hull structure, the shielding gas is CO2.

[0024] As a preferred technical solution for a fillet weld process of a hull structure, the weld gap between two welding plates is 0-2 mm.

[0025] On the other hand, a hull is provided, which is welded by the hull structure fillet welding process described in any of the above schemes.

[0026] The beneficial effects of the present invention are:

[0027] The present invention provides a fillet weld process for a hull structure and a hull. When welding a T-type joint with a weld leg height of 7 mm, the welding gun on the mechanical arm performs arc welding according to preset arc starting parameters; then, the welding gun performs standard welding according to preset welding parameters; finally, the welding gun performs arc extinguishing welding according to preset arc extinguishing parameters; in the above welding process, the welding gun swings according to preset swing parameters to form a weld leg with a weld leg height of 7 mm. When flat fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5 Hz, the swing amplitude is 2 mm, and the swing limit position dwell time is 0; when vertical fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 7 mm, and the swing limit position dwell time is 0.4 s. The welding gun on the mechanical arm adopts the above-mentioned hull structure fillet weld process to form a T-type joint with a weld leg height of 7 mm, ensure the stable quality of the weld, and the welding speed is increased by more than 20% compared with manual welding. Moreover, during welding, the robot arm drives the welding gun to swing along a "Z-shape" so that the welding gun's travel path completely covers the groove. Even if the groove changes, the welding gun can still cover the groove when swinging, increasing the welding area, ensuring the welding quality of the weld, and achieving the effect of weld correction. The above-mentioned preset swing parameters are used for swing welding, and regular lateral swings are performed on the weld, so that the welding energy is more evenly distributed on the weld, thereby improving the uniformity of the weld. Swing welding can form a good fusion between the weld and the welding plate, thereby improving the strength and stability of the welding. BRIEF DESCRIPTION OF THE DRAWINGS

[0028] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments of the present invention. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on the contents of the embodiments of the present invention and these drawings without paying any creative work.

[0029] Figure 1 It is a process flow chart of a fillet welding process for a hull structure provided by a specific embodiment of the present invention;

[0030] Figure 2 It is a front view of a welding gun provided in a specific embodiment of the present invention using flat fillet welding;

[0031] Figure 3 It is a schematic diagram of the angle of the welding gun provided in a specific embodiment of the present invention using a flat fillet welding gun relative to the weld;

[0032] Figure 4 It is a top view of a welding gun provided by a specific embodiment of the present invention using vertical fillet welding;

[0033] Figure 5 It is a schematic diagram of the angle of the welding gun relative to the weld when the welding gun provided by the specific embodiment of the present invention adopts vertical fillet welding.

[0034] The following are marked in the figure:

[0035] 1. Welding plate; 11. Welding seam; 2. Welding gun. DETAILED DESCRIPTION

[0036] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.

[0037] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0038] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.

[0039] In the description of this embodiment, the terms "upper", "lower", "left", "right" and other directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operate in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.

[0040] In modern manufacturing, robotic welding is widely used for its high efficiency and precision. However, a significant limitation is that these robotic systems often lack the adaptive capabilities of welders. Groove changes are a key variable in the welding process. Traditional welding robots weld along a straight line and cannot dynamically perceive the specific shape and size changes of the groove, which leads to rigidity and mismatch of welding parameters and makes it difficult to ensure the consistency of welding quality. Faced with the complex factors of groove changes in the welding process, traditional robots find it difficult to perceive in real time and adjust welding parameters accordingly, which frequently causes welding defects such as lack of fusion, undercut and uneven welds.

[0041] To solve the above problems, Figure 1-Figure 5 As shown, this embodiment provides a hull structure fillet weld process, the welding gun 2 is arranged on the robot arm, and the welding gun 2 adopts the hull structure fillet weld process to be applied to a T-joint with a welding leg height of 7 mm. The hull structure fillet weld process includes the following steps:

[0042] S1, welding gun 2 performs arc welding according to preset arc starting parameters;

[0043] S2, welding gun 2 performs standard welding according to preset welding parameters;

[0044] S3, welding gun 2 performs arc extinguishing welding according to preset arc extinguishing parameters;

[0045] In step S1, step S2 and step S3, the welding gun 2 swings according to the preset swing parameters to form a weld leg with a weld leg height of 7mm; when flat fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0; when vertical fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1Hz, the swing amplitude is 7mm, and the swing limit position dwell time is 0.4s. The welding gun 2 on the robot arm adopts the above-mentioned hull structure fillet weld process to form a T-joint with a weld leg height of 7mm, ensure the stable quality of the weld 11, and the welding speed is increased by more than 20% compared with manual welding. Moreover, during welding, the robot arm drives the welding gun to swing along the "Z-shape" to make the travel path of the welding gun 2 completely cover the groove. Even if the groove changes, the welding gun 2 can cover the groove when swinging, increasing the welding area, ensuring the welding quality of the weld 11, and achieving the effect of correcting the deviation of the weld 11. The above-mentioned preset swing parameters are used for swing welding, and regular lateral swings are performed on the weld 11, so that the welding energy is more evenly distributed on the weld 11, thereby improving the uniformity of the weld 11. Swing welding can form a good fusion between the weld 11 and the welding plate 1, thereby improving the strength and stability of the welding.

[0046] In this embodiment, Figure 2 and Figure 3 As shown, when flat fillet welding is used, the preset swing parameters also include that the angle between the axis of the welding gun 2 and the horizontal plane is 45°, and the axis of the welding gun 2 is perpendicular to the weld 11; Figure 4 and Figure 5 As shown, when vertical fillet welding is adopted, the preset swing parameters also include that the posture of the welding gun 2 is push welding, the angle between the axis of the welding gun 2 and the horizontal plane is 15°, and the axis of the welding gun 2 is located on the angle bisector of the angle between the two welding plates 1, wherein the two welding plates 1 are vertical, and the angle between the axis of the welding gun 2 and the two welding plates 1 is 45°. The appropriate angle of the welding gun 2 helps to reduce defects such as undercut and slag inclusion generated during welding, improve the forming quality of the weld 11 and improve welding efficiency.

[0047] Preferably, in step S1, when flat fillet welding is adopted, the preset arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 25V, and arc starting wire feeding speed is 11000mm / min; when vertical fillet welding is adopted, the preset arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, and arc starting wire feeding speed is 5200mm / min; arc starting welding is performed according to the above-mentioned preset arc starting parameters, which can ensure a smooth transition of the weld foot at the arc starting welding part, ensure the aesthetics of the arc starting part, and the weld foot at the arc starting part is fully formed, thereby improving the strength and reliability of the weld foot.

[0048] Preferably, in step S2, in step S2, when flat fillet welding is adopted, the preset welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 6.5mm / s, and wire feeding speed is 12500mm / min; when vertical fillet welding is adopted, the preset welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 3mm / s, and wire feeding speed is 6400mm / min. The robot arm performs standard welding according to the above preset welding parameters, and can form a weld foot with a weld foot height of 7mm, and the weld 11 is of high quality, and can smoothly transition with the arc welding part, so that the hardness of the heat-affected zone meets the requirements, and the weld 11 is prevented from cracking.

[0049] Furthermore, in step S3, when flat fillet welding is adopted, the preset arc extinction parameters include the following parameters: arc extinction current is 220A, arc extinction voltage is 23V, arc extinction wire feeding speed is 8000mm / min; when vertical fillet welding is adopted, the preset arc extinction parameters include the following parameters: arc extinction current is 160A, arc extinction voltage is 20V, arc extinction wire feeding speed is 4500mm / min. Arc extinction welding is performed according to the above preset arc extinction parameters, and the arc is stable during the arc extinction process, ensuring that the arc pit of the arc extinction welding part is filled, and preventing defects such as looseness, cracks, pores or slag inclusions from occurring in the arc extinction welding part.

[0050] Preferably, in step S1, step S2 and step S3, the welding part is sprayed with shielding gas, and the gas flow rate of shielding gas is 15L / min-25L / min. By spraying shielding gas, the weld 11 area can be isolated from oxygen and moisture in the air, thereby preventing oxidation and corrosion of high-temperature metal. This can not only maintain the metal composition and performance of the weld 11, but also reduce the generation of welding defects such as pores and cracks, and improve the corrosion resistance and durability of the weld 11. The shielding gas can also play a certain protective role on the welding gun 2, reduce equipment damage caused by high temperature and oxidation, and extend the service life of the equipment. In this embodiment, the shielding gas is CO2.

[0051] Further preferably, the shielding gas supply starts 1 second before arc welding, which can ensure that the air in the nozzle is exhausted, and the welding part is within the protection range of the shielding gas at the beginning of welding, reducing the impact of air on welding quality; the shielding gas supply ends 1.5 seconds after arc welding, and the shielding gas can cool and protect the welding point after welding stops. This embodiment improves the quality of the welding part while ensuring welding efficiency.

[0052] In this embodiment, the gap of the weld 11 between the two welding plates 1 is 0-2mm, and the thickness of the welding plate 1 is 3mm-16mm. Before welding, the area to be welded should be cleaned to ensure that there is no impurities such as oil, moisture, rust, etc. The welding wire in this embodiment uses a flux-cored wire with a diameter of 1.2mm.

[0053] This embodiment also provides a hull, which is welded by the above-mentioned hull structure fillet weld process, the weld 11 is qualified, the weld foot height is 7mm-8mm, which meets the requirements, and the weld foot has no defects such as pores, undercuts, inclusions, cracks, etc. The robot adopts the above-mentioned hull structure fillet weld process, which not only significantly improves the forming quality, but also increases the speed by more than 20% compared with the traditional welding method.

[0054] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.

Claims

1. A fillet welding process for hull structure, It is characterized in that A welding gun (2) is arranged on a mechanical arm, and the welding gun (2) is applied to a T-joint with a welding leg height of 7 mm using the hull structure fillet weld process. The hull structure fillet weld process comprises the following steps: S1, welding gun (2) performs arc welding according to preset arc starting parameters; S2, welding gun (2) performs standard welding according to preset welding parameters; S3, the welding gun (2) performs arc extinguishing welding according to preset arc extinguishing parameters; In step S1, step S2 and step S3, the welding gun (2) is swung according to preset swung parameters to form a weld foot with a weld foot height of 7 mm; When flat fillet welding is used, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1.5Hz, the swing amplitude is 2mm, and the swing limit position dwell time is 0; When vertical fillet welding is adopted, the preset swing parameters include the following parameters: the swing form is "Z-shaped", the swing frequency is 1 Hz, the swing amplitude is 7 mm, and the swing limit position dwell time is 0.4 s.

2. The hull structure fillet welding process according to claim 1, It is characterized in that When flat fillet welding is used, the preset swing parameters also include that the angle between the axis of the welding gun (2) and the horizontal plane is 45°, and the axis of the welding gun (2) is perpendicular to the weld (11); When vertical fillet welding is adopted, the preset swing parameters also include that the posture of the welding gun (2) is push welding, the angle between the axis of the welding gun (2) and the horizontal plane is 15°, and the axis of the welding gun (2) is located on the bisector of the angle between the two welding plates (1).

3. The hull structure fillet welding process according to claim 1, It is characterized in that In step S2, when flat fillet welding is used, the preset welding parameters include the following parameters: welding current is 280A, welding voltage is 27V, welding speed is 6.5mm / s, and wire feeding speed is 12500mm / min; When vertical fillet welding is adopted, the preset welding parameters include the following parameters: welding current is 190A, welding voltage is 22V, welding speed is 3mm / s, and wire feeding speed is 6400mm / min.

4. The hull structure fillet welding process according to claim 1, It is characterized in that In step S3, when flat fillet welding is used, the preset arc extinction parameters include the following parameters: arc extinction current is 220A, arc extinction voltage is 23V, and arc extinction wire feeding speed is 8000mm / min; When vertical fillet welding is adopted, the preset arc extinguishing parameters include the following parameters: arc extinguishing current is 160A, arc extinguishing voltage is 20V, and arc extinguishing wire feeding speed is 4500mm / min.

5. The hull structure fillet welding process according to claim 1, It is characterized in that In step S1, when flat fillet welding is used, the preset arc starting parameters include the following parameters: arc starting current is 274A, arc starting voltage is 25V, and arc starting wire feeding speed is 11000mm / min; When vertical fillet welding is adopted, the preset arc starting parameters include the following parameters: arc starting current is 170A, arc starting voltage is 22V, and arc starting wire feeding speed is 5200mm / min.

6. The hull structure fillet welding process according to claim 1, It is characterized in that In step S1, step S2 and step S3, the welding position is sprayed with a shielding gas, and the flow rate of the shielding gas is 15L / min-25L / min.

7. The fillet welding process for hull structure according to claim 6, It is characterized in that The supply of the shielding gas starts 1 second before arc-starting welding, and ends 1.5 seconds after arc-extinguishing welding.

8. The fillet welding process for hull structure according to claim 6, It is characterized in that The protective gas is CO 2 .

9. The hull structure fillet welding process according to claim 1, It is characterized in that The gap of the weld (11) between the two welding plates (1) is 0-2 mm.

10. A hull, It is characterized in that The hull is welded by using the hull structure fillet weld process as described in any one of claims 1 to 9.

Citation Information

Patent Citations

  • Robot welding process for ship curved surface structure

    CN114147317A

  • Intermittent automatic welding method for marine aluminum alloy and welding robot control method

    CN116000412A

  • Pipe fitting full penetration backing welding method suitable for large change range of assembly gaps

    CN117620374A

  • Control method for lap welding of bead joint

    JP1999077305A

  • Method for controlling arc welding

    JP2004174523A

Cited By

  • Welding arc voltage tracking and arc swing control system and method based on collaborative robot

    CN120023427A