Crucible device for automatically adjusting growth of gallium nitride crystal, growth equipment and growth method

By automatically adjusting the overflow tank design and corrosion-resistant materials on the crucible device, the technical problems of floating matter in the growth of GaN single crystals are solved, the nitrogen dissociation rate and growth rate are improved, and the service life of the device is extended.

CN119061461APending Publication Date: 2024-12-03DONGGUAN INST OF OPTO ELECTRONICS PEKING UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411314662.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-19
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

During the growth of GaN single crystal, floating objects (impacts) on the surface of high-temperature melt reduce the gas-liquid dissociation area of ​​nitrogen and reduce the GaN growth rate. The corrosiveness of the crucible device causes Ga/Na to react with the crucible surface to generate Solid solution affects growth efficiency.

Method used

An automatic adjustment crucible device is designed to drive the piston up through the driving member, causing floating objects on the surface of the high-temperature melt to overflow into the overflow tank, increase the contact area between nitrogen and the melt, and use corrosion-resistant materials such as Mo, Ti, Nb or boron nitride materials make crucibles to reduce corrosion.

Benefits of technology

It effectively increases the dissociation rate of nitrogen, increases the growth rate of GaN single crystals, and extends the service life of the device through corrosion-resistant materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119061461A_ABST
    Figure CN119061461A_ABST
Patent Text Reader

Abstract

The invention discloses a crucible device capable of automatically adjusting growth of gallium nitride crystals, growth equipment and a growth method.The crucible device comprises a first crucible, a piston and a driving part; the first crucible is of a hollow structure, the piston is arranged in the hollow structure in a sliding mode, the peripheral edge of the piston is in sealing fit with the inner side wall of the first crucible, the piston and the hollow structure form a containing cavity used for containing high-temperature melt, and the driving part is connected with the piston and drives the piston to slide up and down in the hollow structure so as to adjust the capacity of the containing cavity; an overflow groove is further formed between the inner side wall of the first crucible and the outer side wall of the first crucible, and a top groove opening of the overflow groove is communicated with the top opening of the containing cavity. In the design, impurities on the surface layer of the high-temperature melt can flow out of the high-temperature melt by adjusting the height of the high-temperature melt, so that the contact area between nitrogen and the high-temperature melt is effectively increased, the nitrogen is dissociated into N ions on the surface of the melt more quickly, and growth of GaN single crystals is promoted.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of GaN single crystal growth technology, and in particular to a crucible device, a growth device and a growth method for automatically adjusting the growth of gallium nitride crystals. Background Art

[0002] The process of growing GaN single crystals by the flux method is a gas-liquid-solid three-phase reaction process: the high-temperature nitrogen N2 in the furnace body dissociates in the high-temperature melt, and then the dissociated N combines with the Ga ions in the melt to grow into GaN single crystals. The main factor controlling the growth rate of GaN single crystals is the dissociation rate of high-temperature N gas. High-temperature nitrogen mainly dissociates at the gas-liquid interface and dissociates into N ions. Therefore, in order to increase the growth rate of GaN single crystals, the most important factor is to increase the dissociation rate of N ions.

[0003] In addition to being affected by the gas-liquid interface area, the dissociation rate of N ions also has a major problem in the actual growth process: floating objects (impurities) on the surface of the high-temperature melt. The floating objects in the high-temperature melt mainly come from whether the Na raw material is cleanly processed, because the metal Na is stored in kerosene. After the surface layer is cut with tools, it is inevitable that it will not be cut cleanly, or the Na metal still absorbs kerosene impurities; the second is the crucible device. The high-temperature molten Na-Ga is highly corrosive, and Ga / Na easily reacts with the surface metal of the crucible to form a solid solution; in addition, the high-purity nitrogen in the furnace still contains trace amounts of oxygen or water, and the melt forms oxides with Na or Ga, etc. The floating objects on the surface of the high-temperature melt reduce the gas-liquid dissociation area of ​​the high-temperature nitrogen, further reducing the N concentration in the melt and slowing down the growth rate of GaN.

[0004] Therefore, finding a technical solution that can solve the above technical problems has become an important topic studied by technical personnel in this field. Summary of the invention

[0005] The embodiment of the present invention discloses a crucible device, a growth device and a growth method for automatically adjusting the growth of gallium nitride crystals to solve the above technical problems.

[0006] The present invention provides a crucible device for automatically adjusting gallium nitride crystal growth, comprising a first crucible, a piston and a driving member;

[0007] The first crucible is a hollow structure, the piston is slidably disposed in the hollow structure, and the outer peripheral edge of the piston is sealed and matched with the inner side wall of the first crucible, the piston and the hollow structure constitute a containing cavity for containing high-temperature melt, and the driving member is connected to the piston and drives the piston to slide up and down in the hollow structure to adjust the capacity of the containing cavity;

[0008] An overflow groove is further provided between the inner side wall of the first crucible and the outer side wall of the first crucible, and the top notch of the overflow groove is communicated with the top opening of the accommodating cavity.

[0009] Optionally, a top of the inner side wall of the first crucible is provided with an inclined surface inclined downward toward the overflow groove.

[0010] Optionally, a second crucible is further arranged below the position where the piston contacts the inner wall of the first crucible.

[0011] Optionally, a drainage portion protrudes downward on the surface of the piston facing the second crucible.

[0012] Optionally, the driving member is a linear drive module driven by a motor and a lead screw.

[0013] Optionally, the first crucible is made of Mo metal, Ti metal, Nb metal or boron nitride material.

[0014] Optionally, the second crucible is made of Mo metal, Ti metal, Nb metal or boron nitride material.

[0015] The present invention provides a growth device for automatically adjusting the growth of gallium nitride crystals, comprising a growth furnace, a heater and the above-mentioned crucible device;

[0016] The heater and the crucible device are both arranged inside the growth furnace, nitrogen is introduced into the growth furnace, and the heater is arranged around the crucible device.

[0017] Optionally, the heater is a graphite heater.

[0018] The present invention provides a growth method for automatically adjusting the growth of gallium nitride crystals. The growth method is based on the above-mentioned growth device and comprises the following steps:

[0019] S1, fix the seed crystal on the surface of the piston located in the accommodating chamber, put Ga, Na, C chemical raw materials into the accommodating chamber according to the preset amount, introduce high-pressure nitrogen into the growth furnace, start the heater to heat the crucible device to melt the Ga, Na, C chemical raw materials into a high-temperature melt with a height of h1, and let it stand for a preset time so that impurities in the high-temperature melt float on the surface of the high-temperature melt;

[0020] S2, starting the driving member, the driving member drives the piston to move upward, and when the top surface of the high-temperature melt is higher than the top opening of the accommodating chamber, the driving member is continued to be controlled to drive the piston to move upward so that impurities floating on the surface of the high-temperature melt overflow into the overflow groove;

[0021] S3, when the height of the high-temperature melt reaches a preset process height h0, where h1 is greater than h0, the driving member is closed to stop the piston from rising, and the N ions in the high-temperature melt are combined with the Ga ions on the surface of the seed crystal to grow a GaN single crystal;

[0022] S4. After the growth is completed, the heater is turned off and the crucible device begins to cool down, the pressure is released, and the GaN single crystal is taken out.

[0023] Compared with the prior art, the present invention has the following beneficial effects:

[0024] In the crucible device for automatically regulating the growth of gallium nitride crystals of this embodiment, the piston is driven upward by a driving member, so that floating materials (impurities) on the surface of the high-temperature melt can overflow into the overflow groove, thereby effectively increasing the contact area between nitrogen and the high-temperature melt so that nitrogen can dissociate into N ions more quickly on the surface of the melt, thereby promoting the growth of GaN single crystals. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0026] Figure 1 A schematic diagram of a crucible device for automatically adjusting gallium nitride crystal growth provided by the present invention when the height of the high-temperature melt is h1;

[0027] Figure 2 A schematic diagram of a crucible device for automatically adjusting gallium nitride crystal growth provided by the present invention when floating objects (impurities) on the surface of a high-temperature melt overflow and reach a preset process height h0;

[0028] Figure 3 A schematic diagram of a growth method for automatically regulating gallium nitride crystal growth provided by the present invention;

[0029] 1-growth furnace, 11-heater, 12-high-pressure nitrogen, 2-driving member, 3-first crucible, 31-inclined surface, 32-accommodating chamber, 33-overflow trough, 4-second crucible, 5-piston, 51-drainage part, 6-seed crystal, 7-high-temperature melt. DETAILED DESCRIPTION

[0030] In order to enable those skilled in the art to better understand the scheme of the present invention, the present invention is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0031] See also Figure 1 to Figure 2 , a crucible device for automatically adjusting gallium nitride crystal growth provided by an embodiment of the present invention comprises a first crucible 3, a piston 5 and a driving member 2;

[0032] The first crucible 3 is a hollow structure, the piston 5 is slidably disposed in the hollow structure, and the outer peripheral edge of the piston 5 is sealed and matched with the inner side wall of the first crucible 3, the piston 5 and the hollow structure form a containing cavity 32 for containing the high-temperature melt 7, and the driving member 2 is connected to the piston 5 and drives the piston 5 to slide up and down in the hollow structure to adjust the capacity of the containing cavity 32;

[0033] An overflow groove 33 is further provided between the inner wall of the first crucible 3 and the outer wall of the first crucible 3 , and a top notch of the overflow groove 33 is communicated with a top opening of the accommodating cavity 32 .

[0034] In the crucible device for automatically adjusting the growth of gallium nitride crystals of this embodiment, the piston 5 is driven upward by the driving member 2, so that the floating materials (impurities) on the surface of the high-temperature melt 7 can overflow into the overflow groove 33, thereby effectively increasing the contact area between the nitrogen 12 and the high-temperature melt 7 so that the nitrogen 12 can dissociate into N ions more quickly on the surface of the melt, thereby promoting the growth of the GaN single crystal.

[0035] Furthermore, the top of the inner wall of the first crucible 3 in this embodiment is provided with an inclined surface 31 which is inclined downward toward the overflow groove 33 .

[0036] It should be noted that, through the above design, when the high-temperature melt 7 rises to the top opening of the accommodating cavity 32, the floating objects on the surface of the high-temperature melt 7 can rely on the above-mentioned inclined surface 31 to more easily enter the overflow groove 33, and the inclined surface 31 also plays a certain drainage role.

[0037] Furthermore, a second crucible 4 is provided below the position where the piston 5 in this embodiment contacts the groove wall of the hollow groove.

[0038] It should be noted that, through the above design, when the high-temperature melt 7 leaks from the position where the piston 5 contacts the inner wall of the first crucible 3, the second crucible 4 can effectively catch the leaked high-temperature melt 7 to prevent the leaked high-temperature melt 7 from contaminating other components such as the driving part 2.

[0039] Furthermore, in this embodiment, a drainage portion 51 is protruded downward on the surface of the piston 5 facing the second crucible 4 .

[0040] It should be noted that, through the above-mentioned design, the drainage portion 51 can effectively drain the leaked high-temperature melt 7 into the second crucible 4, ensuring that the leaked high-temperature melt 7 will not cause pollution.

[0041] Furthermore, the driving member 2 in this embodiment is a linear driving module driven by a motor and a lead screw.

[0042] It should be noted that the driving member 2 in this embodiment may also be other types of structures, and this embodiment does not limit this.

[0043] Furthermore, the first crucible 3 in this embodiment is made of Mo metal, Ti metal, Nb metal or boron nitride material.

[0044] The second crucible 4 in this embodiment is made of Mo metal, Ti metal, Nb metal or boron nitride material.

[0045] It should be noted that, through the above design, the first crucible 3 and the second crucible 4 made of the above metal or boron nitride material have higher corrosion resistance, which is conducive to extending the service life.

[0046] See also Figure 1 to Figure 2 , a growth device for automatically adjusting the growth of gallium nitride crystals provided by an embodiment of the present invention comprises a growth furnace 1, a heater 11 and the above-mentioned crucible device;

[0047] The heater 11 and the crucible device are both arranged inside the growth furnace 1 . Nitrogen 12 is introduced into the growth furnace 1 . The heater 11 is arranged around the crucible device.

[0048] In the growth device for automatically regulating the growth of gallium nitride crystals of this embodiment, the piston 5 is driven upward by the driving member 2, so that the floating materials (impurities) on the surface of the high-temperature melt 7 can overflow into the overflow groove 33, thereby effectively increasing the contact area between the nitrogen 12 and the high-temperature melt 7 so that the nitrogen 12 can dissociate into N ions more quickly on the surface of the melt, thereby promoting the growth of the GaN single crystal.

[0049] Specifically, the heater 11 in this embodiment is a graphite heater.

[0050] See also Figures 1 to 3, an embodiment of the present invention provides a growth method for automatically adjusting the growth of gallium nitride crystals, the growth method is based on the above-mentioned growth device, and the growth method includes the following steps:

[0051] S1, fix the seed crystal 6 on the surface of the piston 5 located in the accommodating chamber 32, put Ga, Na, C chemical raw materials into the accommodating chamber 32 according to the preset amount, and introduce high-pressure nitrogen 12 required by the process into the growth furnace 1, such as Figure 1 As shown, the heater 11 is started to heat the crucible device to melt the Ga, Na, and C chemical raw materials into a high-temperature melt 7 with a height h1, and the high-temperature melt 7 is left to stand for a preset time (specifically 10-50 minutes) so that impurities in the high-temperature melt 7 float on the surface of the high-temperature melt 7;

[0052] S2, start the driving member 2, and the driving member 2 drives the piston 5 to move upward. When the top surface of the high-temperature melt 7 is higher than the top opening of the accommodating chamber 32, the driving member 2 is continued to be controlled to drive the piston 5 to move upward so that the impurities floating on the surface of the high-temperature melt 7 overflow into the overflow groove 33;

[0053] S3, such as Figure 2 As shown, after the height of the high-temperature melt 7 reaches a preset process height h0, where h1 is greater than h0, the driving member 2 is closed to stop the piston 5 from rising, and the N ions and Ga ions in the high-temperature melt 7 are combined on the surface of the seed crystal 6 to grow a GaN single crystal;

[0054] S4. After the growth is completed, the heater 11 is turned off and the crucible device starts to cool down, the pressure is released, and the GaN single crystal is taken out.

[0055] It should be noted that the above growth method can effectively increase the contact area between the nitrogen 12 and the high-temperature melt 7 so that the nitrogen 12 can be dissociated into N ions more quickly on the melt surface, thereby promoting the growth of the GaN single crystal.

[0056] The above is a detailed introduction to a crucible device, a growth device and a growth method for automatically adjusting the growth of gallium nitride crystals provided by the present invention. For a person skilled in the art, according to the idea of ​​the embodiments of the present invention, there may be changes in the specific implementation methods and application scopes. In summary, the content of this specification should not be understood as limiting the present invention.

Claims

1. A crucible device for automatically adjusting gallium nitride crystal growth, characterized in that: It comprises a first crucible (3), a piston (5) and a driving member (2); The first crucible (3) is a hollow structure, the piston (5) is slidably disposed in the hollow structure and the outer peripheral edge of the piston (5) is sealed with the inner wall of the first crucible (3), the piston (5) and the hollow structure form a receiving chamber (32) for receiving a high-temperature melt (7), and the driving member (2) is connected to the piston (5) and drives the piston (5) to slide up and down in the hollow structure to adjust the capacity of the receiving chamber (32); An overflow groove (33) is also provided between the inner wall of the first crucible (3) and the outer wall of the first crucible (3), and the top notch of the overflow groove (33) is connected to the top opening of the accommodating cavity (32).

2. The crucible device for automatically adjusting gallium nitride crystal growth according to claim 1, characterized in that: The top of the inner wall of the first crucible (3) is provided with an inclined surface (31) which is arranged obliquely downward toward the overflow groove (33).

3. The crucible device for automatically adjusting gallium nitride crystal growth according to claim 1, characterized in that: A second crucible (4) is also provided below the position where the piston (5) contacts the inner wall of the first crucible (3).

4. The crucible device for automatically adjusting gallium nitride crystal growth according to claim 1, characterized in that: A drainage portion (51) protrudes downward on the surface of the piston (5) facing the second crucible (4).

5. The crucible device for automatically adjusting gallium nitride crystal growth according to claim 1, characterized in that: The driving member (2) is a linear driving module driven by a motor and a lead screw.

6. The growth device for automatically regulating gallium nitride crystal growth according to claim 1, characterized in that: The first crucible (3) is made of Mo metal, Ti metal, Nb metal or boron nitride material.

7. The growth device for automatically regulating gallium nitride crystal growth according to claim 3, characterized in that: The second crucible (4) is made of Mo metal, Ti metal, Nb metal or boron nitride material.

8. A growth device for automatically regulating the growth of gallium nitride crystals, characterized in that: It comprises a growth furnace (1), a heater (11) and a crucible device as claimed in any one of claims 1 to 7; The heater (11) and the crucible device are both arranged inside the growth furnace (1), nitrogen (12) is introduced into the growth furnace (1), and the heater (11) is arranged around the crucible device.

9. The growth device for automatically regulating gallium nitride crystal growth according to claim 8, characterized in that: The heater (11) is a graphite heater.

10. A method for automatically regulating the growth of gallium nitride crystals, characterized in that: The growth method is performed based on the growth device according to any one of claims 8 to 9, and the growth method comprises the following steps: S1, fixing the seed crystal (6) on the surface of the piston (5) located in the accommodating chamber (32), adding Ga, Na, and C chemical raw materials into the accommodating chamber (32) according to a preset amount, introducing high-pressure nitrogen (12) into the growth furnace (1), starting the heater (11) to heat the crucible device so that the Ga, Na, and C chemical raw materials are melted into a high-temperature melt (7) with a height h1, and the high-temperature melt (7) is left to stand for a preset time so that impurities in the high-temperature melt (7) float on the surface of the high-temperature melt (7); S2, starting the driving member (2), the driving member (2) drives the piston (5) to move upward, and when the top surface of the high-temperature melt (7) is higher than the top opening of the accommodating chamber (32), the driving member (2) is continued to be controlled to drive the piston (5) to move upward so that impurities floating on the surface of the high-temperature melt (7) overflow into the overflow groove (33); S3, after the height of the high-temperature melt (7) reaches a preset process height h0, where h1 is greater than h0, the driving member (2) is closed to stop the piston (5) from rising, and the N ions in the high-temperature melt (7) and the Ga ions are combined on the surface of the seed crystal (6) to grow a GaN single crystal; S4. After the growth is completed, the heater (11) is turned off and the crucible device starts to cool down, the pressure is released, and the GaN single crystal is taken out.