Wafer processing method

The wafer processing method uses a second wafer as a barrier layer during laser cutting to prevent slag contamination, improving the reliability of bonding and etching processes in semiconductor manufacturing.

CN119077147APending Publication Date: 2024-12-06HUBEI YANGTZE PILOT-LINE SERVICES CO LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
CN202411193532.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-12-06

AI Technical Summary

Technical Problem

The laser cutting process in semiconductor manufacturing results in the deposition of slag on the bonding surface of the semiconductor wafer, leading to contamination and poor reliability of subsequent bonding and etching processes.

Method used

A wafer processing method involving temporary bonding of a first wafer to a second wafer, using the second wafer as a barrier layer during laser cutting to deposit slag on its surface, thereby preventing contamination of the first wafer's bonding surface and improving the reliability of subsequent processes.

Benefits of technology

The method effectively prevents slag deposition on the first wafer's bonding surface, enhancing the reliability of subsequent bonding and etching processes while reducing process complexity and cost.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119077147A_ABST
    Figure CN119077147A_ABST
Patent Text Reader

Abstract

The invention provides a wafer processing method. The wafer processing method comprises the following steps: providing a first wafer and a second wafer; the first wafer comprises a substrate and a bonding surface located on one side of the two opposite sides of the substrate in the first direction; the first direction is the thickness direction of the first wafer; temporarily bonding the first wafer and the second wafer, and forming a temporary bonding layer between the bonding surface and the second wafer; and performing laser cutting on the first wafer by taking the second wafer as a barrier layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductor technology, and in particular to a wafer processing method. Background Art

[0002] In the manufacturing process of semiconductor chips, multiple chips are first formed on a wafer through a semiconductor process, and then the wafer is cut into separate chips through a cutting process. In the cutting area of ​​the wafer, a conductive structure is often provided in the dielectric layer, for example, a test key for chip testing, and the properties of the conductive material are quite different from the properties of the dielectric material previously filled with the conductive structure. Therefore, a laser cutting process is required to cut the dielectric layer and the conductive structure located in the dielectric layer. However, during the execution of laser cutting, the gaseous substance evaporates upward and is easily condensed to form slag when cooled, resulting in contamination of the surface of the wafer / chip. Therefore, the wafer cutting process needs to be further optimized. Summary of the invention

[0003] In view of this, the present disclosure provides a wafer processing method, comprising:

[0004] A first wafer and a second wafer are provided; the first wafer comprises a substrate and a bonding surface located on one of two sides of the substrate that are opposite to each other along a first direction; the first direction is a thickness direction of the first wafer;

[0005] Temporarily bonding the first wafer to the second wafer, and forming a temporary bonding layer between the bonding surface and the second wafer;

[0006] The first wafer is laser cut using the second wafer as a barrier layer.

[0007] In an optional embodiment, the first wafer includes a first cutting street area extending along a second direction and a second cutting street area extending along a third direction; the second direction intersects with the third direction and is perpendicular to the first direction; and the laser cutting of the first wafer using the second wafer as a barrier layer includes:

[0008] Performing a first laser cutting on the first wafer using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting line region; the first groove extends along the second direction;

[0009] The first wafer is subjected to a second laser cutting process using the second wafer as a barrier layer to form a second trench exposing the substrate in the second scribe line region; the second trench extends along the third direction.

[0010] In an optional embodiment, the first cutting street area and the second cutting street area both include a dielectric layer and a conductive structure located in the dielectric layer; the first laser cutting of the first wafer using the second wafer as a barrier layer and the second laser cutting of the first wafer using the second wafer as a barrier layer include:

[0011] Performing the first laser cutting on the dielectric layer and the conductive structure in the first scribe line region by using the second wafer as a barrier layer;

[0012] The second laser cutting is performed on the dielectric layer and the conductive structure in the second scribe line region by using the second wafer as a barrier layer.

[0013] In an optional implementation, the wafer processing method further includes:

[0014] Before laser cutting the first wafer using the second wafer as a barrier layer, performing a first etching on the second wafer to form a third groove in the second wafer exposing the first scribe line area;

[0015] The step of performing a first laser cutting on the first wafer using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting street region comprises:

[0016] The first laser cutting is performed on the first scribe line region along the third groove to form the first groove.

[0017] In an optional implementation, performing a first etching on the second wafer to form a third groove in the second wafer exposing the first scribe line region includes:

[0018] forming a patterned photoresist layer covering the second wafer;

[0019] Etching the second wafer using the patterned photoresist layer as a mask to form a fourth groove exposing the temporary bonding layer;

[0020] The remaining patterned photoresist layer and the exposed temporary bonding layer are removed to form the third trench in the second wafer.

[0021] In an optional implementation, the wafer processing method further includes:

[0022] Before performing a second laser cutting on the first wafer using the second wafer as a barrier layer, debonding the first wafer from the second wafer;

[0023] rotating the second wafer and temporarily bonding it to the first wafer again, so that the third groove exposes the second scribe line area in the first wafer;

[0024] The step of performing a second laser cutting on the first wafer using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street region comprises:

[0025] The second laser cutting is performed on the second scribe line region along the third groove to form the second groove.

[0026] In an optional implementation, the wafer processing method further includes:

[0027] After or simultaneously with performing the first etching on the second wafer to form the third groove exposing the first scribe line region in the second wafer, performing the second etching on the second wafer to form the fifth groove exposing the second scribe line region in the second wafer; the fifth groove is connected to the third groove;

[0028] The step of performing a second laser cutting on the first wafer using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street region comprises:

[0029] The second laser cutting is performed on the second scribe line region along the fifth groove to form the second groove.

[0030] In an optional embodiment, performing a first laser cutting on the first wafer using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting street area and performing a second laser cutting on the first wafer using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street area include:

[0031] Performing the first laser cutting on the first scribe line region in the second wafer and the first wafer from one side of two sides of the second wafer opposite to each other along the first direction and away from the first wafer, so as to form a first opening in the second wafer and form the first groove in the first scribe line region; the first opening is connected to the first groove;

[0032] The second laser cutting is performed on the second wafer and the second cutting path area in the first wafer from one side of the second wafer opposite to each other along the first direction and away from the first wafer to form a second opening in the second wafer and form the second groove in the second cutting path area; the second opening is connected to the second groove.

[0033] In an optional implementation, the wafer processing method further includes:

[0034] Performing a third etching on the substrate exposed by the first groove using the second wafer as a mask;

[0035] A fourth etching is performed on the substrate exposed by the second groove by using the second wafer as a mask.

[0036] In an optional implementation, the wafer processing method further includes:

[0037] The first wafer and the second wafer are debonded to expose the bonding surface of the first wafer.

[0038] In an optional implementation, the wafer processing method further includes:

[0039] Before laser cutting the first wafer using the second wafer as a barrier layer, the second wafer is thinned on a side away from the first wafer from two opposite sides of the second wafer along the first direction.

[0040] In an optional implementation, the second wafer includes semiconductor material, transparent material or semi-transparent material.

[0041] In the technical solution provided by the present disclosure, the second wafer temporarily bonded to the first wafer can be used as a barrier layer for laser cutting of the first wafer, and the slag generated during the laser cutting process can be deposited on the surface of the second wafer on the side away from the first wafer, thereby avoiding the slag from contaminating the bonding surface of the first wafer and reducing the negative impact on the subsequent bonding process. In addition, the second wafer including the groove can also be used as a mask layer for etching the substrate in the first wafer, thereby omitting the process step of forming the mask layer after the laser cutting process, avoiding the problem of poor reliability of the mask layer formed subsequently due to the deposition of slag generated by laser cutting on the bonding surface, and avoiding the formation of a mask layer on a wafer with grooves already formed, thereby avoiding the contamination of the bonding surface and improving the reliability of the subsequent etching process. BRIEF DESCRIPTION OF THE DRAWINGS

[0042] Figure 1 A schematic diagram of a process flow of a wafer processing method provided by an embodiment of the present disclosure;

[0043] Figures 2 to 21 A schematic diagram of the structure of a wafer processing process provided in an embodiment of the present disclosure. DETAILED DESCRIPTION

[0044] The exemplary embodiments of the present disclosure will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present disclosure are shown in the accompanying drawings, it should be understood that the present disclosure can be implemented in various forms and should not be limited by the specific embodiments set forth herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present disclosure and to fully convey the scope of the present disclosure to those skilled in the art.

[0045] In the following description, a large number of specific details are given to provide a more thorough understanding of the present disclosure. However, it is obvious to those skilled in the art that the present disclosure can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present disclosure, some technical features known in the art are not described; that is, all features of actual embodiments are not described here, and well-known functions and structures are not described in detail.

[0046] In the drawings, like reference numerals refer to like elements throughout.

[0047] It should be understood that spatial relationship terms such as "under", "below", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial description terms used herein are interpreted accordingly.

[0048] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be a limitation of the present disclosure. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0049] In the 3D IC process, in order to achieve the bonding between the chip and the wafer, it is necessary to cut the wafer into multiple chips along the cutting path in the wafer, and then connect the chips with different functions to the wafer through the bonding process. In the cutting path area of ​​the wafer, a conductive structure is often provided in the dielectric layer, for example, a test key for chip testing, and the properties of the conductive material are greatly different from the properties of the dielectric material filled before the conductive structure. Therefore, a laser cutting process is required to cut the dielectric layer and the conductive structure located in the dielectric layer. The laser cutting process uses a high-power density laser beam to irradiate the cutting path of the wafer, so that the material in the cutting path is quickly heated to the vaporization temperature, evaporated to form holes, and as the beam moves, the holes continuously form a very narrow slit to complete the cutting of the wafer. However, during the execution of the laser cutting process, the material vaporized by instantaneous high temperature evaporates upward and is easily condensed to form slag when it is cooled. The slag is easily deposited on the bonding surface of the wafer / chip, resulting in poor flatness of the bonding surface of the wafer / chip, which may seriously affect the reliability of the subsequent bonding process. In addition, after performing the laser cutting process, the substrate may need to be further cut through an etching process, and the slag deposited on the surface of the wafer may also affect the coating of the photoresist or the deposition of the mask layer.

[0050] Therefore, it is necessary to further optimize the wafer cutting process. To this end, the present disclosure proposes the following implementation methods.

[0051] An embodiment of the present disclosure provides a wafer processing method. Figure 1 The following is a flow chart of a wafer processing method provided by an embodiment of the present disclosure. Figure 1 As shown, the wafer processing method includes the following steps:

[0052] Step S10: providing a first wafer and a second wafer; the first wafer comprises a substrate and a bonding surface located on one of two sides of the substrate opposite to each other along a first direction; the first direction is a thickness direction of the first wafer;

[0053] Step S20: temporarily bonding the first wafer to the second wafer, and forming a temporary bonding layer between the bonding surface and the second wafer;

[0054] Step S30: performing laser cutting on the first wafer using the second wafer as a barrier layer.

[0055] Figures 2 to 21 The schematic diagram of the structure of the wafer processing process provided by the embodiment of the present disclosure is as follows. Figures 1 to 21 The wafer processing method provided by the embodiment of the present disclosure is introduced.

[0056] In some embodiments, the wafer processing method includes: executing step S10 to provide a first wafer 10 and a second wafer 20 .

[0057] Figure 2 A top view of a first wafer provided in an embodiment of the present disclosure, Figure 3 for Figure 2 Cross-section along line AA', combined with reference Figure 2 and Figure 3 The first wafer 10 includes a substrate 100 and a bonding surface 103 located on one side of two opposite sides of the substrate 100 along a first direction.

[0058] In some embodiments, Figure 2 As shown, the first wafer 10 includes a first cutting road area 101 extending along the second direction and a second cutting road area 102 extending along the third direction. The first cutting road area 101 and the second cutting road area 102 can intersect, and the two second cutting road areas 102 of two adjacent first cutting road areas 101 surround the chip area. By cutting the first wafer 10 along the first cutting road area 101 and the second cutting road area 102, the first wafer 10 can be divided into multiple chips.

[0059] In the embodiment of the present disclosure, the first direction is the thickness direction of the first wafer 10, and the second direction intersects with the third direction and is perpendicular to the first direction. Here, the first direction is the Z direction, the second direction is the Y direction, and the third direction is the X direction.

[0060] It should be noted that the number of the first cutting line area 101 and the second cutting line area 102 in the figure is only an example, and the present disclosure does not impose any specific limitation on this.

[0061] In some embodiments, the first scribe line region 101 and the second scribe line region 102 both include a dielectric layer 104 and a conductive structure 105 located in the dielectric layer 104. Figure 3 As shown, the conductive structure 105 may include conductive wires, conductive vias, bonding pads and test keys for chip testing, wherein the conductive structures located in the first cutting path area 101 and the second cutting path area 102 are generally test keys for chip testing and conductive wires and conductive vias connected to the test keys, and the bonding pads in the chip areas on both sides of the first cutting path area 101 and the second cutting path area 102 are exposed from the bonding surface 103 for subsequent bonding with other chips or wafers.

[0062] In some specific examples, the substrate 100 can be a single semiconductor material substrate (for example, a silicon substrate, a germanium substrate, etc.), a compound semiconductor material substrate (for example, a germanium silicon substrate, etc.), or a silicon on insulator (SOI) substrate, a germanium on insulator (GeOI) substrate, etc.

[0063] In some specific examples, the material of the dielectric layer 104 may include at least one of dielectric materials such as silicon oxide, silicon nitride or silicon oxynitride; the material of the conductive structure 105 may include one of doped semiconductor materials (for example, doped silicon, doped germanium, etc.), conductive metal nitrides (for example, titanium nitride, tantalum nitride, etc.), metal materials (for example, copper, aluminum, tungsten, titanium, tantalum, etc.) and metal semiconductor compounds (for example, tungsten silicide, cobalt silicide, titanium silicide, etc.).

[0064] In some embodiments, in conjunction with reference Figure 3 and Figure 4 The wafer processing method includes: executing step S20 to temporarily bond the first wafer 10 to the second wafer 20 and to form a temporary bonding layer 201 between the bonding surface 103 and the second wafer 20 .

[0065] In some specific examples, the specific process of executing step S20 may include: spin coating a layer of temporary bonding glue on the bonding surface 103 of the first wafer 10 and on one side surface of the second wafer 20, respectively, and baking them to a certain temperature, and then transferring the first wafer 10 and the second wafer 20 to a temporary bonding device, aligning and bonding them under a vacuum environment, and forming a temporary bonding layer 201 between the first wafer 10 and the second wafer 20.

[0066] In some specific examples, the area of ​​the second wafer 20 is at least equal to the area of ​​the first wafer 10 , and after the first wafer 10 and the second wafer 20 are temporarily bonded, the second wafer 20 may completely cover the bonding surface 103 of the first wafer 10 .

[0067] In some specific examples, the second wafer 20 may include semiconductor material, transparent material or semi-transparent material. Here, the semiconductor material may include silicon, silicon germanium, etc., and the transparent material and semi-transparent material may include glass, plastic, etc.

[0068] In a specific example, the second wafer 20 may be a silicon wafer.

[0069] In another specific example, the second wafer 20 may be a glass wafer.

[0070] It should be noted that in the embodiment of the present disclosure, the second wafer 20 may be, in addition to being a silicon wafer or a glass wafer, any other material layer having a wafer shape or a shape similar to a wafer. For example, the second wafer 20 may also be a plastic layer having a wafer shape.

[0071] In some embodiments, in conjunction with reference Figure 4 and Figure 5Before executing step S30 , the wafer processing method further includes: thinning the second wafer 20 from one side away from the first wafer 10 among two sides of the second wafer 20 that are opposite to each other along the first direction.

[0072] In some specific examples, the thinning process may include one or more of an etching process, a chemical mechanical polishing (CMP) process, and a physical polishing process.

[0073] In other embodiments, before executing step S30, the second wafer 20 may not be thinned. In some specific examples, the second wafer 20 may be a wafer that has been used as a carrier wafer in other processes and has been thinned, thereby saving process costs. In other specific examples, the second wafer 20 may include a transparent material or a translucent material. For example, when the second wafer 20 is a glass wafer, after the first wafer 10 and the second wafer 20 are temporarily bonded, the second wafer 20 does not need to be thinned.

[0074] In some embodiments, in conjunction with reference Figures 5 to 8 Before executing step S30 , the wafer processing method further includes: performing a first etching on the second wafer 20 to form a third trench 202 in the second wafer 20 that exposes the first scribe line region 101 .

[0075] Specifically, the first etching is performed on the second wafer 20 to form a third trench 202 in the second wafer 20 that exposes the first scribe line region 101, including: Figure 5 and Figure 6 , forming a patterned photoresist layer 301 covering the second wafer 20, etching the second wafer 20 using the patterned photoresist layer 301 as a mask to form a fourth groove 302 exposing the temporary bonding layer 201; Figure 6 and Figure 7 , the remaining patterned photoresist layer 301 and the exposed temporary bonding layer 201 are removed to form a third trench 202 in the second wafer 20 .

[0076] In some specific examples, the first etching may include a dry etching process, and the dry etching process includes but is not limited to plasma etching (PE), sputtering etching (SE), ion beam etching (IBE), and reactive ion etching (RIE).

[0077] Figure 8FIG. 2 is a top view of the second wafer 20 after the third trench 202 is formed in the second wafer 20. Figure 7 and 8 The third trench 202 extends along the second direction and exposes the first scribe line region 101 in the first wafer 10 .

[0078] In some embodiments, the specific process of executing step S30 may include: performing a first laser cutting on the first wafer 10 with the second wafer 20 as a barrier layer to form a first groove 203 exposing the substrate 100 in the first cutting road area 101; the first groove 203 extends along the second direction; performing a second laser cutting on the first wafer 10 with the second wafer 20 as a barrier layer to form a second groove 204 exposing the substrate 100 in the second cutting road area 102; the second groove 204 extends along the third direction.

[0079] In some embodiments, in conjunction with reference Figure 7 and Fig. 9 , performing a first laser cutting on the first wafer 10 with the second wafer 20 as a barrier layer to form a first groove 203 exposing the substrate 100 in the first cutting road area 101, including: performing a first laser cutting on the first cutting road area 101 along the third groove 202 to form the first groove 203, and the first groove 203 is connected to the third groove 202.

[0080] In the embodiment of the present disclosure, the first scribe line region 101 includes a dielectric layer 104 and a conductive structure 105 located in the dielectric layer 104. Then, performing the first laser cutting on the first wafer 10 using the second wafer 20 as a barrier layer may specifically include: performing the first laser cutting on the dielectric layer 104 and the conductive structure 105 in the first scribe line region 101 using the second wafer 20 as a barrier layer. Fig. 9 As shown, when the first laser cutting is performed on the dielectric layer 104 and the conductive structure 105, since the material of the conductive structure 105 is vaporized at high temperature, the gaseous material evaporates and rises and is easily condensed to form slag when it is cooled. The slag will be deposited on the side surface of the second wafer 20 away from the first wafer 10, that is, the second wafer 20 can be used as a barrier layer in the laser cutting process to prevent the slag generated by the laser cutting from being directly deposited on the bonding surface of the first wafer 10.

[0081] In some embodiments, in conjunction with reference Fig. 9 and Fig.10 After performing a first laser cutting on the first cutting path area 101 of the first wafer 10 using the second wafer 20 as a barrier layer, the substrate 100 in the first cutting path area 101 is exposed by the first groove 203, and the wafer processing method also includes: performing a third etching on the substrate 100 exposed by the first groove 203 using the second wafer 20 as a mask.

[0082] In some specific examples, the third etching may be plasma etching. Specifically, the third etching may be Bosch etching, and the etching may be performed only along the Z direction through periodic “etching-passivation-etching”.

[0083] In some embodiments, in conjunction with reference Fig.11 and Fig.12 , Fig.12 for Fig.11 In the cross-sectional view along line BB', the wafer processing method further includes: before performing a second laser cutting on the first wafer 10 using the second wafer 20 as a barrier layer, debonding the first wafer 10 from the second wafer 20; and rotating the second wafer 20 and temporarily bonding it to the first wafer 10 again, so that the third groove 202 exposes the second cutting path area 102 in the first wafer 10.

[0084] In some specific examples, combined with reference Figure 8 and Fig.11 After the first wafer 10 and the second wafer 20 are debonded, the second wafer 20 can be rotated 90 degrees and then temporarily bonded to the first wafer 10 again, so that the third groove 202 exposes the second scribe line region 102 in the first wafer 10 .

[0085] In some embodiments, in conjunction with reference Fig.12 and Fig.13 , performing a second laser cutting on the first wafer 10 with the second wafer 20 as a barrier layer to form a second groove 204 exposing the substrate 100 in the second cutting area 102, including: performing a second laser cutting on the second cutting area 102 along the third groove 202 to form the second groove 204.

[0086] Here, the process of performing the second laser cutting is similar to the process of performing the first laser cutting on the first cutting path area 101, including: using the second wafer 20 as a barrier layer to perform the second laser cutting on the dielectric layer 104 and the conductive structure 105 in the second cutting path area 102. In this process, the slag generated during the laser cutting process will still be deposited on the side surface of the second wafer 20 away from the first wafer 10, thereby avoiding contamination of the bonding surface of the first wafer 10.

[0087] In some embodiments, in conjunction with reference Fig.13 and Fig.14 The wafer processing method further includes: performing a fourth etching on the substrate 100 exposed by the second groove 204 using the second wafer 20 as a mask. Here, the fourth etching may be the same etching process as the third etching.

[0088] In some embodiments, in conjunction with reference Fig.14 and Fig.15The wafer processing method further includes: debonding the first wafer 10 and the second wafer 20 to expose the bonding surface 103 of the first wafer 10 .

[0089] In some specific examples, the second wafer 20 may include a semiconductor material, and the first wafer 10 and the second wafer 20 may be debonded by a mechanical separation method or a thermal sliding method.

[0090] In some other specific examples, the second wafer 20 may include a transparent material or a translucent material. Since the second wafer 20 is light-transmissive, in addition to debonding the first wafer 10 and the second wafer 20 by mechanical separation and thermal sliding, the first wafer 10 and the second wafer 20 may also be debonded by a laser separation method. Specifically, the laser separation method may utilize an infrared laser or an ultraviolet laser to penetrate the light-transmissive second wafer 20 at room temperature and induce the photosensitive material in the temporary bonding layer 201 to rapidly decompose, vaporize, or even plasmatize and lose viscosity, thereby achieving debonding of the first wafer 10 and the second wafer 20 without applying mechanical stress.

[0091] In some specific examples, the wafer processing method also includes: after debonding the first wafer 10 and the second wafer 20, thinning the substrate 100 from the surface of the first wafer 10 opposite to the bonding surface 103 until the grooves formed in the substrate 100 by the third etching and the fourth etching are exposed, so that the first wafer 10 can be divided into multiple chips.

[0092] In other specific examples, performing a third etch on the substrate 100 exposed in the first groove 203 using the second wafer 20 as a mask and performing a fourth etch on the substrate exposed in the second groove 204 using the second wafer 20 as a mask may include directly forming an opening through the substrate 100 by an etching process to divide the first wafer 10 into multiple chips.

[0093] In the embodiment of the present disclosure, the second wafer 20 including a plurality of third grooves 202 can be used as a barrier layer for performing the first laser cutting and the second laser cutting on the first wafer 10. The slag generated during the laser cutting process can be deposited on the surface of the second wafer 20 on the side away from the first wafer 10, thereby preventing the slag from contaminating the bonding surface 103 of the first wafer 10 and reducing the negative impact on the subsequent bonding process. In addition, performing laser cutting on the first wafer 10 along the third grooves 202 is conducive to improving the alignment accuracy of the laser cutting.

[0094] In the embodiment of the present disclosure, the second wafer 20 including multiple third grooves 202 can also serve as a mask layer for performing the third etching and the fourth etching on the substrate 100 in the first wafer 10, thereby omitting the process step of forming the mask layer after the laser cutting process. Compared with the processing method of performing laser cutting on the wafer with the bonding surface exposed to the outside and then forming a patterned mask layer on the bonding surface of the wafer to etch the exposed substrate, the wafer processing method provided by the present disclosure can avoid the problem of poor reliability of the mask layer formed subsequently due to the deposition of slag generated by laser cutting on the bonding surface, and can avoid forming a mask layer on the wafer with grooves already formed, thereby improving the reliability of the subsequent etching process while avoiding contamination of the bonding surface.

[0095] The above embodiment takes the example of forming a plurality of third grooves 202 only in the second wafer 20. In other embodiments, in combination with reference to Figure 7 , Figure 8 , Fig.16 and Fig.17 , Fig.17 for Fig.16 In the cross-sectional view along the CC' line, after or at the same time as performing the first etching on the second wafer 20 to form the third groove 202 exposing the first scribe line region 101 in the second wafer 20, the second etching can be performed on the second wafer 20 to form the fifth groove 205 exposing the second scribe line region 102 in the second wafer 20; the fifth groove 205 is connected to the third groove 202. In this case, it is not necessary to debond the first wafer 10 and the second wafer 20 and then perform temporary bonding again. Fig.17 and Fig.18 , performing a second laser cutting on the first wafer 10 with the second wafer 20 as a barrier layer to form a second groove 204 exposing the substrate 100 in the second scribe line area 102, including: performing a second laser cutting on the second scribe line area 102 along the fifth groove 205 to form the second groove 204. Then, the third etching and the fourth etching can be performed on the substrate 100 exposed by the first wafer 10 using the second wafer 20 including the third groove 202 and the fifth groove 205 as a mask.

[0096] In the above embodiment, the second wafer 20 is first etched to form a plurality of grooves in the second wafer 20 to expose the scribe line area in the first wafer 10, and then the second wafer 20 including the plurality of grooves is used as a barrier layer to perform laser cutting on the scribe line area in the first wafer 10. In other embodiments, in combination with reference to Fig.19 , Fig. 20 and Fig.21 , Fig. 20 for Fig.19 Cross-section along line DD', Fig.21 for Fig.19In a cross-sectional view along line EE', a first laser cutting is performed on the first wafer 10 with the second wafer 20 as a barrier layer to form a first groove 203 exposing the substrate 100 in the first cutting street area 101, and a second laser cutting is performed on the first wafer 10 with the second wafer 20 as a barrier layer to form a second groove 204 exposing the substrate 100 in the second cutting street area 102, including: performing a first laser cutting on the first cutting street area 101 in the second wafer 20 and the first wafer 10 from one side of the second wafer 20 that is far away from the first wafer 10, which is opposite to each other along the first direction; Laser cutting is performed to form a first opening 210 in the second wafer 20 and a first groove 203 in the first cutting path area 101; the first opening 210 is connected to the first groove 203; a second laser cutting is performed on the second wafer 20 and the second cutting path area 102 in the first wafer 10 from one side of the second wafer 20 opposite to each other along the first direction and away from the first wafer 10 to form a second opening 211 in the second wafer 20 and a second groove 204 in the second cutting path area 102; the second opening 211 is connected to the second groove 204.

[0097] In the embodiment of the present disclosure, the first laser cutting and the second laser cutting can be directly performed on the second wafer 20 and the first wafer 10 to form a first opening 210 in the second wafer 20 that is connected to the first groove 203 formed in the first scribe line area 101 in the first wafer 10, and a second opening 211 in the second wafer 10 that is connected to the second groove 204 formed in the second scribe line area 102. In this process, the slag generated by the laser cutting can be deposited on the side surface of the second wafer 20 away from the first wafer 10, thereby avoiding contamination of the bonding surface of the first wafer 10. Further, the second wafer 20 including the first opening 210 and the second opening 211 can be used as a mask layer for etching the exposed substrate 100 in the first wafer 10.

[0098] In some specific examples, the first wafer 10 includes an alignment mark for aligning the first wafer 10 and the second wafer 20 when laser cutting is performed simultaneously. In a specific example, when the second wafer 20 includes a transparent material or a semi-transparent material, the alignment accuracy of the laser cutting can be improved.

[0099] In the embodiment of the present disclosure, the second wafer temporarily bonded to the first wafer can serve as a barrier layer when the first wafer is laser cut to prevent slag generated during the laser cutting process from contaminating the bonding surface of the first wafer, thereby reducing the impact on subsequent bonding processes.

[0100] In the embodiment of the present disclosure, after laser cutting, the second wafer including the grooves can also serve as a mask layer for etching the substrate in the first wafer, thereby omitting the process step of forming a mask layer after the laser cutting process, avoiding the problem of poor reliability of the subsequently formed mask layer due to the deposition of slag generated by laser cutting on the bonding surface, and avoiding the formation of a mask layer on the wafer in which the grooves have been formed, thereby improving the reliability of the subsequent etching process while avoiding contamination of the bonding surface.

[0101] In the embodiment of the present disclosure, the second wafer including the groove can also be used as a barrier layer and a mask layer in the cutting process of other wafers, thereby further saving process costs.

[0102] The methods disclosed in several method embodiments provided in the present disclosure can be arbitrarily combined without conflict to obtain new method embodiments.

[0103] The above description is only a specific implementation mode of the present disclosure, but the protection scope of the present disclosure is not limited thereto. Any technician familiar with the technical field can easily think of changes or substitutions within the technical scope disclosed in the present disclosure, which should be included in the protection scope of the present disclosure.

Claims

1. A wafer processing method, characterized in that: include: Providing a first wafer and a second wafer; the first wafer comprises a substrate and a bonding surface located on one of two sides of the substrate that are opposite to each other along a first direction; The first direction is a thickness direction of the first wafer; Temporarily bonding the first wafer to the second wafer, and forming a temporary bonding layer between the bonding surface and the second wafer; The first wafer is laser cut using the second wafer as a barrier layer.

2. The wafer processing method according to claim 1, characterized in that: The first wafer includes a first cutting street area extending along a second direction and a second cutting street area extending along a third direction; the second direction intersects with the third direction and is perpendicular to the first direction; the laser cutting of the first wafer using the second wafer as a barrier layer includes: Performing a first laser cutting on the first wafer using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting line region; the first groove extends along the second direction; The first wafer is subjected to a second laser cutting process using the second wafer as a barrier layer to form a second trench exposing the substrate in the second scribe line region; the second trench extends along the third direction.

3. The wafer processing method according to claim 2, characterized in that: The first cutting path area and the second cutting path area both include a dielectric layer and a conductive structure located in the dielectric layer; the first laser cutting of the first wafer using the second wafer as a barrier layer and the second laser cutting of the first wafer using the second wafer as a barrier layer include: Performing the first laser cutting on the dielectric layer and the conductive structure in the first scribe line region by using the second wafer as a barrier layer; The second laser cutting is performed on the dielectric layer and the conductive structure in the second scribe line region by using the second wafer as a barrier layer.

4. The wafer processing method according to claim 2, characterized in that: The wafer processing method further comprises: Before laser cutting the first wafer using the second wafer as a barrier layer, performing a first etching on the second wafer to form a third groove in the second wafer exposing the first scribe line area; The step of performing a first laser cutting on the first wafer using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting street region comprises: The first laser cutting is performed on the first scribe line region along the third groove to form the first groove.

5. The wafer processing method according to claim 4, characterized in that: The performing a first etching on the second wafer to form a third groove in the second wafer exposing the first scribe line area includes: forming a patterned photoresist layer covering the second wafer; Etching the second wafer using the patterned photoresist layer as a mask to form a fourth groove exposing the temporary bonding layer; The remaining patterned photoresist layer and the exposed temporary bonding layer are removed to form the third trench in the second wafer.

6. The wafer processing method according to claim 4, characterized in that: The wafer processing method further comprises: Before performing a second laser cutting on the first wafer using the second wafer as a barrier layer, debonding the first wafer from the second wafer; rotating the second wafer and temporarily bonding it to the first wafer again, so that the third groove exposes the second scribe line area in the first wafer; The step of performing a second laser cutting on the first wafer using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street region comprises: The second laser cutting is performed on the second scribe line region along the third groove to form the second groove.

7. The wafer processing method according to claim 4, characterized in that: The wafer processing method further comprises: After or simultaneously with performing the first etching on the second wafer to form the third groove exposing the first scribe line region in the second wafer, performing the second etching on the second wafer to form the fifth groove exposing the second scribe line region in the second wafer; the fifth groove is connected to the third groove; The step of performing a second laser cutting on the first wafer using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street region comprises: The second laser cutting is performed on the second scribe line region along the fifth groove to form the second groove.

8. The wafer processing method according to claim 2, characterized in that: The first wafer is subjected to a first laser cutting operation using the second wafer as a barrier layer to form a first groove exposing the substrate in the first cutting street region, and the second wafer is subjected to a second laser cutting operation using the second wafer as a barrier layer to form a second groove exposing the substrate in the second cutting street region, including: Performing the first laser cutting on the first scribe line region in the second wafer and the first wafer from one side of two sides of the second wafer opposite to each other along the first direction and away from the first wafer, so as to form a first opening in the second wafer and form the first groove in the first scribe line region; the first opening is connected to the first groove; The second laser cutting is performed on the second wafer and the second cutting path area in the first wafer from one side of the second wafer opposite to each other along the first direction and away from the first wafer to form a second opening in the second wafer and form the second groove in the second cutting path area; the second opening is connected to the second groove.

9. The wafer processing method according to claim 2, characterized in that: The wafer processing method further comprises: Performing a third etching on the substrate exposed by the first groove using the second wafer as a mask; A fourth etching is performed on the substrate exposed by the second groove by using the second wafer as a mask.

10. The wafer processing method according to claim 9, characterized in that: The wafer processing method further comprises: The first wafer and the second wafer are debonded to expose the bonding surface of the first wafer.

11. The wafer processing method according to claim 1, characterized in that: The wafer processing method further comprises: Before laser cutting the first wafer using the second wafer as a barrier layer, the second wafer is thinned on a side away from the first wafer from two opposite sides of the second wafer along the first direction.

12. The wafer processing method according to claim 1, characterized in that: The second wafer includes semiconductor material, transparent material or semi-transparent material.

Citation Information

Patent Citations

  • Method for removing bubble region in bonding process

    CN105529303A

  • Wafer cutting method

    CN114226984A

  • Wafer cutting method

    CN114446876A

  • Preparation method of semiconductor structure

    CN115799049A

  • Wafer cutting method

    WO2023019819A1