Novel structure aiming at uneven plating in single wafer electroplating process
By designing an inclined fixed plate and a hollow motor to drive the cup plating fixture to rotate in the single wafer electroplating process, combined with the rectifier plate and platinum titanium mesh, the problem of bubbles affecting the uniformity of the coating during cup plating is solved, improving product yield and efficiency.
Patent Information
- Application Number
- CN202420306568.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-20
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2034-02-20
AI Technical Summary
Uneven coating in the single-wafer electroplating process results in low product yield, high cost, and low efficiency. This is mainly due to the fact that bubbles attached to the wafer surface during cup plating electroplating affect the uniformity of the coating thickness across the entire wafer.
A new structure including an upper and lower shell is designed. A tilted fixed plate and a hollow motor are installed in the middle. The motor drives the cup plating fixture to perform 360-degree stepless rotation. It combines the rectifying plate and the platinum titanium mesh to discharge air bubbles through rotation, and A nitrogen protection unit is installed in the lower shell to prevent the gold plating liquid from reacting.
It effectively removes tiny bubbles on the wafer surface during electroplating, improves the uniformity of the coating across the entire wafer, and improves product yield and efficiency.
Smart Images

Figure CN221797701U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of wafer electroplating, in particular to a new structure for uneven plating in a single wafer electroplating process. Background Art
[0002] In recent years, in order to solve the above problems, a series of improved processes have emerged in the industry, but none of them have achieved the expected results. Electroplating equipment can be divided into two categories: horizontal jet cup plating and vertical rack plating. Cup plating covers the wafer on a cup-shaped plating tank, and electroplating is performed in a cup-by-piece manner. Rack plating immerses the wafer vertically in the plating solution, and one plating tank can electroplate multiple wafers at the same time.
[0003] Horizontal jet cup plating has the problem of bubbles attached to the wafer surface during electroplating, which affects the uniformity of the coating thickness across the wafer, resulting in low product yield, high product cost and low efficiency. Therefore, those skilled in the art provide a new structure for uneven coating in a single wafer electroplating process to solve the problems raised in the above background technology. Utility Model Content
[0004] 1. Technical issues to be solved
[0005] In view of the deficiencies of the prior art, the utility model provides a novel structure for uneven coating in a single wafer electroplating process, so as to solve the problem that bubbles generated during cup plating affect the uniformity of the coating thickness over the entire wafer.
[0006] (II) Technical solution
[0007] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a new structure for uneven plating in a single wafer electroplating process, comprising an upper shell and a lower shell, wherein an inclined fixing plate is installed in the upper shell, a hollow motor is installed on the fixing plate, a cup plating fixture is installed at the tail end of the hollow motor, a reflow spraying is installed on the inner bottom side of the lower shell, the bottom side wall of the lower shell is inclined, a rectifier plate is arranged on the side of the reflow spraying facing the inner wall of the inclined plate, a platinum-titanium mesh is arranged on the side of the rectifier plate away from the reflow spraying, and an anode rod is connected to the upper end of the platinum-titanium mesh.
[0008] Preferably, a mercury slip ring is provided in the hollow motor, and the mercury slip ring is connected to the cathode in the hollow motor. The tail end of the cup plating fixture clamps the wafer, and the front side of the wafer is conductively conducted through the mercury slip ring. The cup plating fixture is driven by the hollow motor to drive the wafer to rotate 360 degrees steplessly, and the tiny bubbles generated during electroplating are discharged through rotation.
[0009] Preferably, a nitrogen protection unit is provided above the reflow spraying, and the nitrogen protection unit is connected to the inner wall of the lower shell. The function of the nitrogen protection unit is to protect the gold plating liquid by performing nitrogen blowing operation inside the tank body to prevent the gold plating liquid from reacting with the air.
[0010] Preferably, the hollow motor is fixed at a 45-degree tilt, the cup plating fixture has the same tilt angle as the hollow motor, the rectifier plate and the platinum titanium mesh are both tilted, the rectifier plate is parallel to the end of the cup plating fixture, and the wafer is gold-plated through the rectifier plate. This structure makes the wafer parallel to the anode titanium mesh, and the cup plating fixture drives the wafer to rotate 360 degrees infinitely, thereby discharging hydrogen bubbles on the wafer surface.
[0011] (III) Beneficial effects
[0012] Compared with the prior art, the utility model provides a new structure for uneven plating in a single wafer electroplating process, which has the following beneficial effects:
[0013] Through the design, the cathode is connected to the mercury slip ring, the cup plating fixture is used to conduct electricity to the front side of the wafer, the cup plating fixture is driven by the hollow motor to drive the wafer to rotate 360 degrees steplessly, and the wafer is gold-plated through the rectifier plate. The tiny bubbles generated during electroplating are discharged through rotation. This structure makes the wafer parallel to the anode titanium mesh, and the cup plating fixture drives the wafer to rotate 360 degrees steplessly, so that the hydrogen bubbles on the wafer surface are discharged, which solves the problem of bubbles generated during cup plating affecting the uniformity of the coating thickness throughout the wafer, thereby improving product yield and efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 It is a three-dimensional structural schematic diagram of a new structure for uneven plating in a single wafer electroplating process provided by an embodiment of the present application.
[0015] Figure 2 It is a structural schematic diagram of a hollow motor with a new structure for uneven plating in a single wafer electroplating process provided in an embodiment of the present application.
[0016] Figure 3 It is a schematic diagram of the structure of a cup plating fixture with a new structure for uneven plating in a single wafer electroplating process provided in an embodiment of the present application.
[0017] Figure 4 It is a structural schematic diagram of a rectifier plate in a new structure for uneven plating in a single wafer electroplating process provided in an embodiment of the present application.
[0018] Figure 5 It is a schematic diagram of the structure of a platinum-titanium mesh in a new structure for uneven plating in a single wafer electroplating process provided in an embodiment of the present application.
[0019] In the figure: 1. Hollow motor; 2. Cup plating fixture; 3. Reflow spraying; 4. Rectifier plate; 5. Platinum titanium mesh; 6. Anode rod; 7. Upper shell; 8. Lower shell; 9. Mercury slip ring; 10. Nitrogen protection unit. DETAILED DESCRIPTION
[0020] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0021] The utility model provides a technical solution, a new structure for uneven plating in a single wafer electroplating process, please refer to Figure 1 , Figure 2 , including an upper shell 7 and a lower shell 8, wherein an inclined fixing plate is installed in the upper shell 7, and a hollow motor 1 is installed on the fixing plate, see Figure 2 , Figure 3 , Figure 4 , Figure 5 A cup plating fixture 2 is installed at the tail end of the hollow motor 1, a reflow spraying 3 is installed on the inner bottom side of the lower shell 8, the bottom side wall of the lower shell 8 is inclined, a rectifier plate 4 is arranged on the side of the reflow spraying 3 facing the inner wall of the inclined plate, a platinum titanium mesh 5 is arranged on the side of the rectifier plate 4 away from the reflow spraying 3, an anode rod 6 is connected to the upper end of the platinum titanium mesh 5, a mercury slip ring 9 is arranged in the hollow motor 1, and the mercury slip ring 9 is connected to the cathode in the hollow motor 1, a wafer is clamped at the tail end of the cup plating fixture 2, and the front side of the wafer is electrically conductive through the mercury slip ring 9, The cup plating fixture 2 is driven by the hollow motor 1 to drive the wafer to rotate 360 degrees without limit, and the tiny bubbles generated during electroplating are discharged by rotating. The hollow motor 1 is fixed at a 45-degree tilt, and the cup plating fixture 2 has the same tilt angle as the hollow motor 1. The rectifier plate 4 and the platinum titanium mesh 5 are both tilted at 45 degrees. The rectifier plate 4 is parallel to the end of the cup plating fixture 2. The wafer is gold-plated through the rectifier plate 4. This structure makes the wafer parallel to the anode titanium mesh 5. The cup plating fixture 2 drives the wafer to rotate 360 degrees without limit, so that the hydrogen bubbles on the wafer surface are discharged;
[0022] See also Figure 2 , Figure 3 , Figure 4A nitrogen protection unit 10 is arranged above the reflow spraying 3, and the nitrogen protection unit 10 is connected to the inner wall of the lower shell 8. The function of the nitrogen protection unit 10 is to protect the gold plating liquid by performing nitrogen blowing operation inside the tank body to prevent the gold plating liquid from reacting with the air.
[0023] In the present invention, the cathode is connected to the mercury slip ring 9, the front side of the wafer is electrically conductive through the cup plating fixture 2, the hollow motor 1 drives the cup plating fixture 2 to drive the wafer to rotate 360 degrees, the wafer is gold plated through the rectifier plate 4, and the tiny bubbles generated during electroplating are discharged by rotating. This structure makes the wafer parallel to the anode titanium mesh 5, and the cup plating fixture 2 drives the wafer to rotate 360 degrees, so that the hydrogen bubbles on the surface of the wafer are discharged. Therefore, the application effect of the 45° inclined stepless rotating cup plating is that the tiny hydrogen bubbles attached to the surface of the wafer during electroplating are effectively removed;
[0024] The nitrogen protection unit 10 is used to protect the gold plating liquid by blowing nitrogen into the tank body to prevent the gold plating liquid from reacting with the air.
[0025] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0026] In this document, unless otherwise clearly stipulated and limited, terms such as "installation", "setting", "connection", "fixation", and "screw-on" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integrated connection; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium; it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, ordinary technicians in this field can understand the specific meanings of the above terms in this utility model according to the specific circumstances.
[0027] Although the embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A novel structure for uneven plating in a single wafer electroplating process, comprising an upper shell (7) and a lower shell (8), Features: An inclined fixing plate is installed in the upper shell (7), a hollow motor (1) is installed on the fixing plate, a cup plating fixture (2) is installed at the tail end of the hollow motor (1), a reflow spraying (3) is installed on the inner bottom side of the lower shell (8), the bottom side wall of the lower shell (8) is inclined, a rectifier plate (4) is arranged on the side of the reflow spraying (3) facing the inner wall of the inclined plate, a platinum titanium mesh (5) is arranged on the side of the rectifier plate (4) away from the reflow spraying (3), and an anode rod (6) is connected to the upper end of the platinum titanium mesh (5).
2. A novel structure for uneven plating in a single wafer electroplating process according to claim 1, Features: A mercury slip ring (9) is arranged inside the hollow motor (1), and the mercury slip ring (9) is connected to the cathode inside the hollow motor (1). The tail end of the cup plating fixture (2) clamps a wafer, and conducts electricity to the front side of the wafer through the mercury slip ring (9).
3. A novel structure for uneven plating in a single wafer electroplating process according to claim 2, Features: The hollow motor (1) drives the cup plating fixture (2) to rotate, thereby driving the wafer to rotate 360 degrees steplessly.
4. According to claim 1, a novel structure for uneven plating in a single wafer electroplating process, Features: A nitrogen protection unit (10) is arranged above the reflow spraying (3), and the nitrogen protection unit (10) is connected to the inner wall of the lower shell (8).
5. A novel structure for uneven plating in a single wafer electroplating process according to claim 1, Features: The hollow motor (1) is fixed at an angle of 45 degrees, and the cup plating fixture (2) and the hollow motor (1) have the same angle of inclination.
6. A novel structure for uneven plating in a single wafer electroplating process according to claim 5, Features: The rectifying plate (4) and the platinum titanium mesh (5) are both inclined at 45 degrees, and the rectifying plate (4) is parallel to the end of the cup plating fixture (2).