System for recovering metal from waste

By designing a recovery system including a leaching slag bin, anthracite coal bin and quicklime powder tank, and using high-temperature heating and volatilization kiln technology, the zinc in the leaching slag is effectively extracted, thus solving the waste of zinc resources and environmental pollution in the hydrometallurgical zinc smelting process. problem, improving the zinc refining ratio and reducing coal consumption.

CN221837065UActive Publication Date: 2024-10-15NANJING XIPU INT ENG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202322507241.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-09-15
Publication Date
2024-10-15
Estimated Expiration
2033-09-15

AI Technical Summary

Technical Problem

The leaching residue produced during the hydro-zinc smelting process contains a large amount of zinc. However, due to insufficient zinc metal content, it cannot meet the requirements of hydro-zinc smelting, resulting in resource waste and environmental pollution, and there is a lack of effective treatment methods.

Method used

A system for recovering metals from waste materials is designed, including a leaching slag bin, anthracite coal bunker and quicklime powder tank. The leaching slag is mixed with anthracite coal and quicklime powder through equipment such as elevator, mixer, briquetting machine and volatilization kiln. and high-temperature heating to generate volatile zinc compounds, which are then cooled and collected, and finally metallic zinc is extracted.

Benefits of technology

The zinc refining ratio is increased, the coal consumption and the zinc content of the leaching residue are reduced, environmental pollution is reduced, and the effective recovery of zinc is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221837065U_ABST
    Figure CN221837065U_ABST
Patent Text Reader

Abstract

The utility model discloses a system for recovering metal from waste materials, which comprises a leaching residue bin, an anthracite bin and a quicklime powder tank, the output ends of the leaching residue bin, the anthracite bin and the quicklime powder tank are connected to the inlet of an elevator I, the output end of the elevator I is connected to a blender mixer, the output end of the blender mixer is connected to a ball press machine, and the output end of the ball press machine is connected to the inlet of the elevator II. And the output end of the ball press machine is connected to the volatilization kiln. The zinc is reduced by carbon, substances such as ZnSO4, ZnO, ZnO.FeO3, ZnS and the like are generated by high-temperature heating, and the mixtures can be volatilized at high temperature, then cooled by cooling equipment and collected by dust collection equipment and the like; and finally, metal zinc is extracted according to a normal zinc extraction method. In the whole process, the zinc refining ratio is increased, the coal consumption is reduced, the zinc content of the leaching residues is reduced, and the environmental pollution is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of zinc recovery, and in particular relates to a system for recovering metal from waste materials. Background Art

[0002] After extracting metallic zinc from the raw ore, the leaching residue still contains more than 15.31% zinc. Directly treating the leaching residue as waste wastes resources and pollutes the environment. Hydrometallurgy is the most important zinc smelting method today, and its output accounts for more than 85% of the world's total zinc output. The amount of leaching residue produced is huge. The leaching residue contains a variety of heavy metals and sulfides, which cause environmental pollution. Since the zinc metal content in it cannot meet the requirements of hydrometallurgy, there is currently no effective treatment method to extract the zinc contained in the leaching residue. Utility Model Content

[0003] The purpose of the utility model is to provide a system for recovering metals from waste materials to solve the problems raised in the above background technology.

[0004] To achieve the above-mentioned purpose, the utility model provides the following technical solutions: a system for recovering metals from waste materials, comprising a leaching slag bin, an anthracite bin and a quicklime powder tank, wherein the output ends of the leaching slag bin, the anthracite bin and the quicklime powder tank are connected to the inlet of elevator one, the output end of elevator one is connected to a mixer, the output end of the mixer is connected to a ball press, and the output end of the ball press is connected to a volatilization kiln.

[0005] Preferably, a quantitative feeder is provided at the outlet of the leached slag bin and the anthracite bin, the output end of the quantitative feeder is connected to the conveyor belt three, and the output end of the quicklime powder tank is connected to the inlet of the elevator one through a multi-section conveyor belt.

[0006] Preferably, a storage bin is provided at the outlet of the elevator 1, a buffer bin 1 is provided at the lower side of the storage bin, the outlet of the buffer bin 1 is connected to a quantitative feeder, and the outlet of the quantitative feeder is connected to the inlet of the mixer.

[0007] Preferably, a buffer bin 2 is provided at the lower end of the mixer, and an outlet of the buffer bin 2 is connected to a ball press.

[0008] Preferably, the outlet of the ball press is connected to a conveyor belt four, and a combination of several conveyor belt fours conveys the material to the ball bin.

[0009] Preferably, the outlet of the ball bin is connected to the inlet of the second elevator, and the outlet of the second elevator is connected to the volatilization kiln.

[0010] The technical effects and advantages of the utility model are as follows: zinc is reduced by carbon, and high temperature heating to 1100-1300 degrees Celsius produces ZnSO4, ZnO, ZnO.FeO3, ZnS and other substances, these mixtures can volatilize at high temperature, and then be cooled by cooling equipment, and collected by dust collecting equipment; finally, metallic zinc is extracted according to the normal method of extracting zinc; the whole process improves the zinc refining ratio, reduces coal consumption, reduces the zinc content of leaching slag, and reduces environmental pollution. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is the equipment layout diagram of the utility model;

[0012] Figure 2 for Figure 1 BB cross-sectional view;

[0013] Figure 3 for Figure 1 AA section view;

[0014] Figure 4 for Figure 1 CC section view;

[0015] Figure 5 for Figure 1 DD cross-sectional view;

[0016] Figure 6 It is a structural schematic diagram of the utility model.

[0017] In the figure: 2. Leaching slag bin; 3. Dosing feeder; 4. Anthracite bin; 5. Conveyor belt 2; 6. Crusher; 7. Conveyor belt 3; 8. Quicklime powder tank; 9. Elevator 1; 10. Storage bin; 11. Buffer bin 1; 12. Mixer; 13. Buffer bin 2; 14. Ball press; 15. Conveyor belt 4; 16. Ball bin; 17. Elevator 2; 18. Volatilization kiln. DETAILED DESCRIPTION

[0018] The specific implementation methods of the present invention are further described below in conjunction with the accompanying drawings. It should be noted that the description of these implementation methods is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in each implementation method of the present invention described below can be combined with each other as long as they do not conflict with each other.

[0019] The utility model provides Figure 1-5A system for recovering metals from waste materials is shown, wherein a leaching slag bin 2, an anthracite bin 4 and a quicklime powder tank 8 are provided in a plant, and a quantitative feeder 3 is provided at the outlet of the leaching slag bin 2 and the anthracite bin 4, and the output end of the quantitative feeder 3 on the lower side of the leaching slag bin 2 is connected to a conveying belt three 7, and the quantitative feeder 3 on the lower side of the anthracite bin 4 is connected to the inlet of a crusher 6 through a conveying belt two 5, and the outlet of the crusher 6 is connected to the conveying belt three 7, and the output end of the quicklime powder tank 8 is connected to the inlet of an elevator one 9 through a multi-section conveyor belt, and the end of the conveying belt three 7 is also connected to the inlet of an elevator one 9, and a storage bin 10 is provided at the outlet of the elevator one 9, and a buffer bin one 1 is provided at the lower side of the storage bin 10 1. Buffer bin 11 is used to buffer materials to ensure that the mixer 12 at the lower side has sufficient material supply. A quantitative feeder 3 is arranged under the buffer bin 11, and the outlet of the quantitative feeder 3 is connected to the inlet of the mixer 12. A buffer bin 2 13 is arranged at the lower end of the mixer 12. The outlet of the buffer bin 2 13 is connected to a ball press 14, and the ball press 14 makes balls of the materials; the outlet of the ball press 14 is connected to a conveyor belt 4 15, and a combination of several conveyor belts 4 15 conveys the materials to a ball bin 16, and the outlet of the ball bin 16 is connected to the inlet of an elevator 2 17, and the outlet of the elevator 2 17 is connected to a volatilization kiln 18, and the smoke exhaust port of the volatilization kiln 18 is connected to a dust collector (not shown).

[0020] Specifically, the briquetting machine 14 can wrap the coal in balls, reduce the waste of coal burning in the low-temperature section, and allow as much of the coal as possible to exist as a reducing agent in the high-temperature section.

[0021] Specifically, the volatilization kiln 18 raises the temperature to 1100-1300° C. to provide a reducing environment for zinc;

[0022] The process flow of the metal recovery system from waste materials is as follows Figure 6 As shown, the zinc leaching residue treated by the filter press is transported to the leaching residue bin 2 through a feeding belt, and the bin volume is 26t; a quantitative feeder 3 is set at the bottom of the leaching residue bin 2, and the anthracite is placed in the anthracite bin 4 through a grab bucket, and the bin volume is 15t to ensure continuous production; a quantitative feeder 3 is set at the bottom of the anthracite bin 4, and a crusher 6 is set under the quantitative feeder 3 on the lower side of the anthracite bin 4 to crush the raw coal; quicklime is transported to the quicklime powder tank 8, and the quicklime powder tank 8 has a volume of 50m 3, to ensure continuous production; through the metering scale, to ensure accurate dosage; the leached slag, raw coal and quicklime powder are accurately measured by the quantitative feeder to achieve a proportion and enter the elevator 9 together; all the mixtures enter the storage bin 10 and the buffer bin 11 together, and then enter the mixer 12 (with a certain crushing function) through the quantitative feeder metering scale; after crushing and mixing, they enter the buffer bin 2 13, and the buffer bin 2 13 is equipped with a ball press 14, and the mixture is pressed into balls. It is sent to the ball bin 16 through the conveyor belt 4 15, and the quantitative feeder is set under the ball bin 16. The ball is fed into the volatilization kiln 18 through the elevator 2 17. In the volatilization kiln 18, physical and chemical reactions are generated by calcination. The metals and their oxides are discharged with the flue gas and recovered by the dust collector through the cooler; the recycled materials can re-enter the wet zinc smelting system, and the remaining kiln slag is stored and waits for harmless treatment.

[0023] Working principle introduction:

[0024] At a temperature of 1100-1300℃, valuable metals such as zinc and lead are reduced to metal elements by the carbon in the anthracite through this device and enter the flue gas, where they react with oxygen and sulfur to form ZnSO4, ZnO, ZnO.FeO3, ZnS and other substances, which are then collected by dust collection equipment and enter the original wet zinc smelting process.

[0025] Although the embodiments of the present invention have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations of the present invention. Ordinary technicians in the field can change, modify, replace and modify the above embodiments within the scope of the present invention.

Claims

1. A system for recovering metals from waste materials, characterized in that: The invention comprises a leaching slag bin (2), an anthracite bin (4) and a quicklime powder tank (8), wherein the output ends of the leaching slag bin (2), the anthracite bin (4) and the quicklime powder tank (8) are connected to the inlet of an elevator (9), the output end of the elevator (9) is connected to a buffer bin (11), the output end of the buffer bin (11) is connected to a mixer (12), the output end of the mixer (12) is connected to a ball press (14), and the output end of the ball press (14) is connected to a volatilization kiln (18).

2. A system for recovering metals from waste materials according to claim 1, characterized in that: A quantitative feeder (3) is provided at the outlet of the leached slag bin (2) and the anthracite bin (4), and the output end of the quantitative feeder (3) is connected to a conveyor belt three (7), and the output end of the quicklime powder tank (8) is connected to the inlet of an elevator one (9) through a multi-section conveyor belt.

3. A system for recovering metals from waste materials according to claim 1, characterized in that: A storage bin (10) is arranged at the outlet of the elevator (9), a buffer bin (11) is arranged at the lower side of the storage bin (10), a quantitative feeder (3) is arranged at the outlet of the buffer bin (11), and the quantitative feeder (3) is connected to the inlet of the mixer (12).

4. A system for recovering metals from waste materials according to claim 1, characterized in that: A second buffer bin (13) is provided at the lower end of the mixer (12), and an outlet of the second buffer bin (13) is connected to a ball press (14).

5. A system for recovering metals from waste materials according to claim 1, characterized in that: The outlet of the ball press (14) is connected to a conveyor belt four (15), and a plurality of conveyor belts four (15) are combined to convey the material to the ball bin (16).

6. A system for recovering metals from waste materials according to claim 5, characterized in that: The outlet of the ball bin (16) is connected to the inlet of the second elevator (17), and the outlet of the second elevator (17) is connected to the volatilization kiln (18).