60TY1 wing rail profiling heating coil

By designing a combination of independent electromagnetic induction coils and magnet sheets, the problems of uneven heating and low efficiency of 60TY1 wing rails are solved, and the uniformity of heating temperature and improvement of efficiency are achieved. It is suitable for rapid and rapid heating of asymmetric cross-section rails. Efficient heating.

CN221930179UActive Publication Date: 2024-10-29CHINA RAILWAY BAOJI BRIDGE GROUP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323510457.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-21
Publication Date
2024-10-29
Estimated Expiration
2033-12-21

AI Technical Summary

Technical Problem

The existing technology is difficult to quickly, efficiently and evenly heat asymmetric cross-section rails such as 60TY1 wing rails, especially at the bending points, resulting in uneven heating, safety hazards and low efficiency.

Method used

A profiling heating device including two independent halves of electromagnetic induction coils is designed. The electromagnetic induction coil is wound with a square copper tube, and magnetic conductive sheets are installed on the rail top and rail waist, combined with insulating and high-temperature-resistant materials. Secure components to ensure uniform heating and safety.

Benefits of technology

It achieves improved heating temperature uniformity and efficiency, reduces heating time, avoids overheating and deformation, ensures the stability and safety of the heating process, and is suitable for rapid and efficient heating of asymmetric cross-section rails.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221930179U_ABST
    Figure CN221930179U_ABST
Patent Text Reader

Abstract

The utility model provides a 60TY1 wing rail profiling heating coil which comprises two half independent electromagnetic induction coils. The electromagnetic induction coils are arranged by simulating the outline of a 60TY1 steel rail, and after the two half independent electromagnetic induction coils are close to each other, a space for accommodating the 60TY1 steel rail is formed in the center; the electromagnetic induction coil is formed by winding a red copper tube, and high-temperature-resistant insulating paint is sprayed outside the electromagnetic induction coil; the distance between the coil inner contour of the electromagnetic induction coil corresponding to the upper and lower surfaces of the rail bottom and the steel rail surface is greater than the distance between other inner contours of the coil and the steel rail surface; fixing parts for preventing the coil from deforming are respectively arranged on the electromagnetic induction coil corresponding to the outer vertical end faces of the rail head and the rail bottom along the length direction of the steel rail; and the electromagnetic induction coil is provided with a plurality of magnetizer sheets corresponding to the rail top and the rail waist. The device can ensure that each part of the asymmetric section steel rail can be quickly, efficiently and uniformly heated, ensures the heating consistency effect, is easy to control the temperature, is safe and reliable, and has a good heating effect.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model belongs to the technical field of rail induction heating devices, and in particular relates to a profile heating coil for an asymmetric cross-section rail, especially a 60TY1 wing rail. Background Art

[0002] Railway turnouts are basic equipment that divides a track into two or more tracks, allowing locomotives and vehicles to switch from one line to another. At present, domestic high-speed turnouts all use a movable point rail frog structure, and the wing rail is an important part of the movable point rail frog. The front half supports the wheels, and the rear half supports the point rail and maintains the frog frame structure.

[0003] The existing wing rails are all made of special section wing rails (hereinafter referred to as "60TY 1 wing rails"), which have been in use for more than ten years. They have the advantages of high strength and uniform material. However, due to the wide rail head, many processing parts, complex process and large milling amount, they bring many difficulties to processing.

[0004] During the manufacturing process of 60TY1 wing rails, due to design requirements, certain bending is required. Rails with larger bending angles, especially those with wide rail heads, will have large deformation during the bending process. In addition, offline heat treatment will reduce its toughness, milling will easily produce a white layer, and low temperatures in winter will increase the brittleness of the rails and other unfavorable factors, which will easily cause cracks or even fracture defects. A better way to solve this problem is to heat the bending area to improve toughness, which involves the heating method and heating temperature at the bending point.

[0005] At present, there are three main top bending heating methods in use: one is gas flame heating (mainly propane + oxygen), which has the disadvantages of poor control of heating temperature, large temperature difference between the inside and outside of the rail, and potential safety hazards in the use of combustible gas on site; the second is the rail top bending preheating devices disclosed in publication numbers CN216126380U, CN216864684U, CN217528829U, etc., all of which adopt resistance wire heating. This method improves the shortcomings of flame heating, but the heating time is relatively long, about 15 minutes for one bending point; the third is a rail profiling induction heating device disclosed in publication number CN217173810U. The patent provides an electromagnetic induction coil with a symmetrical cross-section, which is designed for rails with small rail head cross-section and thin rail waist thickness, and the heating is easy to control. However, for asymmetric cross-section rails such as the 60TY1 wing rail, which has a larger cross-section, a thicker rail waist and a thinner rail bottom, how to ensure that parts of the rail at different positions and thicknesses can be heated quickly, efficiently and evenly to ensure the consistency of heating effects is a very critical issue. However, there is currently no relevant patent involving the heating design of electromagnetic induction coils for this type of asymmetric cross-section rail.

[0006] In this regard, it is necessary to design and manufacture a heating coil with easy-to-control temperature, safety and reliability, higher heating efficiency, stable structural dimensions, uniform heating, and good heating effect. The following technical solution is now proposed. Utility Model Content

[0007] The utility model solves the technical problem of providing a 60TY1 wing rail profile heating coil, solving the technical problem of how to design a profile heating coil for asymmetric cross-section wing rails to heat quickly, efficiently and evenly based on the electromagnetic induction heating principle.

[0008] The utility model adopts the following technical scheme: a 60TY1 wing rail profiling heating coil, comprising two independent electromagnetic induction coils; the electromagnetic induction coil is arranged to imitate the contour of the 60TY1 rail, and when the two independent electromagnetic induction coils are brought close together, a space for accommodating the 60TY1 rail is formed in the center; the electromagnetic induction coil is an electromagnetic induction coil wound with a copper tube and sprayed with high-temperature resistant insulating paint on the outside; the distance between the inner contour of the coil at the upper and lower surfaces of the rail bottom corresponding to the electromagnetic induction coil and the rail surface is greater than the distance between the other inner contours of the coil and the rail surface; the electromagnetic induction coil is provided with fixing components for preventing the coil from being deformed at the outer vertical end faces of the rail head and the rail bottom corresponding to the rail along the length direction of the rail; the electromagnetic induction coil is provided with a plurality of magnetic conductive sheets at the rail top and rail waist corresponding to the rail.

[0009] In the above technical solution, preferably: the electromagnetic induction coil is an electromagnetic induction coil wound with a square copper tube.

[0010] In the above technical solution, further: the cross-sectional dimensions of the square copper tube are 10×10×1 mm; a gap of 8 to 12 mm is maintained between adjacent coils; and the span of the entire electromagnetic induction coil is 140 to 160 mm.

[0011] In the above technical solution, further: during heating operation, the inner contour of the electromagnetic induction coil at the upper and lower surfaces of the rail bottom corresponding to the coil is 30 to 40 mm away from the rail surface; the inner contour of the remaining parts of the electromagnetic induction coil is 10 to 25 mm away from the rail surface.

[0012] In the above technical solution, preferably: the fixing component is a fixing component made of insulating high temperature resistant material.

[0013] The advantages of this utility model compared with the prior art:

[0014] 1. Compared with flame heating, the induction heating method of the utility model improves the uniformity of the temperature in the heating area and the internal and external quality, and the temperature of each area is closer, avoiding overheating or even overburning. Compared with the resistance wire heating box, the heating efficiency of the 60TY1 wing rail is improved, and the heating time is reduced from about 15 minutes to about 5 minutes.

[0015] 2. The utility model adopts a fixing component made of insulating high temperature resistant material to fix the coils, which can better prevent the deformation of the coils, maintain the inherent size of the coils, ensure the distance between them and the wing rails, and improve the temperature stability during the heating process.

[0016] 3. The utility model installs magnetic conductive sheets at the corresponding thicker parts of the rail top and rail waist. According to the specific thickness of the heated part, the number of magnetic conductive sheets is finally increased or decreased to balance the temperature of each area of ​​the wing rail heating section and ensure uniform temperature at the bending point of the rail during top bending.

[0017] 4. The utility model sprays high-temperature resistant insulating paint evenly on the surface of the manufactured coil to replace the high-temperature resistant insulating cloth. The appearance is beautiful and neat, and no cloth scraps will fall off during use. Under the premise of ensuring safety, only repainting operation is required after damage, which improves the efficiency and convenience of repair.

[0018] 5. The utility model is aimed at asymmetric cross-section rails, such as the cross-sections of 60AT1 rails and 60TY1 wing rails after processing, and the induction coils can be made by the method of the utility model to perform heating top bending. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 This is the vertical cross-sectional front view of the 60TY1 rail of the utility model;

[0020] Figure 2 It is a three-dimensional diagram of the heating coil of the utility model;

[0021] Figure 3 This is a three-dimensional diagram of the heating coil of the utility model in heating use state;

[0022] In the figure: 1-electromagnetic induction coil, 2-fixed component, 3-magnetic conductive sheet. DETAILED DESCRIPTION

[0023] The following will be combined with the attached embodiment of the present utility model Figure 1-3 , clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of them. Based on the embodiments of the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0024] (like Figure 1 , Figure 2A 60TY1 wing rail profiling heating coil as shown in the figure comprises two independent electromagnetic induction coils 1. The electromagnetic induction coil 1 is arranged to imitate the contour of the 60TY1 rail. When the two independent electromagnetic induction coils 1 are brought close together, a space for accommodating the 60TY1 rail is formed in the center. That is, the heating coil of the utility model can be applied to a rail profiling induction heating device disclosed in the publication number CN217173810U, and the rail is heated by the electromagnetic induction heating principle. The advantages of electromagnetic induction heating, such as fast, clean, energy-saving, efficient, easy to implement, and easy to heat online, are retained.

[0025] On this basis, the biggest improvement of the utility model lies in the following points: First, the electromagnetic induction coil 1 is an electromagnetic induction coil wound with a copper tube and sprayed with high temperature resistant insulating paint on the outside. The copper tube referred to here includes square and round copper tubes.

[0026] In the above embodiment, it is preferred that: the electromagnetic induction coil 1 is an electromagnetic induction coil wound with a square copper tube. When a square copper tube is used for heating, it has the advantages of higher heating efficiency and better heating uniformity. Because the heating area of ​​the square copper tube is larger, electromagnetic energy can be used more effectively to improve heating efficiency; the heating surface of the square copper tube is more uniform, and the heating temperature and heating speed can be better controlled to avoid local overheating or uneven temperature. In addition, the shape of the square copper tube is more regular, and it is easier to install and fix; the shape of the square copper tube is simpler, and it is easier to repair and replace, which can reduce maintenance costs.

[0027] Moreover, in the above embodiment, further: for the 60TY1 wing rail, the cross-sectional dimensions of the square copper tube are 10×10×1mm; a gap of 8 to 12mm is maintained between adjacent coils; and the span of the entire electromagnetic induction coil 1 is 140 to 160mm. The above size range is determined after multiple comparison experiments based on the size characteristics of the 60TY1 wing rail. As the optimal solution: a gap of 10mm is maintained between adjacent coils; and the span of the entire electromagnetic induction coil 1 is 150mm.

[0028] Secondly, the distance between the inner contour of the electromagnetic induction coil 1 at the upper and lower surfaces of the rail bottom and the rail surface is greater than the distance between the rest of the inner contour of the coil and the rail surface.

[0029] In the above embodiment, further: to ensure the uniformity of the heating temperature, the inner contour of the coil at the upper and lower surfaces of the rail bottom corresponding to the electromagnetic induction coil 1 during heating is 30 to 40 mm away from the rail surface; the inner contour of the remaining parts of the electromagnetic induction coil 1 is 10 to 25 mm away from the rail surface. The above distance range is adopted because: the bottom of the 60TY1 wing rail is thinner, while the remaining parts are thicker. Therefore, in order to ensure the consistency of the heating temperature of each surface of the 60TY1 wing rail and obtain a more uniform heating effect, this distance range scheme is adopted after multiple tests. Therefore, the overall purpose of adopting the aforementioned technical scheme is to meet the needs of rapid heating on the basis of complying with the principle of electromagnetic induction heating, and to obtain a better and more uniform heating effect.

[0030] In addition, the electromagnetic induction coil technology solution made by spraying high-temperature resistant insulating paint on the outside of the copper tube aims to improve the safety during use and the convenience of maintenance. That is, the high-temperature resistant insulating paint is evenly sprayed on the surface of the prepared coil to replace the high-temperature resistant cloth and other materials used before, so as to reduce the breakage and falling of the cloth during later use and avoid the inconvenience of overall replacement; when the paint falls off, it can be repainted in time to ensure the safety of on-site use and the convenience of repair after damage.

[0031] Furthermore, the electromagnetic induction coil 1 is provided with fixing components 2 for preventing the coil from deforming at the outer vertical end surfaces of the rail head and the rail bottom corresponding to the rail head and the rail bottom along the length direction of the rail.

[0032] The fixing component 2 is composed of a fixing plate and fixing nails; the fixing plate is a long strip structure, and is arranged along the length direction of the rail corresponding to the outer vertical end surface of the rail head and the rail bottom. The fixing plate is provided with a plurality of fixing holes corresponding to each coil; each fixing hole is respectively installed with a fixing nail, and the strip-shaped fixing plate is connected with a plurality of coils through a plurality of fixing nails, thereby preventing the coils from being deformed. That is, the deformation caused by the heat radiation of the heated part to the coils and the deformation caused by collision during use are prevented, so as to ensure the stability during the heating process.

[0033] In the above embodiment, preferably, the fixing component 2 is made of an insulating high temperature resistant material, for example, polytetrafluoroethylene, alumina ceramics or silicon oxide ceramics.

[0034] Finally, the electromagnetic induction coil 1 is provided with a number of magnetic conductive sheets 3 corresponding to the rail top and rail waist. The specific number and position of the magnetic conductive sheets 3 can be adjusted and determined through the heating test data. In order to ensure that each part of the rail obtains a similar temperature during the heating process: in addition to meeting the requirements on the coil size, it is also necessary to consider the characteristics of the 60TY1 wing rail, which has a large head area, a thicker waist, and a thin bottom. Therefore, a certain number of magnetic conductive sheets 3 are installed on the top surface of the coil and the thicker parts of the rail waist to constrain the magnetic field of the head and waist of the rail, and better utilize the dense magnetic field to generate a larger induced current, thereby increasing the heating rate of the area, avoiding the problem of excessive temperature difference between the head and bottom of the rail caused by the thin bottom of the rail and the rapid heating, that is, to ensure the uniformity of temperature in various parts of the wing rail.

[0035] When in use: when the 60TY1 wing rail is heated, its position remains fixed; the induction coil attached to the utility model opens to both sides and falls to the set position, so that the 60TY1 rail is placed in the coil, and the distance between the coil and each surface of the rail is ensured to meet the requirements as much as possible, such as Figure 3 As shown; then start the heating program according to the set current and heating time; after the heating time is over, the sensor opens to both sides again, the rail runs to the top head of the top bending machine, and the top bending begins.

[0036] In practice: the completed coil of the utility model is installed on the electromagnetic induction heating device, the inlet and outlet of the copper tube are welded to the connector, and then assembled with the high-frequency induction heating device by bolting for easy disassembly and assembly. When heating the 60TY1 wing rail, different current and time parameters are used to heat the 60TY1 wing rail, and the temperature of each part of the 60TY1 wing rail is measured using a handheld infrared thermometer. The data are shown in Table 1. Among them, the wide side refers to the wider side of the 60TY1 wing rail head, and the narrow side refers to the other side.

[0037] Table 1: Temperature measurement data of various parts of 60TY1 wing rail

[0038]

[0039] From the above description, it can be found that: compared with flame heating, the adoption of the induction heating method of the utility model improves the uniformity of the temperature in the heating area and the internal and external quality, and the temperatures in each area are closer, avoiding overheating or even overburning defects; compared with the resistance wire heating box, the heating efficiency of the 60TY1 wing rail is improved, and the heating time is reduced from about 15 minutes to about 5 minutes.

[0040] The utility model adopts the fixing component 2 made of insulating high temperature resistant material to fix the coils, which can better prevent the deformation of the coils, maintain the inherent size of the coils, ensure the distance between the coils and the wing rails, and improve the temperature stability during the heating process.

[0041] The utility model installs magnetic conductive sheets 3 at the corresponding thicker parts of the rail top and rail waist, and finally increases or decreases the number of magnetic conductive sheets 3 according to the specific thickness of the heated part, so as to balance the temperature of each area of ​​the wing rail heating section and ensure uniform temperature at the bending point of the rail during top bending.

[0042] The utility model sprays high temperature resistant insulating paint evenly on the surface of the manufactured coil to replace the high temperature resistant insulating cloth. The appearance is beautiful and neat, and no cloth scraps fall off during use. Under the premise of ensuring safety, only touch-up operation is required after damage, which improves the efficiency and convenience of repair.

[0043] The utility model is aimed at asymmetric cross-section rails, such as the cross-sections of 60AT1 rails and 60TY1 wing rails after processing, and the like, and the induction coils can be manufactured by the utility model to perform heating top bending.

[0044] In summary, the utility model solves the technical problem of how to design a contoured heating coil for asymmetric section wing rails based on the principle of electromagnetic induction heating so that the heating is fast, efficient and uniform. Designed for a specific asymmetric section rail, it can ensure that parts of the asymmetric section rail at different positions and thicknesses can be heated quickly, efficiently and uniformly, especially ensuring the consistency of heating effects of various parts of the asymmetric rail; it realizes an electromagnetic induction coil design that is easy to control temperature, safe and reliable, has higher heating efficiency, uniform heating and good heating effect.

[0045] Each embodiment in this specification is described in a related manner, and the same or similar parts between the embodiments can be referenced to each other, and each embodiment focuses on the differences from other embodiments.

[0046] The above description is only a preferred embodiment of the present invention and is not intended to limit the protection scope of the present invention. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention are included in the protection scope of the present invention.

Claims

1. A 60TY1 wing rail profiling heating coil, comprising two independent electromagnetic induction coils (1); the electromagnetic induction coils (1) are arranged to imitate the contour of the 60TY1 rail, and when the two independent electromagnetic induction coils (1) are brought close together, a space for accommodating the 60TY1 rail is formed in the center; the characteristics are: The electromagnetic induction coil (1) is an electromagnetic induction coil wound with a copper tube and sprayed with high-temperature resistant insulating paint on the outside; the distance between the inner contour of the coil at the upper and lower surfaces of the rail bottom corresponding to the electromagnetic induction coil (1) and the surface of the rail is greater than the distance between the other inner contours of the coil and the surface of the rail; the electromagnetic induction coil (1) is provided with fixing components (2) for preventing the coil from deforming along the length direction of the rail at the outer vertical end surfaces of the rail head and the rail bottom corresponding to the rail; and the electromagnetic induction coil (1) is provided with a plurality of magnetic conductive sheets (3) at the rail top and rail waist corresponding to the rail.

2. The heating coil according to claim 1, characterized in that: The electromagnetic induction coil (1) is an electromagnetic induction coil wound with a square copper tube.

3. The heating coil according to claim 2, characterized in that: The cross-sectional dimensions of the square copper tube are 10×10×1 mm; a gap of 8 to 12 mm is maintained between adjacent coils; and the span of the entire electromagnetic induction coil (1) is 140 to 160 mm.

4. The heating coil according to claim 1, 2 or 3, characterized in that: During heating operation, the inner contour of the electromagnetic induction coil (1) at the upper and lower surfaces of the rail bottom corresponding to the coil is 30 to 40 mm away from the rail surface; the inner contour of the remaining parts of the electromagnetic induction coil (1) is 10 to 25 mm away from the rail surface.

5. The heating coil according to claim 1, characterized in that: The fixing component (2) is made of insulating high temperature resistant material.