Nano photocatalytic self-cleaning paint coating structure

By introducing photocatalytic decomposition and thermal barrier coatings into the nanocoated structure, combined with antistatic wear-resistant coatings, the problems of single functions and poor waterproofing performance of existing nanocoated coatings are solved, and efficient self-cleaning and pollution prevention are achieved Effects, extend service life and enhance multiple performances.

CN222043054UActive Publication Date: 2024-11-22CHONGQING QINGHUI ENERGY SAVING & ENVIRONMENTAL PROTECTION TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323593848.3
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-27
Publication Date
2024-11-22
Estimated Expiration
2033-12-27

AI Technical Summary

Technical Problem

The existing nanocoated structure has a single function, poor waterproof performance, and is prone to damage due to moisture penetration, affecting its service life, and cannot effectively deal with the problem of glass curtain wall pollution caused by urban pollution.

Method used

Using nanophotocatalytic self-cleaning coating structure, including substrate layer, multiple sets of thermal barrier coatings, photocatalytic decomposition coatings and antistatic wear-resistant coatings, nanotitanium dioxide, platinum particles and nanotitanium phosphate, etc., through Photocatalytic and air catalyst action achieve self-cleaning effect, and prevent diffusion and degradation through thermal barrier coating, increasing service life.

Benefits of technology

It realizes the self-cleaning effect through natural light or water, significantly improves the waterproof, anti-bacterial, anti-pollution and service life of the coating, enhances the functions of anti-corrosion, anti-ultraviolet, heat insulation, crack resistance, etc., and extends the service life of the device. .

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222043054U_ABST
    Figure CN222043054U_ABST
Patent Text Reader

Abstract

The utility model discloses a nanometer photocatalytic self-cleaning paint coating structure, which relates to the technical field of nanometer coatings and comprises a base material layer, a nanometer coating is arranged on the outer surface of the upper portion of the base material layer and comprises a high-adhesion coating, and a plurality of thermal barrier coatings are arranged between the base material layer and the high-adhesion coating. A photocatalytic decomposition coating is arranged on the outer surface of the upper portion of the high-adhesion coating, the photocatalytic decomposition coating comprises a nanometer titanium dioxide layer, a platinum particle layer is arranged on the outer surface of the upper portion of the nanometer titanium dioxide layer, and a nanometer titanium phosphate layer is arranged on the outer surface of the upper portion of the platinum particle layer. According to the nanometer photocatalytic self-cleaning paint coating structure, the nanometer titanium dioxide layer can enable adsorbed pollutants to be subjected to oxidation-reduction decomposition so as to remove and kill surface microbacteria, so that the self-cleaning purpose is achieved, and polluted liquid on the base material layer can be subjected to photocatalytic conversion into non-pollutant liquid through natural light activation catalysis.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of nano coatings, in particular to a nano photocatalytic self-cleaning paint coating structure. Background Art

[0002] At present, with the improvement of human living standards, people have begun to have higher and higher requirements for the comfort and cleanliness of their working and living environment. With the diversification of wall decoration at home and abroad, buildings are decorated with glass curtain walls for beauty and novelty. However, due to more and more pollution emissions, contemporary glass curtain walls have been decorated for a period of time. Due to urban pollution problems, dust, automobile exhaust and other pollutants will float in the air and then adhere to the glass curtain walls, making the originally clean and beautiful outer layer of the glass become black and ugly. In order to protect the glass curtain walls, nano-coatings are often applied on the glass curtain walls.

[0003] The existing nano coating structure is not only complex in structure, but also single in function. Moreover, the waterproof performance of current nano coatings is generally poor. Once moisture penetrates, it is easy to cause damage to the exterior wall or the ground, seriously affecting the service life of the coating and bringing certain adverse effects to people's use process. In order to solve the shortcomings of the existing technology, we propose a nano photocatalytic self-cleaning coating structure. Utility Model Content

[0004] The main purpose of the utility model is to provide a nanometer photocatalytic self-cleaning paint coating structure, which can effectively solve the problems in the background technology.

[0005] In order to achieve the above purpose, the technical solution adopted by the utility model is:

[0006] A nano photocatalytic self-cleaning paint coating structure comprises a substrate layer, wherein the substrate layer is provided with multiple groups, a mounting block is provided on the left outer surface of the substrate layer, a user mounting groove is provided on the right outer surface of the substrate layer, the mounting block is located inside the mounting groove, a nano coating is provided on the upper outer surface of the substrate layer, the nano coating comprises a high adhesion coating, the high adhesion coating is located on the upper outer surface of the substrate layer, multiple groups of thermal barrier coatings are provided between the substrate layer and the high adhesion coating, a photocatalytic decomposition coating is provided on the upper outer surface of the high adhesion coating, the photocatalytic decomposition coating comprises a nano titanium dioxide layer, a platinum particle layer is provided on the upper outer surface of the nano titanium dioxide layer, a nano titanium phosphate layer is provided on the upper outer surface of the platinum particle layer, and an antistatic wear-resistant coating is provided on the upper outer surface of the photocatalytic decomposition coating.

[0007] Preferably, the upper outer surface of the antistatic wear-resistant coating is provided with a base layer, the upper outer surface of the base layer is provided with a nano-inorganic non-stick water-based paint layer, the upper outer surface of the nano-inorganic non-stick water-based paint layer is provided with a thermal insulation layer, the upper outer surface of the thermal insulation layer is provided with an epoxy resin coating, the upper outer surface of the epoxy resin coating is provided with a nano-acrylic polymer layer, the upper outer surface of the nano-acrylic polymer layer is provided with an anti-cracking putty coating, the upper outer surface of the anti-cracking putty coating is provided with a silane waterproof coating, and the upper outer surface of the silane waterproof coating is provided with an exterior wall transparent waterproof coating.

[0008] Preferably, the two groups of substrate layers are plug-connected to each other via mounting blocks.

[0009] Preferably, the high adhesion coating, the photocatalytic decomposition coating, and the antistatic wear-resistant coating are glued and connected to each other to form an integrated structure.

[0010] Preferably, the high adhesion coating is distributed in parallel and equidistantly between the substrate layer and the high adhesion coating.

[0011] Preferably, the nano inorganic water-resistant coating layer is located inside the base layer.

[0012] Beneficial Effects

[0013] Compared with the prior art, the utility model has the following beneficial effects:

[0014] 1. In the utility model, photocatalytic self-cleaning is performed by setting a photocatalytic decomposition coating, and the photocatalytic decomposition coating includes a nano titanium phosphate layer, a nano titanium dioxide layer, and a platinum particle layer, wherein the nano titanium dioxide layer is a photocatalyst, which can absorb light of a certain wavelength, generate free electrons and holes, so that pollutants adsorbed on the surface of the membrane undergo redox decomposition and are removed and the surface microbes are killed, thereby achieving the purpose of self-cleaning, and the nano titanium phosphate layer is an air catalyst, which can exert a self-cleaning effect by using only water in the absence of light, wherein the platinum particle layer and the nano titanium dioxide layer are alternately arranged, so that the platinum particle layer is incorporated into the nano titanium dioxide layer, so that the decomposition ability of the nano titanium dioxide layer can be increased by about fifty times, so that the polluted liquid on the substrate layer can be photocatalytically converted into a pollutant-free liquid by activating catalysis through natural light.

[0015] 2. The thermal barrier coating provided in the utility model prevents degradation caused by mutual diffusion between the high adhesion coating and the substrate layer. The thermal barrier coating is provided in parallel and equidistantly between the substrate layer and the high adhesion coating, and a diffusion barrier is provided between the two to avoid mutual diffusion between the high adhesion coating and the substrate layer and cause degradation, thereby increasing the service life of the device. The antistatic and wear-resistant coating can reduce the adhesion of dust. The base layer is a component made of polyurethane prepolymer material. The coating solidifies after contacting with moisture in the air, and a seamless integral waterproof film is formed on the surface of the base layer. The thermal insulation layer plays a role of thermal insulation. The device is provided with a variety of coatings, so that the nano coating has the functions of anti-corrosion, waterproof, anti-bacteria, anti-ultraviolet, heat insulation, anti-cracking, high hydrophobicity, flame retardancy, impact resistance, self-cleaning and anti-pollution, pressure resistance, antifreeze, breathability, wear resistance, etc., thereby increasing the service life of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 It is a schematic diagram of the overall structure of the utility model;

[0017] Figure 2 It is a schematic diagram of the structure of the thermal barrier coating of the utility model;

[0018] Figure 3 It is a schematic structural diagram of the nano coating of the utility model;

[0019] Figure 4 It is a structural schematic diagram of the photocatalytic decomposition coating of the utility model.

[0020] In the figure: 1. substrate layer; 2. high adhesion coating; 3. thermal barrier coating; 4. photocatalytic decomposition coating; 5. antistatic wear-resistant coating; 6. nano titanium phosphate layer; 7. nano titanium dioxide layer; 8. platinum particle layer; 9. base layer; 10. nano inorganic non-stick water-based paint layer; 11. thermal insulation layer; 12. epoxy resin coating; 13. nano acrylic polymer layer; 14. anti-cracking putty coating; 15. silane waterproof coating; 16. exterior wall transparent waterproof coating; 17. mounting block; 18. mounting groove; 19. nano coating. DETAILED DESCRIPTION

[0021] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further described below in conjunction with specific implementation methods.

[0022] Embodiment 1, as Figure 1-4As shown, a nano photocatalytic self-cleaning paint coating structure is provided. When in use, a photocatalytic decomposition coating 4 is arranged on a high adhesion coating 2. The photocatalytic decomposition coating 4 includes a nano titanium phosphate layer 6, a nano titanium dioxide layer 7, and a platinum particle layer 8. The nano titanium dioxide layer 7 can photocatalytically convert the contaminated liquid on the substrate layer 1 into a pollutant-free liquid through natural light, wherein the platinum particle layer 8 can accelerate the conversion speed of the nano titanium dioxide layer 7 and improve the working efficiency. The nano titanium phosphate layer 6 is an air catalyst and can exert a self-cleaning effect even when using only water without light.

[0023] Embodiment 2, as Figure 1-4 As shown, a nano photocatalytic self-cleaning coating structure is provided. The two groups of substrate layers 1 are connected and installed by inserting the mounting block 17 of one group of substrate layers 1 into the mounting groove 18 of another group of substrate layers 1. The nano coating 19 includes a high adhesion coating 2. A thermal barrier coating 3 is arranged parallel and equidistantly between the high adhesion coating 2 and the substrate layer 1. The thermal barrier coating 3 can add a diffusion barrier between the two to avoid mutual diffusion between the high adhesion coating 2 and the substrate layer 1 and cause degradation, thereby increasing the service life of the device. The antistatic wear-resistant coating 5 can reduce dust adhesion. A nano inorganic non-wetting water-resistant coating layer 10 is arranged in the base layer 9, which can form a waterproof film on the base layer 9. The thermal insulation layer 11 plays a role of thermal insulation, thereby improving the density and smoothness of the nano coating 19, making the nano coating 19 finer and more beautiful, while improving the coating quality and effect of the coating, and increasing the service life of the nano coating 19.

[0024] How it works

[0025] It should be noted that the utility model is a nano-photocatalytic self-cleaning coating structure. When in use, the connection and installation of the two groups of substrate layers 1 are completed by inserting the mounting block 17 of one group of substrate layers 1 into the mounting groove 18 of another group of substrate layers 1. The nano-coating 19 includes a high-adhesion coating 2, and a thermal barrier coating 3 is arranged parallel and equidistantly between the high-adhesion coating 2 and the substrate layer 1. The thermal barrier coating 3 can add a diffusion barrier between the two to avoid mutual diffusion between the high-adhesion coating 2 and the substrate layer 1 and cause degradation, thereby increasing the service life of the device. A photocatalytic decomposition coating 4 is arranged on the high-adhesion coating 2, and the photocatalytic decomposition coating 4 includes a nano-titanium phosphate layer 6, a nano-titanium dioxide layer 7, and a platinum particle layer 8. The nano-titanium dioxide layer 7 can photocatalytically convert the contaminated liquid on the substrate layer 1 into a pollutant-free liquid through natural light, wherein the platinum particle layer 8 can accelerate the conversion speed of the nano-titanium dioxide layer 7 and improve work efficiency. The nano-titanium phosphate layer 6 is an air catalyst and can exert a self-cleaning effect even when only water is used in the absence of light.

[0026] The above shows and describes the basic principle and main features of the utility model and the advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection claimed by the utility model is defined by the attached claims and their equivalents.

Claims

1. A nano-photocatalytic self-cleaning coating structure, comprising a substrate layer (1), characterized in that: The substrate layer (1) is provided with a plurality of groups. A mounting block (17) is provided on the left outer surface of the substrate layer (1). A user mounting groove (18) is provided on the right outer surface of the substrate layer (1). The mounting block (17) is located inside the mounting groove (18). A nano coating (19) is provided on the upper outer surface of the substrate layer (1). The nano coating (19) comprises a high adhesion coating (2). The high adhesion coating (2) is located on the upper outer surface of the substrate layer (1). A plurality of groups of thermal barrier coatings (3) are provided between the substrate layer (1) and the high adhesion coating (2). A photocatalytic decomposition coating (4) is provided on the upper outer surface of the high adhesion coating (2). The photocatalytic decomposition coating (4) comprises a nano titanium dioxide layer (7). A platinum particle layer (8) is provided on the upper outer surface of the nano titanium dioxide layer (7). A nano titanium phosphate layer (6) is provided on the upper outer surface of the platinum particle layer (8). An antistatic wear-resistant coating (5) is provided on the upper outer surface of the photocatalytic decomposition coating (4).

2. The nano-photocatalytic self-cleaning coating structure according to claim 1, characterized in that: The upper outer surface of the antistatic wear-resistant coating (5) is provided with a base layer (9), the upper outer surface of the base layer (9) is provided with a nano inorganic non-stick water-based paint layer (10), the upper outer surface of the nano inorganic non-stick water-based paint layer (10) is provided with a thermal insulation layer (11), the upper outer surface of the thermal insulation layer (11) is provided with an epoxy resin coating (12), the upper outer surface of the epoxy resin coating (12) is provided with a nano acrylic polymer layer (13), the upper outer surface of the nano acrylic polymer layer (13) is provided with an anti-cracking putty coating (14), the upper outer surface of the anti-cracking putty coating (14) is provided with a silane waterproof coating (15), and the upper outer surface of the silane waterproof coating (15) is provided with an exterior wall transparent waterproof coating (16).

3. The nano-photocatalytic self-cleaning coating structure according to claim 1 is characterized by: The two groups of substrate layers (1) are plug-connected to each other via a mounting block (17).

4. The nano-photocatalytic self-cleaning coating structure according to claim 1, characterized in that: The high adhesion coating (2), the photocatalytic decomposition coating (4), and the antistatic wear-resistant coating (5) are glued and connected to each other to form an integrated structure.

5. The nano-photocatalytic self-cleaning coating structure according to claim 1, characterized in that: The high adhesion coating (2) is distributed in parallel and equidistantly between the substrate layer (1) and the high adhesion coating (2).

6. The nano-photocatalytic self-cleaning coating structure according to claim 2, characterized in that: The nano inorganic water-resistant coating layer (10) is located inside the base layer (9).