Preparation system of magnesium oxide
By designing a magnesium oxide preparation system, the environmental pollution and resource waste caused by improper handling of refined magnesium slag have been solved, realizing the preparation and recycling of high-purity magnesium oxide, which can be applied in the fields of medicine, rubber, plastics, and dyes.
Patent Information
- Application Number
- CN202420801865.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-17
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-04-17
AI Technical Summary
In the current technology, the treatment method for refined magnesium slag is direct dumping and landfilling, which leads to environmental pollution and resource waste, and there is a lack of effective utilization methods.
A magnesium oxide preparation system was designed, including a mixing reaction module, a filtration and separation module, a mixing and evaporation module, and a high-temperature calcination module. The system reacts with a mixed refined magnesium slag and an extractant, separates and evaporates the slag to obtain magnesium hydroxide, and then calcines it at a high temperature to obtain magnesium oxide.
It has enabled the preparation of high-purity magnesium hydroxide and magnesium oxide, reducing waste emissions, recycling resources, meeting the requirements of sustainable development, and can be applied in the fields of medicine, rubber, plastics, and dyes.
Smart Images

Figure CN222064125U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of industrial manufacturing, and specifically relates to a magnesium oxide preparation system. Background Art
[0002] Refined magnesium slag is a solid waste generated in the process of refining magnesium. In order to produce high-purity magnesium ingots, crude magnesium must be refined and purified. Due to the addition of different fluxes during the purification process, a large amount of refined magnesium slag will be produced in this process, and most companies in my country directly dump and landfill the refined magnesium slag. With the rapid development of the magnesium metallurgical industry, China has become a major magnesium producer and exporter in the world. There are many technologies for magnesium smelting, which can be divided into two categories: silicothermic method and electrolytic method. The production process of 20,000 t / a of metallic magnesium produces 130,000 t / a of reduced slag and 7,100 t / a of refined slag. Reduced slag can be used in cement, building materials, sulfur fixation, etc., and there are many research reports on it, while there are fewer studies on the composition and application of refined slag. These refined magnesium slags are mainly composed of chlorides, oxides, silicates and other impurities. Because they contain harmful substances such as heavy metals and radioactive substances, refined magnesium slag needs to be properly handled to prevent environmental pollution. Therefore, it is crucial to find an effective way to utilize refined magnesium slag. Therefore, this application proposes an efficient and economical process method, which uses low-cost refined magnesium slag as the main raw material to prepare high-purity magnesium hydroxide or magnesium oxide, which has extremely high industrial value. Utility Model Content
[0003] In order to solve the above problems, effectively utilize refined magnesium slag, reduce waste emissions, and achieve effective recycling of resources, the present application provides a magnesium oxide preparation system, and the specific technical solution is as follows:
[0004] A system for preparing magnesium oxide, comprising:
[0005] The mixing reaction module includes a batching bin, a vibrating feeder, a batcher 1, a mixed slurry bin, a slurry delivery pump, a reactor 1, a hydrochloric acid collection tank, a sorting device and a condenser 1, and is used to mix the refined magnesium slag and the extractant to fully react;
[0006] A filtration and separation module, including a molecular membrane filter, is used to filter and separate the material obtained after the above reaction to obtain a mixed solution;
[0007] The mixed evaporation module includes a second reaction kettle, a second batcher, an evaporator, a second condenser and a magnesium hydroxide collection bin, and is used to obtain magnesium hydroxide by evaporating the mixed catalyst and the mixed solution after the reaction;
[0008] The high-temperature calcination module comprises a high-temperature combustion chamber, a magnesium hydroxide finished product silo and a magnesium oxide finished product silo, and is used for high-temperature calcining of magnesium hydroxide to obtain magnesium oxide.
[0009] Preferably, the batching bin comprises a refined magnesium slag batching bin, an extractant batching bin and a catalyst batching bin, wherein the refined magnesium slag batching bin is used to hold crushed refined magnesium slag particles, the extractant batching bin is used to hold the extractant, and the catalyst batching bin is used to hold the catalyst;
[0010] The refined magnesium slag batching bin is connected to the mixed slurry bin inlet through the vibrating feeder, the extractant batching bin is connected to the mixed slurry bin inlet through the batcher 1, and the catalyst batching bin is connected to the reactor 2 inlet through the batcher 2.
[0011] Preferably, the mixed slurry bin is acid-resistant to prevent the container from being corroded or damaged by acidic substances, and the outlet of the mixed slurry bin is connected to the slurry delivery pump, and the outlet of the slurry delivery pump is connected to the inlet of reactor one. Reactor one is provided with three discharge ports, which are respectively a gas discharge port, a solid discharge port and a liquid discharge port.
[0012] Preferably, the reactor is provided with a stirring blade, and the stirring blade is provided with a magnetic block for absorbing powdered metal in the material. The reactor is provided with a jacket layer, and the jacket layer is equipped with a thermocouple heating rod and heat-conducting oil for heating at any time according to the material conditions, and the reactor is also acid-resistant.
[0013] Preferably, the gas outlet of the reactor one is connected to the inlet of the hydrochloric acid collecting tank, the solid outlet of the reactor one is connected to the inlet of the sorting equipment, the sorting equipment is provided with a discharge port and a discharge port, and the liquid outlet of the reactor one is connected to the inlet of the condenser one.
[0014] Preferably, the outlet of the condenser 1 is connected to the inlet of the molecular membrane filter, the outlet of the molecular membrane filter is connected to the inlet 1 of the reactor 2, and the catalyst batching bin is connected to the inlet 2 of the reactor 2.
[0015] Preferably, the evaporator comprises two discharge ports, the first discharge port of the evaporator is connected to the inlet of the second condenser, the second discharge port of the condenser is connected to the inlet of the extractant batching bin, and the second discharge port of the evaporator is connected to the inlet of the magnesium hydroxide collection bin.
[0016] Preferably, the magnesium hydroxide collecting bin comprises two discharge ports, discharge port 1 of the magnesium hydroxide collecting bin is connected to the magnesium hydroxide finished product bin, discharge port 2 of the magnesium hydroxide collecting bin is connected to the inlet of the high-temperature combustion chamber, the discharge port of the high-temperature combustion chamber is connected to the inlet of the magnesium oxide finished product bin, and the outlet of the magnesium hydroxide finished product bin and the outlet of the magnesium oxide finished product bin are each provided with a discharge valve.
[0017] Compared with the prior art, the utility model has the following beneficial effects: high-purity magnesium hydroxide and magnesium oxide can be prepared, which are widely used in the fields of medicine, rubber, plastics, dyes, etc., and are important raw materials in various industrial processes and daily production and life; the utilization of refined magnesium slag helps to reduce waste emissions and achieve effective recycling of resources. Compared with the existing preparation technology, the utility model is more environmentally friendly and meets the requirements of sustainable development; and the utility model adopts a unique process route or innovative technology to make the production process more efficient and stable. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 The utility model is a process flow chart of a magnesium oxide preparation system. DETAILED DESCRIPTION
[0019] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments of the utility model, all other embodiments obtained by ordinary persons in the field without creative work are within the scope of protection of the utility model.
[0020] As shown in the figure, the utility model provides a system for preparing magnesium oxide, comprising:
[0021] The mixing reaction module includes a batching bin, a vibrating feeder, a batcher 1, a mixed slurry bin, a slurry delivery pump, a reactor 1, a hydrochloric acid collection tank, a sorting device and a condenser 1, and is used to mix the refined magnesium slag and the extractant to fully react;
[0022] A filtration and separation module, including a molecular membrane filter, is used to filter and separate the material obtained after the above reaction to obtain a mixed solution;
[0023] The mixed evaporation module includes a second reaction kettle, a second batcher, an evaporator, a second condenser and a magnesium hydroxide collection bin, and is used to obtain magnesium hydroxide by evaporating the mixed catalyst and the mixed solution after the reaction;
[0024] The high-temperature calcination module comprises a high-temperature combustion chamber, a magnesium hydroxide finished product silo and a magnesium oxide finished product silo, and is used for high-temperature calcining of magnesium hydroxide to obtain magnesium oxide.
[0025] The batching bin comprises a refined magnesium slag batching bin, an extractant batching bin and a catalyst batching bin. The refined magnesium slag batching bin is used to hold crushed refined magnesium slag particles, the extractant batching bin is used to hold the extractant, and the catalyst batching bin is used to hold the catalyst. The refined magnesium slag batching bin is connected to the entrance of the mixed slurry bin through a vibrating feeder, the extractant batching bin is connected to the entrance of the mixed slurry bin through the batcher one, and the catalyst batching bin is connected to the entrance of the reactor two through the batcher two.
[0026] The mixed slurry bin is acid-resistant to prevent the container from being corroded or damaged by acidic substances, and the outlet of the mixed slurry bin is connected to the slurry delivery pump, and the outlet of the slurry delivery pump is connected to the inlet of the reactor. The reactor is provided with three discharge ports, namely, a gas discharge port, a solid discharge port and a liquid discharge port.
[0027] The reactor is provided with a stirring blade, on which a metal magnetic block for absorbing powder in the material is provided. The reactor is provided with a jacket layer, in which a thermocouple heating rod and heat-conducting oil are installed, for heating at any time according to the material conditions. The reactor is also acid-resistant.
[0028] The gas outlet of reactor one is connected to the inlet of the hydrochloric acid collecting tank, the solid outlet of reactor one is connected to the inlet of the sorting equipment, the sorting equipment is provided with a discharge port and a discharge port, and the liquid outlet of reactor one is connected to the inlet of condenser one.
[0029] The discharge port of the first condenser is connected to the feed port of the molecular membrane filter, the discharge port of the molecular membrane filter is connected to the first feed port of the second reactor, and the catalyst batching bin is connected to the second feed port of the second reactor.
[0030] The evaporator comprises two discharge ports, the first discharge port of the evaporator is connected to the inlet of the second condenser, the second discharge port of the condenser is connected to the inlet of the extractant batching bin, and the second discharge port of the evaporator is connected to the inlet of the magnesium hydroxide collection bin.
[0031] The magnesium hydroxide collecting bin includes two discharge ports, wherein the first discharge port of the magnesium hydroxide collecting bin is connected to the magnesium hydroxide finished product bin, the second discharge port of the magnesium hydroxide collecting bin is connected to the inlet of the high-temperature combustion chamber, the discharge port of the high-temperature combustion chamber is connected to the inlet of the magnesium oxide finished product bin, and the outlet of the magnesium hydroxide finished product bin and the outlet of the magnesium oxide finished product bin are each provided with a discharge valve.
[0032] First, add the crushed refined magnesium slag into the refined magnesium slag batching bin, add the extractant into the extractant batching bin, add the catalyst into the catalyst batching bin, start the vibrating feeder 1 and the batcher 1, and send the refined magnesium slag and the extractant to the mixed slurry bin for mixing through the vibrating feeder 1 and the batcher 1. The mixed slurry bin is stirred to mix the materials. The mixed materials enter the slurry delivery pump, and the slurry delivery pump delivers the materials to the reactor 1 to react in the reactor 1. The gaseous materials after the reaction enter the hydrochloric acid collection tank, the solid materials enter the sorting equipment, and the liquid materials enter the condenser 1. After the solid materials enter the sorting equipment, two materials are separated, one is magnesium powder and the other is waste slag.
[0033] The liquid material entering condenser one is cooled, and when the temperature drops to a certain temperature, it enters the molecular membrane filter, where it is filtered and separated to intercept large molecular organic matter, particulate matter, etc. The high-purity mixed solution passing through the molecular membrane enters reactor two.
[0034] After the filtered high-purity mixed solution enters the reactor 2, the catalyst in the catalyst batching bin is added to the reactor 2 in a certain proportion, and the two are mixed and then the reactor 2 is started to react in the reactor 2. The reacted material enters the evaporator. After the evaporator is started to evaporate completely, the obtained gaseous substance passes through the condenser 2 and enters the extractant batching bin for recycling. The solid substance left is the high-purity magnesium hydroxide. If it is decided to end the process, the high-purity magnesium hydroxide enters the magnesium hydroxide finished product bin through the magnesium hydroxide collection bin.
[0035] If it is decided to continue to prepare high-purity magnesium oxide, the high-purity magnesium hydroxide entering the magnesium hydroxide collection bin will be calcined in a high-temperature combustion chamber without oxygen to generate high-purity magnesium oxide, which will then enter the magnesium oxide finished product bin.
[0036] It is to be understood that the preferred embodiments of the utility model disclosed above are only used to illustrate the utility model. The preferred embodiments do not describe all the details in detail, nor do they limit the utility model to the specific implementation methods described. Obviously, many modifications and changes can be made according to the content of this specification. This specification selects and specifically describes these embodiments in order to better explain the principles and practical applications of the utility model, so that those skilled in the art can understand and use the utility model well. The utility model is limited only by the claims and their full scope and equivalents.
Claims
1. A system for preparing magnesium oxide, characterized in that: include: The mixing reaction module includes a batching bin, a vibrating feeder, a batcher 1, a mixed slurry bin, a slurry delivery pump, a reactor 1, a hydrochloric acid collection tank, a sorting device and a condenser 1, and is used to mix the refined magnesium slag and the extractant to fully react; A filtration and separation module, including a molecular membrane filter, is used to filter and separate the material obtained after the above reaction to obtain a mixed solution; The mixed evaporation module includes a second reaction kettle, a second batcher, an evaporator, a second condenser and a magnesium hydroxide collection bin, and is used to obtain magnesium hydroxide by evaporating the mixed catalyst and the mixed solution after the reaction; The high-temperature calcination module includes a high-temperature combustion chamber, a magnesium hydroxide finished product silo and a magnesium oxide finished product silo, and is used for high-temperature calcining magnesium hydroxide in a temperature range of 700° C. to 1000° C. to obtain magnesium oxide.
2. A system for preparing magnesium oxide according to claim 1, characterized in that: The batching bin comprises a refined magnesium slag batching bin, an extractant batching bin and a catalyst batching bin, wherein the refined magnesium slag batching bin is used to hold crushed refined magnesium slag particles, the extractant batching bin is used to hold the extractant, and the catalyst batching bin is used to hold the catalyst; The refined magnesium slag batching bin is connected to the mixed slurry bin inlet through the vibrating feeder, the extractant batching bin is connected to the mixed slurry bin inlet through the batcher 1, and the catalyst batching bin is connected to the reactor 2 inlet through the batcher 2.
3. A system for preparing magnesium oxide according to claim 1, characterized in that: The mixed slurry bin is acid-resistant to prevent the container from being corroded or damaged by acidic substances, and the outlet of the mixed slurry bin is connected to the slurry delivery pump, and the outlet of the slurry delivery pump is connected to the inlet of the reactor. The reactor is provided with three discharge ports, which are respectively a gas discharge port, a solid discharge port and a liquid discharge port.
4. A system for preparing magnesium oxide according to claim 3, characterized in that: The reactor is provided with a stirring blade, on which a magnetic block for absorbing powdered metal in the material is disposed. The reactor is provided with a jacket layer, in which a thermocouple heating rod and heat-conducting oil are installed for heating at any time according to the material conditions. The reactor is also acid-resistant.
5. A system for preparing magnesium oxide according to claim 1 or 3, characterized in that: The gas outlet of the reactor one is connected to the inlet of the hydrochloric acid collecting tank, the solid outlet of the reactor one is connected to the inlet of the sorting equipment, the sorting equipment is provided with a discharge port and a discharge port, and the liquid outlet of the reactor one is connected to the inlet of the condenser one.
6. A system for preparing magnesium oxide according to claim 1, characterized in that: The discharge port of the condenser 1 is connected to the feed port of the molecular membrane filter, the discharge port of the molecular membrane filter is connected to the feed port 1 of the reactor 2, and the catalyst batching bin is connected to the feed port 2 of the reactor 2.
7. A system for preparing magnesium oxide according to claim 1, characterized in that: The evaporator comprises two discharge ports, the first discharge port of the evaporator is connected to the inlet of the second condenser, the second discharge port of the condenser is connected to the inlet of the extractant batching bin, and the second discharge port of the evaporator is connected to the inlet of the magnesium hydroxide collection bin.
8. A system for preparing magnesium oxide according to claim 1, characterized in that: The magnesium hydroxide collecting bin comprises two discharge ports, wherein the first discharge port of the magnesium hydroxide collecting bin is connected to the magnesium hydroxide finished product bin, the second discharge port of the magnesium hydroxide collecting bin is connected to the inlet of the high-temperature combustion chamber, the discharge port of the high-temperature combustion chamber is connected to the inlet of the magnesium oxide finished product bin, and the outlet of the magnesium hydroxide finished product bin and the outlet of the magnesium oxide finished product bin are each provided with a discharge valve.