Metal expansion joint of boiler return feeder
By using shale ceramic filler and refractory casting layer to protect the corrugated pipe in the metal expansion joint of the boiler recharger, the heat leakage and corrosion problems caused by the aging of high-temperature elastic blocks are solved, reducing the risk of accidents and extending the service life.
Patent Information
- Application Number
- CN202420216880.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-26
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2034-01-26
AI Technical Summary
The high-temperature elastic blocks of metal expansion joints in existing boilers are prone to aging and falling off, resulting in heat leakage and corrosion, increasing the risk of accidents, and short service life.
The corrugated pipe is equipped with an intermediate pipe and an inner pipe to fill shale ceramic filler, and a refractory casting layer and retaining ring are installed therebetween, and an insulation sheath is added to prevent hot air flow and materials from contacting, reducing temperature and corrosion risks.
Effectively reduce the chance of accidents, extend the service life of metal expansion joints, protect the corrugated pipes through high-temperature, heat insulation and corrosion-resistant ceramic fillers and refractory casting layers, reducing temperature and preventing corrosion.
Smart Images

Figure CN222067928U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the field of boiler returners, in particular to a metal expansion joint of a boiler returner. Background Art
[0002] In existing boilers, there is a plug-in structure between the furnace and the returner, which is mainly to adapt to the distance change caused by thermal expansion and contraction. In order to prevent the material from leaking at the plug-in point, a metal expansion joint is also arranged between the furnace and the returner. For example, in the furnace and returner connection structure of the coal-fired boiler with application number 201822100901.4, the metal expansion joint is a bellows type, which seals the plug-in point between the furnace and the returner, while maintaining its own elasticity and having a certain expansion margin.
[0003] The plug-in structure between the furnace and the returner includes a lower plug-in tube located at the top of the furnace and an upper plug-in tube located at the bottom of the feeder. The upper plug-in tube is inserted into the lower plug-in tube. In order to reduce the rigid stress caused by thermal deformation, the gap between the upper and lower plug-ins is matched, and the gap between the upper and lower plug-ins is filled by a high-temperature resistant elastic block. However, it is found in actual use that the material passing between the upper and lower plug-ins can reach 1000°C. Under the limitation of existing material technology, the heat-resistant temperature of the high-temperature resistant elastic block is insufficient, and it is easy to age into fragments and fall off. The gap between the upper and lower plug-ins is exposed, and heat quickly leaks from the gap, causing the temperature of the metal expansion joint to rise rapidly. The metal expansion joint may even burn red, which is prone to fire, scalding and other accidents. In addition, the material entering the furnace from the returner is corrosive. After the high-temperature resistant elastic block falls off, the material will pass through the gap and adhere to the metal expansion joint, causing the metal expansion joint to corrode and break, resulting in a more dangerous hot gas leakage accident. Utility Model Content
[0004] The utility model aims to provide a boiler return feeder metal expansion joint, which has the advantages of reducing the probability of accidents and having a long service life.
[0005] The technical solution of the utility model is: a metal expansion joint of a boiler returner, comprising a bellows made of metal material, an upper ring plate is provided on the inner side of the upper end of the bellows, a middle tube extending downward is provided on the inner side of the upper ring plate, a lower ring plate is provided on the inner side of the lower end of the bellows, an inner tube extending upward is provided on the inner side of the lower ring plate, a granular filler is provided between the inner tube and the bellows, and the lower end of the middle tube is inserted into the filler.
[0006] In the aforementioned boiler returner metal expansion joint, a first refractory casting layer is provided on the inner circumferential surface of the intermediate tube.
[0007] In the aforementioned boiler return feeder metal expansion joint, a second refractory casting layer is provided on both the inner and outer peripheral surfaces of the inner tube.
[0008] In the aforementioned boiler return feeder metal expansion joint, the filler is shale ceramsite, and a retaining ring made of a high-density material is provided on the top surface of the filler, and the retaining ring is located between the middle tube and the inner tube.
[0009] In the aforementioned boiler return feeder metal expansion joint, a sheath made of heat insulating material is provided on the outer side of the bellows, and the upper end of the sheath is fixed to the upper ring plate.
[0010] In the aforementioned boiler returner metal expansion joint, a plurality of heat dissipation holes are provided on the sheath.
[0011] Compared with the prior art, the utility model arranges an intermediate tube and an inner tube on the inner side of the bellows, the intermediate tube is fixed to the upper end of the bellows, and the inner tube is fixed to the lower end of the bellows, the intermediate tube and the inner tube can freely move axially with the expansion and contraction of the bellows without causing interference, and a granular filler is arranged between the inner tube and the bellows to fill the gap between the intermediate tube and the lower ring plate, blocking the path of materials and hot air flow directly reaching the bellows, preventing the bellows from corrosion and excessive temperature, and reducing the probability of accidents.
[0012] Furthermore, by providing a refractory casting layer on the surfaces of the intermediate tube and the inner tube that may contact the material for protection, the service life of the metal expansion joint is effectively extended.
[0013] The filler is preferably shale ceramsite, which has the characteristics of high temperature resistance, corrosion resistance, good heat insulation effect and light weight. The characteristics of high temperature resistance and corrosion resistance make the filler not easy to pulverize and fail in high temperature and corrosive environment, and have a long service life. The good heat insulation effect reduces the speed of heat transfer from the return feeder to the bellows, further reducing the temperature of the bellows. The light weight increases the fluidity of the filler, reduces the resistance of the bellows when it expands and contracts, and effectively protects the bellows and prevents it from cracking.
[0014] In summary, the utility model has the advantages of reducing the probability of accidents and having a long service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 It is a structural schematic diagram of the utility model.
[0016] Figure 2 It is an installation schematic diagram of the utility model.
[0017] The markings in the accompanying drawings are: 1- bellows, 2- upper ring plate, 3- middle tube, 4- lower ring plate, 5- inner tube, 6- first refractory casting layer, 7- second refractory casting layer, 8- filler, 9- retaining ring, 10- jacket, 11- returner, 12- boiler, 13- upper insert tube, 14- lower insert tube, 15- high temperature resistant elastic block. DETAILED DESCRIPTION
[0018] The present invention is further described below in conjunction with the accompanying drawings and embodiments, but they are not intended to limit the present invention.
[0019] Embodiment. A metal expansion joint for a boiler return feeder, such as Figure 1 As shown, it includes a bellows 1 made of metal material, and an upper ring plate 2 is welded to the inner side of the upper end of the bellows 1.
[0020] An intermediate pipe 3 extending downward is welded to the inner side of the upper ring plate 2 , and a first refractory casting layer 6 is provided on the inner circumference of the intermediate pipe 3 .
[0021] A lower ring plate 4 is welded to the inner side of the lower end of the corrugated tube 1 . An inner tube 5 extending upward is arranged on the inner side of the lower ring plate 4 . A second refractory casting layer 7 is arranged on the inner and outer circumferential surfaces of the inner tube 5 .
[0022] A granular filler 8 is provided between the inner tube 5 and the corrugated tube 1. The filler 8 is shale ceramsite with a diameter of 3-5 mm and a bulk density of 500 kg / m 3 About, the density is small, it has good thermal insulation and corrosion resistance, and the refractoriness can reach above 1200°C. The lower end of the intermediate tube 3 is inserted into the filler 8.
[0023] A steel retaining ring 9 is provided on the top surface of the filler 8. The retaining ring 9 has a thickness of 1 cm and is placed between the middle tube 3 and the inner tube 5 with a clearance fit. The width of the gap left should be smaller than the diameter of the shale ceramsite.
[0024] The outer side of the bellows 1 is provided with a sheath 10 made of asbestos cloth, the upper end of the sheath 10 is fixed to the upper ring plate 2, and the lower end of the sheath 10 is free and lower than the lower ring plate 4. The outer peripheral surface of the sheath 10 is densely covered with a plurality of heat dissipation holes, the thickness of the sheath 10 is 5 mm, and the heat dissipation holes are through holes with a diameter of 3 mm.
[0025] like Figure 2 As shown, when the metal expansion joint is installed, the upper ring plate 2 is fixed to the bottom of the returner 11, the lower ring plate 4 is fixed to the top of the boiler 12, and a gap is formed between the inner tube 5 and the lower insert tube 14 to cope with the thermal deformation margin. When the high temperature resistant elastic block 15 between the upper insert tube 13 and the lower insert tube 14 fails, the material passes through the gap between the upper insert tube 13 and the lower insert tube 14, but is blocked by the middle tube 3, the inner tube 5 and the filler 8 and cannot contact the bellows 1, thereby preventing the bellows 1 from being corroded and damaged. At the same time, the heat is also blocked to prevent the bellows 1 from being overheated. The sheath 10 further prevents the heat of the bellows 1 from being dissipated to the outside, thereby reducing accidents such as burns and fires.
[0026] Due to thermal expansion and contraction, when the distance between the return device 11 and the boiler 12 changes, the bellows 1 expands and contracts accordingly. Since the filler is composed of granular material, the insertion depth of the intermediate tube 3 in the filler changes accordingly.
[0027] Since there is a relatively high-speed airflow between the return device 11 and the boiler 12, a certain vacuum effect will be formed in the bellows 1. The density of shale ceramsite is small and it may be brought into the boiler 12 by the airflow. Therefore, a heavier retaining ring 9 is provided on the filler 8 to apply a load to the shale ceramsite to prevent it from being carried away by the airflow.
[0028] The inner side of the middle tube 3 will contact the material. To prevent the middle tube 3 from being corroded, a first refractory casting layer 6 is provided on the inner side of the middle tube 3. In the same principle, a second refractory casting layer 7 is provided on both the inner and outer peripheral surfaces of the inner tube 5.
Claims
1. A metal expansion joint for a boiler return feeder. Features: The invention comprises a bellows (1) made of metal material, wherein an upper ring plate (2) is provided on the inner side of the upper end of the bellows (1), an intermediate tube (3) extending downward is provided on the inner side of the upper ring plate (2), a lower ring plate (4) is provided on the inner side of the lower end of the bellows (1), an inner tube (5) extending upward is provided on the inner side of the lower ring plate (4), a granular filler (8) is provided between the inner tube (5) and the bellows (1), and the lower end of the intermediate tube (3) is inserted into the filler (8).
2. The boiler return feeder metal expansion joint according to claim 1, Features: A first refractory casting layer (6) is provided on the inner circumferential surface of the intermediate tube (3).
3. The boiler return feeder metal expansion joint according to claim 1, Features: A second refractory casting layer (7) is provided on both the inner and outer circumferential surfaces of the inner tube (5).
4. The boiler return feeder metal expansion joint according to claim 1, Features: The filler (8) is shale ceramsite, and a retaining ring (9) made of a high-density material is provided on the top surface of the filler (8), and the retaining ring (9) is located between the middle tube (3) and the inner tube (5).
5. The boiler return feeder metal expansion joint according to claim 1, Features: A protective sleeve (10) made of a heat-insulating material is provided on the outer side of the corrugated pipe (1), and the upper end of the protective sleeve (10) is fixed to the upper ring plate (2).
6. The boiler return feeder metal expansion joint according to claim 5, Features: The sheath (10) is provided with a plurality of heat dissipation holes.