Cement foaming light partition board

By using locking components and mud extrusion technology of snap grooves and snap blocks on cement foam lightweight partition panels, the problem of insufficient connection strength of existing partition panels is solved, and higher connection stability is achieved and productivity.

CN222295387UActive Publication Date: 2025-01-03SHANDONG TONGJU BUILDING ENERGY SAVING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202422976542.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-12-04
Publication Date
2025-01-03
Estimated Expiration
2034-12-04

AI Technical Summary

Technical Problem

The existing cement foam lightweight partition panels have low connection strength during installation, which are prone to external interference and cause misalignment or separation at the splicing, making it difficult to meet the stability requirements of high wall structures.

Method used

The design of snap slots and snap blocks enables the extension and curing of the snap rod through lock assembly and mud extrusion, enhances the connection strength between partition panels, and simplifies the installation process with removable snap rods.

Benefits of technology

It improves the connection strength and production efficiency between partition panels, reduces processing difficulty, and ensures the stability of the wall structure and the convenience of assembly.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222295387U_ABST
    Figure CN222295387U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of constructional engineering, and discloses a cement foaming light partition board which comprises a partition board body, a buckle groove is formed in the side wall of one end of the partition board body, a buckle block is installed on the side wall of the other end of the partition board body, and the buckle groove is matched with the buckle block. Every two adjacent groups of partition wall boards are mutually buckled and connected through the buckle grooves and the buckle blocks, lock catch assemblies are arranged on the inner sides of the buckle grooves, and buckle assemblies which are locked with the lock catch assemblies through extrusion of mud in the buckle grooves are arranged on the buckle blocks. According to the utility model, through moving pressure generated when the two groups of partition boards are assembled and slurry extrusion in the buckling grooves, the buckling rods on the buckling assemblies can extend into the buckling grooves, and after the slurry is solidified, the buckling rods are wrapped through solidification of the slurry, so that the connection strength between the two groups of partition boards is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of construction engineering, and more specifically to a cement foaming lightweight partition board. Background Art

[0002] The utility model relates to the field of building materials, and in particular to a cement foam lightweight partition board used for building internal partition wall construction. In modern construction projects, partition boards are key materials for dividing indoor spaces, and their performance and installation convenience have a very important impact on the quality, construction progress and user experience of the entire building.

[0003] When installing existing partition boards, usually one set of partition boards is fixed at a specified position, and then the subsequent partition boards are spliced ​​and installed through their own "U"-shaped grooves and matching protrusions with the help of mud. Although this splicing method can connect and fix the two sets of partition boards, the connection strength between the two sets of partition boards is low and is easily affected by external interference, such as collision and vibration, which may cause the splicing to be misaligned or separated. Even after the mud solidifies, the connection strength it can provide is still low, which is difficult to meet some building scenarios with high requirements for wall structure stability. For this reason, we propose a cement foam lightweight partition board. Utility Model Content

[0004] The technical problem to be solved by the utility model is: to overcome the deficiencies of the prior art and to provide a cement foam lightweight partition board to solve the problems existing in the prior cement foam lightweight partition boards.

[0005] The technical solution adopted by the utility model to solve the above technical problems is:

[0006] A cement foam lightweight partition board, comprising a partition board, a buckle groove is provided on one end side wall of the partition board, a buckle block is installed on the other end side wall of the partition board, the buckle groove and the buckle block are adapted to each other, two adjacent groups of partition boards are buckled and connected to each other through the buckle groove and the buckle block, a locking assembly is provided on the inner side of the buckle groove, and a buckle assembly is provided on the buckle block to complete locking with the locking assembly through mud extrusion in the buckle groove;

[0007] The locking assembly comprises an auxiliary block and a locking groove, wherein a plurality of rows of the locking grooves are arranged on both side walls of the inner side of the buckle groove at intervals in the vertical direction, and the auxiliary block is fixedly mounted on the inner side of the buckle groove;

[0008] The buckle assembly includes an extrusion groove, an adjustment groove, a buckle rod and a pressure block. The extrusion groove is arranged at an end of the buckle block away from the partition board, and the extrusion groove vertically penetrates the buckle block. A plurality of adjustment grooves are arranged at intervals in the vertical direction on both sides of the side walls of the buckle block. The positions of the adjustment grooves on the buckle block and the positions of the locking grooves on the buckle grooves correspond to each other, and the adjustment grooves penetrate the buckle block and the interior of the extrusion groove and are interconnected. A plurality of groups of buckle rods are arranged inside the extrusion groove corresponding to the positions of the adjustment grooves. A pressure block is arranged on the inner side of the extrusion groove, and the buckle rod is slidably arranged in the adjustment groove. The mud inside the buckle groove can squeeze the pressure block to make the buckle rod slide and be inserted into the locking groove. The pressure block is triangular in shape on the side close to the buckle rod.

[0009] The buckle rod includes a clamping rod, a blocking block and an auxiliary pressure block. The auxiliary pressure block is arranged on the inner side of the extrusion groove. The inclined surface of the auxiliary pressure block corresponds to the pressure block. The clamping rod is installed on the side of the blocking block away from the auxiliary pressure block. The clamping rod is slidably arranged in the adjustment groove.

[0010] The clamping rod includes an inner rod, an outer rod and a locking piece. The inner rod is fixedly mounted on the side wall of the blocking block away from the auxiliary pressure block. The outer rod is arranged at one end of the inner rod away from the blocking block. The inner rod and the outer rod are connected by a locking piece, and the locking piece adopts a screw and threaded connection method.

[0011] Overflow grooves are provided on both sides of the buckle groove and the buckle block on the partition wall plate.

[0012] The overflow groove is connected with a retention groove, and the retention groove is arranged on both sides of the buckle groove and the buckle block on the partition wall board.

[0013] Both ends of the partition board are provided with multiple rows of slurry coating grooves at intervals, and the slurry coating grooves on the side of the partition board close to the buckle block and the slurry coating grooves on the side of the partition board close to the buckle groove are arranged alternately.

[0014] Compared with the prior art, the utility model has the following beneficial effects:

[0015] 1. In the utility model, the moving pressure generated when two groups of partition boards are assembled and the mud extrusion inside the buckle groove enable the buckle rod on the buckle assembly to extend into the buckle groove. After the mud solidifies, the buckle rod is wrapped by the mud solidification, thereby improving the connection strength between the two groups of partition boards.

[0016] 2. In the present invention, the detachable and installable clamping rod can greatly reduce the processing difficulty of the partition board when it is processed through the template, thereby ensuring the locking effect when two sets of partition boards are assembled and improving the production efficiency of the partition board. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1This is a schematic diagram of the structure of the utility model (two groups of partition boards are assembled);

[0018] Figure 2 It is a partial cross-sectional structural schematic diagram of the utility model (two sets of partition boards are assembled);

[0019] Figure 3 For this utility model Figure 2 A schematic diagram of the local enlarged structure at point A in the middle;

[0020] Figure 4 It is a schematic diagram of the partial structure of the clamping rod in the second embodiment of the utility model.

[0021] Legend:

[0022] 1. Partition board; 2. Snap groove; 3. Snap block; 4. Overflow groove; 5. Retention groove; 6. Auxiliary block; 7. Locking groove; 8. Slurry coating groove; 9. Extrusion groove; 10. Adjustment groove; 11. Clamp rod; 12. Blocking block; 13. Auxiliary pressure block; 14. Pressure block; 15. Inner rod; 16. Outer rod; 17. Locking piece. DETAILED DESCRIPTION

[0023] The present invention is further described below in conjunction with specific embodiments. However, people familiar with the art should understand that the detailed description given here in conjunction with the drawings is for better explanation, and the structure of the present invention necessarily exceeds these limited embodiments. For some equivalent replacement schemes or common means, they are no longer described in detail herein, but still fall within the scope of protection of the present application.

[0024] Figure 1~Figure 3 It is the best embodiment of the utility model, and the following Figure 1 ~Attached Figure 3 The utility model is further described.

[0025] Embodiment 1:

[0026] Figure 1-Figure 3 As shown, a cement foam lightweight partition board includes a partition board 1, a snap groove 2 is opened on the side wall at one end of the partition board 1, and a snap block 3 is installed on the side wall at the other end of the partition board 1, the snap groove 2 and the snap block 3 are adapted to each other, and two adjacent groups of partition boards 1 are snap-connected to each other through the snap groove 2 and the snap block 3, a locking assembly is arranged on the inner side of the snap groove 2, and a snap assembly is arranged on the snap block 3, which is locked with the locking assembly through mud extrusion inside the snap groove 2.

[0027] The locking assembly includes an auxiliary block 6 and a locking groove 7. A plurality of rows of the locking grooves 7 are arranged on the side walls on both sides of the inner side of the snap groove 2 at intervals in the vertical direction. The auxiliary block 6 is fixedly installed on the inner side of the snap groove 2. The auxiliary block 6 can be set to a semicircular block shape.

[0028] The buckle assembly includes an extrusion groove 9, an adjustment groove 10, a buckle rod and a pressure block 14. The extrusion groove 9 is arranged at an end of the buckle block 3 away from the partition board 1, and the extrusion groove 9 vertically penetrates the buckle block 3. A plurality of rows of adjustment grooves 10 are arranged at intervals in the vertical direction on both sides of the side walls of the buckle block 3. The positions of the adjustment grooves 10 on the buckle block 3 and the positions of the locking grooves 7 on the buckle groove 2 correspond to each other, and the adjustment grooves 10 penetrate the buckle block 3 and the interior of the extrusion groove 9 and are connected to each other. A plurality of groups of buckle rods are arranged inside the extrusion groove 9 corresponding to the positions of the adjustment grooves 10. A pressure block 14 is arranged on the inner side of the extrusion groove 9. The buckle rod is slidably arranged in the adjustment groove 10. The mud inside the buckle groove 2 can slide and insert the buckle rod into the locking groove 7 by extruding the pressure block 14. The pressure block 14 is triangular in shape near the buckle rod.

[0029] In this embodiment, the buckle rod can extend to the inside of the buckle groove 7 at the corresponding position through the adjustment groove 10 when the two sets of partition boards 1 are assembled, and the buckle is completed by filling and squeezing the mud. Specifically, through the pressure block 14, when the buckle block 3 is inserted into the buckle groove 2, the mud inside the buckle groove 2 will squeeze the pressure block 14, so that the pressure block 14 is pressed inside the extrusion groove 9 to move, so that the pressure block 14 moves the two buckle rods to squeeze, so that the two buckle rods move, and the buckle operation is completed.

[0030] Specifically, the buckle rod includes a clamping rod 11, a blocking block 12 and an auxiliary pressure block 13. The auxiliary pressure block 13 is arranged on the inner side of the extrusion groove 9. One side of the auxiliary pressure block 13 is an inclined surface. The inclined surface of the auxiliary pressure block 13 corresponds to the pressure block 14. The clamping rod 11 is installed on the side of the blocking block 12 away from the auxiliary pressure block 13. The clamping rod 11 is slidably arranged in the adjustment groove 10. The width of the blocking block 12 is larger than the size of the adjustment groove 10.

[0031] In this embodiment, the movement of the locking rod 11 is limited by the blocking block 12, so that a section of the locking rod is always located inside the extrusion groove 9, which can effectively ensure the locking stability of the two groups of partition boards 1 when they are assembled.

[0032] Overflow grooves 4 are provided on both sides of the buckle groove 2 and the buckle block 3 on the partition board 1.

[0033] In this embodiment, the overflow groove 4 allows the excess mud to effectively overflow through the overflow groove 4 when the two groups of partition boards 1 are squeezed after the mud is applied.

[0034] The overflow groove 4 is connected to a retention groove 5 , and the retention groove 5 is arranged on both sides of the buckle groove 2 and the buckle block 3 on the partition board 1 .

[0035] In this embodiment, when the mud is squeezed and overflows through the overflow groove 4, part of the mud will be retained through the retention groove 5, and the retained mud can fill the space between the two groups of partition boards 1 during the mud solidification process.

[0036] Multiple rows of slurry coating grooves 8 are arranged at both ends of the partition board 1, and the slurry coating grooves 8 on the side of the partition board 1 close to the buckle block 3 and the slurry coating grooves 8 on the side of the partition board 1 close to the buckle groove 2 are arranged alternately.

[0037] In this embodiment, the slurry coating groove 8 can effectively retain the slurry on the side wall of the partition board 1. At the same time, the connection and curing effect of the slurry between the two groups of partition boards 1 can be effectively improved when the two groups of partition boards 1 are assembled.

[0038] The working principle and use process of the utility model are as follows:

[0039] When in use, after a group of partition boards 1 are installed and fixed, mud is brushed on the side close to the buckle groove 2. At the same time, the side close to the buckle block 3 of the partition board 1 to be installed in the fitting position is brushed. Then, the two groups of partition boards 1 coated with mud are spliced ​​and assembled by transportation. When assembling, the pressure-bearing block 14 inside the extrusion groove 9 on the buckle block 3 is squeezed by the mud inside the buckle groove 2 and the moving pressure during splicing and moves toward the extrusion groove 9, so that the auxiliary pressure blocks 13 on the two groups of buckle rods at the corresponding positions are squeezed. Under the limit of the adjustment groove 10, the auxiliary pressure blocks 13 are compressed, which will drive the clamping rod 11 to move into the locking groove 7 at the corresponding position. At the same time, through the pressure generated during extrusion, the mud inside the buckle groove 2 will fill the locking groove 7. When the mud solidifies, the mud inside the locking groove 7 will completely wrap and solidify the clamping rod 11, thereby completing the operation of assembling the two groups of partition boards 1.

[0040] Embodiment 2:

[0041] like Figure 4 As shown, on the basis of embodiment one, the clamping rod 11 includes an inner rod 15, an outer rod 16 and a locking piece 17, the inner rod 15 is fixedly mounted on the side wall of the blocking block 12 away from the auxiliary pressure block 13, the outer rod 16 is arranged at one end of the inner rod 15 away from the blocking block 12, and the inner rod 15 and the outer rod 16 are connected by a locking piece 17, and the locking piece 17 adopts a screw and threaded connection method.

[0042] In this embodiment, by using the detachable and installable clamping rod 11, the two groups of partition boards 1 can be spliced ​​and installed on the adjustment groove 10 before installation, and then the pressure block 14 is placed inside the extrusion groove 9 after the position is calibrated, so that the two groups of partition boards 1 are easier to form when processed through the template, reducing the difficulty of processing the partition boards 1 through the template.

Claims

1. A cement foam lightweight partition board, comprising a partition board (1), wherein a buckle groove (2) is provided on one end side wall of the partition board (1), and a buckle block (3) is installed on the other end side wall of the partition board (1), wherein the buckle groove (2) and the buckle block (3) are matched with each other, and two adjacent groups of partition boards (1) are buckled and connected to each other through the buckle groove (2) and the buckle block (3), characterized in that: A locking assembly is provided on the inner side of the buckle groove (2), and a buckle assembly is provided on the buckle block (3) for locking with the locking assembly through mud extrusion inside the buckle groove (2); The locking assembly comprises an auxiliary block (6) and locking grooves (7), wherein a plurality of rows of locking grooves (7) are arranged at intervals in the vertical direction on the side walls on both sides of the inner side of the buckle groove (2), and the auxiliary block (6) is fixedly mounted on the inner side of the buckle groove (2); The buckle assembly comprises an extrusion groove (9), an adjustment groove (10), a buckle rod and a pressure block (14); the extrusion groove (9) is arranged at an end of the buckle block (3) away from the partition board (1), and the extrusion groove (9) vertically penetrates the buckle block (3); a plurality of rows of adjustment grooves (10) are arranged at intervals in the vertical direction on both sides of the side wall of the buckle block (3); the position of the adjustment groove (10) on the buckle block (3) and the position of the locking groove (7) on the buckle groove (2) correspond to each other. The adjusting groove (10) penetrates the interior of the buckle block (3) and the extrusion groove (9) and is interconnected. A plurality of buckle rods are arranged inside the extrusion groove (9) at positions corresponding to the adjusting groove (10). A pressure block (14) is arranged inside the extrusion groove (9). The buckle rod is slidably arranged in the adjusting groove (10). Mud inside the buckle groove (2) can squeeze the pressure block (14) to make the buckle rod slide and insert into the locking groove (7). The pressure block (14) is triangular in shape on the side close to the buckle rod.

2. The cement foam lightweight partition board according to claim 1, characterized in that: The buckle rod comprises a clamping rod (11), a blocking block (12) and an auxiliary pressure block (13); the auxiliary pressure block (13) is arranged on the inner side of the extrusion groove (9); the inclined surface of the auxiliary pressure block (13) corresponds to the pressure block (14); the clamping rod (11) is installed on the side of the blocking block (12) away from the auxiliary pressure block (13); and the clamping rod (11) is slidably arranged in the adjustment groove (10).

3. The cement foam lightweight partition board according to claim 2, characterized in that: The clamping rod (11) comprises an inner rod (15), an outer rod (16) and a locking member (17); the inner rod (15) is fixedly mounted on a side wall of the barrier block (12) away from the auxiliary pressure block (13); the outer rod (16) is arranged at an end of the inner rod (15) away from the barrier block (12); and the inner rod (15) and the outer rod (16) are connected via the locking member (17); the locking member (17) is connected by a screw and a thread.

4. The cement foam lightweight partition board according to claim 1, characterized in that: Overflow grooves (4) are provided on both sides of the buckle groove (2) and the buckle block (3) on the partition wall plate (1).

5. The cement foam lightweight partition board according to claim 4, characterized in that: The overflow groove (4) is connected to a retention groove (5), and the retention groove (5) is arranged on both sides of the buckle groove (2) and the buckle block (3) on the partition board (1).

6. The cement foam lightweight partition board according to claim 1, characterized in that: Both ends of the partition wall plate (1) are provided with a plurality of rows of slurry coating grooves (8) at intervals, and the slurry coating grooves (8) on the side of the partition wall plate (1) close to the buckle block (3) and the slurry coating grooves (8) on the side of the partition wall plate (1) close to the buckle groove (2) are arranged alternately.