A glass opening frameless component and its manufacturing method
A manufacturing method and borderless technology, applied in the direction of final product manufacturing, sustainable manufacturing/processing, electrical components, etc., can solve the problems of high cost, complicated installation and operation, etc., and achieve the effect of convenient and fast installation and operation, and the realization of integration
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] Such as Figure 1 ~ Figure 4 As shown, a frameless assembly with glass openings is a 60-piece 156-cell assembly, including tin-coated copper strips 4, battery sheets 3, tempered glass 2, mounting holes 1, EVA film and TPT backplane. The tin-coated copper strip 4 is located on the battery sheet 3, the installation hole 1 is located on the tempered glass 2, and the EVA adhesive film is located between the tempered glass 2 and the battery sheet 3 and between the battery sheet 3 and the TPT backplane.
[0034] A method for manufacturing a glass aperture frameless component, comprising the following steps:
[0035] 1) welding the tin-coated copper strip 4 to the single cell 3;
[0036] 2) Use a customized template to connect the cells 3 in series, arranged in a 10×6 matrix;
[0037] 3) Four installation holes 1 are opened at set positions on the tempered glass 2, and a set safety distance is left between the edge of the installation holes 1 and the surrounding correspondin...
Embodiment 2
[0045] Such as Figure 5 ~ Figure 8 As shown, a frameless assembly with glass openings is a 72-piece 125 cell assembly, including tin-coated copper strips 14, battery sheets 13, tempered glass 12, mounting holes 11, EVA film and TPT backplane. The tin-coated copper strip 14 is located on the battery sheet 13, the mounting hole 11 is located on the tempered glass 12, and the EVA adhesive film is located between the tempered glass 12 and the battery sheet 13 and between the battery sheet 13 and the TPT backplane.
[0046] A method for manufacturing a glass aperture frameless component, comprising the following steps:
[0047] 1) welding the tin-coated copper strip 14 to the monolithic cell 13;
[0048] 2) Use a customized template to connect the cells 13 in series, arranged in a 10×6 matrix;
[0049] 3) Four installation holes 11 are opened at set positions on the toughened glass 12, and a set safety distance is left between the edges of the installation holes 11 and the surro...
PUM