A technology for developing components and molecules, which is applied to the equipment of the electric recording process using the charge pattern, the electric recording process using the charge pattern, and the electric recording technique, etc., and can solve problems such as unevenness and stripes
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0092] (Production of Elastic Roller 1)
[0093] The surface of a mandrel with a diameter of 6 mm plated with nickel on the iron surface was coated with a primer (trade name: DY35-051, produced by Dow Corning Toray Co., Ltd.), after which the primer was baked at a temperature of 170° C. 20 minutes. Then, the mandrel was put into a mold having a cylindrical tube with an inner diameter of 12 mm and pieces (pieces) for holding the mandrel provided at both ends of the tube, and used for forming elastic The liquid material of the layer was injected from the piece at one end and then heated at 130° C. for 20 minutes.
[0094] After cooling, the resultant was taken out from the mold to obtain a primary cured elastic roller in which an elastic layer having a thickness of 3.0 mm was provided on the outer periphery of the mandrel. Furthermore, the roll was heated in a furnace at 200° C. for 2 hours to obtain an elastic roll 1 .
[0095] [Table 1]
[0096] Table 1 (Materials constitu...
Embodiment 2
[0131] In addition to further adding 1.5 parts by mass of hydrophobic silica (trade name: RX200, produced by Nippon Aerosil Co., Ltd.) to the material constituting the liquid material for forming the elastic layer of Example 1 in Example 1, with The developing roller 2 was produced in the same manner as in Example 1, and was measured and evaluated in the same manner as in Example 1. Table 2 shows the results.
Embodiment 3
[0133] The developing roller 3 was produced in the same manner as in Example 2 except that the following (B2) was used instead of (B1) in Example 2, and measured and evaluated in the same manner as in Example 1. Table 2 shows the results.
[0134] (B2): contains CH 2 =CH(CH 3 ) 2 SiO 1 / 2 unit, (CH 3 ) 3 SiO 1 / 2 Cell and SiO 4 / 2 The constituent unit of the unit, CH 2 =CH(CH 3 ) 2 SiO 1 / 2 unit and (CH 3 ) 3 SiO 1 / 2 The total amount of unit and SiO 4 / 2 An organopolysiloxane having a molar ratio of units of 0.5, a weight average molecular weight of 6,600, and an average of 4 vinyl groups bonded to silicon atoms in one molecule.