A kind of muddy ice slurry with high ice content and preparation method thereof
A technology of ice content and ice slurry is applied in the field of muddy ice slurry and its preparation. Inhibit ice crystal growth, good flow effect
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Publication Date
- 2021-08-17
Smart Images

Figure 1 
Figure 2 
Figure 3
Abstract
Description
technical field
[0001] The invention relates to the technical field of ice slurry preparation, in particular to a muddy ice slurry with high ice content and a preparation method thereof. Background technique
[0002] Ice slurry is a solid-liquid two-phase fluid with good fluidity composed of solution and ice crystal particles. Because of its good heat transfer characteristics and high density of latent heat storage, it is widely used in construction, medicine, food refrigeration, mine cooling and other fields. It has broad application prospects, but the existing ice slurry has poor fluidity, so it is easy to stick to the wall and has a low ice content.
[0003] The existing technologies for preparing ice slurry mainly include supercooled water ice making technology, water jet evaporative ice making, and silicone oil emulsion ice making.
[0004] Supercooled water ice making technology: When water or aqueous solution is cooled to a supercooled state in the evaporating coil, ...
Examples
Embodiment 1
[0052] A muddy ice slurry with high ice content, which is made of solvent, polyvinyl alcohol, glycerol, borax, ethylene glycol, polyoxyethylene sorbitan fatty acid ester and polyethylene oxide propylene oxide Prepared from glycerol ether;
[0053] Based on the solvent quality, the mass percentages of other components are respectively polyvinyl alcohol 1.0%, glycerol 1.5%, borax 0.6%, ethylene glycol 2.0%, polyoxyethylene sorbitan fatty acid ester 1.5%, polycyclo Ethylene Oxide Propylene Oxide Glyceryl Ether 0.5%.
[0054] The solvent is water.
[0055] A kind of preparation method of muddy ice slurry with high ice content rate, this preparation method comprises the following steps:
[0056] Adding polyvinyl alcohol into a solvent with a mass fraction of 25% and heating and stirring for 13 minutes to obtain a mixture;
[0057] adding glycerol, borax, ethylene glycol, polyoxyethylene sorbitan fatty acid ester and polyethylene oxide propylene oxide glyceryl ether into the mixt...
Embodiment 2
[0078] The mass percentages of "other components" in Example 1 are respectively polyvinyl alcohol 1.0%, glycerol 1.5%, borax 0.6%, ethylene glycol 2.0%, polyoxyethylene sorbitan fatty acid ester 1.5%, poly Ethylene oxide propylene oxide glyceryl ether 0.5%" was changed to "the mass percentages of other components were polyvinyl alcohol 0.7%, glycerin 1.0%, borax 0.6%, ethylene glycol 3.0%, polyoxyethylene sorbitol Anhydride fatty acid ester 1.0%, polyethylene oxide propylene oxide glyceryl ether 0.5%".
Embodiment 3
[0080] The mass percentages of "other components" in Example 1 are respectively polyvinyl alcohol 1.0%, glycerol 1.5%, borax 0.6%, ethylene glycol 2.0%, polyoxyethylene sorbitan fatty acid ester 1.5%, poly Ethylene oxide propylene oxide glyceryl ether 0.5%" was changed to "the mass percentages of other components were polyvinyl alcohol 1.0%, glycerin 1.0%, borax 0.5%, ethylene glycol 1.9%, polyoxyethylene sorbitol Anhydride fatty acid ester 1.5%, polyethylene oxide propylene oxide glyceryl ether 0.7%".
[0081] The following table is the experimental data of ice slurry prepared in embodiment one, embodiment two and embodiment three
[0082] Example Ice content Embodiment one 70% Embodiment two 50% Embodiment three 58%
[0083] The "fixed connection" described in the present invention means that the two parts connected to each other are fixed together, generally by means of welding, screwing or gluing; "rotational connection" means that the tw...