A hydrolysis-resistant LED chip and its manufacturing method and device
By forming a light-transmitting non-conductive barrier layer and an exposed area on the substrate of the LED chip, the edge of the barrier layer exceeds the edge of the epitaxial layer, and the capillary phenomenon is used to prevent water vapor from climbing up, thus solving the problem of water vapor erosion of the LED chip in outdoor displays and improving Improve the reliability and light extraction efficiency of the chip.
Patent Information
- Application Number
- CN202010397225.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-05-12
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2040-05-12
AI Technical Summary
Existing LED chips are easily corroded by water vapor in outdoor display applications, leading to failure. The existing packaging structure cannot effectively prevent water vapor from climbing to the epitaxial layer, affecting reliability.
A light-transmitting and non-conductive barrier layer is formed on the substrate of the LED chip, and exposed areas and columnar structures are formed through etching. The edge of the barrier layer exceeds the edge of the epitaxial layer to form a water-stop layer, which uses capillary phenomena to prevent water vapor from climbing.
It effectively blocks water vapor from corroding the epitaxial layer, improves the reliability of the LED chip, ensures the normal formation and light extraction efficiency of the epitaxial layer, and prevents water vapor from climbing to the epitaxial layer through gaps.
Smart Images

Figure CN111446344B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of light emitting diodes, and in particular to a hydrolysis-resistant LED chip and a manufacturing method and device thereof. Background Art
[0002] The existing LED chip includes a substrate, an epitaxial layer disposed on the substrate, and an electrode disposed on the epitaxial layer. Figure 1 The existing LED packaging device includes an LED chip 10, a bonding adhesive 20 for fixing the LED chip 10 on a substrate, and a packaging adhesive 30 for wrapping the LED chip 10 and covering the bonding adhesive 20. When the LED packaging device is used in outdoor display products, it is easily affected by the weather, and water vapor easily penetrates into the LED chip 10 along the gap between the bonding adhesive 20 and the packaging adhesive 30, causing the LED chip 10 to hydrolyze and fail, and finally causing a dead light. Summary of the invention
[0003] The technical problem to be solved by the present invention is to provide a hydrolysis-resistant LED chip, which prevents water vapor from climbing up to the epitaxial layer, avoids the epitaxial layer from being corroded, and has high reliability.
[0004] Another technical problem to be solved by the present invention is to provide a method for installing a hydrolysis-resistant LED chip to prevent water vapor from climbing up to the epitaxial layer with high reliability.
[0005] The technical problem that the present invention also solves is to provide a hydrolysis-resistant LED device that prevents water vapor from climbing from the gap between the die-bonding glue and the packaging glue and the chip to the epitaxial layer, and has high reliability.
[0006] In order to solve the above technical problems, the present invention provides a hydrolysis-resistant LED chip, characterized in that it comprises:
[0007] Substrate,
[0008] A barrier layer is provided on the substrate, wherein a plurality of exposed areas are provided on the barrier layer, wherein the exposed areas are etched to the surface of the substrate, wherein the total area of the exposed areas accounts for more than 7% of the total area of the substrate, and the area of each exposed area accounts for 1 to 15% of the total area of the exposed areas,
[0009] an epitaxial layer disposed on the barrier layer and the exposed area of the substrate,
[0010] The edge of the barrier layer exceeds the edge of the epitaxial layer, and the barrier layer is made of a light-transmitting non-conductive material.
[0011] As an improvement of the above solution, the barrier layer is made of one or more of silicon dioxide, silicon nitride, and diamond-like film.
[0012] As an improvement of the above solution, the edge of the barrier layer exceeds the edge of the epitaxial layer by 5 to 15 μm.
[0013] As an improvement of the above solution, the edge of the barrier layer exceeds the edge of the epitaxial layer by 6 to 10 μm, and the edge of the barrier layer exceeds the edge of the substrate by 1 to 5 μm.
[0014] As an improvement of the above solution, the thickness of the barrier layer is 300 to 1800 nm.
[0015] As an improvement of the above solution, the area of each exposed region accounts for 1-10% of the total exposed region area.
[0016] As an improvement of the above solution, the substrate is a patterned substrate, a plurality of columnar structures are provided on the substrate, each exposed region includes a columnar structure, and the area of the exposed columnar structure accounts for 50-90% of the area of each exposed region.
[0017] Correspondingly, the present invention also provides a hydrolysis-resistant LED device, comprising the hydrolysis-resistant LED chip, the bonding adhesive and the packaging adhesive as described in the above claims, wherein the bonding adhesive fixes the hydrolysis-resistant LED chip on the substrate, and the packaging adhesive wraps the hydrolysis-resistant LED chip and covers the bonding adhesive.
[0018] Accordingly, the present invention also provides a method for manufacturing a hydrolysis-resistant LED chip, comprising:
[0019] 1. forming a barrier layer on the substrate, wherein the barrier layer is made of a light-transmitting non-conductive material;
[0020] 2. etching the barrier layer to the substrate surface to form a plurality of exposed areas, wherein the total area of the exposed areas accounts for more than 7% of the total area of the substrate;
[0021] 3. forming an epitaxial layer on the barrier layer and the exposed substrate;
[0022] Fourth, etching the edge of the epitaxial layer so that the edge of the barrier layer exceeds the edge of the epitaxial layer.
[0023] As an improvement of the above solution, the method for manufacturing the barrier layer includes:
[0024] Using evaporation or PECVD deposition method, at a temperature of 150-300°C and a pressure of 200-750m torr, SiH4, N2O and N2 gases are introduced at flow rates of 10-20 SCCM, 1200-1300 SCCM and 550-650 SCCM respectively to form SiO2; and / or,
[0025] By evaporation or PECVD deposition, SiH4, NH3 and N2 gases are introduced at a temperature of 150-300°C and a pressure of 200-750m torr, with flow rates of 10-20 SCCM, 2200-2300 SCCM and 250-350 SCCM respectively, to form SN X and / or,
[0026] The PECVD deposition method is used to form DLC by introducing CH4 at a temperature of 900-1100°C.
[0027] The implementation of the present invention has the following beneficial effects:
[0028] The hydrolysis-resistant LED chip of the present invention is provided with a barrier layer between the substrate and the epitaxial layer to block the rise of water vapor and prevent water vapor from corroding the epitaxial layer. Specifically, the barrier layer is provided with a plurality of exposed areas, the exposed areas are etched to the surface of the substrate, and the total area of the exposed areas accounts for more than 7% of the total area of the substrate, and the area of each exposed area accounts for 1-15% of the total area of the exposed areas, so as to ensure the normal formation of the epitaxial layer. In addition, the edge of the barrier layer exceeds the edge of the epitaxial layer to form a water stop layer, so that the gap between the solid crystal glue and the packaging glue forms a capillary phenomenon, and through the effect of the surface tension of the liquid in the gap and the pressure difference between the inside and outside of the curved surface, the water vapor can only be in the gap and cannot climb to the epitaxial layer.
[0029] Furthermore, the present invention improves the density and strength of the barrier layer by adjusting the manufacturing method of the barrier layer, thereby preventing the barrier layer from being too thick. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a structural schematic diagram of an existing LED package;
[0031] Figure 2 It is a schematic diagram of the structure of the hydrolysis-resistant LED chip of the present invention;
[0032] Figure 3 is a top view of a hydrolysis-resistant LED chip of the present invention in which a barrier layer is disposed on a substrate;
[0033] Figure 4 It is a schematic structural diagram of the hydrolysis-resistant LED device of the present invention;
[0034] Figure 5 is an electron microscope photograph of the LED chip of Comparative Example 1 of the present invention;
[0035] Figure 6 yes Figure 5 A in the enlarged view;
[0036] Figure 7 yes Figure 6 The enlarged view of point D in the figure;
[0037] Figure 8 yes Figure 5 The enlarged view of point B in the figure;
[0038] Fig. 9 yes Figure 5 The enlarged view of point C in the figure;
[0039] Fig.10 Example 1 corresponds to Example 1 Figure 5 An enlarged view of the corresponding position at C. DETAILED DESCRIPTION
[0040] In order to make the objectives, technical solutions and advantages of the present invention more clear, the present invention will be further described in detail below with reference to the accompanying drawings.
[0041] The invention provides a hydrolysis-resistant LED chip, comprising a substrate, a barrier layer arranged on the substrate, an epitaxial layer and an electrode.
[0042] See also Figure 2 The substrate 10 of the present invention is a patterned substrate, and a plurality of columnar structures 11 are provided on the substrate 10. The substrate 10 of the present invention may also be a non-patterned substrate.
[0043] The barrier layer 20 is provided with a plurality of exposed regions 21 , and the exposed regions 21 are etched to the surface of the substrate 10 . The epitaxial layer 30 is disposed on the barrier layer 20 and the substrate 10 in the exposed regions 21 .
[0044] Since the material of the barrier layer 20 of the present invention is greatly different from that of the epitaxial layer 30, the epitaxial layer 30 cannot be directly formed on the barrier layer 20. In order to ensure the smooth formation of the epitaxial layer 30, the barrier layer 20 is etched to expose part of the substrate 10, so that part of the epitaxial layer 30 can be formed on the substrate 10.
[0045] Preferably, the total area of the exposed regions 21 accounts for more than 7% of the total area of the substrate 10, and the exposed regions 21 are evenly distributed. If the exposed regions 21 are too small, the formation of the epitaxial layer 30 is affected, and the epitaxial layer 30 is not easy to form a plane.
[0046] In order to further ensure the formation of the epitaxial layer 30 and reduce the lattice mismatch between the epitaxial layer 30 and the substrate 10, the area of each exposed region 21 accounts for 1-15% of the total exposed area. Figure 3As shown. If the area of each exposed region 21 is too small, it is difficult for the epitaxial layer 30 to contact the substrate 10 well. If the area of each exposed region 21 is too large, the epitaxial layer 30 is not in uniform contact with the substrate 10. Preferably, the area of each exposed region 21 accounts for 1 to 10% of the total exposed area. More preferably, the area of each exposed region 21 accounts for 2 to 5% of the total exposed area.
[0047] When the substrate 10 is a patterned substrate, the columnar structure 11 must be exposed. The columnar structure 11 is used to increase the contact area between the substrate 10 and the epitaxial layer 30 and improve the lattice quality of the epitaxial layer 30. Specifically, each exposed area 21 includes a columnar structure 11, and the area of the exposed columnar structure 11 accounts for 50% to 90% of the area of each exposed area 21. If the area of the exposed columnar structure 11 accounts for too small a proportion, the contact area between the substrate 10 and the epitaxial layer 30 will be affected; since the columnar structure 11 is a convex structure, if the area of the exposed columnar structure 11 accounts for too large a proportion, the bonding force between the substrate 10 and the epitaxial layer 30 will be formed, and the two layers are prone to cracking.
[0048] Preferably, in each exposed area 21 , the area of the exposed columnar structure 11 accounts for 50-80% of the area of each exposed area 21 . More preferably, in each exposed area 21 , the area of the exposed columnar structure 11 accounts for 60-70% of the area of each exposed area 21 .
[0049] Furthermore, the distance between each exposed area is 3-10 μm.
[0050] The present invention sets a barrier layer between the substrate and the epitaxial layer. Due to the material of the barrier layer itself, the epitaxial layer cannot be directly formed on the barrier layer. Therefore, the present invention etches the barrier layer to form an exposed area, and controls the size of the exposed area, the distance between the exposed areas, the area ratio of the exposed areas, and the ratio of the columnar structure in each exposed area, so as to ensure the normal formation of the epitaxial layer and the lattice quality of the epitaxial layer.
[0051] The edge of the barrier layer 20 exceeds the edge of the epitaxial layer 30 to form a water stop layer to prevent water vapor from climbing to the side wall of the epitaxial layer 30. The present invention adds a barrier layer 20 between the substrate 10 and the epitaxial layer 30, and forms a capillary phenomenon in the gap between the die-bonding glue and the packaging glue through the water stop layer. Through the effect of the surface tension of the liquid in the gap and the pressure difference between the inside and outside of the curved surface, water vapor can only stay in the gap and cannot climb to the epitaxial layer.
[0052] Preferably, the edge of the barrier layer 20 exceeds the edge of the epitaxial layer by 5 to 15 μm. Specifically, the present invention achieves the edge of the barrier layer exceeding the edge of the epitaxial layer by etching the edge of the epitaxial layer. If the edge of the barrier layer exceeds the edge of the epitaxial layer by more than 15 μm, the light output area of the outer layer is affected, and the light output efficiency of the chip is reduced; if the edge of the barrier layer exceeds the edge of the epitaxial layer by less than 5 μm, water vapor can easily climb over the barrier layer to the side wall of the epitaxial layer, thus affecting the blocking effect.
[0053] Preferably, the edge of the barrier layer exceeds the edge of the epitaxial layer by 6-10 μm to match the thickness of the epitaxial layer of 6 μm.
[0054] The material of the barrier layer 20 must meet the following conditions:
[0055] (1) Light transmission: if the blocking layer is not light-transmissive, the light extraction efficiency of the chip will be affected;
[0056] (2) Non-conductive. If the barrier layer is made of conductive material, the barrier layer will hydrolyze when the chip is powered on, and will not play the role of blocking water vapor.
[0057] (3) Withstand high temperatures above 1100°C. Since the epitaxial layer is formed on the barrier layer, the formation temperature of the epitaxial layer will be greater than 1100°C;
[0058] (4) Similar to the material of the packaging glue.
[0059] Preferably, the barrier layer 20 is made of a light-transmitting non-conductive material. More preferably, the barrier layer 20 is made of silicon dioxide (SiO2), silicon nitride (SiN x ), diamond-like film (DLC) or several thereof.
[0060] More preferably, the barrier layer 20 is made of silicon dioxide (SiO2), silicon nitride (SiN x ) or diamond-like film (DLC).
[0061] Furthermore, the side wall of the epitaxial layer 30 is inclined inwardly at an angle of 30 to 60 degrees. Preferably, the side wall of the epitaxial layer 30 is inclined inwardly at an angle of 30 to 45 degrees. The present invention can further prevent water vapor from climbing onto the side wall of the epitaxial layer 30 by forming an inclined side wall.
[0062] The thickness of the barrier layer 20 plays an important role in preventing water vapor from penetrating and the brightness of the chip. If the barrier layer 20 is too thin, it cannot block water vapor; if the barrier layer 20 is too thick, it will cover the columnar structure 11 of the pattern substrate 10, affecting the growth of the epitaxial layer 30, thereby affecting the light extraction efficiency of the chip.
[0063] Preferably, the barrier layer 20 has a thickness of 300 to 1800 nm. Preferably, the barrier layer 20 has a thickness of 500 to 1000 nm. More preferably, the barrier layer 20 has a thickness of 600 to 800 nm.
[0064] In order to further increase the difficulty of water vapor climbing, the edge of the barrier layer 20 exceeds the edge of the substrate 10. Since the barrier layer 20 is directly formed on the substrate 10, if the edge of the barrier layer 20 exceeds the edge of the substrate 10 too much, the barrier layer 20 is easy to break and the adhesion between it and the packaging glue is affected. Preferably, the edge of the barrier layer 20 exceeds the edge of the substrate 10 by 1 to 5 μm.
[0065] Since the present invention sets a barrier layer on one side between the epitaxial layer and the substrate to prevent water vapor from corroding the epitaxial layer, the epitaxial layer of the present invention does not need to be structurally designed to resist water vapor corrosion, so the epitaxial layer of the present invention can be selected from epitaxial layers of all structures.
[0066] The epitaxial layer of the present invention comprises a buffer layer, an N-GaN layer, an MQW layer and a P-GaN layer which are arranged in sequence.
[0067] The epitaxial layer of the present invention comprises a buffer layer, a U-GaN layer, an N-GaN layer, an MQW layer and a P-GaN layer which are arranged in sequence.
[0068] The epitaxial layer of the present invention comprises an N-GaAs layer, an MQW layer and a P-GaP layer which are arranged in sequence.
[0069] The buffer layer is composed of one or more of AlN, AlGaN, GaN, InGaN and InN, and is used to reduce the lattice mismatch between the substrate and the epitaxial layer. Since the material of the buffer layer is similar to that of the epitaxial layer, in the existing LED chip, the buffer layer will also be corroded by water vapor.
[0070] Preferably, the buffer layer comprises an AlN layer, an AlGaN layer and a GaN layer which are arranged in sequence.
[0071] Preferably, the buffer layer includes an AlN layer, a GaN layer, and an InGaN layer which are arranged in sequence.
[0072] Preferably, the buffer layer comprises an AlN layer, an InGaN layer and an InN layer which are arranged in sequence.
[0073] The electrode of the present invention forms a conductive connection with the epitaxial layer. The electrode structure of the present invention can be the electrode structure of an existing LED chip, and the present invention does not make any specific limitation.
[0074] See also Figure 4The present invention also provides a hydrolysis-resistant LED device, comprising an LED chip 1, a bonding adhesive 2 and a packaging adhesive 3 according to the present invention, wherein the bonding adhesive 2 fixes the LED chip 1 on a substrate, and the packaging adhesive 3 wraps the LED chip 1 and covers the bonding adhesive 2.
[0075] The material of the packaging glue 3 is epoxy resin, polycarbonate, polymethyl methacrylate, glass or silicone material, but not limited thereto. The material of the die-bonding glue 2 is conductive glue or insulating glue, but not limited thereto.
[0076] Accordingly, the present invention also provides a method for manufacturing an LED chip, comprising the following steps:
[0077] 1. forming a barrier layer on a substrate;
[0078] The substrate of the present invention is a pattern substrate, on which a plurality of columnar structures are arranged. The substrate of the present invention can also be a non-pattern substrate.
[0079] The material of the barrier layer must meet the following conditions:
[0080] (1) Light transmission: if the blocking layer is not light-transmissive, the light extraction efficiency of the chip will be affected;
[0081] (2) Non-conductive. If the barrier layer is made of conductive material, the barrier layer will hydrolyze when the chip is powered on, and will not play the role of blocking water vapor.
[0082] (3) Withstand high temperatures above 1100°C. Since the epitaxial layer is formed on the barrier layer, the formation temperature of the epitaxial layer will be greater than 1100°C;
[0083] (4) Similar to the material of the packaging glue.
[0084] Preferably, the barrier layer is made of a light-transmitting, non-conductive material. More preferably, the barrier layer is made of one or more of silicon dioxide (SiO2), silicon nitride (SiNx), and diamond-like film (DLC).
[0085] The thickness of the barrier layer 20 plays an important role in preventing water vapor from penetrating and the brightness of the chip. If the barrier layer 20 is too thin, it cannot block water vapor; if the barrier layer 20 is too thick, it will cover the columnar structure 11 of the pattern substrate 10, affecting the growth of the epitaxial layer 30, thereby affecting the light extraction efficiency of the chip.
[0086] Preferably, the barrier layer 20 has a thickness of 300 to 1800 nm. Preferably, the barrier layer 20 has a thickness of 500 to 1000 nm. More preferably, the barrier layer 20 has a thickness of 600 to 800 nm.
[0087] The method for making the barrier layer plays an important role in the barrier effect of the barrier layer. The present invention improves the density and strength of the barrier layer by adjusting the method for making the barrier layer, and avoids the barrier layer being too thick. Specifically, the method for making the barrier layer includes:
[0088] Using evaporation or PECVD deposition method, at a temperature of 150-300°C and a pressure of 200-750m torr, SiH4, N2O and N2 gases are introduced at flow rates of 10-20 SCCM, 1200-1300 SCCM and 550-650 SCCM, respectively, to form SiO2; and / or,
[0089] By evaporation or PECVD deposition, SiH4, NH3 and N2 gases are introduced at a temperature of 150-300°C and a pressure of 200-750m torr, with flow rates of 10-20 SCCM, 2200-2300 SCCM and 250-350 SCCM respectively, to form SN X and / or,
[0090] The PECVD deposition method is used to form DLC by introducing CH4 at a temperature of 900-1100°C.
[0091] In order to further increase the difficulty of water vapor climbing, the edge of the barrier layer exceeds the edge of the substrate. Since the barrier layer is directly formed on the substrate, if the edge of the barrier layer exceeds the edge of the substrate too much, the barrier layer is easy to break and affect the adhesion between it and the packaging glue. Preferably, the edge of the barrier layer exceeds the edge of the substrate by 1 to 5 μm.
[0092] 2. etching the barrier layer to the surface of the substrate to form a plurality of exposed areas;
[0093] Since the material of the barrier layer of the present invention is greatly different from that of the epitaxial layer, the epitaxial layer cannot be directly formed on the barrier layer. In order to ensure the smooth formation of the epitaxial layer, the barrier layer is etched to expose part of the substrate so that part of the epitaxial layer can be formed on the substrate.
[0094] Specifically, the barrier layer is etched by a dry or wet process to form a plurality of exposed areas on the surface of the substrate, and the plurality of exposed areas are evenly distributed on the substrate.
[0095] Preferably, the total area of the exposed regions accounts for more than 7% of the total area of the substrate, and the exposed regions are evenly distributed. If the exposed regions are too small, the formation of the epitaxial layer will be affected, and the epitaxial layer will not be easy to form a plane.
[0096] In order to further ensure the formation of the epitaxial layer and reduce the lattice mismatch between the epitaxial layer and the substrate, the area of each exposed region accounts for 1 to 15% of the total exposed area. If the area of each exposed region is too small, it is difficult for the epitaxial layer to contact the substrate well. If the area of each exposed region is too large, the contact between the epitaxial layer and the substrate is not uniform. Preferably, the area of each exposed region accounts for 1 to 10% of the total exposed area. More preferably, the area of each exposed region accounts for 2 to 5% of the total exposed area.
[0097] When the substrate is a patterned substrate, the columnar structure must be exposed. The columnar structure is used to increase the contact area between the substrate and the epitaxial layer and improve the lattice quality of the epitaxial layer. Specifically, each exposed area includes a columnar structure, and the area of the exposed columnar structure accounts for 50-90% of the area of each exposed area. If the area of the exposed columnar structure accounts for too small a proportion, the contact area between the substrate and the epitaxial layer will be affected; since the columnar structure is a protruding structure, if the area of the exposed columnar structure accounts for too large a proportion, the bonding force between the substrate and the epitaxial layer will be formed, and the two layers are prone to cracking.
[0098] Preferably, in each exposed region, the area of the exposed columnar structure accounts for 50-80% of the area of each exposed region. More preferably, in each exposed region, the area of the exposed columnar structure accounts for 60-70% of the area of each exposed region.
[0099] Furthermore, the distance between each exposed area is 3-10 μm.
[0100] The present invention sets a barrier layer between the substrate and the epitaxial layer. Due to the material of the barrier layer itself, the epitaxial layer cannot be directly formed on the barrier layer. Therefore, the present invention etches the barrier layer to form an exposed area, and controls the size of the exposed area, the distance between the exposed areas, the area ratio of the exposed areas, and the ratio of the columnar structure in each exposed area, so as to ensure the normal formation of the epitaxial layer and the lattice quality of the epitaxial layer.
[0101] 3. forming an epitaxial layer on the barrier layer and the exposed substrate;
[0102] The epitaxial layer is formed on the barrier layer and the exposed substrate by MOCVD. The epitaxial layer structure of the present invention can be all epitaxial layer structures of existing LED chips, and this application does not make any specific limitation.
[0103] 4. Etching the edge of the epitaxial layer so that the edge of the barrier layer exceeds the edge of the epitaxial layer;
[0104] The edge of the barrier layer exceeds the edge of the epitaxial layer to form a water stop layer to prevent water vapor from climbing to the side wall of the epitaxial layer. The present invention adds a barrier layer between the substrate and the epitaxial layer, and forms a capillary phenomenon in the gap between the die-bonding glue and the packaging glue through the water stop layer. Through the effect of the surface tension of the liquid in the gap and the pressure difference between the inside and outside of the curved surface, water vapor can only stay in the gap and cannot climb to the epitaxial layer.
[0105] Preferably, the edge of the barrier layer exceeds the edge of the epitaxial layer by 5 to 15 μm. Specifically, the present invention achieves the edge of the barrier layer exceeding the edge of the epitaxial layer by etching the edge of the epitaxial layer. If the edge of the barrier layer exceeds the edge of the epitaxial layer by more than 15 μm, the light output area of the outer layer is affected, reducing the light output efficiency of the chip; if the edge of the barrier layer exceeds the edge of the epitaxial layer by less than 5 μm, water vapor can easily climb over the barrier layer to the side wall of the epitaxial layer, thus affecting the blocking effect.
[0106] Preferably, the edge of the barrier layer exceeds the edge of the epitaxial layer by 6-10 μm to match the thickness of the epitaxial layer of 6 μm.
[0107] The present invention will be further described with specific embodiments below.
[0108] Comparative Example 1
[0109] See also Figure 5 , Figure 5 This is an electron microscope photo of the chip of Comparative Example 1, an LED packaging device, comprising a hydrolysis-resistant LED chip 1, a solid crystal adhesive 2 and a packaging adhesive 3, wherein the solid crystal adhesive 2 fixes the LED chip 1 on a substrate 4, and the packaging adhesive 3 wraps the LED chip 1 and covers the solid crystal adhesive 2;
[0110] See also Figure 6 and Figure 7 , Figure 6 yes Figure 5 A in the enlarged view, Figure 7 yes Figure 6 The enlarged view of D in the figure, Figure 6 and Figure 7 It can be seen that cracks occur between the LED chip 1, the die-bonding adhesive 2 and the packaging adhesive 3 in Comparative Example 1, and a large gap exists, which can cause water vapor to invade the chip.
[0111] Figure 8 yes Figure 5 The enlarged view of point B in the figure, Fig. 9 yes Figure 5 The enlarged view of point C in the figure shows Figure 8 and Fig. 9It can be seen that the LED chip 1 includes a substrate 10 and an epitaxial layer, the epitaxial layer includes an n-GaN layer 21, an MQW layer 22 and a p-GaN layer 23, the substrate 10 is a patterned sapphire substrate, which is provided with a columnar structure 11, and the thickness of the epitaxial layer is 6 μm. Water vapor climbs from the gap to the epitaxial layer, and the MQW layer 22 and the p-GaN layer 23 in Comparative Example 1 are corroded and cracked.
[0112] Example 1
[0113] An LED packaging device comprises an LED chip, a bonding adhesive and a packaging adhesive, wherein the bonding adhesive fixes the LED chip on a substrate, and the packaging adhesive wraps the LED chip and covers the bonding adhesive;
[0114] The hydrolysis-resistant LED chip comprises a substrate, a barrier layer arranged on the substrate, and an epitaxial layer arranged on the barrier layer. The barrier layer is provided with a plurality of exposed areas, and the exposed areas are etched to the surface of the substrate. The epitaxial layer is arranged on the barrier layer and the substrate of the exposed areas. The edge of the barrier layer exceeds the edge of the epitaxial layer by 5 to 15 μm. The barrier layer is made of one or more of silicon dioxide, silicon nitride, and diamond-like film.
[0115] Fig.10 Example 1 corresponds to Example 1 Figure 5 An enlarged view of the corresponding position at C is shown. It can be seen from the figure that in the chip of Example 1, the packaging glue 3 wraps the epitaxial layer, and the n-GaN layer 21, MQW layer 22 and p-GaN layer 23 in the epitaxial layer are structurally intact and are not corroded by water vapor or cracked. Therefore, the barrier layer of the present invention effectively prevents water vapor from climbing from the gap to the epitaxial layer.
[0116] The above disclosure is only a preferred embodiment of the present invention, which certainly cannot be used to limit the scope of the present invention. Therefore, equivalent changes made according to the claims of the present invention are still within the scope of the present invention.
Claims
1. A hydrolysis-resistant LED chip, characterized in that: include: substrate; A barrier layer is provided on the substrate, wherein a plurality of exposed regions are provided on the barrier layer, wherein the exposed regions are etched to the surface of the substrate, wherein the total area of the exposed regions accounts for more than 7% of the total area of the substrate, and the area of each exposed region accounts for 1-15% of the total area of the exposed regions, wherein the barrier layer is made of one or more of silicon dioxide, silicon nitride, and a diamond-like film, and wherein the thickness thereof is 300nm-1800nm; An epitaxial layer is arranged on the barrier layer and the exposed area of the substrate; the sidewall of the epitaxial layer is inclined inwardly, and the inclination angle is 30 to 60 degrees; The edge of the barrier layer exceeds the edge of the epitaxial layer by 6-10 μm to form a water stop layer to prevent water vapor from climbing to the side wall of the epitaxial layer; the edge of the barrier layer exceeds the edge of the substrate by 1-5 μm.
2. The hydrolysis-resistant LED chip according to claim 1, characterized in that: The area of each exposed area accounts for 1~10% of the total exposed area.
3. The hydrolysis-resistant LED chip according to claim 1, characterized in that: The substrate is a patterned substrate, and a plurality of columnar structures are arranged on the substrate. Each exposed region includes a columnar structure, and the area of the exposed columnar structure accounts for 50-90% of the area of each exposed region.
4. A hydrolysis-resistant LED device, characterized in that: It comprises the anti-hydrolysis LED chip, the crystal-bonding glue and the packaging glue as described in any one of claims 1 to 3, wherein the crystal-bonding glue fixes the anti-hydrolysis LED chip on the substrate, and the packaging glue wraps the anti-hydrolysis LED chip and covers the crystal-bonding glue.
5. A method for manufacturing a hydrolysis-resistant LED chip as claimed in claim 1, characterized in that: include:
1. forming a barrier layer on the substrate, wherein the barrier layer is made of a light-transmitting non-conductive material; 2. etching the barrier layer to the surface of the substrate to form a plurality of exposed areas, wherein the total area of the exposed areas accounts for more than 7% of the total area of the substrate; 3. forming an epitaxial layer on the barrier layer and the exposed substrate; Fourth, etching the edge of the epitaxial layer so that the edge of the barrier layer exceeds the edge of the epitaxial layer.
6. The method for manufacturing a hydrolysis-resistant LED chip according to claim 5, characterized in that: The method for making the barrier layer comprises: Using an evaporation or PECVD deposition method, at a temperature of 150-300°C and a pressure of 200-750 m torr, SiH4, N2O and N2 gases are introduced at flow rates of 10-20 SCCM, 1200-1300 SCCM and 550-650 SCCM, respectively, to form SiO2; and / or, Using the evaporation or PECVD deposition method, at a temperature of 150~300℃ and a pressure of 200~750m torr, SiH4, NH3 and N2 gases are introduced at flow rates of 10~20SCCM, 2200~2300SCCM and 250~350SCCM respectively to form SN X and / or, The PECVD deposition method is used to form DLC by introducing CH4 at a temperature of 900~1100℃.