Semiconductor device and method for manufacturing semiconductor device

By setting a resin layer with a low dielectric constant on the SOI substrate and optimizing the process, the problem of parasitic capacitance is solved, the high-frequency characteristics and heat dissipation of semiconductor devices are improved, and the cheap and efficient characteristics are improved.

CN111742404BActive Publication Date: 2024-12-06MURATA MFG CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN201980014439.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2018-02-20
Filing Date
2019-02-12
Publication Date
2024-12-06
Estimated Expiration
2039-02-12

AI Technical Summary

Technical Problem

In the SOI substrate, the parasitic capacitance and charge accumulation layer between the semiconductor layer and the insulating layer affect the high-frequency characteristics and heat dissipation of the semiconductor device, resulting in limited improvement in characteristics.

Method used

By providing a first resin layer on the back of the circuit substrate, covering the semiconductor element and grinding and etching, a recess is formed to reduce parasitic capacitance, and a resin material with a low dielectric constant is used to reduce capacitance, thereby improving the mounting strength and heat dissipation of the component. .

Benefits of technology

The high-frequency characteristics and heat dissipation of semiconductor devices are improved, cost reduction, manufacturing processes are simplified, yield improvements are improved, and durability of components is enhanced.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111742404B_ABST
    Figure CN111742404B_ABST
Patent Text Reader

Abstract

The present invention provides a semiconductor device capable of improving characteristics and a method for manufacturing the semiconductor device. The semiconductor device comprises: a substrate having a first surface and a second surface located on the opposite side of the first surface; a first element arranged on the first surface side; and a first resin layer arranged on the first surface side and arranged around the first element in a top view. The substrate has a wiring layer. The first element has a semiconductor layer, an electrode portion located on the surface side of the semiconductor layer opposite to the substrate, and an insulating layer located on the opposite side of the electrode portion across the semiconductor layer. The electrode portion is connected to the wiring layer. The height of the first resin layer from the first surface is higher than the height of the first element from the first surface.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. Background Art

[0002] A SOI (Silicon on Insulator) substrate including a semiconductor layer, an insulating layer, and a support substrate is known. A semiconductor device in which a MOS transistor or the like is provided on the semiconductor layer of the SOI substrate is known (for example, refer to Patent Document 1).

[0003] Patent Document 1: International Publication No. 2011 / 008894

[0004] In an SOI substrate, parasitic capacitance is generated between the semiconductor layer and the support substrate via an insulating layer. In addition, in an SOI substrate, a charge accumulation layer may exist at the interface between the semiconductor layer and the insulating layer. Due to the above-mentioned parasitic capacitance or electric field accumulation layer, it is possible to hinder the improvement of the characteristics of the semiconductor device. Summary of the invention

[0005] The present invention has been made in view of the above, and an object of the present invention is to provide a semiconductor device and a method for manufacturing a semiconductor device capable of improving characteristics.

[0006] A semiconductor device involved in one embodiment comprises: a substrate having a first surface and a second surface located on the opposite side of the above-mentioned first surface; a first element is arranged on the side of the above-mentioned first surface; and a first resin layer is arranged on the side of the above-mentioned first surface and is arranged around the above-mentioned first element in a top view, the above-mentioned substrate has a wiring layer, and the above-mentioned first element has: a semiconductor layer; an electrode portion located on the surface side of the above-mentioned semiconductor layer opposite to the above-mentioned substrate; and an insulating layer located on the opposite side of the above-mentioned electrode portion across the above-mentioned semiconductor layer, the above-mentioned electrode portion is connected to the above-mentioned wiring layer, and the height of the above-mentioned first resin layer from the above-mentioned first surface is higher than the height of the above-mentioned first element from the above-mentioned first surface.

[0007] A method for manufacturing a semiconductor device involved in one embodiment is a method for manufacturing a semiconductor device using an element, wherein the element comprises: a supporting substrate, an insulating layer arranged on one surface side of the supporting substrate, a semiconductor layer arranged on the opposite side of the supporting substrate with the insulating layer interposed therebetween, and an electrode portion arranged on the opposite side of the insulating layer with the semiconductor layer interposed therebetween, wherein the method for manufacturing the semiconductor device comprises: a step of connecting the electrode portion to a wiring layer of the substrate by making the semiconductor layer face the first surface of the substrate; a step of forming a first resin layer on the first surface side of the substrate to cover the element; a step of grinding the first resin layer to expose the supporting substrate; and a step of etching and removing the supporting substrate exposed from the first resin layer.

[0008] According to the present invention, it is possible to provide a semiconductor device and a method for manufacturing the semiconductor device that can improve characteristics. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] Figure 1 It is a plan view showing a configuration example of the semiconductor device according to the first embodiment.

[0010] Figure 2 The section is made at the II-II' line. Figure 1 A cross-sectional view of the top view is shown.

[0011] Figure 3 The diagram is a cross-sectional view showing the method for manufacturing the semiconductor device according to the first embodiment in order of steps.

[0012] Figure 4 The diagram is a cross-sectional view showing the method for manufacturing the semiconductor device according to the first embodiment in order of steps.

[0013] Figure 5 The cross-sectional views are shown in order of steps in a method for manufacturing a semiconductor device according to Modification 1 of Embodiment 1.

[0014] Figure 6 It is a cross-sectional view showing a semiconductor device and a method for manufacturing the same according to a second variation of the first embodiment.

[0015] Figure 7 It is a cross-sectional view showing a semiconductor device and a method for manufacturing the same according to Modification 3 of Embodiment 1.

[0016] Figure 8 This is a cross-sectional view showing a semiconductor device according to Modification 4 of Embodiment 1.

[0017] Fig. 9 This is a cross-sectional view showing a semiconductor device according to Modification 5 of Embodiment 1.

[0018] Fig.10 It is a cross-sectional view showing a configuration example of a semiconductor device according to the second embodiment.

[0019] Fig.11 It is a cross-sectional view showing the method for manufacturing the semiconductor device according to the second embodiment in order of steps.

[0020] Fig.12 It is a cross-sectional view showing the method for manufacturing the semiconductor device according to the second embodiment in order of steps. DETAILED DESCRIPTION

[0021] Hereinafter, the mode (implementation method) for implementing the present invention will be described in detail with reference to the accompanying drawings. In addition, the present invention is not limited by the contents described in the following implementation methods. In addition, the constituent elements described below include contents that can be easily thought of by those skilled in the art, and substantially the same contents. Moreover, the constituent elements described below can be appropriately combined. In addition, in this specification and each figure, the same figure mark is attached to the same elements as the elements related to the already described figures and have been described, and the detailed description is sometimes appropriately omitted.

[0022] (Implementation Method 1)

[0023] Figure 1 It is a plan view showing a configuration example of the semiconductor device according to the first embodiment. Figure 2 The section is made at the II-II' line. Figure 1 The semiconductor device 100 is a semiconductor device for high frequency use that amplifies and outputs a high frequency input signal. For example, the semiconductor device 100 is a transmission unit used in a mobile communication device such as a mobile phone to transmit various signals such as voice and data to a base station. Figure 1 as well as Figure 2 As shown, the semiconductor device 100 involved in embodiment 1 includes a circuit substrate 1, multiple external connection terminals 5, a first resin layer 7, a second resin layer 9, a first semiconductor element 10, a second semiconductor element 50, a first surface mounted component (hereinafter referred to as SMD (Surface Mount Device) component) 60 and a second SMD component 70.

[0024] The circuit substrate 1 is a substrate formed of a dielectric material and a metal, for example, a glass epoxy resin substrate having a wiring layer 3. The circuit substrate 1 has a surface 1a and a back surface 1b located on the opposite side of the surface 1a. In the present disclosure, the back surface 1b is sometimes referred to as the first surface and the surface 1a is sometimes referred to as the second surface. The wiring layer 3 includes a first wiring layer 3a provided on the surface 1a, a second wiring layer 3b provided on the back surface 1b, and a third wiring layer 3c provided between the surface 1a and the back surface 1b. The third wiring layer 3c can be a single layer or a multilayer. A portion of the first wiring layer 3a is connected to a portion of the second wiring layer 3b via the third wiring layer 3c.

[0025] The first semiconductor element 10 is surface mounted on the back surface 1b side of the circuit substrate 1. In the present disclosure, the first semiconductor element 10 is sometimes referred to as the first element. The first semiconductor element 10 has a semiconductor layer 11, an insulating layer 12, and a bump electrode 15. An integrated circuit (IC) is provided in the semiconductor layer 11. The integrated circuit is composed of active elements such as transistors, and passive elements such as resistors and capacitors. The semiconductor layer 11 is, for example, a single crystal silicon layer (Si). The semiconductor layer 11 is called an active layer. The insulating layer 12 is provided on the opposite side of the surface of the semiconductor layer 11 that is opposite to the bump electrode 15. That is, the insulating layer 12 is located on the opposite side of the bump electrode 15 across the semiconductor layer 11. The insulating layer 12 is an oxide of the semiconductor constituting the semiconductor layer 11, for example, a silicon oxide film (SiO2). The insulating layer 12 is also referred to as a BOX layer.

[0026] The bump electrode 15 is located between the semiconductor layer 11 and the circuit substrate 1, and is connected to the second wiring layer 3b of the circuit substrate 1. The bump electrode 15 is used to input power or signals from the circuit substrate 1 to the first semiconductor element 10. In addition, the bump electrode 15 is also used to output signals from the first semiconductor element 10 to the circuit substrate 1. The bump electrode 15 is made of a metal material such as solder.

[0027] As will be described later, the first semiconductor element 10 is formed by removing the supporting substrate 13 (see Figure 3 ). Thus, the thickness of the first semiconductor element 10 is thinner than the thickness of the second semiconductor element 50. Therefore, the first semiconductor element 10 can also be called a thin-layer semiconductor element.

[0028] The external connection terminal 5 is mounted on the back surface 1b side of the circuit substrate 1 and is connected to the second wiring layer 3b of the back surface 1b of the circuit substrate 1. The external connection terminal 5 includes a metal layer 51 and a plating layer 52 covering the metal layer 51. For example, the metal layer 51 is made of copper (Cu). The plating layer 52 has a structure in which nickel (Ni) and gold (Au) are stacked in this order from the metal layer 51 side.

[0029] The first resin layer 7 is provided on the back surface 1b side of the circuit substrate 1. The first resin layer 7 surrounds the first semiconductor element 10 without a gap. For example, when viewed from above, the first resin layer 7 surrounds the first semiconductor element 10 without a gap. In addition, the first resin layer 7 is in close contact with the entire side surface 10s of the first semiconductor element 10. Thus, the first semiconductor element 10 is supported from all sides by the first resin layer 7. In addition, the semiconductor layer 11 of the first semiconductor element 10 is sealed by the first resin layer 7. In addition, in this specification, viewing from above means observing from the normal direction of the back surface 1b of the circuit substrate 1.

[0030] In addition, the first resin layer 7 surrounds the plurality of external connection terminals 5 without gaps. For example, in a plan view, the first resin layer 7 surrounds the external connection terminals 5 without gaps. In addition, the first resin layer 7 is in close contact with the side surfaces 5s of the external connection terminals 5. Thus, the external connection terminals 5 are supported by the first resin layer 7 from the periphery.

[0031] In addition, the first resin layer 7 is filled between the first semiconductor element 10 and the circuit substrate 1, and covers the side surface of the bump electrode 15. Thus, the first semiconductor element 10 is also supported from the circuit substrate 1 side by the first resin layer 7. The first resin layer 7 is composed of a low dielectric constant material having a relative dielectric constant of 4 or less. For example, the first resin layer 7 is a thermosetting epoxy resin.

[0032] Hereinafter, the portion of the first resin layer 7 located around the first semiconductor element 10 is also referred to as a resin dam. Figure 2 As shown, the surface (hereinafter, upper surface) 12 b of the insulating layer 12 opposite to the surface facing the circuit board 1 and the plating layer 52 of the external connection terminal 5 are exposed from the resin dam.

[0033] The height of the first semiconductor element 10 from the back surface 1b is set to T10, the height of the resin dam from the back surface 1b is set to T7, and the height of the external connection terminal 5 from the back surface 1b is set to T5. The height T7 of the resin dam from the back surface 1b is higher than the height T10 of the first semiconductor element 10 from the back surface 1b. In addition, the height T5 of the external connection terminal 5 from the back surface 1b is the same as or higher than the height T7 of the resin dam from the back surface 1b. In other words, in this embodiment, the magnitude relationship of the heights T10, T7, and T5 is T10<T7≤T5.

[0034] According to the above-mentioned size relationship, a recess (depression) H1 surrounded by the resin dam exists in the first resin layer 7. At the bottom of the recess H1, the upper surface 12b of the insulating layer 12 is exposed. For example, the bottom surface of the recess H1 becomes the upper surface 12b of the insulating layer 12. In addition, the plating layer 52 of the external connection terminal 5 is flush with the resin dam or protrudes from the resin dam.

[0035] like Figure 2As shown, the second semiconductor element 50 is surface mounted on the surface 1a side of the circuit substrate 1. In the present disclosure, the second semiconductor element 50 is sometimes referred to as a second element. The second semiconductor element 50 has a semiconductor substrate 55 and a bump electrode 56. The semiconductor substrate 55 is, for example, a single crystal Si substrate, and is provided with an integrated circuit. The bump electrode 56 is located between the semiconductor substrate 55 and the circuit substrate 1, and is connected to the first wiring layer 3a of the circuit substrate 1. The bump electrode 56 is used for power input or signal input from the circuit substrate 1 to the second semiconductor element 50. In addition, the bump electrode 56 is also used for signal output from the second semiconductor element 50 to the circuit substrate 1. The bump electrode 56 is made of, for example, a metal material such as solder.

[0036] The first SMD component 60 and the second SMD component 70 are respectively mounted on the surface 1a side of the circuit substrate 1. In the present disclosure, at least one of the first SMD component 60 and the second SMD component 70 is sometimes referred to as a second element. The first SMD component 60 and the second SMD component 70 are respectively electronic components, and their types are not particularly limited. For example, the first SMD component 60 and the second SMD component 70 are respectively discrete semiconductors. As discrete semiconductors, capacitors, transistors, diodes, MOSFETs (Metal Oxide Semiconductor Field Effect Transistors), IGBTs (Insulated Gate Bipolar Transistors), etc. are exemplified. Alternatively, the first SMD component 60 and the second SMD component 70 may also be capacitor elements or resistor elements, respectively. In addition, the first SMD component 60 and the second SMD component 70 are not limited to Si-based semiconductor devices. The first SMD component 60 and the second SMD component 70 may be compound-based semiconductor devices, or may be electronic components of a MEMS sensor system. In addition, the first SMD component 60 and the second SMD component 70 may also be an Integrated passive Device (IPD).

[0037] The second resin layer 9 is provided on the surface 1a side of the circuit substrate 1. The second resin layer 9 covers the second semiconductor element 50, the first SMD component 60, and the second SMD component 70. The second resin layer 9 is made of a low dielectric constant material having a relative dielectric constant of 4 or less. For example, the second resin layer 9 is a thermosetting epoxy resin.

[0038] Figure 1 as well as Figure 2 The semiconductor device 100 shown is mounted on a substrate (not shown) etc. For example, with the back surface 1 b of the circuit board 1 facing the substrate (not shown), the external connection terminals 5 of the semiconductor device 100 are bonded to a wiring layer of the substrate (not shown).

[0039] Next, Figure 1 as well as Figure 2 A method for manufacturing the semiconductor device 100 shown will be described. Figure 3 as well as Figure 4 1 is a cross-sectional view showing the method for manufacturing a semiconductor device according to Embodiment 1 in order of steps. Figure 3 as well as Figure 4 As shown, the semiconductor device 100 according to the first embodiment is completed through each process of steps ST1 to ST6. Figure 3 as well as Figure 4 In the following Figure 5 to Figure 12 In the figure, the wiring layer 3 included in the circuit board 1 is omitted from illustration.

[0040] exist Figure 3 In step ST1, a manufacturing device (not shown) forms an external connection terminal 5 on the back surface 1b of the circuit substrate 1. In the present disclosure, the method for forming the external connection terminal 5 is not particularly limited. For example, the manufacturing device forms a metal layer 51 by disposing a mask (not shown) on the back surface 1b of the circuit substrate 1 and printing or plating a conductive member such as copper (Cu) in the area exposed from the mask. After forming the metal layer 51, the manufacturing device removes the mask from the back surface 1b of the circuit substrate 1.

[0041] Next, the manufacturing device mounts the first semiconductor element 10A on the back surface 1b of the circuit substrate 1 (step ST2). The first semiconductor element 10A has a supporting substrate 13, an insulating layer 12, a semiconductor layer 11, and a bump electrode 15. The insulating layer 12 is arranged on one side of the supporting substrate 13. The semiconductor layer 11 is arranged on the opposite side of the supporting substrate 13 across the insulating layer 12. The bump electrode 15 is arranged on the opposite side of the insulating layer 12 across the semiconductor layer 11. For example, the supporting substrate 13, the insulating layer 12, and the semiconductor layer 11 constitute an SOI (Silicon on Insulator) substrate. The supporting substrate 13 is a single crystal Si substrate, and the insulating layer 12 is a silicon oxide film. The semiconductor layer 11 is, for example, an extremely thin single crystal silicon layer formed by bonding Si wafers covered with oxide films to each other, smart cutting technology, high-precision grinding and polishing technology, and the like.

[0042] Next, the manufacturing device forms a first resin layer 7 on the back surface 1b side of the circuit substrate 1. For example, the manufacturing device forms the first resin layer 7 by transfer molding technology. As a result, the first semiconductor element 10A and the metal layer 51 are covered and sealed by the first resin layer 7. At this time, the first resin layer 7 is also filled between the first semiconductor element 10A and the circuit substrate 1.

[0043] Next, the manufacturing device grinds the surface of the first resin layer 7 so that the support substrate 13 and the metal layer 51 are exposed from the first resin layer 7 (step ST3). The manufacturing device used for this grinding is, for example, a thinning machine having a grinding tool. The thinning machine grinds the surface of the first resin layer 7 by causing the grinding tool to rotate relative to the first resin layer 7. In addition, the grinding of the first resin layer 7 is not limited to the method using the thinning machine. For example, the grinding of the first resin layer 7 can also be performed by CMP (Chemical Mechanical Polishing).

[0044] Next, the manufacturing device forms a mask M1 on the supporting substrate 13 (step ST4). The mask M1 is, for example, a resin material. The surface of the supporting substrate 13 exposed from the first resin layer 7 is entirely covered by the mask M1. Next, the manufacturing device forms a plating layer 52 by plating the metal layer 51 with metal. For example, the manufacturing device sequentially plates Ni and Au in a state where the supporting substrate 13 is covered by the mask M1 and the metal layer 51 is exposed from the mask M1. Thus, the plating layer 52 is plated only on the metal layer 51, and the external connection terminal 5 having the metal layer 51 and the plating layer 52 is completed. After forming the plating layer 52, the manufacturing device removes the mask M1 from the supporting substrate 13.

[0045] Next, the manufacturing apparatus etches and removes the support substrate 13 under the condition that the support substrate 13 is more easily etched than the first resin layer 7 and the insulating layer 12 (step ST5). Thus, the manufacturing apparatus forms the first semiconductor element 10 in which the support substrate 13 is removed from the first semiconductor element 10A, and forms the recess H1 in the first semiconductor element 10.

[0046] In addition, in order to minimize the damage to the insulating layer 12 as the base, the etching of the supporting substrate 13 is preferably performed by wet etching. In this case, the etching solution is selected to have a reagent and a liquid temperature that selectively stop etching at the insulating layer 12. For example, as an etching solution, a TMAH (tetramethylammonium hydroxide) aqueous solution is listed. The TMAH aqueous solution with a concentration of 10 mass % (wt%) and a liquid temperature of 80°C uses the insulating layer Si composed of SiO2 as an etching stop layer, and can only etch the supporting substrate 13 composed of Si. The above-mentioned TMAH aqueous solution will not etch the first resin layer 7, the plating layer 52 and the metal layer 51, nor will it corrode the first resin layer 7, the plating layer 52 and the metal layer 51.

[0047] Next, the manufacturing device mounts the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 on the surface 1a side of the circuit substrate 1 (step ST6). Next, the manufacturing device forms a second resin layer 9 on the surface 1a side of the circuit substrate 1. For example, the manufacturing device forms the second resin layer 9 by transfer molding technology. As a result, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 are covered and sealed by the second resin layer 9. Thereafter, the manufacturing device Figure 4 As shown by the dotted line, the surface of the second resin layer 9 is ground to adjust the final thickness of the semiconductor device 100. After the above steps, the semiconductor device 100 is completed.

[0048] As described above, the semiconductor device 100 according to the first embodiment includes the circuit substrate 1, the first semiconductor element 10 provided on the back surface 1b side of the circuit substrate 1, and the first resin layer 7 provided on the back surface 1b side of the circuit substrate 1 and surrounding the first semiconductor element 10. Figure 1 As shown, in a plan view, the first resin layer 7 is provided around the first semiconductor element 10 above the circuit substrate 1. The circuit substrate 1 has a wiring layer 3. The first semiconductor element 10 has a semiconductor layer 11, a bump electrode 15 located on the surface side of the semiconductor layer 11 facing the circuit substrate 1, and an insulating layer 12 located on the opposite side of the bump electrode 15 across the semiconductor layer 11. The bump electrode 15 is connected to the wiring layer 3. The height T7 of the first resin layer 7 from the back surface 1b is higher than the height T10 of the first semiconductor element 10 from the back surface 1b.

[0049] Accordingly, a recess H1 surrounded by the resin dam exists on the first semiconductor element 10. An air layer can be arranged in the recess H1. Thus, since the semiconductor device 100 can reduce the parasitic capacitance of the semiconductor layer 11, the high-frequency characteristics of the first semiconductor element 10 can be improved. In addition, the heat generated by the first semiconductor element 10 is diffused to the air layer via the insulating layer 12. Therefore, the semiconductor device 100 can improve the heat dissipation of the first semiconductor element 10.

[0050] Here, the technology compared with the present embodiment is described. Generally speaking, a semiconductor device for high-frequency use has an active layer that forms a transistor, and a supporting substrate that supports the active layer. The resistivity and dielectric constant of the supporting substrate affect the high-frequency characteristics of the semiconductor device. For example, the resistivity and dielectric constant of the supporting substrate hinder the improvement of the high-frequency characteristics of the semiconductor device, and also become an important factor in the degradation of the high-frequency characteristics. In order to reduce such an influence, a method of inserting an SOI substrate with a low dielectric constant insulating layer (SiO2) between the active layer and the supporting substrate, or a method of using a high-resistance substrate of 1kΩ·cm for the supporting substrate is considered. However, in these methods, the substrate is expensive. In addition, a method of further thickening the insulating layer in the SOI substrate, or making the supporting substrate highly resistive to 10kΩ·cm, or inserting a trap-rich layer at the interface between the insulating layer and the supporting substrate is also considered. However, these methods are expensive technologies with increased difficulty or increased working hours.

[0051] In contrast, the semiconductor device 100 according to the present embodiment has a structure that can be realized by common mass production techniques of semiconductor devices such as surface mounting (flip-chip mounting), resin sealing, grinding, and etching. Therefore, the semiconductor device 100 can achieve improved high-frequency characteristics at low cost.

[0052] In addition, in the semiconductor device according to the present embodiment, before the first semiconductor element 10A, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 are mounted on the circuit substrate 1, each of these elements and components can be subjected to a probe inspection or an appearance inspection in advance. Thus, only the first semiconductor element 10A, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 that are judged to be qualified by the probe inspection or the appearance inspection can be mounted on the circuit substrate 1. Thus, the yield rate of the semiconductor device 100 can be improved, and the cost reduction of the semiconductor device 100 can be contributed.

[0053] In addition, the first semiconductor element 10 is surrounded by a resin dam that is higher than the first semiconductor element 10 from the back surface 1b. Thus, the resin dam can protect the first semiconductor element 10 from contact or collision with an external substrate or external equipment, and can prevent damage to the first semiconductor element 10. For example, the resin dam can prevent scratches from entering the first semiconductor element 10, and can reduce the possibility of microcracks or chip breakage caused by scratches in the first semiconductor element 10.

[0054] In addition, in the first semiconductor element 10, the semiconductor layer 11 is covered with the insulating layer 12. Thus, the insulating layer 12 can prevent metals (e.g., Cu, Fe, etc.) that easily diffuse in silicon materials from contacting the semiconductor layer 11. Therefore, the first semiconductor element 10 can prevent the high-frequency characteristics from changing due to contact with the above-mentioned metals.

[0055] The resin dam is in close contact with the side surface 10s of the first semiconductor element 10. Thus, the resin dam can surround the first semiconductor element 10 without a gap. Thus, the resin dam can support the circuit substrate 1 from the side and can improve the strength of mounting the first semiconductor element 10 relative to the circuit substrate 1 (hereinafter referred to as element strength). In addition, the resin dam is in close contact with the side surface 10s of the first semiconductor element 10, thereby preventing the intrusion of liquid or the like from the outside of the first semiconductor element 10 to the inside (for example, the semiconductor layer 11).

[0056] The first resin layer 7 is filled between the first semiconductor element 10 and the circuit board 1. Thus, the first resin layer 7 can improve the adhesion between the first semiconductor element 10 and the circuit board 1, and thus the element strength can be further improved.

[0057] The relative dielectric constant of the first resin layer 7 is not more than 4. Accordingly, the semiconductor device 100 can suppress the parasitic capacitance between the first semiconductor element 10 and the first resin layer 7 to be low.

[0058] The first resin layer 7 is a thermosetting resin. Accordingly, as the material of the first resin layer 7, a material that is a fluid such as a liquid during filling and is cured by heat treatment afterwards can be used. For example, a thermosetting epoxy resin can be used as the first resin layer 7. The manufacturing device can form the first resin layer 7 by transfer molding technology, and can easily make the first resin layer 7 close to the side of the first semiconductor element 10, or fill the first resin layer 7 between the first semiconductor element 10 and the circuit substrate 1.

[0059] The semiconductor device 100 further includes an external connection terminal 5 provided on the back surface 1b side of the circuit substrate 1. A height T5 of the external connection terminal 5 from the back surface 1b is the same as or higher than a height T7 of the resin dam from the back surface 1b. Thus, the semiconductor device 100 can be surface mounted on an external substrate in a state where the back surface 1b side of the circuit substrate 1 faces the external substrate.

[0060] The semiconductor device 100 further includes a second semiconductor element 50, a first SMD component 60, and a second SMD component 70 provided on the surface 1a side of the circuit substrate 1, and a second resin layer 9 provided on the surface 1a side of the circuit substrate 1 and covering the second semiconductor element 50, the first SMD component 60, and the second SMD component 70. Accordingly, the surface 1a side of the circuit substrate 1 also becomes a component mounting area. Therefore, the semiconductor device 100 can increase the mounting density of components in the circuit substrate 1.

[0061] The method for manufacturing a semiconductor device according to the first embodiment uses a first semiconductor element 10A, which includes a support substrate 13, an insulating layer 12 provided on one surface side of the support substrate 13, a semiconductor layer 11 provided on the opposite side of the support substrate 13 via the insulating layer 12, and a bump electrode 15 provided on the opposite side of the insulating layer 12 via the semiconductor layer 11. The method for manufacturing a semiconductor device according to the first embodiment includes: a step of making the semiconductor layer 11 face the back surface 1b of the circuit substrate 1 and connecting the bump electrode 15 to the wiring layer 3 of the circuit substrate 1; a step of forming a first resin layer 7 on the back surface 1b side of the circuit substrate 1 to cover the first semiconductor element 10A; a step of grinding the first resin layer 7 to expose the support substrate 13; and a step of etching and removing the support substrate 13 exposed from the first resin layer 7.

[0062] Thus, the manufacturing apparatus can form the first semiconductor element 10 from the first semiconductor element 10A. In addition, the manufacturing apparatus can form the recess H1 in the first semiconductor element 10 and form the first resin layer 7 in a dam shape surrounding the first semiconductor element 10 and the recess H1.

[0063] In addition, the etching area of ​​the support substrate 13 is determined in a self-matching manner by grinding the first resin layer 7 by the manufacturing device to expose the surface of the support substrate 13. A mask is arranged around the support substrate 13 to determine the etching area, so there is no positional deviation of the mask relative to the etching area. Therefore, the manufacturing device can form the recess H1 with a small number of steps and good position accuracy relative to the first semiconductor element 10. In addition, when forming the recess H1, the insulating layer 12 under the support substrate 13 acts as an etching stopper. Therefore, the depth of the recess H1 is automatically determined according to the thickness of the support substrate 13 before etching. It is easy to control the depth of the recess H1.

[0064] The resistivity of the support substrate 13 is less than 1 kΩ·cm. The support substrate 13 may be a Si substrate having a resistivity less than 1 kΩ·cm. Thus, the manufacturing apparatus can use a relatively cheap general-purpose SOI substrate to manufacture the semiconductor device 100. This can help reduce the manufacturing cost of the semiconductor device 100.

[0065] (Variant 1)

[0066] In the above-mentioned first embodiment, after the recess H1 is formed, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 are mounted on the surface 1a side of the circuit substrate 1. However, in this embodiment, the process sequence for manufacturing the semiconductor device 100 is not limited to the above. For example, the recess H1 may be formed after the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 are mounted.

[0067] Figure 5 1 is a cross-sectional view showing a method for manufacturing a semiconductor device according to a first variation of the first embodiment in order of steps. Figure 5 In step ST11, the manufacturing apparatus forms a metal layer 51 on the back side 1b of the circuit substrate 1. Next, the manufacturing apparatus mounts the first semiconductor element 10A on the back side 1b of the circuit substrate 1. Next, the manufacturing apparatus forms a first resin layer 7 on the back side 1b of the circuit substrate 1. Next, the manufacturing apparatus mounts the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 on the surface 1a of the circuit substrate 1. Thereafter, the manufacturing apparatus forms a second resin layer 9 on the surface 1a of the circuit substrate 1.

[0068] Next, the manufacturing device grinds the surface of the first resin layer 7 to expose the support substrate 13 and the metal layer 51 from the first resin layer 7 (step ST12). Next, the manufacturing device forms a mask M1 on the support substrate 13. Next, the manufacturing device forms a plated layer 52 by plating the metal layer 51 with metal. After forming the plated layer 52, the manufacturing device removes the mask M1 from the support substrate 13.

[0069] Next, the manufacturing apparatus etches and removes the support substrate 13 under conditions that make it easier to etch the support substrate 13 than the first resin layer 7 and the insulating layer 12. Thus, the manufacturing apparatus forms the first semiconductor element 10 by removing the support substrate 13 from the first semiconductor element 10A, and forms the recess H1 in the first semiconductor element 10. Thereafter, the manufacturing apparatus grinds the surface of the second resin layer 9 to adjust the final thickness of the semiconductor device 100.

[0070] Even in such a method, the manufacturing apparatus can form the semiconductor device 100 involved in Embodiment 1. In addition, in the mounting process of the second semiconductor element 50, the first SMD component 60, and the second SMD component 70, and the forming process of the second resin layer 9, the insulating layer 12 is covered by the supporting substrate 13. Therefore, in the manufacturing method involved in this modification 1, it is possible to include the second resin layer 9 in the mounting process of the first SMD component 60 and the second SMD component 70 and the forming process of the second resin layer 9 without damaging it.

[0071] (Variant 2)

[0072] In the above-mentioned first embodiment, the external connection terminals 5 are provided on the back surface 1b side of the circuit board 1. However, in the present embodiment, the external connection terminals 5 may not be provided on the back surface 1b side of the circuit board 1.

[0073] Figure 6 1 is a cross-sectional view showing a semiconductor device according to a second variation of the first embodiment and a method for manufacturing the same. Figure 6 As shown, in the semiconductor device 100A according to the second modification of the first embodiment, the external connection terminals 5 are not provided on the back surface 1b of the circuit board 1. The method for manufacturing the semiconductor device 100A is similar to that of the first embodiment except for the step of forming the external connection terminals 5. Figure 5 The manufacturing method of the semiconductor device 100 shown is the same.

[0074] Specifically, in Figure 6 In step ST21, the manufacturing device mounts the first semiconductor element 10A on the back side 1b of the circuit substrate 1. Next, the manufacturing device forms the first resin layer 7 on the back side 1b of the circuit substrate 1. Next, the manufacturing device mounts the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 on the front side 1a of the circuit substrate 1. Thereafter, the manufacturing device forms the second resin layer 9 on the front side 1a of the circuit substrate 1.

[0075] Next, the manufacturing device grinds the surface of the first resin layer 7 to expose the support substrate 13 from the first resin layer 7 (step ST22). Next, the manufacturing device etches and removes the support substrate 13 under the condition that the support substrate 13 is easier to etch than the first resin layer 7 and the insulating layer 12. Thus, the manufacturing device forms the first semiconductor element 10 in which the support substrate 13 is removed from the first semiconductor element 10A, and forms the recess H1 on the first semiconductor element 10. Thereafter, the manufacturing device grinds the surface of the second resin layer 9 to adjust the final thickness of the semiconductor device 100. After the above steps, the semiconductor device 100A is completed.

[0076] Similar to the semiconductor device 100 described above, the semiconductor device 100A also has a recess H1 on the first semiconductor element 10. Thus, the semiconductor device 100A can improve the high-frequency characteristics of the first semiconductor element 10. In addition, in the semiconductor device 100A, the first semiconductor element 10 is also surrounded by the resin dam. Thus, the resin dam can protect the first semiconductor element 10 from contact or collision with an external substrate or external equipment, and can prevent the first semiconductor element 10 from being damaged.

[0077] Although not shown in the drawings, in the present embodiment, external connection terminals may be provided on at least one of the surface 1 a side of the circuit board 1 and the side surface side of the circuit board 1 .

[0078] (Variant 3)

[0079] In the first embodiment, SMD components or semiconductor elements may be provided on the back surface 1b of the circuit board 1. Furthermore, the SMD components or semiconductor elements may be covered by the resin dam. In other words, the SMD components or semiconductor elements may be built inside the resin dam.

[0080] Figure 7 1 is a cross-sectional view showing a semiconductor device 100B according to a third variation of the first embodiment and a method for manufacturing the same. Figure 7 As shown, in the semiconductor device 100B according to the third variation of the first embodiment, a third semiconductor element 80 is mounted on the back surface 1b of the circuit substrate 1. The third semiconductor element 80 has a semiconductor substrate 85 and a bump electrode 86 similarly to the second semiconductor element 50. In the present disclosure, the third semiconductor element 80 is sometimes referred to as a third element. The semiconductor substrate 85 is, for example, a single crystal Si substrate, and is provided with an integrated circuit. The bump electrode 86 is located between the semiconductor substrate 85 and the circuit substrate 1, and is connected to the second wiring layer 3b (refer to Figure 2 )connect.

[0081] In addition, in the semiconductor device 100B, a third SMD component 90 is mounted on the back side 1b of the circuit substrate 1. The third SMD component 90 is an electronic component, and its type is not particularly limited. In the present disclosure, the third SMD component 90 is sometimes referred to as a third element. For example, the third SMD component 90 is a discrete semiconductor, a capacitor element, or a resistor element. In addition, the third SMD component 90 is not limited to a Si-based semiconductor device. The third SMD component 90 can be a compound-based semiconductor device or an electronic component of a MEMS sensor system. In addition, the third SMD component 90 can also be an Integrated passive Device (IPD).

[0082] In the semiconductor device 100B, the height T10 of the first semiconductor element 10 (see Figure 2 ) is lower than the height T80 of the third semiconductor element 80 and lower than the height T90 of the third SMD component 90. In other words, the first semiconductor element 10 is a thin-layer semiconductor element thinner than the third semiconductor element 80 and the third SMD component 90.

[0083] The manufacturing method of the semiconductor device 100B is similar to the method of manufacturing the semiconductor device 100B except for the steps of mounting the third semiconductor element 80 and the third SMD component 90. Figure 6 The manufacturing method of the semiconductor device 100A shown in FIG. Figure 7 In step ST31 , the manufacturing apparatus mounts the first semiconductor element 10A, the third semiconductor element 80 , and the third SMD component 90 on the back surface 1 b side of the circuit board 1 .

[0084] The height of the first semiconductor element 10A from the back surface 1b is set to T10A, the height of the third semiconductor element 80 from the back surface 1b is set to T80, and the height of the third SMD component 90 from the back surface 1b is set to T90. The height T10A of the first semiconductor element 10A from the back surface 1b is higher than the height T80 of the third semiconductor element 80 from the back surface 1b. In addition, the height T10A of the first semiconductor element 10A from the back surface 1b is higher than the height T90 of the third SMD component 90 from the back surface 1b. In other words, in this embodiment, the magnitude relationship of the heights T10A, T80, and T90 is T10A>T80, and T10A>T90. In addition, the heights T80 and T90 may be the same value or different values.

[0085] Next, the manufacturing apparatus forms a first resin layer 7 on the back surface 1b side of the circuit substrate 1. Thus, the first semiconductor element 10A, the third semiconductor element 80, and the third SMD component 90 are covered with the first resin layer 7. Next, the manufacturing apparatus mounts the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 on the front surface 1a side of the circuit substrate 1, respectively. Thereafter, the manufacturing apparatus forms a second resin layer 9 on the front surface 1a side of the circuit substrate 1.

[0086] Next, the manufacturing apparatus grinds the surface of the first resin layer 7 to expose only the support substrate 13 from the first resin layer 7 (step ST32). As described above, since T10A>T80 and T10A>T90, the manufacturing apparatus can stop grinding in a state where the support substrate 13 is exposed and the third semiconductor element 80 and the third SMD component 90 are not exposed.

[0087] Next, the manufacturing device etches and removes the support substrate 13 under the condition that the support substrate 13 is easier to etch than the first resin layer 7 and the insulating layer 12. As mentioned above, the etching liquid uses a TMAH aqueous solution. Thus, the manufacturing device forms the first semiconductor element 10 with the support substrate 13 removed from the first semiconductor element 10A, and forms a recess H1 on the first semiconductor element 10. Since the third semiconductor element 80 and the third SMD component 90 are covered by the first resin layer 7, the third semiconductor element 80 and the third SMD component 90 are not etched. After that, the manufacturing device grinds the surface of the second resin layer 9 to adjust the final thickness of the semiconductor device 100B. After the above steps, the semiconductor device 100B is completed.

[0088] Similar to the semiconductor device 100 described above, the semiconductor device 100B has a recess H1 on the first semiconductor element 10. Thus, the semiconductor device 100B can improve the high-frequency characteristics of the first semiconductor element 10. In addition, the semiconductor device 100B includes a resin dam surrounding the first semiconductor element 10. The resin dam can protect the first semiconductor element 10 from contact or collision with an external substrate or external equipment, and can prevent the first semiconductor element 10 from being damaged.

[0089] In addition, the semiconductor device 100B includes a third semiconductor element 80 and a third SMD component 90 disposed on the back side 1b of the circuit substrate 1. Accordingly, the semiconductor device 100B can increase the mounting density of the components on the back side 1b of the circuit substrate 1. In addition, the third semiconductor element 80 and the third SMD component 90 are covered by the resin dam. In other words, the third semiconductor element 80 and the third SMD component 90 are built into the resin dam. Thus, the resin dam can protect the third semiconductor element 80 and the third SMD component 90 from contact and collision with an external substrate or an external device, and can prevent the third semiconductor element 80 and the third SMD component 90 from being damaged.

[0090] According to the manufacturing method of the semiconductor device 100B, the height T10A of the first semiconductor element 10A is higher than the height T80 of the third semiconductor element 80, and higher than the height T90 of the third SMD component 90 (T10A>T80 and T10A>T90). In other words, the thickness of the first semiconductor element 10A is greater than the thickness of each of the third semiconductor element 80 and the third SMD component 90. In the grinding process of the first resin layer 7, the support substrate 13 of the first semiconductor element 10A is exposed before the third semiconductor element 80 and the third SMD component 90 are exposed. The support substrate 13 is etched and removed in a state where the third semiconductor element 80 and the third SMD component 90 are covered by the first resin layer 7.

[0091] Thus, the manufacturing apparatus can mix the first semiconductor element (thin-layer semiconductor element) 10 , the third semiconductor element 80 thinner than the first semiconductor element 10 , and the third SMD component 90 on the back surface 1 b of the circuit board 1 .

[0092] (Variant 4)

[0093] Figure 8 FIG. 4 is a cross-sectional view showing a semiconductor device according to a fourth variation of the first embodiment. Figure 8 As shown, the semiconductor device 100C according to the fourth variation of the first embodiment includes an external connection terminal (hereinafter referred to as a first external connection terminal) 5 provided on the back surface 1b side of the circuit substrate 1, and a second external connection terminal 6 provided on the front surface 1a side of the circuit substrate 1. The second external connection terminal 6 includes a metal layer 61 and a plating layer 62 covering the metal layer 61. The plating layer 62 is formed from the surface of the second resin layer 9 (at the Figure 8 The lower surface) is prominent.

[0094] The second external connection terminal 6 can be formed in the same method as the first external connection terminal 5. For example, the manufacturing device sequentially performs: a process of forming the metal layer 61 on the surface 1a side of the circuit substrate 1; a process of mounting the first SMD component 60 and the second SMD component 70 on the surface 1a side of the circuit substrate 1; a process of forming the second resin layer 9 on the surface 1a side of the circuit substrate 1 to cover the metal layer 61, the first SMD component 60, and the second SMD component 70; a process of grinding the surface of the second resin layer 9 to expose only the metal layer 61; and a process of forming the plating layer 62 by plating the metal layer 61 with metal. Thus, the manufacturing device can form the second external connection terminal 6.

[0095] Similar to the semiconductor device 100 described above, the semiconductor device 100C has a recess H1 on the first semiconductor element 10. Thus, the semiconductor device 100C can improve the high-frequency characteristics of the first semiconductor element 10. In addition, the semiconductor device 100C includes a resin dam surrounding the first semiconductor element 10. The resin dam can protect the first semiconductor element 10 from contact or collision with an external substrate or external equipment, and can prevent the first semiconductor element 10 from being damaged.

[0096] The semiconductor device 100C can be connected to an external first substrate (not shown) via the first external connection terminal 5. The semiconductor device 100C can be connected to an external second substrate (not shown) via the second external connection terminal 6. Therefore, the semiconductor device 100C can be sandwiched between the external first substrate and the second substrate.

[0097] (Variant 5)

[0098] Fig. 9 FIG. 4 is a cross-sectional view showing a semiconductor device according to a fifth variation of the first embodiment. Fig. 9 As shown, the semiconductor device 100D according to the fifth variation of the first embodiment includes external connection terminals 5, a first semiconductor element 10, and a first resin layer 7 on the back surface 1b of the circuit substrate 1. Semiconductor elements or electronic components may not be mounted on the front surface 1a of the circuit substrate 1, but a resin layer covering them may be provided.

[0099] Similar to the semiconductor device 100 described above, the semiconductor device 100D has a recess H1 on the first semiconductor element 10. Thus, the semiconductor device 100D can improve the high-frequency characteristics of the first semiconductor element 10. In addition, the semiconductor device 100D includes a resin dam surrounding the first semiconductor element 10. The resin dam can protect the first semiconductor element 10 from contact or collision with an external substrate or external equipment, and can prevent the first semiconductor element 10 from being damaged.

[0100] (Implementation Method 2)

[0101] In the above-mentioned first embodiment, the description is given of providing the recessed portion H1 in the first resin layer 7. In the present embodiment, a third resin layer may be provided in the recessed portion H1.

[0102] Fig.10 FIG. 2 is a cross-sectional view showing a configuration example of a semiconductor device according to Embodiment 2. Fig.10 As shown, the semiconductor device 200 involved in embodiment 2 includes a circuit substrate 1, a plurality of external connection terminals 5, a first resin layer 7, a second resin layer 9, a first semiconductor element 10, a second semiconductor element 50, a first SMD (Surface Mount Device) component 60, a second SMD component 70 and a third resin layer 16.

[0103] The relative dielectric constant of the third resin layer 16 is preferably lower than the relative dielectric constant of Si. The relative dielectric constant of Si is, for example, 11.9. In addition, since the resistivity of the third resin layer 16 is higher than the resistivity of Si. The resistivity of Si is, for example, 1 kΩ·cm. In addition, the thermal conductivity of the third resin layer 16 is preferably higher than the thermal conductivity of SiO2. The thermal conductivity of SiO2 is, for example, 156 W / (m·K). As the third resin layer 16 that satisfies at least one of these three conditions, for example, BCB (benzocyclobutene) resin, PI (polyimide) resin, or a resin containing powder such as AlN, SiC, diamond, etc. is shown.

[0104] The third resin layer 16 is flush with the first resin layer 7. In other words, there is no step difference between the third resin layer and the first resin layer.

[0105] Next, Fig.10 A method for manufacturing the semiconductor device 200 shown will be described. Fig.11 as well as Fig.12 2 is a cross-sectional view showing a method for manufacturing a semiconductor device according to Embodiment 2 in order of steps. Fig.11 as well as Fig.12 As shown in FIG. 1 , the semiconductor device 200 according to the second embodiment is completed through each process of steps ST41 to ST48. Fig.11 as well as Fig.12 In the figure, the wiring layer 3 included in the circuit board 1 is omitted from illustration.

[0106] exist Fig.11 In step ST41, the manufacturing device (not shown) forms the external connection terminal 5 on the back surface 1b of the circuit substrate 1. Next, the manufacturing device mounts the first semiconductor element 10A on the back surface 1b of the circuit substrate 1 (step ST42). Next, the manufacturing device forms the first resin layer 7 on the back surface 1b of the circuit substrate 1. Thus, the first semiconductor element 10A and the metal layer 51 are covered and sealed by the first resin layer 7.

[0107] Next, the manufacturing apparatus grinds the surface of the first resin layer 7 to expose the support substrate 13 from the first resin layer 7 (step ST43). Next, the manufacturing apparatus etches and removes the support substrate 13 under conditions that make it easier to etch the support substrate 13 than the first resin layer 7 and the insulating layer 12 (step ST44). Thus, the manufacturing apparatus forms the first semiconductor element 10 in which the support substrate 13 is removed from the first semiconductor element 10A, and forms the recess H1 in the first semiconductor element 10.

[0108] As in the first embodiment, in the second embodiment, the etching of the support substrate 13 is preferably performed by wet etching to minimize damage to the insulating layer 12 as the base. For example, the manufacturing apparatus uses a TMAH aqueous solution with a concentration of 10 mass percent (wt%) and a liquid temperature of 80° C. as an etching solution. Thus, the manufacturing apparatus can use the insulating layer Si composed of SiO2 as an etching stopper layer and only etch the support substrate 13 composed of Si.

[0109] Next, the manufacturing device fills the material of the third resin layer 16 in the recess H1 (step ST45). It is preferred that the material of the third resin layer 16 is a fluid such as a liquid when filled, and is then cured by heat treatment or UV treatment. As a result, it is easy to configure the third resin layer 16 without a gap in the recess H1. In addition, the manufacturing device can use methods such as screen printing, injection, spin coating, spray coating, etc. as a filling method for the material of the third resin layer 16. For example, according to screen printing, since the material of the third resin layer 16 can be configured only in the recess H1, compared with spin coating, etc., there is less waste of material and the material efficiency can be maintained at a high level. As the material of the third resin layer 16, for example, a solvent containing BCB, a solvent containing PI, or a resin paste containing powder such as AlN, SiC, and diamond is shown.

[0110] Next, the manufacturing device performs a heat treatment or UV treatment on the material of the third resin layer 16 in the recess H1 to cure the material. Thus, the manufacturing device forms the third resin layer 16 in the recess H1. In addition, in this embodiment, the third resin layer 16 may also be in a sheet shape. In this case, the manufacturing device may also place the sheet-shaped material in the recess H1 by a lamination method.

[0111] Next, the manufacturing device mounts the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 on the surface 1a side of the circuit substrate 1 (step ST46). Next, the manufacturing device forms the second resin layer 9 on the surface 1a side of the circuit substrate 1 (step ST47). Thus, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70 are covered and sealed by the second resin layer 9.

[0112] Next, the manufacturing device grinds each surface of the first resin layer 7 and the third resin layer 16 to expose the metal layer 51 from the first resin layer 7 (step ST48). The manufacturing device used for this grinding is, for example, a thinning machine having a grinding tool. The thinning machine grinds each surface of the first resin layer 7 and the third resin layer 16 by rotating the grinding tool relative to the first resin layer 7 and the third resin layer 16. In addition, the grinding of the first resin layer 7 and the third resin layer 16 is not limited to the method using the thinning machine. For example, the grinding of the first resin layer 7 and the third resin layer 16 can also be performed by CMP.

[0113] Next, the manufacturing device forms the plating layer 52 by plating the metal layer 51 with metal. For example, the manufacturing device sequentially plates Ni and Au. Thus, the plating layer 52 is formed only on the metal layer 51, and the external connection terminal 5 having the metal layer 51 and the plating layer 52 is completed. After that, the manufacturing device grinds the surface of the second resin layer 9 to adjust the final thickness of the semiconductor device 200. After the above steps, the semiconductor device 200 is completed.

[0114] As described above, the semiconductor device 200 according to the second embodiment includes the circuit substrate 1, the plurality of external connection terminals 5, the first resin layer 7, the second resin layer 9, the first semiconductor element 10, the second semiconductor element 50, the first SMD component 60, and the second SMD component 70, similarly to the semiconductor device 100 according to the first embodiment. Thus, the semiconductor device 200 can improve the high frequency characteristics of the first semiconductor element 10 and can improve the heat dissipation of the first semiconductor element 10.

[0115] The semiconductor device 200 further includes a third resin layer 16 provided on the first semiconductor element 10, and the first resin layer 7 (resin dam) surrounds the third resin layer 16. For example, the third resin layer 16 is disposed in the recess H1 on the first semiconductor element 10. Thus, the first semiconductor element 10 can be protected by the third resin layer 16.

[0116] The first resin layer 7 and the third resin layer 16 are coplanar. This improves the flatness of the back surface 1b of the circuit board 1. Thus, the semiconductor device 200 can be easily surface-mounted on an external substrate with the back surface 1b of the circuit board 1 facing the external circuit board 1.

[0117] The relative dielectric constant of the third resin layer 16 is lower than that of Si. Thus, the semiconductor device 200 can improve the high frequency characteristics of the first semiconductor element 10 compared to the case where the support substrate 13 is left on the insulating layer 12 .

[0118] The resistivity of the third resin layer 16 is higher than the resistivity of Si. Thus, the semiconductor device 200 can improve the high frequency characteristics of the first semiconductor element 10 compared to the case where the support substrate 13 is left on the insulating layer 12 .

[0119] The thermal conductivity of the third resin layer 16 is higher than that of SiO 2. Therefore, compared with a case where SiO 2 is disposed on the insulating layer 12 (for example, a case where the insulating layer 12 composed of SiO 2 is as thick as the third resin layer 16), the semiconductor device 200 can improve the heat dissipation of the first semiconductor element 10.

[0120] Description of Reference Numerals

[0121] 1 Circuit board (an example of a substrate)

[0122] 1a Surface (an example of the second surface)

[0123] 1b Back side (an example of the first side)

[0124] 3 Wiring Layer

[0125] 5, 6 External connection terminals

[0126] 7. First resin layer

[0127] 9 Second resin layer

[0128] 10. First semiconductor element (an example of a first element)

[0129] 10A First semiconductor element (an example of an element)

[0130] 11 Semiconductor layer

[0131] 12 Insulation layer

[0132] 13 Support base plate

[0133] 15 Bump electrode (an example of an electrode part)

[0134] 16 Third resin layer

[0135] 50 second semiconductor element (an example of a second element)

[0136] 51, 61 metal layer

[0137] 52, 62 coating

[0138] 55, 85 semiconductor substrate

[0139] 56, 86 bump electrode

[0140] 60 First SMD component (an example of the second component)

[0141] 70 Second SMD component (an example of a second element)

[0142] 80 Third semiconductor element (an example of a third element)

[0143] 90 Third SMD component (an example of a third element)

[0144] 100, 100A, 100B, 100C, 100D, 200 semiconductor devices.

Claims

1. A semiconductor device comprising: A substrate having a first surface and a second surface located on the opposite side of the first surface; A first element is disposed on the first surface side; and The first resin layer is provided on the first surface side and is provided around the first element in a plan view. The substrate has a wiring layer. The first element has: Semiconductor layer; an electrode portion located on a surface of the semiconductor layer that is opposite to the substrate; and an insulating layer located on the opposite side of the electrode portion across the semiconductor layer, The electrode portion is connected to the wiring layer. A height of the first resin layer from the first surface is higher than a height of the first element from the first surface.

2. The semiconductor device according to claim 1, wherein The first resin layer is in close contact with a side surface of the first element.

3. The semiconductor device according to claim 1 or 2, wherein: The first resin layer is filled between the first element and the substrate.

4. The semiconductor device according to any one of claims 1 to 3, wherein: The first resin layer has a relative dielectric constant of 4 or less.

5. The semiconductor device according to any one of claims 1 to 4, wherein: The first resin layer is a thermosetting resin.

6. The semiconductor device according to any one of claims 1 to 5, wherein: The semiconductor device further includes an external connection terminal provided on the first surface side. A height of the external connection terminal from the first surface is the same as a height of the first resin layer from the first surface, or a height of the external connection terminal from the first surface is higher than a height of the first resin layer from the first surface.

7. The semiconductor device according to any one of claims 1 to 6, wherein: The semiconductor device further comprises: A second element is disposed on the second surface side; and The second resin layer is provided on the second surface side to cover the second element.

8. The semiconductor device according to any one of claims 1 to 7, wherein: The semiconductor device further includes a third element provided on the first surface side. The third element is covered with the first resin layer.

9. The semiconductor device according to any one of claims 1 to 8, wherein: The semiconductor device further comprises a third resin layer provided on the first element. The first resin layer surrounds the third resin layer.

10. The semiconductor device according to claim 9, wherein The first resin layer and the third resin layer are on the same plane.

11. The semiconductor device according to claim 9 or 10, wherein: The relative dielectric constant of the third resin layer is lower than the relative dielectric constant of Si.

12. The semiconductor device according to any one of claims 9 to 11, wherein: The resistivity of the third resin layer is higher than the resistivity of Si.

13. The semiconductor device according to any one of claims 9 to 12, wherein: The thermal conductivity of the third resin layer is higher than that of SiO2.

14. A method for manufacturing a semiconductor device, the method using an element to manufacture a semiconductor device, The above elements have: support base plate; An insulating layer is provided on one side of the supporting substrate; a semiconductor layer disposed on the opposite side of the support substrate via the insulating layer; as well as an electrode portion disposed on the opposite side of the insulating layer via the semiconductor layer, The method for manufacturing the semiconductor device comprises: a step of connecting the electrode portion to a wiring layer of the substrate by making the semiconductor layer face the first surface of the substrate; forming a first resin layer on the first surface side of the substrate to cover the element; a step of grinding the first resin layer to expose the support substrate; and a step of removing the support substrate exposed from the first resin layer by etching.