Semiconductor structure and method for manufacturing the same
By performing an ion implantation process in the barrier layer during the semiconductor manufacturing process and adjusting the etching rate, the problem of low groove shape accuracy in the existing technology is solved, and higher etching accuracy and lower manufacturing costs are achieved.
Patent Information
- Application Number
- CN201911036460.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-10-29
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2039-10-29
AI Technical Summary
In the semiconductor manufacturing process, it is difficult to ensure the accuracy of groove shapes in existing processes. Especially when etching special-shaped grooves, there is a difference between the groove shape and the preset shape, resulting in low etching accuracy.
By performing an ion implantation process in different areas of the barrier layer, the etching rate is adjusted to improve the etching precision. The specific method includes performing ion implantation in the area to be etched and the gap area, and adjusting the doping ion concentration and implantation dose to Ensure optimization of etching selectivity.
This effectively prevents the gap area from being removed by etching, improves the accuracy of the etching process, reduces manufacturing costs, reduces the impact of uneven etching rates, and ensures the shape accuracy of the groove.
Smart Images

Figure CN112750699B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a semiconductor structure and a manufacturing method thereof. Background Art
[0002] Deep trench etching has always been a common process in semiconductor manufacturing. As the process line width becomes smaller, the aspect ratio of the trench becomes larger and larger, and the shape requirements become more and more stringent. In order to achieve the etching of high aspect ratio trenches, the existing process usually requires a thicker or harder barrier layer to meet the precision requirements of the trench opening. In this way, the barrier layer opening can be prevented from being etched during the etching process, thereby preventing the opening width of the trench from increasing and meeting the aspect ratio requirements of the trench.
[0003] However, it is still difficult to ensure the shape of the groove while ensuring the opening width. Take dry etching as an example. During the dry etching process, the composition of the etching gas needs to be adjusted. During the etching process, the flow direction and uniformity of the gas are difficult to ensure, resulting in a certain difference between the etched groove shape and the preset groove shape. This difference is more obvious when etching grooves of special shapes. Summary of the invention
[0004] The embodiment of the present invention provides a semiconductor structure and a manufacturing method thereof, which improves the etching accuracy of the etching process by changing the etching selectivity ratio of different regions in a barrier layer.
[0005] To solve the above technical problems, an embodiment of the present invention provides a method for manufacturing a semiconductor structure, comprising: providing a substrate, the substrate having at least two discrete protrusions and a barrier layer filled between adjacent protrusions; wherein the barrier layer comprises adjacent areas to be etched and gap areas, and in a direction perpendicular to the substrate, the gap area is located between the protrusions and the substrate; performing an ion implantation process on at least one of the areas to be etched or the gap areas, the ion implantation process being used to make the etching rate of the gap area smaller than the etching rate of the areas to be etched; after performing the ion implantation process, removing the areas to be etched.
[0006] In addition, after the ion implantation process, ion implantation is performed on the area to be etched, with an implantation dose of 1e12 to 1e14 cm -2 .
[0007] In addition, the ion implantation process for at least one of the area to be etched or the gap area specifically includes: performing an ion implantation process on the area to be etched and the gap area; wherein, before performing the ion implantation process on the area to be etched, the ion implantation process is performed on the gap area.
[0008] In addition, the area to be etched includes a first area and a second area, the first area is located above the second area, the top of the second area away from the substrate is higher than the top of the gap area away from the substrate, or the top of the second area away from the substrate is flush with the top of the gap area away from the substrate; the ion implantation process is performed on at least one of the area to be etched or the gap area, and the area to be etched is removed after the ion implantation process, specifically including: performing a first ion implantation process on the first area, and removing the first area after the first ion implantation process; performing a second ion implantation process on the gap area; after removing the first area, performing a third ion implantation process on the second area, and removing the second area after the third ion implantation process.
[0009] In addition, the raised portion includes a conductive layer and a side wall located on the side of the conductive layer; the bottom side wall of the area to be etched is perpendicular to the substrate, and the orthographic projection of the side wall on the substrate partially overlaps with the orthographic projection of the area to be etched on the substrate; after the ion implantation process, it also includes: removing the side wall whose orthographic projection is within the orthographic projection of the area to be etched on the substrate.
[0010] In addition, before removing the side walls whose orthographic projections are located within the orthographic projections of the area to be etched on the substrate, an ion implantation process is performed on the side walls whose orthographic projections are located within the orthographic projections of the area to be etched on the substrate, so that the etching rate of the side walls whose orthographic projections are located within the orthographic projections of the area to be etched on the substrate is greater than the etching rate of the gap area.
[0011] An embodiment of the present invention also provides a semiconductor structure, comprising: a substrate and at least two discrete protrusions located on the substrate; a barrier layer, the barrier layer filling between adjacent protrusions; wherein the barrier layer includes a gap area, the gap area is located between the protrusions and the substrate in a direction perpendicular to the substrate; a groove located in the barrier layer, the sidewall of the groove is perpendicular to the substrate; or, the width of the groove increases in a direction away from the substrate.
[0012] In addition, in the arrangement direction of the protrusions, there are two separate grooves in the barrier layer between adjacent protrusions.
[0013] In addition, the depth-to-width ratio of the groove is 4:1 to 6:1.
[0014] In addition, the protrusion includes a conductive layer and a side wall located on the side of the conductive layer; the gap area is located between the protrusion and the substrate, specifically including: the gap area is located between the side wall and the substrate.
[0015] Compared with the prior art, the technical solution provided by the embodiment of the present invention has the following advantages:
[0016] The present invention provides a method for manufacturing a semiconductor structure. Before removing the area to be etched, the etching selectivity ratio of the area to be etched and the gap area is improved through an ion implantation process, thereby avoiding the gap area from being etched away in the subsequent etching process, thereby ensuring the etching accuracy of the etching process.
[0017] In addition, by first performing the ion implantation process on the gap region, it is possible to avoid the obstruction of other doping ions on the ion implantation path of the gap region, thereby reducing the energy required for ion implantation and reducing manufacturing costs.
[0018] In addition, the etching rate decreases in the direction away from the contact surface, which is beneficial to reduce the uneven etching rate caused by the high hardness and low etching rate of the area to be removed, thereby ensuring the accuracy of the etching process. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplified descriptions do not constitute limitations on the embodiments. Components with the same reference numerals in the drawings represent similar components, and unless otherwise stated, the figures in the drawings do not constitute proportional limitations.
[0020] Figures 1 to 3 It is a schematic cross-sectional structure diagram corresponding to each step of the method for manufacturing a semiconductor structure provided by an embodiment of the present invention;
[0021] Figure 4 is a schematic cross-sectional structural diagram corresponding to each step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention;
[0022] Figure 5 is a schematic cross-sectional structural diagram corresponding to each step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention;
[0023] Figure 6 is a schematic cross-sectional structural diagram corresponding to each step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention;
[0024] Figure 7 is a schematic cross-sectional structural diagram corresponding to each step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention;
[0025] Figure 8 It is a schematic cross-sectional structure diagram of a semiconductor structure provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0026] As can be seen from the background art, there is a certain difference between the groove shape etched in the prior art and the preset groove shape.
[0027] To solve the above problems, an embodiment of the present invention provides a method for manufacturing a semiconductor structure. Before removing the area to be etched to form a groove, an ion implantation process is used to improve the etching selectivity of the area to be etched and its adjacent areas, thereby ensuring the etching accuracy of the etching process.
[0028] In order to make the purpose, technical scheme and advantages of the embodiments of the present invention clearer, the embodiments of the present invention will be described in detail below with reference to the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present invention, many technical details are provided to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.
[0029] The semiconductor manufacturing method provided by the embodiment of the present invention will be described in detail below with reference to the accompanying drawings.
[0030] Figures 1 to 3 A schematic diagram of the cross-sectional structure corresponding to each step of the method for manufacturing a semiconductor structure provided by an embodiment of the present invention.
[0031] Reference Figure 1 , providing a substrate 11 having at least two discrete protrusions 12 and a barrier layer 13 filled between adjacent protrusions 12 .
[0032] Among them, in the direction from the base 11 to the protrusion 12, the top width of the protrusion 12 is greater than the bottom width; the protrusion 12 can be a solid bump composed of a single material, or a device with a complex structure composed of multiple materials, such as a bit line structure; and its material can be a metal material, a non-metal material or a combination thereof.
[0033] In this embodiment, the barrier layer 13 includes adjacent areas to be etched 132 and gap areas 131. In a direction perpendicular to the substrate 11, the gap area 131 is located between the protrusion 12 and the substrate 11, and the gap area 131 is in contact with the protrusion 12. The material of the barrier layer 13 includes dielectric materials such as silicon dioxide, borophosphosilicate glass, borosilicate glass, and low dielectric constant materials.
[0034] It should be noted that there is at least one region 132 to be etched between adjacent protrusions 12. When there are multiple regions 132 to be etched, the multiple regions 132 to be etched are separated from each other. In this embodiment, there are two separate regions 132 to be etched between adjacent protrusions 12.
[0035] In addition, in the present embodiment, the side wall of the area to be etched 132 is perpendicular to the substrate 11, and the orthographic projection of the area to be etched 132 on the substrate 11 contacts the boundary of the orthographic projection of the protrusion 12 on the substrate 11; in other embodiments, the side wall of the area to be etched may also form an acute angle or an obtuse angle with the substrate; and the orthographic projection of the area to be etched on the substrate may also partially overlap with the orthographic projection of the protrusion on the substrate. It should be noted that the "vertical" mentioned in this article refers to "approximately vertical". "Approximately vertical" can be understood as that the side wall surface has a tiny concave-convex structure, but the concave-convex structure does not affect the definition of the plane where the side wall is located.
[0036] The aspect ratio of the to-be-etched region 132 is 4:1-6:1, for example, 4.5:1, 5:1, or 5.5:1.
[0037] Reference Figure 2 , an ion implantation process is performed on at least one of the etched area 132 or the gap area 131 .
[0038] In this embodiment, an ion implantation process is performed on the area to be etched 132. Specifically, before the ion implantation process is performed, a mask layer 14 is formed on the surface of the barrier layer 13 and the protrusion 12, and the mask layer 14 has an opening 141, and the opening 141 exposes the surface of the area to be etched 132. The width d1 of the opening 141 is equal to the top width d of the predefined area to be etched 132.
[0039] It should be noted that, in other embodiments, the opening width may also be smaller than the top width of the area to be etched. In this case, ions are implanted into the area to be etched by adjusting the implantation angle to ensure that any position in the area to be etched has doped ions.
[0040] In this embodiment, the material of the mask layer 14 is photoresist, and the thickness of the mask layer 14 is 80-350nm, for example, 85nm, 200nm, 300nm; in other embodiments, the material of the mask layer can also be a hard mask, and the hardness of the hard mask is greater than the hardness of the photoresist.
[0041] After forming the mask layer 14, an appropriate amount of doping ions is injected into the to-be-etched region 132 through the opening 141. The appropriate amount of doping ions can change the lattice strength of the target region of ion implantation, making the material in the region amorphous or looser, thereby increasing the etching rate of the region. In this way, after the ion implantation process, the etching rate of the to-be-etched region 132 is greater than the etching rate of the gap region 131.
[0042] It should be noted that too large an implanted doping ion dose will result in an excessively high doping ion concentration in the target area, and an excessively high doping ion concentration will cause the material in the area to harden, thereby causing the etching rate of the area to be lower than the etching rate before ion doping.
[0043] Figure 2 The direction of the arrow shown in the figure is only a schematic direction. The actual ion implantation angle is related to factors such as the position of the ion implantation target area and the position of the opening 141. The doping ions in the ion implantation process include one or more of arsenic, indium or chromium. The energy and dose of the ion implantation process are related to the position of the target area and the required doping ion concentration.
[0044] It should be noted that, in this embodiment, the ion implantation direction may be perpendicular to the substrate 11, or may form an acute angle or an obtuse angle with the substrate 11. The ion implantation angle may be selected according to actual conditions.
[0045] The ion dose injected into the area to be etched 132 is 1e12-1e14 cm -2 , for example 2e12cm -2 , 1e13cm -2 、8e13cm -2 .
[0046] In this embodiment, the doping ion concentration in the to-be-etched region 132 increases in a direction away from the substrate 11. This helps prevent the doping ion concentration of the bottom layer from being greater than the doping ion concentration of the top layer due to the doping ions sinking, thereby preventing the etching rate of the bottom layer from being greater than the etching rate of the top layer, and helps reduce the etching of the two side regions at the bottom of the to-be-etched region 132, thereby improving the etching accuracy of the etching process.
[0047] Reference Figure 3 , after the ion implantation process, the area to be etched is removed.
[0048] After the ion implantation process is performed, the area to be etched is removed by dry etching or wet etching to form a groove 15 ; after the groove 15 is formed, the mask layer is removed.
[0049] In this embodiment, by performing an ion implantation process on the area to be etched 132 , the etching rate of the area to be etched 132 is higher than the etching rate of the gap area 131 , which is beneficial to reduce the additional etching of the gap area 131 during the etching process, thereby ensuring the accuracy of the etching process.
[0050] Figure 41 is a schematic diagram of a cross-sectional structure corresponding to a step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention. It should be noted that the manufacturing steps that are the same as or corresponding to the previous method embodiment can refer to the corresponding description of the previous method embodiment, and will not be repeated below. The difference between the method embodiment of the present invention and the previous method embodiment is that an ion implantation process is performed on the gap region 131.
[0051] In this embodiment, an excessive amount of doping ions is injected into the gap region 131 so that the material of the gap region 131 is hardened and the etching rate is reduced.
[0052] It should be noted that since the gap region 131 is located between the protrusion 12 and the substrate 11, the orthographic projection of the gap region 131 on the substrate 11 does not coincide with the orthographic projection of the opening 141 on the substrate 11. Therefore, there is a certain angle between the ion injection direction in this embodiment and the direction perpendicular to the substrate 11. The size of the angle is determined by factors such as the position of the gap region 131 relative to the area to be etched 132 and the aspect ratio of the area to be etched 132.
[0053] In this embodiment, by injecting excess doping ions into the gap region 131, the etching rate of the to-be-etched region 132 is higher than that of the gap region 131, which helps to reduce additional etching of the gap region 131 during the etching process, thereby ensuring the accuracy of the etching process.
[0054] Figure 5 1 is a schematic diagram of a cross-sectional structure corresponding to a step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention. It should be noted that the manufacturing steps that are the same as or corresponding to the previous method embodiment can refer to the corresponding description of the previous method embodiment, and will not be repeated below. The difference between the method embodiment of the present invention and the previous method embodiment is that an ion implantation process is performed on the etching area 132 and the gap area 131.
[0055] In this embodiment, an appropriate amount of doping ions is injected into the region to be etched 132 to increase the etching rate of the region to be etched 132, and an excessive amount of doping ions is injected into the gap region 131 to reduce the etching rate of the region to be etched 131. In this way, the etching selectivity between the gap region 131 and the region to be etched 132 can be further improved, thereby reducing the etching of the gap region 131 during the etching process of the region to be etched 132, thereby improving the accuracy of the etching process.
[0056] The type of doping ions in the to-be-etched region 132 and the type of doping ions in the gap region 131 may be the same or different.
[0057] In this embodiment, the gap region 131 is firstly subjected to ion implantation, and then the region to be etched 132 is subjected to ion implantation. This helps to ensure that there is no other doping ion blocking the ion implantation path of the gap region 131, thereby reducing the energy required for ion implantation and further reducing manufacturing costs.
[0058] It should be noted that, in other embodiments, the ion implantation process is first performed on the area to be etched, and then the ion implantation process is performed on the gap area.
[0059] In this embodiment, the etching rate of the area to be etched 132 is increased while the etching rate of the gap area 131 is reduced, thereby further improving the etching selectivity ratio and improving the accuracy of the etching process; in addition, the gap area 131 is first subjected to an ion implantation process, which can reduce the energy required for ion implantation and thus reduce manufacturing costs.
[0060] Figure 6 It is a schematic diagram of the cross-sectional structure corresponding to a step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention. It should be noted that the manufacturing steps that are the same as or corresponding to the previous method embodiment can refer to the corresponding description of the previous method embodiment, and will not be repeated below. The difference between the method embodiment of the present invention and the previous method embodiment is that the area to be etched 132 includes a first area 133 located at the top and 134 located at the bottom; before ion implantation is performed on the gap area 131, an ion implantation process is performed on the first area 133, and the first area 133 is removed after the ion implantation process is completed.
[0061] Specifically, the area to be etched 132 includes a first area 133 and a second area 134, the first area 133 is located above the second area 134, and the top of the second area 134 away from the substrate 11 is flush with the top of the gap area 131 away from the substrate 11. Accordingly, the first area 133 is firstly subjected to a first ion implantation process, and the first area 133 is removed after the first ion implantation process; after the first area 133 is removed, the gap area 131 is subjected to a second ion implantation process; the second area 134 is subjected to a third ion implantation process, and the second area 134 is removed after the third ion implantation process.
[0062] In this way, the first region 133 can be prevented from blocking the ion implantation in the gap region 131, further reducing the energy required for the ion implantation process, thereby reducing the manufacturing cost; at the same time, the bottom surface of the first region 133 close to the substrate 11 is flush with the top surface of the gap region 133 away from the substrate 11, so that the etching of the first region 133 will not affect the gap region 133.
[0063] It should be noted that, in other embodiments, the top of the second region away from the substrate is higher or lower than the top of the gap region away from the substrate.
[0064] In this embodiment, by performing ion implantation on the area to be etched 132 and the gap area 131, the etching rate of the area to be etched 132 is higher than the etching rate of the gap area 131, which is beneficial to reduce the additional etching of the gap area 131 during the etching process, thereby ensuring the accuracy of the etching process.
[0065] Figure 7 It is a schematic diagram of a cross-sectional structure corresponding to a step of a method for manufacturing a semiconductor structure provided by another embodiment of the present invention. It should be noted that the manufacturing steps that are the same as or corresponding to the previous method embodiment can refer to the corresponding description of the previous method embodiment, and will not be repeated below. The difference between the method embodiment of the present invention and the previous method embodiment is that: the protrusion 22 includes a conductive layer 221 and a side wall 222 located on the side of the conductive layer 221; after the ion implantation process, part of the side wall 222 is removed.
[0066] Specifically, the protrusion 22 includes a conductive layer 221 and a side wall 222 located on the side of the conductive layer 221, and the orthographic projection of the area to be etched 232 on the substrate 21 partially overlaps with the orthographic projection of the side wall 222 on the substrate 21; the side wall 222 includes an area to be removed 223, and the orthographic projection of the area to be removed 223 on the substrate 21 is located within the orthographic projection of the area to be etched 232 on the substrate 21, and overlaps with the boundary of the orthographic projection of the area to be etched 232 on the substrate 21.
[0067] In this embodiment, the ion implantation process is performed on the area to be etched 232, the gap area 231 and the area to be removed 223; in other embodiments, the ion implantation process is performed only on the area to be etched and the gap area, or the ion implantation process is performed only on the area to be etched.
[0068] The ion implantation process for the area to be removed 223 refers to implanting a proper amount of doping ions into the area to be removed 223 , thereby increasing the etching rate of the area to be removed 223 .
[0069] Among them, the ion implantation process performed on the area to be removed 223 and the ion implantation process performed on the area to be etched 232 can be the same ion implantation process or different ion implantation processes; accordingly, after the ion implantation process, the doping ion type in the area to be removed 223 and the doping ion type in the area to be etched 232 can be the same or different, and the doping ion concentration in the area to be removed 223 and the doping ion concentration in the area to be etched 232 can be the same or different.
[0070] It should be noted that the conductive layer 221 can be a solid bump composed of a single material, or a device with a complex structure composed of multiple materials, such as a bit line structure; and its material can be a metal material, a non-metal material or a combination thereof; the side wall 222 is usually an insulating material with a certain hardness, which can play both a protective role and an insulating role.
[0071] The opening 241 of the mask layer 24 exposes the surface of the to-be-etched region 232 and the surface of the to-be-removed area 223 , and the orthographic projection of the opening 241 on the substrate 21 coincides with the orthographic projection of the to-be-etched region 232 on the substrate 21 .
[0072] In this embodiment, the hardness of the sidewall 222 is greater than the hardness of the barrier layer 23; wherein the material of the barrier layer 23 may be silicon dioxide, and the material of the sidewall 222 may be silicon nitride. It should be noted that since the hardness of the sidewall 222 is greater than the hardness of the barrier layer 23, the time required for subsequent groove etching will increase; accordingly, in order to ensure the accuracy of the groove opening, the thickness or hardness of the mask layer 24 needs to be increased accordingly.
[0073] In this embodiment, since part of the to-be-etched region 232 is located between the to-be-removed region 223 and the substrate in the direction perpendicular to the substrate 21, it is necessary to have an ion implantation direction that forms a certain angle with the direction perpendicular to the substrate 21. In this way, it is ensured that any position in the to-be-etched region 232 has doped ions.
[0074] In this embodiment, the sidewall 222 and the area to be etched 232 have a contact surface 233; after the ion implantation process is performed on the area to be etched 232, the etching rate of the area to be etched 232 decreases in the direction away from the contact surface 233. In this way, it is helpful to reduce the uneven etching rate caused by the high hardness and low etching rate of the area to be removed 223, and it is helpful to ensure that the etching of the area to be removed 223 and the area to be etched 232 is completed synchronously, thereby reducing the etching of the surrounding area and ensuring the accuracy of the etching process.
[0075] After the ion implantation process, the to-be-removed area 223 and the to-be-etched area 232 are removed.
[0076] Among them, the same etchant can be used to etch the area to be removed 223 and the area to be etched 232 at the same time; different etchants can also be used to etch the area to be removed 223 and the area to be etched 232 respectively. For example, when the material of the area to be etched 232 is silicon dioxide and the material of the area to be removed 223 is silicon nitride, hydrofluoric acid can be used to etch silicon dioxide and phosphoric acid can be used to etch silicon nitride.
[0077] In this embodiment, the distribution of doped ions in the area to be etched 232 is adjusted and the etching rates of different areas are adjusted, thereby reducing the uneven etching rate caused by the higher hardness and lower etching rate of the area to be removed 223. This is beneficial to ensure that the etching of the area to be removed 223 and the area to be etched 232 are completed synchronously, thereby reducing the etching of the surrounding areas and ensuring the accuracy of the etching process.
[0078] Correspondingly, an embodiment of the present invention further provides a semiconductor structure.
[0079] Reference Figure 8 The semiconductor structure includes: a substrate 31 and at least two discrete protrusions 32 located on the substrate 31; a barrier layer 33, the barrier layer 33 is filled between adjacent protrusions 32; wherein the barrier layer 33 includes a gap region 331, and in a direction perpendicular to the substrate 31, the gap region 331 is located between the protrusion 32 and the substrate 31; a groove 35 located in the barrier layer 33, and the sidewall of the groove 35 is perpendicular to the substrate 31; or, in a direction away from the substrate 31, the width of the groove 35 increases.
[0080] The semiconductor structure provided by this embodiment will be described in detail below with reference to the accompanying drawings.
[0081] In this embodiment, the protrusion 32 includes a conductive layer 321 and a side wall 322 located on the side of the conductive layer 321; the barrier layer 33 includes a gap area 331, and in a direction perpendicular to the substrate 31, the gap area 331 is located between the side wall 322 and the substrate 31; wherein the hardness of the side wall 322 is greater than the hardness of the barrier layer 33.
[0082] It should be noted that the conductive layer 321 can be a solid film layer composed of a single material, or a device composed of multiple materials with a complex structure, such as a bit line structure; and its material can be a metal material, a non-metal material or a combination thereof.
[0083] In this embodiment, the gap region 331 has doping ions, and the doping ions are used to reduce the etching rate of the gap region 331. In other embodiments, the gap region does not have doping ions. The types of doping ions include arsenic, indium or chromium.
[0084] In addition, in the arrangement direction of the protrusions 32, the barrier layer 33 between adjacent protrusions 32 has two separate grooves 35, and the grooves 35 expose the surface of the substrate 31; wherein the aspect ratio of the grooves is 4:1 to 6:1, for example, 4.5:1, 5:1, 5.5:1.
[0085] In this embodiment, the sidewall of the groove 35 is perpendicular to the substrate 31 ; in other embodiments, the width of the groove increases in a direction away from the substrate.
[0086] In this embodiment, the barrier layer 33 further includes a middle region 332, which is located between adjacent grooves 35. The middle region 332 contains doped ions, which are used to reduce the etching rate of the middle region 332. This helps to ensure the flatness of the sidewalls of the grooves 35.
[0087] The concentration of doping ions on the two opposite sides of the middle region 332 is greater than the concentration of doping ions in the middle of the middle region 332. Specifically, the doping ions are only located on the two opposite sides of the middle region 332, and the groove 35 exposes the region where the doping ions are located. This is conducive to reducing the implantation dose of the doping ions and reducing the manufacturing cost.
[0088] It should be noted that, in other embodiments, the middle region does not contain doping ions.
[0089] In this embodiment, the sidewall of the groove 35 is perpendicular to the base 31 , which helps to ensure that the groove 35 is evenly filled.
[0090] Correspondingly, an embodiment of the present invention further provides an electronic device, which includes the above-mentioned semiconductor structure.
[0091] In this embodiment, the grooves in the semiconductor structure can be filled uniformly, which is helpful to ensure that the electronic device has good electrical performance.
[0092] Those skilled in the art will appreciate that the above embodiments are specific examples of the present invention, and in practical applications, various changes may be made to the embodiments in form and detail without departing from the spirit and scope of the present invention. Any person skilled in the art may make changes and modifications without departing from the spirit and scope of the present invention, and therefore the scope of protection of the present invention shall be subject to the scope defined in the claims.
Claims
1. A method for manufacturing a semiconductor structure, It is characterized in that include: Providing a substrate, wherein the substrate has at least two discrete protrusions and a barrier layer filled between adjacent protrusions; wherein the barrier layer includes adjacent to-be-etched areas and gap areas, and in a direction perpendicular to the substrate, the gap area is located between the protrusions and the substrate; Performing an ion implantation process on at least one of the to-be-etched region or the gap region, wherein the ion implantation process is used to make the etching rate of the gap region lower than the etching rate of the to-be-etched region; After performing the ion implantation process, removing the area to be etched; The ion implantation process for at least one of the area to be etched or the gap area specifically includes: performing an ion implantation process on the area to be etched and the gap area; and performing an ion implantation process on the gap area before performing the ion implantation process on the area to be etched.
2. The method for manufacturing a semiconductor structure according to claim 1, It is characterized in that Ion implantation is performed on the area to be etched, with an implantation dose of 1e12~1e14 cm -2 .
3. The method for manufacturing a semiconductor structure according to any one of claims 1 to 2, It is characterized in that The protrusion includes a conductive layer and a side wall located on the side of the conductive layer; the bottom side wall of the to-be-etched area is perpendicular to the substrate, and the orthographic projection of the side wall on the substrate partially overlaps with the orthographic projection of the to-be-etched area on the substrate; After the ion implantation process is performed, the method further includes: removing the sidewall whose orthographic projection is located within the orthographic projection of the to-be-etched area on the substrate.
4. The method for manufacturing a semiconductor structure according to claim 3, It is characterized in that Before removing the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate, an ion implantation process is performed on the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate, so that the etching rate of the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate is greater than the etching rate of the gap area.
5. A method for manufacturing a semiconductor structure, It is characterized in that include: Providing a substrate, wherein the substrate has at least two discrete protrusions and a barrier layer filled between adjacent protrusions; wherein the barrier layer includes adjacent to-be-etched areas and gap areas, and in a direction perpendicular to the substrate, the gap area is located between the protrusions and the substrate; Performing an ion implantation process on at least one of the to-be-etched region or the gap region, wherein the ion implantation process is used to make the etching rate of the gap region lower than the etching rate of the to-be-etched region; After performing the ion implantation process, removing the area to be etched; The area to be etched includes a first area and a second area, the first area is located above the second area, the top of the second area away from the substrate is higher than the top of the gap area away from the substrate, or the top of the second area away from the substrate is flush with the top of the gap area away from the substrate; The ion implantation process is performed on at least one of the area to be etched or the gap area, and the area to be etched is removed after the ion implantation process, specifically comprising: performing a first ion implantation process on the first area, and removing the first area after the first ion implantation process; performing a second ion implantation process on the gap area after removing the first area; performing a third ion implantation process on the second area, and removing the second area after the third ion implantation process.
6. The method for manufacturing a semiconductor structure according to claim 5, It is characterized in that The protrusion includes a conductive layer and a side wall located on the side of the conductive layer; the bottom side wall of the to-be-etched area is perpendicular to the substrate, and the orthographic projection of the side wall on the substrate partially overlaps with the orthographic projection of the to-be-etched area on the substrate; After the ion implantation process is performed, the method further includes: removing the sidewall whose orthographic projection is located within the orthographic projection of the to-be-etched area on the substrate.
7. The method for manufacturing a semiconductor structure according to claim 6, It is characterized in that Before removing the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate, an ion implantation process is performed on the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate, so that the etching rate of the side wall whose orthographic projection is located within the orthographic projection of the area to be etched on the substrate is greater than the etching rate of the gap area.
8. A semiconductor structure, It is characterized in that include: A substrate and at least two discrete protrusions located on the substrate; wherein the top width of the protrusions is greater than the bottom width; a barrier layer, the barrier layer being filled between adjacent protrusions; wherein the barrier layer comprises a gap region and an intermediate region, the gap region being located between the protrusion and the substrate in a direction perpendicular to the substrate, and having doping ions in the gap region; in the arrangement direction of the protrusions, the barrier layer between adjacent protrusions has two separate grooves; the sidewalls of the grooves are perpendicular to the substrate; or, in a direction away from the substrate, the width of the grooves increases; The middle region is located between adjacent grooves, and the concentration of doping ions on two opposite sides of the middle region is greater than the concentration of doping ions at a middle position of the middle region.
9. The semiconductor structure according to claim 8, It is characterized in that The depth-to-width ratio of the groove is 4:1-6:
1.
10. The semiconductor structure according to any one of claims 8 to 9, It is characterized in that The protrusion includes a conductive layer and a side wall located on the side of the conductive layer; The gap region is located between the protrusion and the substrate, which specifically includes: the gap region is located between the side wall and the substrate.
Citation Information
Patent Citations
Method for manufacturing self-alignment metal interconnection wire
CN102034734A
Forming method of semiconductor structure, and semiconductor structure
CN103928383A
Manufacture method of floating gates
CN105206520A
Semiconductor device, fabrication method thereof and electronic device
CN107993978A
Method for forming self-aligned grooves
CN110349906A