Special ammonium nitrate fuel oil explosive for underground inclined upward blast hole, and preparation method thereof
An ammonium explosive, oblique upward technology, applied in explosive processing equipment, explosives, non-explosive/non-thermal agent components, etc., can solve the problems of high mixing labor intensity, affecting the operation cycle, scattered explosives, etc., to reduce moisture The effect of risk, improving operation efficiency, and high success rate of charging
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2021-08-10
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
technical field
[0001] The invention belongs to the technical field of industrial explosives, and in particular relates to an ammonium oil explosive specially used for obliquely upward blastholes in downholes and a production process thereof. Background technique
[0002] Ammonium oil explosives have excellent blasting performance and are widely used in open-pit and underground non-coal mining blasting. Underground blasting operations require on-site preparation of explosives, but usually the site environment is relatively poor, staffing is reduced, and operating conditions are limited.
[0003] When conventional powdery and granular ammonium oil explosives are used in upward blastholes, due to the upward / oblique upward angle, the charge will encounter the problem of explosives falling down, the blasting effect is poor, and it is easy to generate static electricity, which is dangerous and mixed. The labor intensity is high and the charging efficiency is low, which affects t...
Examples
Embodiment 1
[0030] An ammonium oil explosive specially used for obliquely upward blastholes in underground mines, the raw materials of which are the following components by weight percentage: 87% of porous granular ammonium nitrate, 2.4% of polyacrylamide, 4.8% of diesel oil, and 5.8% of binder.
[0031] The raw material of the adhesive is the following components by weight percentage: 37.60% of porous granular ammonium nitrate, 0.77% of polyacrylamide, 53.93% of water, and 7.70% of polyethylene glycol.
[0032] The adhesive is prepared at least one day before the production of the sticky explosive, and the preparation includes the following steps:
[0033] 1) Weigh water and polyethylene glycol in proportion and stir evenly until there is no obvious layering phenomenon to obtain a mixture;
[0034] 2) Weighing porous granular ammonium nitrate into the above mixture, heating and stirring when adding, heating temperature ≤ 70 ° C, until the porous granular ammonium nitrate is completely di...
Embodiment 2
[0041] An ammonium oil explosive specially used for obliquely upward blastholes in downholes, the raw materials of which are the following components by weight percentage: 86.6% of porous granular ammonium nitrate, 2.5% of polyacrylamide, 4.8% of diesel oil, and 6.1% of binder.
[0042] The raw materials of the binder are the following components in weight percentage: 37.00% of porous granular ammonium nitrate, 0.80% of polyacrylamide, 54.25% of water, and 7.95% of polyethylene glycol.
[0043] The adhesive is prepared at least one day before the production of the sticky explosive, and the preparation includes the following steps:
[0044] 1) Weigh water and polyethylene glycol in proportion and stir evenly until there is no obvious layering phenomenon to obtain a mixture;
[0045] 2) Weighing porous granular ammonium nitrate into the above mixture, heating and stirring when adding, heating temperature ≤ 70 ° C, until the porous granular ammonium nitrate is completely dissolve...
Embodiment 3
[0052] An ammonium oil explosive specially used for obliquely upward blastholes in underground mines, the raw materials of which are the following components by weight percentage: 86% of porous granular ammonium nitrate, 2.6% of polyacrylamide, 5.2% of diesel oil, and 6.2% of binder.
[0053]The raw materials of the adhesive are the following components by weight percentage: 37.80% of porous granular ammonium nitrate, 0.70% of polyacrylamide, 53.70% of water, and 7.80% of polyethylene glycol.
[0054] The adhesive is prepared at least one day before the production of the sticky explosive, and the preparation includes the following steps:
[0055] 1) Weigh water and polyethylene glycol in proportion and stir evenly until there is no obvious layering phenomenon to obtain a mixture;
[0056] 2) Weighing porous granular ammonium nitrate into the above mixture, heating and stirring when adding, heating temperature ≤ 70 ° C, until the porous granular ammonium nitrate is completely d...