Secondary battery and method for manufacturing the same
By increasing the heat supply near the electrode terminals of the secondary battery and improving the bonding strength between the electrode plates and the separators, the problem of reduced adhesion between the electrode plates and the separators in the prior art is solved, and the output performance of the battery is improved.
Patent Information
- Application Number
- CN202110804176.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-07-27
- Filing Date
- 2021-07-16
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2041-07-16
AI Technical Summary
During the thermo-compression bonding process of existing secondary batteries between electrode plates and separators, heat dissipation is better at the outer periphery, resulting in reduced adhesion in the central portion, which easily leads to peeling of the electrode plates and separators, thereby reducing the output performance of the battery.
By increasing the supply of heat near the electrode terminal, the bonding strength between the electrode plate and the spacer in this area is higher than that in other areas. The terminal heating part of the hot plate is used to apply additional heat to the electrode terminal part to improve the bonding strength.
It effectively improves the bonding strength between the electrode plate and the spacer near the electrode terminal, suppresses the decrease in battery output performance, and ensures the stable performance of the battery.
Smart Images

Figure CN113991159B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates to a secondary battery and a method of manufacturing the same. Background Art
[0002] As described in Japanese Patent Application Laid-Open No. 2018-56142 (Patent Document 1), as a structure of an electrode body for a secondary battery such as a lithium ion battery, a structure in which an electrode plate and a separator with an adhesive layer are stacked and thermally pressed together is known.
[0003] When the stack of the pole plate and the spacer is heated and pressed from top to bottom for thermocompression bonding, the outer peripheral portion of the stack is easier to dissipate heat than the central portion, so the bonding force between the pole plate and the spacer tends to be easily reduced compared to the central portion. If the bonding force between the pole plate and the spacer is reduced, the pole plate and the spacer may be peeled off unintentionally. As a result, the distance between the pole plates increases, the resistance increases, and thus the output performance of the battery may be reduced. In particular, the vicinity of the electrode terminal is a portion where the current is concentrated, so the above-mentioned peeling has a greater impact in this portion than in other portions. Summary of the invention
[0004] An object of the present disclosure is to provide a secondary battery and a method for manufacturing the same in which the bonding strength between an electrode plate and a separator in the vicinity of an electrode terminal is improved.
[0005] The secondary battery involved in the present disclosure includes: a plate including a main body and an electrode terminal part protruding from the main body along a first direction, and a spacer bonded to the plate, the main body of the plate including: a central area located near the center of the first direction, a first area located on a side close to the electrode terminal part relative to the central area in the first direction, and a second area located on an opposite side of the first area relative to the central area in the first direction, the bonding strength per unit area between the plate and the spacer in the first area is higher than the bonding strength per unit area between the plate and the spacer in the second area.
[0006] The manufacturing method of a secondary battery involved in the present disclosure includes: a process of stacking an electrode plate including a main body and an electrode terminal portion protruding from the main body along a first direction and a spacer, and a process of thermally bonding the stacked electrode plate and the spacer, the main body of the electrode plate includes: a central area located near the center of the first direction, a first area located on a side close to the electrode terminal portion relative to the central area in the first direction, and a second area located on an opposite side of the first area relative to the central area in the first direction, and in the thermal bonding process, the heat per unit area applied to the first area is greater than the heat per unit area applied to the second area.
[0007] According to the present disclosure, it is possible to improve the bonding strength between the electrode plate and the separator in the vicinity of the electrode terminal of the secondary battery, thereby suppressing a decrease in the output performance of the battery.
[0008] The foregoing and other objects, features, aspects and advantages of the present invention will become more apparent from the following detailed description of the present invention when read in conjunction with the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 It is a diagram showing a thermal bonding step in the method for manufacturing a secondary battery according to one embodiment of the present disclosure.
[0010] Figure 2 To express the use Figure 1 Graph showing the distribution of bonded portions formed by the thermal bonding step shown in FIG.
[0011] Figure 3 It is a figure which shows the thermal bonding process concerning a comparative example.
[0012] Figure 4 This is a diagram for explaining heat dissipation from the electrode plate in the thermal bonding process.
[0013] Figure 5 It is a diagram showing components of an electrode body of a secondary battery according to one embodiment of the present disclosure.
[0014] Figure 6 To indicate the use Figure 5 Figure 2 is a diagram of an electrode body formed by the constituent elements shown in FIG.
[0015] Figure 7 To express Figure 6 2 is a diagram showing the arrangement of the positive electrode plate, the negative electrode plate, and the separator in the electrode body shown in FIG.
[0016] Figure 8 The diagram shows the arrangement of the cut-out region and the measurement region for measuring the bonding strength between the electrode plate and the separator.
[0017] Fig. 9 For use in Figure 8 The shapes of the cut-out regions and assay regions shown in the figures are explained in more detail.
[0018] Fig.10 To indicate the measurement Figure 8 FIG. 4 is a diagram showing a process of cutting out a region and measuring the bonding strength between the electrode plate and the separator in the region shown in FIG.
[0019] Fig.11 It is a cross-sectional view showing a state where a separator and an electrode plate are bonded together.
[0020] Fig.12 To indicate from Fig.11 : is a cross-sectional view of the adhesive mark when the separator is peeled off in the state shown in .
[0021] Fig.13 To express Figure 8 Graphs showing measurement results (peel strength) in measurement areas A to D shown in FIG.
[0022] Fig.14 To express Figure 8 Graphs showing measurement results (adhesion mark concentrations) in measurement areas A to D shown in FIG. DETAILED DESCRIPTION
[0023] Hereinafter, the embodiments of the present disclosure will be described. It should be noted that the same reference numerals are given to the same or corresponding parts, and the description thereof may not be repeated.
[0024] Furthermore, in the embodiments described below, when the number, amount, etc. are mentioned, unless otherwise specified, the scope of the present disclosure is not necessarily limited to the number, amount, etc. In addition, in the embodiments described below, each component is not necessarily essential to the present disclosure unless otherwise specified.
[0025] The secondary battery according to the present embodiment is a lithium ion battery, but the scope of the present disclosure is not limited thereto, and other secondary batteries such as a nickel-hydrogen battery may be included, for example.
[0026] Figure 1 1 is a diagram showing a thermal bonding step in a method for manufacturing a secondary battery according to the present embodiment. The secondary battery according to the present embodiment includes an electrode body 100. The secondary battery is formed by housing the electrode body 100 together with an electrolyte in a housing case (not shown).
[0027] The electrode body 100 is manufactured by stacking a positive electrode plate, a negative electrode plate, and a separator between the positive electrode plate and the negative electrode plate, and heat-bonding the electrode plate and the separator while pressing the stack. The electrode body 100 includes a main body 110 and an electrode terminal 120. Figure 1 As shown in FIG. 1 , the electrode body 100 is pressed while being heated by a hot plate 200 . Figure 1 In the example, the hot plate 200 is heated to a substantially uniform temperature.
[0028] The hot plate 200 includes a main body 210 and a terminal heating part 220. The main body 210 includes a first part 211 and a second part 212, and the main body 110 of the electrode body 100 is pressurized by the first part 211 and the second part 212. The terminal heating part 220 includes a first part 221 and a second part 222, and the electrode terminal part 120 of the electrode body 100 is pressurized by the first part 221 and the second part 222.
[0029] When hot plate 200 presses electrode body 100, heat is applied from body 210 of hot plate 200 to body 110 of electrode body 100 along arrow DR210. Also, heat is applied from terminal heating unit 220 of hot plate 200 to electrode terminal 120 of electrode body 100 along arrow DR220.
[0030] Figure 2 To express the use Figure 1 The distribution of the bonding portion AD formed by the thermal bonding process shown in FIG. Figure 2 As shown in FIG. 1 , the electrode plate 10 includes a rectangular main body 11 and an electrode tab 12 (electrode terminal portion) protruding from the main body 11. The electrode tab 12 extends from the main body 11 to the electrode terminal portion. Figure 2 It is formed in a protruding manner on the upper side.
[0031] When the electrode plates 10 and the separators are stacked, the main body 11 constitutes the main body 110 of the electrode body 100 , and the electrode tabs 12 constitute the electrode terminal 120 of the electrode body 100 .
[0032] Dot-shaped adhesive portions AD are formed on the main body 110. The adhesive portions AD are portions that exert adhesive force between the electrode plate 10 and the separator. Figure 2 As shown in FIG. 1 , the bonding portion AD is formed at a relatively high density on the side close to the electrode pad 12 . That is, a relatively high bonding strength is obtained on the side close to the electrode pad 12 .
[0033] Figure 3 FIG. 2 is a diagram showing a thermal bonding process according to a comparative example. Figure 3 In the comparative example shown in FIG, no Figure 1 The terminal heating part 220 shown in FIG. The main body 110 of the electrode body 100 is heated from the main body 210 of the hot plate 200 along the arrow DR210, thereby forming a bonding part between the electrode plate and the separator, and the electrode terminal part 120 is not directly heated. Figure 3 In the example of FIG. 1 , the hot plate 200 is also heated to a substantially uniform temperature.
[0034] Second, use Figure 4 The heat dissipation from the electrode body 100 during the thermal bonding process will be described. Figure 4 As shown in , in the thermal bonding process, heat is released from the outer periphery of the main body 110 of the electrode body 100 in the direction of arrow H. Thus, heat is easily dissipated in the outer periphery of the main body 110 compared to the central part, and the temperature during thermal bonding is relatively lower, so the bonding strength between the electrode plate and the separator is easily reduced compared to the central part. If the bonding strength between the electrode plate and the separator is reduced, the electrode plate and the separator may be peeled off unintentionally.
[0035] The electrode plate 10 has an active material layer formed on the core material. Figure 4 The thickness of the active material layer tends to be relatively thin. Therefore, when the electrode plates 10 are stacked, the thickness of the active material layer tends to be relatively thin. Figure 4 Compared with the lower edge of the electrode 10, the distance between the electrode plates 10 is large near the electrode tab 12, and the thermal resistance is large. As a result, it is difficult to obtain sufficient bonding strength, so the above-mentioned unintentional peeling tends to occur easily.
[0036] As a result of the above, the distance between the pole plates 10 increases in the outer periphery of the main body 110 of the electrode body 100, and the resistance may increase. Therefore, the output performance of the battery is reduced. In particular, the vicinity of the electrode terminal portion 120 is the part where the current is concentrated when the battery is working, so the above-mentioned peeling has a greater impact than other parts. Therefore, near the electrode terminal portion 120, it is important to increase the bonding strength between the pole plate 10 and the spacer to stabilize the distance between the pole plates 10.
[0037] In this embodiment, if Figure 1 As shown in FIG. 1 , by providing the terminal heating portion 220 on the hot plate 200, heat input in the direction of arrow DR220 can be performed on the electrode body 100 in addition to heat input in the direction of arrow DR210. Thus, on the side close to the electrode terminal portion 120 ( Figure 1 The right side of Figure 2 and Figure 4 The "first region" located on the upper side of the electrode terminal portion 120 is applied with a lower side ( Figure 1 The left side of Figure 2 and Figure 4 In a state where the heat per unit area is large in the "second region" (the lower side in the figure), the electrode plate 10 and the separator can be thermally bonded.
[0038] That is, in the present embodiment, the thermal bonding process of the electrode plate 10 and the separator includes heating the "first region" on the side of the electrode terminal portion 120 close to the electrode body 100 at a higher temperature than the "second region" on the opposite side. Since the electrode terminal portion 120 is heated by the terminal heating unit 220, the electrode terminal portion 120 side is heated at a relatively high temperature.
[0039] Thus, the main body 110 located near the electrode terminal 120 can be heated at a relatively high temperature without an additional process, thereby improving the bonding strength between the electrode plate 10 and the separator in this portion. Therefore, the bonding strength near the electrode terminal 120 can be improved without reducing productivity.
[0040] The scope of the present disclosure is not limited to the above-mentioned examples. For example, the "first region" of the main body 110 is not necessarily heated at a higher temperature than the "second region". For example, even at the same temperature, by heating the "first region" for a relatively longer time than the "second region", the heat applied to the "first region" can be greater than the heat applied to the "second region".
[0041] Furthermore, the electrode terminal portion 120 does not necessarily need to be heated by the terminal heating portion 220 . For example, by spraying hot air to the electrode terminal portion 120 during the thermal bonding process, additional heat may be applied to the side close to the electrode terminal portion 120 .
[0042] Second, use Figure 5 to Figure 7 , the structure of the electrode body 100 is described in detail. Figure 5 2 is a diagram showing components of the electrode body 100. Figure 6 To indicate the use Figure 5 FIG. 1 is a diagram of an electrode body 100 formed by the constituent elements shown in FIG. Figure 7 2 is a diagram showing the arrangement of electrode plates and separators in the electrode assembly 100 .
[0043] like Figure 5 to Figure 7 As shown in , the electrode body 100 is formed by stacking a plurality of electrode plates 10 including a positive electrode plate 10A and a negative electrode plate 10B and a separator 13. The positive electrode plates 10A and the negative electrode plates 10B are alternately stacked via separators 13. The positive electrode plate 10A has a main body 11A and an electrode tab 12A, and the negative electrode plate 10B has a main body 11B and an electrode tab 12B.
[0044] As an example, the positive electrode plate 10A is formed by providing positive electrode composite layers on both sides of a core material composed of an aluminum foil having a thickness of 13 μm. The single-sided thickness of the positive electrode composite layer after compression treatment is 62 μm. The positive electrode composite layer contains LiNiCoMnO2 (positive electrode active material), acetylene black (conductive material) and PVDF [polyvinylidene fluoride resin] (binder) in a mass ratio of 97:2:1. The width of the main body 11A of the positive electrode plate 10A in the short side direction is 76.5 mm, and the width in the long side direction is 138.9 mm. The protrusion of the electrode tab 12A is 19.6 mm.
[0045] As an example, the negative electrode plate 10B is formed by providing negative electrode composite layers on both sides of a core material composed of a copper foil having a thickness of 8 μm. The single-sided thickness of the negative electrode composite layer after compression treatment is 76 μm. The negative electrode composite layer contains graphite (negative electrode active material), CMC [carboxymethyl cellulose] (thickener) and SBR [styrene-butadiene copolymer] (binder) in a mass ratio of 98:1:1. The width of the main body 11B of the negative electrode plate 10B in the short side direction is 78.2 mm, and the width in the long side direction is 142.8 mm. The protrusion of the electrode tab 12B is 18.2 mm.
[0046] As an example, the spacer 13 is a strip-shaped member in which a ceramic heat-resistant layer is applied on one side of a polyethylene single-layer substrate, and an adhesive layer composed of an acrylic resin is applied on both sides in the form of dots. The amount of adhesive in each dot is roughly the same. The number density of dots is roughly constant on one side of the spacer. The thickness of the substrate layer in the spacer 13 is 12 μm, and the thickness of the heat-resistant layer is 4 μm. The width of the spacer 13 is 80.7 mm.
[0047] As an example, the electrode body 100 is made using the positive electrode plate 10A, the negative electrode plate 10B and the separator 13 involved in the above-mentioned example. The electrode plates 12A and 12B of the positive electrode plate 10A and the negative electrode plate 10B are arranged in a manner that they do not overlap each other, and the positive electrode plates 10A and the negative electrode plates 10B are alternately stacked via the separator 13, thereby making the electrode body 100 as a stack. The number of stacking layers of the positive electrode plate 10A is 35, and the number of stacking layers of the negative electrode plate 10B is 36. The electrode body 100 is heated and pressurized using a hot plate 200 heated to a set temperature of 115°C. At this time, a pressure of 2MPa is continuously applied from both sides of the electrode body 100 for 57 seconds.
[0048] Next, an example of a method for measuring the bonding strength and a measurement result using the method will be described. In particular, the electrode body 100 involved in the above example is used as a measurement object, and heating using the terminal heating unit 220 is performed as an "Example" (see Figure 1 ) and as a "comparative example" the case where heating by the terminal heating unit 220 is not performed (other conditions are the same) (refer to Figure 3 ) are described below.
[0049] Figure 8 The diagram shows the arrangement of the cut-out region and the measurement region for measuring the adhesive strength. Fig. 9 FIG. 2 is a diagram showing the cutout region 20A in more detail. Fig.10 It is a diagram showing a process of measuring the bonding strength between the positive electrode plate 10A and the separator 13 .
[0050] like Figure 8As shown in FIG. 1 , the cut-out regions 20A to 20D each include measurement regions A to D. The measurement regions A, B, and D are located at the periphery of the main body 11A of the positive electrode plate 10A. The measurement region A is located directly below the electrode tab 12A, and the measurement regions B and D are located in the long side direction ( Figure 8 The measurement areas A and B are the "first area" located on the side of the main body 11A close to the electrode pad 12A. The measurement area D is the "second area" located on the side of the main body 11A opposite to the electrode pad 12A. The measurement area C is located in the short side direction of the main body 11A (first direction: Figure 8 The up-down direction in the image) and the long side direction (the second direction: Figure 8 The “central area” near the center (in the left-right direction).
[0051] First, the positive electrode plate 10A located at the center in the thickness direction (the 18th layer among the 35 layers) is taken out from the electrode body 100 after heating and pressing. Figure 8 , Fig. 9 The cutout regions 20A to 20D shown in FIG. 5 are cut out as samples (20 mm×70 mm).
[0052] Secondly, if Fig.10 As shown in FIG. 1 , a double-sided tape 30 (NW-20 manufactured by NICHIBAN Co., Ltd.) is attached to one positive electrode composite layer of the positive electrode plate 10A sample and fixed to a smooth plastic substrate. Next, the spacer 13 is stretched in a direction of 90° relative to the substrate surface, and the spacer 13 is stretched along the positive electrode layer. Fig. 9 One end of the spacer 13 in the long side direction of the sample was fixed to the movable clamp 40 of the digital dynamometer (FGP-5 manufactured by Nidec Synpo Co., Ltd.) in such a manner that the sample (test piece) was peeled off in the direction of the arrow DR20. Then, the movable clamp 40 was moved in such a manner that the positive electrode composite layer of the sample (test piece) and the spacer were peeled off at a speed of 50 mm / min. The direction of stretching was always maintained at 90° relative to the substrate surface of the plastic substrate to which the sample (test piece) was fixed.
[0053] For example, in the case of measuring the cutout region 20A, Fig. 9 The average value of the force applied to the digital dynamometer measured at 0.1 mm intervals during peeling in the measurement area A (20 mm × 20 mm) shown in the figure is defined as the peel strength (peel strength) between the positive electrode composite layer and the separator. The same applies to the cut-out areas 20B to 20D. The peel strength (peel strength) corresponds to the "bonding strength per unit area" between the electrode plate 10 and the separator 13 in this portion.
[0054] Second, use Fig.11 , Fig.12, the bonding marks between the electrode plate 10 and the separator 13 will be described. Fig.11 1 is a cross-sectional view showing a state where the separator 13 is bonded to the positive electrode plate 10A. Fig.12 To indicate from Fig.11 The state shown in FIG. 1 is a cross-sectional view of a state in which the spacer 13 is peeled off.
[0055] like Fig.11 As shown in FIG. 1 , the main body 11A of the positive electrode plate 10A is bonded to the separator 13 via the adhesive 14 . The separator 13 includes a base material 13A and a heat-resistant layer 13B. The heat-resistant layer 13B and the main body 11A of the positive electrode plate 10A are bonded to each other via the adhesive 14 .
[0056] The base material 13A of the spacer 13 and the heat-resistant layer 13B are bonded with a relatively weak force of about 5 to 7 N / m. Fig.10 When a peel test (peel test) is performed by the method shown in , the adhesive 14 is not peeled off from the positive electrode plate 10A and the heat-resistant layer 13B, but the heat-resistant layer 13B is peeled off from the substrate 13A. That is, since the bonding strength between the substrate 13A of the separator 13 and the heat-resistant layer 13B is weak, if the separator 13 is to be peeled off, the heat-resistant layer 13B and the adhesive 14 remain as "transfer marks" on the positive electrode plate 10A. As a result, the bonded portion is transferred to the surface of the positive electrode plate 10A in a white color. By binarizing the image of the surface taken by a camera, scanner, etc., it is possible to calculate the bonding mark concentration = [(white area) / (black area)] as the "ratio of the area occupied by the transfer mark".
[0057] Fig.13 To express Figure 8 , which is a graph showing the measurement results of the peel strength (peel strength) in the measurement areas A to D shown in, Fig.14 It is a figure which shows the measurement result of the adhesion mark density in the measurement area|region A-D. Fig.13 , Fig.14 The results shown in the Figure 8 The measurement areas A to D shown in FIG. 1 are the results of measuring the peel strength (peel strength) and the adhesion mark concentration under the above-mentioned specific conditions.
[0058] exist Fig.13 , Fig.14 In the embodiment, "heating with electrode plate" is as follows Figure 1 The measurement results when the main body 110 and the electrode terminal 120 of the electrode body 100 are heated and pressurized as shown in the "No electrode sheet heating" (comparative example) are as follows Figure 3 ] is a measurement result when only the main body 110 of the electrode body 100 is heated and pressurized as shown in FIG.
[0059] like Fig.13As shown in the figure, in the case of "electrode-free pole piece heating" involved in the comparative example, the peel strengths of measurement areas A, B, and D located on the periphery of the main body 11A in the positive electrode plate 10A (A: 3.60, B: 3.61, D: 3.61 [N / m]) are approximately the same, and the peel strength of measurement area C located near the center of the main body 11A (4.13 [N / m]) is higher than the peel strengths of measurement areas A, B, and D.
[0060] In the case of "heating with electrode pad" in the embodiment, the side close to the electrode pad 12A ( Figure 8 The peel strength of measurement areas A and B (A: 4.60, B: 4.54 [N / m]) on the upper side of the electrode sheet 12A increased. The peel strength of measurement areas C and D (C: 4.16, D: 3.60 [N / m]) was roughly the same as the case of "no electrode sheet heating". As a result, the peel strength of measurement areas A and B located on the electrode sheet 12A side was higher than the peel strength of measurement areas C and D.
[0061] From the perspective of achieving stable adhesion on the side close to the electrode sheet 12A, the peel strength of measurement areas A and B is equal to or higher than the peel strength of measurement area C, that is, when measured using the above-mentioned measurement method, it is preferably 4.2 [N / m] or higher.
[0062] like Fig.14 As shown in FIG. 1 , in the case of “no electrode sheet heating” according to the comparative example, the adhesion mark concentrations of the measurement areas A, B, and D located on the periphery of the main body 11A of the positive electrode plate 10A (A: 1.49, B: 2.9, D: 2.9 [ppm×10 3 ]) or slightly lower in measurement area A, while the adhesion mark concentration in measurement area C located near the center of the main body 11A (5.7 [ppm × 10 3 ]) is higher than the adhesion mark concentration in measurement areas A, B, and D.
[0063] In the case of "heating with electrode pad" involved in the embodiment, the electrode pad 12A side ( Figure 8 The adhesion mark concentrations of the measurement areas A and B (A: 30.9, B: 27.4 [ppm×10 3 The concentration of adhesive marks in the measurement areas C and D (C: 7.3, D: 3.9 [ppm × 10 3 ]) is not much different from the case of "no electrode sheet heating". As a result, the adhesion mark concentration of the measurement areas A and B located on the electrode sheet 12A side is higher than that of the measurement areas C and D.
[0064] From the viewpoint of achieving stable adhesion on the side close to the electrode pad 12A, the adhesion mark concentration in the measurement areas A and B is equal to or higher than that in the measurement area C, that is, preferably 1.0×10 4 [ppm] or above.
[0065] As described above, in the electrode body 100, the bonding strength per unit area between the positive electrode plate 10A and the separator 13 in the measurement area A, B (first area) located on the side close to the electrode tab 12A is higher than the bonding strength per unit area between the positive electrode plate 10A and the separator 13 in the measurement area D (second area) located on the opposite side of the measurement area A, B relative to the measurement area C (central area). This is considered to be because, in the thermal bonding process between the electrode plate and the separator, the heat per unit area applied to the measurement area A, B is greater than the heat per unit area applied to the measurement area D. The above is similarly realized in at least a part, preferably all, of the positive electrode plate 10A and the negative electrode plate 10B constituting the electrode body 100.
[0066] It should be noted that the scope of the present disclosure is not limited to forming the adhesive layer (adhesive 14) in dots on the surface of the separator 13, and the present disclosure also includes a structure in which the adhesive layer is formed on the entire surface of the separator, a structure in which the separator itself has adhesiveness, and a structure in which the adhesive layer is formed on the surface of the positive electrode plate and the negative electrode plate. That is, as long as there is an adhesive layer between the separator and the electrode plate (including the separator itself), it will suffice.
[0067] In addition, in the present disclosure, the material and shape of the adhesive layer are not particularly limited, and known materials can be appropriately selected for use. The adhesive layer can be formed by a plurality of adhesive particles. The adhesive layer can be welded, or can be softened by heating and enter the concave and convex parts of the surface of the electrode plate or even the separator, thereby bonding the electrode plate and the separator.
[0068] Although the embodiments of the present invention have been described, it should be understood that the embodiments disclosed this time are illustrative in all aspects and are not restrictive. The scope of the present invention is indicated by the claims, and it is intended to include all modifications within the meaning and scope equivalent to the claims.
Claims
1. A secondary battery comprising: A pole plate comprising a main body and an electrode terminal portion protruding from the main body along a first direction, a spacer bonded to the pole plate, and an adhesive layer arranged between the spacer and the pole plate, wherein the main body of the pole plate comprises: a central area located near the center of the first direction, a first area located on a side close to the electrode terminal portion relative to the central area in the first direction, and a second area located on an opposite side of the first area relative to the central area in the first direction, wherein the bonding strength per unit area between the pole plate and the spacer in the first area is higher than the bonding strength per unit area between the pole plate and the spacer in the second area.
2. The secondary battery according to claim 1, wherein The bonding strength per unit area between the electrode plate and the separator in the first region is greater than or equal to the bonding strength per unit area between the electrode plate and the separator in the central region.
3. The secondary battery according to claim 1 or claim 2, wherein: When the separator having a width of 20 mm was peeled off from the electrode plate at a rate of 50 mm / min, the bonding strength between the electrode plate and the separator in the first region was 4.2 N / m or more.
4. The secondary battery according to claim 1, wherein The adhesion mark concentration in the first region when the separator is peeled off from the electrode plate is 1.0×10 4 ppm or above.
5. The secondary battery according to claim 1, wherein The electrode plate has a first thickness in the first region and a second thickness in the second region, wherein the first thickness is thinner than the second thickness.
6. The secondary battery according to claim 1, wherein A plurality of the electrode plates are provided, the plurality of electrode plates include a positive electrode plate and a negative electrode plate, and the positive electrode plates and the negative electrode plates are alternately stacked with the separator interposed therebetween.
7. The secondary battery according to claim 1, wherein The secondary battery is a lithium ion battery.
8. A method for manufacturing a secondary battery, comprising: A process of stacking an electrode plate including a main body and an electrode terminal portion protruding from the main body along a first direction and a spacer, and a process of thermally bonding the stacked electrode plate and the spacer, wherein the main body of the electrode plate includes: a central area located near the center of the first direction, a first area located on a side close to the electrode terminal portion relative to the central area in the first direction, and a second area located on an opposite side of the first area relative to the central area in the first direction, and in the thermal bonding process, the heat per unit area applied to the first area is greater than the heat per unit area applied to the second area, so that the bonding strength per unit area between the electrode plate and the spacer in the first area is higher than the bonding strength per unit area between the electrode plate and the spacer in the second area.
9. The method for manufacturing a secondary battery according to claim 8, wherein: The step of thermal bonding includes heating the first region at a higher temperature than the second region.
10. The method for manufacturing a secondary battery according to claim 8 or claim 9, wherein: The thermal bonding step includes heating the electrode terminal portion.
11. The method for manufacturing a secondary battery according to claim 10, wherein: The thermal bonding step includes applying pressure while heating the electrode terminal portion.
12. The method for manufacturing a secondary battery according to claim 8, wherein: The step of thermal bonding includes heating the first region for a longer period of time than heating the second region.
13. The method for manufacturing a secondary battery according to claim 8, wherein: The secondary battery is a lithium ion battery.