Metal oxide semiconductor field effect transistor and manufacturing method thereof

By adopting epitaxial layer and implantation zone structures with different conductivity types in metal oxide semiconductor field effect tubes, combined with ion implantation technology, the problems of high on-resistance and large leakage current are solved, and low on-resistance and high output are achieved The balance of current improves the voltage withstandability and power quality of the device.

CN114203823BActive Publication Date: 2024-12-06XI'AN UNIVERSITY OF ARCHITECTURE AND TECHNOLOGY
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111490719.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-08
Publication Date
2024-12-06
Estimated Expiration
2041-12-08

AI Technical Summary

Technical Problem

While the existing metal oxide semiconductor type field effect tubes increase the on-resistance and output current, it is difficult to maintain low leakage current and high breakdown voltage, resulting in a decrease in power quality factor.

Method used

Two epitaxial layers with different conductivity types are formed on the silicon-germanium alloy substrate, and multiple implantation regions with different conductivity types are formed in the trench. The shielded gate electrode and interpole isolation layer are formed through ion implantation technology to reduce conduction. Resistance, improve voltage withstandness.

Benefits of technology

It effectively reduces the on-resistance, improves the working performance and avalanche resistance of the field effect tube, and improves the voltage resistance and power quality factor of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114203823B_ABST
    Figure CN114203823B_ABST
Patent Text Reader

Abstract

The present invention discloses a metal oxide semiconductor field effect transistor and a manufacturing method thereof, which mainly solves the problems of too high on-resistance and too large saturation current of the existing field effect transistor. The field effect transistor comprises: a substrate, two epitaxial layers, a groove, an insulating layer, a gate oxide layer, a shielding gate electrode, an inter-electrode isolation layer, a gate electrode, three injection regions and two dielectric layers; the manufacturing method comprises: firstly, forming a first and a second epitaxial layer of different conductivity types on the substrate by epitaxial growth technology, adopting a groove structure extending from the second epitaxial layer to the first epitaxial layer, then sequentially generating an insulating layer, a gate oxide layer, a shielding gate electrode, an inter-electrode isolation layer and a gate electrode in the groove, and finally forming a first injection region and two second and third injection regions of different conductivity types in the second epitaxial layer by ion implantation technology, and coating a dielectric layer. The present invention effectively improves the working performance of the field effect transistor, and has the characteristics of low on-resistance and strong voltage resistance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention belongs to the technical field of semiconductor devices, and in particular relates to a metal oxide semiconductor field effect transistor, which can be used to manufacture power devices, digital logic circuit devices or power electronic devices. Background Art

[0002] Field effect transistor, also known as unipolar transistor, is a semiconductor device that uses the electric field effect of the control input loop to control the output loop current. It is usually divided into junction type and metal oxide semiconductor type. Field effect transistors are conducted by the majority of carriers, and have the advantages of high input resistance, low noise, low energy consumption, large dynamic range, easy integration, and no secondary breakdown. And with these advantages, field effect transistors have become a strong competitor to the other two types of transistors. Metal oxide semiconductor field effect transistors are a switching device. Changing the applied voltage on the gate can control the current between the drain and the source. On-resistance, output current, leakage current and breakdown voltage are important indicators used to evaluate the performance of metal oxide semiconductor field effect transistors. Trench gate metal oxide semiconductor field effect transistor is a new type of vertical structure field effect transistor developed on the basis of metal oxide semiconductor field effect transistors. Due to its low on-resistance and low gate and drain charge density, it has the characteristics of low power loss and fast switching speed.

[0003] In the design of metal oxide semiconductor field effect transistors, although increasing the distance between the gate and the drain and reducing the channel doping concentration can reduce the leakage current and increase the breakdown voltage, it will lead to a significant increase in on-resistance, increased conduction loss, and may even reduce the power quality factor of the field effect transistor. Therefore, it is difficult to prepare a high power quality factor field effect transistor with excellent characteristics such as low on-resistance, large output current, low leakage current and high breakdown voltage at the existing technical level. Summary of the invention

[0004] The purpose of the present invention is to address the deficiencies of the above-mentioned prior art and propose a metal oxide semiconductor field effect transistor and a method for manufacturing the same, which is used to solve the problems of the existing field effect transistor having too high on-resistance and too large saturation current. First, a first epitaxial layer and a second epitaxial layer are formed on a substrate by epitaxial growth technology, and then an insulating layer, a gate oxide layer, a shielding gate electrode, an inter-electrode isolation layer and a gate electrode are sequentially generated in the trench, and finally three implantation regions are formed by ion implantation technology, and a dielectric layer is coated. The present invention effectively improves the working performance of the field effect transistor, and has the characteristics of low on-resistance and strong voltage resistance.

[0005] To achieve the above-mentioned purpose, the present invention proposes a metal oxide semiconductor field effect transistor, comprising: a substrate, two epitaxial layers, a trench 4, an insulating layer 5, a gate oxide layer 6, a shielding gate electrode 7, an inter-electrode isolation layer 8, a gate electrode 9, three injection regions and two dielectric layers; wherein the substrate is a silicon germanium alloy substrate 1, which is located at the bottom layer;

[0006] The two epitaxial layers are respectively a first epitaxial layer 2 of a first conductivity type and a second epitaxial layer 3 of a second conductivity type, which are formed from bottom to top on a silicon-germanium alloy substrate 1;

[0007] The trench 4 penetrates the second epitaxial layer 3 and extends into the first epitaxial layer 2 , and a shielding gate electrode 7 and a gate electrode 9 are formed inside the trench 4 ;

[0008] The shielding gate electrode 7 is located at the bottom of the trench 4, and there is an insulating layer 5 between the shielding gate electrode 7 and the inner wall of the trench; an inter-electrode isolation layer 8 is formed on the upper surface of the shielding gate electrode 7, and a gate electrode 9 is formed on the isolation layer. A gate oxide layer 6 is formed between the gate electrode 9 and the inner wall of the trench 4;

[0009] The three injection regions are all formed in the second epitaxial layer 3, namely, the first injection region 10, the second injection region 11 and the third injection region 12; wherein the first injection region 10 is formed between the trenches 4; the second injection region 11 is of the second conductivity type, formed in the middle of the upper surface of the first injection region 10, and the top is flush with the upper surface of the second epitaxial layer 3; the third injection region 12 is of the first conductivity type, and is located away from the second injection region 11;

[0010] The two dielectric layers are respectively a first dielectric layer 13 and a second dielectric layer 14 coated on the upper surface of the second epitaxial layer 3 , and the second dielectric layer 14 is located on the first dielectric layer 13 .

[0011] Furthermore, the inter-electrode isolation layer 8 is an isolation layer formed by growing a layer of oxide on the upper surface of the shielding gate electrode 7 through a thermal oxidation process and then dry-etching the oxide.

[0012] Furthermore, the doping concentration of the first injection region 10 is lower than the doping concentration of the second injection region 11 , the doping concentration of the second injection region 11 is higher than the doping concentration of the second epitaxial layer 3 , and the concentration of the third injection region 12 is higher than the concentration of the first injection region 10 .

[0013] Furthermore, the first dielectric layer 13 includes oxide, and the second dielectric layer 14 includes one or more of oxide, nitride, and organic polymer.

[0014] The present invention provides a method for manufacturing a metal oxide semiconductor field effect transistor, comprising the following steps:

[0015] 1) Providing a heavily doped silicon-germanium alloy substrate;

[0016] 2) forming an epitaxial layer on a silicon-germanium alloy substrate, first forming a first epitaxial layer of a first conductivity type, and then forming a second epitaxial layer of a second conductivity type on the first epitaxial layer;

[0017] 3) forming a trench in the epitaxial layer, and forming an insulating layer on the bottom surface and sidewalls of the lower portion of the trench, and forming a gate oxide layer on the upper sidewalls;

[0018] 4) forming a shielding gate electrode in the trench and forming an inter-electrode isolation layer on the upper surface of the shielding gate electrode;

[0019] 5) Filling the gate electrode material and etching back to form a gate electrode;

[0020] 6) forming a first implantation region and a second implantation region of the second conductivity type in the second epitaxial layer through an ion implantation process, and forming a third implantation region of the first conductivity type in the second epitaxial layer and away from the second implantation region;

[0021] 7) Coating a first dielectric layer and a second dielectric layer on the upper surface of the second epitaxial layer.

[0022] Compared with the prior art, the present invention has the following beneficial effects:

[0023] First, the present invention forms two epitaxial layers of different conductivity types on a substrate, forms a first epitaxial layer on a heavily doped silicon germanium substrate, and forms a second epitaxial layer of a second conductivity type on the first epitaxial layer, so that the withstand voltage performance of the device is significantly enhanced;

[0024] Second, the present invention forms multiple implantation regions of different conductivity types in the second epitaxial layer, which can significantly improve the avalanche resistance of the device;

[0025] Third, since the groove of the field effect tube of the present invention adopts a structural design that penetrates the second epitaxial layer and extends into the first epitaxial layer, and a shielding gate electrode is formed in the groove, it is more conducive to reducing the on-resistance of the device, thereby effectively improving the working performance of the field effect tube. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] Figure 1 It is a schematic diagram of the cross-sectional structure of the device of the present invention;

[0027] Figure 2 It is a schematic diagram of the cross-sectional structure of the device of the present invention before the injection region is formed;

[0028] Figure 3 It is a flow chart for realizing the method of the present invention. DETAILED DESCRIPTION

[0029] In order to make the purpose, technical solutions and advantages of the present invention more clearly understood, the present invention is further described below in conjunction with the accompanying drawings and specific embodiments.

[0030] Embodiment 1:

[0031] Reference Figure 1 and Figure 2 The metal oxide semiconductor field effect transistor device proposed in the present invention comprises a silicon germanium alloy substrate 1, a first epitaxial layer 2, a second epitaxial layer 3, a groove 4, an insulating layer 5, a gate oxide layer 6, a shielding gate electrode 7, an inter-electrode isolation layer 8, a gate electrode 9, a first injection region 10, a second injection region 11, a third injection region 12, a first dielectric layer 13, and a second dielectric layer 14. The substrate 1 is the bottom layer; the insulating layer 4 and the gate oxide layer 5 are respectively located at the bottom and the side wall of the groove 3; and the inter-electrode isolation layer 8 is located on the upper surface of the shielding gate electrode 7.

[0032] It includes: a substrate, two epitaxial layers, a trench 4, an insulating layer 5, a gate oxide layer 6, a shielding gate electrode 7, an inter-electrode isolation layer 8, a gate electrode 9, three implantation regions and two dielectric layers; wherein the substrate is a silicon-germanium alloy substrate 1, which is located at the bottom layer;

[0033] The two epitaxial layers are respectively a first epitaxial layer 2 of a first conductivity type and a second epitaxial layer 3 of a second conductivity type, which are formed from bottom to top on a silicon-germanium alloy substrate 1;

[0034] The trench 4 penetrates the second epitaxial layer 3 and extends into the first epitaxial layer 2 , and a shielding gate electrode 7 and a gate electrode 9 are formed inside the trench 4 ;

[0035] The shielding gate electrode 7 is located at the bottom of the trench 4, and there is an insulating layer 5 between the shielding gate electrode 7 and the inner wall of the trench; an inter-electrode isolation layer 8 is formed on the upper surface of the shielding gate electrode 7, and the isolation layer is formed by growing a layer of oxide on the upper surface of the shielding gate electrode 7 by a thermal oxidation process, and then dry etching the oxide; a gate electrode 9 is provided on the inter-electrode isolation layer 8, and there is a gate oxide layer 6 between the gate electrode 9 and the inner wall of the trench 4;

[0036] The three injection regions are all formed in the second epitaxial layer 3, namely the first injection region 10, the second injection region 11 and the third injection region 12; wherein the first injection region 10 is formed between the grooves 4; the second injection region 11 is of the second conductivity type, formed in the middle position of the upper surface of the first injection region 10, and the top is flush with the upper surface of the second epitaxial layer 3; the third injection region 12 is of the first conductivity type, and is located away from the second injection region 11; regarding the doping concentrations of the three injection regions here, in this embodiment, the doping concentration of the first injection region 10 is less than the doping concentration of the second injection region 11, the doping concentration of the second injection region 11 is greater than the doping concentration of the second epitaxial layer 3, and the concentration of the third injection region 12 is greater than the concentration 10 of the first injection region.

[0037] The two dielectric layers are respectively a first dielectric layer 13 and a second dielectric layer 14 coated on the upper surface of the second epitaxial layer 3, and the second dielectric layer 14 is located above the first dielectric layer 13; here, the first dielectric layer 13 includes oxide, and the second dielectric layer 14 includes: one or more of oxide, nitride, and organic polymer.

[0038] Embodiment 2:

[0039] Reference Figure 1-3 The present invention provides a method for manufacturing a metal oxide semiconductor field effect transistor, which is used to obtain the device described in Example 1. The specific implementation steps are as follows:

[0040] Step 1). Providing a heavily doped silicon-germanium alloy substrate;

[0041] Step 2). Forming an epitaxial layer on a silicon-germanium alloy substrate, first forming a first epitaxial layer of a first conductivity type, and then forming a second epitaxial layer of a second conductivity type on the first epitaxial layer;

[0042] Step 3). A trench is formed in the epitaxial layer, and an insulating layer is formed on the bottom surface and sidewalls of the lower portion of the trench, and a gate oxide layer is formed on the upper sidewalls;

[0043] Step 4). Forming a shield gate electrode in the trench and forming an inter-electrode isolation layer on the upper surface of the shield gate electrode;

[0044] Step 5). Filling the gate electrode material and etching back to form a gate electrode;

[0045] Step 6). Let the first conductivity type be N and the second conductivity type be P; through ion implantation, a first implantation region and a second implantation region of the second conductivity type are formed in the second epitaxial layer, and a third implantation region of the first conductivity type is formed in the second epitaxial layer and away from the second implantation region; in this embodiment, the first implantation region is formed by implanting the first conductivity type ions and the second conductivity type ions into the second epitaxial layer in multiple steps; wherein the first conductivity type ions are phosphorus ions, and the implantation concentration is 3e13cm -3 The second conductive type ions are boron ions, with an implantation concentration of 5e15cm -3 The second implantation region is formed by implanting the second conductive type ions into the second epitaxial layer; wherein the second conductive type ions are boron ions, and the implantation concentration is 1e16cm -3 The first conductive type ions are implanted into the second epitaxial layer to form an implantation junction, and the implantation junction is thermally annealed to activate the implanted impurities to form a third implantation region; at this time, the first conductive type ions implanted are phosphorus ions, and their implantation concentration is 3e16cm -3 ; The annealing temperature is between 1400-1800K and the annealing time is 1-8h.

[0046] Step 7). Coating a dielectric layer on the upper surface of the second epitaxial layer. Specifically, firstly coating a first dielectric layer on the upper surface of the second epitaxial layer, and then coating a second dielectric layer on the upper surface of the first dielectric layer; finally completing the manufacture of the entire device.

[0047] Embodiment three:

[0048] Based on the production steps of Example 2, specific parameter values ​​are selected to further provide a specific example of the method of the present invention:

[0049] Step 1: Select the substrate.

[0050] First, a heavily doped silicon-germanium alloy is selected as the starting material and used as a substrate;

[0051] Step 2: Growing the epitaxial layer.

[0052] A first epitaxial layer of a first conductivity type is formed on the silicon-germanium alloy substrate by using epitaxial growth technology; and a second epitaxial layer of a second conductivity type is formed on the first epitaxial layer by using epitaxial growth.

[0053] Step 3: Make the groove.

[0054] A trench penetrating the second epitaxial layer and extending to the first epitaxial layer is formed between the first and second epitaxial layers by dry etching technology. The upper surface width of the trench formed in this embodiment is 0.1-0.8 μm and the depth is 1-2 μm. An insulating layer and a gate oxide layer are formed at the bottom and sidewalls of the trench respectively by thermal oxidation, and the insulating layer is an oxide layer.

[0055] Step 4: Make the gate electrode.

[0056] A shielding gate electrode is formed in the trench, wherein the shielding gate electrode in this embodiment is made of polysilicon; the shielding gate electrode is thermally oxidized to form an inter-electrode isolation layer; a gate electrode material is filled and etched back to form a gate electrode;

[0057] Step 5: Forming the implantation region.

[0058] A first dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the first dielectric layer is an oxide; phosphorus ions and boron ions are implanted into the second epitaxial layer in multiple steps to form a first implantation region; wherein the implantation concentration of the phosphorus ions is 3e13cm -3 The implantation concentration of boron ions is 5e15cm -3 .

[0059] A second dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the second dielectric layer is a composite layer of oxide and nitride; boron ions are implanted into the second epitaxial layer to form a second implantation region of the second conductivity type; wherein the implantation concentration of the boron ions is 1e16cm -3 .

[0060] Phosphorus ions are implanted into the second epitaxial layer to form an implantation junction, and the implantation junction is thermally annealed to activate the implanted impurities to form the third implantation region; wherein the phosphorus ion implantation concentration is 3e16cm -3 , the annealing temperature is between 1400-1800K, and the annealing time is 1-8h.

[0061] Embodiment 4:

[0062] Based on Example 3, this example adjusts some operations and parameters therein, and further provides a specific example of the method of the present invention:

[0063] Steps AB in this embodiment are the same as steps 1-2 in the third embodiment.

[0064] Step C: Making the grooves.

[0065] A trench penetrating the second epitaxial layer and extending to the first epitaxial layer is formed between the first and second epitaxial layers by dry etching technology. The upper surface width of the trench formed in this embodiment is 0.8-1.2 μm and the depth is 3-4 μm. An insulating layer and a gate oxide layer are formed on the bottom and sidewalls of the trench respectively by deposition method, and the insulating layer is an oxide layer.

[0066] Step D: Making a gate electrode.

[0067] A shielding gate electrode is formed in the trench, wherein the shielding gate electrode is made of polysilicon; an inter-electrode isolation layer is formed by a thermal oxidation method and a deposition method; a gate electrode material is filled and etched back to form a gate electrode;

[0068] Step E: forming an implantation region.

[0069] A first dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the first dielectric layer is an oxide; arsenic ions and indium ions are implanted into the second epitaxial layer in multiple steps to form a first implantation region; wherein the implantation concentration of the arsenic ions is 3e13cm -3 The implantation concentration of boron ions is 5e15cm -3 .

[0070] A second dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the second dielectric layer is a composite layer of oxide and organic polymer; indium ions are injected into the second epitaxial layer to form a second injection region of the second conductivity type; wherein the injection concentration of the indium ions is 1e16cm -3 .

[0071] Arsenic ions are implanted into the second epitaxial layer to form an implantation junction, and the implantation junction is thermally annealed to activate the implanted impurities to form the third implantation region; wherein the arsenic ion implantation concentration is 3e16cm -3, the annealing temperature is between 1400-1800K, and the annealing time is 1-8h.

[0072] Embodiment five:

[0073] Based on Example 3, this example adjusts some operations and parameters therein, and further provides a specific example of the method of the present invention:

[0074] Steps ab in this embodiment are the same as steps 1-2 in the third embodiment.

[0075] Step c: Making grooves.

[0076] A trench penetrating the second epitaxial layer and extending to the first epitaxial layer is formed between the first and second epitaxial layers by using a thermal ion etching technique. The upper surface width of the trench formed in this embodiment is 0.1 to 0.8 μm and the depth is 1 to 2 μm. An insulating layer and a gate oxide layer are formed at the bottom and sidewalls of the trench respectively by a deposition method, and the insulating layer is an oxide layer.

[0077] Step d: Making a gate electrode.

[0078] A shielding gate electrode is formed in the trench, wherein the shielding gate electrode is composed of polysilicon; the shielding gate electrode is thermally oxidized to form an inter-electrode isolation layer; a gate electrode material is filled and etched back to form a gate electrode;

[0079] Step e: forming an implantation region.

[0080] A first dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the first dielectric layer is an oxide; phosphorus ions and boron ions are implanted into the second epitaxial layer in multiple steps to form a first implantation region; wherein the implantation concentration of the phosphorus ions is 1e13 cm -3 The implantation concentration of boron ions is 1e15cm -3 .

[0081] A second dielectric layer is coated on the upper surface of the second epitaxial layer, wherein the second dielectric layer is a composite layer of nitride and organic polymer; boron ions are implanted into the second epitaxial layer to form a second implantation region of the second conductivity type; wherein the implantation concentration of the boron ions is 1e16cm -3 .

[0082] Phosphorus ions are implanted into the second epitaxial layer to form an implantation junction, and the implantation junction is thermally annealed to activate the implanted impurities to form the third implantation region; wherein the phosphorus ion implantation concentration is 1e16cm -3 , the annealing temperature is between 1400-1800K, and the annealing time is 1-8h.

[0083] Parts of the present invention that are not described in detail belong to common knowledge among those skilled in the art.

[0084] The above descriptions are only a few specific examples of the present invention. Obviously, for professionals in this field, after understanding the content and principles of the present invention, it is possible to make various modifications and changes in form and details without departing from the principles and structures of the present invention. However, these modifications and changes based on the ideas of the present invention are still within the scope of protection of the claims of the present invention.

Claims

1. A metal oxide semiconductor field effect transistor, It is characterized in that include: A substrate, two epitaxial layers, a groove (4), an insulating layer (5), a gate oxide layer (6), a shielding gate electrode (7), an inter-electrode isolation layer (8), a gate electrode (9), three injection regions and two dielectric layers; wherein the substrate is a silicon-germanium alloy substrate (1) and is located at the bottom layer; The two epitaxial layers are respectively a first epitaxial layer (2) of a first conductivity type and a second epitaxial layer (3) of a second conductivity type, which are formed from bottom to top on a silicon-germanium alloy substrate (1); The trench (4) penetrates the second epitaxial layer (3) and extends into the first epitaxial layer (2), and a shielding gate electrode (7) and a gate electrode (9) are formed inside the trench (4); The shielding gate electrode (7) is located at the bottom of the groove (4) and has an insulating layer (5) between it and the inner wall of the groove; an inter-electrode isolation layer (8) is formed on the upper surface of the shielding gate electrode (7), a gate electrode (9) is located above the isolation layer, and a gate oxide layer (6) is located between the gate electrode (9) and the inner wall of the groove (4); The three injection regions are all formed in the second epitaxial layer (3), and are respectively a first injection region (10), a second injection region (11) and a third injection region (12); wherein the first injection region (10) is formed between the trenches (4); the second injection region (11) is of the second conductivity type and is formed in the middle of the upper surface of the first injection region (10), and the top is flush with the upper surface of the second epitaxial layer (3); the third injection region (12) is of the first conductivity type and is located away from the second injection region (11); The two dielectric layers are respectively a first dielectric layer (13) and a second dielectric layer (14) coated on the upper surface of the second epitaxial layer (3), and the second dielectric layer (14) is located on the first dielectric layer (13).

2. The field effect transistor according to claim 1, Features: The inter-electrode isolation layer (8) is an isolation layer formed by growing a layer of oxide on the upper surface of the shielding gate electrode (7) through a thermal oxidation process and then dry-etching the oxide.

3. The field effect transistor according to claim 1, Features: The doping concentration of the first injection region (10) is lower than the doping concentration of the second injection region (11), the doping concentration of the second injection region (11) is higher than the doping concentration of the second epitaxial layer (3), and the concentration of the third injection region (12) is higher than the concentration of the first injection region (10).

4. The field effect transistor according to claim 1, Features: The first dielectric layer (13) comprises oxide, and the second dielectric layer (14) comprises one or more of oxide, nitride and organic polymer.

5. A method for manufacturing a metal oxide semiconductor field effect transistor, It is characterized in that The steps include: 1) Providing a heavily doped silicon-germanium alloy substrate; 2) forming an epitaxial layer on a silicon-germanium alloy substrate, first forming a first epitaxial layer of a first conductivity type, and then forming a second epitaxial layer of a second conductivity type on the first epitaxial layer; 3) forming a trench in the epitaxial layer, and forming an insulating layer on the bottom surface and sidewalls of the lower portion of the trench, and forming a gate oxide layer on the upper sidewalls; 4) forming a shielding gate electrode in the trench and forming an inter-electrode isolation layer on the upper surface of the shielding gate electrode; 5) Filling the gate electrode material and etching back to form a gate electrode; 6) forming a first implantation region and a second implantation region of the second conductivity type in the second epitaxial layer through an ion implantation process, and forming a third implantation region of the first conductivity type in the second epitaxial layer and away from the second implantation region; 7) Coating a first dielectric layer and a second dielectric layer on the upper surface of the second epitaxial layer.

6. The method according to claim 5, Features: In step 6), the first implantation region is formed by implanting the first conductive type ions and the second conductive type ions into the second epitaxial layer in multiple steps; the first conductive type ions are phosphorus ions with an implantation concentration of 3e13cm -3 The second conductive type ions are boron ions, with an implantation concentration of 5e15cm -3 .

7. The method according to claim 5, Features: The second implanted region of the second conductivity type in step 6) is formed by implanting the second conductivity type ions into the second epitaxial layer; the second conductivity type ions are boron ions with an implantation concentration of 1e16 cm -3 .

8. The method according to claim 5, Features: In step 6), the third implantation region of the first conductivity type is formed by implanting first conductivity type ions into the second epitaxial layer to form an implantation junction, and performing thermal annealing on the implantation junction to activate the implanted impurities.

9. The method according to claim 8, Features: The first conductive type ions are phosphorus ions, and the implantation concentration is 3e16cm -3 ; The annealing temperature is between 1400-1800K and the annealing time is 1-8h.

10. The method according to claim 5, Features: The first conductivity type is N, and the second conductivity type is P.