A high remanence and low coercivity permanent magnetic material and preparation method thereof
By designing a combination of rotating rods and auxiliary mechanisms, the coarse powder of permanent magnet materials was fully mixed, solving the problem of low mixing efficiency in existing equipment and improving material performance.
Patent Information
- Application Number
- CN202211315406.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-10-26
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2042-10-26
AI Technical Summary
Existing mixing equipment has poor mixing efficiency and effect when mixing coarse permanent magnet material powder, which affects the performance of the subsequent permanent magnet material.
A device for preparing permanent magnet materials with high remanence and low coercivity is used, comprising components such as a rotating rod, a driven disk, an elliptical groove, a slider, a pull rope, a reel, a gear, a gear ring, and a flipping plate. The rotating rod drives the driven disk and the elliptical groove to rotate, the slider slides in the elliptical groove to pull the pull rope, which drives the reel and the gear to rotate, the gear ring flipping plate flips the material, and the vibration mechanism accelerates the falling of the material to achieve thorough mixing.
It improves the uniformity of coarse powder mixing, avoids the impact of uneven mixing on the performance of permanent magnet materials, and enhances the mixing effect.
Smart Images

Figure CN115910513B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of permanent magnetic material preparation, in particular to a high remanence and low coercivity permanent magnetic material and a preparation method thereof. Background Art
[0002] Permanent magnetic materials, also known as "hard magnetic materials", are materials that can maintain constant magnetism once magnetized. In the preparation process of permanent magnetic materials, the coarse powder after medium crushing needs to be stirred by a stirring device. However, when stirring the coarse powder, the existing stirring equipment generally directly uses a common stirring rod to stir and mix the materials piled inside the device. This conventional stirring method can only stir the coarse powder at the same horizontal position, which will make the stirring efficiency and stirring effect of the coarse powder poor, which is not conducive to the production and processing of permanent magnetic materials.
[0003] Therefore, to solve these problems, we need a high remanence and low coercivity permanent magnet material and its preparation method. Summary of the invention
[0004] In view of the shortcomings of the prior art, the present invention provides a high remanence and low coercive force permanent magnet material and a preparation method thereof, which has the advantage of being able to fully mix the coarse powder when the permanent magnet material is coarsely powdered and stirred, thereby solving the problem that the coarse powder mixing process is poor and affects the performance of subsequent permanent magnet materials.
[0005] In order to achieve the above-mentioned purpose of fully mixing the coarse powder when the permanent magnetic material is coarsely stirred, the present invention provides the following technical solution: a high remanence and low coercive force permanent magnetic material preparation device, comprising a main body, a rotating rod arranged inside the main body, and a stirring rod arranged on the outer surface of the rotating rod, an auxiliary mechanism is arranged inside the main body, and the auxiliary mechanism includes a driven disk, an elliptical groove, a slider, a pull rope, a mounting rod, a wire wheel, a gear, a gear ring, a flip plate, and a torsion spring. The driven disk is fixedly connected to the outside of the rotating rod, the elliptical groove is opened on the lower surface of the driven disk, the slider is slidably connected to the inner side surface of the elliptical groove, the pull rope is fixedly connected to the bottom of the slider, the mounting rod is fixedly connected to the inner side surface of the main body, the wire wheel is rotatably connected to the inner side surface of the mounting rod, the gear is rotatably connected to the inner side surface of the main body, the gear ring is meshed with the outer surface of the gear, the flip plate is fixedly connected to the outer surface of the gear ring, and the torsion spring is fixedly connected to the outer surface of the wire wheel.
[0006] Furthermore, the auxiliary mechanism also includes a guide rod and a wiring groove. The guide rod is arranged on the inner side of the main body, and the wiring groove is opened on the inner side of the mounting rod. There are two guide rods, and the two guide rods are respectively arranged on the inner side of the main body and the inner side of the mounting rod. The pull rope is slidingly connected to the outer surface of the guide rod, so that the guide rod can guide the direction of the pull rope, thereby avoiding the existence of the pull rope and the internal structure such as the stirring rod. Collision may cause obstruction of the normal operation of the device.
[0007] Furthermore, the pull rope is wound on the outer surface of the pulling wheel, the gear ring is rotatably connected to the outer surface of the mounting rod, and the torsion spring is fixedly connected to the inner side surface of the mounting rod, so that the torsion spring can drive the pulling wheel to rotate in the opposite direction when the pull rope no longer pulls the pulling wheel, thereby allowing the gear ring to maintain a continuous rotation state to turn over the coarse powder.
[0008] Furthermore, a rotating rod is provided on the inner side of the mounting rod, and the wire wheel and the gear are fixedly connected via the rotating rod, so that the rotation of the wire wheel can drive the gear ring to rotate synchronously, and the number of the flip plates is at least three, and all the flip plates are distributed at equal angles on the outer surface of the gear ring.
[0009] Furthermore, a vibration mechanism is arranged inside the main body, and the vibration mechanism includes a coil, a magnetic strip, and a vibration spring. The coil is arranged on the inner side of the driven disk, the magnetic strip is fixedly connected to the outer surface of the slider, and the vibration spring is arranged on the inner side of the mounting rod.
[0010] Furthermore, the position and specifications of the magnetic strip match the coil, and the coil is coupled to the vibration spring, so that when current is intermittently generated inside the coil, the vibration spring can be energized, so that the vibration spring can be compressed, so that the vibration spring can collide with the inner wall of the mounting rod during the recovery process and drive it to vibrate.
[0011] A high remanence and low coercivity permanent magnetic material, the atomic composition of the material is R x Fe a Al b Cu c B d , wherein R is a rare earth element, Fe, Al, Cu, and B represent the chemical elements iron, aluminum, copper, and boron respectively; the R is Nd, Nb, and Dy; the material composition ratios of the elements are: Nd 30%, Nb 0.4%, Dy 0.8%, Fe 67.2%, Al 0.4%, Cu 0.1%, and B 1.1%.
[0012] A method for preparing a high remanence and low coercivity permanent magnetic material comprises the following steps:
[0013] Weigh the various materials required according to the actual proportion of the materials required for the preparation of permanent magnet materials, and send the weighed materials into the furnace for melting and casting; vacuum treatment is required during the melting process to reduce the internal air pressure to below 0.07MPa, and then inert gas is filled, such as argon. When the filling reaches 0.05MPa, the filling is stopped and heating and melting are started; after the melting is completed, it needs to be left to stand for 3 minutes before casting, and it needs to be cooled for 30 minutes after the casting is completed;
[0014] The castings obtained after cooling are crushed, pulverized and the coarse material is stirred to make the components in the coarse material evenly mixed;
[0015] Grinding the mixed coarse material and stirring the ground fine powder again;
[0016] The fine powder after grinding and stirring is pressed, and the block or sheet magnetic material obtained by pressing is sintered, and then the obtained material is tempered to eliminate the high temperature processing residual stress of the magnetic material, so as to obtain the required permanent magnetic material.
[0017] Beneficial effects:
[0018] 1. The high remanence and low coercive force permanent magnet material and the preparation method thereof drive the driven disk to rotate by rotating the rotating rod, so that under the guidance of the elliptical groove, the slider moves in the horizontal direction and pulls the pull rope, so that the wire wheel rotates and drives the gear to rotate, so that the gear ring rotates and drives the flip plate to rotate to flip the coarse material inside the device up and down, so that the flipping of the coarse material inside the device is more sufficient and uniform, so as to achieve better mixing effect, and avoid the situation that the uneven mixing of the coarse material affects the performance of the permanent magnet material in the later stage.
[0019] 2. The high remanence and low coercive force permanent magnetic material and its preparation method drive the magnetic strip to move by moving the slider, so that the magnetic strip cuts the magnetic flux lines outside the coil, thereby generating an induced current intermittently inside the coil and energizing the compression spring, so that the compression spring is intermittently compressed, thereby hitting the inner wall of the mounting rod, causing the mounting rod to vibrate and drive the coarse material near its surface to vibrate, thereby accelerating the falling speed of the coarse material, so that the stirring rod and the flip plate can fully contact the coarse material each time they rotate, thereby playing a certain auxiliary role in the stirring and mixing of the coarse material, so that the mixing effect of the coarse material is better. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 It is a schematic diagram of a partial cross-sectional structure of the present invention;
[0021] Figure 2 For the present invention Figure 1 The enlarged structural diagram at A in the middle;
[0022] Figure 3 For the present invention Figure 1 Schematic diagram of the structural connection relationship of the middle part;
[0023] Figure 4 It is a schematic diagram of the internal structure of the driven disk of the present invention.
[0024] In the figure: 1. main body; 2. rotating rod; 3. stirring rod; 4. auxiliary mechanism; 41. driven disk; 42. elliptical groove; 43. slider; 44. pull rope; 45. mounting rod; 46. reel; 47. gear; 48. gear ring; 49. flip plate; 410. torsion spring; 411. guide rod; 412. wiring groove; 5. vibration mechanism; 51. coil; 52. magnetic strip; 53. vibration spring. DETAILED DESCRIPTION
[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0026] See also Figure 1 - Figure 4 A high remanence and low coercive force permanent magnetic material preparation device comprises a body 1, a rotating rod 2 arranged inside the body 1 and a stirring rod 3 arranged on the outer surface of the rotating rod 2, an auxiliary mechanism 4 is arranged inside the body 1, and the auxiliary mechanism 4 comprises a driven disk 41, an elliptical groove 42, a slider 43, a pull rope 44, a mounting rod 45, a wire wheel 46, a gear 47, a gear ring 48, a flip plate 49, and a torsion spring 410. The driven disk 41 is fixedly connected to the outside of the rotating rod 2, the elliptical groove 42 is opened on the lower surface of the driven disk 41, the slider 43 is slidably connected to the inner side of the elliptical groove 42, and the pull rope 44 is fixedly connected to the inner side of the elliptical groove 42. Connected to the bottom of the slider 43, the mounting rod 45 is fixedly connected to the inner side of the body 1, the wire wheel 46 is rotatably connected to the inner side of the mounting rod 45, the gear 47 is rotatably connected to the inner side of the body 1, the gear ring 48 is meshed with the outer surface of the gear 47, and the flip plate 49 is fixedly connected to the outer surface of the gear ring 48. A rotating rod is provided on the inner side of the mounting rod 45, and the wire wheel 46 and the gear 47 are fixedly connected through the rotating rod, so that the rotation of the wire wheel 46 can drive the gear ring 48 to rotate synchronously. The number of the flip plates 49 is at least three, and all the flip plates 49 are distributed at equal angles on the outer surface of the gear ring 48;
[0027] The torsion spring 410 is fixedly connected to the outer surface of the line wheel 46, the pull rope 44 is wound on the outer surface of the line wheel 46, the ring gear 48 is rotatably connected to the outer surface of the mounting rod 45, and the torsion spring 410 is fixedly connected to the inner side surface of the mounting rod 45, so that the torsion spring 410 can drive the line wheel 46 to rotate in the opposite direction when the pull rope 44 no longer pulls the line wheel 46, so that the ring gear 48 can maintain a continuous rotation state to turn the coarse powder. The auxiliary mechanism 4 also includes a guide rod 411 and a wiring groove 412. The guide rod 411 is arranged on the inner side of the main body 1, and the wiring groove 412 is opened on the inner side of the mounting rod 45. There are two guide rods 411, and the two guide rods 411 are respectively arranged on the inner side surface of the main body 1 and the inner side surface of the mounting rod 45. The pull rope 44 is slidably connected to the outer surface of the guide rod 411, so that the guide rod 411 can guide the direction of the pull rope 44, thereby avoiding the collision between the existence of the pull rope 44 and the internal structure such as the stirring rod 3, which may cause the normal operation of the device to be obstructed.
[0028] A vibration mechanism 5 is arranged inside the main body 1, and the vibration mechanism 5 includes a coil 51, a magnetic strip 52, and a vibration spring 53. The coil 51 is arranged on the inner side of the driven disk 41, the magnetic strip 52 is fixedly connected to the outer surface of the slider 43, and the vibration spring 53 is arranged on the inner side of the mounting rod 45. The position and specification of the magnetic strip 52 match those of the coil 51. The coil 51 is coupled with the vibration spring 53, so that when current is intermittently generated inside the coil 51, the vibration spring 53 can be energized, so that the vibration spring 53 can be compressed, so that the vibration spring 53 can collide with the inner wall of the mounting rod 45 during the recovery process and drive it to vibrate.
[0029] A high remanence and low coercivity permanent magnetic material, the atomic composition of the material is R x Fe a Al b Cu c B d , where R is a rare earth element, Fe, Al, Cu, and B represent the chemical elements iron, aluminum, copper, and boron respectively; R is Nd, Nb, and Dy; the material composition ratio of each element is: Nd 30%, Nb 0.4%, Dy 0.8%, Fe 67.2%, Al 0.4%, Cu 0.1%, and B 1.1%.
[0030] A method for preparing a high remanence and low coercivity permanent magnetic material comprises the following steps:
[0031] S1. Weigh the various materials required according to the actual proportion of the materials required for the preparation of permanent magnet materials, and send the weighed materials into the furnace for melting and casting; during the melting process, vacuum treatment is required to reduce the internal air pressure to below 0.07MPa, and then inert gas is filled, such as argon. When the filling reaches 0.05MPa, the filling is stopped and heating and melting are started; after the melting is completed, it needs to be left to stand for 3 minutes before casting, and after the casting is completed, it needs to be cooled for 30 minutes;
[0032] S2. The casting obtained after the cooling of the melt is crushed, pulverized and the coarse material is stirred to make the components in the coarse material evenly mixed;
[0033] S3. The mixed coarse material is ground and the ground fine powder is stirred again;
[0034] S4. The fine powder after grinding and stirring is pressed, and the block or sheet magnetic material obtained by pressing is sintered, and then the obtained material is tempered to eliminate the high temperature processing residual stress of the magnetic material, so as to obtain the required permanent magnetic material.
[0035] Working principle: During the working process, the coarse powder inside the device is stirred by rotating the rotating rod 2 to drive the stirring rod 3 to rotate. During the rotation of the rotating rod 2, the driven disk 41 is driven to rotate, and the rotation of the driven disk 41 drives the elliptical groove 42 on its bottom surface to rotate. During the rotation of the elliptical groove 42, the slider 43 slides along the inner side of the elliptical groove 42, thereby pulling the pull rope 44. When the pull rope 44 is pulled, it also drives the wire wheel 46 to rotate. During the rotation of the wire wheel 46, the rotating rod is driven to rotate, and the rotation of the rotating rod drives the gear 47 to rotate. The rotation of the gear 47 drives the gear ring 48 to rotate. The rotation of the gear ring 48 drives the flip plate 49 on its outer surface to rotate, so that the stirring rod 3 stirs and mixes the materials in the horizontal direction, and the flip plate 49 flips the materials in the vertical direction. In this way, the materials inside the device are mixed evenly, avoiding the poor mixing effect of the coarse materials inside the device, which leads to the poor performance of the permanent magnetic material produced later.
[0036] When the slider 43 slides along the inner side surface of the elliptical groove 42, it will drive the magnetic strip 52 outside it to continue to move synchronously. During the movement, the magnetic strip 52 will intermittently pass through the outside of the coil 51, so as to cut the magnetic flux lines and change the magnetic flux of the coil 51. The coil 51 intermittently generates current and energizes the vibration spring 53. The vibration spring 53 will shrink when energized. When the power is cut off, the vibration spring 53 will recover under the action of the rebound force and hit the inner wall of the mounting rod 45, so that the mounting rod 45 vibrates and drives the coarse powder nearby to vibrate, thereby accelerating the falling speed of the coarse powder after flipping, so that the flip plate 49 and the stirring rod 3 can fully contact the coarse powder during each rotation, thereby playing a certain auxiliary role in the stirring and mixing of the coarse powder, making the mixing of the coarse powder more sufficient and uniform.
[0037] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A device for preparing a high remanence and low coercive force permanent magnetic material, comprising a body (1), a rotating rod (2) arranged inside the body (1), and a stirring rod (3) arranged on the outer surface of the rotating rod (2), characterized in that: An auxiliary mechanism (4) is arranged inside the body (1), and the auxiliary mechanism (4) comprises a driven disc (41), an elliptical groove (42), a slider (43), a pull rope (44), a mounting rod (45), a wire wheel (46), a gear (47), a gear ring (48), a flip plate (49), and a torsion spring (410). The driven disc (41) is fixedly connected to the outside of the rotating rod (2), the elliptical groove (42) is formed on the lower surface of the driven disc (41), and the slider (43) is slidably connected to the elliptical groove (42). ), the pull rope (44) is fixedly connected to the bottom of the slider (43), the mounting rod (45) is fixedly connected to the inner side of the body (1), the wire wheel (46) is rotatably connected to the inner side of the mounting rod (45), the gear (47) is rotatably connected to the inner side of the body (1), the gear ring (48) is meshed with the outer surface of the gear (47), the flip plate (49) is fixedly connected to the outer surface of the gear ring (48), and the torsion spring (410) is fixedly connected to the outer surface of the wire wheel (46); The auxiliary mechanism (4) further comprises a guide rod (411) and a wiring groove (412), wherein the guide rod (411) is arranged on the inner side surface of the body (1), and the wiring groove (412) is opened on the inner side of the mounting rod (45), and the number of the guide rods (411) is two, and the two guide rods (411) are arranged on the inner side surface of the body (1) and the inner side surface of the mounting rod (45), respectively, and the pull rope (44) is slidably connected to the outer surface of the guide rod (411); The pull rope (44) is wound on the outer surface of the wire wheel (46), the gear ring (48) is rotatably connected to the outer surface of the mounting rod (45), and the torsion spring (410) is fixedly connected to the inner side surface of the mounting rod (45); The inner side surface of the mounting rod (45) is provided with a rotating rod, the wire wheel (46) and the gear (47) are fixedly connected via the rotating rod, the number of the flap plates (49) is at least three, and all the flap plates (49) are distributed at equal angles on the outer surface of the gear ring (48); A vibration mechanism (5) is arranged inside the body (1), and the vibration mechanism (5) comprises a coil (51), a magnetic strip (52), and a vibration spring (53), wherein the coil (51) is arranged on the inner side surface of the driven disk (41), the magnetic strip (52) is fixedly connected to the outer surface of the slider (43), and the vibration spring (53) is arranged on the inner side surface of the mounting rod (45); The position and specifications of the magnetic strip (52) match those of the coil (51), and the coil (51) is coupled to the vibration spring (53).
2. A permanent magnetic material prepared by the high remanence and low coercivity permanent magnetic material preparation device according to claim 1, characterized in that: The atomic composition of the material is R x Fe a Al b Cu c B d , wherein R is a rare earth element, Fe, Al, Cu, and B represent the chemical elements iron, aluminum, copper, and boron respectively; the R is Nd, Nb, and Dy; the material composition ratio of each element is: Nd 30%, Nb 0.4%, Dy 0.8%, Fe 67.2%, Al 0.4%, Cu 0.1%, and B 1.1%.
3. A method for preparing the high remanence and low coercivity permanent magnetic material according to claim 2, characterized in that: The following steps are involved: S1. Weigh the various materials required according to the actual proportion of the materials required for the preparation of permanent magnet materials, and send the weighed materials into the furnace for melting and casting; during the melting process, vacuum treatment is required to reduce the internal air pressure to below 0.07MPa, and then argon gas is filled. When the filling reaches 0.05MPa, the filling is stopped and heating and melting are started; after the melting is completed, it needs to be left to stand for 3 minutes before casting, and it needs to be cooled for 30 minutes after the casting is completed; S2. The casting obtained after the cooling of the melt is crushed, pulverized and the coarse material is stirred to make the components in the coarse material evenly mixed; S3. The mixed coarse material is ground and the ground fine powder is stirred again; S4. The fine powder after grinding and stirring is pressed, and the block or sheet magnetic material obtained by pressing is sintered, and then the obtained material is tempered to eliminate the high temperature processing residual stress of the magnetic material, so as to obtain the required permanent magnetic material.