Bionic micro-texture micro-grinding head and machining process thereof
By using a bionic micro-texture micro-grinding head in bone grinding technology, and using bionic bird feathers, fish scales or phyllotaxic structures to arrange abrasive grains and grooves, the thermal-force problems caused by unreasonable abrasive grain arrangement in the grinding head are solved. Damage and abrasive particle shedding problems are eliminated, and grinding efficiency and processing quality are improved.
Patent Information
- Application Number
- CN202410819506.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-24
- Publication Date
- 2024-10-01
AI Technical Summary
In the existing bone grinding technology, the unreasonable arrangement of abrasive grains on the grinding head leads to problems such as thermal damage, low material removal rate, high surface roughness, and easy wear and fall of abrasive grains.
A bionic micro-textured micro-grinding head is used. The surface of the grinding head is arranged with abrasive grains according to a bionic bird feather, fish scale or phyllotaxic structure. Grooves are set up to reduce thermal damage and abrasive grain shedding, and improve grinding efficiency and material removal rate. .
It effectively reduces thermal-mechanical damage during bone grinding, improves grinding efficiency and abrasive particle utilization, reduces the roughness of the surface of the processed object, and enhances cooling efficiency and wear resistance of the grinding head.
Smart Images

Figure CN118717221A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of bone grinding, in particular to a bionic micro-texture micro-grinding head and a processing technology thereof. Background Art
[0002] The statements in this section merely provide background information related to the present invention and do not necessarily constitute prior art.
[0003] Bone grinding is one of the common and basic surgical operations in skull base tumor removal surgery. In clinical practice, surgeons often use high-speed micro-grinding tools such as grinding heads instead of grinding wheels to remove bone pathology. However, high-speed grinding generates a lot of heat, leading to bone necrosis and thermal damage to surrounding tissues, and also has a certain impact on the coagulation function of tissues. In clinical practice, drip cooling with saline is often used to remove part of the grinding heat by natural convection. Grinding heat damage has received clinically recognized attention because the temperature cannot be determined during the grinding process and the degree of thermal damage cannot be controlled. Researchers pointed out that under the pouring saline cooling method, the highest critical temperature of thermal damage is 43°C. When it is higher than 43°C, the optic nerve will be damaged, and in severe cases, blindness will occur. Involving bone grinding, facial paralysis and femoral head necrosis are also common problems in orthopedic surgery. Therefore, in bone grinding surgery, temperature control is directly related to the success or failure of the operation.
[0004] The inventors found that the existing grinding heads have unreasonable abrasive grain arrangement, and abrasive grains agglomerate during electroplating, which makes the grinding stress more concentrated during the grinding process, and causes greater thermal-mechanical damage during bone grinding, affecting the success of the operation; and the unreasonable arrangement of abrasive grains affects the material removal rate during grinding, which increases the surface roughness of the object being ground; in addition, the abrasive grains on the surface of the grinding head are easy to wear, and the abrasive grains are prone to micro-fracture and falling off; although the prior art uses bionic structures to improve the structure of the grinding wheel surface so that the efficiency of the grinding wheel surface participating in cooling during the grinding process is improved, there is no research in the relevant direction on what kind of bionic structure to use for the grinding head with abrasive grains, and some grinding systems also have related research. Summary of the invention
[0005] In view of the shortcomings of the prior art, the object of the present invention is to provide a bionic micro-textured micro-grinding head to improve the grinding efficiency and the processing quality of the surface of the processing object.
[0006] In order to achieve the above object, the present invention is implemented through the following technical solutions:
[0007] A bionic micro-textured micro-grinding head, comprising a micro-grinding head base, the micro-grinding head base comprising a connecting piece, the connecting piece being connected to the grinding head, a plurality of abrasive grain groups or a plurality of abrasive grains being sequentially arranged on the surface of the grinding head, the plurality of abrasive grain groups being arranged according to a bionic bird feather microstructure or a bionic fish scale structure, and the plurality of abrasive grains being arranged according to a bionic phyllotaxy microstructure;
[0008] When multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure or the bionic fish scale structure, each group of abrasive grains includes multiple abrasive grains, and when multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure or the bionic fish scale structure, a groove is provided between two adjacent groups of abrasive grains;
[0009] When the multiple abrasive grains are arranged according to the bionic phyllotaxis microstructure, the multiple abrasive grains are arranged in multiple rows and columns, and some rows where the abrasive grains are located and some columns where the abrasive grains are located are respectively inclined relative to the radial plane passing through the center of the grinding head, and the radial plane passing through the center is perpendicular to the central axis of the connecting member;
[0010] The abrasive grains are arranged to protrude from the surface of the grinding head.
[0011] As described above, the micro-grinding head has abrasive groups or abrasives arranged on the surface of the grinding head, and the abrasive groups or abrasives are arranged according to a variety of bionic structures, which changes the abrasive layout of the traditional grinding head. The abrasives are arranged in an orderly manner, which reduces the concentration of grinding force and reduces the thermal-mechanical damage during bone grinding, thereby avoiding surgical problems caused by high temperature; the improved micro-grinding head can effectively improve the grinding efficiency and abrasive utilization rate; it can also effectively avoid abrasive wear, micro-fracture, macro-fracture and shedding; the improved micro-grinding head can effectively improve the material removal rate during use, reduce the roughness of the surface of the processing object, and improve the processing quality of the surface of the processing object.
[0012] As described above, in a bionic micro-textured micro-grinding head, when multiple groups of the abrasive grain groups are arranged according to the bionic bird feather microstructure, each group of the abrasive grain groups is arranged along the circumference of the grinding head, and each of the grooves has multiple bends, so that the grooves are arranged in a wavy shape, and the directions of the bends of the grooves are perpendicular to or intersecting with the central axis of the connecting piece. The abrasive grain groups arranged according to the bionic bird feather microstructure are arranged in a set direction and have bends, extending the length of the grooves, so that the micro-grinding head has the functions of directional drainage and drag reduction, and a groove is arranged between two adjacent abrasive grain groups. The arrangement of the grooves can effectively take away the heat generated during the grinding process, which is beneficial to controlling the temperature during the bone grinding process.
[0013] In the bionic micro-textured micro-grinding head as described above, considering the rationality of the structural setting, the groove has a set width and a set depth, and the depth of the groove is less than the height of the abrasive particles in the abrasive particle group;
[0014] The abrasive grain group is located at the boss, and the width of the groove is smaller than the width of the boss where the abrasive grain group is located.
[0015] A bionic micro-textured micro-grinding head as described above, wherein the arrangement shape of each group of abrasive grains is consistent with the shape of the groove, and the bending angle of the groove at its bending point is an obtuse angle;
[0016] Each group of abrasive grains is provided with at least two rows of abrasive grains, and the distance between two adjacent rows of abrasive grains in each group of abrasive grains is smaller than the width of the groove.
[0017] As described above, in a bionic micro-textured micro-grinding head, when multiple groups of the abrasive groups are arranged according to the bionic fish scale structure, the grooves are formed between two adjacent groups of abrasive groups, each group of abrasive groups is fan-shaped, and the longer side of the abrasive group is arranged in a direction away from the connecting piece. The abrasive group is arranged with the position close to the center of the connecting piece as the focus and radiates to the surroundings. The abrasive group is arranged according to the bionic fish scale structure, and the abrasive group is arranged with the position close to the center of the connecting piece as the focus and radiates to the surroundings. The surface presents a pecten structure, and more striped grooves are formed on the surface of the micro-grinding head, which effectively reduces the friction with the coolant, enhances the hydrophobicity, and achieves the purpose of rapid heat exchange.
[0018] As described above, in a bionic micro-textured micro-grinding head, each group of the abrasive grains includes 6-10 abrasive grains, all the abrasive grains in each group of the abrasive grains are arranged in multiple rows, the abrasive grains in two adjacent rows are staggered, the distance between two adjacent abrasive grains in each column of abrasive grains in the interval row is greater than the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains, and the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains is greater than the width of the groove, which is beneficial to further ensure the rationality of the setting of the abrasive grain group.
[0019] As described above, when a plurality of abrasive grains are arranged according to the bionic phyllotaxy microstructure, it is beneficial to ensure the density of the abrasive grains and facilitate the smooth progress of the grinding process. The distance between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance between the two adjacent abrasive grains in the Y direction, and the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance between two adjacent abrasive grains in the same row in the X direction.
[0020] In a second aspect, the present invention further provides a processing technology for a bionic micro-textured micro-grinding head, comprising the following contents:
[0021] The micro-grinding head substrate is placed in a degreasing liquid for degreasing treatment;
[0022] The micro-grinding head substrate in which the abrasive particles are arranged according to the bionic bird feather microstructure is subjected to structural processing, so that grooves are prepared on the surface of the micro-grinding head substrate;
[0023] Pre-plating the micro-grinding head substrate;
[0024] Glue is dispensed on the surface of the pre-plated micro-grinding head substrate to form glue dots on the surface of the micro-grinding head substrate, and the glue dots are arranged according to a bionic bird feather microstructure, a bionic fish scale structure, or a bionic leaf sequence microstructure;
[0025] The abrasive grains are pickled and oxidized to prevent them from falling off from the micro-grinding head substrate;
[0026] The abrasive grains after oxidation treatment are sprinkled on the surface of the micro-grinding head substrate, and the abrasive grains are fixed at the glue points to form a micro-grinding head. The formed micro-grinding head is thickly plated to obtain a bionic micro-textured micro-grinding head.
[0027] In the processing technology of a bionic micro-textured micro-grinding head as described above, the degreasing liquid includes sodium hydroxide NaOH, sodium carbonate Na2CO3, sodium phosphate Na3PO4, and sodium silicate Na2SiO3. After the micro-grinding head substrate is degreased, the micro-grinding head substrate is roughened to form tiny pits on the surface of the micro-grinding head substrate to enhance the adhesion to the coating.
[0028] The processing technology of the bionic micro-textured micro-grinding head as described above, wherein the micro-grinding head substrate is pre-plated, comprises the following contents: placing the micro-grinding head substrate in an electroplating solution containing nickel sulfate NiSO4, nickel chloride NiCl2, boric acid H3BO3, and sodium dodecyl sulfate C12H25-OSO3Na.
[0029] The beneficial effects of the present invention are as follows:
[0030] 1) The micro-grinding head of the present invention is provided with abrasive groups or abrasive grains on the surface of the grinding head, and the abrasive groups or abrasive grains are arranged according to a variety of bionic structures, thereby avoiding the agglomeration of abrasive grains during electroplating, changing the abrasive grain layout of the traditional grinding head, and the abrasive grains are arranged in an orderly manner, which reduces the concentration of grinding force and reduces the thermal-mechanical damage during bone grinding, thereby avoiding surgical problems caused by high temperature; the improved micro-grinding head can effectively improve the grinding efficiency and abrasive grain utilization rate.
[0031] 2) The grinding head surface of the micro-grinding head of the present invention has a reasonable layout of abrasive groups and abrasive particles, and the abrasive groups or abrasive particles are reasonably distributed, which can effectively avoid abrasive wear, micro-fracture, macro-fracture and shedding; the improved micro-grinding head can effectively improve the material removal rate during use, reduce the roughness of the surface of the processing object, and improve the processing quality of the surface of the processing object.
[0032] 3) The abrasive grain group arranged according to the bionic bird feather microstructure in the present invention is arranged in a set direction and has a bend, which extends the length of the groove, so that the micro-grinding head has the functions of directional drainage and drag reduction, effectively allowing the coolant to break through the obstruction of the air layer and enter the grinding area. The coolant enters the grinding area for effective lubrication and cooling, and further reduces the grinding temperature; a groove is arranged between two adjacent abrasive grain groups, and the arrangement of the groove can effectively take away the heat generated during the grinding process, which is conducive to controlling the temperature during the bone grinding process;
[0033] At the same time, as the debris generated by grinding and the particles produced by the breakage of abrasive particles gather in the grooves on the surface of the grinding head, the bird-feather-shaped grooves help to guide the uniform flow and carry away the debris, reducing the blockage of the grinding head, reducing the temperature rise caused by blockage, and improving the processing quality of the processing object.
[0034] 4) In the present invention, the arrangement of the abrasive grains is in accordance with the bionic fish scale structure, with the position close to the center of the connector as the focus and radiating to the surrounding area. The surface presents a pecten structure, and a large number of striped grooves are formed on the surface of the micro-grinding head, which effectively reduces the friction with the coolant, enhances the hydrophobicity, and achieves the purpose of rapid heat exchange.
[0035] 5) In the present invention, a plurality of abrasive grains are arranged according to the bionic phyllotaxy microstructure, and the density of the abrasive grains is effectively guaranteed by limiting the distance between two adjacent abrasive grains in the X direction and the Y direction.
[0036] 6) The processing technology proposed in the present invention is to first process the micro-grinding head substrate, process the grooves after the processing is completed, and pre-plate it. The pre-plating treatment can enhance the stability of the subsequent abrasive particles. The abrasive particles are then processed and finally fixed to the micro-grinding head substrate to form a bionic micro-textured micro-grinding head. The overall process is reasonably set up, and the abrasive particles are pickled and oxidized, which can effectively prevent the abrasive particles from falling off the micro-grinding head substrate, thereby ensuring the service life of the micro-grinding head as a whole. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] The accompanying drawings in the specification, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.
[0038] Figure 1 This is a front view of a bionic micro-texture micro-grinding head in Example 1 of the present invention.
[0039] Figure 2 yes Figure 1 Enlarged view of point A in the middle.
[0040] Figure 3 yes Figure 1 Enlarged view of point B in the middle.
[0041] Figure 4This is a front view of a bionic micro-texture micro-grinding head in the second embodiment of the present invention.
[0042] Figure 5 yes Figure 4 Enlarged view of the middle part.
[0043] Figure 6 This is a front view of a bionic micro-texture micro-grinding head in embodiment 3 of the present invention.
[0044] Figure 7 yes Figure 6 Enlarged view of point C in the middle.
[0045] Figure 8 It is a flow chart of a processing technology of a bionic micro-texture micro-grinding head in the fourth embodiment of the present invention.
[0046] In the figure: the distances or sizes between parts are exaggerated to show the positions of various parts, and the schematic diagram is for reference only.
[0047] Among them: 1. Connecting piece, 2. Abrasive grains, 3. Grooves, 4. Bosses, 5. Grinding heads, 6. Abrasive grain groups. DETAILED DESCRIPTION
[0048] It should be noted that the following detailed descriptions are illustrative and intended to provide further explanation of the present invention. Unless otherwise specified, all technical and scientific terms used in the present invention have the same meanings as those commonly understood by those skilled in the art to which the present invention belongs.
[0049] It should be noted that the terms used herein are only for describing specific embodiments and are not intended to limit the exemplary embodiments according to the present invention. As used herein, unless otherwise explicitly stated in the present invention, the singular form is also intended to include the plural form. In addition, it should be understood that when the terms "include" and / or "include" are used in this specification, it indicates the presence of features, steps, operations, devices, components and / or combinations thereof;
[0050] As introduced in the background art, the bone grinding process in the prior art is prone to thermal damage. In order to solve the above technical problem, the present invention proposes a bionic micro-textured micro-grinding head.
[0051] Embodiment 1
[0052] In a typical embodiment of the present invention, reference is made to Figure 1 As shown, a bionic micro-textured micro-grinding head comprises a micro-grinding head base, the micro-grinding head base comprises a connecting member 1, the connecting member 1 is connected to a grinding head 5, the connecting member 1 is specifically a connecting rod, the grinding head 5 is specifically spherical, a notch is arranged on one side of the grinding head to connect with one end of the connecting member, a plurality of abrasive grain groups are sequentially arranged on the surface of the grinding head 5, and the plurality of abrasive grain groups are arranged according to the bionic bird feather microstructure;
[0053] When the multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure, each group of abrasive grains includes multiple abrasive grains, and when the multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure, a groove is provided between two adjacent groups of abrasive grains;
[0054] When multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure, each group of abrasive grains is arranged along the circumference of the grinding head, each groove has multiple bends, and the directions of adjacent bends are opposite so that the grooves are arranged in a wave shape, and the directions of the bends of the grooves are perpendicular to or intersecting with the central axis of the connecting member, and the grooves extend from one side close to the connecting member to the other end of the grinding head. The abrasive grains arranged according to the bionic bird feather microstructure are arranged in a set direction and have bends;
[0055] Considering the rationality of the structural setting, the groove 3 has a set width and a set depth. In this embodiment, the depth h (10-50 μm) of the groove 3 is less than the height of the abrasive grain 2 in the abrasive grain group; the abrasive grain group is located at the boss, referring to Figure 2 As shown, the width m of the groove (20-100 μm) is smaller than the width n (50-300 μm) of the boss 4 where the abrasive grain group is located.
[0056] The arrangement shape of each group of abrasive grains is consistent with the shape of the groove, and the bending angle of the groove at the bend is an obtuse angle; each group of abrasive grains is provided with at least two rows of abrasive grains, Figure 3 As shown, the angle α (30-75°) between the row where the abrasive grains are located and the horizontal line on one side is an acute angle. In this embodiment, two rows of abrasive grains are arranged, and the abrasive grains in two adjacent rows of abrasive grains are staggered. The distance d (20-50 μm) between two adjacent rows of abrasive grains in each group of abrasive grains is smaller than the width m (20-100 μm) of the groove.
[0057] It is understandable that when a micro-grinding head is used for bone grinding, due to the high-speed rotation of the micro-grinding head, an air layer will be formed on the surface of the grinding head, which will hinder the coolant from entering the grinding area. In addition, due to the close contact between the grinding head and the workpiece during grinding, the coolant cannot effectively remove the heat from the grinding area. At the same time, the debris generated by grinding is difficult to discharge from the grinding area, and gradually accumulates in the gaps between the abrasive particles, causing the grinding head to be blocked, affecting the processing quality, and causing the heat dissipation performance of the grinding head to decrease, causing thermal damage to the bone tissue and reducing the processing efficiency. In this embodiment, multiple groups of abrasive particles are arranged according to the bionic bird feather microstructure, and the flow-guiding and drag-reducing effect of the bird feather-like structure can effectively allow the coolant to break through the obstruction of the air layer and enter the grinding area. The coolant enters the grinding area for effective lubrication and cooling, further reducing the grinding temperature; at the same time, the debris generated by grinding and the particles generated by the breakage of the abrasive particles gather in the grooves on the surface of the grinding head. The bird-feather-shaped grooves help to guide the uniform flow and carry away the debris, reducing the blockage of the micro-grinding head, reducing the temperature rise caused by blockage, and improving the processing quality of the workpiece.
[0058] Embodiment 2
[0059] The difference between this embodiment and the first embodiment is that:
[0060] Multiple groups of abrasive grains are arranged according to the bionic fish scale structure and set according to the required mesh size (100#~1200#); Figure 4 As shown, when multiple groups of abrasive grain groups are arranged according to the bionic fish scale structure, grooves 3 are formed between two adjacent groups of abrasive grain groups 6, each group of abrasive grain groups is fan-shaped, the surrounding sides of the abrasive grain groups are grooves, and each side of the abrasive grain group is arc-shaped, so that the surface of the grinding head is covered with fish scales composed of the abrasive grain groups, the thickness of all abrasive grain groups remains the same or similar, the longer side of the abrasive grain group is set in the direction away from the connecting member, the abrasive grain groups are arranged according to the bionic fish scale structure, and the arrangement of the abrasive grain groups radiates to the surroundings with the position close to the center of the connecting member as the focus, and the surface presents a pecten structure. The center lines of some abrasive grain groups (along the center point of the fan-shaped abrasive grain group) are located in the same straight line, and the straight line is parallel to or intersecting with the central axis of the connecting member. When intersecting, the angle between the straight line and the central axis of the connecting member is 0-10°, and more stripe grooves are formed on the surface of the micro-grinding head, which effectively reduces the friction with the coolant, enhances the hydrophobicity, and achieves the purpose of rapid heat exchange.
[0061] Each abrasive grain group includes 6-10 abrasive grains, specifically 7 abrasive grains. All abrasive grains in each abrasive grain group are arranged in multiple rows. Two abrasive grains are arranged in a row close to the connecting piece, three abrasive grains are arranged in the middle, and two abrasive grains are arranged in a row away from the connecting piece. The abrasive grains in two adjacent rows are staggered. Figure 5As shown, the distance d4 (100-150 μm) between two adjacent abrasive grains in each row in the horizontal direction is greater than the distance d6 (90-120 μm) between two adjacent abrasive grains in each column of abrasive grains in the interval row, the distance d6 (90-120 μm) between two adjacent abrasive grains in each column of abrasive grains in the interval row is greater than the distance d5 (60-100 μm) between two adjacent rows of abrasive grains, and the distance d5 (60-100 μm) between two adjacent rows of abrasive grains is greater than the width w (20-100 μm) of the groove, which is conducive to further ensuring the rationality of the setting of the abrasive group.
[0062] It should be noted that, since the spacing between two adjacent groups of abrasive grains in this embodiment is relatively small, smaller parameters are used when using a laser beam to perform structured processing on the surface of the micro-grinding head substrate. For example, in this embodiment, the parameters of current intensity 20A, pulse interval 20ns, laser frequency 20kHz, and marking speed 20mm / s can be used for processing to ensure the size and accuracy of the grooves.
[0063] For the micro-grinding head in Example 1 or Example 2, when the micro-grinding head grinds bone tissue, the wear of the abrasive particles is inevitable. How to ensure the wear resistance of the micro-grinding head by changing the abrasive particle structure is an important indicator for evaluating the performance of the micro-grinding head. The wear resistance of the micro-grinding head is usually judged by the grinding ratio G, which represents the ratio of the amount of material removed from the processing object and the amount of wear of the micro-grinding head per unit time. A higher grinding ratio means better wear resistance and longer service life. The calculation formula is as follows:
[0064]
[0065] Where V t is the wear amount of the micro-grinding head, V m To remove the volume of the object being machined, for surface grinding, the calculation formula is as follows:
[0066]
[0067] Where l is the length of the workpiece, B is the grinding width, r is the radius of the grinding head, W is the abrasive width, d is the grinding depth, and Δr is the wear amount of the grinding head radius per unit time. The grinding ratio G can be changed by adjusting the above parameters.
[0068] It should be noted that the presence of the rough surface makes the actual solid-liquid contact area larger than the apparent geometric contact area, geometrically enhancing the hydrophilicity (or hydrophobicity). Assuming that the coolant droplets always fill the grooves on the grinding head surface, the apparent contact angle β of the rough surface is * With β e Relationship:
[0069] cosβ*=r(γSG -γ SL ) / γ LG = r cos β e
[0070] Where: γ SG , γ SL , γ LG are the surface tensions between solid-gas, solid-liquid, and liquid-gas contacts, respectively; r is the material surface roughness factor, which is the ratio of the actual contact area to the apparent contact area, r≥1. Therefore, by changing the surface roughness of the grinding head, the apparent contact angle can be adjusted, thereby changing the wetting properties of its surface.
[0071] In addition, the contact of coolant droplets on the rough surface is a composite contact. The droplets cannot fill the grooves on the rough surface of the grinding head. There is trapped air under the droplets in the grooves. Therefore, the apparent liquid-solid contact is actually composed of liquid-solid and gas-solid contact. From the perspective of thermodynamics:
[0072] dG=f s (γ SL -γ SG )dx+(1-f s )γ LG dx+γ LG dxcosβ*
[0073] When the droplet is in equilibrium, the apparent contact angle β on the rough surface is * is the intrinsic contact angle of a smooth flat surface β e and the average of 180°:
[0074] cosβ*=f s (1+cosβ e )-1
[0075] Where: f s is the area fraction of the protruding solid in the composite contact surface (f s <1).
[0076] The most important factor affecting the dynamic behavior of surface droplets is the three-phase contact boundary. Figure 5 As shown, when the droplet is in equilibrium, the contact angle is β (state d); if a small amount of liquid is added and the solid-liquid-gas three-phase contact boundary remains stationary, the contact angle will inevitably increase to β2 (state e); conversely, if a small amount of liquid is extracted while keeping the solid-liquid-gas three-phase contact boundary stationary, the contact angle will inevitably decrease to β1 (state c). Assuming that there are only three interfacial tensions at the solid-liquid-gas three-phase contact boundary, when in equilibrium, states d, e, and c are:
[0077]
[0078] The above shows that if the droplets in the equilibrium spreading position want to continue to spread along the solid wall, they need to overcome the pinning effect of the solid on the contact boundary. During the cooling process of skull grinding in neurosurgery, coolant continuously enters the grinding area. The previous drop of coolant hits the bone surface at a set speed and angle and spreads into a liquid film. The most favorable state for cooling and lubricity is that the subsequent drop continues to spread when it hits the position of the previous drop, that is, the coolant drop can overcome the pinning effect of the rough bone surface on its contact boundary.
[0079] Embodiment 3
[0080] The difference between this embodiment and the first embodiment is that:
[0081] refer to Figure 6 As shown, multiple abrasive grains are arranged according to the bionic phyllotaxy microstructure. When the multiple abrasive grains are arranged according to the bionic phyllotaxy microstructure, the multiple abrasive grains are arranged in multiple rows and columns, and the rows where some abrasive grains are located and the columns where some abrasive grains are located are respectively inclined relative to the radial plane passing through the center of the grinding head, and the angle between each row of abrasive grains and the horizontal line is γ, and γ is less than 45°. Here, the radial plane passing through the center is perpendicular to the central axis of the connecting part.
[0082] When multiple abrasive grains are arranged according to the bionic phyllotaxy microstructure, it is beneficial to ensure the density of the abrasive grains in the grinding head and facilitate the smooth progress of the grinding process. The distance between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance between the two adjacent abrasive grains in the Y direction. Figure 7 As shown, the distance d3 between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance d2 between two adjacent abrasive grains in the same row in the X direction, and the distance d3 between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance d1 between two adjacent abrasive grains in two adjacent rows of abrasive grains in the Y direction.
[0083] Embodiment 4
[0084] This embodiment discloses a processing technology of a bionic micro-textured micro-grinding head in the first embodiment, the second embodiment, or the third embodiment, referring to Figure 8 As shown, including the following:
[0085] Step 1: Place the micro-grinding head substrate in an electrolyte containing 30g / L sodium hydroxide NaOH, 30g / L sodium carbonate Na2CO3, 40g / L sodium phosphate Na3PO4, and 20g / L sodium silicate Na2SiO3, treat it at 50°C and 4ASD (amperes / square decimeter) for 2 minutes, and then dry it to remove impurities such as oil and solid particles on the surface of the micro-grinding head substrate; then put it into 150mL / L hydrogen chloride HCl solution for roughening treatment, pickle it at 40°C and 9ASD for 2 minutes, and then dry it to form tiny pits on the surface of the micro-grinding head substrate to enhance the adhesion to the coating.
[0086] Since there is an oxide layer on the surface of the micro-grinding head substrate that has not been cared for, if electroplating is performed directly, the bonding force between the plating layer and the surface of the micro-grinding head substrate will be too low, causing the plating layer to fall off the surface of the micro-grinding head substrate, affecting the processing quality and reducing the service life of the micro-grinding head.
[0087] Step 2: Use a laser beam to cut the surface of the micro-grinding head substrate according to a set pattern, and prepare a bionic pattern groove with a set depth on its surface through processes such as gasification and melting.
[0088] The specific parameter range is current intensity 25A, pulse interval 20ns, laser frequency 30kHz, and marking speed 8mm / s.
[0089] Step 3: Pre-plating the micro-grinding head substrate. Before fixing the abrasive grains on the surface of the micro-grinding head substrate, the micro-grinding head substrate needs to be pre-plated to enhance the stability of the abrasive grains. The micro-grinding head substrate is placed in an electroplating solution containing 250 g / L nickel sulfate NiSO4, 50 g / L nickel chloride NiCl2, 40 g / L boric acid H3BO3, and 0.05 g / L sodium dodecyl sulfate C12H25-OSO3Na, and electroplated at 40°C and 2ASD for 30 minutes. No drying is performed after completion.
[0090] Step 4: Glue is dispensed on the surface of the pre-plated micro-grinding head substrate to form glue dots on the surface of the micro-grinding head substrate, and the glue dots are arranged according to a bionic bird feather microstructure, a bionic fish scale structure, or a bionic leaf sequence microstructure;
[0091] Step 5: Perform hydrophilic treatment on the diamond abrasive grains. In order to remove oil stains and solid particle impurities on the surface of the diamond abrasive grains, the abrasive grains are placed in a mixed solution of 1wt% polyacrylamide and 98wt% fuming nitric acid in a volume ratio of 3:1, and pickled at room temperature. After completion, they are rinsed with deionized water for 3 times; the diamond abrasive grains are oxidized at room temperature with a mixed solution of 30wt% sodium dodecylbenzene sulfonate and 96wt% concentrated nitric acid in a volume ratio of 3:1. After completion, they are rinsed with deionized water until the pH value remains within the range of 6.5 to 7.0.
[0092] Step 6: Thick plating of the micro-grinding head. The hydrophilized diamond abrasives are evenly sprinkled on the surface of the substrate, and the abrasives are fixed at the glue point. Since the substrate is not dried after pre-plating, there is residual plating liquid on the surface of the micro-grinding head substrate to adhere to the diamond abrasives, so there is no need to fix the abrasives. Keep the composition of the plating liquid unchanged, electroplate for 1.5 minutes at 1ASD and 40℃, and repeat the operation 8 times; after completion, keep other conditions unchanged, electroplate for 40 minutes, and perform thick plating.
[0093] It needs to be explained that the coating may have an uneven surface during the electroplating process. There are two main reasons: one is the presence of oil stains and solid particle impurities on the surface of the micro-grinding head substrate and abrasive particles that have not been degreased; the other is the hydrogen evolution reaction during the electroplating process.
[0094] When the micro-grinding head base and abrasive grains are not degreased, the impurities attached to their surfaces will contaminate the plating solution during electroplating, resulting in low purity of the coating and pits on the surface of the coating. There are two main reasons for the pits: one is that there are various insoluble or undissolved solid particles called mechanical impurities in the plating solution or on the surface of untreated diamond abrasive grains. When they settle on the surface of the micro-grinding head base and are coated in the coating, the coating is obviously rough because it is larger than the suspended solid particles. Therefore, degreasing the micro-grinding head base and hydrophilizing the abrasive grains can effectively remove oil and impurities and make the coating surface smooth.
[0095] In addition, the hydrogen evolution reaction in the electroplating process is mainly due to the decomposition of water in the electrolyte and the reduction of anions in the electrolyte. In the electrolytic cell, the electrode transfers the current to the substrate, and the water molecules in the electrolyte decompose into hydrogen and oxygen. This water decomposition reaction and the fact that some anions are reducing, that is, they can release hydrogen under the action of current, are inevitable in the electroplating process, especially in DC electroplating. The hydrogen evolution phenomenon in electroplating is mainly due to the hydrogen produced in the water decomposition reaction generating bubbles on the metal surface.
[0096] The electroplating process of the micro-grinding head substrate can be divided into two parts: First, as the cathode polarization current density increases rapidly, the Ni + After obtaining electrons, it is reduced to nickel and deposited on the substrate surface; second, when polarization continues, the H + The redox potential of the micro-grinding head is high, and a large amount of hydrogen H2 is released, that is, a hydrogen evolution reaction occurs. In addition, the surface of the micro-grinding head substrate before and after electroplating was observed to show that the coating thickness was uneven. Analysis showed that the micro-grinding head substrate was acid-etched and roughened before electroplating, which formed pits of different sizes on the surface of the grinding head. The convex points represent higher skewness and peaks, which can promote the nucleation and growth of the coating, as well as the height difference between the convex points and the concave points, resulting in a higher surface roughness. On the other hand, due to the leveling effect, the change in coating thickness first fills the pits to maintain the final uniformity and surface roughness.
[0097] In the processing technology proposed in this embodiment, the micro-grinding head substrate is first processed, the grooves are processed after the processing is completed, and pre-plating is performed. The pre-plating treatment can enhance the stability of the subsequent abrasive particles. The abrasive particles are then processed, and finally the abrasive particles are fixed to the micro-grinding head substrate to form a bionic micro-textured micro-grinding head. The overall process is reasonably set up, and the abrasive particles are pickled and oxidized to effectively prevent the abrasive particles from falling off the micro-grinding head substrate. The electroplating process can effectively fill the pits on the surface of the object, which is beneficial to the uniformity of the surface of the finally formed micro-grinding head, and the overall service life of the micro-grinding head is guaranteed.
[0098] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. A bionic micro-textured micro-grinding head, characterized in that: The micro-grinding head substrate includes a connecting piece, which is connected to the grinding head. A plurality of abrasive grain groups or a plurality of abrasive grains are sequentially arranged on the surface of the grinding head. The plurality of abrasive grain groups are arranged according to a bionic bird feather microstructure or a bionic fish scale structure, and the plurality of abrasive grains are arranged according to a bionic phyllotaxy microstructure. When multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure or the bionic fish scale structure, each group of abrasive grains includes multiple abrasive grains, and when multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure or the bionic fish scale structure, a groove is provided between two adjacent groups of abrasive grains; When the multiple abrasive grains are arranged according to the bionic phyllotaxis microstructure, the multiple abrasive grains are arranged in multiple rows and columns, and some rows where the abrasive grains are located and some columns where the abrasive grains are located are respectively inclined relative to the radial plane passing through the center of the grinding head, and the radial plane passing through the center is perpendicular to the central axis of the connecting member; The abrasive grains are arranged to protrude from the surface of the grinding head.
2. The bionic micro-texture micro-grinding head according to claim 1, characterized in that: When multiple groups of abrasive grains are arranged according to the bionic bird feather microstructure, each group of abrasive grains is arranged along the circumference of the grinding head, and each groove has multiple bends, so that the groove is arranged in a wavy shape, and the direction of the groove bend is perpendicular to or intersecting the central axis of the connecting part.
3. The bionic micro-texture micro-grinding head according to claim 2, characterized in that: The groove has a set width and a set depth, and the depth of the groove is less than the height of the abrasive particles in the abrasive particle group; The abrasive grain group is located at the boss, and the width of the groove is smaller than the width of the boss where the abrasive grain group is located.
4. The bionic micro-texture micro-grinding head according to claim 3, characterized in that: The arrangement shape of each group of abrasive particles is consistent with the shape of the groove, and the bending angle of the groove at its bending point is an obtuse angle; Each abrasive grain group is provided with at least two rows of abrasive grains, and the distance between two adjacent rows of abrasive grains in each abrasive grain group is smaller than the width of the groove.
5. The bionic micro-texture micro-grinding head according to claim 1, characterized in that: When multiple groups of the abrasive grain groups are arranged according to the bionic fish scale structure, the grooves are formed between two adjacent groups of abrasive grain groups. Each group of abrasive grain groups is fan-shaped. The arrangement of the abrasive grain groups radiates to the surrounding areas with the position close to the center of the connecting member as the focus, and the longer side of the abrasive grain group is arranged in a direction away from the connecting member.
6. The bionic micro-texture micro-grinding head according to claim 5, characterized in that: Each group of abrasive grains includes 6-10 abrasive grains, all the abrasive grains in each group of abrasive grains are arranged in multiple rows, the abrasive grains in two adjacent rows are staggered, the distance between two adjacent abrasive grains in each column of abrasive grains in the interval row is greater than the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains, and the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains is greater than the width of the groove.
7. The bionic micro-texture micro-grinding head according to claim 1, characterized in that: When a plurality of abrasive grains are arranged according to the bionic phyllotaxy microstructure, the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance between the two adjacent abrasive grains in the Y direction, and the distance between two adjacent abrasive grains in two adjacent rows of abrasive grains in the X direction is greater than the distance between two adjacent abrasive grains in the same row in the X direction.
8. A processing technology for a bionic micro-textured micro-grinding head according to any one of claims 1 to 7, characterized in that: It includes the following: The micro-grinding head substrate is placed in a degreasing liquid for degreasing treatment; The micro-grinding head substrate in which the abrasive particles are arranged according to the bionic bird feather microstructure is subjected to structural processing, so that grooves are prepared on the surface of the micro-grinding head substrate; Pre-plating the micro-grinding head substrate; Glue is dispensed on the surface of the pre-plated micro-grinding head substrate to form glue dots on the surface of the micro-grinding head substrate, and the glue dots are arranged according to a bionic bird feather microstructure, a bionic fish scale structure, or a bionic leaf sequence microstructure; The abrasive grains are pickled and oxidized to prevent them from falling off from the micro-grinding head substrate; The abrasive grains after oxidation treatment are sprinkled on the surface of the micro-grinding head substrate, and the abrasive grains are fixed at the glue points to form a micro-grinding head. The formed micro-grinding head is thickly plated to obtain a bionic micro-textured micro-grinding head.
9. The processing technology of the bionic micro-texture micro-grinding head according to claim 8, characterized in that: The degreasing liquid includes sodium hydroxide, sodium carbonate, sodium phosphate and sodium silicate. After the micro-grinding head substrate is degreasingly treated, the micro-grinding head substrate is roughened.
10. The processing technology of the bionic micro-texture micro-grinding head according to claim 8, characterized in that: The pre-plating of the micro-grinding head substrate comprises the following steps: placing the micro-grinding head substrate in an electroplating solution containing nickel sulfate, nickel chloride, boric acid and sodium dodecyl sulfate.