Reaction device and method for producing tetramethoxysilane
Through the series connection process of two-stage reactors and turning on the turbine agitator, combined with the filter centrifuge, the problems of high raw material toxicity, high reaction risk and low production efficiency in the production of tetramethoxysilane are solved, and an efficient and safe continuous process is achieved. Chemical production to achieve high purity and high yield.
Patent Information
- Application Number
- CN202410775838.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-17
- Publication Date
- 2024-10-01
AI Technical Summary
The existing tetramethoxysilane production technology has problems such as high raw material toxicity, high reaction risk, high equipment requirements, difficult purification and low production efficiency, and cannot meet the needs of industrial production.
The two-stage reactor cascade process is adopted and the turbine agitator is turned on. The space and time interval are rationally utilized through the cascade process of the first reactor and the second reactor, combined with the filter centrifuge for continuous production, and the use of nano-copper powder and other catalysts and High-temperature organic solvents control reaction temperature and material replenishment to achieve continuous production.
It improves the production efficiency and product yield of tetramethoxysilane, achieves high purity (greater than 99.9%) and high product yield (95%), avoids the generation of by-products, and enhances reaction safety and equipment safety. service life.
Smart Images

Figure CN118718894A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of chemical production, and in particular to a reaction device and a method for producing tetramethoxysilane. Background Art
[0002] Tetramethoxysilane is a high-quality organic silicon source. Compared with inorganic silicon sources, it has the advantages of good process adaptability and high purity. It has broad application prospects in the fields of optical glass, electronics and electrical, construction, organic silicon synthesis, precision casting, etc. ① In the field of optical glass, tetramethoxysilane can be used to produce coagulants and treatment agents to improve the transparency, wear resistance and high temperature resistance of optical glass; ② In the electronics industry, tetramethoxysilane can be used as a low dielectric constant material to prepare microelectronic devices and integrated circuits. It forms a uniform film on the substrate, with excellent insulation properties, high temperature stability and low dielectric loss. The film also has good compatibility and processability, and can be compounded or etched with other materials. ③ In the field of construction, tetramethyl silicate can be used to produce organic silicon aerogels, and insulation boards, insulating pipes, etc. are its end products; tetramethoxysilane is used as an adhesive in precision casting to improve the accuracy and surface quality of models and castings; tetramethoxysilane is used for filler modification to improve the mechanical properties, water resistance, flame retardancy, etc. of organic silicone resins.
[0003] The main preparation methods of tetramethoxysilane include silicon powder direct method, silicon tetrachloride method, alkoxysilane esterification method and sodium fluorosilicate method. 1) The more traditional method is the silicon tetrachloride method, which uses silicon tetrachloride produced as a byproduct of polysilicon as a raw material and undergoes an esterification reaction with methanol. The raw material SiCl4 is highly toxic and corrosive. During the reaction, it will also generate highly corrosive gas HCl, which is highly corrosive to equipment and pipelines. At the same time, it is easy to leak and cause environmental pollution or personal injury. 2) By using sodium fluorosilicate produced as a byproduct of the phosphate fertilizer industry as a raw material, reacting with concentrated sulfuric acid to generate silicon fluoride, and reacting with methanol, the sodium fluorosilicate method will produce byproducts of hydrofluoric acid and sodium sulfate in the reaction. It also has high requirements for equipment and pipelines, and the purification is also difficult. 3) Using trimethoxysilane as a raw material, the alkoxysilane esterification method for disproportionation reaction, in this production method, monosilane is very easy to burn, and the reaction is highly dangerous. 4) The direct method uses silicon powder and methanol as raw materials to directly react. This method does not introduce chlorine-containing compounds and has become a hot research topic in recent years. However, this technology is currently mainly in the hands of overseas companies such as Dow Corning in the United States, Evonik in Germany, and Fuso Chemical in Japan, which have implemented a technical monopoly on the silicon powder direct method.
[0004] In recent years, domestic scholars have made some initial breakthroughs in the direct method. For example, in CN101041668A, sodium methoxide, sodium ethoxide or sodium salt of diethylene glycol monobutyl ether is used as a catalyst, and alcohol and silicon powder are used to synthesize tetraalkoxysilane, and tetramethoxysilane has high selectivity; patent CN107216348A introduces a method for preparing tetramethoxysilane by direct method; patent CN115672363 A introduces a catalyst for synthesizing tetramethoxysilane and its preparation method and application. The above research is still in the laboratory research stage, and there is still room for optimization in the current industrial scale-up stage. Summary of the invention
[0005] The main purpose of the present invention is to propose a reaction device and method for the production of tetramethoxysilane, aiming to provide a device and method for the direct continuous production of methyl orthosilicate, improve the reaction efficiency and product yield, and meet the needs of industrial production.
[0006] To achieve the above object, the present invention provides a reaction device for producing tetramethoxysilane, the reaction device comprising:
[0007] A first reactor, wherein the top of the first reactor is provided with solid and liquid feed ports and a gas phase discharge port, the lower part of the outer wall of the first reactor is provided with a first slurry feed port and a methanol feed port, and the upper middle part of the outer wall of the first reactor is provided with a first overflow port;
[0008] A second reactor, wherein a gas phase discharge port is provided at the top of the second reactor, a second slurry feed port and a methanol feed port are provided at the lower part of the outer wall of the second reactor, the second slurry feed port is connected to the first overflow port through a pipeline, and a second overflow port is provided at the middle and upper part of the outer wall of the second reactor; and
[0009] A filtering centrifuge, wherein the inlet of the filtering centrifuge is connected to the second overflow port through a pipeline.
[0010] Optionally, a stirrer is provided on the top of the first reactor and the second reactor.
[0011] Optionally, the agitator is an open turbine agitator.
[0012] Optionally, the first reactor and the second reactor are both provided with slag discharge ports at the bottom.
[0013] Optionally, inner walls of the first reactor and the second reactor are both provided with remote liquid level gauges.
[0014] Optionally, inner walls of the first reactor and the second reactor are both provided with remote pressure gauges.
[0015] The present invention also provides a method for producing tetramethoxysilane, using the reaction device as described above, the method comprising the following steps:
[0016] S1. Mixing silicon powder and catalyst in a certain proportion in a batching tank to obtain a mixed material;
[0017] S2, feeding the mixed material through the solid and liquid phase feed ports at the top of the first reactor, and starting stirring;
[0018] S3, adding a certain proportion of solvent through the solid and liquid phase feed ports at the top of the first reactor;
[0019] S4, start heating, raise the temperature to 150-200°C for activation for 1.5-2.5 hours, and then raise the temperature to 230-245°C;
[0020] S5, open the methanol feed port and introduce methanol;
[0021] S6. After reacting for 22-26 hours, add a slurry prepared by silicon powder, catalyst and solvent in a certain ratio through the first slurry feed port;
[0022] S7, the slurry in the first reactor enters the second reactor from the first overflow port through the pipeline. When the liquid level of the second reactor reaches 20%-30%, stirring and heating are started to the temperature of 230-245°C;
[0023] S8. As the reaction continues, the liquid level of the second reactor continues to rise, and the slurry in the second reactor enters the filtering centrifuge from the second overflow port in the upper middle portion through a pipeline;
[0024] S9, After the slurry of the filtering centrifuge enters the filter through the inlet, the liquid phase is discharged from the drum through the filter medium and the perforated drum wall under the action of centrifugal force and enters the solvent recovery tank. The solid phase particles are trapped on the filter medium to form a filter cake layer, which is discharged from the drum under the push of the spiral;
[0025] S10. During the reaction, the products are collected through the top gas phase outlets of the first reactor and the second reactor, respectively, and are cooled before proceeding to the next step.
[0026] Optionally, in step S1, the catalyst is at least two of nano copper powder, copper oxide, copper hydroxide, cuprous oxide, copper acetate, and bis(diethyl)copper phosphate.
[0027] Optionally, in step S3, the solvent is an organic solvent having a boiling point of not less than 230°C.
[0028] Optionally, the solvent is any one of hexamethylphosphinate triamide, hexamethylphosphoric acid triamide, quinoline, ethylene glycol carbonate, diethylene glycol, succinonitrile, and cyclopentane sulfone.
[0029] Compared with the prior art, the beneficial effects of the present invention are:
[0030] (1) In the technical solution provided by the present invention, a two-stage reactor series process is adopted to rationally utilize space and time intervals to improve production efficiency.
[0031] (2) The open turbine agitator used in the present invention is a mixed flow agitator, which can generate a strong radial flow during stirring, and the material is tumbled up and down, which will not cause the material to gather at the bottom. At the same time, it can also generate a certain axial flow.
[0032] (3) Methanol is fed from the bottom of the reactor parallel to the top of the agitator. The high-speed flow rate causes the bottom material to tumble, which is beneficial to the exchange of upper and lower materials. In addition, since the agitator will generate a certain axial flow when stirring, it is beneficial to mix the materials, increase the retention time of methanol, and help improve the surface contact between methanol and silicon powder, thereby improving the reaction efficiency.
[0033] (4) A slurry feed port is provided at the bottom of the reactor, which allows material to be replenished at the bottom of the reactor, facilitating the separation of the bottom material.
[0034] (5) During the reaction process, silicon powder, catalyst and other raw materials can be intermittently added to the reactor according to the reaction situation. While adding materials, waste materials from the reactor are also intermittently discharged to maintain the active state of the reaction system, thereby extending the cycle of continuous production. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without paying creative work.
[0036] Figure 1 This is a diagram of a reaction device for producing tetramethoxysilane provided by the present invention.
[0037] Description of the accompanying drawings of the embodiments provided by the present invention:
[0038] Label name Label name 1 First reactor 17 Slag outlet 11 Solid and liquid feed ports 2 Second reactor 12 Gas phase outlet 21 Second slurry feed port 13 First slurry feed port 22 Second overflow port 14 Methanol feed port 3 Filter centrifuge 15 First overflow port 31 import 16 Agitator
[0039] The realization of the purpose, functional features and advantages of the present invention will be further explained in conjunction with embodiments and with reference to the accompanying drawings. DETAILED DESCRIPTION
[0040] To make the purpose, technical scheme and advantages of the embodiment of the present invention clearer, the technical scheme in the embodiment of the present invention will be clearly and completely described below. If the specific conditions are not specified in the embodiment, it is carried out according to the normal conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified in the reagents or instruments used, they are all conventional products that can be purchased commercially. In addition, the technical schemes between the various embodiments can be combined with each other, but must be based on the ability of ordinary technicians in the field to achieve. When the combination of technical solutions is contradictory or cannot be achieved, it should be considered that the combination of such technical solutions does not exist, and is not within the scope of protection required by the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in the field without making creative work belong to the scope of protection of the present invention.
[0041] In view of the fact that the existing direct method for producing tetramethoxysilane is not mature enough, the production efficiency is low, and it cannot meet the needs of industrial production, the present invention proposes a reaction device for producing tetramethoxysilane. Figure 1 The following is a diagram of a reaction device for producing tetramethoxysilane provided by the present invention. The reaction device for producing tetramethoxysilane of the present invention is described in detail in conjunction with the accompanying drawings.
[0042] Please refer to Figure 1 The reaction device for producing tetramethoxysilane provided by the present invention comprises a first reactor 1, a second reactor 2 and a filtering centrifuge 3, wherein the top of the first reactor 1 is provided with a solid and liquid phase feed port 11 and a gas phase discharge port 12, the lower part of the outer wall of the first reactor 1 is provided with a first slurry feed port 13 and a methanol feed port 14, and the middle and upper part of the outer wall of the first reactor 1 is provided with a first overflow port 15; the top of the second reactor 2 is provided with a gas phase discharge port 12, the lower part of the outer wall of the second reactor 2 is provided with a second slurry feed port 21 and a methanol feed port 14, the second slurry feed port 21 is connected with the first overflow port 15 through a pipeline, and the middle and upper part of the outer wall of the second reactor 2 is provided with a second overflow port 22; the inlet 31 of the filtering centrifuge 3 is connected with the second overflow port 22 through a pipeline.
[0043] The present invention utilizes the first reactor 1 and the second reactor 2 as reaction vessels for simultaneous reaction, adopts a two-stage reactor series process, rationally utilizes space and time intervals, and improves production efficiency. At the same time, a slurry feed port is provided at the middle and lower part of each reactor, so that during the reaction process, silicon powder, catalyst and other raw materials can be intermittently added to the reactor according to the reaction situation. While adding materials, waste from the reactor is also intermittently discharged to maintain the active state of the reaction system, thereby extending the cycle of continuous production.
[0044] For further information, please refer to Figure 1, the top of the first reactor 1 and the second reactor 2 are both provided with an agitator 16. Preferably, the agitator 16 is an open turbine agitator. The open turbine agitator 16 used in the present invention is a mixed flow agitator, which can generate a strong radial flow during stirring, and the material tumbles up and down with a good effect, and will not cause the material to gather at the bottom, and can also generate a certain axial flow. Methanol is fed from the bottom of the reactor parallel to the agitator 16, and the high-speed flow rate causes the bottom material to tumble, which is beneficial to the exchange of upper and lower materials, and because the agitator 16 generates a certain axial flow during stirring, it is beneficial to mix the materials, increase the retention time of methanol, and help to improve the surface contact between methanol and silicon powder, thereby improving the reaction efficiency.
[0045] Preferably, please refer to Figure 1 The first reactor 1 and the second reactor 2 are both provided with a slag discharge port 17 at the bottom. The slag discharge port 17 at the bottom of the first reactor 1 is connected to the bottom of the second reactor 2 through a pipeline, and is discharged together with the tailings produced by the second reactor 2, or the slag discharge port 17 at the bottom of the first reactor 1 is directly discharged through valve control.
[0046] In order to facilitate monitoring of the remaining amount of slurry in each reactor, the inner walls of the first reactor 1 and the second reactor 2 are both provided with remote level gauges. By providing the remote level gauges, the volume and other parameters of the slurry in the reactor can be known through the numbers displayed on the display, and then the slurry can be added as needed. Preferably, the first reactor 1 is provided with a plurality of level gauge ports h1-h4 from top to bottom, and the installation of the level gauges facilitates the viewing of the liquid level height and the degree of mixed reaction in the reactor and the separation tank.
[0047] Preferably, the inner walls of the first reactor 1 and the second reactor 2 are both provided with remote pressure gauges, and over-limit alarms are set. When the pressure in the reactor exceeds the pressure, the pressure gauges are interlocked to open the vent valves.
[0048] The present invention also provides a method for producing tetramethoxysilane, using the reaction device as described above, the method comprising the following steps:
[0049] S1. Silicon powder and catalyst are mixed in a certain ratio in a batching tank to obtain a mixed material; wherein the mass ratio of silicon powder to catalyst is 10:1.
[0050] S2, feeding the mixed material through the solid and liquid phase feed port 11 at the top of the first reactor 1, and starting stirring;
[0051] S3. Add a certain proportion of solvent through the solid and liquid phase feed port 11 at the top of the first reaction kettle 1; add according to the dosage ratio of 1g silicon powder to 20mL solvent.
[0052] S4, start heating, raise the temperature to 200°C for activation for 1.5 hours, and then raise the temperature to 240°C;
[0053] S5, opening the methanol feed port 14, and introducing methanol;
[0054] S6. After 24 hours of reaction, as the reaction proceeds, the silicon powder content gradually decreases and the catalyst activity gradually decreases. At this time, a centrifugal pump is used to add a certain ratio of silicon powder, catalyst and solvent to the slurry through the slurry feed port. The amount of addition is determined by the remote level gauges of the two kettles.
[0055] S7, as the material continues to enter the first reactor 1, the liquid level of the first reactor 1 continues to rise, and the slurry in the first reactor 1 enters the second reactor 2 from the first overflow port 15 through the pipeline. When the liquid level of the second reactor 2 reaches 20%, stirring and heating are started to a temperature of 240°C;
[0056] S8, as the reaction continues, the liquid level of the second reactor 2 continues to rise, and the slurry in the second reactor 2 enters the filtering centrifuge 3 from the second overflow port 22 in the middle and upper part through the pipeline;
[0057] S9, after the slurry of the filtering centrifuge 3 enters the filter through the inlet 31, the liquid phase is discharged from the drum through the filter medium and the perforated drum wall under the action of centrifugal force and enters the solvent recovery tank, and the solid phase particles are retained on the filter medium to form a filter cake layer, which is discharged from the drum under the push of the spiral; the entire feeding, separation, liquid discharge and material discharge are completed automatically and continuously.
[0058] S10, during the reaction process, the products are collected through the top gas phase outlets 12 of the first reactor 1 and the second reactor 2, respectively, and are cooled before the next step.
[0059] Preferably, in step S1, the catalyst is at least two of nano copper powder, copper oxide, copper hydroxide, cuprous oxide, copper acetate, and bis(diethyl)copper phosphate. In step S3, the solvent is an organic solvent having a boiling point of not less than 230° C. Preferably, the solvent is any one of hexamethylphosphinyl triamide, hexamethylphosphoric acid triamide, quinoline, ethylene glycol carbonate, diethylene glycol, succinonitrile, and cyclopentane sulfone.
[0060] The present invention adopts the above-mentioned direct method to continuously produce tetramethoxysilane, takes silicon powder and methanol as raw materials, directly generates tetramethoxysilane under the catalytic action of a catalyst, and controls the reaction temperature to be above 230 degrees, so that the generated tetramethoxysilane becomes a gas phase and overflows from the top of the reactor for collection, which is convenient and fast. At the same time, no chlorine-containing by-products are generated in the reaction process, and the dechlorination process is omitted. The reaction process is safe and simple.
[0061] It has been determined that the purity of tetramethoxysilane obtained by the device and method for preparing tetramethoxysilane provided in the embodiment of the present invention is greater than 99.9%, and the product yield is 95%.
[0062] The above are only preferred embodiments of the present invention, and do not limit the patent scope of the present invention. For those skilled in the art, the present invention may have various changes and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the patent protection scope of the present invention.
Claims
1. A reaction device for producing tetramethoxysilane, characterized in that: The reaction device comprises: A first reactor (1), wherein the top of the first reactor (1) is provided with solid and liquid phase feed ports (11) and a gas phase discharge port (12), the lower portion of the outer wall of the first reactor (1) is provided with a first slurry feed port (13) and a methanol feed port (14), and the middle upper portion of the outer wall of the first reactor (1) is provided with a first overflow port (15); a second reactor (2), wherein a gas phase discharge port (12) is provided at the top of the second reactor (2), a second slurry feed port (21) and a methanol feed port (14) are provided at the lower part of the outer wall of the second reactor (2), the second slurry feed port (21) is connected to the first overflow port (15) through a pipeline, and a second overflow port (22) is provided at the middle upper part of the outer wall of the second reactor (2); and A filtering centrifuge (3), wherein the inlet (31) of the filtering centrifuge (3) is connected to the second overflow port (22) via a pipeline.
2. The reaction device for producing tetramethoxysilane according to claim 1, characterized in that: A stirrer (16) is provided on the top of each of the first reaction kettle (1) and the second reaction kettle (2).
3. The reaction device for producing tetramethoxysilane according to claim 2, characterized in that: The stirrer (16) is an open turbine stirrer.
4. The reaction device for producing tetramethoxysilane according to claim 1, characterized in that: The bottom of each of the first reaction kettle (1) and the second reaction kettle (2) is provided with a slag discharge port (17).
5. The reaction device for producing tetramethoxysilane according to claim 1, characterized in that: The inner walls of the first reaction kettle (1) and the second reaction kettle (2) are both provided with remote liquid level gauges.
6. The reaction device for producing tetramethoxysilane according to claim 1, characterized in that: The inner walls of the first reaction kettle (1) and the second reaction kettle (2) are both provided with remote pressure gauges.
7. A method for producing tetramethoxysilane, characterized in that Using the reaction device according to any one of claims 1 to 6, the method comprises the following steps: S1. Mixing silicon powder and catalyst in a certain proportion in a batching tank to obtain a mixed material; S2, feeding the mixed material through the solid and liquid phase feed ports (11) at the top of the first reaction kettle (1), and starting stirring; S3, adding a certain proportion of solvent through the solid and liquid phase feed ports (11) at the top of the first reaction kettle (1); S4, start heating, raise the temperature to 150-200°C for activation for 1.5-2.5 hours, and then raise the temperature to 230-245°C; S5, opening the methanol feed port (14) and introducing methanol; S6, after reacting for 22-26 hours, adding a slurry prepared by silicon powder, catalyst and solvent in a certain ratio through the first slurry feed port (13); S7, the slurry in the first reactor (1) enters the second reactor (2) from the first overflow port (15) through the pipeline. When the liquid level of the second reactor (2) reaches 20%-30%, stirring and heating are started to the temperature of 230-245°C; S8. As the reaction continues, the liquid level of the second reaction kettle (2) continues to rise, and the slurry in the second reaction kettle (2) enters the filtering centrifuge (3) from the second overflow port (22) in the upper middle portion through a pipeline; S9, after the slurry of the filtering centrifuge (3) enters the filter through the inlet (31), the liquid phase is discharged from the drum through the filter medium and the perforated drum wall under the action of centrifugal force and enters the solvent recovery tank, and the solid phase particles are trapped on the filter medium to form a filter cake layer, which is discharged from the drum under the push of the spiral; S10. During the reaction, the products are collected through the top gas phase outlets (12) of the first reaction kettle (1) and the second reaction kettle (2), respectively, and are cooled before the next step.
8. The reaction device for producing tetramethoxysilane according to claim 1, characterized in that: In step S1, the catalyst is at least two of nano copper powder, copper oxide, copper hydroxide, cuprous oxide, copper acetate, and bis(diethyl)copper phosphate.
9. The reaction device for producing tetramethoxysilane according to claim 7, characterized in that: In step S3, the solvent is an organic solvent having a boiling point of not less than 230°C.