Additive manufacturing method, additive manufacturing system, and additive manufacturing program
Through cutting processing and arc melting technology in the additive manufacturing area, preheating and adding molten metal is realized, which solves the problems of complex heating devices and long processing time in the existing technology, and improves the efficiency and quality of additive manufacturing.
Patent Information
- Application Number
- CN202280092341.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2022-02-28
- Publication Date
- 2024-10-01
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In additive manufacturing, existing technology requires the use of complex heating devices for preheating, which results in extended processing time and complicated system structure. The rapid cooling rate of molten metal can easily lead to thermal stress hardening and embrittlement.
By cutting in the additive manufacturing area to heat, use ceramic or CBN tools for dry cutting, avoid cooling media, use arc discharge to melt and move the wire to form a weld bead, achieve preheating and attach molten metal.
It simplifies the system structure, shortens the processing time, prevents thermal stress hardening and embrittlement, and improves the efficiency and quality of additive manufacturing.
Smart Images

Figure CN118742408A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to an additive manufacturing method, an additive manufacturing system and an additive manufacturing program. Background Art
[0002] In additive manufacturing, in which a metal material is melted and added to a base material to form a metal object, if the surface temperature of the base material is low, the molten metal added to the base material cools rapidly, which easily causes hardening and embrittlement of the heat-affected portion. Therefore, preheating is performed to make the surface temperature of the base material above a certain temperature in order to slow down the cooling rate of the molten metal and prevent hardening and embrittlement of the heat-affected portion.
[0003] For example, Patent Document 1 discloses that in a construction process of repairing the tip portion of a moving blade of a gas turbine by build-up welding, before welding, the tip portion is cut or ground and surface-finished, and then build-up welding is performed using a rod-shaped filler material or the like after preheating. Preheating is performed by bringing a high-frequency heating mechanism or a heating mechanism composed of an arc lamp or the like into contact with the outer side near the tip portion of the moving blade. Prior art literature
[0004] Patent Document 1: Japanese Patent Application Laid-Open No. 10-80767
[0005] When such a preheating heater, gas burner or other heating device is manually set by a person, the workpiece needs to be transported between the preheating process and the additive manufacturing process, which increases the processing time. In addition, since the heating device is assembled into the system, there is a problem of complicating the system structure. Summary of the invention
[0006] Therefore, an object of the present invention is to provide an additive manufacturing method, an additive manufacturing system, and an additive manufacturing program that can shorten the processing time without complicating the structure of the system in additive manufacturing.
[0007] The additive manufacturing method of the present invention includes: a preheating step, in which a cutting area of a workpiece including an additive manufacturing area is cut to heat the workpiece so that the temperature of the additive manufacturing area becomes above a preheating lower limit temperature; and an additive manufacturing step, in which molten metal is added to the additive manufacturing area of the workpiece that has been preheated by the preheating step.
[0008] On this basis you can: (1) Further cutting the cutting area when the temperature of the cutting area after cutting is low, (2) Determine the position where molten metal is added based on the shape of the workpiece after cutting. (3) Cutting the workpiece without supplying cooling medium. (4) Use ceramic tools or CBN tools as cutting tools for cutting. (5) The workpiece is gripped by a claw-shaped fixture and maintained in the gripping state during the preheating process and the additive manufacturing process. (6) Additive manufacturing uses arc discharge to melt a metal wire while moving it to stack weld beads.
[0009] In addition, the additive manufacturing system of the present invention includes: an additive manufacturing unit, which adds molten metal to the workpiece; a cutting processing unit, which cuts the surface of the workpiece; and a control unit, which sends a control signal for controlling the action to the additive manufacturing unit and the cutting processing unit, the control unit causes the cutting processing unit to cut the cutting area of the workpiece including the additive manufacturing area, thereby heating it so that the temperature of the additive manufacturing area becomes above the preheating lower limit temperature, and the control unit causes the additive manufacturing unit to add molten metal to the additive manufacturing area of the workpiece in the preheated state.
[0010] On this basis you can: (1) when the temperature of the additive manufacturing region after cutting is low, the control unit causes the cutting processing unit to further cut the cutting region to heat the additive manufacturing region; (2) The control unit determines the position where the molten metal is to be added based on the shape of the workpiece after cutting. (3) the control unit causes the cutting processing unit to cut the cutting area without supplying a cooling medium, (4) The control unit causes the cutting processing unit to use a ceramic tool or a CBN tool as a cutting tool to cut the cutting area. (5) also includes a claw-shaped clamp for holding the workpiece, (6) The additive manufacturing section causes the wire to move while being melted by arc discharge to stack weld beads.
[0011] In addition, the additive manufacturing program of the present invention includes a preheating routine in which a cutting processing unit cuts a cutting area of a workpiece including an additive manufacturing area, thereby heating the cutting area so that the temperature of the additive manufacturing area becomes above a preheating lower limit temperature; and an additive manufacturing routine in which the additive manufacturing unit adds molten metal to the additive manufacturing area of the workpiece in a preheated state.
[0012] On this basis you can: (1) based on the measurement result of the temperature of the additive manufacturing region after cutting, if the temperature of the additive manufacturing region is low, the cutting region is further cut to heat it, (2) Determine the position where molten metal is to be added to the workpiece based on the shape of the workpiece after cutting, (3) In the preheating routine, the cutting process is performed without supplying cooling medium to the cutting part. (4) During the preheating routine, use a ceramic tool or a CBN tool as a cutting tool for cutting. (5) In the additive manufacturing routine, the wire is moved while being melted by arc discharge to stack weld beads.
[0013] According to the above invention, since preheating can be performed without using a heating device, steps such as moving the heating device are not required, and the processing time can be shortened without complicating the structure of the processing system. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] Figure 1 is a perspective view of an additive manufacturing system according to an embodiment of the present invention. Figure 2 It is a perspective view of the main parts of the additive manufacturing system according to one embodiment of the present invention. Figure 3 It is a cross-sectional perspective view (partial module view) of an additive manufacturing system according to an embodiment of the present invention. Figure 4 This is a block diagram of the control unit included in the additive manufacturing system. Figure 5A is a side view showing a portion of an additive manufacturing method. Figure 5B is a side view showing a portion of an additive manufacturing method. Figure 6 is a flow chart showing an additive manufacturing method according to one embodiment of the present invention. Figure 7 is a flowchart showing an additive manufacturing method according to another embodiment of the present invention. Figure 8 This is a side view of a main part of the workpiece showing the shape after cutting and the position of additive manufacturing. Fig.9A It is a side view showing the method of the warm-up test. Fig. 9B It is a top view of the workpiece showing the cutting path of the preheating test. Fig.10 It is a graph showing the results of the warm-up test. DETAILED DESCRIPTION
[0015] Below, use Figures 1 to 8 The additive manufacturing method, additive manufacturing system and additive manufacturing program of the present invention are described in detail.
[0016] First, the additive manufacturing system will be described.
[0017] like Figure 1 and Figure 2As shown, the processing system 10 that can be used as an additive manufacturing system includes: a cutting processing unit 33 for cutting a workpiece W; and an additive manufacturing unit 34 for adding molten metal to the workpiece W. In addition, in this embodiment, the additive manufacturing unit 34 can form a weld bead while the metal wire is melted and moved by arc discharge, and additive manufacturing is performed by forming and laminating the weld bead.
[0018] The processing system 10 includes a cover 1 covering all sides, and a door 2, a window 3 and an operating panel 4 are provided in the front (close side) of the cover 1. The door 2 can be slid to the side to open and close, and the operator or the automatic assembly and disassembly device can install and disassemble the workpiece W from the outside of the cover 1. The window 3 is provided in order to visually confirm the workpiece W being processed from the outside. In the case of strong light emitted by arc discharge or the like in additive manufacturing, it is preferred that the window 3 can be switched to a filter plate, which can block the light of the arc discharge to a degree that can be observed from the outside by the naked eye. For example, the switching can be performed by changing the amount of light transmitted by a liquid crystal panel. In addition, in order to enable the operator to operate the processing system 10, an operating panel 4 is provided, and the operating panel 4 has an input device for inputting manufacturing processing programs and other action commands, and a display device for confirming the input content and actions.
[0019] The processing system 10 has a base 30 on the inner side of the cover 1, and the base 30 is the base of the processing system 10. In addition, the processing system 10 also includes: a saddle 31 supported to be freely movable in the left-right direction relative to the base 30 when viewed from the door 2 side; a column 32 supported to be freely movable in the front-back direction relative to the saddle 31; and a cutting processing unit 33 supported to be freely movable in the up-down direction relative to the column 32. In addition, an additive manufacturing unit 34 is provided in the cutting processing unit 33, which can move together with the cutting processing unit 33.
[0020] The cutting processing section 33 includes a cutting tool 35. In particular, the cutting processing section 33 includes a mechanism for holding and rotating the cutting tool 35, and the workpiece W can be processed by cutting processing such as milling while rotating the cutting tool 35. In addition, the additive manufacturing section 34 includes a welding torch 36, which can perform additive manufacturing on the workpiece W. Here, the cutting processing section 33 and the additive manufacturing section 34 are configured so that the cutting tool 35 and the welding torch 36 are separated from each other by a predetermined distance, and if one side is approached to the workpiece W, the other side is simultaneously avoided from the workpiece W so that there is no interference between the devices. In addition, the cutting processing section 33 is provided with a mechanism capable of automatically replacing the cutting tool 35, for example, it is preferred that the cutting tool 35 can be removed and avoided when performing arc discharge. In addition, the additive manufacturing section 34 is provided with a mechanism capable of accommodating the welding torch 36 therein, for example, it is preferred that the welding torch 36 can be retreated inside when performing cutting processing. In addition, the additive manufacturing section 34 can also be set to move freely up and down relative to the cutting processing section 33.
[0021] The processing system 10 is provided with a holding table 41 for holding the workpiece W and a fixture 42 for fixing the workpiece W to the holding table 41 in a manner supported by the base 30 below the cutting processing unit 33 and the additive manufacturing unit 34. In addition, the holding table 41 can be configured to be supported so as to be rotatable around an axis extending in the front-rear direction in a horizontal plane, and the workpiece W can be rotated around an axis extending in a direction orthogonal to the axis. That is, the workpiece W can be held by the holding table 41 so as to be rotatable around two axes. Thus, cutting processing such as turning can be performed while the workpiece W is rotated.
[0022] Furthermore, the machining system 10 includes a temperature measuring device 45 capable of measuring the temperature of the surface of the workpiece W. As the temperature measuring device 45, for example, a temperature measuring device capable of optically measuring the temperature in a non-contact manner, such as an infrared radiation thermometer, can be preferably used.
[0023] like Figure 3 As shown in FIG. 1 , the processing system 10 further includes an upper mask 5. The upper mask 5 includes a front portion 5a extending horizontally from the upper end of the mask 1 on the near side to the rear, and an inclined portion 5b extending downward and rearward behind the front portion 5a. In addition, the inclined portion 5b includes a hole 5c for inserting the lower part of the cutting processing part 33 and the additive manufacturing part 34 from the upper rear. That is, the upper mask 5 covers the cutting tool 35 and the welding torch 36 provided below the cutting processing part 33 and the additive manufacturing part 34 from above.
[0024] In addition, a driving mechanism 40 is provided inside or behind the base 30 (see Figure 4 ), the drive mechanism 40 generates and transmits power for moving the saddle 31, the column 32, the cutting processing part 33, the additive manufacturing part 34, the holding table 41, etc. The drive mechanism includes a power device such as a servo motor, and a power transmission mechanism such as a ball screw and a gear.
[0025] In addition, the processing system 10 includes a control unit 11, which sends a control signal for giving an operation instruction to these drive mechanisms, etc., and controls the operation of the entire processing system 10 including the saddle 31, the column 32, the cutting processing unit 33, the additive manufacturing unit 34, the holding table 41 and the temperature measuring device 45. The control unit 11 is also connected to the operation panel 4, and can receive input from the operation panel 4 and reflect it on the operation of the processing system 10.
[0026] In detail, Figure 4As shown in FIG. 1 , the control unit 11 includes a processor 14 implemented by an electronic circuit such as a central processing unit (CPU) and a memory 13 as a storage medium. A machining program 12 as a computer program is stored in the memory 13. In addition, the memory 13 also stores other programs 12a for controlling the operation of the machining system 10 and control data 12b including various parameters and assigned values related to the drive mechanism 40 for controlling the operation of the drive mechanism 40.
[0027] The control unit 11 also has a first input-output interface 15 that converts electrical signals to mediate the sending and receiving of information with the operating panel 4, and a second input-output interface 16 that similarly mediates the sending and receiving of information with the driver of the power device of the above-mentioned drive mechanism 40, etc., and a bus 17 that serves as a communication channel for electrical signals includes the memory 13 and is interconnected with the processor 14.
[0028] That is, the first input / output interface 15 can receive input from the input device of the operation panel 4 and transmit it to the processor 14, and can output signals from the processor 14 to the operation panel 4. Furthermore, the operation panel 4 can display information based on the signals output from the first input / output interface 15 on a display device or the like.
[0029] On the other hand, the second input / output interface 16 is connected to the drive mechanism 40, and can receive a control signal including an instruction for actuating the drive mechanism 40 from the processor 14, and transmit it to a driver of a power device in the drive mechanism, etc. In addition, in order to perform feedback control such as PID control on the drive mechanism, the second input / output interface 16 can receive a signal from a sensor, etc., and transmit it to the processor 14, wherein the sensor senses the action of the drive mechanism.
[0030] The drive mechanism 40 is mechanically connected to the saddle 31, the column 32, the cutting processing part 33, the additive manufacturing part 34, the holding table 41, and other mechanical devices included in the processing system 10 and operating, and transmits power to operate them. In addition, it is also connected to various sensors and temperature measuring devices 45 attached to them, and can send electrical signals about data such as measurement results to the processor 14 via the second input and output interface 16. That is, the control unit 11 sends a control signal to the drive mechanism 40 via the second input and output interface 16, thereby controlling the operation of the saddle 31, the column 32, the cutting processing part 33, the additive manufacturing part 34, the holding table 41, and other mechanical devices included in the processing system 10 and operating.
[0031] With these structures, the control unit 11 can operate the machining system 10 by causing the processor 14 to execute the machining program 12 stored in the memory 13 , thereby realizing the additive manufacturing method described later.
[0032] Next, the additive manufacturing method of this embodiment will be described. The additive manufacturing method can use the processing system 10 as described above.
[0033] In additive manufacturing, in which metal is melted and attached to a base material, preheating is generally required. After the molten metal is attached at a high temperature, it cools due to heat dissipation to the atmosphere, etc., which generates thermal stress and is prone to cracking. Therefore, first, before adding the molten metal, the surface of the base material in the additive manufacturing area to which the molten metal is to be attached is made to a temperature above the preheating lower limit temperature set according to the temperature range in which no cracks are generated. Then, in the preheated state before the temperature drops below the preheating lower limit temperature, additive manufacturing is started, thereby suppressing the generation of thermal stress and preventing the generation of cracks. In this case, the workpiece is generally preheated by an external heating device, etc., to ensure a temperature above the preheating lower limit temperature, and additive manufacturing is performed. On the other hand, the use of an external heating device prolongs the processing time due to the need to transport the workpiece. In addition, assembling the heating device inside will complicate the system structure.
[0034] Therefore, if Figure 5A As shown, in this embodiment, before adding molten metal, the surface of the workpiece W as the base material is cut, so that the workpiece W is preheated by cutting heat. In detail, first, the workpiece W is used as the base material and is mounted on the holding table 41 of the processing system 10 by means of the clamp 42. Then, as a preheating process, the cutting region as the region to be cut of the workpiece W is cut by the cutting processing unit 33, and the additive manufacturing region as the region to be additively manufactured in the workpiece W is heated by the cutting heat to perform preheating. That is, cutting is performed as a preheating process.
[0035] At this time, when additive manufacturing starts after cutting, cutting is performed in such a way that the surface temperature of the additive manufacturing area of the workpiece W becomes a temperature above the preheating lower limit temperature. Therefore, it is preferred that dry cutting is performed without supplying a cooling medium to the workpiece W during cutting in the preheating process. When performing dry cutting, it is preferred that, as the cutting tool 35, a tool made of a material having excellent mechanical strength at high temperatures, such as a ceramic tool or a CBN (Cubic Boron Nitride) tool, is used. In addition, dry cutting generally refers to a situation where cutting oil is not used, but in the present embodiment, dry cutting in which the additive manufacturing area of the workpiece W is cooled, such as dry cutting using gas as a cooling medium, is excluded. That is, in the present embodiment, dry cutting is dry cutting in which a liquid cooling medium such as cutting oil is not used, and it means that no other cooling medium is used either.
[0036] Moreover, if Figure 5BAs shown, following the preheating performed by the cutting process, molten metal is added by the additive manufacturing section 34. In detail, the wire 37 extending from the welding torch 36 of the additive manufacturing section 34 is moved along the surface of the workpiece W while the wire 37 is melted by arc discharge to form a weld bead 21. By forming such a weld bead 21, additive manufacturing is performed in the additive manufacturing area. Here, as described above, additive manufacturing is started in the preheating state before the temperature drops below the preheating lower limit temperature. In addition, an example is shown in which the cutting area 22 is the entire upper surface of the workpiece W and the additive manufacturing area 23 is a narrower range than it. In addition, by repeatedly performing additive manufacturing, for example, weld beads are stacked, so that a metal stacked shape can be obtained.
[0037] That is, Figure 6 As shown, the additive manufacturing method of this embodiment includes a preheating step (S1), and the preheating step (S1) heats the cutting area 22 while cutting, thereby preheating the additive manufacturing area 23. Since the preheating step (S1) preheats the additive manufacturing step (S2) of adding molten metal, the temperature of the cutting surface of the workpiece can be maintained at a preheated state above the preheating lower limit temperature when the additive manufacturing step (S2) starts. For example, considering the time from cutting to the start of additive manufacturing, the temperature in the preheating step can be made high with a margin relative to the preheating lower limit temperature.
[0038] In the additive manufacturing process (S2), the generation of cracks is prevented by adding molten metal in the preheated state. That is, the additive manufacturing process (S2) starts adding molten metal before the temperature drops below the preheating lower limit temperature. Additive manufacturing can be performed multiple times as needed to stack the weld beads 21 in multiple layers.
[0039] After the additive manufacturing, the finishing process (S3) is performed as needed. Preheating is not required in the finishing process, and the cutting conditions are determined from the perspective of finishing accuracy such as dimensional accuracy and surface roughness, and from the perspective of manufacturing efficiency.
[0040] In addition, as described above, the processing program 12 of this embodiment operates the processing system 10 to implement the above-mentioned processing method. That is, the processing program 12 at least includes a preheating routine and an additive manufacturing routine corresponding to each of the above-mentioned preheating step (S1) and additive manufacturing step (S2).
[0041] As described above, in this embodiment, by adjusting the cutting conditions such as dry cutting without using a cooling medium, the workpiece W is heated by the cutting heat accompanying the cutting process to perform preheating. Here, by adjusting the cutting conditions, the preheating temperature can be adjusted. For example, if the feed amount is reduced and the feed speed is increased, the cutting heat can be increased, and the preheating temperature can be increased. In addition, if the cutting path of the cutting process is not a unidirectional path for intermittent cutting, but a spiral path for continuous cutting, the cutting heat is continuously generated and the cutting heat per hour is increased, which can increase the preheating temperature. In addition, by increasing the cutting amount (the accumulation of the feed amount of multiple cutting), the total amount of cutting heat can be increased, thereby increasing the preheating temperature. In the case of lowering the preheating temperature, in addition to dissipating heat by waiting, the cutting conditions can also be adjusted in the opposite way to the above, such as reducing the feed speed. In addition, as cutting conditions, there are feed amount, cutting speed (rotational speed of the cutting tool 35), feed speed, cutting path, cutting amount, etc.
[0042] The temperature required for preheating of additive manufacturing is determined by the materials used in additive manufacturing, such as the wire used to form the weld bead, but it is preferred that the preheating lower limit temperature be determined to be within the range of 100°C to 300°C for most materials. For example, when using SUS630, if the temperature at the beginning of weld bead formation is less than 100°C, the possibility of low-temperature cracking increases, and if it exceeds 300°C, the possibility of weld penetration increases. Therefore, when using SUS630, the above-mentioned preheating lower limit temperature can be determined to be within the range of 100°C to 300°C. In addition, for example, when using SKD61, the possibility of cracking and peeling increases if it is less than 150°C. Therefore, in the case of SKD61, the above-mentioned predetermined temperature is determined to be within the range of 150°C or above.
[0043] As described above, according to this embodiment, before the additive manufacturing process of adding molten metal, preheating is performed at a preheating lower limit temperature or higher by cutting, and the cooling rate of the molten metal added to the base material is slowed down, thereby preventing the hardening and embrittlement of the heat-affected layer. In this way, according to the processing system 10, the workpiece W can be preheated without the external heating device that takes time to transport and the assembly-type heating device that makes the system complicated. Therefore, the structure of the processing system 10 can be kept simple and the processing time can be shortened.
[0044] In this embodiment, the additive manufacturing process forms a weld bead by melting the metal wire through arc discharge, but it can also be performed by other methods as long as it is a lamination process accompanied by preheating. For example, it can also be a method of adding by melting metal powder through arc discharge.
[0045] In addition, if Figure 7As shown, the cutting conditions can also be automatically adjusted according to the measured temperature before and after the preheating process. For example, before the preheating process (S1-2), the temperature of a predetermined part can be measured by the temperature measuring device 45, and the cutting conditions (S1-1) can be adjusted based on the result of the temperature measurement. As the cutting conditions, as described above, the cutting speed, feed speed, feed amount, cutting path, cutting amount, etc. can be adjusted on the premise that the cooling medium is not used (set to OFF). For example, when the temperature is relatively high, the cutting speed and feed speed can be reduced, so that the preheating is performed without burdening the tool. On the other hand, when the temperature is low, the cutting conditions are adjusted to a higher temperature. In addition, the temperature can be measured at the end of the preheating process (S1-2) to determine whether a temperature above the preheating lower limit temperature is obtained (S1-3). In the case where a temperature above the preheating lower limit temperature is not obtained (S1-3 is "No"), the cutting conditions (S1-1) can be adjusted again, and preheating (S1-2) performed by cutting processing can be further added to ensure the preheating temperature. In this case, the cutting conditions are adjusted to at least increase the cutting amount. When a temperature equal to or higher than the preheating lower limit temperature is obtained (S1-3: YES), additive manufacturing is performed in the additive manufacturing step. The machining program 12 may include a cutting condition automatic adjustment routine for adjusting cutting conditions based on such temperature measurement results.
[0046] At this time, refer to Figure 8 It is preferable that the position of the path including the position where the addition of molten metal starts in the additive manufacturing process is determined based on the shape of the workpiece W after the cutting process in the preheating process. For example, in the same figure, there is an inclined surface 54 that expands downward and outward on the side surface of the workpiece W, and when the upper surface 52 is cut in the preheating process, a part of the inclined surface 54 is cut. Considering that there is a case where the cutting amount is adjusted, it is conceivable that the cutting amount is adjusted more than this relative to the cut upper surface 52a. In this case, if the molten metal is added in a manner that ensures the inclined surface 54a after finishing, the weld bead 53a is formed when the upper surface 52a becomes after preheating. In contrast, when the upper surface 52b becomes, the weld bead 53b is formed in a wider range and at a deeper position relative to the upper surface 52 before cutting. In this way, it is preferable to adjust the position where the addition of molten metal starts and the position of the path in the additive manufacturing process based on the three-dimensional shape of the workpiece W and the shape of the workpiece W after the cutting in the preheating process obtained by the cutting amount in the preheating process.
[0047] Therefore, in the additive manufacturing process, additive manufacturing (S2-2) of adding molten metal can be performed on the basis of performing additive manufacturing path adjustment (S2-1). That is, in this case, the processing program 12 can include an additive manufacturing position automatic adjustment routine, which adjusts the position of the path including the starting position in additive manufacturing. And, finally, finishing cutting (S3) is performed as needed.
[0048] [Warm-up test] Using Figure 9 and Fig.10 The results of a preheating test of the workpiece W performed by cutting will be described.
[0049] like Fig.9A As shown in FIG. 1 , the temperature of the workpiece W when the surface of the flat workpiece W is dry-cut was investigated. Specifically, a disk-shaped workpiece W made of S25C steel and having a size of φ250 mm×t40 mm was prepared, and its main surface was made substantially horizontal and held on a holding table 41 by a clamp 42. In addition, a thermocouple 51 was attached to the workpiece W so that its bottom surface abutted against a warm junction. Then, the entire upper surface of the workpiece W was dry-cut with a feed amount of 0.25 mm, and the temperature measured by the thermocouple 51 was stored as the temperature of the workpiece W.
[0050] like Fig. 9B As shown in FIG. 1 , the cutting path P is a path that alternately turns back along a plurality of parallel straight lines from one end of the workpiece W to the opposite end. The turning portion of the cutting path P between the straight lines is a path along the circumference of the upper surface of the workpiece W, and the radial machining allowance is 30 mm. The temperature of the workpiece W was measured when cutting was performed multiple times along such a cutting path P.
[0051] like Fig.10 As shown in the figure, when a workpiece W at room temperature is cut twice along a cutting path P with a feed amount of 0.25 mm (2 paths) and a cutting amount of 0.5 mm, the temperature rises to 51.3°C at the end of the cutting process, and then rises by 0.2°C to 51.5°C in 3 minutes. It is considered that the temperature rise caused by heat conduction from the cutting surface is greater than the temperature drop caused by heat dissipation after the cutting is completed due to the relatively low temperature. In the 4-path, 6-path, and 8-path, the temperature drops by 3.6°C, 5.3°C, and 6.4°C respectively from 84.8°C, 117.8°C, and 145.5°C at the end of the cutting process in the 3-minute period.
[0052] This indicates that, at least in the case of the workpiece W used in the present preheating test, preheating to approximately 140° C. is sufficiently feasible.
[0053] In the actual processing method, the conditions of the combination of cutting processing and additive manufacturing in the preheating process can be determined in advance based on the data obtained by performing the preheating test as described above, and the manufacturing process according to the combination can be performed. In addition, the speed of temperature drop varies depending on the heat capacity of the workpiece W, the contact condition with the fixture described later, the temperature difference with the surroundings, etc., so it is preferable to determine the conditions of the combination of cutting processing and additive manufacturing based on these considerations.
[0054] In addition, if Fig.9A As shown, the clamp 42 is preferably a claw-shaped clamp. That is, in the clamp 42, the workpiece W can be gripped by the claw-shaped chuck portion 42a. Thus, when gripping the workpiece W, the heat dissipation from the clamp 42 is suppressed by abutting against the workpiece W with a smaller area, and the heat conduction to the processing system 10 via the holding table 41 is reduced as much as possible, so that the temperature of the workpiece W is maintained at a high level and preheating is performed efficiently. Preferably, the material of the chuck portion 42a is a material with a relatively low thermal conductivity. In addition, if the gripping state achieved by such a claw-shaped clamp is maintained through the preheating process and the additive manufacturing process, the heat dissipation from the workpiece W can be suppressed not only in the preheating process but also until the start of additive manufacturing.
[0055] The representative embodiments of the present invention and the accompanying variations are described above, but the present invention is not necessarily limited thereto and can be appropriately modified by those skilled in the art. That is, those skilled in the art can think of various alternative embodiments and variations without departing from the scope of the claims recorded in this application. Description of Reference Numerals
[0056] 10 Processing system 11. Control Unit 21 weld pass 33 Cutting Processing Department 34 Additive Manufacturing Department 35 Cutting tools 36 Welding torch 45 Temperature measuring device S1 Preheating process W Workpiece
Claims
1. An additive manufacturing method, in, Include: A preheating step of heating the workpiece by cutting a cutting region including an additive manufacturing region so that the temperature of the additive manufacturing region becomes equal to or higher than a preheating lower limit temperature; and The additive manufacturing step adds molten metal to the additive manufacturing region of the workpiece that has been preheated in the preheating step.
2. The additive manufacturing method according to claim 1, in, In the preheating step, the temperature of the additive manufacturing region is measured after the workpiece is cut, and when the temperature is lower than the preheating lower limit temperature, the cutting region is further cut to heat the additive manufacturing region.
3. The additive manufacturing method according to claim 1 or 2, in, In the additive manufacturing step, a position at which the molten metal is to be added to the workpiece is determined based on the shape of the workpiece after cutting in the preheating step.
4. The additive manufacturing method according to claim 1, in, The cutting in the preheating step is performed without supplying a cooling medium to the workpiece.
5. The additive manufacturing method according to claim 1, in, The cutting in the preheating step uses a ceramic tool or a CBN tool as a cutting tool.
6. Additive manufacturing method according to one of claims 1 to 5, in, The workpiece is gripped by a claw-shaped clamp, and the gripped state is maintained during the preheating step and the additive manufacturing step.
7. Additive manufacturing method according to one of claims 1 to 6, in, The additive manufacturing process causes a metal wire to move while being melted by arc discharge to stack weld beads.
8. An additive manufacturing system, in, The invention comprises: an additive manufacturing part for adding molten metal to a workpiece; a cutting processing part for cutting a surface of the workpiece; and a control part for sending a control signal for controlling the operation of the additive manufacturing part and the cutting processing part. The control unit causes the cutting processing unit to cut a cutting region including an additive manufacturing region of the workpiece, thereby heating the cutting region so that a temperature of the additive manufacturing region becomes equal to or higher than a preheating lower limit temperature. The control unit causes the additive manufacturing unit to add the molten metal to the additive manufacturing region of the workpiece in a preheated state.
9. The additive manufacturing system according to claim 8, in, Also includes a temperature measuring device for measuring the surface temperature of the workpiece, The control unit controls the cutting unit to further cut the cutting area based on a measurement result of the temperature of the additive manufacturing area after cutting the workpiece by the temperature measuring device, thereby heating the additive manufacturing area when the temperature is lower than the preheating lower limit temperature.
10. The additive manufacturing system according to claim 8 or 9, in, The control unit determines a position at which the molten metal is to be added to the workpiece based on a shape of the workpiece cut by the cutting processing unit, and the additive manufacturing unit adds the molten metal.
11. Additive manufacturing system according to one of claims 8 to 10, in, The control unit causes the cutting unit to cut the cutting region without supplying a cooling medium.
12. Additive manufacturing system according to one of claims 8 to 11, in, The control unit causes the cutting unit to cut the cutting region using a ceramic tool or a CBN tool as a cutting tool.
13. Additive manufacturing system according to one of claims 8 to 12, in, Also included is a claw-like clamp for holding the workpiece.
14. Additive manufacturing system according to one of claims 8 to 13, in, The additive manufacturing unit moves a metal wire while being melted by arc discharge to stack weld beads.
15. An additive manufacturing process, in, Include: A preheating routine of causing a cutting section to cut a cutting region including an additive manufacturing region of a workpiece to heat the cutting region so that the temperature of the additive manufacturing region becomes equal to or higher than a preheating lower limit temperature; and An additive manufacturing routine in which an additive manufacturing unit adds molten metal to the additive manufacturing region of the preheated workpiece.
Citation Information
Patent Citations
Combined processing apparatus and combined processing method
CN108472776A
Inertial friction welding method based on preheating by friction
CN109590598A
Composite manufacturing system and method of additive manufacturing and laser preheating assisted subtractive cutting
CN111702322A
Dry cutting work strengthening heat-transmission method in consideration of cuttings heat exchange
CN111730408A
Manufacturing method for additively manufactured body and manufacturing device for additively manufactured body
CN112334253A