Ceramic capacitor with double L-shaped pins and preparation method thereof

Through the double L-shaped pin structure and welding technology, the problem of insufficient strength of traditional ceramic capacitors in high-intensity vibration tests is solved, the welding area and stability are improved, and it is suitable for high-reliability environments such as aerospace and aviation.

CN118866554AActive Publication Date: 2024-10-29FUJIAN TORCH ELECTRON TECH CO LTD

Patent Information

Application Number
CN202411060458.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-05
Publication Date
2024-10-29
Estimated Expiration
2044-08-05

AI Technical Summary

Technical Problem

Traditional L-shaped lead ceramic capacitors are not strong enough in high-intensity vibration tests and cannot meet the high reliability requirements in harsh environments such as aerospace and aerospace. Their small welding area limits their application.

Method used

It adopts a double L-shaped pin structure, and the two symmetrically arranged frames are welded with solder as a bracket to increase the welding area and strength. During the welding process, solder layers and exhaust holes with different melting points are used to improve the welding strength and stability.

Benefits of technology

It improves the welding strength of ceramic capacitors and PCB boards, increases resistance to high-intensity vibration, improves product reliability, and is suitable for high-reliability aerospace and other fields.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118866554A_ABST
    Figure CN118866554A_ABST
Patent Text Reader

Abstract

The invention relates to a ceramic capacitor with double L-shaped pins and a preparation method thereof, and the ceramic capacitor comprises two supports which are oppositely arranged, one or more ceramic chips which are arranged between the two supports, and two first solder layers which are respectively arranged between the end parts of the one or more ceramic chips and the opposite supports. The support comprises two frames which are symmetrically arranged and a second solder layer arranged between the two frames. Each frame comprises a frame body, a plurality of L-shaped pins arranged at the bottom of the frame body at intervals, a plurality of supporting plates arranged between every two adjacent L-shaped pins and a plurality of exhaust holes evenly formed in the frame body. According to the invention, the structure of the ceramic capacitor is limited, and the two symmetrically arranged frames are mutually welded through the welding flux to serve as the support, so that the welding area of the prepared support and the PCB is doubled, the welding strength of the prepared ceramic capacitor is improved, and the bonding strength of the ceramic capacitor and the PCB is better.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of ceramic capacitor preparation, and in particular relates to a double L-shaped pin ceramic capacitor and a preparation method thereof. Background Art

[0002] With the rapid and continuous development of science and technology, the demand for small-size, large-capacity, and high-power capacitors in fields such as power supply, industry, automobile, military industry, and aerospace is increasing. Traditional chip ceramic capacitors are difficult to meet the demand for large capacity. Therefore, multiple ceramic capacitors are assembled in parallel to meet the demand for large capacity capacitors.

[0003] In harsh environments such as aerospace, more reliable components are needed. The characteristic of ceramic chips is that they are resistant to compression but not tension. Single chips are directly welded on PCB boards and are easily affected by board bending stress. Therefore, by welding the chip together through leads, the board bending stress will act on the leads without affecting the ceramic chip, thus solving the board bending stress problem; however, the existing L-shaped pin structure is not strong enough, the contact area with the PCB board is small, and it cannot adapt to higher-intensity vibration tests, which greatly limits its application occasions and needs further improvement. Summary of the invention

[0004] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a double L-shaped pin ceramic capacitor with high welding strength and good vibration resistance. Another purpose is to provide a method for preparing the above ceramic capacitor.

[0005] The present invention adopts the following technical solution:

[0006] A double L-shaped pin ceramic capacitor comprises two brackets arranged opposite to each other, one or more ceramic chips arranged between the two brackets, and two first solder layers respectively arranged between the ends of the one or more ceramic chips and the opposite brackets, wherein the bracket comprises two symmetrically arranged frames and a second solder layer arranged between the two frames.

[0007] The frame includes a frame body, a plurality of L-shaped pins spaced apart at the bottom of the frame body, a plurality of support plates disposed between two adjacent L-shaped pins, and a plurality of exhaust holes evenly arranged on the frame body. The plurality of L-shaped pins of the two frames are stacked and disposed at the lower end of the bracket.

[0008] Furthermore, a clearance area is formed between two adjacent L-shaped pins, and the support plate is arranged in the clearance area.

[0009] Furthermore, the double L-shaped pin includes a vertical section connected to the frame body and a horizontal section arranged perpendicular to the vertical section, the support plate is arranged higher than the horizontal section, and the horizontal section and the support section are arranged in the same direction.

[0010] A method for preparing a double L-shaped lead ceramic capacitor comprises the following steps:

[0011] Step 1: first place a frame in a frame welding jig, with the L-shaped pin facing downward, then apply a second solder on the surface opposite to the other frame, then place another frame, fit it with the second solder, and set its L-shaped pin facing upward; then assemble the frame welding jig, and send it into a reflow oven for welding to obtain the bracket;

[0012] Step 2: Place the welded bracket into a finished welding jig, and apply a first solder on the opposite surface of the bracket and another bracket, then stack one or more ceramic chips as required, then apply the first solder on the ends of the stacked one or more ceramic chips, and place another bracket; then assemble the finished welding jig, place the multiple L-shaped pins of the bracket upwards, and send it into a reflow oven for welding to obtain the double L-shaped pin ceramic capacitor.

[0013] Furthermore, in step one, the temperature of the reflow soldering is 290-310°C; in step two, the temperature of the reflow soldering is 250-270°C.

[0014] Furthermore, the frame welding fixture includes a base, a pressure block arranged on the base, and a positioning mechanism arranged between the base and the pressure block. The base is provided with a welding groove for installing the frame, and the opposing surfaces of the pressure block and the base are formed with a positioning portion that can be embedded in the welding groove and abut against the frame.

[0015] Furthermore, the positioning mechanism includes two positioning posts relatively arranged on the base and extending upward, and two positioning holes arranged on the pressing block and capable of respectively embedding the two positioning posts.

[0016] Furthermore, the finished welding jig includes an upper mold base and a lower mold base that are relatively arranged and a limiting mechanism arranged between the upper mold base and the lower mold base, and the opposing surfaces of the upper mold base and the lower mold base are formed with an upper mounting groove extending upward for mounting a bracket and multiple ceramic chip ends, and the opposing surfaces of the lower mold base and the upper mold base are formed with a lower mounting groove extending downward for mounting a bracket and a ceramic chip end.

[0017] Furthermore, the upper mounting groove includes a first upper mounting groove and a second upper mounting groove which are arranged in sequence from top to bottom, the length of the second upper mounting groove is greater than the length of the first upper mounting groove, the bracket opposite to the upper mold base is arranged in the first upper mounting groove, and the end of the ceramic chip opposite to the upper mold base is arranged in the second upper mounting groove.

[0018] Furthermore, the limiting mechanism includes two limiting columns arranged relatively to each other on the upper die base and two limiting holes arranged on the upper die base into which the limiting columns can be embedded.

[0019] From the above description of the present invention, it can be seen that compared with the prior art, the beneficial effects of the present invention are as follows: the present application limits the structure of the ceramic capacitor, and uses two symmetrically arranged frames welded to each other by solder as a bracket, so that the welding area between the prepared bracket and the PCB board is doubled, and the welding strength of the prepared ceramic capacitor is improved, so that the bonding strength between the ceramic capacitor and the PCB board is better. Compared with the single-frame ceramic capacitor, it can withstand higher intensity vibration, improve the reliability of the product, and can be applied to high-reliability occasions such as aerospace. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 Schematic diagram of the structure of a ceramic capacitor Figure 1 ;

[0021] Figure 2 Schematic diagram of the structure of a ceramic capacitor Figure 2 ;

[0022] Figure 3 The structure of the bracket is shown in Figure 2. Figure 1 ;

[0023] Figure 4 The structure of the bracket is shown in Figure 2. Figure 2 ;

[0024] Figure 5 Schematic diagram of the frame welding fixture Figure 1 ;

[0025] Figure 6 Schematic diagram of the frame welding fixture Figure 2 ;

[0026] Figure 7 Schematic diagram of the frame welding fixture Figure 3 ;

[0027] Figure 8 The structure of the finished welding fixture is shown in Figure 1. Figure 1 ;

[0028] Fig. 9 The structure of the finished welding fixture is shown in Figure 1. Figure 2 ;

[0029] Fig.10 The structure of the finished welding fixture is shown in Figure 1. Figure 3 ;

[0030] Fig.11 The structure of the finished welding fixture is shown in Figure 1. Figure 4 ;

[0031] Fig.12 The structure of the finished welding fixture is shown in Figure 1. Figure 5 ;

[0032] Fig.13It is a cross-sectional view of the internal structure of the ceramic chip;

[0033] In the figure, 1-bracket, 2-ceramic chip, 3-first solder layer, 4-frame, 5-second solder layer, 6-frame welding fixture, 7-finished product welding fixture, 21-capacitor chip body, 22-external electrode layer, 221-first external electrode, 222-second external electrode, 223-third external electrode, 23-dielectric layer, 24-first internal electrode layer, 241-first long internal electrode, 242-first short internal electrode, 25-second internal electrode layer, 251-second short internal electrode, 252-second long internal electrode, 41-frame body, 42-L-shaped pin, 421-vertical pin Straight section, 422-horizontal section, 43-support plate, 44-exhaust hole, 45-allowance area, 61-base, 611-welding groove, 62-pressing block, 621-positioning part, 622-heat dissipation hole, 63-positioning mechanism, 631-positioning column, 632-positioning hole, 71-upper die base, 711-upper mounting groove, 712-first upper mounting groove', 713-second upper mounting groove, '72-lower die base, 721-lower mounting groove, 722-first lower mounting groove, 723-second lower mounting groove, 73-limiting mechanism, 731-limiting column, 732-limiting hole. DETAILED DESCRIPTION

[0034] The present invention is further described below through specific implementation modes.

[0035] Reference Figures 1 to 13 As shown, a double L-shaped pin ceramic capacitor includes two brackets 1 arranged opposite to each other, one or more ceramic chips 2 arranged between the two brackets 1, and a first solder layer 3 respectively arranged at the end of one or more ceramic chips 2 and the brackets 1 opposite to each other.

[0036] The bracket 1 includes two symmetrically arranged frames 4 and a second solder layer 5 arranged between the two frames 4, wherein the melting point of the second solder layer 5 is higher than the melting point of the first solder layer 3, so that during the secondary reflow soldering, the second solder layer 5 will not melt and cause the risk of the bracket 1 falling apart; specifically, the second solder layer 5 uses tin-lead alloy solder, whose composition is Sn10Pb90, and the melting point of the solder after welding is 287°C; the first solder layer 3 uses tin-antimony alloy solder, whose composition is Sn90Sb10, and the melting point of the solder after welding is 240°C.

[0037] The frame 4 includes a frame body 41, a plurality of L-shaped pins 42 spaced apart at the bottom of the frame body 41, a plurality of support plates 43 disposed between two adjacent L-shaped pins 42, and a plurality of exhaust holes 44 evenly arranged on the frame body 41. The plurality of L-shaped pins 42 of the two frames 4 are symmetrically disposed at the lower end of the bracket 1. By arranging a plurality of exhaust holes 44 on the frame body 41, during the welding process of the bracket 1, not only heat can be dissipated, but also the evaporated flux in the solder can be discharged through the exhaust holes 44, so that the second solder layer 5 is more compact; specifically, a clearance area 45 is formed between the two L-shaped pins 42, and the support plate 43 is disposed in the clearance area 45; further, the double L-shaped pins 42 include a vertical section 421 connected to the frame body 41 and a horizontal section 422 disposed perpendicular to the vertical section 421, and the support plate 43 is disposed in the same direction as the horizontal section 422 and is disposed higher than the horizontal section 422.

[0038] The ceramic chip 2 includes a capacitor chip body 21 and two outer electrode layers 22 arranged at both ends of the capacitor chip body 21, wherein the capacitor chip body 21 is formed by stacking and firing a plurality of dielectric layers, the dielectric layer includes a dielectric layer 23 and an inner electrode group printed on the dielectric layer 23, the inner electrode group includes a plurality of first inner electrode layers 24 and a second inner electrode layer 25 alternately arranged at intervals in the upper and lower parts, specifically, the first inner electrode layer 24 includes a first long inner electrode 241 and a first short inner electrode 242 arranged at intervals in the left and right parts, the second inner electrode layer 25 includes a second short inner electrode 251 and a second long inner electrode 252 arranged at intervals in the left and right parts, and the first long inner electrode 241 and the second long inner electrode 252 are alternately arranged in the upper and lower parts; further, the dielectric layer 23 is made of barium titanate ceramic, and the inner electrode group is made of palladium silver metal.

[0039] The outer electrode layer 22 includes a first outer electrode 221 , a second outer electrode 222 and a third outer electrode 223 arranged in sequence from the inside to the outside. The first outer electrode on the left is connected to the second short inner electrode 251 , and the first outer electrode on the right is connected to the first short inner electrode 242 .

[0040] A method for preparing a double L-shaped lead ceramic capacitor comprises the following steps:

[0041] Step 1: first place a frame 4 in a frame welding jig 6, with the L-shaped pin 42 facing downward, then apply a second solder on the surface opposite to the other frame, then place another frame, fit it with the second solder, and set its L-shaped pin upward; then assemble the frame welding jig 5, send it into a reflow oven, and weld it at 290-310° C. to obtain the bracket 1;

[0042] Step 2, place the welded bracket 1 into the finished welding fixture 7, and apply the first solder on the opposite surface of the bracket 1 and the other bracket, then stack one or more ceramic chips 2 as required, then apply the first solder on the ends of the stacked one or more ceramic chips 2, and place another bracket; then assemble the finished welding fixture 7, and place the multiple L-shaped pins 42 of the bracket upwards, send it into the reflow oven, and perform welding at 250-270°C to obtain the double L-shaped pin ceramic capacitor.

[0043] The frame welding fixture 6 includes a base 61, a pressing block 62 arranged on the base 61, and a positioning mechanism 63 arranged between the base 61 and the pressing block 62. Specifically, the base 61 is provided with a welding groove 611 for mounting the frame 4; the pressing block 62 and the base 61 have opposite surfaces formed with a positioning portion 621 that can be embedded in the welding groove 611 and abut against the frame 4; the positioning mechanism 63 includes two positioning columns 631 that are relatively arranged on the base 61 and extend upward, and two positioning holes 632 that are arranged on the pressing block 62 and can be respectively embedded in the two positioning columns 631; further, the pressing block 62 is provided with A heat dissipation hole 622 extends inward from its top surface and is opposite to the welding groove 611. The heat dissipation hole 622 can not only dissipate heat, but also allow the evaporated flux in the solder to be discharged through the heat dissipation hole 622. When the frame 4 is welded, first place one frame 4 in the welding groove 611, then apply the second solder and stack another frame to make it fit with the second solder. Then, through the cooperation of the positioning column 631 and the positioning hole 632, the positioning part 621 on the pressing block 62 is embedded in the welding groove 611 and abutted against the frame located above, so as to press the two frames 4 tightly. Ensure that after reflow soldering, a stable connection can be formed between the two frames 4.

[0044] The finished welding fixture 7 comprises an upper die seat 71 and a lower die seat 72 which are arranged opposite to each other, and a limiting mechanism 73 which is arranged between the upper die seat 71 and the lower die seat 72, wherein the upper die seat 71 and the lower die seat 72 have an upper mounting groove 711 which extends upwards for mounting the relative bracket and the ends of the plurality of ceramic chips; the lower die seat 72 and the upper die seat 71 have a lower mounting groove 721 which extends downwards for mounting the relative bracket and the ends of the ceramic chips; the limiting mechanism 73 comprises two limiting columns 731 which are arranged opposite to each other on the upper die seat 71 and a limiting mechanism 73 which is arranged between the upper die seat 71 and the lower die seat 72. Two limiting holes 732 are arranged on the upper mold base 71 for the relative limiting column 731 to be embedded; specifically, the upper mounting groove 711 includes a first upper mounting groove 712 and a second upper mounting groove 713 which are arranged in sequence from top to bottom, and the length of the second upper mounting groove 713 is longer than the length of the first upper mounting groove 712, the bracket opposite to the upper mold base 71 is arranged in the first upper mounting groove 712, and the end of the ceramic chip opposite to the upper mold base 71 is arranged in the second upper mounting groove 713; the lower mounting groove 721 includes a first lower mounting groove 722 and a The second lower mounting groove 723, and the length of the first lower mounting groove 722 is longer than the length of the second lower mounting groove 723, the bracket opposite to the lower mold base 72 is arranged in the second lower mounting groove 723, and the end of the ceramic chip opposite to the lower mold base is arranged in the first lower mounting groove 722; when the finished product is welded, first place a bracket 1 in the second lower mounting groove 721, apply the first solder, and then stack one or more ceramic chips 2 on the first solder according to needs; then apply the first solder to the end of one or more ceramic chips 2, and attach another bracket The first solder is applied; then the upper mold base 71 and the lower mold base 72 are pressed tightly by the cooperation of the limiting column 731 and the limiting hole 732, and at the same time, the multiple L-shaped pins 42 of the bracket 1 are placed upward, and sent into a reflow oven for welding at 250-270°C to obtain a double L-shaped pin ceramic capacitor; during reflow welding, the multiple L-shaped pins 42 are placed upward to avoid tin creeping during welding and prevent the first solder from melting and gathering at the bottom of the bracket pin, which will affect the appearance of the product on the one hand and reduce the product's anti-bending performance on the other hand.

[0045] A single frame was used as a bracket, and a ceramic capacitor was prepared according to the method defined in the present application as a comparative example. Then, the double L-shaped pin ceramic capacitor prepared in the present application and the comparative example were subjected to vibration finite element simulation test, wherein the experimental conditions and steps are as follows:

[0046] (a) Before the test, set the test parameters (according to Table 1), and conduct a pre-test appearance inspection and function and performance test on the test product under the standard atmospheric conditions of the test, and conduct an appearance inspection and record the results;

[0047] (b) The test product shall be subjected to a 36-hour vibration test under the specified test conditions. After the vibration function test, the function and performance of the test product shall be tested and recorded;

[0048] (c) After the test, the test product shall be inspected for appearance, function and performance under the standard atmospheric conditions of the test, and the appearance inspection results shall be recorded.

[0049] For specific results, see Table 1 and Table 2.

[0050] Table 1 Vibration test spectrum conditions

[0051]

[0052] Table 2 Simulation results

[0053]

[0054]

[0055] From the data in Table 2, we can see that after 36 hours of vibration, the root mean square stress of the bracket and welding point of the double L frame structure is 98.25MPa and 10.14MPa respectively, and the root mean square stress of the bracket and welding point of the single L frame structure is 315.2MPa and 56.71MPa respectively. The double L-type structure is much smaller than the single L-type structure in terms of data, so the double L-type structure has stronger anti-vibration ability than the single L-type structure.

[0056] The present application limits the structure of the ceramic capacitor, and uses two symmetrically arranged frames 4 welded to each other by solder as a bracket 1, so that the welding area between the prepared bracket 1 and the PCB board is doubled, the welding strength of the prepared ceramic capacitor is improved, and the bonding strength between the ceramic capacitor and the PCB board is better. Compared with a single-frame ceramic capacitor, it can withstand higher intensity vibrations, thereby improving the reliability of the product and can be applied to high-reliability occasions such as aerospace.

[0057] The above description is only a preferred embodiment of the present invention, and therefore cannot be used to limit the scope of implementation of the present invention. That is, equivalent changes and modifications made according to the application scope of the present invention and the contents of the specification should still fall within the scope of the present invention.

Claims

1. A double L-shaped lead ceramic capacitor, characterized in that: The invention comprises two brackets arranged opposite to each other, one or more ceramic chips arranged between the two brackets, and two first solder layers respectively arranged between the ends of the one or more ceramic chips and the opposite brackets, wherein the bracket comprises two symmetrically arranged frames and a second solder layer arranged between the two frames. The frame includes a frame body, a plurality of L-shaped pins spaced apart at the bottom of the frame body, a plurality of support plates disposed between two adjacent L-shaped pins, and a plurality of exhaust holes evenly arranged on the frame body. The plurality of L-shaped pins of the two frames are stacked and disposed at the lower end of the bracket.

2. A double L-shaped lead ceramic capacitor according to claim 1, characterized in that: A clearance area is formed between two adjacent L-shaped pins, and the support plate is arranged in the clearance area.

3. A double L-shaped lead ceramic capacitor according to claim 1, characterized in that: The double L-shaped pin comprises a vertical section connected to the frame body and a horizontal section arranged perpendicular to the vertical section. The support plate is arranged higher than the horizontal section, and the horizontal section and the support section are arranged in the same direction.

4. The method for preparing a double L-shaped lead ceramic capacitor according to claim 1, characterized in that: The following steps are involved: Step 1: first place a frame in a frame welding jig, with the L-shaped pin facing downward, then apply a second solder on the surface opposite to the other frame, then place another frame, fit it with the second solder, and set its L-shaped pin facing upward; then assemble the frame welding jig, and send it into a reflow oven for welding to obtain the bracket; Step 2: Place the welded bracket into a finished welding jig, and apply a first solder on the opposite surface of the bracket and another bracket, then stack one or more ceramic chips as required, then apply the first solder on the ends of the stacked one or more ceramic chips, and place another bracket; then assemble the finished welding jig, place the multiple L-shaped pins of the bracket upwards, and send it into a reflow oven for welding to obtain the double L-shaped pin ceramic capacitor.

5. The method for preparing a double L-shaped lead ceramic capacitor according to claim 4, characterized in that: In step 1, the temperature of the reflow soldering is 290-310°C; in step 2, the temperature of the reflow soldering is 250-270°C.

6. The method for preparing a double L-shaped lead ceramic capacitor according to claim 4, characterized in that: The frame welding fixture includes a base, a pressure block arranged on the base and a positioning mechanism arranged between the base and the pressure block. The base is provided with a welding groove for installing the frame, and the opposing surfaces of the pressure block and the base are formed with a positioning portion that can be embedded in the welding groove and abut against the frame.

7. The method for preparing a double L-shaped lead ceramic capacitor according to claim 6, characterized in that: The positioning mechanism comprises two positioning posts which are arranged on the base and extend upwards, and two positioning holes which are arranged on the pressing block and can be respectively embedded in the two positioning posts.

8. The method for preparing a double L-shaped lead ceramic capacitor according to claim 4, characterized in that: The finished welding jig includes an upper mold base and a lower mold base arranged opposite to each other and a limiting mechanism arranged between the upper mold base and the lower mold base. The opposing surfaces of the upper mold base and the lower mold base are formed with upper mounting grooves extending upward for mounting brackets and multiple ceramic chip ends. The opposing surfaces of the lower mold base and the upper mold base are formed with lower mounting grooves extending downward for mounting brackets and ceramic chip ends.

9. The method for preparing a double L-shaped lead ceramic capacitor according to claim 8, characterized in that: The upper mounting groove includes a first upper mounting groove and a second upper mounting groove which are arranged in sequence from top to bottom. The length of the second upper mounting groove is greater than the length of the first upper mounting groove. The bracket opposite to the upper mold base is arranged in the first upper mounting groove, and the end of the ceramic chip opposite to the upper mold base is arranged in the second upper mounting groove.

10. The method for preparing a double L-shaped lead ceramic capacitor according to claim 8, characterized in that: The limiting mechanism comprises two limiting posts arranged relatively on the upper die seat and two limiting holes arranged on the upper die seat for the relative limiting posts to be embedded.

Citation Information

Patent Citations

  • High-capacity multi-pin support capacitor and preparation method thereof

    CN113130206A

  • High-voltage pulse capacitor and production method thereof

    CN117457390A

  • Bracket ceramic capacitor and welding jig thereof

    CN211728085U

  • Ceramic capacitor impact test device

    CN218726243U

  • Radio frequency microwave chip type multilayer ceramic dielectric capacitor

    CN220171930U

Cited By

  • Structural optimization method of multi-core-group ceramic dielectric capacitor support based on finite element

    CN120597605A