CMP process polishing table, device and process method

By designing a polishing platform with independent polishing areas and gaps in the CMP process and using different abrasive fluids in these areas, the problem of uneven wafer dispersion is solved, and better polishing effect and integrated circuit performance is achieved.

CN118893570APending Publication Date: 2024-11-05CHENGDU HIGH-TECH JIN SCI&TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310489222.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-04
Publication Date
2024-11-05

AI Technical Summary

Technical Problem

In the semiconductor manufacturing process, especially in the CMP process, it is difficult to control the polishing amount in the outermost corner edge field of the wafer, resulting in uneven wafer dispersion, affecting the performance and reliability of the integrated circuit.

Method used

Design a CMP process polishing platform, with the surface divided into two areas of the common rotation axis, one inner and one outer areas as polishing areas, and a gap is set between the two areas, and abrasive liquid of different ratios is sprayed to achieve different polishing Characteristics: polishing is performed by using different abrasive fluids in the inner circular area and the outer ring area of ​​the polishing platform.

Benefits of technology

By dividing the polishing platform into two independent areas and using different abrasive fluids, the dispersion of wafers is effectively improved, the better polishing effect is achieved, the planarization of the wafer surface is enhanced, and the performance and reliability of the integrated circuit are improved. sex.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118893570A_ABST
    Figure CN118893570A_ABST
Patent Text Reader

Abstract

The invention provides a CMP (chemical mechanical polishing) process polishing table, device and process method, the surface of the polishing table is divided into an inner area and an outer area which share a rotating shaft, the inner area and the outer area serve as polishing areas, different polishing characteristics are achieved, and a gap is formed between the two polishing areas. According to the invention, the polishing table is divided into two independent areas, and the polishing table has different polishing characteristics by adopting different grinding liquids, so that the dispersion of wafers can be effectively improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a CMP process polishing table, a device and a process method. Background Art

[0002] CMP (Chemical Mechanical Polishing) is a key process in semiconductor manufacturing to achieve global uniform planarization of wafers. The wafer manufacturing process mainly includes seven independent process flows: photolithography, etching, thin film growth, diffusion, ion implantation, chemical mechanical polishing, and metallization. As one of the key process technologies in wafer manufacturing, chemical mechanical polishing refers to the efficient removal of excess material on the wafer surface and global nano-level planarization through the synergistic effect of chemical corrosion and mechanical grinding.

[0003] Since integrated circuit components currently generally use multi-layer stereo wiring, the front-end process of integrated circuit manufacturing requires multi-layer cycles. In this process, the CMP process is needed to flatten the surface of the wafer. Simply put, if the chip manufacturing process is compared to building a high-rise building, each floor needs to be flat and even enough before another floor can be built on top of it, otherwise the floor will be uneven, affecting the overall performance and reliability. CMP is a key process technology that can effectively make the "floors" of integrated circuits reach nanometer-level global flatness.

[0004] Wafer spread is particularly important in the CMP process. To reduce this spread, various methods are being used, such as membrane zone control of the polishing head and pad conditioning tuning. However, it is still difficult to control the CMP amount in the outermost corner edge area of ​​the wafer. Summary of the invention

[0005] In view of the problems existing in the prior art, a CMP process polishing table, device and process method are provided, which control wafer spreading by using a new polishing table and selectively using more than two grinding liquids in specific areas.

[0006] The technical solution adopted by the present invention is as follows: a CMP process polishing table, the surface of which is divided into two areas, one inside and one outside, which share a common rotation axis, both serving as polishing areas to achieve different polishing characteristics, and a gap between the two polishing areas.

[0007] As a preferred solution, the polishing table is cylindrical as a whole.

[0008] As a preferred solution, the surface area of ​​the polishing table is divided into an inner circular area and an outer annular area, and the two areas are respectively sprayed with grinding liquids of different proportions.

[0009] As a preferred solution, the gap between the two polishing areas has a certain width for draining the grinding liquid.

[0010] The present invention also provides a CMP device, which uses the above-mentioned CMP process polishing table.

[0011] The present invention also proposes a process method based on the above CMP device, comprising:

[0012] Step 1: Place the wafer on the polishing head and rotate it in the same direction as the polishing table;

[0013] Step 2: In the outer annular area of ​​the polishing table, the grinding liquid is sprayed out to grind the wafer;

[0014] Step 3: When the wafer spread needs to be improved, use another abrasive slurry with a different ratio to perform fine grinding in the circular area inside the polishing table.

[0015] As a preferred solution, the grinding liquid used in step 2 or step 3 can be replaced by a chemical liquid having the same effect.

[0016] Compared with the prior art, the beneficial effects of adopting the above technical solution are as follows: the present invention divides the polishing table into two independent areas, adopts different grinding liquids to make it have different polishing characteristics, and can effectively improve the distribution of wafers. BRIEF DESCRIPTION OF THE DRAWINGS

[0017] Figure 1 This is a top view of the polishing table proposed by the present invention.

[0018] Figure 2 This is a side view of the polishing table proposed by the present invention.

[0019] Figure numerals: 1 - inner circular area, 2 - outer annular area, 3 - gap, 4 - grinding liquid. DETAILED DESCRIPTION

[0020] Embodiments of the present application are described in detail below, and examples of the embodiments are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar modules or modules with the same or similar functions. The embodiments described below with reference to the accompanying drawings are exemplary and are only used to explain the present application, and cannot be construed as limitations on the present application. On the contrary, the embodiments of the present application include all changes, modifications and equivalents that fall within the spirit and connotation of the appended claims.

[0021] like Figure 1 , Figure 2As shown, an embodiment of the present invention proposes a CMP process polishing table, wherein the surface of the polishing table is divided into two areas, one inside and one outside, which share a common rotation axis, both serving as polishing areas to achieve different polishing characteristics, and a gap 3 is provided between the two polishing areas.

[0022] Preferably, the polishing table is cylindrical in shape as a whole. The surface area of ​​the polishing table is divided into an inner circular area 1 and an outer annular area 2, and the two areas are respectively sprayed with grinding liquid 4 of different proportions.

[0023] Meanwhile, the gap 3 between the two polishing areas has a certain width.

[0024] When in use, the grinding liquid in the inner circular area is discharged through the gap, while the grinding liquid in the outer annular area is discharged from the outermost side due to centrifugal force. In addition, the gap between the two polishing areas can also prevent the grinding liquids in the two areas from mixing, so that the two polishing areas have different polishing characteristics.

[0025] The polishing table proposed in this embodiment can be used in a CMP device. Accordingly, this embodiment also proposes a process method for using the polishing table. The specific process is as follows:

[0026] Step 1: Place the wafer on the polishing head and rotate it in the same direction as the polishing table;

[0027] Step 2: In the outer annular area of ​​the polishing table, the grinding liquid is sprayed out to grind the wafer;

[0028] Step 3: When the wafer spread needs to be improved, use another abrasive slurry with a different ratio to perform fine grinding in the circular area inside the polishing table.

[0029] It should be noted that the grinding liquid used in step 2 or step 3 can be replaced by a chemical liquid having the same effect.

[0030] Example 1

[0031] This embodiment proposes a CMP process polishing table, wherein the surface of the polishing table is divided into two areas, an inner area and an outer area, which share a common rotation axis, both serving as polishing areas to achieve different polishing characteristics, and a gap is provided between the two polishing areas.

[0032] Example 2

[0033] On the basis of Example 1, the polishing table in this embodiment is cylindrical as a whole.

[0034] Example 3

[0035] On the basis of Example 2, the surface area of ​​the polishing table in this embodiment is divided into an inner circular area and an outer annular area, and the two areas are respectively sprayed with grinding liquids of different proportions.

[0036] Example 4

[0037] On the basis of Example 3, in this embodiment, the gap between the two polishing areas has a certain width for draining the grinding liquid.

[0038] Example 5

[0039] This embodiment also proposes a CMP device, which uses the CMP process polishing table described in any one of embodiments 1-4.

[0040] Example 6

[0041] This embodiment proposes a process method based on the CMP device described in Embodiment 5, including:

[0042] Step 1: Place the wafer on the polishing head and rotate it in the same direction as the polishing table;

[0043] Step 2: In the outer annular area of ​​the polishing table, the grinding liquid is sprayed out to grind the wafer;

[0044] Step 3: When the wafer spread needs to be improved, use another abrasive slurry with a different ratio to perform fine grinding in the circular area inside the polishing table.

[0045] Example 7

[0046] On the basis of Example 6, the grinding liquid used in step 2 or step 3 of this embodiment can be replaced by a chemical liquid having the same effect.

[0047] The present invention divides the polishing table into two independent areas, adopts different grinding liquids to make it have different polishing characteristics, and can effectively improve the distribution of wafers.

[0048] It should be noted that in the description of the embodiments of the present invention, unless otherwise clearly specified and limited, the terms "setting" and "connection" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances; the drawings in the embodiments are used to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings herein can be arranged and designed in various different configurations.

[0049] Although the embodiments of the present application have been shown and described above, it can be understood that the above embodiments are exemplary and cannot be understood as limitations on the present application. Ordinary technicians in this field can change, modify, replace and modify the above embodiments within the scope of the present application.

Claims

1. A CMP process polishing table, characterized in that: The surface of the polishing table is divided into two areas, one inside and one outside, which share a common rotation axis, both serving as polishing areas to achieve different polishing characteristics, with a gap between the two polishing areas.

2. The CMP process polishing table according to claim 1, characterized in that: The polishing table is cylindrical in shape as a whole.

3. The CMP process polishing table according to claim 1 or 2, characterized in that: The surface area of ​​the polishing table is divided into an inner circular area and an outer annular area, and the two areas are respectively sprayed with grinding liquids of different proportions.

4. The CMP process polishing table according to claim 1, characterized in that: The gap between the two polishing areas has a certain width for draining the grinding liquid.

5. A CMP device, characterized in that: A CMP process polishing table using any one of claims 1-4.

6. A process method based on the CMP device according to claim 5, characterized in that: include: Step 1: Place the wafer on the polishing head and rotate it in the same direction as the polishing table; Step 2: In the outer annular area of ​​the polishing table, the grinding liquid is sprayed out to grind the wafer; Step 3: When the wafer spread needs to be improved, use another abrasive slurry with a different ratio to perform fine grinding in the circular area inside the polishing table.

7. The process according to claim 6, characterized in that: The grinding liquid used in step 2 or step 3 can be replaced by a chemical liquid having the same effect.