Structure and process for improving heat dissipation efficiency of laser working substance

By installing a gold-plated layer on the connection surface between the laser working substance and the metal matrix and filling it with gold-tin alloy foil to form a welding connection, the problems of unstable heat dissipation performance and low production efficiency of the laser working substance are solved, and efficient heat conduction and connection are achieved reliability.

CN118905494APending Publication Date: 2024-11-08LUOYANG DINGYANG PHOTOELECTRIC TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411000762.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-08

AI Technical Summary

Technical Problem

The heat dissipation performance in the existing laser working substance installation process is unstable and the production efficiency is low, resulting in the accumulation of heat of the working substance during work, affecting the product's energy efficiency and quality.

Method used

A gold-plated layer is provided on the connecting surface between the working substance and the metal matrix, and a welding connection is achieved by filling the gold-tin alloy foil to form a gold-tin alloy layer to improve heat transfer performance.

Benefits of technology

Through the heat transfer performance of gold-tin alloy, heat in working substances can be quickly transmitted, heat accumulation is avoided, connection tightness and heat transfer performance are enhanced, and filling consistency and high efficiency are ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118905494A_ABST
    Figure CN118905494A_ABST
Patent Text Reader

Abstract

The invention discloses a structure and a process for improving the heat dissipation efficiency of a laser working substance, the structure comprises the working substance and a metal matrix for supporting the working substance, and gold-plated layers with the thickness of 20-50 microns are arranged on the mutually connected surfaces of the working substance and the matrix. And a gold-tin alloy layer for welding and connecting the two gold-plated layers is arranged between the gold-plated layers. The process comprises the following steps of: 1, arranging a gold-plated layer on a mutually connected surface of a working substance and a metal matrix for supporting the working substance; and 2, filling alloy foil between the working substance and the matrix, so that the gold-plated layer is tightly attached to the alloy foil. And thirdly, the working substance and the base body which are obtained in the second step and tightly attached to each other are heated so that the alloy foil can form an alloy layer connected with the gold-plated layer in a welded mode. And 4, cooling to room temperature after heating. According to the invention, the technical problems of unstable heat dissipation performance and low production efficiency of the existing laser working substance installation process can be solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of laser equipment, in particular to a structure and a process for improving the heat dissipation efficiency of laser working materials. Background Art

[0002] The working material plays the role of an energy transfer bridge in laser measurement products. The light emitted by the light source resonates in the working material and outputs laser light. During this process, a large amount of heat will be generated in the working material. If the generated heat cannot be conducted away in time, the working material will be deformed or even broken, thus affecting the energy efficiency and quality of the product.

[0003] The existing process generally involves bonding the working material to the metal substrate, and applying as little glue as possible during the bonding process to maximize the contact area between the working material and the metal substrate. This method requires high operator literacy and has uncertainties. It can neither fundamentally solve the problem of heat accumulation of the working material during operation nor reduce production efficiency. Summary of the invention

[0004] The purpose of the present invention is to provide a structure and process for improving the heat dissipation efficiency of laser working materials, which can solve the technical problems of unstable heat dissipation performance and low production efficiency of existing laser working material installation processes.

[0005] In order to achieve the above object, the present invention adopts the following technical solution.

[0006] A structure for improving the heat dissipation efficiency of laser working material, comprising a working material 1 and a metal substrate 2 for supporting the working material 1, wherein the working material 1 and the substrate 2 are both provided with gold-plated layers on the surfaces connected to each other, and an alloy layer 3 for welding the two gold-plated layers is provided between the gold-plated layers.

[0007] Furthermore, the thickness of the gold-plated layer is 20 micrometers to 50 micrometers.

[0008] Furthermore, the alloy layer 3 is a gold-tin alloy layer 3 .

[0009] A process for improving the heat dissipation efficiency of laser working material includes the following steps.

[0010] Step 1: a gold-plated layer is provided on the interconnected surfaces of the working substance 1 and the metal substrate 2 for supporting the working substance 1.

[0011] Step 2: Fill the alloy foil between the working substance 1 and the substrate 2, and then use a clamp to press the working substance 1 onto the metal substrate 2 so that the gold-plated layer fits tightly with the alloy foil.

[0012] Step 3: heating the closely fitted working material 1 and substrate 2 obtained in step 2, so that the alloy foil forms an alloy layer 3 which is welded to the gold-plated layer.

[0013] Step 4: After heating is completed, wait until the temperature drops to room temperature and remove the fixture, and the process steps are completed.

[0014] Furthermore, in step one, the thickness of the gold-plated layer is set to be 20 microns to 50 microns.

[0015] Furthermore, in step 2, the alloy foil is gold-tin foil.

[0016] Furthermore, the temperature rise rate during heating is 100 degrees Celsius per minute, and after heating to 420 degrees Celsius, the temperature is kept for 3 minutes.

[0017] Furthermore, in step three, a resistance wire heating furnace is used for heating.

[0018] After adopting the above technical solution, the present invention has the following beneficial effects: 1. The present invention uses a gold-tin alloy to fill the gap between the working substance and the substrate, and utilizes the excellent heat transfer performance of the gold-tin alloy to quickly conduct the heat generated in the working substance to the metal substrate, thereby preventing the heat from accumulating in the working substance and causing damage to the working substance; 2. The present invention provides a gold-plated layer at the part where the working substance and the substrate contact each other, and uses the gold-plated layer and the gold-tin alloy foil to achieve welding connection, further increasing the tightness of the connection, maintaining a reliable connection, and enhancing the heat transfer performance; 3. Use gold-tin foil to fill and heat to achieve welding, and use the stable thickness of gold-tin foil to ensure the consistency of filling, stable quality, and high efficiency. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] Figure 1 It is a schematic diagram of the overall state of the laser working material and the metal matrix in the present invention.

[0020] Figure 2 yes Figure 1 Schematic diagram of the main view of the state shown.

[0021] Figure 3 yes Figure 2 Schematic diagram of the cross-section state at AA in the middle.

[0022] Figure 4 yes Figure 3 Schematic diagram of the connection structure at B in the figure.

[0023] Description of the drawings: 1. working material, 11. first gold-plated layer, 2. substrate, 21. second gold-plated layer, 3. alloy layer. DETAILED DESCRIPTION

[0024] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the following is a further detailed description of the features and performance of a structure and process for improving the heat dissipation efficiency of laser working materials in the present invention in conjunction with the accompanying drawings and embodiments.

[0025] Embodiment 1 Please see attached Figures 1 to 4 A structure for improving the heat dissipation efficiency of laser working material, including a working material 1 and a metal substrate 2 for supporting the working material 1, the working material 1 and the substrate 2 are both provided with a gold-plated layer on the surfaces connected to each other, and an alloy layer 3 for welding the two gold-plated layers is provided between the gold-plated layers, and the alloy layer 3 is a gold-tin alloy layer.

[0026] In particular, the thickness of the gold-plated layer is 20 microns to 50 microns. Preferably, the thickness of the gold-plated layer in this embodiment is 20 microns.

[0027] A process for improving the heat dissipation efficiency of laser working material includes the following steps.

[0028] Step 1: a gold-plated layer is provided on the interconnected surfaces of the working substance 1 and the metal substrate 2 for supporting the working substance 1, wherein the thickness of the gold-plated layer is 20 microns.

[0029] Step 2: Fill alloy foil between the working substance 1 and the substrate 2, and then use a clamp to press the working substance 1 onto the metal substrate 2 so that the gold-plated layer fits tightly with the alloy foil. The alloy foil used is gold-tin foil.

[0030] Step 3: Heat the tightly fitted working material 1 and substrate 2 obtained in step 2 to form an alloy layer 3 welded to the gold-plated layer. The temperature rise rate during heating is 100 degrees Celsius / minute. After heating to 420 degrees Celsius, keep warm for 3 minutes. A resistance wire heating furnace is used for heating.

[0031] Step 4: After heating is completed, wait until the temperature drops to room temperature and remove the fixture, and the process steps are completed.

[0032] In the specific implementation, the surfaces where the working material 1 and the substrate 2 contact each other are first gold-plated. The thickness of the gold-plated layer is controlled to be 20 microns. A first gold-plated layer 11 is formed on the working material 1, and a second gold-plated layer 21 is formed on the substrate 2.

[0033] Gold foil is laid between the first gold-plated layer 11 and the second gold-plated layer 21 to ensure that the thickness is consistent everywhere, and a special clamp is used to clamp the working material 1 and the substrate 2 so that the first gold-plated layer 11 and the second gold-plated layer 21 press the gold foil.

[0034] The clamped working substance 1 and the substrate 2 are placed in a resistance wire heating furnace for heating. The temperature rise rate of the resistance wire heating furnace is controlled to be 100 degrees Celsius per minute, and the temperature is kept at 420 degrees Celsius for 3 minutes. During the heating process, the gold foil will be welded to the first gold-plated layer 11 and the second gold-plated layer 21 under high temperature to form an alloy layer 3.

[0035] After heating is completed, cool naturally. After cooling to room temperature, remove the clamp and the process steps are completed.

[0036] Embodiment 2 Different from the first embodiment, in the second embodiment, the thickness of the gold-plated layer is 50 microns. A thicker gold-plated layer can achieve a better welding effect during the heating process to weld the gold foil and the gold-plated layer.

[0037] It should be noted that the parts not described in detail in this scheme are all prior art, and the above embodiments are only used to illustrate the present invention, but the present invention is not limited to the above embodiments. Any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention fall within the protection scope of the present invention.

Claims

1. A structure for improving the heat dissipation efficiency of a laser working substance, comprising a working substance (1) and a metal substrate (2) for supporting the working substance (1). Features: The working substance (1) and the substrate (2) are both provided with gold-plated layers on the surfaces connected to each other, and an alloy layer (3) for welding the two gold-plated layers is provided between the gold-plated layers.

2. A structure for improving the heat dissipation efficiency of laser working material as claimed in claim 1, Features: The thickness of the gold-plated layer is 20 microns to 50 microns.

3. A structure for improving the heat dissipation efficiency of laser working material as claimed in claim 1, Features: The alloy layer (3) is a gold-tin alloy layer.

4. A process for improving the heat dissipation efficiency of laser working materials, Features: The following steps are included: Step 1: a gold-plated layer is provided on the interconnected surfaces of the working substance (1) and the metal substrate (2) for supporting the working substance (1); Step 2: Fill the alloy foil between the working substance (1) and the substrate (2), and then use a clamp to press the working substance (1) onto the metal substrate (2) so that the gold-plated layer fits tightly with the alloy foil. Step 3: heating the closely fitted working material (1) and substrate (2) obtained in step 2, so that the alloy foil forms an alloy layer (3) which is welded to the gold-plated layer. Step 4: After heating is completed, wait until the temperature drops to room temperature and remove the fixture, and the process steps are completed.

5. A process for improving the heat dissipation efficiency of laser working material as claimed in claim 4, Features: In step 1, the thickness of the gold-plated layer is set to 20 microns to 50 microns.

6. A process for improving the heat dissipation efficiency of laser working material as claimed in claim 4, Features: In step 2, the alloy foil is gold-tin foil.

7. A process for improving the heat dissipation efficiency of laser working material as claimed in claim 6, Features: The temperature rise rate during heating is 100 degrees Celsius per minute, and after heating to 420 degrees Celsius, it is kept warm for 3 minutes.