Transparent electromagnetic shielding anti-friction composite film and preparation method thereof
By combining the transparent electromagnetic shielding film with the friction-resistant film, special structural design and process methods are adopted to solve the problem of insufficient friction-resistant characteristics in the existing technology, and the transparency of high transmittance, strong electromagnetic shielding and high wear resistance is achieved. Electromagnetic shielding anti-friction composite film meets application needs in many fields.
Patent Information
- Application Number
- CN202410979139.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-22
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
When existing transparent electromagnetic shielding films take into account high transmittance and strong electromagnetic shielding effects, their anti-friction characteristics cannot meet the needs of modern optoelectronic instruments.
By combining the transparent electromagnetic shielding film with the friction-resistant film, special structural design and process methods are adopted, including ion cleaning pretreatment, thin film deposition connecting layer, transparent electromagnetic shielding layer, urgency film layer and friction-resistant layer deposition, using different parameters and auxiliary technology to form a transparent electromagnetic shielding anti-friction composite film.
It realizes the high transmittance, strong electromagnetic shielding effect and high wear resistance of transparent electromagnetic shielding film, and meets the application needs of communication equipment, medical equipment, aerospace and other fields.
Smart Images

Figure CN118910552A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of optical film preparation, and in particular to a transparent electromagnetic shielding anti-friction composite film and a preparation method thereof. Background Art
[0002] Transparent electromagnetic shielding films have strong application demands in many fields such as communication equipment, medical equipment, instrumentation, aerospace, weapons and equipment, such as optoelectronic guided missiles, laser guided missiles and fighter cockpits, and have attracted widespread attention. As the use environment becomes more and more demanding and the system performance index requirements become higher and higher, while taking into account high transmittance and strong shielding effect, higher requirements are also put forward for anti-friction. Even the representative ones such as indium tin oxide (ITO) and ultra-thin metal films can take into account both visible high transmittance and strong electromagnetic shielding effect, but the current anti-friction properties still cannot meet the use requirements and cannot meet the needs of modern optoelectronic instruments. Therefore, it is of great significance to invent a transparent electromagnetic shielding anti-friction composite film. Summary of the invention
[0003] Therefore, in order to overcome the shortcomings of the above-mentioned prior art, the present invention provides a transparent electromagnetic shielding anti-friction composite film and a preparation method thereof which combines a transparent electromagnetic shielding film with a friction-resistant film through a special structural design to achieve transparent electromagnetic shielding and friction-resistant multifunctional properties.
[0004] In order to achieve the above object, the present invention provides a method for preparing a transparent electromagnetic shielding anti-friction composite film, comprising: placing a sample substrate on a sample rack of a coating machine and evacuating the sample, baking the sample substrate at a first predetermined temperature for a first time, and when the vacuum degree reaches 5.0×10 -4 Pa, turn on the radio frequency ion source to perform ion cleaning pretreatment on the sample substrate; after cleaning, wait until the vacuum degree stabilizes at 3.0×10 -4 Pa, the first parameter is used to deposit the connection layer of the thin film, and the first auxiliary parameter is used for ion beam assisted deposition; the second parameter is used to deposit the transparent electromagnetic shielding layer of the thin film, and the ion beam assisted deposition process is not used for this layer; the third parameter is used to deposit the first layer of the anti-reflection film layer of the thin film, and the ion beam assisted deposition process is not used for this layer; the fourth parameter is used to deposit the remaining number of layers of the anti-reflection film layer of the thin film, and the fourth auxiliary parameter is used for ion beam assisted deposition; after the deposition of the anti-reflection film layer is completed, wait for the vacuum degree to return to 3.0×10 -4 Pa, the friction-resistant layer is deposited by resistance evaporation, and this layer does not use ion beam assisted deposition process; then the vacuuming and heating are stopped, and natural cooling begins. When it drops to room temperature, a transparent electromagnetic shielding and anti-friction composite film is obtained.
[0005] In one embodiment, the working conditions of the ion cleaning pretreatment are: the RF ion source parameter voltage is 1100V, the current is 1000mA, and the cleaning time is 5-10 minutes.
[0006] In one embodiment, the connecting layer is a SiO2 film layer or an Al2O3 film layer, the transparent electromagnetic shielding layer is an indium tin oxide film layer, an ultra-thin Al-Ag film layer or an ultra-thin Cu-Ag film layer, the high refractive index film layer is a TiO2 film layer or a Ti3O5 film layer, the low refractive index film layer is a SiO2 film layer or a MgF2 film layer, and the friction-resistant layer is an AS coating.
[0007] In one of the embodiments, the first parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s, and the first auxiliary parameter is a voltage of 1000 V to 1100 V and a current of 900 mA to 950 mA.
[0008] In one embodiment, the second parameter is to deposit the thin film at a rate of 0.5 nm / s to 0.6 nm / s.
[0009] In one embodiment, the third parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s.
[0010] In one embodiment, the anti-reflection film layer is composed of a high refractive index film layer and a low refractive index film layer, and the fourth parameter includes a fifth parameter for depositing the high refractive index film layer and a sixth parameter for depositing the low refractive index film layer.
[0011] In one embodiment, the fifth parameter is to deposit the thin film at a rate of 0.4nm / s to 0.5nm / s, the fifth auxiliary parameter is a voltage of 1050V to 1100V and a current of 1000mA to 1050mA, and the sixth parameter is to deposit the thin film at a rate of 0.8nm / s to 0.9nm / s, and the sixth auxiliary parameter is a voltage of 1000V to 1100V and a current of 900mA to 950mA.
[0012] In one of the embodiments, the working parameter of the resistance evaporation is to deposit the friction-resistant layer at a rate of 1.0 to 1.5 nm / s.
[0013] A transparent electromagnetic shielding anti-friction composite film is prepared by adopting the above method.
[0014] Compared with the prior art, the advantages of the present invention are: the transparent electromagnetic shielding film and the friction-resistant film are combined through the film system design, so that it can take into account the visible high transmittance and strong electromagnetic shielding effect and high wear resistance at the same time, and realize the transparent electromagnetic shielding and friction-resistant multifunctional characteristics, thereby meeting the strong application needs in many fields such as communication equipment, medical equipment, instrumentation, aerospace, and weapon equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] In order to more clearly illustrate the technical solutions of the embodiments of the present application, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0016] Figure 1 is a schematic structural diagram of a transparent electromagnetic shielding anti-friction composite film in an embodiment of the present invention;
[0017] Figure 2 The invention relates to a method for preparing a transparent electromagnetic shielding anti-friction composite film in an embodiment of the present invention;
[0018] Figure 3 is a theoretically designed visible light range spectral transmittance curve in one embodiment of the present invention;
[0019] Figure 4 This is a spectral transmittance curve in the visible light range actually prepared in one embodiment of the present invention. DETAILED DESCRIPTION
[0020] The embodiments of the present application are described in detail below with reference to the accompanying drawings.
[0021] The following describes the implementation methods of the present application through specific examples, and those skilled in the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification. Obviously, the described embodiments are only a part of the embodiments of the present application, rather than all the embodiments. The present application can also be implemented or applied through other different specific implementation methods, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present application. It should be noted that, in the absence of conflict, the following embodiments and the features in the embodiments can be combined with each other. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work belong to the scope of protection of the present application.
[0022] It should be noted that various aspects of the embodiments within the scope of protection of the present invention are described below. It should be apparent that the aspects described herein can be embodied in a wide variety of forms, and any specific structure and / or function described herein is merely illustrative. Based on the present application, it should be understood by those skilled in the art that an aspect described herein can be implemented independently of any other aspect, and two or more of these aspects can be combined in various ways. For example, any number and aspect described herein can be used to implement the device and / or practice the method. In addition, other structures and / or functionalities other than one or more of the aspects described herein can be used to implement this device and / or practice this method.
[0023] It should also be noted that the illustrations provided in the following embodiments are only schematic illustrations of the basic concept of the present application. The drawings only show components related to the present application rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0024] Additionally, in the following description, specific details are provided to facilitate a thorough understanding of the examples. However, it will be understood by those skilled in the art that the aspects described may be practiced without these specific details.
[0025] The present application embodiment provides a transparent electromagnetic shielding anti-friction composite film, such as Figure 1 As shown, the transparent electromagnetic shielding and anti-friction composite film 100 includes a substrate 10 connected in sequence, a connecting layer 20 connected to the substrate, a transparent electromagnetic shielding layer 30, an anti-reflection film layer 40 and an anti-friction layer 50.
[0026] The substrate 10 is used to carry the film (i.e., prepare the film on its surface), and the substrate can be at least one of K9 glass substrate, JGS1 quartz substrate, JGS2 quartz substrate, JGS3 quartz substrate, Al2O3 sapphire substrate, ULE substrate, PET substrate and other visible transparent substrates.
[0027] The connecting layer 20 is used to improve the adhesion between the transparent electromagnetic shielding layer and the substrate and enhance the reliability of the film layer. The connecting layer can be a SiO2 film layer or an Al2O3 film layer. The connecting layer 20 is deposited on the substrate 10 using a thin film deposition method, and the thin film deposition method can be a chemical deposition method or a physical deposition method.
[0028] The transparent electromagnetic shielding layer 30 is used to shield visible light from passing electromagnetic waves. The transparent electromagnetic shielding layer can be an indium tin oxide (ITO) film layer, an ultra-thin Al-Ag film layer, or an ultra-thin Cu-Ag film layer. The transparent electromagnetic shielding layer 30 is deposited on the connecting layer 20 by a thin film deposition method, and the thin film deposition method can be a chemical deposition method or a physical deposition method.
[0029] The anti-reflection film 40 is used to cooperate with the composite substrate composed of the substrate, the connecting layer and the transparent electromagnetic shielding layer to improve the visible light transmittance. In one embodiment, the anti-reflection film layer 40 is composed of a high refractive index film layer 41 and a low refractive index film layer 42. The high refractive index film layer is a TiO2 film layer or a Ti3O5 film layer, and the low refractive index film layer is a SiO2 film layer or a MgF2 film layer. The high refractive index film layer 41 and the low refractive index film layer 42 can be arranged alternately in multiple layers or in single layers. The anti-reflection film 40 is deposited on the transparent electromagnetic shielding layer 30 by a thin film deposition method, and the thin film deposition method can be a chemical deposition method or a physical deposition method.
[0030] The friction-resistant layer 50 is used to improve the friction-resistant property of the film layer. The friction-resistant layer can be AS coating. AS coating mainly deposits organic fluoride materials on the substrate to make the substrate surface waterproof, oil-proof, scratch-proof, anti-fingerprint, anti-pollution and easy to clean.
[0031] The thickness of each film layer can be obtained by combining the characteristic matrix formula of the film with computer-aided film system design.
[0032] like Figure 2 As shown, the preparation method of the transparent electromagnetic shielding anti-friction composite film comprises the following steps:
[0033] Step S1, placing the sample substrate on the sample rack of the coating machine and evacuating the sample, baking it at a first predetermined temperature for a first time, and when the vacuum degree reaches 5.0×10 -4 When ρ = 0.05 Pa, the radio frequency ion source is turned on to perform ion cleaning pretreatment on the sample substrate.
[0034] The sample substrate is clean and can be cleaned and removed from the surface of the substrate using ultrasonic cleaning technology. The sample substrate is placed on the sample rack of the coating machine, and the sample rack of the coating machine with the sample substrate is placed in a vacuum chamber for evacuation. The sample substrate is baked at a first predetermined temperature for a first time to ensure that the sample substrate is fully and evenly heated, increase the energy of the deposited particles on its surface, and increase the adhesion effect between the film layer and the substrate. The first predetermined temperature is 80°C to 90°C. The first time is 20min to 30min.
[0035] The radio frequency ion source can remove residual pollutants on the surface of the sample substrate, improve surface activity, and enhance the adhesion between the film layer and the substrate. -4 Pa, the radio frequency ion source is turned on to perform ion cleaning pretreatment on the sample substrate. The vacuum degree is 5.0×10 -4Pa can ensure that there are few residual impurity gases in the vacuum chamber and improve the purity of the ion beam produced by the ion source. The vacuum is pumped from the beginning of the ion cleaning pretreatment to the end of the AS deposition in the last step S6, during which the vacuum is always maintained.
[0036] Step S2: After cleaning, wait until the vacuum degree stabilizes at 3.0×10 -4 Pa, the first parameter is used to perform thin film deposition of the connection layer, and the first auxiliary parameter is used to perform ion beam assisted deposition.
[0037] Step S3, using the second parameters to perform thin film deposition of a transparent electromagnetic shielding layer, and this layer does not use an ion beam assisted deposition process.
[0038] Since the ion beam will have a certain impact on the electromagnetic shielding effect of the transparent electromagnetic shielding layer, the ion beam assisted deposition process cannot be used in this step.
[0039] Step S4, using the third parameter to perform thin film deposition on the first layer of the anti-reflection film, and this layer does not use the ion beam assisted deposition process.
[0040] Since the ion beam will cause etching and oxidation to the transparent electromagnetic shielding layer, affecting the microstructure and stoichiometric ratio of the electromagnetic shielding film, thereby causing the electromagnetic shielding effect to deteriorate, the ion beam assisted deposition process cannot be used in this step.
[0041] Step S5, using the fourth parameter to perform thin film deposition of the remaining number of anti-reflection film layers, and using the fourth auxiliary parameter to perform ion beam assisted deposition.
[0042] The anti-reflection film layer can be an anti-reflection film layer formed of different components.
[0043] Step S6, after the deposition of the anti-reflection film layer is completed and the vacuum degree is restored to 3.0×10-4Pa, the friction-resistant layer is deposited by resistance evaporation, and this layer does not use ion beam assisted deposition process; then stop vacuuming and heating, start natural cooling, and when it drops to room temperature, a transparent electromagnetic shielding anti-friction composite film is obtained.
[0044] There are two reasons for the change in vacuum degree: (1) When evaporating the anti-reflection film, the electron beam heats the coating material, and the coating material will release gas; (2) During the anti-reflection film coating process, the ion-assisted process is used, and the reaction gas will also cause the vacuum degree to change. Therefore, after the anti-reflection film layer is deposited, the vacuum degree will be restored to 3.0×10-4Pa, and the friction-resistant layer will be deposited by resistance evaporation; then the vacuum pumping and heating are stopped, and the temperature begins to drop naturally. When it drops to room temperature, a transparent electromagnetic shielding and anti-friction composite film is obtained.
[0045] The above method combines the transparent electromagnetic shielding film with the friction-resistant film through film system design, so that it can take into account the visible high transmittance, strong electromagnetic shielding effect and high wear resistance at the same time, and realize the transparent electromagnetic shielding and friction-resistant multifunctional characteristics, thereby meeting the strong application needs in many fields such as communication equipment, medical equipment, instrumentation, aerospace, and weapons and equipment.
[0046] In one embodiment, the working conditions of the ion cleaning pretreatment are as follows: the RF ion source parameter voltage is 1100V, the current is 1000mA, and the cleaning time is 5-10 minutes.
[0047] In one embodiment, the first parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s, and the first auxiliary parameter is a voltage of 1000 V to 1100 V and a current of 900 mA to 950 mA.
[0048] In one embodiment, the second parameter is to deposit the thin film at a rate of 0.5 nm / s to 0.6 nm / s.
[0049] In one embodiment, the third parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s.
[0050] In one embodiment, the anti-reflection film layer is composed of a high refractive index film layer and a low refractive index film layer, and the fourth parameter includes a fifth parameter for depositing the high refractive index film layer and a sixth parameter for depositing the low refractive index film layer.
[0051] In one embodiment, the fifth parameter is to deposit the thin film at a rate of 0.4nm / s to 0.5nm / s, the fifth auxiliary parameter is a voltage of 1050V to 1100V and a current of 1000mA to 1050mA, and the sixth parameter is to deposit the thin film at a rate of 0.8nm / s to 0.9nm / s, and the sixth auxiliary parameter is a voltage of 1000V to 1100V and a current of 900mA to 950mA.
[0052] In one embodiment, the working parameter of the resistance evaporation is to deposit the friction-resistant layer at a rate of 1.0-1.5 nm / s.
[0053] In some embodiments, since SiO2 material can be used as both the material of the connecting layer and the raw material of the low refractive index film layer in the anti-reflection film layer, different layers of SiO2 film layers may exist in the film system structure. When manufacturing this type of transparent electromagnetic shielding and anti-friction composite film, the same component SiO2 film layers may be deposited at the same speed or at different speeds.
[0054] Embodiment 1
[0055] A 1300 type vacuum coating machine is used, which is equipped with dual electron guns, two sets of anti-evaporation systems, RF17cm radio frequency ion source, six-probe quartz crystal monitoring system and low temperature pump + dry pump oil-free exhaust system.
[0056] The transparent electromagnetic shielding and anti-friction composite film was prepared on a JGS1 substrate with a diameter of 30 mm and a thickness of 2 mm using an electron beam thermal evaporation deposition system. Figure 3 As shown, the transmittance spectrum of the theoretically designed film system in the visible light range has high transmittance at wavelengths of 415nm to 750nm.
[0057] The connecting layer is a SiO2 film layer. The transparent electromagnetic shielding layer is an ITO film layer. The anti-reflection film layer is composed of a high refractive index film layer 41 and a low refractive index film layer 42; the high refractive index film layer is a TiO2 film layer, and the low refractive index film layer is a SiO2 film layer. The anti-friction layer is an AS film layer.
[0058] According to the characteristic matrix formula of the film combined with computer-aided calculation, the specific parameters of the film structure are:
[0059]
[0060] The specific preparation process of the transparent electromagnetic shielding anti-friction composite film is:
[0061] 1) Use ultrasonic cleaning technology to clean the JGS1 substrate and remove pollutants on the substrate surface;
[0062] 2) Place the cleaned sample on the sample rack of the coating machine, evacuate the vacuum chamber, and bake at 80°C. When the vacuum degree reaches 5.0×10 -4 When Pa, turn on the radio frequency ion source to perform ion cleaning pretreatment on the sample. The radio frequency ion source parameter voltage is 1100V, current is 1000mA, and cleaning takes 5-10 minutes.
[0063] 3) After cleaning, wait until the vacuum degree stabilizes at 3.0×10 -4 Pa, thin film deposition began, and a 15nm thick SiO2 film was deposited as a connecting layer at a rate of 0.8nm / s. The ion beam assisted deposition parameters were voltage 1000V and current 900mA.
[0064] 4) Depositing a 30 nm thick ITO film layer at a rate of 0.5 nm / s; this layer does not use ion beam assisted deposition process;
[0065] 5) Depositing a 26.25 nm thick SiO2 film at a rate of 0.8 nm / s, without using an ion beam assisted deposition process;
[0066] 6) The fourth to ninth layers are deposited alternately in sequence, and the deposition thickness is shown in the above table. The deposition rate of TiO2 is 0.4 nm / s, and the ion beam assisted deposition parameters are voltage 1050 V and current 1000 mA; the deposition rate of SiO2 is 0.8 nm / s, and the ion beam assisted deposition parameters are voltage 1000 V and current 900 mA;
[0067] 7) After the ninth layer is deposited, wait until the vacuum degree returns to 3.0×10 -4 When the temperature is 2000 Pa, a 10 nm AS film is deposited at a rate of 1.0-1.5 nm / s by resistance evaporation, and the ion beam assisted deposition process is not used for this layer. Then the vacuum and heating are stopped, and the temperature is naturally cooled down. When the temperature drops to room temperature, the sample is taken out.
[0068] The transmittance of the transparent electromagnetic shielding anti-friction composite film in the visible light range was measured by UV-visible-near infrared spectrophotometer. Figure 4 As shown, the average transmittance is about 95.7%.
[0069] The electromagnetic shielding tester was used to measure the electromagnetic shielding of the transparent electromagnetic shielding anti-friction composite film in the frequency band of 20MHz to 5GHz, and the average electromagnetic shielding was 18dB.
[0070] The prepared transparent electromagnetic shielding anti-friction composite film was subjected to a friction test, using steel wool to rub the film surface 50 times per minute, setting the load pressure to 5N, and rubbing a total of 8000 times. The optical contact angle meter was used to detect the change of the sample water drop angle by 1.8° before and after friction, indicating that the transparent electromagnetic shielding anti-friction composite film has strong friction resistance.
[0071] Therefore, the super composite film can simultaneously meet the requirements of high transmittance, strong electromagnetic shielding and friction resistance.
[0072] The above is only a specific implementation of the present application, but the protection scope of the present application is not limited thereto. Any changes or substitutions that can be easily conceived by any technician familiar with the technical field within the technical scope disclosed in the present application should be included in the protection scope of the present application.
Claims
1. A method for preparing a transparent electromagnetic shielding anti-friction composite film, characterized in that: include: The sample substrate is placed on the sample rack of the coating machine and evacuated, and baked at the first predetermined temperature for the first time. When the vacuum degree reaches 5.0×10 -4 Pa, turn on the radio frequency ion source to perform ion cleaning pretreatment on the sample substrate; After cleaning, wait until the vacuum degree stabilizes at 3.0×10 -4 Pa, the first parameter is used to deposit the connecting layer of the thin film, and the first auxiliary parameter is used to perform ion beam assisted deposition; The transparent electromagnetic shielding layer is deposited in a thin film by using the second parameter, and the ion beam assisted deposition process is not used for this layer; The first layer of the antireflection film is deposited by using the third parameter, and the ion beam assisted deposition process is not used for this layer; Using the fourth parameter to deposit the remaining number of anti-reflection film layers, and using the fourth auxiliary parameter to perform ion beam assisted deposition; After the deposition of the antireflection film is completed, the vacuum degree is restored to 3.0×10 -4 Pa, the friction-resistant layer is deposited by resistance evaporation, and this layer does not use ion beam assisted deposition process; then the vacuuming and heating are stopped, and natural cooling begins. When it drops to room temperature, a transparent electromagnetic shielding and anti-friction composite film is obtained.
2. The preparation method according to claim 1, characterized in that: The working conditions of the ion cleaning pretreatment are as follows: the RF ion source parameter voltage is 1100V, the current is 1000mA, and the cleaning time is 5-10 minutes.
3. The preparation method according to claim 1, characterized in that: The connecting layer is a SiO2 film layer or an Al2O3 film layer; the transparent electromagnetic shielding layer is an indium tin oxide film layer, an ultra-thin Al-Ag film layer or an ultra-thin Cu-Ag film layer; the anti-reflection film layer is composed of a high refractive index film layer and a low refractive index film layer, the high refractive index film layer is a TiO2 film layer or a Ti3O5 film layer, and the low refractive index film layer is a SiO2 film layer or a MgF2 film layer; the friction-resistant layer is an AS coating.
4. The preparation method according to claim 1, characterized in that: The first parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s, and the first auxiliary parameter is a voltage of 1000 V to 1100 V and a current of 900 mA to 950 mA.
5. The preparation method according to claim 1, characterized in that: The second parameter is to deposit the thin film at a rate of 0.5 nm / s to 0.6 nm / s.
6. The preparation method according to claim 1, characterized in that: The third parameter is to deposit the thin film at a rate of 0.8 nm / s to 0.9 nm / s.
7. The preparation method according to claim 1, characterized in that: The anti-reflection film layer is composed of a high refractive index film layer and a low refractive index film layer, and the fourth parameter includes a fifth parameter for depositing the high refractive index film layer and a sixth parameter for depositing the low refractive index film layer.
8. The preparation method according to claim 7, characterized in that: The fifth parameter is to deposit the thin film at a rate of 0.4nm / s to 0.5nm / s, the fifth auxiliary parameter is a voltage of 1050V to 1100V and a current of 1000mA to 1050mA, and the sixth parameter is to deposit the thin film at a rate of 0.8nm / s to 0.9nm / s, and the sixth auxiliary parameter is a voltage of 1000V to 1100V and a current of 900mA to 950mA.
9. The preparation method according to claim 1, characterized in that: The working parameter of the resistance evaporation is to deposit the friction-resistant layer at a rate of 1.0 to 1.5 nm / s.
10. A transparent electromagnetic shielding anti-friction composite film, characterized in that: The transparent electromagnetic shielding and anti-friction composite film is prepared by the method described in any one of claims 1 to 9.
Citation Information
Patent Citations
Large-size sapphire substrate multi-spectral hard antireflection film and preparation method thereof
CN109182972A
Sapphire optical window with electromagnetic shielding function and preparation method
CN110519976A
Ultra-wideband transparent electromagnetic protection material structure and preparation method thereof
CN113068387A
Aperture for electromagnetic radiation, method for aligning an aperture, system for applying electromagnetic radiation onto a source material and dispersing element
US20240047092A1