Reduction rotary kiln for refining tungsten-molybdenum powder
By designing a spiral guide groove and slope structure in the rotary kiln, combining hydrogen and nitrogen mixture streams, the problem of liquefaction and adhesion of powdered materials at high temperatures is solved, and the stable reduction of materials and high output rate is achieved.
Patent Information
- Application Number
- CN202411199888.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-11-08
AI Technical Summary
In a rotary kiln, powdered materials tend to liquefy at high temperatures and stick to the inner wall of the kiln body, resulting in kiln body loss and unstable production.
A reduction rotary kiln for tungsten-molybdenum powder refining is designed, with spiral guide grooves and guide blocks inside, and the powder material is guided through spiral guide grooves and slope structures to avoid direct contact with flames, and through hydrogen and The nitrogen mixture stream further reduces and controls the temperature.
It effectively avoids liquefaction and adhesion of powdered materials, ensures high-temperature reduction and output rate of materials, extends the service life of the kiln body, and improves production stability.
Smart Images

Figure CN118912895A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of reduction rotary kilns, in particular to a reduction rotary kiln for refining tungsten and molybdenum powders. Background Art
[0002] A rotary kiln is a rotary calcining kiln widely used in building materials, metallurgy, chemical industry, environmental protection and other fields. It mainly drives the material to move through a kiln body that rotates continuously at a certain angle, and uses natural gas as a fuel to calcine the material in the kiln body.
[0003] According to the publication (announcement) number CN103952541B, the publication (announcement) date is 2016-01-20, a double rotary kiln is disclosed, including a first rotary kiln, with a refractory layer inside, characterized in that a second rotary kiln is connected to the slag outlet of the first rotary kiln, the axial inclination angle of the second rotary kiln is the same as that of the first rotary kiln, the diameter is larger than that of the first rotary kiln, and steel outlets are symmetrically provided on both sides of the slag outlet of the second rotary kiln; the refractory layer inside the first rotary kiln and the second rotary kiln is circumferentially evenly spaced with lifting plates 200 to 400 mm higher than the refractory material. The modification of the rotary kiln structure solves the ringing problem in the production process of the rotary kiln, reduces and eliminates accidents, and reflects scientific and technological value; the lifting plate has multiple functions such as guiding, equalizing flow, and lifting, and is completely in contact with the hot air flow, so that all mineral materials can achieve the purpose of fully utilizing thermal energy and the temperature is uniform.
[0004] In the prior art including the above patents, the rotary kiln rotates continuously during operation, and the materials therein move with the kiln body and move to a high place under the action of friction, and then move along the inclined kiln body under the action of gravity, and then approach the ignition point. Due to the movement and collision of the materials in the kiln body, there will be a lot of powder in the materials, which will quickly liquefy when in contact with the flame. After the liquid materials move to the ignition point, the temperature will drop rapidly. This part of the liquid materials is easy to combine with small particles and condense on the inner wall of the kiln body, resulting in rings on the inner wall of the kiln body, which not only consumes materials but also affects the normal operation of the kiln body. Summary of the invention
[0005] The purpose of the present invention is to provide a reduction rotary kiln for refining tungsten and molybdenum powders, aiming to solve the above problems.
[0006] In order to achieve the above-mentioned object, the present invention provides a reduction rotary kiln for refining tungsten and molybdenum powders, comprising a support base and a kiln body obliquely arranged thereon, characterized in that the interior of the kiln body is provided with:
[0007] A spiral guide groove distributed in a circumferential array, wherein guide blocks distributed in a linear array are arranged inside the guide groove, and a first slope for guiding powdered materials is provided on the guide block;
[0008] A connecting path connecting two adjacent guide grooves and distributed in a linear array, wherein a first end of the connecting path faces the end of the first slope of the guide block in the previous guide groove, and a second end faces the middle of the first slope of the guide block in the next guide groove, wherein:
[0009] When the kiln body rotates, the powdered material in the guide groove moves along the first slope and passes through the connecting path into the next guide groove.
[0010] Preferably, the guide block is provided with a second slope intersecting with the first slope, and the first slope, the second slope, the straight surface of the next guide block and the inner wall of the guide groove form a funnel-shaped chamber.
[0011] Preferably, a second notch is provided on the second slope to facilitate leakage of small particle materials.
[0012] Preferably, the bottom of the first slope is provided with first notches distributed in a linear array for facilitating the leakage of powdered materials.
[0013] Preferably, a mounting plate for closing the upper half of the kiln head of the kiln body is provided on the support seat.
[0014] Preferably, the mounting plate is provided with a second gas pipe for the flow of a mixture of hydrogen and nitrogen and a first gas pipe for the flow of a mixture of natural gas and compressed air.
[0015] Preferably, a first inclined surface and a second inclined surface are respectively provided on the side walls on opposite sides of the guide groove, and the guide block is embedded in the second inclined surface.
[0016] Preferably, the first inclined surface is provided with a raised portion for guiding the airflow from the kiln head.
[0017] Preferably, the length of the first air pipe extending into the kiln body is one eighth of the length of the kiln body.
[0018] Preferably, the guide groove extends from the kiln head of the kiln body to one fifth of the length of the kiln body.
[0019] In the above technical scheme, a reduction rotary kiln for refining tungsten and molybdenum powders provided by the present invention has the following beneficial effects: when refining tungsten and molybdenum powders, the raw materials are put into the kiln tail of the working kiln body, and the raw materials move along the rotating kiln body and gradually approach the kiln head. The raw materials are preheated under the high temperature of the kiln body and gradually approach the flame part. At this time, the powder in the material falls into the spiral guide groove to avoid the powdered material from directly contacting the flame and liquefying or even adhering to other materials. At the same time, the temperature conducted by the flame in the air is sufficient to reduce the powdered material. During the rotation of the kiln body, the powdered material The material moves along the spiral guide groove and contacts the first slope of the guide block. The first slope can increase the slope of the slope for the powdered material to slide, thereby guiding the powder to move as much as possible to avoid the powder being trapped on the guide groove with a smaller slope. The powdered material gradually moves to the end of the first slope and falls into the middle of the first slope of the guide block in the next guide groove, thereby allowing the powdered material to continue to move, ensuring that the powdered material is always located in the guide groove and at the bottom of the kiln body, away from the flame, ensuring that the temperature of the powdered material is not too high, thereby ensuring the output rate of the powdered target product. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] In order to more clearly illustrate the embodiments of the present application or the technical solutions in the prior art, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can also be obtained based on these drawings.
[0021] Figure 1 A schematic diagram of the overall structure provided for an embodiment of the present invention;
[0022] Figure 2 A schematic diagram of the internal structure provided by an embodiment of the present invention;
[0023] Figure 3 for Figure 2 Enlarged view of point A in the middle;
[0024] Figure 4 A schematic diagram of the structure of a kiln body provided in an embodiment of the present invention;
[0025] Figure 5 A schematic diagram of the structure of a guide groove provided in an embodiment of the present invention;
[0026] Figure 6 for Figure 5 Enlarged view of point B in the middle;
[0027] Figure 7 A schematic diagram of the structure of a guide block provided by an embodiment of the present invention;
[0028] Figure 8 for Figure 7Enlarged view of point C in the middle;
[0029] Fig. 9 A schematic structural diagram of a kiln body in a first position provided by an embodiment of the present invention;
[0030] Fig.10 A schematic structural diagram of a kiln body in a second position provided in an embodiment of the present invention.
[0031] Description of reference numerals:
[0032] 1. kiln body; 11. guide groove; 111. first inclined surface; 112. second inclined surface; 113. lifting portion; 12. guide block; 121. first slope; 122. second slope; 123. first notch; 124. second notch; 125. straight surface; 13. connecting channel; 2. support seat; 21. mounting plate; 22. first air pipe; 23. second air pipe. DETAILED DESCRIPTION
[0033] In order to enable those skilled in the art to better understand the technical solution of the present invention, the present invention will be further described in detail below with reference to the accompanying drawings.
[0034] like Figure 1-10 As shown, a reduction rotary kiln for refining tungsten and molybdenum powders comprises a support base 2 and a kiln body 1 obliquely arranged thereon, characterized in that the interior of the kiln body 1 is provided with:
[0035] A spiral guide groove 11 is arranged in a circumferential array, and guide blocks 12 are arranged in a linear array inside the guide groove 11. The guide blocks 12 are provided with a first slope 121 for guiding powdered materials;
[0036] A connecting path 13 connecting two adjacent guide grooves 11 and arranged in a linear array, wherein a first end of the connecting path 13 faces the end of the first slope 121 of the guide block 12 in the previous guide groove 11, and a second end faces the middle of the first slope 121 of the guide block 12 in the next guide groove 11, wherein:
[0037] When the kiln body 1 rotates, the powdered material in the guide groove 11 moves along the first slope 121 and passes through the connecting path 13 to enter the next guide groove 11 .
[0038] Specifically, the next guide groove 11 in the above embodiment refers to the next guide groove 11 that moves to the position during the rotation of the kiln body 1.
[0039] Furthermore, when refining tungsten and molybdenum powders, the raw materials are put into the tail of the working kiln body 1, and the raw materials move along the rotating kiln body 1 and gradually approach the kiln head. The raw materials are preheated under the high temperature of the kiln body 1 and gradually approach the flame. At this time, the powder in the material falls into the spiral guide groove 11 to prevent the powdered material from directly contacting the flame and liquefying or even adhering to other materials. At the same time, the temperature conducted by the flame in the air is sufficient to restore the powdered material. During the rotation of the kiln body 1, the powdered material moves along the spiral guide groove 11 and contacts the guide groove 11. The first slope 121 of the guide block 12 can increase the slope of the slope for the powdered material to slide, thereby guiding the powder to move as much as possible to avoid the powder staying on the guide groove 11 with a smaller slope. The powdered material gradually moves to the end of the first slope 121 and falls into the middle of the first slope 121 of the guide block 12 in the next guide groove 11, thereby allowing the powdered material to continue to move, ensuring that the powdered material is always located in the guide groove 11 and at the bottom of the kiln body 1, away from the flame, and ensuring that the temperature of the powdered material is not too high.
[0040] In the above technical solution, when the tungsten and molybdenum powders are being refined, the raw materials are put into the tail of the working kiln body 1, and the raw materials move along the rotating kiln body 1 and gradually approach the kiln head. The raw materials are preheated at the high temperature of the kiln body 1 and gradually approach the flame. At this time, the powder in the material falls into the spiral guide groove 11 to prevent the powdered material from directly contacting the flame and liquefying or even adhering to other materials. At the same time, the temperature conducted by the flame in the air is sufficient to restore the powdered material. During the rotation of the kiln body 1, the powdered material moves along the spiral guide groove 11 and contacts with the flame. The first slope 121 of the guide block 12 is in contact with the first slope 121 of the guide block 12, and the first slope 121 can increase the slope of the slope for the powdered material to slide, thereby guiding the powder to move as much as possible to avoid the powder from being trapped on the guide groove 11 with a smaller slope. The powdered material gradually moves to the end of the first slope 121 and falls into the middle of the first slope 121 of the guide block 12 in the next guide groove 11, thereby allowing the powdered material to continue to move, ensuring that the powdered material is always located in the guide groove 11 and at the bottom of the kiln body 1, away from the flame, and ensuring that the temperature of the powdered material is not too high.
[0041] As a further embodiment of the present invention, a second slope 122 intersecting with the first slope 121 is provided on the guide block 12. The first slope 121, the second slope 122, the straight surface 125 of the next guide block 12, and the inner wall of the guide groove 11 form a funnel-shaped chamber.
[0042] Specifically, the next guide block 12 in the above embodiment is an adjacent guide block 12 that guides the guide groove 11 from the inside to the outside, and the number of the guide grooves 11 is an odd number.
[0043] Furthermore, during the rotation of the kiln body 1, the material in the kiln body 1 gradually enters the first slope 121, the second slope 122, the straight surface 125 of the next guide block 12, and the inner wall of the guide groove 11 to form a funnel-shaped chamber, wherein the powdered material enters the connecting groove along the first slope 121, and then enters the next guide groove 11, and the material in the funnel-shaped chamber moves to the top of the flame as the kiln body 1 rotates, and then from the second position (such as Fig.10 The large particles of material remaining in the funnel pass through the flame under the action of gravity, the flame heats the material, and the material falls from above and collides with the bottom of the inner wall of the kiln body 1, and the large particles of material are broken, which makes it more convenient to obtain the powdered target product. The number of guide grooves 11 distributed in a circular array is an odd number, and there are no opposite guide grooves 11, which can prevent the material from being stuck between the guide block 12 and the guide groove 11 when falling quickly.
[0044] As another embodiment further provided by the present invention, a second notch 124 is formed on the second slope 122 to facilitate the leakage of small particle materials.
[0045] Specifically, during the rotation of the kiln body 1, the material in the kiln body 1 gradually enters the first slope 121, the second slope 122, the straight surface 125 of the next guide block 12, and the inner wall of the guide groove 11 to form a funnel-shaped chamber, and the powdered material enters the connecting groove along the first slope 121, and then enters the next guide groove 11, and the material in the funnel-shaped chamber will move to the top of the flame as the kiln body 1 rotates, and the small particles of material will be in the first position (such as Fig. 9 The kiln body 1 continues to rotate and move to the second position, and the large particles fall from the second position. The remaining large particles in the funnel pass through the flame under the action of gravity. The flame heats the material, and the material falls from the top and collides with the bottom of the inner wall of the kiln body 1. The large particles are broken, which makes it more convenient to obtain the powdered target product. The number of guide grooves 11 distributed in a circular array is an odd number, and there is no opposite guide groove 11, which can prevent the material from being stuck between the guide block 12 and the guide groove 11 when falling quickly.
[0046] As another embodiment further provided by the present invention, the bottom of the first slope 121 is provided with first notches 123 distributed in a linear array for facilitating the leakage of the powdered material.
[0047] Specifically, after the small particle material is stuck between the first slope 121 of the guide block 12 and the straight surface 125 of the next guide block 12, the gap between the small particle material and the guide block 12 is very small, and the first notch 123 allows a gap to still exist between the small particle material and the guide block 12, so that the powdery material can continue to move smoothly into the connecting channel 13.
[0048] As another embodiment further provided by the present invention, a mounting plate 21 is provided on the support seat 2 for sealing the upper half of the kiln head of the kiln body 1 .
[0049] Specifically, the mounting plate 21 seals the upper half of the kiln head of the kiln body 1, which can prevent the high temperature inside the kiln body 1 from leaking out from the kiln head, avoid the high temperature air from affecting the equipment around the kiln body 1, and improve the thermal efficiency inside the kiln body 1, saving fuel.
[0050] As another embodiment further provided by the present invention, a second gas pipe 23 for the flow of a mixture of hydrogen and nitrogen and a first gas pipe 22 for the flow of a mixture of natural gas and compressed air are provided on the mounting plate 21 .
[0051] Specifically, a mixture of natural gas and compressed air is ejected from the first air pipe 22 and ignited, with the flame directed toward the kiln tail. The air inside the kiln body 1 flows at a high speed to generate negative pressure, and fresh air is sucked in from the kiln head. A mixture of hydrogen and nitrogen flows out from the second air pipe 23. Hydrogen can further reduce the material that is still in a high temperature state. Hydrogen can be used as fuel when in contact with the flame, and the mixture of nitrogen and hydrogen can prevent the flame from spreading to the kiln head.
[0052] As another embodiment further provided by the present invention, a first inclined surface 111 and a second inclined surface 112 are respectively provided on the side walls at two opposite sides of the guide groove 11 , and the guide block 12 is embedded in the second inclined surface 112 .
[0053] Specifically, the first inclined surface 111 and the second inclined surface 112 of the guide groove 11 can increase the internal space of the guide groove 11 while reducing the opening size of the guide groove 11, thereby preventing materials from falling directly into the guide groove 11 from above. The guide block 12 cooperates with the second inclined surface 112 to guide the powdered material, thereby facilitating the powdered material to enter the connecting channel 13.
[0054] As another embodiment further provided by the present invention, a raised portion 113 for guiding the airflow from the kiln head is provided on the first inclined surface 111 .
[0055] Specifically, when the kiln body 1 is working, the raised portion 113 on the first inclined surface 111 can guide the airflow from the kiln head to move toward the axis of the kiln body 1 to prevent the airflow from the kiln head from blowing the powdered material in the guide groove 11, thereby ensuring smooth discharge of the powdered material.
[0056] As another embodiment further provided by the present invention, the length of the first air pipe 22 extending into the kiln body 1 is one eighth of the length of the kiln body 1 , and the guide groove 11 extends from the kiln head of the kiln body 1 to one fifth of the length of the kiln body 1 .
[0057] Specifically, when refining tungsten and molybdenum powders, a mixture of natural gas and compressed air is ejected from the first air pipe 22 and ignited, with the flame directed toward the kiln tail. The air inside the kiln body 1 flows at a high speed to generate negative pressure, and fresh air is sucked in from the kiln head. The raw materials are put into the kiln tail of the working kiln body 1, and the raw materials move along the rotating kiln body 1 and gradually approach the kiln head. The raw materials are preheated at the high temperature of the kiln body 1 and gradually approach the flame. Before the materials come into contact with the flame, the materials will first enter the guide groove 11. During the rotation of the kiln body 1, the powdered materials move along the spiral guide groove. 11 moves and contacts with the first slope 121 of the guide block 12. The first slope 121 can increase the slope of the slope for the powdered material to slide, thereby guiding the powder to move as much as possible to avoid the powder from being trapped on the guide groove 11 with a smaller slope. The powdered material gradually moves to the end of the first slope 121 and falls into the middle of the first slope 121 of the guide block 12 in the next guide groove 11, thereby allowing the powdered material to continue to move, ensuring that the powdered material is always located in the guide groove 11 and at the bottom of the kiln body 1, away from the flame, and ensuring that the temperature of the powdered material is not too high.
[0058] During the rotation of the kiln body 1, the material in the kiln body 1 gradually enters the first slope 121, the second slope 122, the straight surface 125 of the next guide block 12, and the inner wall of the guide groove 11 to form a funnel-shaped chamber, and the powdered material enters the connecting groove along the first slope 121, and then enters the next guide groove 11. The material in the funnel-shaped chamber will move to the top of the flame as the kiln body 1 rotates, and the small particles will leak out from the second notch 124 when the kiln body 1 is in the first position. The small particles move a small distance in the flame range. After a certain distance, the temperature of the small particles is sufficient for their reduction, and the kiln body 1 continues to rotate and move to the second position, and the large particles fall from the second position. The remaining large particles in the funnel pass through the flame under the action of gravity, and the flame heats the materials. The materials fall from above and collide with the bottom of the inner wall of the kiln body 1, and the large particles are broken, which makes it more convenient to obtain the powdered target product. The number of guide grooves 11 distributed in a circular array is an odd number, and there are no opposite guide grooves 11, which can prevent the materials from being stuck between the guide block 12 and the guide groove 11 when falling rapidly.
[0059] At the same time, a mixture of hydrogen and nitrogen flows out from the second air pipe 23. Hydrogen can further reduce the material that is still in a high-temperature state. Hydrogen can be used as fuel when in contact with the flame, and the mixture of nitrogen and hydrogen can prevent the flame from spreading to the kiln head. The first inclined surface 111 and the second inclined surface 112 of the guide groove 11 can increase the internal space of the guide groove 11 while reducing the opening size of the guide groove 11, thereby preventing the material from falling directly into the guide groove 11 from above. The guide block 12 cooperates with the second inclined surface 112 to guide the powdered material, thereby facilitating the powdered material to enter the connecting channel 13. The raised portion 113 on the first inclined surface 111 can guide the airflow from the kiln head to move toward the axial direction of the kiln body 1, thereby preventing the airflow from the kiln head from blowing the powdered material in the guide groove 11, thereby ensuring the smooth discharge of the powdered material.
[0060] The above description is only by way of illustration of certain exemplary embodiments of the present invention. It is undoubted that those skilled in the art can modify the described embodiments in various ways without departing from the spirit and scope of the present invention. Therefore, the above drawings and descriptions are illustrative in nature and should not be construed as limiting the scope of protection of the claims of the present invention.
Claims
1. A reduction rotary kiln for refining tungsten and molybdenum powders, comprising a support base (2) and a kiln body (1) obliquely arranged thereon, characterized in that: The interior of the kiln body (1) is provided with: A spiral guide groove (11) distributed in a circumferential array, wherein guide blocks (12) distributed in a linear array are arranged inside the guide groove (11), and a first slope (121) for guiding powdered materials is provided on the guide block (12); A connecting path (13) connecting two adjacent guide grooves (11) and arranged in a linear array, wherein a first end of the connecting path (13) faces the end of a first slope (121) of a guide block (12) in a previous guide groove (11), and a second end faces the middle of a first slope (121) of a guide block (12) in a next guide groove (11), wherein: When the kiln body (1) rotates, the powdered material in the guide groove (11) moves along the first slope (121) and passes through the connecting path (13) to enter the next guide groove (11).
2. A reduction rotary kiln for refining tungsten and molybdenum powders according to claim 1, characterized in that: The guide block (12) is provided with a second slope (122) intersecting with the first slope (121); the first slope (121), the second slope (122), the straight surface (125) of the next guide block (12), and the inner wall of the guide groove (11) form a funnel-shaped chamber.
3. A reduction rotary kiln for refining tungsten and molybdenum powders according to claim 2, characterized in that: The second slope (122) is provided with a second notch (124) for facilitating the leakage of small particle materials.
4. The reduction rotary kiln for refining tungsten and molybdenum powders according to claim 1, characterized in that: The bottom of the first slope (121) is provided with first notches (123) distributed in a linear array for facilitating the leakage of powdered materials.
5. The reduction rotary kiln for refining tungsten and molybdenum powders according to claim 1, characterized in that: The support seat (2) is provided with a mounting plate (21) for sealing the upper half of the kiln head of the kiln body (1).
6. A reduction rotary kiln for refining tungsten and molybdenum powders according to claim 5, characterized in that: The mounting plate (21) is provided with a second gas pipe (23) for the flow of a mixture of hydrogen and nitrogen and a first gas pipe (22) for the flow of a mixture of natural gas and compressed air.
7. The reduction rotary kiln for refining tungsten and molybdenum powders according to claim 1, characterized in that: A first inclined surface (111) and a second inclined surface (112) are respectively provided on the side walls at two opposite sides of the guide groove (11), and the guide block (12) is embedded in the second inclined surface (112).
8. The reduction rotary kiln for refining tungsten and molybdenum powders according to claim 7, characterized in that: The first inclined surface (111) is provided with a raised portion (113) for guiding the airflow from the kiln head.
9. A reduction rotary kiln for refining tungsten and molybdenum powders according to claim 6, characterized in that: The length of the first air pipe (22) extending into the kiln body (1) is one eighth of the length of the kiln body (1).
10. The reduction rotary kiln for refining tungsten and molybdenum powders according to claim 8, characterized in that: The guide groove (11) extends from the kiln head of the kiln body (1) to one fifth of the length of the kiln body (1).
Citation Information
Patent Citations
Double rotary kiln and method for reducing nickel and iron
CN103952541B