Molten pool smelting accompanying flow cooling slag adhering protection spray gun and design and control method thereof
By designing a spray gun with accompanying cooling and slag protection during molten pool smelting, and utilizing swirl blades and cooling air ducts to convert kinetic energy, combined with refractory material layer protection, the problems of short spray gun life and small stirring radius were solved, achieving a highly efficient and safe smelting process.
Patent Information
- Application Number
- CN202411154034.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-21
- Publication Date
- 2024-11-08
AI Technical Summary
Existing technologies suffer from problems such as short spray gun life, severe top-blowing splashing, and small stirring radius, resulting in high smelting costs and low efficiency.
Design a slag-coating and protective spray gun for molten pool smelting, comprising a central channel, a swirl spray layer, a cooling air duct, and a refractory material layer. Cooling is enhanced by swirl blades and a cooling air duct, the swirl spray layer converts axial kinetic energy into tangential kinetic energy, increases the stirring radius, and the refractory material layer prevents high-temperature corrosion.
Extend the service life of the spray gun, improve smelting efficiency, reduce molten splashing, enhance stirring ability, reduce the risk of equipment damage, and improve product quality and resource utilization.
Smart Images

Figure CN118912911A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of metallurgical equipment, and in particular to a molten pool smelting accompanying flow cooling slag protection spray gun and a design and control method thereof. Background Art
[0002] Metallurgy is a scientific and technological field that studies and applies the physical and chemical properties of metals and alloys and related processes. It involves the extraction of metals from ores, the preparation, processing and application of alloys. The process of injecting particulate materials or gases into the molten pool through a spray gun is widely used in metallurgy. Among them, several common processes include: Powder spraying metallurgy: by spraying metal powder or alloy powder into the molten pool, metal parts are prepared by high-temperature melting and solidification process. This process can be used to manufacture high-strength and high-precision metal parts. Spray melting: using a spray gun to spray metal or alloy materials in a molten state onto the base material, forming a coating during the cooling process. This process is often used in applications such as coating protection, surface modification and repair, and can provide excellent wear resistance, corrosion resistance and thermal barrier properties. Blowing steelmaking: injecting oxygen or other gases into the molten pool through a spray gun, using the oxidation effect of the gas to change the composition and quality of the metal in the molten pool. This process is often used in deoxidation, desulfurization, alloying and other operations during the smelting process. Blowing bubbling: injecting gas into the molten pool through a spray gun to generate bubbles to stir the metal in the molten pool to promote mixing and reaction of the molten pool. This process is often used for impurity removal and alloy homogenization during smelting and refining. Injecting particulate materials or gas into the molten pool through a spray gun is a common process in metallurgy, such as submerged top blowing tin smelting and side blowing copper smelting. When the spray gun is immersed in the melt, the spray gun will be mechanically scour, chemically corroded and damaged by high temperature stress of the melt. This leads to a short service life and frequent replacement of the spray gun, which not only increases the smelting cost, but also reduces the effective operating time, which is not conducive to the cost reduction and efficiency improvement of the enterprise. Therefore, how to effectively protect the spray gun and extend the service life of the spray gun has always been a difficult problem faced by the smelting industry. In addition, for submerged top blowing smelting, there are also problems such as excessive axial momentum impact, small stirring area and severe melt splashing. Therefore, the existing technology needs to be improved.
[0003] Prior art 1, application number: CN202310745202.8 discloses a gun position monitoring and early warning method and system for top-blown submerged spray gun molten pool smelting copper. A graphite electrode is pre-buried on the inner side of the side wall of the top-blown smelting furnace and located in the copper matte layer area. The positive power wire in the gun position monitoring and early warning instrument is connected to the steel rod on the graphite electrode, and the negative power wire in the gun position monitoring and early warning instrument is connected to the original spray gun to form a closed loop. The resistance is measured by the gun position monitoring and early warning instrument. When the measured resistance data is abnormal, the gun position monitoring and early warning instrument will alarm. Although the system forms online monitoring and early warning of the gun position for submerged spray gun molten pool smelting copper, it can accurately control the spray gun position, extend the life of the spray gun, improve the equipment operation rate, and ultimately strengthen the smelting. However, the high-temperature melt cannot be placed to directly flush the spray gun, and the effect of extending the life of the spray gun is not obvious over a certain length.
[0004] Prior art 2, application number: CN 202310199495.4 discloses an oxygen-enriched molten pool smelting furnace and a heat-consuming material smelting method, which are used for smelting heat-consuming materials such as laterite, red mud, and iron-containing waste slag. The oxygen-enriched molten pool smelting furnace includes a furnace body, a furnace chamber inside the furnace body, and a molten pool area at the bottom of the furnace chamber. A spray gun for spraying materials, fuel and oxygen-enriched air is installed on the furnace body, and the spray gun's blowing port faces the molten pool area, and the spray gun can be lifted and moved; a siphon slag discharge device is also provided outside the furnace body, and the siphon slag discharge device is connected to the molten pool area to discharge the generated slag by siphoning. Although the oxygen-enriched molten pool smelting furnace has high smelting efficiency and avoids the problem of uneven hot and cold molten pool; the spray gun has a large air supply volume and flexible and changeable layout; the overflow of the slag is continuously discharged without blocking or sticking, and the liquid level in the furnace is maintained stable. However, submerged top-blowing smelting has the problems of excessive axial momentum impact and small stirring area.
[0005] Prior art three, application number: CN 202410277852.9 discloses a metallurgical furnace for top-blown molten pool refining, including a furnace body and a top-blown lance system, the top-blown lance system including a top-blown redox lance, a top-blown combustion lance and a lance control device, the top-blown redox lance is located above the furnace body, and a top-blown combustion lance is arranged in front of the top-blown redox lance. Although the slag-making agent can be continuously added by using the auxiliary material addition port, the impurities in the metallurgical furnace melt can be continuously oxidized and slag-made; the refractory material of the furnace pool bottom below the lance is built in an inverted arch structure, which can make the compressed gas injected by the redox lance stir the melt, the lower part of the feed port is built in a convex structure, which buffers the impact of adding solid materials and reduces the splashing of liquids, and the lower part of the slag outlet is built in a convex structure, and the slag is automatically discharged from the slag outlet with the melt surge formed by the gas injected by the top-blown lance. However, the melt splashes seriously and cannot effectively improve the efficiency of submerged top-blown smelting.
[0006] At present, the existing technologies 1, 2 and 3 have the problems of short spray gun life, serious top-blowing splashing and small stirring radius. Therefore, the present invention provides a molten pool smelting accompanying flow cooling slag protection spray gun and its design and control method, and the cooling layer is set to enhance the cooling capacity, reduce the temperature of the outer wall of the refractory material of the spray gun, and make it easier to slag at the nozzle; adding swirl sheets to the swirl layer and cooling layer of the spray gun effectively converts axial kinetic energy into tangential kinetic energy, and enhancing the tangential kinetic energy is conducive to enhancing the stirring capacity and increasing the stirring radius. Summary of the invention
[0007] The main purpose of the present invention is to provide a molten pool smelting accompanying flow cooling slag protection spray gun and its design and control method to solve the problems of short spray gun life, serious top blowing splashing and small stirring radius in the prior art.
[0008] To achieve the above object, the present invention provides the following technical solutions:
[0009] A molten pool smelting accompanying flow cooling slag protection spray gun, the molten pool smelting accompanying flow cooling slag protection spray gun comprises: at least three layers of channels; the central channel is used for pure gas phase or gas-solid mixed blowing; the swirl blowing layer is equipped with swirl blades for generating most of the blowing kinetic energy to stir the melt and provide oxygen for the central layer fuel; the cooling air duct is used to generate cooling swirl to promote the nozzle immersed in the melt to generate cooling slag;
[0010] A swirl spray layer is arranged outside the central channel, the swirl spray layer is equipped with swirl blades, swirlers are arranged in the swirl spray channel and cooling air duct of the swirl spray layer, and a cooling air duct is arranged outside the swirl spray layer.
[0011] As a further improvement of the present invention, a refractory material layer is arranged on the outer layer of the nozzle; cyclones are installed in the swirl injection channel and the cooling air duct, and the swirl expands the stirring radius.
[0012] As a further improvement of the present invention, a refractory material layer is arranged on the outer side of the bottom end of the cooling air duct, and a slag layer is arranged on the outer side of the refractory material layer; a mixing zone is arranged at the lowest end of the central channel, an impact pit is arranged below the mixing zone, a free surface layer is arranged on the right side of the impact pit, and a melt is arranged on the left side, and the free surface layer, the impact pit and the melt are arranged inside the molten pool wall.
[0013] As a further improvement of the present invention, the outermost channel is a sleeve ventilation channel, and a sleeve ventilation channel is arranged outside the cooling air channel;
[0014] Protect the fluid in the cooling air duct from being heated by the high-temperature molten pool and strengthen the cooling at the nozzle.
[0015] To achieve the above object, the present invention provides the following technical solutions:
[0016] A method for designing a slag protection spray gun for accompanying flow cooling of molten pool smelting is applied to the slag protection spray gun for accompanying flow cooling of molten pool smelting. The method for designing a slag protection spray gun for accompanying flow cooling of molten pool smelting includes: calculating the temperature of the outer wall of the spray gun, obtaining input parameters under any working condition, obtaining interpolation under any working condition and optimizing the nozzle.
[0017] As a further improvement of the present invention, the temperature calculation of the outer wall of the spray gun is a heat transfer calculation through the circular tube, including: the heat flow Φ through each link is constant, and for a unit length of the pipeline, the temperature difference of each link is expressed as:
[0018]
[0019] where t wi is the inner wall temperature of the tube, t wo is the outer wall temperature of the tube refractory material; t fi is the air flow temperature in the tube, t fo is the air flow temperature outside the tube; h i is the convection heat transfer coefficient in the tube, h o is the external convection heat transfer coefficient of the refractory material; d i is the inner diameter of the refractory material, d o is the outer diameter of the refractory material, λ is the thermal conductivity of the tube wall;
[0020] The evaluation of input parameters under any working condition adopts the method of numerical simulation, and the heat flow Φ is obtained as:
[0021]
[0022] Get the temperature of the inner wall of the tube:
[0023]
[0024] Get the temperature of the outer wall of the tube:
[0025]
[0026] Under any working condition t fi , t fo ,h i and h o The acquisition of is evaluated by the conjugate heat transfer numerical simulation method, and the heat transfer of the injection flow field and the solid area is solved at the same time. The control equation is as follows:
[0027] Continuity equation:
[0028]
[0029] in is the velocity vector;
[0030] Momentum conservation equation:
[0031]
[0032] Where t is time, ρ is density, is the acceleration due to gravity, P is the pressure, is the stress tensor of the Newtonian fluid, The expression is as follows:
[0033]
[0034] Where μ is the dynamic viscosity;
[0035] Energy conservation equation:
[0036]
[0037] Where T is temperature, λ is thermal conductivity, c p is the specific heat capacity at constant pressure, S T is the source term;
[0038] Turbulence equations
[0039] The SST k-ω turbulence model is used;
[0040]
[0041] Where k is the turbulent kinetic energy, ω is the specific dissipation rate, ε is the turbulent dissipation rate, v t is the turbulent kinematic viscosity, u j (j=1,2,3) are velocity components, β, σ ω2 is a closed constant; F1 is a weighting function.
[0042] As a further improvement of the present invention, the specific solution process includes:
[0043] The solid domain and the fluid domain are three-dimensionally modeled and spatially discretized to form a grid. The grid is continuous at the interface between the solid domain and the fluid domain;
[0044] Given boundary conditions, including the flow rate Q1 of the central channel, the flow rate Q2 of the swirl channel, and the flow rates Q3 and Q4 of the peripheral sleeve ventilation; the inlet temperatures of the three channels are T1, T2, T3, and T4 respectively; the ambient temperature is 1500K; the static pressure boundary condition is given at the outlet, and the value is a standard atmospheric pressure; the impact pit is set as the wall surface, and the airflow will flow back when it impacts the wall surface, which is closer to the real impact melt pit, and the temperature is 1500K; the furnace wall is set to a no-slip adiabatic boundary condition;
[0045] Set up the physical model to solve the continuity and momentum equations, energy equations, turbulence equations, and transient heat conduction equations in the solid domain;
[0046] Initialize flow field,calculation;
[0047] Process the calculation results and extract t from the results fi , t fo ,h i and h o ;
[0048] Change the inlet conditions Q1, Q2, Q3, Q4, T1, T2, T3, T4, refractory thickness δ, repeat the above steps to obtain t under different working conditions fi , t fo ,h i and h o , forming a database;
[0049] (1) Initialization: fill all missing values with mean, median, and random sampling to obtain a complete initial data set;
[0050] (2) Iteration: Multiple iterations are performed, and each iteration interpolates one or more variables containing missing values. In each iteration, for each variable Y containing missing values, i , use a prediction model to estimate the missing value Y based on the other complete variables Xi i ;
[0051] (3) Multiple iterations: Repeat the iteration until the convergence condition is met, when the interpolation results of several consecutive iterations do not change much, or when the preset maximum number of iterations is reached;
[0052] (4) Integration: After all iterations are completed, the interpolation results obtained in each iteration are integrated, and the average of multiple interpolation results is taken for each missing value;
[0053] The estimation process of MICE is represented by mathematical symbols:
[0054] For the imputation of the i-th variable, assume that the variable with missing values is Y i , the complete set of variables is X, where Xi represents the removal of Y i A set of variables;
[0055] The prediction model is expressed as follows: Yi = f(Xi) + ε i Among them, f is a prediction function, ε i is the error term;
[0056] For each iteration, the missing values are estimated using the prediction model, and then the missing values in the data set are updated; after multiple iterations, multiple complete data sets are obtained, and finally the final estimated value is obtained by integrating the results of the data sets;
[0057] Nozzle optimization design, variable parameters include:
[0058] Geometric parameters: center layer spray gun diameter d1, swirl layer diameter d2, cooling layer diameter d3 and outermost channel wind diameter d4, refractory material thickness δ;
[0059] Operation parameters: central layer blowing flow rate Q1, swirl layer flow rate Q2, cooling layer flow rate Q3, and outermost layer flow rate Q4, as well as the blowing temperatures T1, T2, T3, T4 of each layer from the inside to the outside;
[0060] The t value under different geometric parameters and operating conditions is obtained through the interpolation database class. fi , t fo ,h i and h o , combined with the formula and formula Get the temperature of the outer wall of the refractory material under the corresponding working conditions.
[0061] To achieve the above object, the present invention provides the following technical solutions:
[0062] A method for controlling a slag protection spray gun for cooling a molten pool smelting accompanying flow, which is applied to the slag protection spray gun for cooling a molten pool smelting accompanying flow, and the method for controlling a slag protection spray gun for cooling a molten pool smelting accompanying flow comprises:
[0063] Open the air flow of the cooling air duct and start the spraying system of the central channel to spray out the gas mixture; adjust the air flow of the central channel to achieve oxygen supply and spraying kinetic energy;
[0064] Adjust the spraying angle and position of the spray gun according to the melt state and target mixing effect; use thermal imaging or temperature detection instruments to monitor the melt pool temperature; adjust the movement state of the cyclone according to the melt state;
[0065] After smelting is completed, gradually reduce the gas flow until the blowing and cooling process stops; keep the cooling air duct ventilated; after smelting is completed, check and clean the spray gun and its channel; record key data of the smelting process, including temperature, melt composition and spray gun status.
[0066] As a further improvement of the present invention, the process of controlling the air flow rate of the central channel includes:
[0067] Use a flow meter to monitor the gas flow and pressure, install a flow regulating valve in the gas delivery pipeline, and change the gas flow by adjusting the servo valve opening;
[0068] Set the gas flow parameters according to the temperature of the molten pool, the properties of the melt and the required mixing effect; monitor the gas flow and molten pool temperature through flow sensors, temperature sensors and vortex meters installed on the spray gun and the molten pool, and input the data into the control system;
[0069] According to the deviation between the actual airflow and the set airflow, fuzzy processing is performed to convert the input variable into a fuzzy value; a fuzzy rule is established, which contains the numerical value of the increase or decrease of the airflow corresponding to the deviation; the fuzzy reasoning mechanism is used to obtain the fuzzy output through combination and association rules based on the fuzzy input and rule base; the fuzzy output is converted into a control quantity, and the opening of the airflow control valve is adjusted according to the defuzzification result.
[0070] As a further improvement of the present invention, the process of adjusting the spray angle and position of the spray gun includes:
[0071] Adjust the vertical and horizontal positions of the spray gun according to the state of the melt;
[0072] Select the injection angle according to the required gas mixing ratio and the temperature and fluidity of the melt; coordinate with the movement of the cyclone to promote mixing;
[0073] Monitor the temperature and fluidity of the melt, as well as the mixing uniformity in real time, and keep records of each adjustment of the spray angle, spray gun position and melt state parameters.
[0074] The spray gun of the present invention has 4 layers of channels. The central channel is a traditional round tube, which can be used for pure gas phase or gas-solid mixed spraying; the swirl spraying layer is equipped with swirl blades to generate most of the spraying kinetic energy to stir the melt and provide oxygen for the central layer fuel; the cooling air duct is used to generate cooling swirl to promote the nozzle immersed in the melt to produce cooling slag. It should be noted that the cooling air duct is separated from the mixing at the nozzle, so as to prevent the air flow velocity of the cooling air duct from attenuating and enhance the cooling effect; the outermost channel is the sleeve ventilation duct. Since the heat transfer coefficient of air is much lower than that of metal, a certain flow rate of sleeve ventilation can effectively protect the fluid in the cooling air duct from being heated by the high-temperature molten pool and enhance the cooling effect at the nozzle. In order to avoid the sleeve from being corroded by the melt, its position should be higher than the molten pool by a certain distance. In addition, the outer layer of the nozzle is arranged with a refractory layer. During the spraying process, since the refractory material is cooled, its temperature is lower than the melting point of the slag, and a layer of slag will be formed on the surface of the refractory material. Since the slag and the melt are the same material, the slag layer can be prevented from being corroded and damaged from the source. And as long as the nozzle maintains a low temperature, the thickness of the slag layer can be maintained at a certain value. If mechanical scouring occurs and causes the slag to become thinner, the slag will be immediately recooled under the action of low temperature. In addition, cyclones are installed in the swirl injection channel and the cooling air duct. The swirl can enhance the injection stirring capacity, expand the stirring radius, and reduce melt splashing. Specifically, the cyclone can convert pressure energy into kinetic energy, and redistribute the circumferential kinetic energy and axial kinetic energy; by significantly increasing the circumferential kinetic energy, the diameter of the impact pit can be expanded; by reducing the axial kinetic energy, the melt splashing can be reduced, and the smoke rate and lining corrosion damage can be reduced. BRIEF DESCRIPTION OF THE DRAWINGS
[0075] Figure 1 It is a structural schematic diagram of an embodiment of a slag protection spray gun for cooling with accompanying flow during molten pool smelting according to the present invention;
[0076] Figure 2 A schematic flow chart of the steps of an embodiment of a method for controlling a slag protection spray gun during cooling of a molten pool smelting accompanying flow according to the present invention;
[0077] Figure 3 A schematic diagram of the calculation of the outer wall temperature of a lance in one embodiment of a method for controlling a slag protection lance during accompanying flow cooling during molten pool smelting according to the present invention;
[0078] Figure 4 A schematic diagram of the calculation domain of an embodiment of a method for controlling a slag protection spray gun during accompanying flow cooling during molten pool smelting according to the present invention;
[0079] Figure 5 Schematic diagram of the stirring area comparison of an embodiment of the method for controlling the slag protection spray gun during the accompanying flow cooling of the molten pool smelting of the present invention; (a) without rotation; (b) with rotation;
[0080] Figure 6A schematic diagram showing a comparison of the amount of spatter in one embodiment of a method for controlling a slag protection spray gun during accompanying flow cooling during molten pool smelting according to the present invention;
[0081] Figure 7 It is a structural schematic diagram of an embodiment of an electronic device of the present invention;
[0082] Figure 8 It is a schematic structural diagram of an embodiment of the storage medium of the present invention. DETAILED DESCRIPTION
[0083] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0084] The terms "first", "second" and "third" in the present invention are only used for descriptive purposes and cannot be understood as indicating or implying relative importance or implicitly indicating the number of indicated technical features. Therefore, the features defined as "first", "second" and "third" can explicitly or implicitly include at least one of the features. In the description of the present invention, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined. All directional indications (such as up, down, left, right, front, back...) in the embodiments of the present invention are only used to explain the relative position relationship, movement, etc. between the components under a certain specific posture (as shown in the accompanying drawings). If the specific posture changes, the directional indication also changes accordingly. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions. For example, a process, method, system, product or device that includes a series of steps or units is not limited to the listed steps or units, but optionally also includes steps or units that are not listed, or optionally also includes other steps or units inherent to these processes, methods, products or devices.
[0085] Reference to an "embodiment" herein means that a particular feature, structure, or characteristic described in conjunction with the embodiment may be included in at least one embodiment of the present invention. The appearance of the phrase in various places in the specification does not necessarily refer to the same embodiment, nor is it an independent or alternative embodiment that is mutually exclusive with other embodiments. It is explicitly and implicitly understood by those skilled in the art that the embodiments described herein may be combined with other embodiments.
[0086] like Figure 1As shown, this embodiment provides an embodiment of a slag protection spray gun for accompanying flow cooling of molten pool smelting. In this embodiment, the slag protection spray gun for accompanying flow cooling of molten pool smelting specifically includes: a central channel 1, a swirl blowing layer 2, a cooling air duct 3, a sleeve air duct 4, a cyclone 5, a refractory material layer 6, a slag layer 7, a free surface layer 8, a molten pool wall 9, an impact pit 10, a melt 11, and a mixing zone 12;
[0087] Among them, the central channel 1 is arranged in the innermost layer of the spray gun, the swirl spray layer 2 is arranged on the outside of the central channel 1, the swirl spray layer 2 is installed with swirl blades, the swirl spray channel and the cooling air duct 3 of the swirl spray layer 2 are installed with cyclones 5, the cooling air duct 3 is arranged on the outside of the swirl spray layer 2, the sleeve ventilation duct 4 is arranged on the outside of the cooling air duct 3, the refractory material layer 6 is arranged on the outside of the bottom end of the cooling air duct 3, and the slag layer 7 is arranged on the outside of the refractory material layer 6; a mixing zone 12 is arranged at the lowest end of the central channel 1, an impact pit 10 is arranged below the mixing zone 12, a free surface layer 8 is arranged on the right side of the impact pit 10, a melt 11 is arranged on the left side, and the free surface layer 8, the impact pit 10 and the melt 11 are arranged inside the molten pool wall 9;
[0088] Preferably, the working principle of this embodiment ensures that the components such as the central channel 1, the swirl spray layer 2, the cooling air duct 3, the sleeve air duct 4, the refractory material layer 6, the slag layer 7 are intact and firmly connected; clean the nozzle, channel and cyclone 5 to ensure that there is no slag accumulation or impurities affecting the spray and cooling effect; check the refractory material layer 6 to ensure that the refractory material has not fallen off or damaged; ensure that the used fuel (gas or solid) and the stored raw materials (such as metals, ores) meet the quality requirements. Turn on the air flow of the cooling air duct 3 to ensure that the air flow speed in the cooling air duct 3 is stable so that the cooling effect is optimal; after determining that the cooling air duct 3 is working properly, start the spray system of the central channel 1 to spray the gas mixture; adjust the air flow of the central channel 1 according to the temperature and demand of the molten pool to achieve a good oxygen supply and spray kinetic energy; adjust the spray angle and position of the spray gun according to the state of the melt 11 and the target mixing effect; use thermal imaging or temperature detection instruments to monitor the temperature of the molten pool 11 in real time to ensure that it is within a safe range; regularly check the formation of slag to ensure Its thickness and stability, and avoid timely corrosion; according to the state of the melt 11, adjust the movement state (such as rotation speed) of the cyclone 5 to enhance the stirring effect and avoid melt splashing; after the smelting is completed, gradually reduce the gas flow until the spraying and cooling process is stopped; keep the cooling air duct 3 ventilated for a period of time to ensure that the spray gun and its channel are fully cooled; after the smelting is completed, check and clean the spray gun and its channel to prevent the accumulation of slag and untreated materials; record the key data of the smelting process, including temperature, melt composition, spray gun state, etc., to provide a basis for subsequent analysis and improvement;
[0089] The spray gun of this embodiment has four layers of channels. The central channel 1 is a traditional round tube, which can be used for pure gas phase or gas-solid mixed spraying; the swirl spray layer 2 is equipped with swirl blades to generate most of the spray kinetic energy to stir the melt 11 and provide oxygen for the central layer fuel; the cooling air duct 3 is used to generate cooling swirl to promote the nozzle immersed in the melt 11 to produce cooling slag. It should be noted that the cooling air duct 3 is separated from the nozzle and the mixing zone 12, which is to prevent the air flow velocity of the cooling air duct 3 from attenuating and enhance the cooling effect; the outermost channel is the sleeve ventilation duct 4. Since the heat transfer coefficient of air is much lower than that of metal, a certain flow of sleeve ventilation can effectively protect the fluid in the cooling air duct 3 from being heated by the high-temperature molten pool and enhance the cooling effect at the nozzle. In order to prevent the sleeve from being corroded by the melt 11, its position should be higher than the molten pool by a certain distance. In addition, the outer layer of the nozzle is arranged with a refractory layer 6. During the spraying process, since the refractory material is cooled and its temperature is lower than the melting point of the slag, a layer of slag will be formed on the surface of the refractory material. Since the slag and the melt 11 are made of the same material, the slag layer can be prevented from being corroded and damaged at the source. And as long as the nozzle maintains a low temperature, the thickness of the slag layer can be maintained at a certain value. If mechanical scouring occurs and causes the slag to become thinner, the slag will be immediately recooled under the action of low temperature. In addition, a cyclone 5 is installed in the swirl injection channel and the cooling air duct 3. The swirl can enhance the injection stirring ability, expand the stirring radius, and reduce the splash of the melt. Specifically, the cyclone 5 can convert pressure energy into kinetic energy, and redistribute the circumferential kinetic energy and axial kinetic energy; by significantly increasing the circumferential kinetic energy, the diameter of the impact pit 10 can be expanded; by reducing the axial kinetic energy, the splash of the melt 11 can be reduced, and the smoke rate and corrosion damage to the furnace lining can be reduced.
[0090] The central channel 1 of this embodiment is the innermost layer of the spray gun. The central channel 1 is responsible for guiding and spraying the gas mixture; ensuring efficient oxygen supply and the spraying of other gases, which helps to fully carry out the smelting reaction and improve the smelting effect. The swirl spray layer 2 forms a swirl through the swirl blades to enhance the mixing effect of the gas; improve the contact between the gas and the melt, improve the efficiency of the oxidation reaction, and then improve the smelting efficiency and quality. The cooling air duct 3 provides a cooling airflow to protect the spray gun and the surrounding of the molten pool from high temperature damage, extend the service life of the equipment, prevent equipment failure caused by overheating, and improve the safety of the overall smelting process. The sleeve ventilation duct 4 is used as a gas channel to increase the conveying efficiency of the airflow; help to more evenly distribute the cooling airflow and reaction gas to ensure the stability and reliability of the smelting process. The cyclone 5 adjusts the gas flow state and enhances the stirring effect of the melt; promotes the formation of a good mixture inside the melt, reduces the stratification phenomenon, ensures the uniformity of the melt, and improves the quality of the finished product. The refractory layer 6 is resistant to high temperatures to prevent the loss of heat in the molten pool; protects other components inside the spray gun from high temperatures to ensure the durability and reliability of the equipment. The slag layer 7 forms a protective layer above the molten pool, and regulates the heat exchange with the molten pool to a certain extent; controls the temperature fluctuation of the molten pool, reduces the oxidation loss of the melt, reduces unnecessary slag generation, and improves the smelting efficiency. The free surface layer 8 maintains the stability of the surface state of the melt; avoids splashing and loss caused by excessive fluctuations of the melt surface, and provides a stable environment for the smelting process. The molten pool wall 9 surrounds the molten pool and provides structural support; ensures the stability of the molten pool shape, reduces melt leakage and heat loss. The impact pit 10 is used to gather and improve the contact between the gas and the melt; optimizes the reaction conditions, improves the smelting efficiency, and promotes the uniform mixing of the melt. The melt 11, as the main smelting material, is heated and gas-acted; realizes the melting and chemical reaction of the metal material, and provides conditions for subsequent casting and processing. The mixing zone 12 forms an effective mixing area between the gas and the melt; ensures that the melt has a consistent temperature and composition, and improves the uniformity and quality stability of the smelting process.
[0091] In summary, through the efficient collaboration of the above-mentioned mechanisms, the in-flow cooling slag protection spray gun system in molten pool smelting in this embodiment can optimize the entire smelting process and achieve the following goals: improve smelting efficiency, enhance the reactivity of the melt and shorten the smelting time through better gas supply and mixing. Ensure safety, effective cooling and protection measures, reduce the risk of equipment damage, and ensure safe operation. Improve product quality, ensure the consistency of the composition and properties of the final product through uniform mixing and control of reaction conditions. Reduce resource waste, reduce slag and harmful emissions, and improve resource utilization by optimizing the smelting process. It plays an important role in improving the modernization level of the smelting industry and promoting efficient utilization and sustainable development of resources.
[0092] This embodiment provides a cooling layer on the basis of the traditional spray gun, which can enhance the cooling capacity, reduce the temperature of the outer wall of the refractory material of the spray gun, and make it easier for slag to hang on the nozzle. Once slag is formed, it can effectively prevent the high-temperature melt from directly washing the spray gun head. At the same time, the slag and the cooled and solidified slag are different forms of the same substance, which fundamentally avoids the corrosion of the spray gun head by the slag. Ultimately, the service life of the spray gun is greatly improved; by adding swirl sheets to the swirl layer and cooling layer of the spray gun, the axial kinetic energy can be effectively converted into tangential kinetic energy, thereby effectively reducing the vertical impact of the airflow and reducing the splashing of the melt; at the same time, enhancing the tangential kinetic energy is conducive to enhancing the stirring ability and increasing the stirring radius.
[0093] like Figure 2 As shown, this embodiment also provides an embodiment of a method for controlling a slag protection spray gun for a molten pool smelting accompanying flow cooling. In this embodiment, the method for controlling a slag protection spray gun for a molten pool smelting accompanying flow cooling is applied to the slag protection spray gun for a molten pool smelting accompanying flow cooling in the above embodiment. The method for controlling a slag protection spray gun for a molten pool smelting accompanying flow cooling specifically includes the following steps:
[0094] Step S1: Open the air flow of the cooling air duct, start the spraying system of the central channel, and spray out the gas mixture; adjust the air flow of the central channel to achieve oxygen supply and spraying kinetic energy;
[0095] Step S2: adjusting the spraying angle and position of the spray gun according to the melt state and the target mixing effect; using thermal imaging or temperature detection equipment to monitor the temperature of the molten pool; adjusting the motion state of the cyclone according to the melt state;
[0096] Step S3: After the smelting is completed, the gas flow rate is gradually reduced until the blowing and cooling process are stopped; the cooling air duct is kept ventilated; after the smelting is completed, the spray gun and its channel are inspected and cleaned; key data of the smelting process are recorded, including temperature, melt composition and spray gun status.
[0097] Preferably, step S1 of this embodiment starts the airflow of the cooling air duct, starts the blowing system of the central channel, and sprays the gas mixture; adjusts the airflow of the central channel to achieve oxygen supply and blowing kinetic energy; cooling and protection: starting the airflow of the cooling air duct can effectively reduce the surface temperature of the equipment, prevent overheating, and ensure the safety of the nozzle and other components; blowing gas supply: after the blowing system of the central channel is started, ensure the rapid and effective spraying of oxygen and other gases, and increase the contact opportunity between the gas and the melt; safety: ensure the stability of the equipment during the smelting process and reduce the equipment failure rate; reaction efficiency: improving the oxygen blowing efficiency helps to accelerate the melting of the melt and increase the reaction rate, thereby increasing the smelting efficiency. Step S2 adjusts the spraying angle and position of the spray gun according to the melt state and the target mixing effect; uses thermal imaging or temperature detection instruments to monitor the molten pool temperature; adjusts the movement state of the cyclone according to the melt state; precise control: adjusts the spraying angle and position of the spray gun to achieve targeted mixing and reaction, and effectively improves the mixing uniformity of the melt; temperature monitoring: real-time monitoring of the molten pool temperature, timely adjustment of operating parameters, and avoidance of overheating or overcooling; enhanced stirring: adjusts the movement of the cyclone according to the melt state to optimize the mixing effect of the gas and the melt; quality assurance: ensures the uniformity of the melt composition through precise regulation and improves the quality of the final product; process controllability: establishes a real-time feedback mechanism for the smelting process to achieve dynamic adjustment and improve the safety and efficiency of the process. Step S3: After smelting is completed, the gas flow rate is gradually reduced until the blowing and cooling process are stopped; the cooling air duct is kept ventilated; after smelting is completed, the spray gun and its channel are inspected and cleaned; key data of the smelting process, including temperature, melt composition and spray gun status, are recorded; gradual shutdown: the gas flow rate is gradually reduced to ensure the smooth shutdown of the spray gun and related equipment to avoid material splashing or temperature drop caused by sudden stop; equipment maintenance: the spray gun and its channel are inspected and cleaned to prevent slag and impurities from accumulating, and to maintain the cleanliness and performance of the equipment; safe operation: steady shutdown helps avoid accidents and ensure the safety of operators; data accumulation and analysis: by recording key data in the smelting process, it can provide reference for subsequent operations, help optimize the process, and improve the smelting process level.
[0098] In summary, this embodiment, through the control method of the above three steps, can realize the effective combination of various technical effects in the molten pool smelting process, and achieve the following overall significance: improve smelting efficiency and quality: by accurately controlling the airflow and mixing effect, ensure that the melt is smelted under optimal conditions; enhance operational safety: real-time monitoring and timely adjustment to ensure safe operation of equipment and reduce the probability of accidents; promote sustainable development: by cleaning and recording data, optimize the production process, improve resource utilization and reduce waste.
[0099] Furthermore, the process of controlling the air flow rate of the central channel in step S1 specifically includes the following steps:
[0100] Step S11: using a flow meter to monitor the gas flow and pressure, installing a flow regulating valve in the gas delivery pipeline, and changing the gas flow by adjusting the servo valve opening;
[0101] Step S12: setting gas flow parameters according to the temperature of the molten pool, the properties of the melt and the desired mixing effect; monitoring the gas flow and the molten pool temperature through sensors (flow sensor, temperature sensor and vortex meter) installed on the spray gun and the molten pool, and inputting the data into the control system;
[0102] Step S13: Perform fuzzy processing according to the deviation between the actual airflow and the set airflow, and convert the input variable into a fuzzy value; establish a fuzzy rule, which contains the numerical value of the increase or decrease of the airflow corresponding to the deviation; use the fuzzy reasoning mechanism, according to the fuzzy input and the rule base, through combination and association rules, to obtain the fuzzy output; convert the fuzzy output into a control quantity, and adjust the opening of the airflow control valve according to the defuzzification result.
[0103] Preferably, in step S11 of this embodiment, flow monitoring and regulation, using a flow meter to monitor gas flow and pressure, can obtain the flow state of the gas in real time, and provide reliable basic data for subsequent control; by installing a flow control valve, the flow of the gas can be accurately controlled by adjusting the servo valve, providing a flexible flow regulation method; real-time monitoring of the flow state of the gas helps to prevent safety hazards caused by abnormal flow and ensure the normal operation of the equipment; dynamically adjust the gas flow to ensure the stability of gas supply, so that the melting process can be carried out under optimal conditions, and improve the efficiency and safety of melting. Step S12 parameter setting and data monitoring, according to the temperature of the molten pool, the properties of the melt and the required mixing effect, reasonably set the target parameters of the gas flow to meet the needs of different melting conditions; through the monitoring of various sensors such as flow sensors, temperature sensors and vortex meters, obtain rich real-time data, and input it into the control system for analysis and decision-making; effective parameter setting enables the control system to automatically adjust the gas flow under different working conditions, realize reasonable control of the molten pool state, and enhance the flexibility of the process; real-time monitoring data provides a basis for control decisions, so that the system can respond in time under dynamic conditions to ensure product quality. Step S13 fuzzy processing and reasoning, fuzzy processing is performed on the deviation between the actual gas flow rate and the set value, and it is converted into a fuzzy value to facilitate the subsequent application of fuzzy rules; a fuzzy rule library is established so that the system can make corresponding gas flow adjustments according to the degree of deviation; the fuzzy input is converted into a fuzzy output through a fuzzy reasoning mechanism, and finally defuzzification is performed to obtain a clear control quantity; fuzzy control is suitable for processing complex, nonlinear, and changeable systems, which can not only cope with situations that cannot be accurately described, but also flexibly cope with changes in the state of the molten pool; fuzzy control can quickly adapt to changes in gas flow, accurately adjust the gas flow, reduce prediction errors, and improve the sensitivity of system response, thereby improving the stability and consistency of the smelting process.
[0104] In summary, in this embodiment, through the synergistic effect of these three steps, the control of the gas flow rate in the central channel is realized: real-time monitoring and dynamic control, through effective monitoring and adjustment, the gas flow rate is kept within the ideal range; the smelting process is optimized, through reasonable setting of parameters and the use of fuzzy control, effective management of complex working conditions is achieved to ensure product quality; the safety and stability of the system are improved, through monitoring and rapid response, potential risks are prevented, and the safety of equipment and the stability of the process are improved; sufficient data support and decision-making basis are provided for the continuous improvement and optimization of the smelting process, which helps to achieve more efficient and intelligent industrial production.
[0105] Furthermore, the process of establishing fuzzy rules in step S13 specifically includes the following steps:
[0106] Step S131: Determine input variables and output variables;
[0107] Input variable: The input variable is the "deviation", which is the difference between the actual air flow and the set air flow;
[0108] Output variable: The output used for control is the "airflow adjustment amount", that is, the amount of change in the airflow rate adjusted according to the deviation;
[0109] Step S132: define fuzzy sets, perform fuzzification processing on input and output variables, and define corresponding fuzzy sets; for example:
[0110] Deviation (e); Positive Large (PL); Positive Small (PS); Zero (Z); Negative Small (NS); Negative Large (NL)
[0111] Airflow adjustment amount (ΔQ): Increase Large (IL); Increase Small (IS); No Change (NC); Decrease Small (DS); Decrease Large (DL);
[0112] Step S133: construct a fuzzy rule base, where each rule adopts the format of "if...then..." to describe the relationship between input and output;
[0113] Example fuzzy rules include: if the deviation is negative NL, then the airflow decreases DL; if the deviation is negative NS, then the airflow decreases DS; if the deviation is zero Z, then the airflow remains unchanged NC; if the deviation is positive PS, then the airflow increases IS; if the deviation is positive PL, then the airflow increases IL.
[0114] Preferably, step S131 of this embodiment determines the input variables and output variables, clarifies the main input and output variables used for control, the input variable is "deviation", and the output variable is "airflow adjustment amount", and the clarity makes the control logic clearer; ensures that the system can make adjustments based on the difference (deviation) between the real-time measured airflow and the set value; simplifies the complex control problem into the relationship between input and output, which is convenient for subsequent fuzzy processing and rule construction; focuses on the variables directly related to the control decision, which can improve the pertinence and effectiveness of the control strategy. Step S132 defines the fuzzy set, and by defining the fuzzy set of "deviation" and "airflow adjustment amount", the exact value is converted into a fuzzy set, which enables the system to handle uncertainty and fuzziness problems; uses fuzzy language (such as "positive big", "negative small") to describe variables, making it more in line with human thinking; establishes an understandable language model for complex physical phenomena, so that the system can better combine with empirical knowledge and improve control accuracy; can adapt to environmental changes or the unpredictability of system behavior, and enhance the flexibility and robustness of the system. Step S133 constructs a fuzzy rule base, and forms a set of fuzzy rules based on the fuzzy set of input and output variables. These rules describe the behavior of the system and its decision-making process through the "if...then..." pattern; these rules not only realize the system's response to the state, but also form a complex control logic by combining multiple rules; a decision-making method based on experience and actual dynamic characteristics is provided, so that the controller can make corresponding adjustments according to the fuzzy input; the fuzzy rule base is equivalent to systematizing and rationalizing expert experience and system behavior patterns, forming a debuggable knowledge base; by refining the understanding of airflow regulation rule by rule, the intelligence and accuracy of the control strategy are improved, which helps to achieve the target airflow.
[0115] In summary, the entire process of establishing fuzzy rules in this embodiment ensures that the fuzzy control system can flexibly respond to different working conditions and effectively deal with the challenges caused by uncertainty and fuzziness. This design process not only promotes the system's adaptability to complex working conditions, but also improves the intelligence and effect of the control process, thereby improving the stability and reliability of gas flow control, and ultimately ensuring the efficiency and safety of the smelting process.
[0116] Furthermore, the process of adjusting the spraying angle and position of the spray gun in step S2 specifically includes the following steps:
[0117] Step S21: adjusting the vertical position and horizontal position of the spray gun according to the state of the melt;
[0118] Step S22: Select the spraying angle according to the required gas mixing ratio and the temperature and fluidity of the melt; coordinate the movement mode of the cyclone to promote mixing;
[0119] Step S23: monitor the temperature and fluidity of the melt, as well as the mixing uniformity in real time, and keep a record of the spray angle, spray gun position and melt state parameters adjusted each time.
[0120] Preferably, step S21 of this embodiment adjusts the vertical and horizontal positions of the spray gun according to the state of the melt, and adjusts the height of the spray gun. By adjusting the vertical position of the spray gun, the contact area between the gas and the melt can be changed, so that the gas can act on the melt at the optimal height, thereby improving the mixing efficiency; the horizontal position of the spray gun is adjusted to optimize the horizontal distance between the spray gun and the molten pool to meet the melt flow characteristics and mixing requirements, ensuring that the gas can be effectively sprayed into the molten pool and guide the melt flow. Improve melt fluidity: A reasonable spray gun position can improve the flow of the melt and reduce the dead angle of the melt, thereby ensuring the uniformity and mixing effect of the melt; Enhance the interaction between the gas and the melt: By adjusting the position of the spray gun, the effective contact area between the gas and the melt is increased, making the mixing more uniform and helping to control the temperature of the molten pool. Step S22: Select the spray angle according to the required gas mixing ratio and the temperature and fluidity of the melt; Select the appropriate spray angle: Select the optimized spray angle according to the fluidity and temperature of the melt to ensure that the gas is effectively dispersed into the molten pool and guide the flow direction of the melt; Cooperate with the movement mode of the cyclone: Adjust the spray angle to make it compatible with the setting of the cyclone, enhance the circulation of the melt and the secondary mixing effect of the gas and the melt. Achieve the best mixing effect: Through the appropriate spray angle, the gas enters the molten pool in the best way to promote the uniform mixing of the melt components; Optimize the gas use efficiency: Reasonable selection of the nozzle angle helps to achieve the required gas mixing ratio, thereby avoiding resource waste and improving the economy of the smelting process. Step S23: Real-time monitoring of the temperature and fluidity of the melt, as well as the mixing uniformity, and record the parameters adjusted each time; Real-time monitoring: Real-time monitoring of the temperature, fluidity and mixing uniformity of the molten pool, timely acquisition of changes in the melt state, and improvement of the accuracy of the operation; Data recording: Keep records of the spray angle, spray gun position and melt state parameters adjusted each time, and provide data support for subsequent process adjustment and optimization. Decision-making basis: Real-time monitoring data provides a basis for operational decisions, can quickly respond to changes in the melt state, and adjust the control strategy in time; Optimize subsequent processes: By recording data, the impact of spray gun adjustment on the melt mixing effect can be analyzed, providing a reference for the optimization of subsequent smelting processes, helping to form an experience library and ensure the improvement of melting quality and efficiency.
[0121] In summary, the above steps of this embodiment can effectively improve the flow and mixing state of the melt, improve the efficiency of the smelting process and the product quality by adjusting the injection angle and position of the spray gun; through each step, it can be seen that these adjustments are not only technical improvements, but also improve the control level of the smelting process as a whole, making it more intelligent and precise, and ensuring the stability and economy of production.
[0122] Furthermore, the process of adjusting the vertical position and the horizontal position of the spray gun in step S21 specifically includes the following steps:
[0123] Step S211: installing a temperature sensor above or around the molten pool to monitor the temperature change of the melt in real time; using a flow sensor to measure the flow state of the melt to determine the viscosity and flow condition of the melt; an online spectrometer is used to monitor the composition of the melt to ensure real-time evaluation of the melt mixing uniformity;
[0124] Step S212: All sensors upload the measured data to the control system through the digital interface. The control system uses the data processing algorithm to analyze the temperature, fluidity, composition uniformity and other data in real time, and uses the machine learning algorithm to build a model to predict the relationship between the melt state change and the control effect;
[0125] Step S213: Use neural network control to automatically adjust the vertical and horizontal positions of the spray gun, use an electric servo system or a pneumatic actuator to adjust the vertical and horizontal positions of the spray gun, and the actuator is controlled by the control system; install an encoder to provide real-time feedback on the actual position of the spray gun and perform error correction; set a threshold value, and when the melt state exceeds the preset range or the spray gun position is abnormal, the system automatically alarms.
[0126] Preferably, in step S211 of this embodiment, the sensor monitors the melt state, and the temperature sensor can accurately measure the temperature change of the melt during the smelting process and provide key data information; the flow sensor measures the flow state and viscosity of the melt in real time to ensure that the smelting is carried out under appropriate flow conditions; the online spectrometer detects the melt composition in real time, and timely evaluates the mixing uniformity to ensure that all components meet the target specifications. Accurately monitoring the melt state helps to adjust the control strategy in time to maintain the stability of the smelting process; real-time monitoring reduces smelting defects caused by uneven composition and excessively high or low temperature, and improves the quality control of smelting products. Step S212 data upload and processing, the data of each sensor is centrally uploaded to the control system through a digital interface to achieve unified data management; the control system uses data processing algorithms to analyze the temperature, fluidity and composition uniformity of the melt in real time to provide a basis for subsequent control decisions; machine learning algorithms are used to establish models to predict the relationship between melt state changes and control effects, forming a more intelligent control strategy. Enhanced precision and flexibility: Real-time data analysis and machine learning models can make the control system more adaptable and respond quickly under different working conditions; Predictive control: By predicting changes in the melt state, the control system can take measures in advance to reduce risks and unexpected failures. Step S213 automatically adjusts the spray gun position, and the neural network control algorithm automatically adjusts the vertical and horizontal positions of the spray gun to enhance the degree of automation of control; Use precise electric servo systems or pneumatic actuators to quickly and accurately adjust the spray gun position to meet the needs of different melt states; Install encoders to affect the spray gun position, and the real-time feedback mechanism enables the control system to perform error correction to ensure the accuracy of the spray gun position. Improve control efficiency: Through automated control, human intervention is reduced, and the system response speed and stability are improved. Improve production safety: Real-time monitoring and accurate position control reduce safety hazards that may be caused by equipment failure or operating errors, and ensure safe production operations.
[0127] In summary, the process of adjusting the vertical and horizontal positions of the spray gun in this embodiment realizes a closed-loop control system from sensor detection to intelligent data processing, automatic regulation and real-time feedback. Intelligent control engineering not only improves the accuracy and stability of the smelting process, optimizes product quality, but also promotes the modernization and intelligent development of smelting technology. It makes the smelting process more efficient, safe and sustainable, and adapts to the ever-changing industrial needs.
[0128] Further, the process of predicting the relationship between the melt state change and the control effect in step S212 specifically includes the following steps:
[0129] Step S2121: The temperature sensor, flow sensor and online spectrum analyzer transmit real-time measured data to the control system, and each sensor uploads data points at a high frequency through a digital interface; the collected real-time data is filtered to remove abnormal values;
[0130] Step S2122: extract key features from the temperature data, such as the temperature change rate, average temperature, etc.; extract dynamic features such as flow rate, flow pattern, etc. from the fluidity data; extract the concentration changes of each component from the component analysis, including different proportions of alloy components and additives; use principal component analysis to select the features that have the greatest impact on the melt state;
[0131] Step S2123: Use historical data to establish a prediction model to associate the current state data of the melt with the final smelting effect; use the feature data acquired in real time and input it into the trained model for reasoning to predict the melt state (viscosity, mixing uniformity) and the impact of the spray gun position adjustment; based on the output results of the model, evaluate the current state of the melt (such as temperature is too high or too low, insufficient fluidity, etc.), and at the same time evaluate its need to adjust the spray gun position.
[0132] Preferably, in step S2121 of this embodiment, data transmission and outlier removal, temperature sensors, flow sensors and composition analysis instruments upload data at a high frequency, and improve the system's real-time monitoring capability of the melt state; the collected data is processed by filtering, outliers are removed, and the accuracy of subsequent analysis is ensured; real-time and accurate data lays the foundation for subsequent analysis. The removal of outliers can reduce the interference of noise on the results and ensure that the patterns learned by the model are more reliable; timely acquisition of effective data enables the system to respond quickly to changes in the melt state, thereby improving the control effect. Step S2122 feature extraction and selection, extract key features from temperature, fluidity and composition data, so that the model can focus on important information related to changes in the melt state; use principal component analysis to select the features that have the greatest impact on the melt state, reduce input dimensions, and improve the efficiency of model training and reasoning; by extracting and selecting features, the model can reduce the computational burden, speed up processing, and make real-time monitoring possible; selecting key features helps the model better understand the important patterns in the data, thereby improving the accuracy of prediction of the melt state. Step S2123: Model establishment and reasoning. Use historical data to establish a prediction model (such as a regression model, a neural network, etc.), associate the current state data of the melt with the final smelting effect, and form a knowledge base; input the acquired feature data into the trained model for reasoning, covering the influence of the melt state (viscosity, mixing uniformity, etc.) and the adjustment of the spray gun position; through the reasoning ability of the model, the system can make intelligent decisions in complex situations and optimize the operation of the spray gun; by accurately predicting changes in the melt state, the process parameters can be adjusted in time to ensure the stability of the smelting process and improve the quality of the final product; continuously evaluate the state of the melt (such as temperature, fluidity, and composition uniformity, etc.) according to the output results of the model; when it is found that the state exceeds the preset threshold, the system automatically generates corresponding instructions to adjust the spray gun position; real-time monitoring and evaluation of the melt state enables the system to respond quickly and make necessary adjustments to achieve online optimization of the process; reduce risks and enhance safety: through automated instruction generation, the risk of human operating errors is reduced, and the safety and reliability of the smelting process are improved.
[0133] In summary, through the implementation of each of the above steps, the entire prediction process of this embodiment can efficiently monitor the melt state and accurately predict it. It not only enhances the intelligence level of the system, but also creates conditions for achieving highly automated production control, which is of great significance for improving product quality, improving production efficiency, and reducing operational risks. Through this intelligent production process, enterprises can better adapt to changes in market demand and lay the foundation for efficient and flexible manufacturing.
[0134] Furthermore, the process of coordinating the spray angle with the cyclone in step S22 specifically includes the following steps:
[0135] Step S221: The spraying direction of the spray gun should be consistent with the rotation direction of the cyclone, and the rotation speed of the cyclone is set according to the fluidity and viscosity of the melt;
[0136] Step S222: using sensors to monitor the temperature, fluidity and mixing uniformity of the melt in real time; when the system detects that the mixing effect does not meet the preset standard, the spray gun is fine-tuned according to the motion trajectory of the cyclone; for example, if it is found that the gas fails to diffuse well in the melt and accumulates in a certain area, the inclination angle or injection direction of the spray gun is appropriately adjusted to form a better combination of the gas flow and the vortex of the cyclone;
[0137] Step S223: By combining the sensor data with the control algorithm, closed-loop control is performed to automatically adjust the direction, spray angle and injection speed of the spray gun, while controlling the rotation speed of the cyclone.
[0138] Preferably, in step S221 of this embodiment, the spray direction of the spray gun is set to be consistent with the rotation direction of the cyclone, ensuring that the spray direction of the spray gun is consistent with the rotation direction of the cyclone, thereby promoting the diffusion and mixing of the gas in the melt, helping to form an effective flow field, so that the gas and the melt can contact under optimal conditions; according to the fluidity and viscosity of the melt, set the appropriate rotation speed of the cyclone to adapt to different process requirements; optimize the mixing process of gas and melt and improve the mixing efficiency; by adjusting the rotation speed of the cyclone, ensure that the system can achieve the best mixing effect under different melt states and enhance production flexibility. Step S222 real-time monitoring and fine-tuning of the spray gun, using sensors to monitor the temperature, fluidity and mixing uniformity of the melt in real time, provide first-hand feedback data, and ensure accurate grasp of the melt state; when the system detects that the mixing effect is not up to standard, it can fine-tune the spray gun according to the motion trajectory of the cyclone to optimize the interaction between gas and melt; real-time monitoring enables the system to quickly respond to changes in the melt state and ensure timely adjustment of the mixing process; by timely fine-tuning the spray gun, improve the gas distribution to make it more uniform, and improve the quality and consistency of the final product. Step S223 closed-loop control and system optimization combines sensor data with control algorithms to form a closed-loop control system that can automatically adjust the direction, spray angle and injection speed of the spray gun, and dynamically control the rotation speed of the cyclone; it can perform real-time optimization and process sensor feedback through algorithms to ensure that the system is always in the best working state; closed-loop control significantly improves the intelligence level of the system, making the mixing process of gas and melt not only automated, but also adaptive, and can maintain an ideal mixing effect under different working conditions; this dynamic optimization capability can reduce human intervention and errors, improve production efficiency and product quality, while reducing energy consumption and improving the overall economy of the system.
[0139] In summary, through the implementation of these three steps, the coordination process of the injection angle and the cyclone in this embodiment can achieve efficient gas and melt mixing, ensuring the consistency and quality of the product. Each step together constitutes a complete control and optimization system, making the entire production process more intelligent, automated and efficient.
[0140] Furthermore, the process of recording the key data of the smelting process in step S3 specifically includes the following steps:
[0141] Step S31: determine the key data indicators that need to be recorded, including temperature data: real-time temperature of the molten pool, cooling duct temperature, spray gun temperature, etc.; melt composition: chemical composition of the melt at different time points, element content, etc.; spray gun status: spray gun blowing angle, gas flow, blowing pressure and nozzle temperature, etc.; cyclone status: cyclone speed, motion mode, etc.;
[0142] Step S32: Use PLC to record and store data in real time, and set the time interval for data collection according to the frequency of changes in the smelting process; the temperature sensor automatically records the temperature changes of the molten pool and the spray gun, the flow meter records the changes in the gas flow rate, and the component analyzer monitors the chemical composition of the melt in real time and transmits the data to the data processing system;
[0143] Step S33: Set data storage rules, store the collected real-time data in the database, and perform data backup regularly; after the smelting is completed, conduct a preliminary analysis of the recorded data to identify key trends and anomalies and check the effectiveness of the smelting process; write a record report of the smelting process, including key data, operating parameters and observations.
[0144] Preferably, step S31 of this embodiment determines the key data indicators that need to be recorded, determines a complete set of monitoring indicator systems, covers all important parameters involved in the smelting process, including temperature, melt composition, spray gun state and cyclone state, and can fully grasp the dynamics of the smelting process; provides a clear framework for subsequent data collection, analysis and optimization, and ensures that all key factors are considered; a clear indicator system can help operators focus on the most important parameters during the smelting process to ensure the accuracy and consistency of production; provides a basis for data analysis, and facilitates the formulation of subsequent quality control, production optimization and improvement strategies. Step S32 uses PLC to record and store data in real time. With the help of the PLC system, real-time monitoring and recording of various parameters of the smelting process are achieved to ensure data standardization and automation; the time interval for data collection can be flexibly adjusted according to the frequency of changes in various parameters during the smelting process to ensure that sufficient details are obtained; real-time recording ensures that every change in the smelting process can be captured in time, which helps to quickly respond and adjust process parameters, avoid adverse events, improve the reliability of the production process, reduce errors in manual recording, and improve the integrity and accuracy of data. Step S33 sets data storage rules and data analysis to ensure that the collected data is stored according to systematic rules to avoid data loss and confusion. Regular backup can protect data security; by analyzing the recorded data, key trends and anomalies in the smelting process can be identified and the smelting effect can be evaluated; the systematization and backup of data provide a reliable basis for subsequent analysis and decision-making, and help to quickly restore the system in the event of a failure; preliminary data analysis and report writing are not only a summary of the smelting process, but also a guide for future improvements, promoting a culture of continuous improvement and quality improvement.
[0145] In summary, this embodiment not only realizes comprehensive and accurate monitoring and recording of key data of the smelting process through the above steps, but also promotes process optimization, quality control and production efficiency through effective data management and integration. A feedback and optimization mechanism is constructed, laying a scientific foundation for improving the product quality and productivity of enterprises.
[0146] Furthermore, the control method of the molten pool smelting accompanying flow cooling slag protection spray gun provided in this embodiment also includes: a design method of the molten pool smelting accompanying flow cooling slag protection spray gun, including: calculation of the outer wall temperature of the spray gun, acquisition of input parameters under any working condition, acquisition of interpolation under any working condition and nozzle optimization;
[0147] Among them, the calculation of the outer wall temperature of the spray gun is: first evaluate the temperature of the outer wall of the refractory material of the spray gun head without slag. It is necessary to design and match the area ratio, air volume and other parameters of the appropriate swirl layer and cooling layer to ensure that the outer wall temperature of the refractory material of the spray gun head is lower than the melting point of the melt to achieve cooling and slag. Figure 3As shown, the calculation of the temperature of the outer wall of the spray gun can be simplified to the calculation of heat transfer through the circular tube. It should be pointed out that in this calculation, the thermal resistance of the spray gun wall is ignored because the thermal resistance of the refractory material is much greater than the thermal resistance of the metal spray gun wall itself;
[0148] (1) The heat flow Φ through each link remains unchanged. For a unit length of pipeline, the temperature difference of each link can be expressed as:
[0149]
[0150] where t wi is the inner wall temperature of the tube, t wo is the outer wall temperature of the tube refractory material; t fi is the air flow temperature in the tube, t fo is the air flow temperature outside the tube; h i is the convection heat transfer coefficient in the tube, h o is the external convection heat transfer coefficient of the refractory material; d i is the inner diameter of the refractory material, d o is the outer diameter of the refractory material, and λ is the thermal conductivity of the pipe wall. Among these parameters, after the pipe structure and material are determined, d i , d o and λ are known. After the air volume, inlet temperature, furnace temperature and other parameters are determined, t fi , t fo ; According to the air volume and spray characteristics, the convection heat transfer coefficient h can be basically determined i and h o
[0151] Furthermore, for t fi , t fo ,h i and h o The evaluation can be done by numerical simulation;
[0152] Through equations 1, 2, and 3, the heat flow Φ can be obtained as:
[0153]
[0154] The temperature of the inner wall of the tube can be obtained by equations 4 and 1:
[0155]
[0156] The temperature of the outer wall of the tube can be obtained by using equation 4 and equation 3:
[0157]
[0158] (2) Under any working condition, t fi , t fo ,h i and ho Acquisition of
[0159] CFD simulation:
[0160] In the above calculation process, t fi , t fo ,h i and h o is the input parameter of the design and can be evaluated by the conjugate heat transfer numerical simulation method. In this method, the heat transfer of the jet flow field and the solid area is solved simultaneously, and the governing equation is as follows:
[0161] (1) Continuity equation:
[0162]
[0163] in is the velocity vector;
[0164] (2) Momentum conservation equation:
[0165]
[0166] Where t is time, ρ is density, is the acceleration due to gravity, P is the pressure, is the stress tensor of the Newtonian fluid, The expression is as follows:
[0167]
[0168] Where μ is the dynamic viscosity;
[0169] (3)Energy conservation equation:
[0170]
[0171] Where T is temperature, λ is thermal conductivity, c p is the specific heat capacity at constant pressure, S T is the source term;
[0172] (4) Turbulence equation
[0173] Due to the complexity of the flow field in the cooling chamber, the present invention adopts the SST k-ω turbulence model;
[0174]
[0175] Where k is the turbulent kinetic energy, ω is the specific dissipation rate, ε is the turbulent dissipation rate, v t is the turbulent kinematic viscosity, u j (j=1,2,3) are velocity components, β, σ ω2 is a closed constant; F1 is a weighting function;
[0176] like Figure 4 As shown, the specific solution process is as follows:
[0177] The solid domain and the fluid domain are three-dimensionally modeled and spatially discretized to form a grid. The grid is continuous at the interface between the solid domain and the fluid domain;
[0178] Given boundary conditions, including the flow rate Q1 of the central channel, the flow rate Q2 of the swirl channel, and the flow rates Q3 and Q4 of the peripheral sleeve ventilation; the inlet temperatures of the three channels are T1, T2, T3, and T4 respectively; the ambient temperature is 1500K; the static pressure boundary condition is given at the outlet, and the value is a standard atmospheric pressure; in order to reduce the amount of calculation, the impact pit is set as the wall surface, and the airflow will flow back when it impacts the wall surface, which is closer to the real impact melt pit, avoiding setting it to a no-slip condition, and the temperature is 1500K; the furnace wall is set to a no-slip adiabatic boundary condition;
[0179] Set up the physical model to solve the fluid flow equations (continuity equation and momentum equation), energy equation, turbulence equation and transient heat conduction equation in the solid domain;
[0180] Given the physical properties of fluid and solid, the ideal gas state equation is used to solve the gas phase density; the viscosity, specific heat capacity and heat transfer coefficient of the gas phase are solved using linear interpolation functions; given the specific heat capacity and thermal conductivity of the refractory material;
[0181] Initialize flow field,calculation;
[0182] Process the calculation results and extract t from the results fi , t fo ,h i and h o ;
[0183] Change the inlet conditions Q1, Q2, Q3, Q4, T1, T2, T3, T4, refractory thickness δ, repeat the above steps to obtain t under different working conditions fi , t fo ,h i and h o , forming a database.
[0184] (3)(1) Initialization: fill all missing values with mean, median, and random sampling to obtain a complete initial data set;
[0185] (2) Iteration: Multiple iterations are performed, and each iteration interpolates one or more variables containing missing values. In each iteration, for each variable Y containing missing values, i , use a prediction model to estimate the missing value Y based on the other complete variables Xi i ;
[0186] (3) Multiple iterations: Repeat the iteration until the convergence condition is met, when the interpolation results of several consecutive iterations do not change much, or when the preset maximum number of iterations is reached;
[0187] (4) Integration: After all iterations are completed, the interpolation results obtained in each iteration are integrated, and the average of multiple interpolation results is taken for each missing value;
[0188] The estimation process of MICE is represented by mathematical symbols:
[0189] For the imputation of the i-th variable, assume that the variable with missing values is Y i , the complete set of variables is X, where Xi represents the removal of Y i A set of variables;
[0190] The prediction model is expressed as follows: Yi = f(Xi) + ε i Among them, f is a prediction function, ε i is the error term;
[0191] For each iteration, the missing values are estimated using the prediction model, and then the missing values in the data set are updated. After multiple iterations, multiple complete data sets are obtained, and the final estimated value is finally obtained by integrating the results of these data sets.
[0192] (4) Nozzle optimization design
[0193] Variable parameters of nozzle design include:
[0194] Geometric parameters: center layer spray gun diameter d1, swirl layer diameter d2, cooling layer diameter d3 and outermost channel wind diameter d4, refractory material thickness δ;
[0195] Operation parameters: central layer blowing flow rate Q1, swirl layer flow rate Q2, cooling layer flow rate Q3, and outermost layer flow rate Q4, as well as the blowing temperatures T1, T2, T3, T4 of each layer from the inside to the outside;
[0196] By interpolating the database in the second step, we can obtain t under different geometric parameters and operating conditions. fi , t fo ,h i and h o , combined with formula (4) and formula (6), the temperature of the outer wall of the refractory under the corresponding working conditions can be obtained. The lower the temperature, the more conducive to slag hanging.
[0197] Preferably, the temperature calculation of the outer wall of the spray gun in this embodiment, the stability of the heat flow: by analyzing the invariance of the heat flow of the link, the temperature state of the spray gun head can be accurately evaluated. This provides a basis for the subsequent optimization of the spray gun design and operating parameters; simplify the heat transfer model: by ignoring the thermal resistance of the spray gun wall, the complexity of the heat conduction model is simplified, making the calculation more efficient and faster; through reasonable temperature control, the slag phenomenon of the spray gun head can be effectively prevented, the service life and stability of the spray gun can be improved, which helps to reduce maintenance costs and improve production efficiency; accurately estimating the spray gun temperature is crucial to optimizing the cooling and air injection strategies during the smelting process to ensure safe production.
[0198] Application of CFD simulation technology, multi-physics coupling analysis: Through numerical simulation of conjugate heat transfer between fluid and solid, comprehensive consideration of fluid flow, temperature field and turbulence effect, a comprehensive simulation analysis is achieved; Accurate boundary condition setting: Combining the physical models of fluid and solid domains, using different flow and temperature conditions, the simulation results are closer to the actual working conditions, which can predict the performance of the spray gun and its cooling system in the design stage, reduce the trial and error cost in actual operation, and shorten the development cycle; greatly improve the accuracy and efficiency of process optimization, and provide a scientific basis for the design and improvement of the spray gun. Data interpolation and estimation method Efficient data utilization: Through the MICE algorithm to interpolate missing data, sufficient information can be obtained on limited computing resources, reducing the computing burden; Systematic information acquisition: Multiple rounds of iteration and integration improve the reliability of data, thereby maintaining the prediction accuracy of the model under different working conditions; Through interpolation technology, the temperature and missing parameters can be quickly calculated between multiple working conditions, providing key decision support for designers and engineers; Filling data gaps with scientific methods helps to form a comprehensive database, thus providing a data basis for subsequent research and engineering applications. Comprehensive effect of spray gun optimization design Multi-parameter interactive impact evaluation: can comprehensively analyze the impact of geometric parameters and operating parameters on spray gun performance and optimize the design scheme; Design under low temperature environment: through the data obtained from the database, ensure that the temperature of the outer wall of the spray gun is controlled, thereby minimizing the possibility of slag hanging; improve the adaptability and stability of the spray gun, make the smelting process more efficient and safe, and help improve the overall production efficiency; Optimizing the spray gun design can not only reduce operating costs, but also provide higher production quality, which will win the company an advantage in market competition.
[0199] like Figure 5 As shown, the stirring area is compared (a) without rotation; (b) with rotation; Figure 6 As shown, the splash volume comparison.
[0200] In summary, the whole process of this embodiment forms an interconnected system through calculation and simulation, data analysis and interpolation, spray gun design and optimization. It aims to achieve efficient, safe and economical operation of the smelting process. Through this systematic method, not only the controllability and reliability of the production process are improved, but also a scientific basis and data support are provided for the long-term development of enterprises.
[0201] like Figure 7 As shown, this embodiment provides an embodiment of an electronic device. In this embodiment, the electronic device 13 includes a processor 131 and a memory 132 coupled to the processor 131. The memory 132 stores program instructions for implementing the control method of the molten pool smelting accompanying flow cooling slag protection spray gun of any of the above embodiments. The processor 131 is used to execute the program instructions stored in the memory 132 to design the molten pool smelting accompanying flow cooling slag protection spray gun. Among them, the processor 131 can also be called a CPU (Central Processing Unit). The processor 131 may be an integrated circuit chip with signal processing capabilities. The processor 131 can also be a general-purpose processor, a digital signal processor (DSP), an application-specific integrated circuit (ASIC), a field programmable gate array (FPGA) or other programmable logic devices, discrete gates or transistor logic devices, discrete hardware components. The general-purpose processor can be a microprocessor or the processor can also be any conventional processor, etc.
[0202] Further, Figure 8 The schematic diagram of the structure of the storage medium of an embodiment of the present application is that the storage medium 14 of the embodiment of the present application stores program instructions 141 that can implement all the above methods, wherein the program instructions 141 can be stored in the above storage medium in the form of a software product, including several instructions for enabling a computer device (which can be a personal computer, server, or network device, etc.) or a processor to execute all or part of the steps of the methods described in each embodiment of the present application. The aforementioned storage medium includes: various media that can store program codes, such as a USB flash drive, a mobile hard disk, a read-only memory (ROM), a random access memory (RAM), a magnetic disk or an optical disk, or terminal devices such as a computer, a server, a mobile phone, and a tablet.
[0203] In the several embodiments provided by the present invention, it should be understood that the disclosed systems, devices and methods can be implemented in other ways. For example, the device embodiments described above are only schematic, for example, the division of units is only a logical function division, and there may be other division methods in actual implementation, such as multiple units or components can be combined or integrated into another system, or some features can be ignored or not executed. Another point, the mutual coupling or direct coupling or communication connection shown or discussed can be through some interfaces, indirect coupling or communication connection of devices or units, which can be electrical, mechanical or other forms. In addition, each functional unit in each embodiment of the present invention can be integrated into a processing unit, or each unit can exist physically separately, or two or more units can be integrated into one unit. The above integrated unit can be implemented in the form of hardware or in the form of software functional units. The above is only an embodiment of the present invention, and does not limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made by using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
[0204] The specific implementation methods of the invention are described in detail above, but they are only examples, and the invention is not limited to the specific implementation methods described above. For those skilled in the art, any equivalent modification or substitution of the invention is also within the scope of the invention, therefore, the equalization, modification, improvement, etc. made without departing from the spirit and principle of the invention should be included in the scope of the invention.
Claims
1. A slag protection spray gun for cooling with accompanying flow in molten pool smelting, characterized in that: The molten pool smelting accompanying flow cooling slag protection spray gun comprises: at least 3 layers of channels; the central channel is used for pure gas phase or gas-solid mixed spraying; the swirl spraying layer is equipped with swirl blades for generating most of the spraying kinetic energy to stir the melt and provide oxygen for the central layer fuel; the cooling air duct is used to generate cooling swirl to promote the nozzle immersed in the melt to generate cooling slag; A swirl spray layer is arranged outside the central channel, the swirl spray layer is equipped with swirl blades, swirlers are arranged in the swirl spray channel and cooling air duct of the swirl spray layer, and a cooling air duct is arranged outside the swirl spray layer.
2. The molten pool smelting accompanying flow cooling slag protection spray gun according to claim 1, characterized in that: The outer layer of the nozzle is arranged with a refractory material layer; cyclones are installed in the swirl injection channel and the cooling air duct, and the swirl expands the stirring radius.
3. The molten pool smelting accompanying flow cooling slag protection spray gun according to claim 1, characterized in that: A refractory material layer is arranged on the outer side of the bottom end of the cooling air duct, and a slag layer is arranged on the outer side of the refractory material layer; a mixing zone is arranged at the lowest end of the central channel, an impact pit is arranged below the mixing zone, a free surface layer is arranged on the right side of the impact pit, and a melt is arranged on the left side; the free surface layer, the impact pit and the melt are arranged inside the molten pool wall.
4. The molten pool smelting accompanying flow cooling slag protection spray gun according to claim 1, characterized in that: The outermost channel is a sleeve ventilation channel, and a sleeve ventilation channel is arranged outside the cooling air channel; Protect the fluid in the cooling air duct from being heated by the high-temperature molten pool and strengthen the cooling at the nozzle.
5. A method for designing a slag protection spray gun for cooling a molten pool smelting accompanying flow, which is applied to the slag protection spray gun for cooling a molten pool smelting accompanying flow as claimed in any one of claims 1 to 4, characterized in that: The method for designing a slag protection spray gun for accompanying flow cooling during molten pool smelting comprises: calculating the temperature of the outer wall of the spray gun, obtaining input parameters under any working condition, obtaining interpolation values under any working condition and optimizing the nozzle.
6. The method for designing a slag protection spray gun for accompanying flow cooling in molten pool smelting according to claim 5, characterized in that: The calculation of the temperature of the outer wall of the spray gun is the heat transfer calculation through the circular tube, including: the heat flow Φ through each link is constant, and for a unit length of the pipeline, the temperature difference of each link is expressed as: where t wi is the inner wall temperature of the tube, t wo is the outer wall temperature of the tube refractory material; t fi is the air flow temperature in the tube, t fo is the air flow temperature outside the tube; h i is the convection heat transfer coefficient in the tube, h o is the external convection heat transfer coefficient of the refractory material; d i is the inner diameter of the refractory material, d o is the outer diameter of the refractory material, λ is the thermal conductivity of the tube wall; The evaluation of input parameters under any working condition adopts the method of numerical simulation, and the heat flow Φ is obtained as: Get the temperature of the inner wall of the tube: Get the temperature of the outer wall of the tube: Under any working condition t fi , t fo ,h i and h o The acquisition of is evaluated by the conjugate heat transfer numerical simulation method, and the heat transfer of the injection flow field and the solid area is solved at the same time. The control equation is as follows: Continuity equation: in is the velocity vector; Momentum conservation equation: Where t is time, ρ is density, is the acceleration due to gravity, P is the pressure, is the stress tensor of the Newtonian fluid, The expression is as follows: Where μ is the dynamic viscosity; Energy conservation equation: Where T is temperature, λ is thermal conductivity, c p is the specific heat capacity at constant pressure, S T is the source term; Turbulence equations The SST k-ω turbulence model is used; Where k is the turbulent kinetic energy, ω is the specific dissipation rate, ε is the turbulent dissipation rate, v t is the turbulent kinematic viscosity, u j is the velocity component, j=1,2,3,β,σ ω2 is a closed constant; F1 is a weighting function.
7. The method for designing a slag protection spray gun for accompanying flow cooling in molten pool smelting according to claim 6, characterized in that: The specific solution process includes: The solid domain and the fluid domain are three-dimensionally modeled and spatially discretized to form a grid; the grid is continuous at the interface between the solid domain and the fluid domain; Given boundary conditions, including the flow rate Q1 of the central channel, the flow rate Q2 of the swirl channel, and the flow rates Q3 and Q4 of the peripheral sleeve ventilation; the inlet temperatures of the three channels are T1, T2, T3, and T4 respectively; the ambient temperature is 1500K; the static pressure boundary condition is given at the outlet, and the value is a standard atmospheric pressure; the impact pit is set as the wall surface, and the airflow will flow back when it impacts the wall surface, which is closer to the real impact melt pit, and the temperature is 1500K; the furnace wall is set to a no-slip adiabatic boundary condition; Set up the physical model to solve the continuity and momentum equations, energy equations, turbulence equations, and transient heat conduction equations in the solid domain; Initialize flow field,calculation; Process the calculation results and extract t from the results fi , t fo ,h i and h o ; Change the inlet conditions Q1, Q2, Q3, Q4, T1, T2, T3, T4, refractory thickness δ, repeat the above steps to obtain t under different working conditions fi , t fo ,h i and h o , forming a database; The interpolation of any load case adopts the following steps: (1) Initialization: fill all missing values with mean, median, and random sampling to obtain a complete initial data set; (2) Iteration: Multiple iterations are performed, and each iteration interpolates one or more variables containing missing values. In each iteration, for each variable Y containing missing values, i , use a prediction model to estimate the missing value Y based on the other complete variables Xi i ; (3) Multiple iterations: Repeat the iteration until the convergence condition is met, when the interpolation results of several consecutive iterations do not change much, or when the preset maximum number of iterations is reached; (4) Integration: After all iterations are completed, the interpolation results obtained in each iteration are integrated, and the average of multiple interpolation results is taken for each missing value; The estimation process of MICE is represented by mathematical symbols: For the imputation of the i-th variable, assume that the variable with missing values is Y i , the complete set of variables is X, where Xi represents the removal of Y i A set of variables; The prediction model is expressed as follows: Yi = f(Xi) + ε i Among them, f is a prediction function, ε i is the error term; For each iteration, the missing values are estimated using the prediction model, and then the missing values in the data set are updated; after multiple iterations, multiple complete data sets are obtained, and finally the final estimated value is obtained by integrating the results of the data sets; Nozzle optimization design, variable parameters include: Geometric parameters: center layer spray gun diameter d1, swirl layer diameter d2, cooling layer diameter d3 and outermost channel wind diameter d4, refractory material thickness δ; Operation parameters: central layer spray flow rate Q1, swirl layer flow rate Q2, cooling layer flow rate Q3, and outermost layer flow rate Q4, as well as the blowing temperatures T1, T2, T3, T4 of each layer from the inside to the outside; The t value under different geometric parameters and operating conditions is obtained through the interpolation database class. fi , t fo ,h i and h o , combined with the formula and formula Get the temperature of the outer wall of the refractory material under the corresponding working conditions.
8. A method for controlling a slag protection spray gun for cooling a molten pool smelting accompanying flow, which is applied to a slag protection spray gun for cooling a molten pool smelting accompanying flow as claimed in any one of claims 1 to 4, characterized in that: The control method for slag protection spray gun during molten pool smelting accompanying flow cooling comprises: Open the air flow of the cooling air duct and start the spraying system of the central channel to spray out the gas mixture; adjust the air flow of the central channel to achieve oxygen supply and spraying kinetic energy; Adjust the spraying angle and position of the spray gun according to the melt state and target mixing effect; use thermal imaging or temperature detection instruments to monitor the melt pool temperature; adjust the movement state of the cyclone according to the melt state; After smelting is completed, gradually reduce the gas flow until the blowing and cooling process stops; keep the cooling air duct ventilated; after smelting is completed, check and clean the spray gun and its channel; record key data of the smelting process, including temperature, melt composition and spray gun status.
9. The method for controlling the slag protection spray gun during the cooling of the accompanying flow of molten pool smelting according to claim 8, characterized in that: The process of controlling the air flow in the central channel includes: Use a flow meter to monitor the gas flow and pressure, install a flow regulating valve in the gas delivery pipeline, and change the gas flow by adjusting the servo valve opening; Set the gas flow parameters according to the temperature of the molten pool, the properties of the melt and the required mixing effect; monitor the gas flow and molten pool temperature through flow sensors, temperature sensors and vortex meters installed on the spray gun and the molten pool, and input the data into the control system; According to the deviation between the actual airflow and the set airflow, fuzzy processing is performed to convert the input variable into a fuzzy value; a fuzzy rule is established, which contains the numerical value of the increase or decrease of the airflow corresponding to the deviation; the fuzzy reasoning mechanism is used to obtain the fuzzy output through combination and association rules based on the fuzzy input and rule base; the fuzzy output is converted into a control quantity, and the opening of the airflow control valve is adjusted according to the defuzzification result.
10. The method for controlling the slag protection spray gun during the cooling of the accompanying flow of molten pool smelting according to claim 8, characterized in that: The process of adjusting the spray angle and position of the spray gun includes: Adjust the vertical and horizontal positions of the spray gun according to the state of the melt; Select the injection angle according to the required gas mixing ratio and the temperature and fluidity of the melt; coordinate with the movement of the cyclone to promote mixing; Monitor the temperature and fluidity of the melt, as well as the mixing uniformity in real time, and keep records of each adjustment of the spray angle, spray gun position and melt state parameters.
Citation Information
Cited By
Reducing atmosphere detection adjusting system and adjusting method for high-manganese-content manganese-silicon alloy
CN119860665A