Casting system and casting head for feeding differential shell

By using structures such as flow blocking seats and flow blocking bosses in the casting system of the transmission case, and combining with the pouring riser unit to extend the solidification time of the riser, the problem of uneven solidification of the metal liquid is solved. , significantly improve product quality and production rate.

CN118926484APending Publication Date: 2024-11-12HENAN AOUDI CD LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411051394.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-01
Publication Date
2024-11-12

AI Technical Summary

Technical Problem

During the casting of existing gearbox shells, the mixing of dirty slags of metal liquid leads to poor quality of products after solidification, and the pouring riser structure is too simple to lead to unbalanced solidification, which is prone to defects in shrinking the lock hole.

Method used

A casting system and pouring riser for differential housing are designed. By setting up a flow blocking seat and a flow blocking boss, the flow blocking speed is delayed, and the residue is floated up and collected through the slag collecting package, and the flow blocking port is blocked. Slow down the flow rate of metal liquid, ensure the purity of metal liquid, and extend the solidification time of the riser through the pouring unit to reduce heat loss.

Benefits of technology

It effectively improves the purity of the metal liquid and casting quality, reduces the defects of the shrinkage keyhole, extends the solidification time of the riser, and improves the density and yield of the workpiece.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118926484A_ABST
    Figure CN118926484A_ABST
Patent Text Reader

Abstract

The invention relates to the technical field of differential shell casting, and discloses a casting system and a casting head for feeding of a differential shell, the other end of a cross gate is communicated with a first slag collecting ladle, and a flow blocking seat is fixed to the bottom of the side, close to a straight gate, of an inner cavity of the cross gate; a flow choking boss staggered with the flow choking seat is fixed to the top of an inner cavity of the cross gate, the side wall of the cross gate communicates with an inner gate formed in the lower casting mold seat, a casting mold cavity is formed in the lower casting mold seat, and a flow choking opening is formed in the communicating position of the inner gate and the casting mold cavity; a second slag collecting bag is arranged at the position, corresponding to the flow blocking opening, of the bottom of the upper casting mold base, and a casting head unit is fixedly installed at the position, corresponding to the casting head, of the upper casting mold base, so that impure slag can be stored through the first slag collecting bag, and follow-up guided-in molten metal is clean; the flowing speed of molten metal in the ingate can be effectively slowed down, and the casting quality of workpieces is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of differential case casting, and in particular to a casting system and a casting riser for shrinkage compensation of a differential case. Background Art

[0002] The gearbox housing in current technology has become a product with very high quality requirements due to its special structure and the inherent requirements of its own use function. In order to speed up the production speed, a casting molding process is generally used to manufacture such products. In the casting pouring system of the gearbox housing in the prior art, dirty slag of the molten metal is mixed in the molten metal, which will cause the gearbox housing after solidification to have problems such as poor quality.

[0003] In a casting pouring system of a gearbox housing with application number 202210579564.X, a first riser part and a second riser part are connected to a casting mold, and a gas outlet part and a waste liquid discharge channel are connected to the casting mold. The present invention filters the molten metal by setting a molten metal purifier, thereby avoiding problems such as poor quality of the gearbox housing after solidification.

[0004] During casting, risers are used for venting, shrinkage compensation, and slag collection in order to compensate for the shrinkage generated during gradual solidification to prevent the defects of shrinkage lock holes. However, the structure of the pouring and rising heads used on the market is too simple, and shrinkage compensation agents are usually covered at the risers to reduce the efficiency of heat loss. However, in actual use, the casting material at the pouring and rising heads cools faster during the casting process, resulting in uneven solidification, making the solidification time of the risers earlier than the solidification time of the molten metal in the cavity. It is easy to form a closed solidified crust at the risers, so that the displacement effect of the atmospheric pressure disappears. Since there is no shrinkage compensation, shrinkage lock holes will appear when the molten metal solidifies, which greatly reduces the quality of the product after molding and has poor practicality.

[0005] Therefore, the present invention solves the above problems through a casting system and a casting riser for shrinkage compensation of a differential housing. Summary of the invention

[0006] The object of the present invention is to provide a casting system and a casting riser for shrinkage compensation of a differential housing, so as to solve the problems raised in the above background technology.

[0007] To achieve the above-mentioned object, the present invention provides the following technical solutions: a casting system for differential housing shrinkage compensation, comprising a matching lower mold base and an upper mold base, wherein a sprue is provided in the upper mold base, the top of the sprue is equipped with a pouring cup, the lower mold base is provided with a buffer groove arranged at the bottom of the sprue, a cross runner is provided between the lower mold base and the upper mold base, the other end of the cross runner is connected to a first slag collecting bag, and the bottom of the inner cavity of the cross runner close to the sprue is solidified. A baffle seat is fixed thereon, a baffle boss staggered with the baffle seat is fixed on the top of the inner cavity of the cross runner, an endocastor opened on the lower mold seat is connected on the side wall of the cross runner, a casting mold cavity is opened in the lower mold seat, a baffle port is opened at the connection between the endocastor and the casting mold cavity, a second slag collecting bag is opened at the corresponding position of the bottom of the upper mold seat and the baffle port, risers are set at the corresponding positions of the upper mold seat and the casting mold cavity, and a pouring and riser unit is fixedly installed at the corresponding riser position on the upper mold seat.

[0008] Preferably, the casting mold cavity comprises a lower cavity opened on the lower casting mold seat and an upper cavity opened on the bottom of the upper casting mold seat, and the riser is opened on the top of the upper casting mold seat, and the riser is communicated with the upper cavity.

[0009] Preferably, the ratio of the height of the sprue, the length of the runner and the length of the ingates is 4:8:3.

[0010] Preferably, the height position of the ingrate is set at 1 / 3 of the height of the cross runner, the aperture of the ingrate is 1 / 4 of the aperture of the cross runner, and the top of the ingrate is flush with the bottom of the upper mold seat.

[0011] Preferably, the aperture of the blocking port is 1 / 4-1 / 3 of the aperture of the endogate, and the blocking port is an upwardly inclined arc-shaped spoiler port, the second slag collecting bag is directly opposite to the arc-shaped surface of the blocking port, and the arc-shaped surface of the blocking port is convex.

[0012] Preferably, the height of the baffle seat is 1 / 3 of the height of the cross runner, the surface of the baffle seat is an arc-shaped surface, the height of the baffle boss is 1 / 3 of the height of the cross runner, the bottom of the baffle boss is set as a serrated guide tooth, and the inclination angle of the guide tooth gradually decreases from the outside to the inside, and the direction of the guide tooth is the center line direction of the cross runner.

[0013] The present invention provides a casting riser for shrinkage compensation of a differential housing, comprising a casting riser unit;

[0014] The pouring and riser unit includes a riser seat fixedly mounted on the top of the upper mold seat and corresponding to the riser position, a conical riser piece is plugged and assembled on the top of the riser seat, a heat preservation cavity is opened in the riser piece, three groups of shrinkage units with the same structure are slidably assembled on the inner side wall of the riser piece, and the size of a single group of shrinkage units and the riser piece are adapted.

[0015] Preferably, the shrinkage compensation unit includes a slideway opened on the inner wall of the riser part, a slide seat is slidably installed in the slideway, a pressure spring is fixedly connected between the bottom of the slide seat and the inner wall of the slideway, a guide seat is fixedly connected to the outer wall of the slide seat, and a "bowl"-shaped supporting seat is integrally formed at the bottom of the guide seat.

[0016] Preferably, a guide port is provided at the end of the supporting seat, and an assembly gap is provided between two adjacent groups of the feeding units, and a moving gap is reserved between a single group of the feeding units and the inner side wall of the riser member.

[0017] Technical effects and advantages of the present invention:

[0018] 1. The use of the baffle seat in the present invention can slow down the flow rate of the molten metal, and by reducing the cross-section of the runner, the slag in the molten metal can be caused to float to the top of the molten metal, which has the effect of filtering the slag. At the same time, the baffle boss can block the flowing molten metal, so that the slag on the surface of the molten metal can be blocked by the baffle boss to slow down its flow rate. The length of the runner is relatively long, so that the slag can be given enough time to float to the surface of the molten metal. In this way, when the molten metal flows inside the runner, the slag floats to the top of the runner, while the molten metal below has a high purity, which is more conducive to being introduced into the casting mold cavity through the inner runner for casting.

[0019] 2. In the present invention, when the molten metal flows in the runner, the floating slag will be introduced into the first slag bag along the runner for centralized collection, so that the slag remaining on the surface of the molten metal just introduced can be diverted and collected, and the impure slag can be stored through the first slag bag, so that the impurities in the molten iron will not come out. The purity of the molten metal that is continuously introduced is very high, and the molten metal that is introduced subsequently is clean and can be smoothly introduced into the casting mold cavity through the inner runner.

[0020] 3. The reduction in the aperture of the baffle in the present invention can significantly slow down the speed at which the molten metal flows into the casting mold cavity, thereby improving the uniformity of the texture of the molten metal. In addition, the setting of the baffle can make the molten metal in the ingrowth channel in a flooded state, thereby slowing down the flow speed of the molten metal in the ingrowth channel, thereby increasing the time for impurities in the molten metal to float up. At the same time, when the molten metal flows through the baffle, the molten metal has an upward flow potential, thereby enabling the impurities floating on the top of the molten metal to enter the second slag bag, thereby achieving the purpose of secondary cleaning, further improving the purity of the molten metal when entering the casting mold cavity, and improving the quality of the workpiece casting mold.

[0021] 4. The pouring and riser unit in the present invention has a long heat preservation time for the riser and a long heating duration, which can greatly extend the solidification time of the riser, so that the oxides, inclusions and gases in the cavity have sufficient time to float into the riser, thereby improving the process yield. It can also enhance the solidification delay effect of the riser, and can significantly reduce the size of the riser, thereby increasing the utilization rate of the molten metal. Combined with the pressure, the molten metal is pressed into the casting, thereby improving the density of the casting and reducing the possibility of leakage during the pressure test of the casting. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of the overall structure of the present invention;

[0023] Figure 2 It is a schematic diagram of the overall cross-sectional structure of the present invention;

[0024] Figure 3 It is a schematic diagram of the overall longitudinal cross-sectional structure of the present invention;

[0025] Figure 4 It is a schematic diagram of a partial cross-sectional structure of the present invention;

[0026] Figure 5 This is a schematic diagram of the structure of the lower mold base of the present invention;

[0027] Figure 6 It is a schematic diagram of the structure of the upper mold base of the present invention;

[0028] Figure 7 It is a schematic diagram of the overall transverse cross-sectional structure of the present invention;

[0029] Figure 8 It is a schematic diagram of the enlarged structure of part A of the present invention;

[0030] Fig. 9 It is a schematic diagram of the enlarged structure of part B of the present invention;

[0031] Fig.10 This is a schematic diagram of the structure of the pouring and riser unit of the present invention;

[0032] Fig.11 It is a schematic diagram of the feeding unit structure of the present invention.

[0033] In the figure: 1, lower mold base; 2, upper mold base; 3, sprue; 4, pouring cup; 5, buffer groove; 6, runner; 7, first slag bag; 8, baffle seat; 9, baffle boss; 10, inner runner; 11, casting mold cavity; 111, lower cavity; 112, upper cavity; 12, baffle port; 13, second slag bag; 14, riser seat; 15, riser piece; 16, insulation cavity; 17, shrinkage compensation unit; 171, slide seat; 172, pressure spring; 173, guide seat; 174, support seat; 18, riser. DETAILED DESCRIPTION

[0034] The technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.

[0035] Embodiment 1:

[0036] This embodiment provides Figures 1 to 8 The casting system for differential housing shrinkage compensation shown in the figure comprises a matching lower mold base 1 and an upper mold base 2, a sprue 3 is provided in the upper mold base 2, a pouring cup 4 is provided on the top of the sprue 3, a buffer tank 5 is provided at the bottom of the sprue 3 on the lower mold base 1, a horizontal runner 6 is provided between the lower mold base 1 and the upper mold base 2, a first slag collecting bag 7 is provided at the other end of the horizontal runner 6, and a slag collecting bag 7 is provided at the bottom of the inner cavity of the horizontal runner 6 near the sprue 3. A baffle seat 8 and a baffle boss 9 are fixed on the top of the inner cavity of the cross runner 6, which are staggered with the baffle seat 8. The side wall of the cross runner 6 is connected with an endocasting channel 10 opened on the lower mold seat 1. A casting mold cavity 11 is opened in the lower mold seat 1. A baffle port 12 is opened at the connection between the endocasting channel 10 and the casting mold cavity 11. A second slag bag 13 is opened at the bottom of the upper mold seat 2 and the corresponding position of the baffle port 12. A riser 18 is set at the corresponding position of the upper mold seat 2 and the casting mold cavity 11.

[0037] After the lower mold base 1 and the upper mold base 2 are installed, they can provide better sealing for the mold cavity 11. When the molten metal is introduced into the sprue 3 through the pouring cup 4, the molten metal will first be collected in the buffer tank 5 to achieve buffering when the molten metal falls, and then flow into the runner 6. In this process, the buffer tank 5 slows down the flow rate of the molten metal. At the same time, the use of the upper baffle 8 can delay the flow rate of the molten metal, and the slag in the molten metal is caused to float to the metal by reducing the cross section of the runner 6. The slag is above the molten metal, which has the effect of filtering the slag. At the same time, the flow-blocking boss 9 can block the flowing molten metal. In this way, the slag on the surface of the molten metal can be blocked by the flow-blocking boss 9 to slow down its flow speed. The length of the runner 6 is relatively long, which can give the slag enough time to float to the surface of the molten metal. In this way, when the molten metal flows inside the runner 6, the slag floats to the top of the runner 6, while the molten metal below has a high purity, which is more conducive to being introduced into the casting mold cavity 11 through the inner runner 10 for casting.

[0038] It should be noted that the height of the baffle seat 8 is 1 / 3 of the height of the runner 6, the surface of the baffle seat 8 is an arc-shaped surface, the height of the baffle boss 9 is 1 / 3 of the height of the runner 6, the bottom of the baffle boss 9 is set as a serrated guide tooth, and the inclination angle of the guide tooth gradually decreases from the outside to the inside, and the direction of the guide tooth is the center line direction of the runner 6. In the process of the baffle boss 9 blocking the slag, the molten metal can be disturbed, so that the liquid and slag on the surface of the molten metal are concentrated in the middle position of the molten metal as the molten metal flows. This can avoid the slag from flowing against the side wall of the runner 6 during the flow, so as to prevent the hidden danger of slag entering the inner runner 10. It has a guiding effect on the slag and improves the purity of the molten metal.

[0039] It is worth mentioning that the ratio of the height of the straight channel 3, the length of the cross runner 6 and the length of the ingrowth 10 is 4:8:3. When the slag flows with the molten metal in the cross runner 6, the height of the molten metal is higher than the ingrowth 10. Therefore, the slag cannot be introduced into the casting mold cavity 11 through the ingrowth 10, thereby ensuring the quality of the casting mold and avoiding the defects of uneven texture of the casting mold and sand holes. At the same time, when the molten metal flows in the cross runner 6, the floating slag will be introduced into the first slag bag 7 along the cross runner 6 for centralized collection, so that the slag remaining on the surface of the molten metal that has just been introduced can be diverted and collected, and the impure slag can be stored through the first slag bag 7, so that impurities in the molten iron cannot come out. The purity of the molten metal that is continuously introduced is very high, and the molten metal that is introduced subsequently is clean and can be smoothly introduced into the casting mold cavity 11 through the ingrowth 10.

[0040] It is worth noting that the height position of the ingrowth 10 is set at 1 / 3 of the height of the cross runner 6, the aperture of the ingrowth 10 is 1 / 4 of the aperture of the cross runner 6, and the top of the ingrowth 10 is flush with the bottom of the upper mold base 2. When the molten metal flows into the ingrowth 10, since the aperture of the cross runner 6 is larger than the aperture of the ingrowth 10, the four groups of ingrowths 10 are used to synchronously divert the molten metal in the cross runner 6, so that the flow rate of the molten metal flowing into the ingrowth 10 is reduced. In this way, the flow rate of the molten metal flowing from the cross runner 6 to the ingrowth 10 can be reduced, and at the same time, the casting speed of the molten metal can also be reduced to avoid sand washing and other phenomena.

[0041] See also Figure 5-Figure 7 The casting mold cavity 11 includes a lower mold cavity 111 opened on the lower mold base 1 and an upper mold cavity 112 opened at the bottom of the upper mold base 2, and the riser 18 is opened on the top of the upper mold base 2, and the riser 18 is connected to the upper mold cavity 112, and the molten metal through the inner runner 10 will be directly introduced into the lower mold cavity 111, and then the casting mold cavity 11 will be filled with the continuous inflow of the molten metal.

[0042] See also Figure 7-Figure 8 The aperture of the blocking port 12 is 1 / 4-1 / 3 of the aperture of the ingrowth channel 10, and the blocking port 12 is an upwardly inclined arc-shaped spoiler port, the second slag collecting bag 13 is directly opposite to the arc-shaped surface of the blocking port 12, and the arc-shaped surface of the blocking port 12 is a convex surface. In the process of the molten metal flowing from the ingrowth channel 10 to the casting mold cavity 11, the reduction of the aperture of the blocking port 12 can greatly slow down the speed of the molten metal flowing into the casting mold cavity 11, and improve the texture uniformity of the molten metal. Moreover, the setting of the blocking port 12 can make the molten metal in the ingrowth channel 10 in a flooded state, which can slow down the flow speed of the molten metal in the ingrowth channel 10, thereby increasing the time for impurities in the molten metal to float up. At the same time, when the molten metal flows through the blocking port 12, the molten metal has an upward flow potential energy, so that the impurities floating on the top of the molten metal can enter the second slag collecting bag 13, so as to achieve the purpose of secondary cleaning, further improve the purity of the molten metal when entering the casting mold cavity 11, and improve the quality of the workpiece casting mold.

[0043] Embodiment 2:

[0044] This embodiment discloses a pouring and rising head for shrinkage compensation of a differential housing, including a pouring and rising head unit, and the pouring and rising head unit is fixedly mounted on the upper mold base 2 at a position corresponding to the riser 18, and the pouring and rising head unit is used to perform shrinkage compensation operation on the workpiece in the mold cavity 11, thereby improving the mold quality of the workpiece to prevent the occurrence of shrinkage and shrinkage defects, specifically:

[0045] Please refer to 7- Fig.11The pouring and rising unit includes a riser seat 14 fixedly mounted on the top of the upper mold seat 2 and corresponding to the position of the riser 18. A conical riser piece 15 is plugged and assembled on the top of the riser seat 14. A heat preservation cavity 16 is provided in the riser piece 15. Three groups of shrinkage units 17 with the same structure are slidably assembled on the inner side wall of the riser piece 15. The size of a single group of shrinkage units 17 is adapted to that of the riser piece 15. The size of the riser seat 14 matches that of the riser 18. The riser piece 15 is engaged with the riser seat 14 to facilitate the disassembly and assembly of the riser piece 15. In the actual casting operation, after the introduction of the molten metal is completed, a riser shrinkage agent needs to be added to the riser piece 15 to achieve the effect of heat preservation of the molten metal. In this way, the shrinkage agent will cover the riser 18. At the same time, The feeding agent is accumulated on the feeding unit 17, so that the heat loss efficiency of the molten metal is reduced by using the feeding agent, and the heat preservation chamber 16 can greatly slow down the heat dissipation, which can greatly extend the solidification time of the riser 18, so that the oxides, inclusions and gases in the casting mold cavity 11 have enough time to float to the riser 18, so as to achieve the purpose of impurity removal and improve the process yield. The existence of the feeding unit 17 can pressurize the feeding agent to prevent the molten metal from being directly exposed to the air due to the lack of feeding agent during the exhaust process, which will accelerate the cooling of the molten metal and easily produce shrinkage and shrinkage holes. Therefore, the feeding agent is limited by the feeding unit 17 to slow down the heat dissipation efficiency of the molten metal.

[0046] See also Fig.10 and 11 The feeding unit 17 includes a slideway provided on the inner wall of the riser 15, a slide seat 171 is slidably mounted in the slideway, a pressure spring 172 is fixedly connected between the bottom of the slide seat 171 and the inner wall of the slideway, a flow guide seat 173 is fixedly connected to the outer wall of the slide seat 171, a "bowl"-shaped support seat 174 is integrally formed at the bottom of the flow guide seat 173, a flow guide port is provided at the end of the support seat 174, and an assembly gap is provided between two adjacent groups of feeding units 17, and a moving gap is reserved between a single group of feeding units 17 and the inner wall of the riser 15. When the feeding agent is placed inside the riser 15, it will naturally fill the assembly gap between the two adjacent groups of feeding units 17. In the gap and the moving gap, the riser 15 can be covered. At this time, since the molten metal has not cooled, the oxides, inclusions and gases in the molten metal are in a stage of moving upward and being discharged. At this time, the shrinkage agent is easily dispersed under the impact of the high-temperature gas, resulting in direct contact between the molten metal and the air to produce a contact heat node. At this time, the shrinkage unit 17 can pressurize and limit the shrinkage agent, increase the coverage of the shrinkage agent on the molten metal, and greatly increase the solidification delay effect of the molten metal at the riser 18. Therefore, when the molten metal at the riser 18 just begins to cool, the purpose of the shrinkage unit 17 is to enhance the coverage of the shrinkage agent on the molten metal and avoid the occurrence of a shrinkage gap.

[0047] It is worth noting that, since the shrinkage agent is accumulated on the shrinkage unit 17, under the guiding effect of the guide seat 173, the supporting seat 174 can well accommodate the shrinkage agent, so that the weight of the shrinkage agent can cause the pressure spring 172 to be compressed, and the weight of the shrinkage agent can generate downward pressure on the molten metal, so that the molten metal at the riser 18 can be squeezed downward during the cooling and solidification process of the molten metal, and the utilization rate of the molten metal can be increased while completing the shrinkage. In this way, the size of the riser can be significantly reduced. During the solidification process of the molten metal at the riser 18, the shrinkage unit 17 can exert downward pressure on the molten metal, providing the molten metal with shrinkage feeding ability while facilitating the discharge of gas in the molten metal.

[0048] When the molten metal at the riser 18 completes the feeding action, the height of the feeding agent in the riser part 15 will drop, so that the feeding agent on the feeding unit 17 will automatically fill the assembly gap and the moving gap inside the riser part 15, so that the pressure on the feeding unit 17 gradually decreases. At this time, the pressure spring 172 uses its own resilience to drive the supporting seat 174 to gradually reset. Through the design of the feeding unit 17, on the premise of slowing down the heat dissipation efficiency of the molten metal at the riser 18, not only can the gap in the feeding agent be avoided to accelerate the cooling and solidification of the molten metal, but also the downward pressure on the molten metal can be applied by its own gravity, so that the utilization rate of the molten metal is increased, the molten metal is pressed into the casting, the density of the casting is improved, and the possibility of leakage during the casting pressure test is reduced.

[0049] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, it is still possible for those skilled in the art to modify the technical solutions described in the aforementioned embodiments or to make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A casting system for shrinkage compensation of a differential housing, comprising a matching lower casting mold base (1) and an upper casting mold base (2), Features: A sprue (3) is provided in the upper mold base (2), and a pouring cup (4) is provided at the top of the sprue (3). A buffer groove (5) is provided on the lower mold base (1) and is arranged at the bottom of the sprue (3). A cross runner (6) is provided between the lower mold base (1) and the upper mold base (2), and a first slag collecting bag (7) is provided at the other end of the cross runner (6). A flow blocking seat (8) is fixed at the bottom of the inner cavity of the cross runner (6) close to the sprue (3), and a flow blocking boss staggered with the flow blocking seat (8) is fixed at the top of the inner cavity of the cross runner (6). (9), the side wall of the cross runner (6) is connected to an endocasting channel (10) provided on the lower mold base (1), a casting mold cavity (11) is provided in the lower mold base (1), a flow blocking port (12) is provided at the connection point between the endocasting channel (10) and the casting mold cavity (11), a second slag collecting bag (13) is provided at the corresponding position of the bottom of the upper mold base (2) and the flow blocking port (12), a riser (18) is provided at the corresponding position of the upper mold base (2) and the casting mold cavity (11), and a pouring and rising port unit is fixedly installed at the position corresponding to the riser (18) on the upper mold base (2).

2. The casting system for shrinkage compensation of a differential housing according to claim 1, Features: The casting mold cavity (11) comprises a lower mold cavity (111) opened on the lower casting mold base (1) and an upper mold cavity (112) opened at the bottom of the upper casting mold base (2), and the riser (18) is opened at the top of the upper casting mold base (2), and the riser (18) and the upper mold cavity (112) are connected.

3. The casting system for shrinkage compensation of a differential housing according to claim 1, Features: The ratio of the height of the sprue (3), the length of the runner (6) and the length of the ingrate (10) is 4:8:

3.

4. The casting system for shrinkage compensation of a differential housing according to claim 3, Features: The height position of the ingrate (10) is set at 1 / 3 of the height of the runner (6), the aperture of the ingrate (10) is 1 / 4 of the aperture of the runner (6), and the top of the ingrate (10) is flush with the bottom of the upper mold base (2).

5. The casting system for shrinkage compensation of a differential housing according to claim 4, Features: The aperture of the blocking port (12) is 1 / 4 to 1 / 3 of the aperture of the endogate (10), and the blocking port (12) is an upwardly inclined arc-shaped spoiler port, the second slag collecting bag (13) is directly opposite to the arc-shaped surface of the blocking port (12), and the arc-shaped surface of the blocking port (12) is a convex surface.

6. The casting system for shrinkage compensation of a differential case according to claim 1, Features: The height of the flow blocking seat (8) is 1 / 3 of the height of the cross runner (6), the surface of the flow blocking seat (8) is an arc-shaped surface, the height of the flow blocking boss (9) is 1 / 3 of the height of the cross runner (6), the bottom of the flow blocking boss (9) is arranged as a sawtooth-shaped flow guiding tooth, and the inclination angle of the flow guiding tooth gradually decreases from the outside to the inside, and the direction of the flow guiding tooth is the center line direction of the cross runner (6).

7. A casting riser for shrinkage compensation of a differential housing, comprising a casting riser unit, Features: The pouring and rising head unit is the pouring and rising head unit according to claim 1; The pouring and rising unit comprises a rising seat (14) fixedly mounted on the top of the upper mold seat (2) and corresponding to the position of the rising head (18); a conical rising member (15) is plugged and assembled on the top of the rising seat (14); a heat preservation cavity (16) is provided in the rising member (15); three groups of shrinkage compensation units (17) with the same structure are slidably assembled on the inner side wall of the rising member (15); and the sizes of a single group of shrinkage compensation units (17) and the rising member (15) are adapted.

8. The pouring and rising head for shrinkage compensation of a differential case according to claim 7, Features: The shrinkage compensation unit (17) comprises a slideway provided on the inner wall of the riser member (15), a slide seat (171) being slidably mounted in the slideway, a pressure spring (172) being fixedly connected between the bottom of the slide seat (171) and the inner wall of the slideway, a flow guide seat (173) being fixedly connected to the outer wall of the slide seat (171), and a "bowl"-shaped supporting seat (174) being integrally formed at the bottom of the flow guide seat (173).

9. The pouring and rising head for shrinkage compensation of a differential case according to claim 8, Features: A guide port is provided at the end of the supporting seat (174), and an assembly gap is provided between two adjacent groups of the feeding units (17), and a moving gap is reserved between a single group of the feeding units (17) and the inner side wall of the riser member (15).