Directional sputtering target material and magnetron sputtering process

Through the directional sputtering target and magnetron sputtering process, the distance between the target and the substrate and the exit angle of metal atoms are adjusted, and the problem of low film coverage on the micropore and trench surfaces in the prior art is solved, and the further development is achieved. High step coverage and coating filling effect.

CN118957525APending Publication Date: 2024-11-15WUXI SHANGJI SEMICON TECH CO LTD

Patent Information

Application Number
CN202411272267.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-15

AI Technical Summary

Technical Problem

When the existing magnetron sputtering technology deposits the substrate surface with micropores and trenches, the film coverage is low, and it is easy to form punctured or unfilled voids at steep steps, making it difficult to achieve uniform thin layer deposition and filling. .

Method used

Using directional sputtering target and magnetron sputtering process, by setting grooves and support tubes on the target, adjusting the distance between the target and the substrate and the exit angle of the metal atoms, ensuring uniform downward movement of the metal atoms and improving the coating. stair coverage.

Benefits of technology

The film coverage of micropores and trench surfaces is significantly improved, ensuring that more metal atoms are deposited on the side walls or bottoms, improving the step coverage of the coating, and solving the problems of low coverage and high filling difficulty in the prior art.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118957525A_ABST
    Figure CN118957525A_ABST
Patent Text Reader

Abstract

The invention belongs to the field of magnetron sputtering, and particularly relates to a directional sputtering target and a magnetron sputtering technology.The directional sputtering target is characterized in that the side, close to a substrate, of a base plate is a front plate, the other face of the base plate is a back plate, and a plurality of grooves are formed in the front plate of the base plate; the target materials are located in the grooves and are lower than the surface of the substrate by more than 1mm, and the back plate is connected with the target materials in the grooves and is used for electrifying the target materials; when the target material is used, the air cylinder is arranged to control the target material to ascend and descend, the distance between the target material and the surface is adjusted, then the emergence angle of metal atoms is adjusted, the target material metal atoms diffused to the periphery can hit the inner wall face of the groove of the target material, and only the vertically-downward or small-angle-downward metal atoms can be sputtered out of the groove. And metal atoms accumulated at the top of the micro-hole or the groove in the surface of the substrate are reduced, so that more metal atoms can be deposited on the side wall or the bottom of the groove, and the step coverage rate of a coating film is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of magnetron sputtering, and in particular relates to a directional sputtering target material and a magnetron sputtering process. Background Art

[0002] Magnetron sputtering is a type of physical vapor deposition (PVD). The basic principle is that Ar is filled under vacuum conditions, and argon gas is glow discharged under high pressure, and Ar atoms are ionized into Ar + Ions and electrons - ,Ar + Under the action of the electric field, the electrons are accelerated to bombard the cathode target, and the target atoms are deposited on the wafer surface to form a thin film. - Under the action of electromagnetic field, the electrons drift in the direction indicated by E×B, and make spiral motion on the surface of the target material in a cycloid-like manner. They are bound in the plasma area on the target surface, and collide and ionize a large amount of Ar in this area. + to bombard the target, thereby achieving a high deposition rate.

[0003] In layered metal contacts or interconnect structures, a uniform but thin diffusion barrier layer must be deposited at the bottom and sidewalls of vias and trenches. As device size shrinks, the aspect ratio of contact vias and trenches increases, making uniform thin layer deposition and filling more difficult. The atoms sputtered from the target surface move in different directions and will change continuously due to scattering. Figure 1 As shown in (a) in the figure, pinch-off or unfillable voids may even form in the through holes and trenches with steep steps. Summary of the invention

[0004] In order to solve the problem that the coverage rate of the deposited thin film on the substrate surface with micropores and grooves is very low when sputtering an ordinary flat target material, the present invention discloses a directional sputtering target material and a magnetron sputtering process. By using the directional sputtering target material and the directional deposition process, the step coverage rate of the thin film on the substrate surface with micropores and grooves can be significantly improved.

[0005] To achieve the above object, the technical solution of the present invention is as follows: The present invention provides a directional sputtering target material, comprising: The substrate comprises a front plate on one side close to the substrate and a back plate on the other side. The front plate is provided with a plurality of grooves, a through hole is provided at the bottom of the groove, a connecting tube is connected to the through hole toward the front plate, the top of the connecting tube is connected to the edge of the through hole, a bellows is welded to the bottom of the connecting tube, a plurality of supporting tubes (which may be welded or connected in a detachable manner, such as thread, etc.) are provided on one side of the back plate close to the front plate, the supporting tubes are placed in the through hole, the connecting tube and the bellows, and the other side of the back plate is connected to the cylinder; the back plate is connected to a power supply.

[0006] The target material is placed in the groove, the diameter of the target material is the same as the inner diameter of the groove, the target material is welded and connected to the bottom end of the bellows, and is more than 1mm away from the surface of the front plate away from the back plate.

[0007] The setting of the cylinder can control the lifting and lowering of the target, adjust the distance between the target and the surface, and then adjust the exit angle of the metal atoms, so that the metal atoms can move downward at the expected angle. When the target moves downward, the angle of metal atoms sputtering downward is larger. When the target moves upward, the angle of metal atoms sputtering downward becomes smaller, which can infinitely approach vertical downward movement.

[0008] Furthermore, the positive plate is made of insulating material, which can prevent plasma from bombarding it.

[0009] The back plate connects the target material and the cathode of the DC power supply to realize the power supply to the target material, and the setting of the insulating material prevents the entire substrate from being conductive.

[0010] Furthermore, the material of the target is one of titanium, copper, tantalum and aluminum.

[0011] Furthermore, the back plate is made of metal material.

[0012] Furthermore, a wiring harness is arranged in the support tube, and the wiring harness connects the back plate and the target material, and is used for electrifying the target material.

[0013] The present invention also provides a magnetron sputtering process for the directional sputtering target as described above, comprising the following steps: adjusting the distance between the substrate and the target to 90 mm-270 mm; controlling the sputtering power to 6000 W; introducing argon gas, maintaining the pressure at 2.3-2.5 mTorr, sputtering for 170 seconds, depositing a metal film on the substrate surface, and completing a coating. As the sputtering is used, the distance between the target and the surface of the front plate and away from the back plate increases, and the position of the target can be adjusted using a cylinder.

[0014] Furthermore, the flow rate of argon gas is 35-45 sccm.

[0015] Furthermore, the method further includes the following steps: after N times of coating, an argon gas flow rate of 80-100 sccm, a total sputtering power of 10000 W, and a sputtering time of 5 s are used to ensure that a small amount of metal residue on the side wall of the groove is completely cleaned.

[0016] Furthermore, N>50.

[0017] The beneficial effects of the present invention are: During operation, the target is energized, the reaction gas enters the chamber and ionizes to form plasma, the positive ions in the plasma accelerate upward to bombard the target, and the metal atoms detach from the target. Since the target is installed inside the groove and is lower than the surface of the substrate, there is an empty space from the groove to the surface of the substrate, which has a certain guiding effect on the metal atoms.

[0018] In the prior art, the metal atoms of the target material fall and diffuse in all directions. When coating a substrate with micropores or grooves, since the metal atoms diffuse in all directions at multiple angles, most of the metal atoms will be plated on the top of the micropores or grooves on the substrate, and only a few metal atoms will be deposited inside the substrate grooves, resulting in a very low coverage rate of the micropores or grooves. Figure 1 As shown in (a). Figure 1 As shown in (b), the side wall film is very thin and the coverage is very low. (a) is non-directional sputtering and (b) is directional sputtering.

[0019] When the target material of the present invention is in use, the metal atoms of the target material diffused in all directions will hit the inner wall surface of the groove of the target material, and only the metal atoms moving vertically downward or at a small angle downward can be sputtered out from the groove. Therefore, the metal atoms can move vertically or at a small angle downward, reducing the accumulation of metal atoms at the top of the micropores or grooves on the surface of the substrate, so that more metal atoms can be deposited on the side walls or bottom of the grooves, thereby improving the step coverage of the coating. In addition, the sputtering angle of the target material atoms will gradually approach the vertical as the use time of the target material increases. The schematic diagram of the sputtering angle range of a single target material is shown in FIG. Figure 2 shown.

[0020] In addition, when the target material of the present invention is in use, the metal atoms diffused in all directions will hit the inner wall surface of the target groove. Even if a certain amount of target atoms are deposited on the inner wall surface, due to its close distance to the target surface, the inner wall will also be hit to a certain extent by Ar+ ions or other target atoms, causing it to detach from the inner wall. Ultimately, the target metal atoms can still move downward in a nearly vertical or small angle, so that more target metal atoms can be deposited on the side wall or bottom of the substrate groove, thereby improving the step coverage.

[0021] Step coverage is defined as the ratio of the film thickness on the sidewall or bottom to the film thickness at the top plane. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Schematic diagram of the effect of non-directional and directional sputtering on through-hole and trench step coverage; Figure 2 It is a schematic diagram of the initial sputtering range of target atoms and the atomic sputtering range after the target is sputtered for a period of time; Figure 3 It is a schematic structural diagram of a directional sputtering target material of the present invention; Figure 4 It is a schematic diagram of the structure of a planar target; Figure 5 Schematic diagram of film measurement points; Figure 6 This is the step coverage of the target material during directional sputtering in Example 1 of the present invention; Figure 7 The step coverage of the planar target in Example 1 of the present invention; Figure 8 It is a cross-sectional view of a directional sputtering target material according to Example 1 of the present invention; Fig. 9 for Figure 8 Enlarged view of part A in the figure.

[0023] List of Figure Symbols: 1. Base plate; 2. Positive plate; 3. Groove; 4. Target material; 5. Film at the top plane; 6. On the side wall; 7. In the side wall; 8. Under the side wall; 9. Bottom; 10. Substrate; 11. Cylinder; 12. Back plate; 13. Bellows; 14. Connecting tube; 15. Support tube; 16. Baffle; 17 Through hole; 18. Front side. DETAILED DESCRIPTION

[0024] The present invention will be further explained below in conjunction with the accompanying drawings and specific embodiments. It should be understood that the following specific embodiments are only used to illustrate the present invention and are not used to limit the scope of the present invention.

[0025] A directional sputtering target material 4; comprising: A substrate 1, a side of the substrate 1 close to the substrate 10 is a positive plate 2, and the other side is a back plate 12. The positive plate 2 is provided with a plurality of grooves 3, and the positive plate 2 is made of insulating material; a through hole 17 is provided at the bottom of the groove 3, and a connecting tube 14 is connected to the through hole 17 toward the positive plate 2, and the top of the connecting tube 14 is connected to the edge of the through hole 17, and a bellows 13 is welded to the bottom of the connecting tube 14; a plurality of supporting tubes 15 are provided on one side of the back plate 12 close to the positive plate 2, and the supporting tubes 15 are placed in the through holes 17, the connecting tubes 14 and the bellows 13, and the other side of the back plate 12 is connected to the cylinder 11; a wiring harness is provided in the supporting tube 15, and the wiring harness connects the back plate 12 and the target material 4, and is used for electrifying the target material 4.

[0026] Connect the back plate 12 to the cathode of the DC power supply to realize power supply to the target 4; The target material 4 is placed in the groove 3, the target material 4 is welded to the end of the bellows 13, and is more than 1 mm away from the surface of the positive plate 2 away from the back plate 12. As an embodiment of the present invention, the groove 3 has a diameter of 0.3-0.8 cm and is 1-2 mm away from the surface of the positive plate 2 away from the back plate 12.

[0027] The positive plate 2 is made of insulating material.

[0028] The material of the target 4 is one of titanium, copper, tantalum and aluminum.

[0029] The back plate 12 is made of metal material.

[0030] As a specific embodiment of the present invention, a baffle 16 may be further provided at the open end of the groove 3; the baffle 16 is cylindrical and connected to the positive plate 2 by snap connection, rotation connection, thread connection or other connection methods. The baffle 16 can further control the exit angle of the metal atoms.

[0031] A magnetron sputtering process of the directional sputtering target 4 as described above includes the following steps: adjusting the distance between the substrate 10 and the target 4 to 90mm-270mm; controlling the sputtering power to 6000W; introducing 40sccm argon gas, maintaining the pressure at 2.3-2.5mTorr, sputtering for 170s, and depositing a metal film on the surface of the substrate 10 to complete a coating. Example 1

[0032] like Figure 3 , Figure 8 and Fig. 9 As shown, a directional sputtering target material 4 is provided; it comprises: a substrate 1, a side of the substrate 1 close to the substrate 10 is a positive plate 2, and the other side is a back plate, the positive plate 2 is provided with 43 grooves 3, the diameter of the groove 3 is 0.6 cm, the positive plate 2 is made of an insulating material, and the back plate 12 is made of a metal material; a through hole 17 is provided at the bottom of the groove 3, a connecting tube 14 is connected to the through hole 17 in the direction of the positive plate 2, the top of the connecting tube 14 is connected to the edge of the through hole 17, a bellows 13 is welded to the bottom of the connecting tube 14, a plurality of support tubes 15 (which can be welded or connected in a detachable manner, such as thread, etc.) are provided on one side of the back plate 12 close to the positive plate 2, the support tubes 15 are placed in the through holes 17, the connecting tubes 14 and the bellows 13, and the other side of the back plate 12 is connected to the cylinder 11; a wiring harness is provided in the support tube 15, and the wiring harness connects the back plate 12 and the target material 4, and is used for electrifying the target material 4; Connect the back plate to the cathode of the DC power supply to energize the target 4; The target material 4 is placed in the groove 3 , and the target material 4 is welded to the end of the bellows 13 , and is 1-2 mm away from the surface of the front plate 2 away from the back plate 12 .

[0033] The schematic diagram of the planar target 4 structure is as follows Figure 4 As shown, it includes a substrate 1, the side of the substrate 1 close to the substrate 10 is the front side 18, and the other side is the back side. The target material 4 is installed on the front side 18, and a conductive plate is installed on the back side of the substrate 1. The conductive plate is connected to the cathode of the DC power supply to realize the power supply to the target material 4.

[0034] A magnetron sputtering process using the directional sputtering target 4 as described above comprises the following steps: The above-mentioned directional sputtering target 4 was used to carry out magnetron sputtering coating tests. The material of the directional sputtering target 4 was titanium (as another embodiment of the present invention, the target 4 material can also be copper, tantalum, aluminum, etc.), the distance between the substrate 10 and the target 4 was 180 mm, the substrate 10 used an 8-inch silicon oxide substrate wafer, the sputtering power was 6000 W, the argon gas flow rate was 40 sccm, the chamber pressure was maintained at 2.4 mTorr, the sputtering time was 170 s, and a Ti film was deposited on the surface of the 8-inch silicon oxide substrate wafer.

[0035] The existing planar target 4 is subjected to a magnetron sputtering coating test using the same magnetron sputtering process as described above, except that the directional sputtering target 4 is replaced by the existing planar target 4 .

[0036] The film thickness distribution of the cross section at the micropore of the substrate 10 was observed under a scanning electron microscope. The film measurement points are as follows: Figure 5 The step coverage is defined as the ratio of the film thickness on the sidewall or bottom 9 to the film thickness on the top plane 5. The step coverage of the directional sputtering target 4 and the existing planar target 4 is shown in Figure 6 and Figure 7 The coverage at the side wall is the average value of the film thickness on both sides of the side wall. The calculated step coverage is shown in Table 1.

[0037] Table 1

[0038] pass Figure 6 , Figure 7 As shown in Table 1, when the existing planar target 4 is sputtered, the thin film step coverage at the side wall 7, the side wall bottom 8 and the bottom 9 is very poor and almost unobservable; while when the directional sputtering target 4 in this application is sputtered, the step coverage is good, the average step coverage of the side wall is close to 20%, and the step coverage of the bottom 9 reaches 17%. Therefore, the step coverage of the micropore by the sputtering directional sputtering target 4 is much better than that of the planar target 4. Example 2

[0039] The magnetron sputtering process of the directional sputtering target 4 of Example 1 is the same. The target 4 materials of the directional sputtering target 4 and the planar target 4 are both titanium. The distance between the substrate 10 and the target 4 is 180 mm. The substrate 10 uses an 8-inch silicon oxide substrate wafer. The sputtering power is 6000 W, the argon flow rate is 40 sccm, the chamber pressure is maintained at 2.4 mTorr, and the sputtering time is 170 s. A Ti film is deposited on the surface of the 8-inch silicon oxide substrate wafer. After each N times of coating is completed (N>50; as another embodiment of the present invention, N is 60 times or 70 times, 80 times, 90 times, 100 times), an argon flow rate of 80-100 sccm, a sputtering power of 10000 W, and a sputtering time of 10 s. High flow increases plasma concentration, and high power increases the kinetic energy of Ar+ ions, which can accelerate the cleaning of metal residues on the side walls of the groove 3 of the target 4. Example 3

[0040] The directional sputtering target 4 of the present invention was used to carry out a magnetron sputtering coating test. The material of the target 4 is titanium, the substrate 10 is an 8-inch silicon oxide substrate wafer, the sputtering power is 6000W, the argon gas flow rate is 40sccm, the chamber pressure is maintained at 2.4mTorr, the distance between the substrate 10 and the target 4 is adjusted to 90, 180, and 270mm respectively, the sputtering time is 170s, and a Ti film is deposited on the surface of the 8-inch silicon oxide substrate wafer. The step coverage is shown in Table 2. It can be seen from Table 2 that by changing the distance between the target 4 and the substrate 10, the step coverage at the inner side wall and the bottom 9 of the micropore can be adjusted accordingly. For example, if the distance between the target 4 and the substrate 10 becomes larger, the step coverage at the bottom 9 of the micropore can be further improved; conversely, the step coverage at the inner side wall of the micropore is improved.

[0041] Table 2 Example 4

[0042] The life of the directional sputtering target 4 of the present invention is about 600kWh. When the service life of the target 4 is 0kWh, 150kWh, 300kWh, and 450kWh, magnetron sputtering coating tests are carried out. The material of the target 4 is titanium, the substrate 10 uses an 8-inch silicon oxide substrate wafer, the sputtering power is 6000W, the argon gas flow rate is 40sccm, the chamber pressure is maintained at 2.4mTorr, the distance between the substrate 10 and the target 4 is adjusted to 150mm, the sputtering time is 170s, and a Ti film is deposited on the surface of the 8-inch silicon oxide substrate wafer. The step coverage is shown in Table 3.

[0043] Table 3

[0044] It can be seen from the table that with the continuous consumption of the target material 4, the film step coverage inside the micropores gradually increases.

[0045] It should be noted that the above content only illustrates the technical idea of ​​the present invention and cannot be used to limit the protection scope of the present invention. For ordinary technicians in this technical field, several improvements and modifications can be made without departing from the principle of the present invention. These improvements and modifications all fall within the protection scope of the claims of the present invention.

Claims

1. A directional sputtering target, It is characterized in that include: Base plate, one side of the base plate close to the substrate is a front plate, and the other side is a back plate, the front plate is provided with a plurality of grooves, the bottom of the groove is provided with a through hole, a connecting pipe is connected to the through hole toward the front plate, and a bellows is welded to the other end of the connecting pipe, a plurality of supporting pipes are arranged on one side of the back plate close to the front plate, the supporting pipes are placed in the through hole, the connecting pipe and the bellows, and the other side of the back plate is connected to the cylinder; The target material is placed in the groove, the target material is welded and connected to the end of the bellows, and is more than 1 mm away from the surface of the front plate away from the back plate.

2. A directional sputtering target according to claim 1, It is characterized in that The positive plate is made of insulating material.

3. A directional sputtering target according to claim 1, It is characterized in that The target material is one of titanium, copper, tantalum and aluminum.

4. A directional sputtering target according to claim 1, It is characterized in that The back plate is made of metal material and is connected to a power source.

5. A directional sputtering target according to claim 1, It is characterized in that A wiring harness is arranged in the support tube, and the wiring harness connects the back plate and the target material.

6. A magnetron sputtering process for a directional sputtering target according to any one of claims 1 to 5, It is characterized in that The following steps are involved: The distance between the substrate and the directional sputtering target is adjusted to 90 mm-270 mm; the sputtering power is controlled to 6000 W; argon gas is introduced and the pressure is maintained at 2.3-2.5 mTorr. The sputtering is performed for 170 seconds. A metal film is deposited on the surface of the substrate, and a coating is completed.

7. The magnetron sputtering process of a directional sputtering target according to claim 6, It is characterized in that The argon flow rate is 35-45 sccm.

8. The magnetron sputtering process of a directional sputtering target according to claim 6, It is characterized in that The following steps are also included: After N times of coating, an argon gas flow rate of 80-100sccm, a total sputtering power of 10000W, and a sputtering time of 5s were used to quickly clean the metal residues on the side walls of the grooves.

9. The magnetron sputtering process of a directional sputtering target according to claim 8, It is characterized in that N>50。

Citation Information

Patent Citations

  • Sputtering device

    JP1996020864A

  • Composite sputtering cathode and sputtering device using the cathode

    JP1998121235A

  • Optical disk, manufacturing device therefor and manufacture thereof

    JP1999185308A

  • Sputtering method and sputtering system

    JP2001234336A

  • Sputtering apparatus

    JP2004256849A

Cited By

  • Sputtering process for improving step coverage rate of metal film