Bio-based oxygen bleaching stabilizer as well as preparation method and application thereof

By combining amino acid chelating agents, sodium gluconate, polyepoxysuccinic acid and starch grafts, bio-based oxygen bleach stabilizers without silicon and phosphorus are prepared, and the existing oxygen bleach stabilizers are solved in the textile industry. The eutrophication problems of medium silica scale and water bodies improve fabric whiteness and stability, reduce fiber damage, and achieve environmental friendliness.

CN118979373APending Publication Date: 2024-11-19JIANGSU NEW REBA TECH CO LTD +1
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411232161.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

The existing oxygen bleach stabilizers have problems such as silica scale formation, eutrophication of water bodies and high toxicity in the textile industry, making it difficult to effectively stabilize hydrogen peroxide, and have a great impact on fabric whiteness and equipment efficiency.

Method used

Bio-based oxygen bleach stabilizers are prepared by combining natural materials such as amino acid chelating agents, sodium gluconate, polyepoxysuccinic acid, starch grafts and magnesium salts. Through chelation, scale inhibition and passivation, they work together to stabilize Hydrogen peroxide, avoid the use of silicon and phosphorus.

Benefits of technology

A bio-based oxygen bleach stabilizer without silicon and phosphorus is realized, which improves the whiteness of the fabric, reduces fiber damage, is environmentally friendly, and has good biodegradation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118979373A_ABST
    Figure CN118979373A_ABST
Patent Text Reader

Abstract

The invention provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The bio-based oxygen bleaching stabilizer is prepared from the following raw materials: an amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, a starch graft, a passivator and water. The bio-based oxygen bleaching stabilizer provided by the invention is silicon-free, phosphorus-free and pollution-free to the environment, so that the hydrogen peroxide has better stability, and invalid decomposition of the hydrogen peroxide can be effectively reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of oxygen bleaching stabilizers, and specifically relates to a bio-based oxygen bleaching stabilizer and a preparation method and application thereof. Background Art

[0002] As an excellent bleaching agent, hydrogen peroxide has the characteristics of high bleaching whiteness, good stability and low cost, and is widely used in the desizing and bleaching of fabrics in the textile industry. 3+ and Cu 2+ Heavy metal ions such as ions will cause catalytic decomposition of hydrogen peroxide during the bleaching process, causing fiber damage and even forming oxygen bleaching holes on the bleached cloth. In order to control the decomposition of hydrogen peroxide and obtain a good bleaching effect, it is necessary to add an auxiliary agent to enable hydrogen peroxide to decompose effectively. This auxiliary agent is an oxygen bleaching stabilizer, also known as a hydrogen peroxide stabilizer. According to its mechanism of action, it can be divided into adsorption-type oxygen bleaching stabilizers and chelating-type oxygen bleaching stabilizers.

[0003] The most typical adsorption-type oxygen bleaching stabilizer is sodium silicate. CN104928906A discloses a textile oxygen bleaching stabilizer, which is made of the following raw materials in parts by weight: 8-16 parts of barium sulfate, 2-4 parts of hexamethylenetetramine, 3-6 parts of polyurethane resin, 2-4 parts of sodium silicate, 4-6 parts of ethyl acetate, 2-5 parts of magnesium persulfate, 4-7 parts of polyoxyethylene octylphenyl alcohol, 6-11 parts of 2-ethylhexanoate barium, 4-8 parts of diglycidyl ether, 1-3 parts of magnesium sulfate, 5-7 parts of sodium ethylenediaminetetraacetate, 3-6 parts of boric acid, 10-14 parts of barium metal organic liquid, 4-8 parts of lubricant, and 1-2 parts of trihydroxymethylpropane. The textile oxygen bleaching stabilizer provided by this technical solution has a good stabilizing effect on hydrogen peroxide. Although sodium silicate can have a good stabilizing effect on hydrogen peroxide and its cost is not high, it will react with Ca 2+ and Mg 2+ The reaction can easily produce silica scale on fabrics and equipment, which reduces the whiteness of the fabric and the efficiency of the equipment.

[0004] Chelating oxygen bleaching stabilizers mainly include phosphates, carboxylates, etc. CN102199869A discloses an oxygen bleaching stabilizer and its application, wherein the oxygen bleaching stabilizer is formulated from the following components in weight percentage: 50% to 70% of organic phosphate, 20% to 30% of polycarboxylic acid dispersant, and 10% to 20% of polyether surfactant; the organic phosphate is any one of diethylenetriamine pentasodium methylene phosphonate and ethylenediaminetetrasodium methylene phosphonate; the polycarboxylic acid dispersant is polyacrylic acid; the polyether surfactant is any one of isooctyl alcohol polyoxyethylene ether phosphate and fatty alcohol polyoxyethylene ether sodium carboxylate. The oxygen bleaching stabilizer provided by the technical solution can effectively inhibit the decomposition of invalid oxygen and increase the proportion of hydrogen peroxide participating in the reaction. Although phosphate stabilizers have good stability, they will cause eutrophication of water bodies and destroy the aquatic ecological balance. Carboxylate stabilizers, such as diethylenetriaminepentaacetic acid (DTPA) and ethylenediaminetetraacetic acid (EDTA), are highly toxic and poorly biodegradable.

[0005] CN111560768A discloses a phosphorus-free and silicon-free oxygen bleaching stabilizer and a preparation method thereof. The phosphorus-free and silicon-free oxygen bleaching stabilizer comprises the following raw materials in parts by weight: 3.0% to 9.0% reducing sugar, 1.0% to 6.0% alcohol amine, 0.5% to 3.0% aminocarboxylate, 1.0% to 4.0% auxiliary agent, 20% to 78% hydrogen peroxide, 1.0% to 4.0% chelating agent, and 1.0% to 4.0% stabilizer. The phosphorus-free and silicon-free oxygen bleaching stabilizer provided by the technical solution does not contain phosphorus and silicon substances that are harmful to the environment, and solves the problems of silicon scale and eutrophication of water bodies, but the stability of the oxygen bleaching stabilizer to hydrogen peroxide and the application performance of the oxygen bleaching stabilizer still need to be further improved.

[0006] Therefore, it is necessary to develop a bio-based oxygen bleaching stabilizer that is silicon-free, phosphorus-free, environmentally friendly, and has a good stabilizing effect on hydrogen peroxide. Summary of the invention

[0007] In view of the shortcomings of the prior art, the present invention aims to provide a bio-based oxygen bleaching stabilizer and its preparation method and application. The bio-based oxygen bleaching stabilizer is prepared from natural raw materials, is degradable, is silicon-free and phosphorus-free, and does not pollute the environment. It is used in the pre-treatment oxygen bleaching process of fabrics to obtain higher whiteness of the fabrics and less intensive damage.

[0008] In order to achieve the purpose of the invention, the present invention adopts the following technical solutions:

[0009] In a first aspect, the present invention provides a bio-based oxygen bleaching stabilizer, wherein raw materials for preparing the bio-based oxygen bleaching stabilizer include an amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, a starch graft, a passivator and water.

[0010] In the present invention, the raw materials for preparing the bio-based oxygen bleaching stabilizer include amino acid chelating agents, sodium gluconate, polyepoxysuccinic acid, starch grafts, passivators and water. The raw materials are natural, degradable, silicon-free and phosphorus-free, and have no pollution to the environment. The bio-based oxygen bleaching stabilizer has the characteristics of high whiteness and little damage to fabrics during a long continuous oxygen bleaching process, and is suitable for wide application.

[0011] Preferably, the amino acid chelating agent comprises tetrasodium glutamate diacetate.

[0012] Preferably, the starch graft comprises starch grafted polyacrylic acid.

[0013] Preferably, the passivating agent comprises a magnesium salt.

[0014] Preferably, the magnesium salt comprises magnesium sulfate and / or magnesium chloride.

[0015] Preferably, the raw materials for preparing the bio-based oxygen bleaching stabilizer include the following components by mass percentage: 10% to 20% (e.g., 11%, 12%, 13%, 14%, 15%, 16%, 17%, 18% or 19%) of amino acid chelating agent, 5% to 10% (e.g., 5.5%, 6%, 6.5%, 7%, 7.5%, 8%, 8.5%, 9% or 9.5%) of sodium gluconate, 3% to 10% (e.g., 5.5%, 6%, 6.5%, 7%, 7.5%, 8%, 8.5%, 9% or 9.5%) of polyepoxysuccinic acid, 4%, 5%, 6%, 7%, 8% or 9%, etc.), starch grafts 5% to 15% (for example 6%, 7%, 8%, 9%, 10%, 11%, 12%, 13% or 14%, etc.), passivator 5% to 20% (for example 7%, 9%, 11%, 13%, 15%, 17% or 19%, etc.) and water 25% to 72% (for example 30%, 35%, 40%, 45%, 50%, 55%, 60%, 65% or 70%, etc.).

[0016] Preferably, the raw materials for preparing the bio-based oxygen bleaching stabilizer include the following components by mass percentage: 10% to 20% (e.g., 11%, 12%, 13%, 14%, 15%, 16%, 17%, 18% or 19%) of tetrasodium glutamate diacetate, 5% to 10% (e.g., 5.5%, 6%, 6.5%, 7%, 7.5%, 8%, 8.5%, 9% or 9.5%) of sodium gluconate, 3% to 10% (e.g., 5.5%, 6%, 6.5%, 7%, 7.5%, 8%, 8.5%, 9% or 9.5%) of polyepoxysuccinic acid, 4%, 5%, 6%, 7%, 8% or 9%, etc.), starch grafted polyacrylic acid 5% to 15% (for example, 6%, 7%, 8%, 9%, 10%, 11%, 12%, 13% or 14%, etc.), magnesium salt 5% to 20% (for example, 7%, 9%, 11%, 13%, 15%, 17% or 19%, etc.) and water 25% to 72% (for example, 30%, 35%, 40%, 45%, 50%, 55%, 60%, 65% or 70%, etc.).

[0017] In the present invention, the tetrasodium glutamate diacetate and sodium gluconate are used as chelating agents. The main raw material for preparing tetrasodium glutamate diacetate is sodium glutamate, which is a natural fermentation product, is biodegradable, does not contain phosphorus, and is more in line with environmental protection requirements. Tetrasodium glutamate diacetate can stably exist in an acidic environment and can chelate iron ions. Under alkaline conditions, it can be widely used as an aminopolycarboxylic acid and can chelate calcium ions and other metal ions well. And tetrasodium glutamate diacetate can also maintain stable performance in a high temperature environment for a long time. Sodium gluconate has a strong complexing ability for calcium ions, magnesium ions and iron ions, and a strong scale inhibition ability, especially for Fe 3+ It has excellent chelating properties and works even in the full pH range.

[0018] In the present invention, the polyepoxysuccinic acid and starch-grafted polyacrylic acid are used as scale inhibitors. Polyepoxysuccinic acid is a nitrogen-free, non-phosphorus organic compound with dual functions of scale inhibition and corrosion inhibition. It can form a colloid in the solution and adsorb Fe 3 + , Cu 2+ It can degrade metal ions such as chlorinated polyacrylic acid, making them lose their catalytic activity, thus stabilizing hydrogen peroxide. It also has good biodegradability and is suitable for water systems with high alkali and high metal content. It is a green water treatment chemical. Starch grafted polyacrylic acid is a simple and easy-to-obtain natural polymer-based bifunctional water treatment agent that has both high-efficiency scale inhibition and flocculation effects and is environmentally friendly.

[0019] In the present invention, the magnesium salt mainly plays a passivation role, improves the alkali resistance stability of hydrogen peroxide, can generate positively charged Mg(OH)2 flocculent micelles in alkaline oxygen bleaching liquid, has an adsorption effect, can prevent hydrogen peroxide from further reacting to generate HOO· free radicals, thereby inhibiting the reaction chain of hydrogen peroxide.

[0020] In the present invention, the bio-based oxygen bleaching stabilizer has both adsorption performance and chelation effect through the synergistic effect between the chelating agent, the scale inhibitor and the magnesium salt. The raw materials interact with each other through a certain ratio, and the advantages of each are retained and the disadvantages of each are overcome, so that the cost can be reduced and the hydrogen peroxide can be made more stable during the bleaching process of the oxygen bleaching process, so that the treated fabric can obtain a higher whiteness and less strong damage.

[0021] In a second aspect, the present invention provides a method for preparing the bio-based oxygen bleaching stabilizer as described in the first aspect, the preparation method comprising mixing an amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, a starch graft, a passivator and water to obtain the bio-based oxygen bleaching stabilizer.

[0022] Preferably, the preparation method specifically comprises the following steps:

[0023] (1) Sodium gluconate, a passivating agent and water are mixed to obtain a mixture.

[0024] (2) Mixing the mixture obtained in step (1), an amino acid chelating agent, polyepoxysuccinic acid and a starch graft, stirring and reacting, and obtaining the bio-based oxygen bleaching stabilizer.

[0025] Preferably, the mixing further includes a filtering step.

[0026] In a third aspect, the present invention provides a use of the bio-based oxygen bleaching stabilizer as described in the first aspect in a pre-treatment bleaching process of fabrics.

[0027] Compared with the prior art, the present invention has the following beneficial effects:

[0028] The raw materials for preparing the bio-based oxygen bleaching stabilizer of the present invention include a combination of amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, starch graft, passivating agent and water, so that the bio-based oxygen bleaching stabilizer has both adsorption performance and chelating effect. The bio-based oxygen bleaching stabilizer is free of silicon and phosphorus and has no pollution to the environment. When used in the pre-treatment oxygen bleaching process of fabric, the fabric can obtain higher whiteness and less strong damage. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1 This is a comparison chart of the results of measuring the decomposition rate of hydrogen peroxide when the bio-based oxygen bleaching stabilizer provided in Examples 1-6 and the oxygen bleaching stabilizer provided in Comparative Example 1 are added respectively. DETAILED DESCRIPTION

[0030] The technical solution of the present invention is further described below by specific implementation methods. It should be understood by those skilled in the art that the embodiments are only to help understand the present invention and should not be regarded as specific limitations of the present invention.

[0031] The sources of some components in the embodiments and comparative examples are as follows:

[0032] Polyepoxysuccinic acid: Product No. P923986, analytical grade, manufactured by Shanghai MacLean Biochemical Technology Co., Ltd.

[0033] Starch grafted polyacrylic acid: Acrylic acid grafted starch 300, the manufacturer is Beijing Taide Pharmaceutical Co., Ltd.

[0034] Example 1

[0035] The present embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The bio-based oxygen bleaching stabilizer includes the following components by mass percentage: 10% tetrasodium glutamate diacetate, 5% sodium gluconate, 3% polyepoxysuccinic acid, 5% starch grafted polyacrylic acid, 5% magnesium sulfate and 72% water.

[0036] The preparation method specifically comprises the following steps:

[0037] (1) adding sodium gluconate and magnesium sulfate into water successively and stirring and dissolving them at room temperature (25° C.) to obtain a mixture;

[0038] (2) Tetrasodium glutamate diacetate, polyepoxysuccinic acid and starch-grafted polyacrylic acid are added to the mixture obtained in step (1), mixed, stirred at room temperature (25° C.) for 2 h, and filtered to obtain the bio-based oxygen bleaching stabilizer.

[0039] Example 2

[0040] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which is different from Example 1 only in that the mass percentage of sodium gluconate is adjusted to 8%, the mass percentage of water is adjusted to 69%, and other conditions are the same as those in Example 1.

[0041] Example 3

[0042] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between the bio-based oxygen bleaching stabilizer and the embodiment 1 is that the bio-based oxygen bleaching stabilizer includes the following components by mass percentage: 10% tetrasodium glutamate diacetate, 8% sodium gluconate, 6% polyepoxysuccinic acid, 10% starch grafted polyacrylic acid, 15% magnesium sulfate and 51% water. Other conditions are the same as those in the embodiment 1.

[0043] Example 4

[0044] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between the bio-based oxygen bleaching stabilizer and the embodiment 1 is that the bio-based oxygen bleaching stabilizer includes the following components by mass percentage: 15% tetrasodium glutamate diacetate, 8% sodium gluconate, 6% polyepoxysuccinic acid, 10% starch grafted polyacrylic acid, 10% magnesium sulfate and 51% water. Other conditions are the same as those in the embodiment 1.

[0045] Example 5

[0046] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between the bio-based oxygen bleaching stabilizer and the embodiment 1 is that the bio-based oxygen bleaching stabilizer includes the following components by mass percentage: 20% tetrasodium glutamate diacetate, 10% sodium gluconate, 10% polyepoxysuccinic acid, 15% starch grafted polyacrylic acid, 15% magnesium sulfate and 30% water. Other conditions are the same as those in the embodiment 1.

[0047] Example 6

[0048] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between the bio-based oxygen bleaching stabilizer and the embodiment 1 is that the bio-based oxygen bleaching stabilizer includes the following components by mass percentage: 20% tetrasodium glutamate diacetate, 10% sodium gluconate, 10% polyepoxysuccinic acid, 15% starch grafted polyacrylic acid, 20% magnesium sulfate and 25% water. Other conditions are the same as those in the embodiment 1.

[0049] Example 7

[0050] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which is different from Example 1 only in that magnesium sulfate is replaced with magnesium chloride of the same mass, and other conditions are the same as those in Example 1.

[0051] Example 8

[0052] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between this embodiment and embodiment 1 is that the mass percentage of tetrasodium glutamate diacetate is adjusted to 6%, the mass percentage of water is adjusted to 76%, and other conditions are the same as those in embodiment 1.

[0053] Example 9

[0054] This embodiment provides a bio-based oxygen bleaching stabilizer and a preparation method thereof. The only difference between this embodiment and embodiment 1 is that the mass percentage of tetrasodium glutamate diacetate is adjusted to 24%, the mass percentage of water is adjusted to 58%, and other conditions are the same as those in embodiment 1.

[0055] Comparative Example 1

[0056] This comparative example provides an oxygen bleaching stabilizer, wherein the oxygen bleaching stabilizer is sodium silicate.

[0057] Comparative Example 2

[0058] This comparative example provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which differs from Example 1 only in that sodium gluconate is not added, the mass percentage of tetrasodium glutamate diacetate is adjusted to 15%, and other conditions are the same as those in Example 1.

[0059] Comparative Example 3

[0060] This comparative example provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which differs from Example 1 only in that tetrasodium glutamate diacetate is not added, the mass percentage of sodium gluconate is adjusted to 15%, and other conditions are the same as those in Example 1.

[0061] Comparative Example 4

[0062] This comparative example provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which differs from Example 1 only in that polyepoxysuccinic acid is not added, the mass percentage of starch grafted polyacrylic acid is adjusted to 15%, and other conditions are the same as those in Example 1.

[0063] Comparative Example 5

[0064] This comparative example provides a bio-based oxygen bleaching stabilizer and a preparation method thereof, which differs from Example 1 only in that starch-grafted polyacrylic acid is not added, the mass percentage of polyepoxysuccinic acid is adjusted to 15%, and other conditions are the same as those in Example 1.

[0065] The bio-based oxygen bleaching stabilizers provided in the above Examples 1-9 and Comparative Examples 2-5 and the oxygen bleaching stabilizer provided in Comparative Example 1 were tested, and the specific testing method is as follows:

[0066] (1) Determination of hydrogen peroxide decomposition rate

[0067] Prepare 200mL of oxygen bleach working solution with bio-based oxygen bleach stabilizer or oxygen bleach stabilizer, NaOH, H2O2 and water, wherein NaOH is 3g / L, H2O2 is 15g / L, bio-based oxygen bleach stabilizer or oxygen bleach stabilizer is 16g / L, and water is used as solvent. Prepare 200mL of blank oxygen bleach working solution with NaOH, H2O2 and water, wherein NaOH is 3g / L, H2O2 is 15g / L, as blank comparison.

[0068] The oxygen bleaching working solution or the blank oxygen bleaching working solution was transferred into a ground-mouth conical flask, and then placed in a constant temperature dyeing small sample machine, oscillated at a frequency of 10 times / min, and heated from 40°C to 98°C at a heating rate of 2°C / min. Then, 10 mL of solution was taken from the bottle at 0 min, 15 min, 30 min, 45 min and 60 min, respectively, and the hydrogen peroxide decomposition rate was calculated according to the formula in HG / T 4916-2016 "Determination of the stability of hydrogen peroxide by hydrogen peroxide stabilizers in textile dyeing and finishing auxiliaries", and the test results are shown in Table 1.

[0069] (2) Chelating metal ion capacity: Fe was determined according to GB / T 21884-2008 3+ , Ca 2+ The chelation value of the test results is shown in Table 2.

[0070] (3) Oxygen bleaching effect

[0071] Prepare 200 mL of oxygen bleaching working solution with bio-based oxygen bleaching stabilizer or oxygen bleaching stabilizer, NaOH, H2O2 and water, wherein NaOH is 3 g / L, H2O2 is 15 g / L, and bio-based oxygen bleaching stabilizer or oxygen bleaching stabilizer is 16 g / L.

[0072] The enzyme desized fabric sample (21×21 pure cotton yarn card grey cloth) was dipped into the oxygen bleaching working solution, steamed at 102° C. for 30 minutes, and then washed and dried to obtain the oxygen bleached fabric sample.

[0073] Fabric strength: According to GB / T 3917.2-2009 "Tear properties of textile fabrics - Part 2: Determination of tear strength of trouser-type test specimens (single seam)", the tear strength test of the fabric samples after oxygen bleaching is carried out. The degree of damage to the fabric is reflected by the strength value. The larger the value, the smaller the degree of damage to the fabric.

[0074] Fabric whiteness and capillary effect test: According to ZBW04019-1990 "Professional Standard Textile Capillary Effect Test Method", the capillary effect of the fabric sample after oxygen bleaching is measured. The larger the capillary effect value, the better the performance of the oxygen bleaching stabilizer.

[0075] The test results are shown in Table 3.

[0076] Table 1

[0077]

[0078] Table 2

[0079]

[0080]

[0081] Table 3

[0082]

[0083] From the contents of Table 1, Table 2 and Table 3, it can be seen that the bio-based oxygen bleaching stabilizer provided in Examples 1-9 effectively reduces the ineffective decomposition of hydrogen peroxide, making hydrogen peroxide have better stability at 98°C; 3+ and Ca 2+ Has good chelating ability and is effective for Fe 3+ The chelating ability of Fe 3+ The chelation value of Ca is 310~598mg / g. 2+ The chelating value is 57-85 mg / g. During the oxygen bleaching process, the fabric has high whiteness and little damage.

[0084] Compared with the blank sample, the addition of the working solution of the bio-based oxygen bleaching stabilizer prepared in the example slowed down the ineffective decomposition of hydrogen peroxide and increased the stability of hydrogen peroxide in the process of bleaching fabrics.

[0085] Compared with Comparative Example 1, the bio-based oxygen bleaching stabilizers prepared in Examples 3-6 further inhibited the decomposition of hydrogen peroxide, and the decomposition rate of hydrogen peroxide decreased. The bio-based oxygen bleaching stabilizers prepared in Examples 5 and 6 inhibited the decomposition rate of hydrogen peroxide more significantly, indicating better stability for hydrogen peroxide. The decomposition rate of hydrogen peroxide in the working solution to which the oxygen bleaching stabilizer provided in Comparative Example 1 was added was still relatively fast, causing part of the hydrogen peroxide to be wasted, resulting in a decrease in fiber strength. The results of the determination of the decomposition rate of hydrogen peroxide when the bio-based oxygen bleaching stabilizers provided in Examples 1-6 and the oxygen bleaching stabilizer provided in Comparative Example 1 were added respectively are shown in FIG. Figure 1 shown.

[0086] Compared with Comparative Example 1, the bio-based oxygen bleaching stabilizers prepared in Examples 1-9 have a significant effect on Fe 3+ and Ca 2+ Has better chelating ability and is more effective for Fe 3+ The chelating ability is stronger. The bio-based oxygen bleaching stabilizer of the present invention chelates Fe 3+ and Ca 2+ Metal ions such as Fe 3+ Ineffective decomposition of hydrogen peroxide and by chelating Ca 2+ And starch grafted polyacrylic acid changes the calcium carbonate crystal form from stable calcite to the most unstable aragonite crystal form, effectively preventing the formation of calcium carbonate scale.

[0087] Compared with Comparative Example 1, the whiteness of the cloth sample after oxygen bleaching with the oxygen bleaching working solution of the bio-based oxygen bleaching stabilizer prepared in Examples 1-9 is 76.53-79.89, which is higher than the whiteness of 71.30 in Comparative Example 1, and the capillary effect and weft tear strength are also higher. The whiteness and capillary effect of the cloth sample after oxygen bleaching with the bio-based oxygen bleaching stabilizer of the present invention are better than those in Comparative Example 1, and the damage to the cloth sample is less.

[0088] Compared with Example 1, if the mass percentage of tetrasodium glutamate diacetate is too low (Example 8), the bio-based oxygen bleaching stabilizer chelates Ca 2+ The ability of the bio-based oxygen bleaching stabilizer to chelate Ca 2+ and Fe 3+ The ability of weft direction tearing strength is slightly increased, but not obvious, and the weft tearing strength is slightly reduced.

[0089] Compared with Example 1, if sodium gluconate is not added (Comparative Example 2), the bio-based oxygen bleaching stabilizer chelates Fe 3+ The ability of oxygen bleaching decreases rapidly, and the whiteness, gross value and weft tear strength of oxygen bleaching are reduced; if tetrasodium glutamate diacetate is not added (Comparative Example 3), the bio-based oxygen bleaching stabilizer chelates Ca 2+The ability of oxygen bleaching decreases rapidly, and the whiteness, gross effect value and weft tear strength of oxygen bleaching are reduced. It can be seen that the bio-based oxygen bleaching stabilizer prepared by combining sodium gluconate and tetrasodium glutamate diacetate as chelating agents has better performance.

[0090] Compared with Example 1, if polyepoxysuccinic acid is not added (Comparative Example 4), the bio-based oxygen bleaching stabilizer chelates Ca 2+ If starch grafted polyacrylic acid is not added (Comparative Example 5), the bio-based oxygen bleaching stabilizer chelates Ca 2+ The ability of the scale inhibitor also decreases. It can be seen that the bio-based oxygen bleaching stabilizer prepared by compounding polyepoxysuccinic acid and starch-grafted polyacrylic acid as scale inhibitors has better performance.

[0091] The applicant declares that the present invention illustrates the process method of the present invention through the above-mentioned embodiments, but the present invention is not limited to the above-mentioned process steps, that is, it does not mean that the present invention must rely on the above-mentioned process steps to be implemented. Those skilled in the art should understand that any improvement of the present invention, equivalent replacement of the raw materials selected by the present invention, addition of auxiliary components, selection of specific methods, etc., all fall within the protection scope and disclosure scope of the present invention.

Claims

1. A bio-based oxygen bleaching stabilizer, characterized in that: The raw materials for preparing the bio-based oxygen bleaching stabilizer include amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, starch graft, passivator and water.

2. The bio-based oxygen bleaching stabilizer according to claim 1, characterized in that The amino acid chelating agent includes tetrasodium glutamate diacetate.

3. The method according to claim 1 or 2, characterized in that: The starch grafted material comprises starch grafted polyacrylic acid.

4. The bio-based oxygen bleaching stabilizer according to any one of claims 1 to 3, characterized in that The passivating agent includes a magnesium salt.

5. The bio-based oxygen bleaching stabilizer according to any one of claims 1 to 4, characterized in that The magnesium salt includes magnesium sulfate and / or magnesium chloride.

6. The bio-based oxygen bleaching stabilizer according to any one of claims 1 to 5, characterized in that The raw materials for preparing the bio-based oxygen bleaching stabilizer include the following components by mass percentage: 10% to 20% of an amino acid chelating agent, 5% to 10% of sodium gluconate, 3% to 10% of polyepoxysuccinic acid, 5% to 15% of a starch graft, 5% to 20% of a passivating agent and 25% to 72% of water.

7. The bio-based oxygen bleaching stabilizer according to any one of claims 1 to 6, characterized in that The raw materials for preparing the bio-based oxygen bleaching stabilizer include the following components by mass percentage: 10% to 20% of tetrasodium glutamate diacetate, 5% to 10% of sodium gluconate, 3% to 10% of polyepoxysuccinic acid, 5% to 15% of starch-grafted polyacrylic acid, 5% to 20% of magnesium salt and 25% to 72% of water.

8. A method for preparing a bio-based oxygen bleaching stabilizer according to any one of claims 1 to 7, characterized in that: The preparation method comprises the steps of mixing and reacting an amino acid chelating agent, sodium gluconate, polyepoxysuccinic acid, a starch graft, a passivating agent and water to obtain the bio-based oxygen bleaching stabilizer.

9. The preparation method according to claim 8, characterized in that: The preparation method specifically comprises the following steps: (1) mixing sodium gluconate, a passivating agent and water to obtain a mixture; (2) mixing the mixture obtained in step (1), an amino acid chelating agent, polyepoxysuccinic acid and a starch graft, stirring and reacting to obtain the bio-based oxygen bleaching stabilizer; Preferably, the mixing further includes a filtering step.

10. Use of the bio-based oxygen bleaching stabilizer according to any one of claims 1 to 7 in a pre-treatment bleaching process of fabrics.

Citation Information

Patent Citations

  • Textile hydrogen peroxide bleaching stabilizer

    CN101643997A

  • Phosphorus-free biodegradable hydrogen peroxide bleaching stabilizer

    CN101798745A

  • Hydrogen peroxide bleaching stabilizer for cotton fabrics

    CN105019270A

  • Non-phosphorus and non-silicon oxygen bleaching stabilizer and manufacturing method thereof

    CN111560768A