Circuit board manufacturing method capable of avoiding ion migration
By selecting high-density fiberglass fabric materials and controlling the drilling, slag removal and hole metallization process, combined with environmental control, the problem of ion migration in circuit board manufacturing is solved, and the product insulation performance and stability are improved.
Patent Information
- Application Number
- CN202411205671.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-30
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-08-30
AI Technical Summary
ion migration is prone to circuit boards during manufacturing, resulting in degraded insulation performance and abnormal quality such as leakage. It is difficult for the existing technology to effectively avoid this problem.
By selecting high-density fiberglass fabric materials, controlling the drilling parameters and the removal process of slag, using black holes or conductive film processes to metallize the holes, and establishing a prevention mechanism under storage conditions to ensure minimum hole spacing and environmental control, and prevent metals Ion migration.
It effectively avoids the formation of ion migration channels, improves the quality and durability of the circuit board, and prevents metal ion migration problems caused by material moisture absorption.
Smart Images

Figure CN118984533A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of circuit board manufacturing, and in particular to a circuit board manufacturing method that avoids ion migration. Background Art
[0002] Conductive Anodic Filament (CAF) refers to the ionization of metals such as copper, silver, and tin on the circuit board under certain temperature and humidity conditions, and migration through the insulating layer to the other pole under the action of the electric field, resulting in a decrease in insulation performance. This failure mode of the circuit board is generally manifested as improper management and control in the previous production process after the adjacent through holes are copper-plated, such as the type of glass fiber cloth used, drilling method, drilling parameters, design, environment and other factors, resulting in the slow migration of copper ions along the glass fiber cloth, and then leakage.
[0003] In the process of circuit board manufacturing, the main situations where ion migration occurs are as follows: between holes, between holes and wires, between wires and between layers, such as Figure 1 In the four cases, ions migrate between the positive and negative electrodes, causing conduction between the insulation of the circuit board, resulting in quality abnormalities such as leakage.
[0004] In view of this, it is necessary to provide a circuit board manufacturing method that can avoid ion migration to solve the above technical problems. Summary of the invention
[0005] The technical problem to be solved by the present invention is to provide a circuit board manufacturing method that avoids ion migration, and to control the process from multiple aspects to avoid the formation of ion migration channels, thereby improving the quality of the product.
[0006] The technical solution of the present invention is as follows:
[0007] A method for manufacturing a circuit board to avoid ion migration comprises the following steps:
[0008] Select 1080 type glass fiber cloth material suitable for high-layer and high-density through-hole connection, fully soak it in epoxy resin, press it, cool it, and solidify it to obtain the circuit board substrate;
[0009] When drilling, the spindle speed of the drilling rig is ≥200kprm, the spindle swing is ≤20um, the air pressure is controlled at 0.6-0.7Mpa, the drill bit is selected within the second grinding, and the hole thickness is controlled to be ≤20um; when designing the drilling holes, according to the longitude and latitude of the glass fiber of the substrate, the holes are designed to be at an angle of 45° so that they are not on a glass fiber bundle;
[0010] After drilling, the hole wall is debonded. For double-sided circuit board debonding, the bath temperature is controlled at 75±3℃. The debonding solution used includes potassium permanganate / sodium permanganate with a concentration of 40-60g / L and sodium hydroxide with a concentration of 35-45g / L. The debonding amount is 0.05-0.25mg / cm 2 For desmearing of multi-layer circuit boards, the bath temperature is controlled at 85±3℃, the desmearing solution used includes potassium permanganate / sodium permanganate with a concentration of 75-85g / L and sodium hydroxide with a concentration of 48-58g / L, and the desmearing amount is 0.15-0.4mg / cm 2 ; In the desmearing process, the hexavalent manganese in the by-product is controlled to be less than 25g / L;
[0011] Specifically, when the double-sided circuit board is subjected to desmear treatment, the concentration of potassium permanganate / sodium permanganate is 40g / L, 50g / L or 60g / L, or other values within the range; the concentration of sodium hydroxide is 35g / L, 40g / L or 45g / L, or other values within the range; the desmearing amount is 0.05mg / cm 2 , 0.1mg / cm 2 , 0.15mg / cm 2 , 0.2mg / cm 2 or 0.25mg / cm 2 , or other values within this range;
[0012] When desmearing a multilayer circuit board, the concentration of potassium permanganate / sodium permanganate is 75g / L, 80g / L or 85g / L, and the concentration of sodium hydroxide can be 48g / L, 50g / L, 52g / L, 55g / L or 58g / L, or other values within the range; the desmearing amount is 0.15mg / cm 2 , 0.2mg / cm 2 , 0.3mg / cm 2 or 0.4mg / cm 2 , or other values within this range;
[0013] The hole metallization process is carried out by using black hole or conductive film technology, and then the copper plating is carried out to thicken the hole. The black hole or conductive film process forms an insulating layer between the electroplated copper and the hole wall to prevent the migration of metal ions.
[0014] Furthermore, the vacuum pressure of the drilling rig during drilling is controlled at -10 to -16 Kpa, such as -10 Kpa, -12 Kpa, -14 Kpa or -16 Kpa, or other values within the range.
[0015] Furthermore, when the circuit boards are stored, the ambient temperature is controlled at 16-26°C and the humidity is controlled at 40-70%; wherein the storage ambient temperature can be 16°C, 20°C, 25°C or 16°C, or other values within this range; the humidity can be 40%, 50%, 60% or 70%, or other values within this range.
[0016] Furthermore, when the circuit board is a multi-layer board, an annular ring design is added to the inner layer.
[0017] Furthermore, when designing the hole arrangement, the minimum hole spacing is determined by testing the ion migration failure time of different hole spacings.
[0018] Furthermore, the test conditions are: under the conditions of temperature 85° C., humidity 85%, and DC voltage 50V, the ion migration resistance is achieved for 1000 hours.
[0019] Compared with the prior art, the circuit board manufacturing method for avoiding ion migration provided by the present invention has the following beneficial effects:
[0020] 1. The circuit board manufacturing method for avoiding ion migration provided by the present invention can effectively avoid ion migration by controlling the type of substrate material used, drilling parameters, desmear parameters, hole metallization method, hole layout design, minimum hole spacing design and other processes during the production process, thereby improving product quality.
[0021] 2. The circuit board manufacturing method for avoiding ion migration provided by the present invention establishes a mechanism to prevent ion migration from the storage conditions to prevent the material from absorbing moisture and providing a channel for metal ion migration. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] In order to more clearly illustrate the technical solutions in the embodiments of the present invention, the following briefly introduces the drawings required for use in the description of the embodiments. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.
[0023] Figure 1 It is a schematic diagram of several forms of ion migration in the prior art;
[0024] Figure 2 This is a schematic diagram of the pulling effect after drilling holes in glass fiber cloth of different thicknesses;
[0025] Figure 3 It is a schematic diagram of drilling holes;
[0026] Figure 4 This is a schematic diagram showing the effect of the pore wall erosion degree on the formation of ion migration channels;
[0027] Figure 5 It is a schematic diagram of the ion migration isolation wall formed on the hole wall after drilling. DETAILED DESCRIPTION
[0028] In order to enable those skilled in the art to better understand the technical solutions in the embodiments of the present invention and to make the above-mentioned objects, features and advantages of the present invention more obvious and understandable, the specific implementation modes of the present invention are further described below.
[0029] It should be noted that the description of these embodiments is used to help understand the present invention, but does not constitute a limitation of the present invention. In addition, the technical features involved in each embodiment of the present invention described below can be combined with each other as long as there is no conflict between them.
[0030] A method for manufacturing a circuit board to avoid ion migration comprises the following steps:
[0031] (1) Selecting 1080 type glass fiber cloth material suitable for high-layer and high-density through-hole connection, fully impregnating it with epoxy resin, and then pressing, cooling, and curing it to obtain a circuit board substrate;
[0032] It has been found through experiments that if the density of the glass cloth is poor, metal ions will migrate through the loose gauze channels; in terms of CAF resistance, the looseness of the glass fibers needs to be considered, so the present invention selects a glass fiber cloth with better density.
[0033] Since drilling will cause pulling force on the sheet material, the solidified dielectric layer will be damaged. After electroplating, the pulled glass fiber will be copper plated to form an ion migration channel. Through experiments, it is found that the pulling effect of thin 1080 glass cloth is significantly smaller than that of thick 7628 glass cloth. Figure 2 Therefore, in the present invention, the substrate is selected to be 1080 type glass fiber cloth suitable for high multi-layer and high-density through-hole connection.
[0034] (2) When drilling, the spindle speed of the drill rig is ≥200kprm, the spindle swing is ≤20um, the air pressure is controlled at 0.6-0.7Mpa, the vacuum pressure is controlled at -10~-16Kpa, the drill bit is selected within the second grinding, and the hole thickness is controlled to be ≤20um. By limiting the drilling rig and drilling parameters, it is possible to prevent the glass fiber from being pulled during the drilling process and forming an ion migration channel after the hole is metallized; when designing the drilling holes, according to the longitude and latitude of the glass fiber on the substrate, the holes are designed to be at an angle of 45° so that they are not on a glass fiber bundle, thereby preventing the metal ions from migrating along the glass fiber bundle. The drilling arrangement is as follows: Figure 3 As shown;
[0035] At the same time, when designing the hole layout, the minimum hole spacing is determined by testing the failure time of ion migration resistance at different hole spacings. The test conditions are: 1000 hours of ion migration resistance at a temperature of 85°C, a humidity of 85%, and a DC voltage of 50V.
[0036] Preferably, when the circuit board is a multi-layer board, a hole ring design is added to the inner layer to prevent the mechanical force from pulling the hole wall during the drilling process and forming an ion migration channel after metallization.
[0037] (3) After drilling, the hole wall is desemarized. For desemarization of double-sided circuit boards, the bath temperature is controlled at 75°C. The desemarization solution used includes 50g / L potassium permanganate / sodium permanganate and 40g / L sodium hydroxide. The desemarization amount is 0.1mg / cm 2 For multi-layer circuit board desmearing, the bath temperature is controlled at 85°C, the desmearing solution used includes 80g / L potassium permanganate / sodium permanganate and 55g / L sodium hydroxide, and the desmearing amount is 0.3mg / cm 2 ; In the desmearing process, the hexavalent manganese in the by-product is controlled to be less than 25g / L;
[0038] Because the drill bit rotates at high speed, the hole wall after drilling is covered with a layer of drilling scum, which needs to be cleaned before metallization. The present invention can effectively avoid the problem of ion migration channel formed due to chemical erosion of the hole wall by controlling the composition and concentration of the desmear solution and the desmearing amount. Figure 4 As shown in the figure, the more times the glue is removed, the greater the hole wall erosion, the higher the probability of ion migration channels forming between holes, and the greater the probability of ion migration causing circuit board failure. Therefore, it is necessary to prevent the formation of ion migration channels by controlling the amount of glue removed.
[0039] (4) Use black hole or conductive film process to metallize the hole, and then electroplating copper to thicken it. The black hole or conductive film process forms an insulating layer between the electroplated copper and the hole wall, and forms an ion migration isolation wall on the hole wall to prevent metal ion migration, such as Figure 5 As shown;
[0040] (5) When the circuit board is stored after production, the ambient temperature is controlled at 25°C and the humidity is controlled at 40-70% to prevent the material from absorbing moisture and providing a channel for the migration of metal ions.
[0041] Therefore, the present invention starts from the types of substrate materials used, drilling parameters, desmear parameters, hole metallization methods, hole layout design, minimum hole spacing, storage conditions and other aspects, establishes a mechanism to prevent ion migration, and makes special control over the mode in which ion migration causes circuit board failure, so that the prepared circuit board effectively avoids the problems caused by ion migration and improves product quality.
[0042] The embodiments of the present invention are described in detail above, but the present invention is not limited to the described embodiments. For those skilled in the art, various changes, modifications, substitutions and variations made to these embodiments without departing from the principles and spirit of the present invention are still within the protection scope of the present invention.
Claims
1. A method for manufacturing a circuit board to avoid ion migration, characterized in that: The steps include: Select 1080 type glass fiber cloth material suitable for high-layer and high-density through-hole connection, fully soak it in epoxy resin, press it, cool it, and solidify it to obtain the circuit board substrate; When drilling, the spindle speed of the drilling rig is ≥200kprm, the spindle swing is ≤20um, the air pressure is controlled at 0.6-0.7Mpa, the drill bit is selected within the second grinding, and the hole thickness is controlled to be ≤20um; when designing the drilling holes, according to the longitude and latitude of the glass fiber of the substrate, the holes are designed to be at an angle of 45° so that they are not on a glass fiber bundle; After drilling, the hole wall is debonded. For double-sided circuit board debonding, the bath temperature is controlled at 75±3℃. The debonding solution used includes potassium permanganate / sodium permanganate with a concentration of 40-60g / L and sodium hydroxide with a concentration of 35-45g / L. The debonding amount is 0.05-0.25mg / cm 2 For desmearing of multi-layer circuit boards, the bath temperature is controlled at 85±3℃, the desmearing solution used includes potassium permanganate / sodium permanganate with a concentration of 75-85g / L and sodium hydroxide with a concentration of 48-58g / L, and the desmearing amount is 0.15-0.4mg / cm 2 ; In the desmearing process, the hexavalent manganese in the by-product is controlled to be less than 25g / L; The hole metallization is carried out by using black hole or conductive film process, and then the hole is thickened by electroplating copper. The black hole or conductive film process forms an insulating layer between the electroplated copper and the hole wall.
2. The method for manufacturing a circuit board for avoiding ion migration according to claim 1, characterized in that: When drilling, the vacuum pressure of the drilling rig is controlled at -10~-16Kpa.
3. The method for manufacturing a circuit board for avoiding ion migration according to claim 1, characterized in that: When storing circuit boards, the ambient temperature should be controlled at 16-26°C and the humidity should be controlled at 40-70%.
4. The method for manufacturing a circuit board for avoiding ion migration according to claim 1, characterized in that: When the circuit board is a multi-layer board, an aperture ring design is added to the inner layer.
5. The method for manufacturing a circuit board for avoiding ion migration according to claim 1, characterized in that: When designing the hole layout, the minimum hole spacing is determined by testing the ion migration failure time of different hole spacings.
6. The method for manufacturing a circuit board for avoiding ion migration according to claim 5, characterized in that: The test conditions are: 1000 hours of ion migration resistance at a temperature of 85°C, a humidity of 85%, and a DC voltage of 50V.
Citation Information
Patent Citations
Method for improving ionic migration of PCB
CN105592632A
Method for producing positively etched printed circuit board
CN108200734A
Manufacturing method for via hole metallization of rigid-flex printed circuit board
CN112672522A
Multilayer printed wiring board and manufacturing method therefor
JP2009176897A
Method for manufacturing flexible copper clad laminate with metalized through-hole
WO2015149580A1
Cited By
Circuit board CAF failure control method
CN120711622A