Manufacturing method of anti-bending signal cable

By combining the flattened and inflatable softened copper strips with fiber wires in the signal cables and designing with multi-layer shielding and insulating materials, the problem of insufficient bending performance of existing cables is solved, and higher signal transmission stability is achieved and anti-interference ability.

CN119008133APending Publication Date: 2024-11-22BAOJI FIBERHOME WIRE & CABLE CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411170638.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-23
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The existing signal cables are insufficient in terms of bending resistance and cannot meet the requirements for signal transmission stability in the fields of aviation, communication and other fields.

Method used

It is rolled into a copper strip with hard copper wire and then inflatrated and softened, wrapped around the fiber wire and combined with the round copper wire to form a conductor structure, and is designed through multi-layer shielding and insulating materials, including combined wire braiding and electrical isolation paper wrapping. Improve the bending resistance of the cable.

Benefits of technology

The electrical insulation and bending performance of the signal cable are significantly improved, so that it can be bent back and forth for 35,000 times without damage when it withstands tensile force of 20N, and improves the anti-interference ability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008133A_ABST
    Figure CN119008133A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of an anti-bending signal cable, and the method comprises the steps: flattening a hard copper wire to form a copper strip, carrying out the inflation CO2 softening, wrapping the softened copper strip on fibers, and combining the softened copper strip with a round copper wire to form a conductor structure for transmitting an electric signal; wrapping a first shielding layer outside the conductor structure to form a shielding wire core; the first shielding layer is formed by weaving a metal-covered wire; according to requirements, the plurality of shielding wire cores and the insulating wire cores are lined with reinforcing fibers according to a preset pitch to form a cable, and then the cable is wrapped by electrical isolation paper to form a wrapped cable core; the wrapping cable core is wrapped by a second shielding layer and an isolating layer to form a cable core. The multiple structures of the wire structure, the insulating material and the shielding layer are prepared, so that the electrical insulation performance and the bending performance of the cable are improved, and a shielding net or an insulating wire core is not damaged to form a cable core when the sheath of the cable is stripped.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of cable manufacturing, and in particular to a method for manufacturing a bending-resistant signal cable. Background Art

[0002] Most existing signal cables use pure copper wire as conductor and shield, and the outer covering insulation material provides protection for the internal metal wire to achieve the purpose of signal transmission, which cannot meet the actual use requirements. With the rapid development of aviation, communication, and electronic information in my country, improving the stable transmission of signals and video transmission and improving the bending resistance of the entire cable have become problems to be solved. Summary of the invention

[0003] In view of the above defects or shortcomings, an object of the present invention is to provide a method for manufacturing a bending-resistant signal cable.

[0004] To achieve the above purpose, the technical solution of the present invention is:

[0005] A method for manufacturing a bending-resistant signal cable, comprising:

[0006] After the hard copper wire is flattened to form a copper strip, it is inflated with CO2 to soften it. The softened copper strip is wrapped around the fiber wire and then bundled with the round copper wire to form a conductor structure for transmitting electrical signals.

[0007] A first shielding layer is wrapped around the conductor structure to form a shielded wire core; the first shielding layer is formed by braiding a combination of wires;

[0008] According to the requirements, multiple shielded wire cores and insulated wire cores are cabled with reinforcing fibers at a preset pitch, and then wrapped with electrical isolation paper to form a wrapped cable core;

[0009] A second shielding layer and an isolation layer are wrapped around the cable core to form a cable core.

[0010] The combined silk preparation process is as follows:

[0011] The hard copper wire is flattened into a copper strip, and after vacuuming, the pressure in the furnace is reduced to -0.1MPa, and then CO2 gas is filled into the furnace and pressurized to 0.2-0.3MPa;

[0012] Adopt annealing temperature 160~180℃ heating and heat preservation for 3h, after the gas in the furnace expands, the pressure does not exceed 0.45MPa, lift the furnace body out, and cool it for not less than 12h to soften it;

[0013] According to the tensile strength requirements, the copper tape is wound around the fiber wire to form the gold-skin fiber wire;

[0014] The gold-skin fiber wire and the pure copper wire are combined into a combined wire, and four groups of combined wires and 12 groups of copper wires are woven according to a preset pitch to form a combined wire.

[0015] The diameter of the tinned round copper wire or the bare round copper wire is 0.05-0.10 mm.

[0016] The diameter of the hard copper wire is 0.03-0.10 mm.

[0017] The diameter of the round copper wire is 0.03-0.05 mm, and the number is 100-200.

[0018] The shielding wire core is also wrapped with a first electrical isolation paper to form an isolation wire core.

[0019] The isolation layer is a second electrical isolation paper.

[0020] Compared with the prior art, the beneficial effects of the present invention are:

[0021] The present invention provides a method for manufacturing a bending-resistant signal cable. By preparing multiple structures of a conductor structure, an insulating material, and a shielding layer, the electrical insulation performance and the bending performance of the cable are increased, and the shielding net or the insulating wire core constituting the cable core is not damaged when the sheath is stripped off. A sheath is then extruded outside the cable core, so that the signal cable can be bent back and forth by ±90° under a tensile force of 20N and can withstand 35,000 times of unbroken circuits and short circuits with a bending resistance. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a flowchart of a method for manufacturing a bending-resistant signal cable of the present invention;

[0023] Figure 2 It is a specific control flow diagram of an embodiment of the present invention;

[0024] Figure 3 It is a schematic diagram of the cable structure of the present invention. DETAILED DESCRIPTION

[0025] The present invention will be described in detail below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, rather than all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the protection scope of the present invention.

[0026] like Figure 1 As shown, the present invention provides a method for manufacturing a bending-resistant signal cable, comprising:

[0027] S1. Flatten the hard copper wire to form a copper strip, then soften it with CO2, wrap the softened copper strip around the fiber wire, and then bundle it with the round copper wire to form a conductor structure for transmitting electrical signals;

[0028] Specifically, the hard copper wire is flattened into a copper strip, and after vacuuming, the pressure in the furnace is reduced to -0.1MPa, CO2 gas is filled into the furnace and pressurized to 0.2-0.3MPa; the annealing temperature is 160-180℃ and the temperature is kept at 3h. After the gas in the furnace expands, the pressure does not exceed 0.45MPa, and the furnace body is lifted out and cooled for not less than 12h to soften it. The first layer of weaving uses a gold-skinned wire combined with fine bare copper wire or tinned copper wire, and then combined with pure bare copper wire or tinned copper wire and alloy wire to form a conductor structure.

[0029] S2. Wrapping a first shielding layer outside the conductor structure to form a shielded wire core; the first shielding layer is formed by braiding a combination of wires;

[0030] Specifically, in S2, the combined yarn preparation process is:

[0031] 2.1. Flatten the hard copper wire into copper strips, evacuate the furnace to a pressure of -0.1 MPa, and then fill the furnace with CO2 gas to increase the pressure to 0.2-0.3 MPa;

[0032] 2.2. Heat and keep the annealing temperature at 160-180℃ for 3 hours. After the gas in the furnace expands, the pressure does not exceed 0.45MPa. Lift the furnace body out and cool it for at least 12 hours to soften it.

[0033] 2.3. According to the tensile strength requirements, the copper tape is wound around the fiber wire to form the gold-skin fiber wire;

[0034] 2.4. Weave the gold-skinned fiber wire with 2 to 3 tinned round copper wires or bare round copper wires to form a combined wire.

[0035] S3. After multiple shielded wire cores and insulated wire cores are cabled according to preset pitches and reinforced with fibers, they are wrapped with electrical isolation paper to form a wrapped cable core;

[0036] S4. Wrap the second shielding layer and the isolation layer around the cable core to form a cable core.

[0037] It should be noted that, in the present invention, the diameter of the tinned round copper wire or the bare round copper wire is 0.05-0.10 mm. The diameter of the hard copper wire is 0.03-0.10 mm. The diameter of the round copper wire is 0.03-0.05 mm, and the number is 100-200. The shielding core is also wrapped with a first electrical isolation paper to form an isolation core. The isolation layer is a second electrical isolation paper.

[0038] like Figure 2As shown, in this embodiment, a method for improving the bending resistance of a signal cable is to use multiple strands of fine and soft round copper wires and aramid wires with excellent tensile strength combined with a (0.03-0.10) mm hard copper, which is rolled flat, filled with CO2 and annealed, and then wrapped on nylon or aramid wire to form a conductor structure for transmitting electrical signals. This improves the bending performance of the cable from the conductor structure, from 500-600 times to 4000-5000 times, and the bending performance is improved by seven times. Second, a material with a higher elongation rate is used for the insulating material. Under the condition that the shielding effect of anti-interference and complex external environment can be met, a new method is used as much as possible to make the shielding wire core itself not bendable enough during the bending test, and after breaking, it is transformed into a cutter for the cable core. The original pure copper wire braiding or winding shield is changed into a combination of fine copper wire and micro hard copper wire rolled flat and annealed and wrapped on the fiber wire to form a gold skin wire and copper wire interval weaving to form a high-density shielding layer, which does not increase the outer diameter of the cable and can enhance the bending performance of the cable. In addition, it blocks the interference of external interference sources on the signal. The shielded cable core is wrapped with electrical isolation paper to form a wire core, which further increases its bending performance. After multiple shielded wire cores and insulated wire cores are lined with reinforcing fibers at a certain pitch, they are wrapped with thin electrical isolation paper to further improve the bending performance of the cable. Fine copper wires and 4 groups of combined braided wires are used outside the wrapped cable core according to a certain rule to weave the shielded wire core outside the cable core. First, it further improves the bending resistance of the cable, and second, it makes the cable have good anti-interference performance. A layer of electrical isolation paper 2 with a overlap of 1 / 3 is wrapped around the shielded core to increase the electrical insulation and bending performance of the cable. It can also prevent the shielding net or the insulating core from being damaged when the sheath is stripped off. The sheath is then extruded outside the cable core, so that the signal cable can be bent back and forth by ±90° under a tensile force of 20N and withstand 35,000 times of uninterrupted and short-circuited bending resistance.

[0039] The ideal embodiment of the present invention is described. Figure 2 The flow chart of the embodiment of the present invention is as follows: Figure 2As shown, this method wraps the capillary copper wire (0.03-0.05) mm with different strands according to the current carrying requirements of signal transmission. The new high-tech synthetic fiber aromatic polyamide fiber (100-200) denier has excellent mechanical properties, stable chemical structure, ideal mechanical properties, and excellent properties such as ultra-high strength, high modulus, high temperature resistance, acid and alkali resistance, light weight, and wear resistance. The strength is 5-6 times that of steel wire, the toughness is 2 times that of steel wire, and the weight is only about 1 / 5 of that of steel wire to form a conductor of the bending-resistant model line, which can increase the bending performance of the signal cable by 3 times. When selecting insulating materials, choosing those with excellent ductility and tensile properties can increase its bending properties. Wrap a thin electrical isolation paper around the cable core to prevent the copper wire shielding layer from breaking during the bending process and cutting the insulation. (4) When shielding external interference sources, the (0.03-0.10) mm hard copper wire is flattened into a small copper strip, and the pressure in the furnace is reduced to -0.1 MPa after vacuuming. CO2 gas is filled into the furnace to a pressure of (0.2-0.3) MPa. Heat at 160-180°C and keep warm for 3 hours. The pressure of the gas in the furnace after expansion shall not exceed 0.45MPa. The furnace body shall be lifted out and cooled for not less than 12 hours to soften it. According to the tensile strength requirements of the product, it is wound on different fiber wires to form gold-skin fiber wires. The gold-skin fiber wires are combined with (2-3) (0.05-0.10) mm tinned round copper wires or bare round copper wires. Due to the influence of the cable design outer diameter, shielding effect, welding difficulty, etc., this combination cannot be used in full, but 1 / 4 of it is used to increase the bending resistance of the cable. This method can increase the bending resistance of the cable by more than 3 times. The thin electrical isolation paper is continued to be wound around the shielded wire core. This method can increase the bending resistance of the cable by 7-8 times.

[0040] like Figure 3 As shown, for example: a cabling structure is made by the above-mentioned method for making a bending-resistant signal cable, and its structure includes high-tech synthetic fiber aromatic polyamide fiber 1, (0.03-0.05) mm capillary copper wire 2, insulating material 3, electrical isolation paper 4, (0.05-0.10) mm tinned round copper wire or bare round copper wire 5, gold-skinned fiber wire 6, and 0.06 mm electrical isolation paper 7.

[0041] The present invention is not limited to the above-described embodiments, and the method of using can be enlarged or reduced as required. In addition, various changes of materials can be arranged in the present invention.

[0042] It is obvious to those skilled in the art that the above-mentioned specific examples are only preferred embodiments of the present invention. Therefore, the improvements and changes that may be made by those skilled in the art to certain parts of the present invention still embody the principles of the present invention and achieve the purpose of the present invention, and all belong to the scope of protection of the present invention.

Claims

1. A method for manufacturing a bending-resistant signal cable, characterized in that: include: After the hard copper wire is flattened to form a copper strip, it is inflated with CO2 to soften it. The softened copper strip is wrapped around the fiber wire and then bundled with the round copper wire to form a conductor structure for transmitting electrical signals. A first shielding layer is wrapped around the conductor structure to form a shielded wire core; the first shielding layer is formed by braiding a combination of wires; According to the requirements, multiple shielded wire cores and insulated wire cores are cabled with reinforcing fibers at a preset pitch, and then wrapped with electrical isolation paper to form a wrapped cable core; A second shielding layer and an isolation layer are wrapped around the cable core to form a cable core.

2. The method for manufacturing a bending-resistant signal cable according to claim 1, characterized in that: The combined silk preparation process is as follows: The hard copper wire is flattened into a copper strip, and after vacuuming, the pressure in the furnace is reduced to -0.1MPa, and then CO2 gas is filled into the furnace and pressurized to 0.2-0.3MPa; Adopt annealing temperature 160~180℃ heating and heat preservation for 3h, after the gas in the furnace expands, the pressure does not exceed 0.45MPa, lift the furnace body out, and cool it for not less than 12h to soften it; According to the tensile strength requirements, the copper tape is wound around the fiber wire to form the gold-skin fiber wire; The gold-skin fiber wire and the pure copper wire are combined into a combined wire, and four groups of combined wires and 12 groups of copper wires are woven according to a preset pitch to form a combined wire.

3. The method for manufacturing a bending-resistant signal cable according to claim 2, characterized in that: The diameter of the tinned round copper wire or the bare round copper wire is 0.05-0.10 mm.

4. The method for manufacturing a bending-resistant signal cable according to claim 2, characterized in that: ss The diameter of the hard copper wire is 0.03-0.10 mm.

5. The method for manufacturing a bending-resistant signal cable according to claim 1, characterized in that: The diameter of the round copper wire is 0.03-0.05 mm, and the number is 100-200.

6. The method for manufacturing a bending-resistant signal cable according to claim 1, characterized in that: The shielding wire core is also wrapped with a first electrical isolation paper to form an isolation wire core.

7. The method for manufacturing a bending-resistant signal cable according to claim 1, characterized in that: The isolation layer is a second electrical isolation paper.