Method for reducing dust pollution of TOPCON battery piece in high-temperature process
By performing nitrogen purge before and after the high-temperature process in TOPCON battery cell production, the dust pollution problem is solved, the yield rate of the battery cell is improved, and the adhesion of dust particles and deformation of the silicon matrix structure is avoided.
Patent Information
- Application Number
- CN202411143949.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Dust pollution caused by high-temperature processes during TOPCON battery cells leads to the cleanliness of not meeting the requirements, and dust particles adhere to the surface of the semi-finished product, affecting the crystal structure of the silicon matrix, resulting in yield problems such as star-shaped cracks, black spots, and black spots.
Before the high-temperature reaction, the first purge removes the particulate matter in the furnace tube, and the second purge is carried out under low pressure to avoid dust adhesion. Combined with the diaphragm pump to form an airflow to ensure that the dust is removed .
It effectively prevents dust particles from entering the surface of the battery cell, reduces adverse manifestations, and improves the yield rate of TOPCON battery cells.
Smart Images

Figure CN119050199A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of TOPCON cell processing, and more specifically, to a method for reducing dust pollution in a high-temperature process of a TOPCON cell. Background Art
[0002] High-temperature process dust pollution refers to the dust generated by the high-temperature process itself during the production and manufacturing of TOPCON solar cells.
[0003] The high-temperature process is one of the core processes of TOPCON battery cells. The cleanliness of the high-temperature section has an important impact on the yield of the battery cells. A large amount of dust particles will be generated in the manufacturing process, resulting in the cleanliness not meeting the process requirements. The sources of dust particles are mainly from two aspects: one is the environmental factors of the production workshop, such as the machines and floor hygiene in the production workshop that do not meet the standards; the other is the boric acid and other particles generated during the process inside the furnace tube.
[0004] At present, a large amount of dust particles generated in the manufacturing process will adhere to the surface of the TOPCON battery cell semi-finished products. When the TOPCON battery cell semi-finished products undergo a high-temperature process, they are directly heated to the target temperature for reaction, causing the dust particles to directly enter the silicon matrix of the TOPCON battery cell, causing the crystal structure of the silicon to deform, and ultimately resulting in star-shaped cracks, black spots, black dots and other yield problems at the battery end. Summary of the invention
[0005] The purpose of this application is to provide a method for reducing dust pollution in the high-temperature process of TOPCON battery cells. This application reduces the impact of dust in the production and manufacturing process of TOPCON battery cells and improves the yield rate of TOPCON battery cells.
[0006] The present application provides a method for reducing dust pollution in a high-temperature process of a TOPCON cell, the method comprising:
[0007] Before opening the furnace door of the furnace tube required for high temperature reaction, the furnace tube is purged for the first time with nitrogen;
[0008] After the first purge is completed, check whether the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened;
[0009] When it is detected that the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened, the operation procedures of opening the furnace door, releasing the boat and closing the furnace door are performed in sequence;
[0010] After the furnace door of the furnace tube was closed, a second purge of the furnace tube was performed with nitrogen.
[0011] In one implementation, the process parameters of the first purge and the second purge include nitrogen flow rate, purge pressure, purge temperature and purge time.
[0012] In one implementation, the nitrogen flow rate, purge pressure, and purge time of the first purge are consistent with those of the second purge.
[0013] In one implementation, the purge process is as follows: adjusting the flow rate of nitrogen during the purge process to a maximum flow rate and adjusting the purge pressure to be less than a pressure value at which the furnace door can be opened.
[0014] In one implementation, the purge time is inversely proportional to the value of the purge pressure.
[0015] In one implementation, the maximum flow rate of the nitrogen is 20000r.
[0016] In one implementation, the purge temperature of the second purge is greater than the purge temperature of the first purge.
[0017] In one implementation, the purge pressure has a value range of greater than or equal to 500 mbar and less than 1000 mbar.
[0018] In one implementation, the pressure parameters and temperature parameters of the furnace door opening, boat placing and furnace door closing operations are consistent.
[0019] In one implementation, the nitrogen flow rate is kept consistent during the first purge, the detection of whether the real-time pressure of the furnace tube is a pressure value at which the furnace door can be opened, and the second purge.
[0020] Compared with the prior art, this application has the following beneficial effects:
[0021] In a method for reducing dust pollution in the high-temperature process of TOPCON cells provided in the present application, by making improvements on the basis of the existing high-temperature process, before opening the furnace door of the furnace tube required for the high-temperature reaction, under the condition of ensuring that it is lower than the normal pressure of the furnace tube, a first purge process is added, that is, the furnace tube is purged for the first time by nitrogen, so that the diaphragm pump can be used to form an airflow blowing to the tail of the furnace tube, so as to take away the particles inside the quartz tube before the high-temperature process begins, wherein ensuring that it is lower than the normal pressure of the furnace tube is conducive to quickly removing the particles such as boric acid generated during the process inside the furnace tube. Secondly, before the process of the TOPCON cell semi-finished product undergoing the high-temperature reaction, the second purge is performed under the set pressure conditions, which can avoid the dust particles caused by environmental factors such as the machine and the ground hygiene not meeting the standards from adhering to the surface of the TOPCON cell semi-finished product. In summary, the present application directly avoids the appearance of dust particles on the surface of the TOPCON cell semi-finished product, thereby solving the problem that the dust particles enter the silicon substrate and cause the subsequent crystal structure deformation of the silicon. Therefore, the high-temperature process improved based on the method provided by the present application can improve the yield rate of the TOPCON cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The drawings described herein are used to provide a further understanding of the embodiments of the present application, constitute a part of the present application, and do not constitute a limitation on the embodiments of the present application. In the drawings:
[0023] Figure 1 A schematic flow chart of a method for reducing dust pollution in a high-temperature process of TOPCON cells provided in an embodiment of the present application. DETAILED DESCRIPTION
[0024] In order to make the objectives, technical solutions and advantages of the present application more clearly understood, the present application is further described in detail below in conjunction with examples and drawings. The illustrative implementation scheme of the present application and its description are only used to explain the present application and are not intended to limit the present application.
[0025] It should be noted that the terms "include" or "may include" used in various embodiments of the present application indicate the presence of the function, operation or element applied for, and do not limit the addition of one or more functions, operations or elements. In addition, as used in various embodiments of the present application, the terms "include", "have" and their cognates are only intended to indicate specific features, numbers, steps, operations, elements, components or a combination of the foregoing items, and should not be understood as first excluding the presence of one or more other features, numbers, steps, operations, elements, components or a combination of the foregoing items or the possibility of adding one or more features, numbers, steps, operations, elements, components or a combination of the foregoing items.
[0026] First, the process steps of the high temperature process provided by the prior art are described as follows: start → open furnace door → place boat → close furnace door → heat up → heat up → constant temperature → leak detection → heat up → oxidation → diffusion → constant temperature → diffusion → constant temperature → diffusion → heat up → heat up → deep diffusion → cool down → cool down → nitrogen filling → open furnace door → take boat → close furnace door → end. The above process steps are the conventional process steps of the current high temperature process, a total of 26 process steps, which can be defined by digital numbers 1-26 in order, among which the diffusion is currently more common phosphorus diffusion and boron diffusion, which is a more conventional diffusion process, and this embodiment does not make a specific description, and secondly, for the 26 processes described above, the values of their respective process time, process pressure, process temperature, process humidity, and nitrogen flow rate are conventional technical means in the field of this technology, and this embodiment does not make a detailed introduction.
[0027] Please refer to Figure 1 , Figure 1 A schematic diagram of a method for reducing dust pollution in a high-temperature process of a TOPCON cell provided in an embodiment of the present application is shown in FIG. Figure 1 As shown, the method includes:
[0028] S101, before opening the furnace door of the furnace tube required for high temperature reaction, the furnace tube is purged for the first time with nitrogen.
[0029] In this embodiment, combined with the process steps of the high temperature process described in the above embodiment, it can be known that before the furnace door of the furnace tube required for the high temperature reaction is opened, that is, before the furnace door opening process, the furnace tube is purged for the first time by nitrogen. Specifically, in the first purging process, the three parameters mainly considered are pressure, purging time and nitrogen flow rate. The requirements for setting the above three parameters are: in order to increase production capacity and reduce costs, the process time is as short as possible under the premise of ensuring quality. After experimental verification, when the pressure is 500mbar, the purpose of purging dust particles can be achieved, but it takes more time to return to the normal pressure of opening the furnace door, which eventually leads to a longer overall process time, and does not meet the requirements of setting the above three parameters. When the pressure is 1000mbar, there is no pressure difference in the furnace tube, the gas flow rate is the slowest, there is no purging effect, and the dust particles cannot be reduced. Therefore, the numerical range of the purging pressure is greater than or equal to 500mbar and less than 1000mbar, that is, 500mbar≤P<1000mbar, and P represents the purging pressure. Therefore, the purge pressure of the first purge provided in this embodiment is 800 mbar, which can ensure that the purge purpose is achieved and the process time is short. Under the same conditions, the larger the nitrogen flow rate, the better the purge effect and the shorter the time. Combined with the current process equipment, the maximum nitrogen flow rate is determined to be 20000r. For example, when the purge pressure of the first purge is 800 mbar, the purge time is 120s.
[0030] S102, after the first purge is completed, detecting whether the real-time pressure of the furnace tube is a pressure value at which the furnace door can be opened.
[0031] In this embodiment, since the purge pressure is adjusted during the purge, and the purge pressure is lower than the normal pressure at which the furnace door of the furnace tube is opened, if the normal pressure is not returned, the pressure outside the furnace tube will be higher than the pressure inside the furnace tube, and the furnace door of the furnace tube cannot be opened. Therefore, after the first purge in step S101 is executed, the normal pressure return detection provided in this embodiment needs to be executed, that is, whether the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened. When the detected real-time pressure is the pressure value at which the furnace door can be opened, the subsequent furnace door opening process can be executed.
[0032] S103, when it is detected that the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened, the operation procedures of opening the furnace door, releasing the boat and closing the furnace door are performed in sequence.
[0033] In this embodiment, based on the implementation scheme described in step S102 above and the conventional technical process flow of the high-temperature process provided by the prior art, when it is detected that the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened, the operation procedures of opening the furnace door, releasing the boat and closing the furnace door are sequentially performed. It can be understood that the process parameters (such as temperature, humidity, etc.) of the operation procedures of opening the furnace door, releasing the boat and closing the furnace door sequentially performed in this embodiment are common sense for those skilled in the art, and no unnecessary explanation is given in this embodiment.
[0034] S104, after the furnace door of the furnace tube is closed, the furnace tube is purged for the second time with nitrogen.
[0035] In this embodiment, the temperature of the process parameters of the second purge is consistent with the remaining operating procedures (i.e., heating) of the high-temperature process. This is to facilitate the subsequent heating process, save the time required for heating, and reduce the time of the entire high-temperature process. For example, the temperature of the process parameters of the second purge can be 880 degrees Celsius, but the remaining process parameters are consistent with the first purge recorded in step S101, so this embodiment does not make unnecessary elaboration.
[0036] The method provided in this embodiment first purges the furnace tube with nitrogen for the first time before opening the furnace door of the furnace tube required for the high-temperature reaction (as the second step of the original high-temperature process), and sets the furnace tube pressure to be lower than normal pressure, which is conducive to quickly removing the boric acid and other particulate matter generated in the process inside the furnace tube. Secondly, after the first purge (step 2) is completed, the furnace door can be opened smoothly by returning to normal pressure (as the third step of the original high-temperature process) (then the process of opening the furnace door of the original high-temperature process is postponed to step 4). If it does not return to normal pressure, the pressure outside the furnace tube is greater than that inside the furnace tube, and the furnace door cannot be opened. Finally, the semi-finished battery cell is purged for the second time under the set pressure before the high-temperature reaction (in addition to opening the furnace door, placing the boat and closing the furnace door as steps 4-6 respectively, so the second purge provided in this embodiment is the seventh step of the improved high-temperature process), which can avoid the dust particles caused by environmental factors such as the machine and ground hygiene not meeting the standards from adhering to the surface of the semi-finished battery cell.
[0037] Therefore, steps 2, 3, and 7 directly prevent dust particles from appearing on the surface of the semi-finished battery cells, thereby solving the problem of dust particles entering the silicon substrate and causing deformation of the crystal structure, and improving the yield rate of TOPCON battery cells.
[0038] In this embodiment, the verification of the proportion of star-shaped cracks, black spots, and black spots before and after the improvement of the high-temperature process is also given. It should be noted that the experimental premise of the verification is that the parameter settings of the process steps of the unimproved high-temperature process are consistent, and secondly, the data of the experimental processes such as boron diffusion, alkali polishing, and phosphorus diffusion are also consistent. Finally, when there is no purge process, the main defects of TOPCON battery cells are star-shaped cracks accounting for 1.00%, black spots accounting for 0.66%, and black spots accounting for 0.19%. When the purge process is added, the main defects of TOPCON battery cells are grid line cracks accounting for 0.67%, virtual printing accounting for 0.67%, and basket printing accounting for 0.31%. It is verified that the star-shaped cracks are 0pcs, and the star-shaped cracks account for 0.00%; the black spots are 3pcs, and the black spots account for 0.15%; the black spots are 0pcs, and the black spots account for 0.00%. Therefore, it can be seen that the method for reducing dust pollution in the high-temperature process of TOPCON battery cells provided in the embodiment of the present application can effectively reduce the adverse performance of TOPCON battery cells caused by dust, thereby improving the yield rate of TOPCON battery cells.
[0039] It is understandable that after the second purge is completed, the remaining operation steps are performed according to the flow of the high-temperature process of the TOPCON battery cell. The remaining operation steps have been mentioned above and will not be repeated here.
[0040] In some embodiments, the purge process is performed by adjusting the flow rate of nitrogen during the purge process to a maximum flow rate and adjusting the purge pressure to be less than a pressure value at which the furnace door can be opened.
[0041] In this embodiment, the maximum flow rate during the purging process is 20000r, the pressure value at which the furnace door can be opened is 1000mbar, and the purging pressure is 800mbar.
[0042] In some embodiments, the purge time is inversely proportional to the value of the purge pressure.
[0043] It can be understood that the functional relationship between the purge time and the purge pressure is a curve graph, that is, it is not an inversely proportional change.
[0044] In some embodiments, the purge temperature of the second purge is greater than the purge temperature of the first purge.
[0045] In this embodiment, the purge temperature of the second purge is divided into six gradients, and the temperatures of the six gradients are all 880 degrees Celsius. The purge temperature of the first purge is also divided into six gradients, among which the temperatures of gradients one and two are both 820 degrees Celsius, and gradients three to six are all 800 degrees Celsius.
[0046] In some embodiments, the pressure parameters and temperature parameters of the furnace door opening, boat placing and furnace door closing operations are consistent.
[0047] In this embodiment, the pressure parameters for opening the furnace door, placing the boat, and closing the furnace door are all 1000 mbar, and the temperature parameters are divided into six gradients, which are briefly described as gradients one to six in this embodiment, where the temperature of gradients one and two is 820 degrees Celsius, and the temperature of gradients three to six is 800 degrees Celsius.
[0048] In some embodiments, the nitrogen flow rate during the first purge, the detection of whether the real-time pressure of the furnace tube is a pressure value at which the furnace door can be opened, and the second purge remain consistent.
[0049] In this embodiment, the nitrogen flow rate during the first purge, the detection of whether the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened, and the second purge is 20000r.
[0050] Therefore, in a method for reducing dust pollution in the high-temperature process of TOPCON cells provided in an embodiment of the present application, improvements are made on the basis of the existing high-temperature process technology. Before opening the furnace door of the furnace tube required for the high-temperature reaction, a first purge process is added while ensuring that it is lower than the normal pressure of the furnace tube. That is, the furnace tube is purged for the first time with nitrogen, so that the diaphragm pump can be used to form an airflow blowing to the tail of the furnace tube, so as to take away the particles inside the quartz tube before the high-temperature process begins. Ensuring that it is lower than the normal pressure of the furnace tube is conducive to the rapid removal of particles such as boric acid generated during the process inside the furnace tube. Secondly, before the TOPCON cell semi-finished product undergoes a high-temperature reaction process, a second purge is performed under set pressure conditions to prevent dust particles from adhering to the surface of the TOPCON cell semi-finished product due to environmental factors such as substandard machine and ground hygiene. In summary, the present application directly avoids the appearance of dust particles on the surface of the semi-finished TOPCON battery cell, thereby solving the problem of dust particles entering the silicon substrate and causing subsequent deformation of the silicon crystal structure. Therefore, the high-temperature process improved based on the method provided in the present application can improve the yield rate of TOPCON battery cells.
[0051] The specific implementation methods described above further illustrate the purpose, technical solutions and beneficial effects of the present application in detail. It should be understood that the above description is only the specific implementation method of the present application and is not intended to limit the scope of protection of the present application. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present application should be included in the scope of protection of the present application.
Claims
1. A method for reducing dust pollution in the high-temperature process of TOPCON cells. Characterized in that the method include: Before opening the furnace door of the furnace tube required for high temperature reaction, the furnace tube is purged for the first time with nitrogen; After the first purge is completed, check whether the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened; When it is detected that the real-time pressure of the furnace tube is the pressure value at which the furnace door can be opened, the operation procedures of opening the furnace door, releasing the boat and closing the furnace door are performed in sequence; After the furnace door of the furnace tube was closed, a second purge of the furnace tube was performed with nitrogen.
2. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 1, It is characterized in that The process parameters of the first purge and the second purge include nitrogen flow rate, purge pressure, purge temperature and purge time.
3. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 2, It is characterized in that The nitrogen flow rate, purge pressure and purge time of the first purge are consistent with those of the second purge.
4. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 3, It is characterized in that The execution process of purging is: adjusting the flow rate of nitrogen during purging to be at the maximum flow rate and adjusting the purging pressure to be lower than the pressure value at which the furnace door can be opened.
5. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 4, It is characterized in that The purge time is inversely proportional to the value of the purge pressure.
6. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 4, It is characterized in that The maximum flow rate of the nitrogen is 20000r.
7. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 2, It is characterized in that The purge temperature of the second purge is greater than the purge temperature of the first purge.
8. A method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 2, It is characterized in that The purge pressure has a numerical range of greater than or equal to 500 mbar and less than 1000 mbar.
9. The method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 1, It is characterized in that The pressure parameters and temperature parameters of the furnace door opening, boat placing and furnace door closing operation procedures are consistent.
10. The method for reducing dust pollution in a high-temperature process of TOPCON cells according to claim 1, It is characterized in that The nitrogen flow rate is kept consistent during the first purge, the detection of whether the real-time pressure of the furnace tube is a pressure value at which the furnace door can be opened, and the second purge.
Citation Information
Patent Citations
Solar cell and manufacturing method thereof
CN111063766A
Oxidation process of PERC battery
CN115036394A
Boron diffusion method and device for TOPCon battery
CN116387400A
Method for reducing cross subfissure rate of polycrystalline silicon layer in TopCon battery
CN117352598A
Horizontal diffusion furnace and solar cell production method
WO2017115573A1