Device, in particular a composite beam, and method for producing and detaching said device

By using the swelling properties of fiber composites in wood to form friction connections and shape-fitting locking, wood durability and dismantling problems are solved, high-strength, low-cost wood-metal composite beams are achieved, and the production and recycling process is simplified.

CN119053416APending Publication Date: 2024-11-29HYCOBILITY ENGINEERING & TECHNOLOGIES GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202280095000.7
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2022-04-19
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

In the prior art, wood has insufficient durability in outdoor environments, especially when carrying static and dynamic loads, and the use of wood and metal composite materials has difficulties in disassembly and recycling, resulting in high manufacturing costs and environmental pollution.

Method used

Using hollow profile devices with hygroscopic fiber composite materials, the swelling properties of the fiber composite materials generate pressure when in contact with the fluid, forming frictional connections and shape-fitting locking, improving the strength and durability of the wood, and through fluid sealing and chemical treatment Enhance connection stability for easy disassembly and recycling.

Benefits of technology

It achieves improved strength and durability of wood, reduces fatigue strength load, simplifies the production and disassembly process, reduces material usage and carbon dioxide emissions, and improves the mechanical properties of composite materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119053416A_ABST
    Figure CN119053416A_ABST
Patent Text Reader

Abstract

The invention relates to a device (1), in particular a composite beam, comprising: an outer body (2) having an inner part (4); and a core (3) arranged in said interior (4), in which: the core (3) comprises or is formed from a fibrous composite material, in particular wood, which is swellable upon contact with a fluid; and the core (3) in the interior (4) is swelled by a fluid in the operating state and the pressure resulting from the swelling is applied to the outer body (2).
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to an apparatus, in particular a composite beam, and methods for manufacturing and disassembling the apparatus. Background Art

[0002] Beam-like devices or load-bearing elements are designed to adapt to the loads and are known in the prior art in different material variations. On the one hand, steel beams in particular are used in the construction industry due to their high load-bearing capacity. On the other hand, wooden beams are also used for construction purposes and are a particularly ecological material for construction works.

[0003] For the reasons mentioned above, the use of wood as a material is often desirable, but for decades the durability of wood in outdoor areas has been a major challenge for wood technology and the use of wood in technical elements. This requirement very quickly becomes a limiting factor, especially when supporting components or beams are subject to static and dynamic loads, since wood loses strength and stiffness over long periods of time, sometimes significantly, due to abiotic and biotic degradation.

[0004] The use of wood in technical applications presents technical and procedural challenges. Highly anisotropic materials and raw materials require precise material expertise in their application. On the one hand, innovative, efficient and cost-effective solutions can be achieved using homogeneous and isotropic materials such as steel and plastics, which in many cases are technically feasible with wood but are not competitive from an economic point of view due to more complex and delicate forming.

[0005] Furthermore, calculations are easier to make relative to homogeneous materials such as plastics and metals, and these materials are also easier to control. This predictability has only been available for a relatively short time for wood.

[0006] In the past, wood was also widely used in various technical products and devices. Another disadvantage of wood is its relatively low energy absorption in the event of fracture due to its brittle failure under tension. In the event of tensile fracture, mainly sharp-edged fracture surfaces are observed, which can lead to an increased risk of injury to people involved in accidents, for example.

[0007] In order to overcome these disadvantages, chemical and / or physical modification of wood is known in the prior art. Various methods are used to modify or impregnate wood cross sections in whole or in part, which improves the properties of the material. In addition to increasing durability and minimizing swelling, thermal denaturation initially leads to a slight improvement in mechanical properties (rigidity and strength), a reduction in density and hygroscopicity. However, wood modification leads to mechanical changes, such as embrittlement, and additional costs.

[0008] Another way to improve the durability of wood is to coat it. However, coating does not fully guarantee protection. Impregnation with protective agents requires additional costs and involves the release of environmentally harmful substances. On the other hand, plastic housings have disadvantages when it comes to disposal and recycling after the component has been used.

[0009] While wood-metal composites are known to overcome the shortcomings of wood, they represent a group of materials that have received little use and scientific research to date.

[0010] Steel is known to have a high elastic limit and significantly better strength properties, particularly isotropic strength properties, than wood. However, the thermal conductivity of steel is also increased compared to wood, so that steel beams are naturally designed to conduct more heat in a building than wood or similar fibrous materials. There may be limitations to the use of wood compared to other building materials, particularly due to weather conditions.

[0011] Currently, previous considerations include gluing and screwing wood and metal parts together. In some cases, the two materials are joined by a plastic shell. These technical solutions also almost always involve major problems regarding disassembly and recycling.

[0012] The use of additional connecting means has considerable disadvantages, wherein, for example, holes are provided in the beam and the individual components of the composite beam are ultimately screwed together. This may require a notched cross section, which may represent a weak point in the structure in terms of strength, since the necessary holes for the screw connection may lead to cracking of the notches. In addition, composite beams formed using connecting means also lead to increased manufacturing costs. Summary of the invention

[0013] Therefore, the problem of providing a device that overcomes the disadvantages of the prior art and combines certain advantageous properties of fiber composite materials, in particular wood and metal, can be considered as a conflict of objectives. Optionally, an object of the present invention is to overcome these conflicts of objectives. Optionally, another object of the present invention is to provide a durable beam with improved thermal and strength properties for ecological building and construction projects, without forming load-critical cut-out points that impair the fatigue strength of the beam. Optionally, another object of the present invention is to provide a device, in particular a composite beam, which is particularly easy to produce, but can also be disassembled or recycled.

[0014] These and other objects are optionally solved by an apparatus and a method having the features of the independent claims.

[0015] The invention is based in particular on the observation that in particular hygroscopic fiber composites, such as wood, have the property of undergoing strong dimensional changes when absorbing polar fluids, i.e. liquids or gases, in particular when absorbing water, for example through contact with water or changes in humidity and / or temperature.

[0016] The introduction of polar fluids into a fiber composite structure results in an increase in the volume of the material. In the context of the present invention, this increase in volume is alternatively also referred to as swelling. In addition to water, these swelling phenomena may also be caused by various polar liquids and substances such as saline solutions, alcohols, ammonia, etc. Removing fluids from the fiber composite material in turn results in a decrease in volume, also referred to as shrinkage.

[0017] The volume change is only very small in the longitudinal direction, i.e. in the fiber direction of the fiber composite material, but occurs mainly transversely to the fiber direction. In particular, in the context of the present invention, swellable fiber composite materials, such as wood, have a main extension direction of the fibers. Swelling occurs in particular transversely to the main extension direction of the fibers.

[0018] Swelling and shrinkage are generally considered to be the main technical disadvantages in wood technology. In the prior art, attempts are often made to counteract volume changes in wood. However, in the context of the present invention, it has surprisingly been achieved to utilize the swelling properties of fiber composite materials in an advantageous manner in order to solve at least one of the mentioned objects.

[0019] The device according to the invention optionally comprises an outer body formed of a hollow profile with an interior space and a core arranged in the interior space, wherein the core comprises or is formed of a fiber composite material, in particular wood, which is swellable when in contact with a fluid. Optionally, it is proposed that the core is swollen by the fluid in the interior space, in particular in the operating state, and exerts the pressure generated by the swelling on the outer body.

[0020] In a preferred embodiment, the core is formed of or comprises wood.Alternatively or additionally, other materials may also be used, in particular bio-based or technical materials, which have a corresponding volume increase due to water or other liquids or gas absorption or chemical reaction.

[0021] The swelling property, in particular the hygroscopicity of the core can enable the core to be permanently bonded to the outer body. In particular, this can achieve at least one friction connection, in particular a form and friction connection, between the core and the outer body, in particular the inner surface of the outer body.

[0022] The volume change of the core due to its swelling optionally leads to a plastic deformation of the core in the region of the contact surface of the outer body and the core. This compression zone adjacent to the contact surface may also be referred to as a compaction zone. In particular, the resulting compaction of the core, in particular of wood, transversely to the fibers leads to a significant increase in strength and stiffness along the fibers.

[0023] Besides wood, for example nanocellulose materials can also be used as fiber composite materials. Optionally, the core comprises a compressed facing material.

[0024] Depending on the curvature of the contact surface, the maximum equivalent stress acts in the core close to the outer surface of the core, so that a compressive deformation optionally occurs in the compaction area, resulting in an outward force against the outer body. This force generates a normal force at the contact surface, especially forming a friction connection in the transverse direction of the beam.

[0025] In the context of the present invention, a beam is understood to be any elongated element or component which, in particular, has a dimension in the longitudinal extension direction which is greater than a maximum dimension transversely to the longitudinal extension direction. In the context of the present invention, a composite beam may be, for example, a load-bearing composite element. Such a beam may be used, for example, as a beam for building structures, as a pillar for a chassis or body of a vehicle, as a supporting element for lightweight structures, as a beam for mechanical engineering structures, etc.

[0026] Positive-locking elements may optionally be provided to enable an additional positive connection between the outer body and the core. Such positive-locking elements may be designed in different ways. For example, at least one positive-locking extension, for example in the form of a rib, may be arranged on the inner surface of the outer body. When the device is in an operating state, the positive-locking extension may be pressed into a part of the core, whereby a positive connection may be obtained. Optionally, the core may also have a positive-locking recess, in which the positive-locking extension engages. The positive-locking recess may be, for example, a groove.

[0027] The core and the outer body optionally extend along a common main extension direction, and the hollow outer body preferably surrounds the core at least laterally, so that optionally there is a lateral connection between the outer body and the core. Therefore, the main extension direction is particularly considered to be the direction corresponding to the maximum spatial extension of the device. In particular, the lateral direction is considered to be a direction pointing orthogonally away from the main extension direction. In particular, the swelling of the core can be radial as well as tangential.

[0028] In particular, a cross section of the beam is to be understood as a surface cross section extending transversely to the longitudinal extension direction. For example, the outer body can be a tube, wherein the cross section of the outer body is therefore circular and, in particular, closed. The term "closed cross section" therefore refers in particular to a continuous cross section without interruptions, in particular in the case of a tube cross section.

[0029] Optionally, it is provided that in the operating state the core exerts an internal pressure which acts on the outer body. The pressure which is distributed as evenly as possible enables the compacted region in which the compression deformation occurs to be formed over a wide area.

[0030] It can also be provided that the outer body has a closed cross section. This can ensure that deformation of the cross section is avoided as much as possible when the composite beam is subjected to load. In particular, the closed cross section ensures a uniform distribution of pressure between the core and the inner surface of the outer body.

[0031] In particular, the pressure exerted by the core on the outer body in the operating state is at least 3 N / mm 2 , in particular at least 5 N / mm 2 or at least 10N / mm 2 Thus, under the usual friction conditions between wood and steel, a sufficiently large normal force can be generated so that the core is held in the outer body.

[0032] Optionally, provision is made that, in the operating state, the core is supported in the inner space. Thus, if the composite beam is subjected to particularly high loads, the core can still remain dimensionally stable, in particular in the outer body, while the beam deforms, without relative movements occurring at the contact surfaces.

[0033] Preferably, it is proposed that the outer body is designed as a metal profile, in particular a steel profile. This can provide an outer body that is particularly suitable for the building industry or other construction, such as automotive engineering, mechanical engineering or plant engineering. Optionally, the device can be used as a covering, for example instead of a brick or steel covering.

[0034] Optionally, it is proposed that the core is insertable and / or removable into the inner space in the engaged state, wherein the core is more swollen in the operating state than in the engaged state due to fluid absorption, and / or wherein the core has a higher fluid content in the operating state than in the engaged state. In particular, the core is loosely included in the outer body in the engaged state, and in particular, there is no friction connection between the inner surface of the core and the outer body.

[0035] In particular, the dimensions of the cores are selected so that they can be pushed or inserted in the connected state into the inner space of an outer body, such as a molded pipe, an extrusion, etc. Optionally, the shape of the cores is selected so that the desired cross section is produced by material contraction during reduction of the fluid content.

[0036] Optionally, it can be provided that the core and the interior space have a clearance fit in the engaged state, wherein the core is optionally undersized relative to the interior space. This can be used to determine the degree of frictional engagement between the core and the outer body in the swollen state. Furthermore, in the engaged state, the core can be easily removed from the interior space of the outer body.

[0037] It can be proposed that, in the operating state, the core completely fills the inner space of the outer body. In this way, the outer surface of the core can be completely enclosed by the outer body, and a firm connection between the bodies is achieved.

[0038] Optionally, it is proposed that in the operating state, the core is fluid-tightly enclosed. Thus, the core can be protected from fluid loss and shrinkage of the swelling in the swollen state. In particular, permanent stability of the device can be achieved.

[0039] Preferably, it is proposed that the core is enclosed in a fluid-tight manner by an outer body and at least one closure arranged on the outer body. This can be another measure to prevent fluid loss. Alternatively or additionally, the core can be enclosed in a fluid-tight manner. In the context of the present invention, fluid-tightness refers in particular to the property that the material is substantially impermeable to fluids, in particular to fluids that cause the core to swell. For example, in the case where the fluid is water, fluid-tightness means in particular that the material is substantially impermeable to water in liquid and gaseous form.

[0040] Optionally, it is provided that the fluid is selected from one or more of the following fluids: water, salt solution, alcohol, ammonia. The preferred fluid is water. Thus, the hygroscopic effect of wood can be utilized.

[0041] In particular, it is provided that the core has a compacted region along its outer circumference. Thus, the normal force for the friction connection can be generated as a result of the core deformation. In addition, the mechanical properties of the core material are further improved in the compacted region.

[0042] Alternatively, it is proposed that the stress along the circumference of the profile cross section of the outer body is increased by the pressure generated by the swelling. Thus, a prestressing device can be formed.

[0043] It can be provided that the outer surface of the core is at least partially in direct contact with the inner side of the outer body, and / or a connecting layer, such as an adhesive layer, is arranged between the outer surface of the core and the inner side of the outer body. This can provide a further measure to prevent relative movement between the core and the outer body at the contact surface. Optionally, it can also be provided that the surface of the core is treated to improve the friction connection. For example, the surface of the core can be roughened.

[0044] The friction connection between the outer body and the core can also be improved by coating the wood surface with a substance that increases the friction coefficient or the adhesion properties to the inner side of the outer body. The substance that increases the friction coefficient can be, for example, a coating agent containing corundum. The substance that increases the adhesion properties can be, for example, a contact glue.

[0045] In particular, preferably, a corresponding coating is applied to the inner side of the outer body to increase the adhesive properties. The interaction of the two coatings may lead to a chemical reaction and thus to a higher coefficient of friction or adhesion of the two materials.

[0046] Optionally, the connection between the core and the outer body may be improved by oxidizing the outer surface of the core and / or the inner surface of the outer body.

[0047] Optionally, the connection between the core and the outer body may be improved by chemically treating the surface of the core. Optionally, the treated core is then reacted with the inner surface of the outer body.

[0048] Alternatively, the connection between the core and the outer body may be improved by mechanical treatment of the outer body, for example by embossing and / or rolling.

[0049] Additional planar or point sensors, in particular pressure sensors, may be connected to the contact surface between the core and the outer body, for example to check the swelling state of the core.

[0050] The outer surface of the core may also be a carrier for conductive traces for current and signal routing.

[0051] Optionally, it is proposed that the core is designed as a hollow body, which optionally has a cavity extending substantially in the direction of its longitudinal extension, in particular a cavity open on at least one side. This can make it easier to introduce a fluid to swell the core and remove it again if necessary. Optionally, it can be proposed that the core is designed as a hollow profile.

[0052] The cavity can also optionally be used to insert pipes or conductive tracks for conveying gas or liquid into the device after the swelling process.

[0053] Optionally, the inner profile body may be arranged in a cavity, such as a duct. Optionally, the core exerts a pressure on the inner profile body resulting from its swelling.

[0054] Optionally, it is provided that the fluid is water and / or that in the operating state the fluid content of the core is at least 1 wt %, in particular 5 wt %, preferably 10 wt % higher than in the joined state. Thus, sufficient swelling can optionally be achieved.

[0055] In particular, it is provided that the outer body and the core frictionally engage with each other.

[0056] Optionally, it is proposed that the outer body has on its inner side at least one form-fitting locking element, in particular a form-fitting locking extension, for a form-fitting connection between the outer body and the core.

[0057] Optionally, it is provided that the core has at least one positive-fitting recess for engagement with the positive-fitting extension.

[0058] Optionally, it is proposed that the core is thermally modified, in particular by a treatment at a temperature of at least 120° C., preferably at a temperature of in particular about 200° C. In particular, the core is thermally modified by a temperature treatment between 120° C. and 250° C. Optionally, the core is thermally modified by a temperature treatment for at least 5 minutes, preferably at least 10 minutes. Optionally, the core is thermally modified by a temperature treatment for a maximum of 30 minutes. Thus, the mechanical properties of the core can be improved.

[0059] Furthermore, the present invention optionally comprises a method for manufacturing a device, in particular a composite beam. In particular, the device comprises an outer body formed of a hollow profile having an inner space and a core arranged in the inner space, wherein the core comprises or is formed of a fiber composite material, in particular wood, which is swellable when in contact with a fluid. Optionally, the method comprises the following steps:

[0060] (a) providing a core, wherein the core has a first fluid content,

[0061] (b) inserting the core into the interior space of the outer body,

[0062] (c) increasing the fluid content of the core so that the core is swollen by the fluid and applies a compressive force generated by the swelling to the outer body, wherein the core has a second fluid content.

[0063] Thus, the device according to the invention can be formed in an advantageous manner, wherein in particular there is a friction connection between the outer body and the core.

[0064] Optionally, it is provided that the fluid is water and / or the second fluid content is at least 1 wt%, in particular at least 5 wt%, preferably at least 10 wt% higher than the first fluid content. In particular, this can achieve sufficient swelling for the connection between the outer body and the core.

[0065] Optionally, in step (b), the core and the inner space have a clearance fit. In particular, this can be used to determine the normal force acting on the connection in the operating state.

[0066] Optionally, it is proposed that the fluid is water and that the first fluid content is at most 10 wt%, in particular at most 5 wt%, and / or that the first fluid content is below the equilibrium moisture content of the fiber composite material of the core at a temperature of 20° C. and a relative humidity of 50%. In particular, at a temperature of 20° C. and a relative humidity of 50%, the first fluid content may be at least 5 wt%, optionally at least 10 wt% below the equilibrium moisture content of the fiber composite material of the core.

[0067] Optionally, moisture is mostly or completely removed from the core by drying or by other methods. The wood loses volume due to dehydration. Thus, the core can be inserted into the interior space of the outer body in a joined state.

[0068] Optionally, it is proposed that the method further comprises the following steps:

[0069] (d) Forming a positive locking element by deforming the outer body. Thus, an additional restraining force can be obtained between the outer body and the core, thereby fixing the bodies to each other.

[0070] Optionally, it is proposed that the method further comprises the following steps:

[0071] (d) Rolling of the device. Thus, the core can be compacted, which further improves the mechanical properties.

[0072] Optionally, the core is covered with liquid and / or gaseous water between step (a) and step (b).

[0073] Optionally, prior to step (b), the core is chemically treated, for example with ammonia, to enable it to swell better.

[0074] The invention optionally also relates to a method for disassembling a device, in particular a composite beam. In particular, the device optionally comprises an outer body formed of a hollow profile having an inner space and a core arranged in the inner space, wherein the core comprises or is formed of a fiber composite material, in particular wood, which is swellable when in contact with a fluid. Optionally, the method comprises the following steps:

[0075] (a) providing the device, the core in the inner space is swollen by a fluid and exerts a compressive force generated by the swelling on the outer body, wherein the core has a second fluid content,

[0076] (b) reducing the fluid content of the core so that the core has a first fluid content,

[0077] (c) Removing the core from the outer body.

[0078] Thus, the device may optionally be separated and its various parts recovered individually.

[0079] Optionally, it is proposed that reducing the fluid content of the core in step (b) is achieved by heating the core. Thus, the pressure acting between the outer body and the core can be reduced, making in particular that there is no longer a frictional engagement and / or a form-fitting connection between the outer body and the core.

[0080] Optionally, it is provided that the fluid is water and / or that the second fluid content is at least 1 wt%, in particular at least 5 wt%, preferably at least 10 wt% higher than the first fluid content. In particular, this may result in the shrinkage required to release the connection.

[0081] Optionally, in step (c), the core and the inner space have a clearance fit.

[0082] In one arrangement, provision can also be made for the fibers of the core to extend substantially in a main extension direction of the core.

[0083] The cross section of the core and / or the outer body can be quadrilateral, in particular rectangular or square, circular, polygonal, hyperbolic, convex, concave, trapezoidal, elliptical, hexagonal, manifold, rhombic, triangular, T-shaped, U-shaped or even polygonal. Thus, suitable cross sections can be provided for different applications.

[0084] Alternatively, it is provided that, in the operating state, the structural mechanical compression energy of the core corresponds to the structural mechanical swelling energy of the outer body.

[0085] Optionally, it is proposed that a radial cross-section of the device has the same area moment of inertia about the two principal stress axes.

[0086] It can be provided that the core is formed in a one-piece or multi-piece design. For example, it can be provided that the core has several individual parts.

[0087] Optionally, it is proposed that the cross-section of the device has different moments of area inertia about the two principal stress axes and / or that the shape of the core is adapted to the shape of the interior space.

[0088] Optionally, the device has a size in the connected state that allows the core to be inserted into and removed from the inner space of the outer body, and the device has a swollen size in the operating state so that there is a secure connection between the core and the outer body. Optionally, the size is an oversize or undersize of a clearance fit.

[0089] It is optionally provided that the fluid is reversibly added to the core, wherein the core is removed from the outer body after the fluid content, in particular the wood moisture content, in the core has decreased.

[0090] In further embodiments, the following features may be provided additionally or alternatively in the apparatus and / or method of the present invention:

[0091] Optionally, a recyclable joining technique for a wood-metal composite material is provided. In particular, the core and the outer body are joined by a hydrothermal method and optionally separated again. The wood material, in particular hygroscopic, optionally has the property of changing volume when it absorbs moisture through contact with water or changes in humidity and / or temperature.

[0092] Adding water to the core wood structure may cause an increase in volume. This property can be called swelling.

[0093] In the case of water, an increase in volume occurs optionally in the wood moisture range of 0 to about 30 wt%, the fiber saturation range. Above this value, generally no volume change is observed.

[0094] Optionally, the core is or will be pre-compacted to facilitate subsequent compaction during swelling. Due to the compressive pressure generated when the wood swells (theoretical compressive pressure of lignified cell walls ~ about 500 N / mm 2 range) and the low transverse compressive strength of wood (about 1 to 15 N / mm 2 The wood of the core may optionally be compressed by the outer body, within a range depending on the type of wood.

[0095] Plastic deformation of wood in radial or tangential directions can be achieved more easily at increased humidity or temperature or after chemical pretreatment.

[0096] Optionally, the multi-layer core can also be constructed from optionally pre-compressed wood layers and layers of other materials, such as ceramics, plastics, metal foams or the like.

[0097] The device can also be deformed by applying external compressive pressure. This can optionally change the moment of inertia or selectively compact the core. The core can be bonded to the outer body by a swelling process or by an additional forming process of form-fitting locking and frictional engagement. This bonding connection can also be improved by special surface designs such as roughening or undercutting.

[0098] Furthermore, the device can also be plastically deformed by means of a bending device, such as a profile bender.

[0099] Pre-compacting of the core optionally increases rigidity and strength. In particular, the wooden body or core can be compacted in its peripheral area by the joining process, which increases strength and rigidity and improves the overall mechanical properties of the device. The main advantage of the device is that, in particular, when the device is overloaded, ductile fracture with increased energy absorption occurs.

[0100] In particular, the absorbable fracture energy can be further increased by compacting the core.After the volume increase, the device is sealed at the front on both sides, whereby the swollen state of the wood is permanently maintained by the diffusion tightness of the metal and the sealing material, such as PU rigid foam or other plastics.

[0101] The sealing at the end face of the outer body can be achieved by caps of different shapes and materials. The cap can be connected to the outer body by friction, form fit and / or material bonding.

[0102] In the case of friction and material bonding, the cap can simply be released again by screwing it tighter, pulling it off or heating it.

[0103] The device can also be disassembled or removed by removing the fluid-tight closure of the core and exposing the device to atmospheric or physical conditions, under which the core again loses moisture or other fluid and shrinks. The shrinking process optionally continues until the two joined parts can be separated again.

[0104] Optionally, the main advantage of this method is that the metal parts or outer body and the wood parts or core can be used again or recycled. In addition, by improving the mechanical properties of the composite material, the size of the parts can be optionally reduced and material can be saved.

[0105] If the outer body is steel, the recycling process in a blast furnace requires the addition of carbon dioxide and heat. During the recycling process, the energy and chemical composition stored in the core can save energy and coal.

[0106] The outer body may also be formed from or comprise another non-swellable and diffusion-tight material, such as ceramic, plastic or fiber-reinforced plastic.

[0107] The apparatus of the present invention optionally allows one or more of the following advantages over conventional geometrically similar steel beams:

[0108] - At approximately the same load and mass, the improvement in deflection is at least 2%, optionally 8%.

[0109] - Reduce raw material costs by up to 40% while maintaining the same quality

[0110] - Up to 20% less CO2 emissions during production while maintaining the same quality

[0111] If a high core is used, raw material costs can optionally be reduced by up to 50% and carbon dioxide emissions by up to 40%. BRIEF DESCRIPTION OF THE DRAWINGS

[0112] Further features of the invention are apparent from the description of the exemplary embodiments, the drawings, and the claims.

[0113] The invention is explained in detail below by means of non-exclusive, merely exemplary embodiments.

[0114] Figure 1a A schematic diagram shows an embodiment of an embodiment of a device according to the invention in an operating state according to a first exemplary embodiment;

[0115] Figure 1b shows the device according to the first exemplary embodiment in an engaged state;

[0116] Figure 2aA schematic diagram shows an embodiment of an embodiment of a device according to the invention in an operating state according to a second exemplary embodiment;

[0117] Figure 2b shows the device according to the second exemplary embodiment in an engaged state;

[0118] Figure 3a The operating state of a third exemplary embodiment of an embodiment of the device according to the invention is shown schematically;

[0119] Figure 3b The device according to the third exemplary embodiment is shown in an engaged state

[0120] Figure 4a A schematic diagram shows an embodiment of a fourth embodiment of the device according to the invention in a working state;

[0121] Figure 4b The device according to the fourth exemplary embodiment is shown in an engaged state. DETAILED DESCRIPTION

[0122] Unless otherwise stated, the drawings show the following features: composite beam 1 , outer body 2 , core 3 , inner space 4 , inner surface 5 , outer surface 6 , form-fitting locking extension 7 , cavity 8 , inner profile body 9 , outer surface 10 .

[0123] Figure 1a An embodiment of a device according to the invention is shown in an operating state according to a first exemplary embodiment. Figure 1a The device is shown in a schematic cross-sectional view, wherein the cross-sectional plane is arranged essentially perpendicular to the longitudinal extension of the device.

[0124] The device is designed as a composite beam 1 with a circular cross section and comprises an outer body 2 of a hollow profile shape with an inner space 4. A core 3 is arranged in the inner space 4. The core 3 is swellable when in contact with a fluid and is made of wood in this embodiment. Figure 1a The composite beam is shown in its operating state, i.e. with the core 3 swollen. In this state, the core 3 in the inner space 4 is swollen by water and exerts pressure on the outer body 2 due to the swelling. The outer surface 6 of the core 3 is in direct contact with the inner surface 5 of the outer body 2.

[0125] In other embodiments not shown, a connecting layer, for example an adhesive layer, is arranged between the outer surface 6 of the core 3 and the inner side 5 of the outer body 2 .

[0126] In this embodiment, the outer body 2 is designed as a tubular steel profile. The core 3 is an elongated, substantially cylindrical rod made of wood.

[0127] The core 3 is fluid-tightly enclosed in the inner space 4 of the outer body 2, wherein plastic closures are provided at the two open ends (not shown) of the outer body 2. Thus, the fluid content of the core 3 can be kept substantially constant even under changing external conditions.

[0128] Figure 1b An embodiment of the device according to the invention is shown in an engaged state. In this state, the outer surface 6 of the core 3 is spaced from the inner side 5 of the outer body 2, so that in particular there is a clearance fit between the core 3 and the inner surface 5 of the outer body 2. For further features, see Figure 1a Description.

[0129] In particular, during the production of the device or composite beam 1, the device can assume a joint state. In the joint state, the core 3 can be inserted into the inner space 4 of the outer body 2. By increasing the water content, the composite beam 1 is brought into an operating state, so that the core 3 is pressed against the inner surface 5 of the outer body 2 with its outer surface 6.

[0130] In this exemplary embodiment, the water content of the core 3 is approximately 25 wt % in the operating state and approximately 10 wt % in the joined state.

[0131] If the composite beam is to be disassembled, at least one of the closing pieces is removed. Excess moisture can then escape and the core 3 contracts, which in turn leads to a joint state in which the core 3 can be removed from the interior space 4 of the outer body 2. The escape of moisture can be enhanced by heating the device.

[0132] Figure 2a A schematic diagram shows an embodiment of an embodiment of a device according to the invention in an operating state according to a second exemplary embodiment; Figure 2b The device according to the second exemplary embodiment is shown in an engaged state. Figure 2a and 2b The device is shown in each case in a schematic cross-sectional view, wherein the cross-sectional plane is arranged substantially perpendicular to the longitudinal extension of the device.

[0133] The composite beam 1 according to the second exemplary embodiment corresponds largely to the beam according to the first exemplary embodiment described in detail.

[0134] In contrast to the first exemplary embodiment, the core 3 and the outer body 2 in the second exemplary embodiment have a square cross section.

[0135] Furthermore, form-fitting locking extensions 7 in the form of ribs are arranged on the inner surface 5 of the outer body 2. In the operating state, the form-fitting locking extensions 7 are pressed into the surface of the core 3, which also forms a form-fitting connection between the core and the outer body. These ribs are arranged at regular intervals along the longitudinal extension direction of the composite beam 1.

[0136] Furthermore, unlike the first embodiment, there is no fluid-tight encapsulation of the core 3 in the interior space 4 of the outer body 2. In this exemplary embodiment, the outer body 2 is open on both sides. In this exemplary embodiment, the friction connection between the core 3 and the outer body 2 is achieved by having a moisture content of the core 3 in the joined state below a moisture content corresponding to the moisture content equilibrium of the core material at a temperature of 20° C. and a relative humidity of 50%. Therefore, the core is dried so that its moisture content is in particular less than 5 wt %.

[0137] In the engaged state, there is no longer a positive connection between the positive locking element 7 and the core 3 either.

[0138] In the joined state, the core 3 can be inserted into the inner space 4 of the outer body. The composite beam 1 is then kept under ambient conditions and the moisture content of the core 3 will gradually increase until the moisture content corresponds to the moisture content equilibrium. The device is then in an operational state, achieving similar effects as the first exemplary embodiment. However, no fluid-tight closure is required, which further simplifies the design.

[0139] To dismantle the device, the composite beam 1 may be heated so that the fluid content of the core 3 is reduced.

[0140] Figure 3a The operating state of a third exemplary embodiment of an embodiment of the device according to the invention is shown schematically; Figure 3b The device according to the third exemplary embodiment is shown in an engaged state. Figure 3a and 3b The device is shown in each case in a schematic cross-sectional view, wherein the cross-sectional plane is arranged substantially perpendicular to the longitudinal extension of the device.

[0141] The third embodiment is essentially the same as the second embodiment, except that the core 3 is designed as a hollow body with a cavity 8. This facilitates the change of the water content, wherein the larger the free surface area, the faster the change of the water content. In this embodiment, the core 3 is configured as a box-shaped profile. The cavity 8 can be used for pipes, pipelines, cables, etc.

[0142] In an exemplary embodiment not shown, a positive locking extension can also be provided in this embodiment.

[0143] Furthermore, unlike the second embodiment, no positive locking extension 7 is provided.

[0144] Figure 4a A schematic diagram shows an embodiment of a fourth embodiment of the device according to the invention in an operating state; Figure 4b The device according to the fourth exemplary embodiment is shown in an engaged state. Figure 4a and 4b The device is shown in each case in a schematic cross-sectional view, wherein the cross-sectional plane is arranged substantially perpendicular to the longitudinal extension of the device.

[0145] The fourth exemplary embodiment corresponds substantially to the third exemplary embodiment, with the difference that the outer body 2 and the core 3 are designed in the shape of a hollow cylinder. An inner profile body 9 , which is a steel tube in this exemplary embodiment, is arranged in the cavity 8 of the core 3 .

[0146] In the operating state, Figure 4a As shown, the core 3 presses against the inner surface 5 of the outer body 2 and against the outer surface 10 of the inner profile body 9 due to swelling.

[0147] In this embodiment, the device can be used as a load-bearing member and at the same time as a conduit for conveying liquids or gases, for example as a water pipe.

Claims

1. A device, in particular a composite beam (1), comprising an outer body (2) formed of a hollow profile with an inner space (4) and a core (3) arranged in the inner space (4), wherein the core (3) comprises or is formed of a fiber composite material, in particular wood, which is capable of swelling when in contact with a fluid, characterized in that The core (3) in the inner space (4) is swollen by fluid in an operating state, and exerts pressure generated by the swelling on the outer body (2).

2. The device according to claim 1, characterized in that The core (3) exerts an internal pressure acting on the outer body (2) in an operating state.

3. The device according to claim 1 or 2, characterized in that: The outer body (2) has a closed cross section.

4. The device according to any one of claims 1 to 3, characterized in that The pressure exerted by the core on the outer body in the operating state is at least 3 N / mm 2 , in particular at least 5 N / mm 2 or in particular at least 10 N / mm 2 .

5. The device (1) according to any one of claims 1 to 4, characterized in that The core (3) is supported in the inner space (4) in an operating state.

6. The device (1) according to any one of claims 1 to 5, characterized in that The outer body (2) is designed as a metal profile, in particular a steel profile.

7. The device (1) according to any one of claims 1 to 6, characterized in that The core (3) can be inserted and / or removed into the inner space (4) in a joined state, wherein due to fluid absorption, the core (3) is more swollen in the operating state than in the joined state, and / or wherein the core (3) has a higher fluid content in the operating state than in the joined state.

8. The device (1) according to any one of claims 1 to 7, characterized in that The core (3) and the interior (4) have a clearance fit in the joined state, wherein there is optionally an underdimensioning of the core (3) relative to the interior (4).

9. The device (1) according to any one of claims 1 to 8, characterized in that In the operating state, the core (3) completely fills the inner space (4) of the outer body (2).

10. The device (1) according to any one of claims 1 to 9, characterized in that The core (3) is enclosed in a fluid-tight manner in the operating state.

11. The device according to any one of claims 1 to 10, characterized in that The core is enclosed in a fluid-tight manner by the outer body (2) and at least one closure arranged on the outer body (2).

12. The device according to any one of claims 1 to 11, characterized in that The fluid is selected from one or more of the following fluids: water, salt solution, alcohol, ammonia.

13. The device according to any one of claims 1 to 12, characterized in that The core (2) has a compacted area along its outer circumference.

14. The device (1) according to any one of claims 1 to 13, characterized in that The stress along the circumference of the profile cross section of the outer body (2) is increased by the pressure generated by the swelling.

15. The device (1) according to any one of claims 1 to 14, characterized in that The outer surface (6) of the core (3) is at least partially in direct contact with the inner side (5) of the outer body (2), and / or a connecting layer, such as an adhesive layer, is arranged between the outer surface (6) of the core (3) and the inner side (5) of the outer body (2).

16. The device (1) according to any one of claims 1 to 15, characterized in that The core (3) is designed as a hollow body, which optionally has a cavity (8) extending substantially in the longitudinal extension direction thereof, and which is open in particular on at least one side.

17. The device (1) according to any one of claims 1 to 16, characterized in that An inner profile body (9) is arranged in the cavity (8), wherein the core (3) exerts a pressure on the inner profile body (9) caused by its swelling.

18. The device (1) according to any one of claims 1 to 17, characterized in that The fluid is water and / or the fluid content of the core (3) in the operating state is at least 1 wt% higher than the fluid content in the engaged state.

19. The device according to any one of claims 1 to 18, characterized in that The outer body (2) and the core (3) are frictionally engaged with each other.

20. The device according to any one of claims 1 to 19, characterized in that The outer body (2) has on its inner side (5) at least one form-fitting locking element, in particular a form-fitting locking extension (7), for a form-fitting connection between the outer body (2) and the core (3).

21. The device according to claim 20, characterized in that The core (3) has at least one form-fitting locking recess for engaging with the form-fitting locking extension (7).

22. A method for manufacturing a device (1), in particular a composite beam, comprising an outer body (2) formed of a hollow profile with an inner space (4) and a core (3) arranged in the inner space (4), wherein the core (3) comprises or is formed of a fiber composite material, in particular wood, which is swellable when in contact with a fluid, wherein the method comprises the following steps: (a) providing the core (3), wherein the core (3) has a first fluid content, (b) inserting the core (3) into the inner space (4) of the outer body (2), (c) increasing the fluid content of the core (3) such that the core (3) is swollen by the fluid and exerts a compressive force on the outer body (2) caused by the swelling, wherein the core has a second fluid content.

23. The method according to claim 22, characterized in that The fluid is water, and / or the second fluid content is at least 1 wt %, in particular at least 2 wt % higher than the first fluid content.

24. The method according to claim 22 or 23, characterized in that In step (b), the core (3) and the inner space (4) have a clearance fit.

25. The method according to any one of claims 22 to 24, characterized in that The fluid is water and the first fluid content is at most 10 wt%, at most 5 wt%, and / or the first fluid content is below the equilibrium moisture content of the fibrous composite material of the core at a temperature of 20°C and a relative humidity of 50%.

26. The method according to any one of claims 22 to 25, characterized in that The method further comprises the following steps: (d) Forming a positive locking element by deforming the outer body (2).

27. A method for dismantling a device, in particular a composite beam, comprising an outer body (2) formed of a hollow profile with an inner space (4) and a core (3) arranged in the inner space (4), wherein: The core (3) comprises or is formed from a fiber composite material, in particular wood, which is swellable when in contact with a fluid, wherein the method comprises the following steps: (a) providing the device (1), wherein the core (3) in the inner space (4) is swollen by a fluid and exerts a compressive force generated by the swelling on the outer body (2), wherein the core (3) has a second fluid content, (b) reducing the fluid content of the core (3) so that the core (3) has a first fluid content, (c) Removing the core (3) from the outer body (2).

28. The method according to claim 27, characterized in that Reducing the fluid content of the core (3) in step (b) comprises heating the core (3), in particular to a temperature above 50°C, preferably above 100°C.

29. The method according to claim 27 or 28, characterized in that The fluid is water, and / or the second fluid content is at least 1 wt %, in particular at least 2 wt % higher than the first fluid content.

30. The method according to any one of claims 27 to 29, characterized in that The core (3) and the inner space (4) in step (c) have a clearance fit.