Plasma arc welding processing technology and equipment for titanium and titanium alloy thick plates

The gap between the plate is fixed by tungsten argon arc welding and combined with transfer arc welding technology, the problem of air pores in titanium welding is solved, and 14mm titanium is achieved at one-time penetration and efficient welding, which improves product qualification rate and production efficiency.

CN119057192APending Publication Date: 2024-12-03LINHAI TAITONG MEDICAL EQUIP CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411450843.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-10-17
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

When welding titanium materials, as the plate thickness increases, the number of welding layers increases, the chance of generating pores increases, which affects the product's pass rate. It is also difficult to follow-up repair work, especially for titanium materials with a bevel of 14mm and above, it is necessary to open a bevel to be weld at one time. It increases process complexity and cost.

Method used

Tungsten electrode argon arc welding is used to fix the plate gap, and arc-induced plate and arc extinguishing plate are used to cooperate with transfer arc welding to ensure the permeability of the weld, and cover the surface layer after plasma arc welding, and control welding parameters such as nozzle aperture and tungsten The electrode diameter, yaw speed and wire feeding speed combine protection air release and semiconductor radiator cooling to improve welding stability and efficiency.

Benefits of technology

14mm titanium plasma arc welding is achieved at one time, reducing the generation of pores, improving welding quality and product qualification rate, reducing the difficulty of repair and production costs, and improving welding efficiency and stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119057192A_ABST
    Figure CN119057192A_ABST
Patent Text Reader

Abstract

The invention provides a titanium and titanium alloy thick plate plasma arc welding machining process. The titanium and titanium alloy thick plate plasma arc welding machining process comprises the following steps that S1, an oxide layer on the surface of a plate is cleaned; s2, the gap between every two adjacent plates is 1-1.5 mm, and the two adjacent plates are fixed through argon tungsten-arc welding spot welding; s3, a run-on plate and a run-off plate are welded to the plate, and the run-on plate and the run-off plate are located at the two ends of the weld joint correspondingly; s4, on the premise that the shielding gas is released, transfer type electric arcs are adopted for welding, arc striking is conducted on the arc striking plate, and arc quenching is conducted on the arc quenching plate; and S5, after plasma arc welding is completed, after the plate is cooled to 120 DEG C or below, a cover surface layer is welded through argon tungsten-arc welding, and the purpose of welding the 14 mm titanium plate is achieved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of welding, and in particular to a plasma arc welding process and equipment for titanium and titanium alloy thick plates. Background Art

[0002] Titanium and titanium alloys have many excellent properties, active chemical properties, strong affinity with oxygen, and a stable and tough oxide film will quickly form on a clean surface at room temperature. Due to the protective effect of the oxide film, titanium and titanium alloys have excellent corrosion resistance in seawater and most acid, alkali, and salt media.

[0003] At present, a Chinese patent with authorization announcement number CN203610848U discloses a titanium equipment welding device, including a welding head, a workpiece clamping device corresponding to the welding head, the welding head includes a welding nozzle, an inert gas output nozzle is arranged at the position adjacent to the welding nozzle, and the workpiece clamping device also includes a protective drag hood matched therewith.

[0004] This titanium equipment welding equipment effectively avoids the problems of large welding deformation of titanium equipment workpieces, difficulty in shape correction, and easy cracking of titanium during cold processing.

[0005] However, according to the experience of the same industry in China, for titanium welding, for titanium materials below 8mm, plasma arc welding is used, which does not require beveling and can be welded through in one go. For titanium materials exceeding 8mm, especially 14mm, beveling is required to weld through in one go. Moreover, as the thickness of the plate increases, the number of welding layers gradually increases, and the chance of generating pores also increases, which will seriously affect the first-time pass rate of product flaw detection, and the subsequent rework work is very difficult. Summary of the invention

[0006] In view of this, the object of the present invention is to provide a plasma arc welding process and equipment for titanium and titanium alloy thick plates.

[0007] In order to solve the above technical problems, the technical solution of the present invention is: a plasma arc welding process for titanium and titanium alloy thick plates, comprising the following steps: S1: Clean the oxide layer on the surface of the plate; S2: The gap between adjacent plates is 1-1.5 mm, and the two adjacent plates are fixed by spot welding with tungsten inert gas welding; S3: welding an arc-starting plate and an arc-extinguishing plate on the plate, wherein the arc-starting plate and the arc-extinguishing plate are respectively located at two ends of the weld; S4: Under the premise of releasing the shielding gas, the transferred arc is used for welding, and the arc is started on the arc-starting plate and extinguished on the arc-extinguishing plate; S5: After the plasma arc welding is completed, wait for the plate to cool to below 120°C and use tungsten inert gas arc welding to weld the cover layer.

[0008] To implement the above technical solution, the oxide scale on the surface of the plate is thoroughly cleaned to reveal the metallic luster; a gap is reserved for pairing, and the gap is controlled at 1-1.5mm, and then it is fixed by manual tungsten inert gas arc welding. No welding wire is added during spot welding. After spot welding, arc starting plates and arc extinguishing plates of the same material and thickness are added at both ends of the steel plate weld; the front weld releases the shielding gas at the same time; the shielding gas is also released on the back of the weld; plasma arc welding: tungsten electrode diameter φ4.0, nozzle aperture φ4.0, tungsten electrode retraction 3.0mm, the distance from the nozzle to the upper surface of the workpiece to be welded is 10mm; motorized tungsten inert gas arc welding: tungsten electrode diameter φ4.0, nozzle diameter φ19; during the second layer of tungsten inert gas arc welding, the sway speed is 1550mm / min, the sway width is 10.4mm, and the wire feeding speed is 3700mm / min; it is ensured that the 14mm plate plasma arc welding is fully penetrated once, achieving the effect of single-sided welding and free forming on the back.

[0009] As a preferred solution of the present invention, the step S3.1 is also included: cleaning the oil stains within a range of 25 mm on both sides of the weld with anhydrous ethanol.

[0010] Implement the above technical solution to improve welding stability.

[0011] The present invention also provides a processing equipment for plasma arc welding of titanium and titanium alloy thick plates, including a plasma arc welding machine and a support table. The support table is used to place plates. There is a gap between adjacent plates. The length direction of the gap is set along the length direction of the support table. The support table is provided with an arc-starting plate and an arc-extinguishing plate. The arc-starting plate and the arc-extinguishing plate are both fixed on the plates and are respectively located at both ends of the gap. The main machine of the plasma arc welding machine is connected to a support frame, and the support frame is connected to an upper air outlet pipe, and the air outlet of the upper air outlet pipe faces the support table.

[0012] To implement the above technical solution, two plates are placed on a support table and located on both sides of the gap respectively, an arc striking plate and an arc extinguishing plate are fixed on the plates and located at both ends of the gap respectively, and then the shielding gas is led into the gap from the upper gas outlet pipe, the main machine is turned on, the plasma arc welding gun is used to weld the plates, and the plasma arc welding machine is moved along the length direction of the gap to complete the welding process.

[0013] As a preferred solution of the present invention, a protective gas release groove is provided on the support platform, the width of the protective gas release groove is greater than the width of the gap, a lower air outlet pipe penetrating the protective gas release groove is fixedly connected to the support platform, a connecting hole is provided on the outer wall of the lower air outlet pipe, and the connecting hole is connected to the protective gas release groove.

[0014] To implement the above technical solution, while the upper air outlet pipe discharges the shielding gas, the lower air outlet pipe also discharges the shielding gas from the connecting hole, so that both sides of the plate are surrounded by the shielding gas at the same time, thereby improving the welding quality and reducing the possibility of the plate being oxidized.

[0015] As a preferred solution of the present invention, the support frame is square in shape, and the first protective curtain and the second protective curtain are connected to the side walls of the support frame. The first protective curtain and the second protective curtain are arranged adjacent to each other, and a power motor is arranged on the support frame. The power motor is started and the first protective curtain and the second protective curtain are lifted synchronously through the conduction structure.

[0016] To implement the above technical solution, the provision of the first protective curtain and the second protective curtain enhances the protection of the workers and, at the same time, can prevent the protective gas from dispersing, thereby improving the quality of welding. After the first plasma arc welding is completed, it is necessary to wait for the plate to cool down to below 120°C, turn on the power motor, and use the conduction structure to simultaneously lift the first protective curtain and the second protective curtain to increase the cooling speed. When the welding temperature exceeds 400°C, the protective gas protects the plate.

[0017] As a preferred embodiment of the present invention, the conductive structure includes a first pull rope, a first connecting ring, a first connecting shaft, a first support, a second pull rope, a second connecting ring, a second connecting shaft, and a second support. The first support is connected to the support frame, and the first connecting shaft is rotatably connected to the first support. One end of the first pull rope is connected to the first connecting shaft, and the other end of the first pull rope is connected to the first protective curtain. The first connecting ring is fixed on the first connecting shaft and coaxially arranged. The second support is connected to the support frame, and the second connecting shaft is rotatably connected to the second support and coaxially fixedly connected to the second connecting ring. One end of the second pull rope is connected to the second connecting shaft, and the other end of the second pull rope is connected to the second protective curtain. The first connecting ring is meshed with the second connecting ring.

[0018] To implement the above technical solution, the power motor is started, the first connecting shaft rotates, the first connecting ring rotates synchronously with the first connecting shaft, the second connecting ring rotates synchronously with the first connecting ring, and the second connecting shaft rotates with the second connecting ring, so that the first pull rope and the second pull rope are respectively wound on the first connecting shaft and the second connecting shaft, so that the first protective curtain and the second protective curtain are lifted synchronously.

[0019] As a preferred solution of the present invention, the first support is fixedly connected to a first gear, the second support is rotatably connected to a second gear for meshing with the first gear, the second support is embedded with a positioning rod, and the positioning rod is embedded in the second gear.

[0020] To implement the above technical solution, the second gear is rotated along the axis of the first gear. The second gear rotates to adjust the position of the second support. Then the positioning rod is embedded in the second support and the second gear to position the second support, so that the second connecting shaft can adapt to support frames of different shapes, thereby improving practicality.

[0021] As a preferred solution of the present invention, a semiconductor heat sink is connected to the support frame, the first connecting shaft is connected to a rotating rod through a linkage structure, a fixing seat is fixedly connected to the support frame, the fixing seat is threadedly connected to the rotating rod, and the rotating rod rotates and interferes with the switch of the semiconductor heat sink.

[0022] To implement the above technical solution, the first protective curtain and the second protective curtain are lifted, and at the same time, the rotating rod is rotated through the linkage structure so that the rotating rod contacts the switch of the semiconductor radiator, and the semiconductor radiator is started, so that the plate can be cooled down quickly, reducing the time waiting for the plate to cool down, so as to improve production efficiency; similarly, when welding is to be performed, the first connecting shaft rotates, the first protective curtain and the second protective curtain are lowered, and at the same time the rotating rod is separated from the switch of the semiconductor radiator, and the semiconductor radiator stops working.

[0023] As a preferred solution of the present invention, the linkage structure includes a first connecting gear, a second connecting gear, and a rack. The first connecting gear is fixed on the first connecting shaft and is coaxially arranged, the second connecting gear is fixed on the rotating rod and is coaxially arranged, the rack is meshed with the first connecting gear and the second connecting gear at the same time, and the rack is slidably connected to the support frame.

[0024] To implement the above technical solution, the first connecting shaft rotates, the first connecting shaft drives the first connecting gear to rotate, the first connecting gear pushes the rack to move, thereby rotating the second connecting gear, and the second connecting gear drives the rotating rod to rotate. The rotating rod rotates, and through the conduction of the thread, the rotating rod contacts the switch of the semiconductor radiator, and the semiconductor radiator is started to quickly cool the plate.

[0025] As a preferred solution of the present invention, a fan is rotatably connected to the support frame, a body of the fan corresponds to the semiconductor heat sink, and a switch of the fan is used to interfere with the rotating rod.

[0026] To implement the above technical solution, when the rotating rod contacts the switch of the semiconductor heat sink, the rotating rod contacts the switch of the fan, the fan is started, and the cold air generated by the start-up of the semiconductor heat sink can be quickly blown to the weld by the fan to further improve the cooling efficiency; when welding is required, the rotating rod is separated from the switch of the semiconductor heat sink and the switch of the fan to stop the semiconductor heat sink and the fan from working. BRIEF DESCRIPTION OF THE DRAWINGS

[0027] Figure 1 It is a schematic diagram of the position structure of the support platform and the plasma arc welding machine in the embodiment; Figure 2 To reflect the structural diagram of the lower air outlet pipe; Figure 3 A schematic diagram showing the positions of the plate and the support platform; Figure 4 A schematic diagram showing the structure of the first protection curtain and the second protection curtain; Figure 5 A schematic diagram showing the structure of the conduction structure; Figure 6 Schematic diagram of the structure of the rotating rod.

[0028] 1. support platform; 2. shielding gas release groove; 3. plasma arc welding machine; 4. support frame; 5. infrared thermometer; 6. plate; 7. arc-starting plate; 8. arc-extinguishing plate; 9. gap; 10. upper air outlet pipe; 11. lower air outlet pipe; 12. connecting hole; 13. first protective curtain; 14. second protective curtain; 15. power motor; 16. conduction structure; 17. first pull rope; 18. first connecting ring; 19. first connecting shaft; 20. first support; 21. second pull rope; 22. second connecting ring; 23. second connecting shaft; 24. second support; 25. first gear; 26. second gear; 27. positioning rod; 28. second support; 29. ​​first gear; 30. second gear; 31. positioning rod; 32. support plate; 33. arc-starting plate; 34. arc-extinguishing plate; 35. gap; 36. upper air outlet pipe; 37. lower air outlet pipe; 38. connecting hole; 39. first protective curtain; 40. second protective curtain; 41. upper air outlet pipe; 42. lower air outlet pipe; 42. connecting hole; 51. first protective curtain; 52. second protective curtain; 53. power motor; 6. conduction structure; 61. first pull rope; 62. first connecting ring; 63. first connecting shaft; 64. first support; 65. second pull rope; 66. second connecting ring; 67. second connecting shaft; 68. second support; 691. first gear; 692. second gear; 693. positioning rod; 694. support plate; 70. semiconductor radiator; 7. linkage structure; 71. first connecting gear; 72. second connecting gear; 73. rack; 74. rotating rod; 75. fixing seat; 8. fan. DETAILED DESCRIPTION

[0029] The specific implementation modes of the present invention are further described below in conjunction with the accompanying drawings to make the technical solutions of the present invention easier to understand and grasp.

[0030] Embodiment 1: A plasma arc welding process for titanium and titanium alloy thick plates, comprising the following steps: S1: Before welding, use a carbide rotary file to thoroughly clean the oxide scale on the surface of the plate 32 at the welding position and within 25mm on both sides to reveal the metallic luster; S2: two plates 32 are placed on the support platform 1 and arranged opposite to each other, with a reserved gap 35 for pairing, the gap 35 is controlled to be 1-1.5 mm, and fixed by manual tungsten inert gas arc welding, without adding welding wire during spot welding; S3: welding an arc-starting plate 33 and an arc-extinguishing plate 34 on the plate 32 , wherein the arc-starting plate 33 and the arc-extinguishing plate 34 are respectively located at two ends of the weld, and the material and thickness of the arc-starting plate 33 and the arc-extinguishing plate 34 are the same as those of the plate 32 .

[0031] S3.1: Use anhydrous ethanol to clean and remove oil stains within 25mm on both sides of the weld; S4: Add argon protection to the upper and lower sides of the plate 32, and supply argon gas 8 seconds in advance to the front and back of the weld. For the front weld, transfer arc welding is used. The arc is started on the arc-starting plate 33 and extinguished on the arc-extinguishing plate 34. After the welding is completed, the gas is stopped after a delay of 15 seconds. S5: After the plasma arc welding is completed, wait for the workpiece to cool to below 120°C, use an infrared thermometer 31 to detect the temperature of the welding joint to ensure that the interlayer temperature does not exceed 120°C. Finally, use motorized tungsten inert gas welding and φ1.0 welding wire to weld the cover layer.

[0032] Among them, plasma arc welding: tungsten electrode diameter φ4.0, nozzle aperture φ4.0, tungsten electrode retraction 3.0mm, the distance from the nozzle to the upper surface of the workpiece to be welded is 10mm; motorized tungsten inert gas arc welding: tungsten electrode diameter φ4.0, nozzle diameter φ19. For the second layer of tungsten inert gas arc welding, the sway speed is 1550mm / min, the sway width is 10.4mm, and the wire feeding speed is 3700mm / min. A weld tail protection hood is fixed on the welding gun, and the weld tail protection hood is located on the front of the weld.

[0033] The welding process is performed using an iAdvanced Plasma 5000 plasma arc welder 2, using a transferred arc.

[0034] The plate 32 is a titanium material with a thickness of 14 mm.

[0035] Embodiment 2: A processing equipment for plasma arc welding of titanium and titanium alloy thick plates, comprising a plasma arc welding machine 2 and a support table 1. The support table 1 is used to place a plate 32, and the plate 32 is a titanium material with a thickness of 14 mm. There is a gap 35 between the two plates 32, and the width of the gap 35 is 1-1.5 mm. The length direction of the gap 35 is set along the length direction of the support table 1, and an arc-starting plate 33 and an arc-extinguishing plate 34 are set on the support table 1, and the arc-starting plate 33 and the arc-extinguishing plate 34 are both fixed on the plate 32 and are respectively located at the two ends of the gap 35.

[0036] The host of the plasma arc welding machine 2 is connected to a support frame 3, and an upper gas outlet pipe 41 is connected to the support frame 3, and the gas outlet of the upper gas outlet pipe 41 faces the support platform 1. A shielding gas release groove 11 is provided on the support platform 1, and the width of the shielding gas release groove 11 is 100 mm. The width of the shielding gas release groove 11 is greater than the width of the gap 35, and the length direction of the shielding gas release groove 11 is parallel to the length direction of the gap 35. A lower gas outlet pipe 42 is fixedly connected to the support platform 1 and penetrates the shielding gas release groove 11. A connecting hole 421 is provided on the outer wall of the lower gas outlet pipe 42, and a plurality of connecting holes 421 are arranged along the length direction of the lower gas outlet pipe 42. The connecting hole 421 is connected to the shielding gas release groove 11.

[0037] Argon is injected into the upper gas outlet pipe 41 and the lower gas outlet pipe 42 so that the argon can simultaneously wrap the weld area and the heat affected zone from the upper side and the lower side of the plate 32, the upper side of the plate 32 being the front side and the lower side of the plate 32 being the back side.

[0038] The structure of the support frame 3 is rectangular, and the first protection curtain 51 and the second protection curtain 52 are fixedly connected to the side wall of the support frame 3. The first protection curtain 51 and the second protection curtain 52 are arranged adjacent to each other, and two first protection curtains 51 and the second protection curtain 52 are arranged opposite to each other. When the first protection curtain 51 and the second protection curtain 52 are hung down, the support platform 1 is located in the cavity surrounded by the first protection curtain 51 and the second protection curtain 52, which enhances the protection of workers during the welding process. A power motor 53 is fixed on the support frame 3. The power motor 53 is started and the first protection curtain 51 and the second protection curtain 52 are synchronously lifted through the conductive structure 6, so as to facilitate the heat dissipation of the plate 32.

[0039] The conductive structure 6 includes a first pull rope 61, a first connecting ring 62, a first connecting shaft 63, a first support 64, a second pull rope 65, a second connecting ring 66, a second connecting shaft 67, and a second support 68. The first support 64 is fixedly connected to the support frame 3. The first connecting shaft 63 is rotatably connected to the first support 64 through a bearing, one end of the first pull rope 61 is connected to the first connecting shaft 63, and the other end of the first pull rope 61 is fixedly connected to the lower edge of the first protective curtain 51. The first connecting ring 62 is fixed to the first connecting shaft 63 and is coaxially arranged.

[0040] The second connecting shaft 67 is rotatably connected to the second support 68 through a bearing and is coaxially fixedly connected to the second connecting ring 66. One end of the second pull rope 65 is connected to the second connecting shaft 67, and the other end of the second pull rope 65 is connected to the lower edge of the second protective curtain 52. The first connecting ring 62 is meshed with the second connecting ring 66. The first protective curtain 51 and the second protective curtain 52 are used to block the light generated during the welding process.

[0041] The power motor 53 is a servo motor. When the power motor 53 is started, the first connecting shaft 63 rotates, and the first pull rope 61 is wound around the first connecting shaft 63 so that the first protection curtain 51 is lifted. At the same time, the first connecting ring 62 is engaged with the second connecting ring 66, so that the second connecting shaft 67 rotates, and the second pull rope 65 is wound around the second connecting shaft 67 so that the second protection curtain 52 is lifted, so that the first protection curtain 51 and the second protection curtain 52 are lifted synchronously. The first pull rope 61 and the second pull rope 65 are made of fluorocarbon fishing line and pass through the support frame 3.

[0042] In order to adapt to the support frame 3 of different shapes, a first gear 691 is fixedly connected to the first support 64 through a first positioning shaft, and a second gear 692 for meshing with the first gear 691 is rotatably connected to the second support 68 through a second positioning shaft. One end of the support plate 694 is placed between the first support 64 and the first gear 691, and the other end of the support plate 694 is placed between the second support 68 and the second gear 692. The first positioning shaft and the second positioning shaft are both rotatably connected to the support plate 694. The support plate 694 plays the role of supporting the second support 68. A positioning rod 693 is embedded in the second support 68, and the positioning rod 693 is embedded in the second gear 692 to realize the positioning of the second support 68.

[0043] A semiconductor heat sink 70 is fixedly connected to the support frame 3, and the cold surface of the semiconductor heat sink 70 is located on the inner side of the support frame 3, that is, facing the plate 32, and the hot surface of the semiconductor heat sink 70 is located on the outer side of the support frame 3. The first connecting shaft 63 is connected to a rotating rod 74 through a linkage structure 7. A fixing seat 75 is fixedly connected to the support frame 3, and the fixing seat 75 is threadedly connected to the rotating rod 74. The rotating rod 74 rotates and conflicts with the switch of the semiconductor heat sink 70. When the first connecting shaft 63 rotates in the forward direction, the first protective curtain 51 is lifted, and at the same time, the rotating rod 74 is rotated by the linkage structure 7, and the rotating rod 74 is moved along its own length direction through the conduction effect of the thread to conflict with the switch of the semiconductor heat sink 70, and the semiconductor heat sink 70 is started, producing a cooling effect, so that the plate 32 is quickly cooled, the waiting time is reduced, and the production efficiency is improved.

[0044] The linkage structure 7 includes a first connecting gear 71, a second connecting gear 72, and a rack 73. The first connecting gear 71 is fixed on the first connecting shaft 63 and is coaxially arranged, and the second connecting gear 72 is fixed on the rotating rod 74 and is coaxially arranged. The rack 73 is meshed with the first connecting gear 71 and the second connecting gear 72 at the same time. The rack 73 is slidably connected to the support frame 3. The first connecting gear 71 and the second connecting gear 72 are both spur gears. The width of the second connecting gear 72 is much larger than the width of the rack 73.

[0045] A fan 8 is rotatably connected to the support frame 3, and the body of the fan 8 corresponds to the semiconductor heat sink 70, and the switch of the fan 8 is used to conflict with the rotating rod 74. When the rotating rod 74 moves along its length direction to conflict with the switch of the semiconductor heat sink 70, the rotating rod 74 and the switch of the fan 8 are used to conflict with the rotating rod 74. At this time, the fan 8 is started and the semiconductor heat sink 70 is started, so that the cold wind blows to the plate 32, further improving the cooling effect.

[0046] An infrared thermometer 31 is fixedly connected to the support frame 3 .

[0047] Of course, the above are only typical examples of the present invention. In addition, the present invention may also have many other specific implementations. All technical solutions formed by equivalent replacement or equivalent transformation fall within the scope of protection required by the present invention.

Claims

1. A plasma arc welding process for titanium and titanium alloy thick plates, characterized by: The steps include: S1: cleaning the oxide layer on the surface of the plate (32); S2: The gap (35) between adjacent plates (32) is 1-1.5 mm, and two adjacent plates (32) are fixed by spot welding using tungsten inert gas welding; S3: welding an arc-starting plate (33) and an arc-extinguishing plate (34) on the plate (32), wherein the arc-starting plate (33) and the arc-extinguishing plate (34) are respectively located at two ends of the weld; S4: welding is performed using a transferred arc under the premise of releasing the shielding gas, with the arc being started on the arc starting plate (33) and the arc being extinguished on the arc extinguishing plate (34); S5: After the plasma arc welding is completed, the plate (32) is cooled to below 120°C, and the cover layer is welded by tungsten inert gas arc welding.

2. The plasma arc welding process for titanium and titanium alloy thick plates according to claim 1 is characterized by: The step S3.1 is also included: using anhydrous ethanol to clean the oil stains within a range of 25 mm on both sides of the weld.

3. A plasma arc welding processing equipment for titanium and titanium alloy thick plates, comprising a plasma arc welding machine (2) and a support platform (1), wherein the support platform (1) is used to place plates (32), and there is a gap (35) between adjacent plates (32), and the length direction of the gap (35) is arranged along the length direction of the support platform (1), wherein: The support platform (1) is provided with an arc-starting plate (33) and an arc-extinguishing plate (34), the arc-starting plate (33) and the arc-extinguishing plate (34) are both fixed on the plate (32) and are respectively located at the two ends of the gap (35), the main machine of the plasma arc welding machine (2) is connected to a support frame (3), the support frame (3) is connected to an upper air outlet pipe (41), and the air outlet of the upper air outlet pipe (41) faces the support platform (1).

4. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 3 is characterized by: The support platform (1) is provided with a protective gas release groove (11), the width of the protective gas release groove (11) is greater than the width of the gap (35), and the support platform (1) is fixedly connected with a lower air outlet pipe (42) penetrating the protective gas release groove (11), and a connecting hole (421) is provided on the outer wall of the lower air outlet pipe (42), and the connecting hole (421) is connected with the protective gas release groove (11).

5. A plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 3 or 4, characterized in that: The support frame (3) is square in shape, and a first protective curtain (51) and a second protective curtain (52) are connected to the side wall of the support frame (3). The first protective curtain (51) and the second protective curtain (52) are arranged adjacent to each other. A power motor (53) is arranged on the support frame (3). When the power motor (53) is started, the first protective curtain (51) and the second protective curtain (52) are synchronously lifted through the conduction structure (6).

6. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 5 is characterized by: The conductive structure (6) comprises a first pull rope (61), a first connecting ring (62), a first connecting shaft (63), a first support (64), a second pull rope (65), a second connecting ring (66), a second connecting shaft (67), and a second support (68). The first support (64) is connected to the support frame (3). The first connecting shaft (63) is rotatably connected to the first support (64). One end of the first pull rope (61) is connected to the first connecting shaft (63). The other end of the first pull rope (61) is connected to the first support (68). The protective curtain (51) is connected, the first connecting ring (62) is fixed on the first connecting shaft (63) and is coaxially arranged, the second support (68) is connected to the support frame (3), the second connecting shaft (67) is rotatably connected to the second support (68) and is coaxially fixedly connected to the second connecting ring (66), one end of the second pull rope (65) is connected to the second connecting shaft (67), the other end of the second pull rope (65) is connected to the second protective curtain (52), and the first connecting ring (62) is meshed with the second connecting ring (66).

7. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 6 is characterized by: The first support (64) is fixedly connected to a first gear (691), the second support (68) is rotatably connected to a second gear (692) for meshing with the first gear (691), the second support (68) is embedded with a positioning rod (693), and the positioning rod (693) is embedded in the second gear (692).

8. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 6 is characterized by: The support frame (3) is connected to a semiconductor heat sink (70); the first connecting shaft (63) is connected to a rotating rod (74) via a linkage structure (7); a fixing seat (75) is fixedly connected to the support frame (3); the fixing seat (75) is threadedly connected to the rotating rod (74); the rotating rod (74) rotates and contacts the switch of the semiconductor heat sink (70).

9. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 8, characterized in that: The linkage structure (7) comprises a first connecting gear (71), a second connecting gear (72), and a rack (73); the first connecting gear (71) is fixed on the first connecting shaft (63) and is coaxially arranged; the second connecting gear (72) is fixed on the rotating rod (74) and is coaxially arranged; the rack (73) is meshed with the first connecting gear (71) and the second connecting gear (72) at the same time; and the rack (73) is slidably connected to the support frame (3).

10. The plasma arc welding processing equipment for titanium and titanium alloy thick plates according to claim 8, characterized in that: A fan (8) is rotatably connected to the support frame (3); the body of the fan (8) corresponds to the semiconductor heat sink (70); and the switch of the fan (8) is used to contact the rotating rod (74).