Die roughing method
By presetting the top rod hole and the barrel hole in the rear model cavity of the automobile mold, and performing finishing and milling and opening the thick platform, the problems of mold demolding and BOSS column accuracy are solved, and rapid demolding and accuracy guarantee are achieved.
Patent Information
- Application Number
- CN202411297891.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-12-03
AI Technical Summary
When the car mold is demolded, the plastic is easily adhered to the model cavity, and the manufacturing accuracy of the BOSS column is difficult to ensure, and the conventional opening method leads to a reduction in accuracy.
The front and rear model cavity are combined with injection plastic, and the pole hole and the pole hole are preset on the rear model cavity. The drill bit is used to finish and mill the thick platform to ensure the accuracy of the pole hole and the BOSS column.
It realizes rapid mold release and guarantees the accuracy of the BOSS column, avoiding the problems of plastic adhesion and reduction of accuracy.
Smart Images

Figure CN119058024A_ABST
Abstract
Description
Technical Field
[0001] The invention discloses a mold roughing method and belongs to the technical field of mold roughing. Background Art
[0002] Demolding is required during the roughing of automobile molds, but the plastic will adhere to the mold cavity after cooling. If it is forcibly separated, the appearance of the plastic product will be damaged. In addition, automobile molds often use snap-on structures, which are fixed by BOSS columns. Therefore, automobile molds also need to consider how to manufacture BOSS columns. BOSS columns generally require high precision and are relatively deep. Conventional hole-opening methods will reduce precision as the hole is punched deeper, resulting in the BOSS column not meeting manufacturing requirements. Summary of the invention
[0003] The purpose of the present invention is to provide a mold roughing method to solve the problem of difficulty in pre-arranging holes in the mold cavity in the prior art.
[0004] A mold roughing method includes making a front mold cavity and a rear mold cavity according to a product shape, buckling the front mold cavity and the rear mold cavity together to form a product cavity between the front mold cavity and the rear mold cavity, injecting molten plastic into the product cavity, forming a product after the plastic is cooled, and finally removing the front mold cavity to complete demoulding.
[0005] The rear mold cavity is provided with a plurality of pre-arranged holes.
[0006] The pre-arranged holes are divided into two categories: ejector holes and sleeve holes.
[0007] The ejector pin holes are evenly distributed on the rear mold cavity.
[0008] The structure of the pre-arranged holes includes a matching section and an avoidance section. The matching section is arranged in the rear model cavity and passes through the top and bottom of the rear model cavity. The matching section extends to the bottom of the rear model cavity and the end is nested in the avoidance section. The outer diameter of the matching section is consistent with the inner diameter of the avoidance section.
[0009] Before making the rear model cavity, preset the position of the ejector hole. When the ejector hole is at a steep slope position at the top of the rear model cavity, make a rough mark on this position.
[0010] When making the rear model cavity, reserve a roughing platform at all roughing mark positions, use a drill at the preset position of the ejector hole, drill out the avoidance section and the matching section from the bottom to the top of the rear model cavity, and perform fine milling to remove the roughing platform.
[0011] Before making the rear model cavity, mark the sleeve hole according to the position of the BOSS column and make a rough mark on the location of the sleeve hole.
[0012] When making the rear model cavity, reserve roughing platforms at all roughing mark positions. At the sleeve hole, use a drill to drill the matching section from the top to the bottom of the rear model cavity, and use a drill to drill the avoidance section from the bottom to the top of the rear model cavity, and perform fine milling to remove the roughing platform.
[0013] After removing the front mold cavity, insert the ejector pin into the ejector pin hole, and the ejector pin extends along the ejector pin hole to eject the product and complete demoulding.
[0014] Compared with the prior art, the present invention has the following beneficial effects: rapid demoulding of the mold is achieved through the ejector hole, and the accuracy of the ejector hole and the BOSS column is ensured by the roughing platform. BRIEF DESCRIPTION OF THE DRAWINGS
[0015] Figure 1 is a schematic diagram of the rear mold cavity of the present invention;
[0016] Figure 2 It is a schematic diagram of the front model cavity of the present invention;
[0017] Figure 3 It is a schematic diagram of the front model cavity and the rear model cavity buckled together;
[0018] Figure 4 It is a schematic diagram of the adhesion between the rear mold cavity and the plastic product;
[0019] Figure 5 It is a schematic diagram of demoulding using a ejector pin;
[0020] Figure 6 It is a schematic diagram of the distribution of ejector pins in the rear mold cavity;
[0021] Figure 7 It is a schematic diagram of the position of the ejector pin on the plastic product;
[0022] Figure 8 This is a schematic diagram of the location of the BOSS column on the plastic product;
[0023] Fig. 9 It is a schematic diagram of the matching section and the avoidance section;
[0024] Fig.10 It is a schematic diagram of the top of the ejector hole at the steep slope position of the rear mold cavity;
[0025] Fig.11 It is a schematic diagram of the roughing platform of the ejector hole;
[0026] Fig.12 This is a schematic diagram of the roughing platform of the sleeve hole;
[0027] Fig.13 This is a schematic diagram of the roughing platform for finishing milling the sleeve hole;
[0028] The accompanying drawings include: 1-rear model cavity, 2-plastic product, 3-push rod, 4-position of push rod in plastic product, 5-column position of BOSS in plastic product, 6-matching section of push rod hole, 7-avoidance section of push rod hole, 8-steep slope position, 9-roughing platform, 10-matching section of BOSS column, 11-avoidance section of BOSS column. DETAILED DESCRIPTION
[0029] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention is described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, but not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0030] A mold roughing method includes making a front mold cavity and a rear mold cavity 1 according to a product shape, buckling the front mold cavity and the rear mold cavity 1 together to form a product cavity between the front mold cavity and the rear mold cavity 1, injecting molten plastic into the product cavity, forming a product after the plastic is cooled, and finally removing the front mold cavity to complete demoulding.
[0031] The rear mold cavity 1 is provided with a plurality of pre-arranged holes.
[0032] The pre-arranged holes are divided into two categories: ejector holes and sleeve holes.
[0033] The ejector pin holes are evenly distributed on the rear mold cavity 1.
[0034] The structure of the pre-arranged holes includes a matching section and an avoidance section. The matching section is arranged in the rear model cavity 1 and passes through the top and bottom of the rear model cavity 1. The matching section extends to the bottom of the rear model cavity 1 and the end is nested in the avoidance section. The outer diameter of the matching section is consistent with the inner diameter of the avoidance section.
[0035] Before making the rear mold cavity 1, the position of the ejector hole is preset. When the ejector hole is at a steep slope position 8 at the top of the rear mold cavity 1, this position is roughly marked.
[0036] When making the rear model cavity 1, reserve a roughing platform 9 at all roughing mark positions, use a drill bit at the preset position of the push rod hole, drill out the avoidance section and the matching section from the bottom to the top of the rear model cavity 1 in sequence, and perform fine milling to remove the roughing platform 9.
[0037] Before making the rear model cavity 1, mark the sleeve hole according to the position of the BOSS column, and roughly mark the position of the sleeve hole.
[0038] When making the rear model cavity 1, reserve a roughing platform 9 at all roughing mark positions. At the sleeve hole, use a drill to drill a fitting section from the top to the bottom of the rear model cavity 1, and use a drill to drill an avoidance section from the bottom to the top of the rear model cavity 1, and perform fine milling to remove the roughing platform 9.
[0039] After the front mold cavity is removed, the ejector pin 3 is inserted into the ejector pin hole, and the ejector pin 3 extends along the ejector pin hole to eject the product, thereby completing demoulding.
[0040] The rear mold cavity 1 and the front mold cavity of the present invention are as follows Figure 1 and Figure 2 As shown, the front mold cavity and the rear mold cavity 1 are buckled together as shown in FIG. Figure 3 As shown, after the plastic is cooled, a product is formed, and the adhesion between the mold cavity 1 and the plastic product 2 is as shown in FIG. Figure 4 Use ejector pin 3 to demould. Figure 5 The distribution of the ejector pin 3 in the rear mold cavity 1 is shown in Figure 6 As shown, the position of the ejector pin 3 on the plastic product 2 is as follows Figure 7 As shown in the figure, the position of the top rod 3 on the plastic product 4 is shown, and the position of the BOSS column on the plastic product 2 is shown in Figure 8 As shown, the figure shows BOSS in column position 5 of the plastic product.
[0041] The matching section 6 of the ejector hole and the avoidance section 7 of the ejector hole are both opened from the bottom of the rear mold cavity 1. When the ejector hole is at a steep slope position 8 at the top of the rear mold cavity 1, that is, Fig.10 If the hole is drilled directly, the steep slope at the top will cause uneven force on the drill bit, which will lead to a skewed top rod hole. Fig.11 , add a roughing platform 9 on the top to avoid uneven force application, and then remove the roughing platform 9 through fine machining in the later stage to restore it to Fig.10 looks like.
[0042] For the sleeve hole, since the BOSS column is relatively deep, if the hole is drilled in a similar way to the push rod hole, the depth of the hole will reduce the accuracy of the BOSS column, which will cause inaccurate snapping of the auto parts. Therefore, for the BOSS column, a hole is drilled from the top to form the matching section 10 of the BOSS column, and a hole is drilled from the bottom to form the avoidance section 11 of the BOSS column, so as to ensure its accuracy. Fig.12 As shown, the roughing platform 9 of the sleeve hole is removed by fine milling. Fig.13 shown.
[0043] In the present invention, when the push rod hole is processed, the rear model cavity 1 has been roughed, that is, the shape has been processed on the front side, and the push rod 3 is drilled from the back side. When the drill bit drills out, due to the shape of the cavity, it may encounter a steep slope when the drill bit drills out, and the drill bit is unevenly stressed, resulting in the drill bit swinging and poor hole processing. A roughing platform tool is developed to automatically determine whether there is a steep slope when the drill bit drills out, and automatically design a roughing platform. When the drill bit drills out, it encounters a plane, and the drill bit is evenly stressed and does not swing. After the push rod 3 is processed with the hole, the avoidance section 7 of the push rod hole is processed.
[0044] The sleeve hole is used to form the boss column, so it must meet the requirements of highly accurate positioning. The deeper the deep hole drilling, the worse the positioning accuracy. Therefore, in order to ensure accuracy, the matching section 10 of the BOSS column is processed from the front, and the avoidance section 11 of the BOSS column is processed from the back. Develop a roughing platform tool to automatically determine the sleeve matching section hole and automatically design the roughing platform. After the matching section hole is processed, the avoidance hole is processed. After the drilling is completed, fine processing is performed to mill off the roughing platform.
[0045] The above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit the same. Although the present invention has been described in detail with reference to the aforementioned embodiments, a person skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some or all of the technical features may be replaced by equivalents, and these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A mold roughing method, characterized in that: The process includes making a front mold cavity and a rear mold cavity according to the shape of the product, buckling the front mold cavity and the rear mold cavity together to form a product cavity between the front mold cavity and the rear mold cavity, injecting molten plastic into the product cavity, forming a product after the plastic is cooled, and finally removing the front mold cavity to complete demolding.
2. A mold roughing method according to claim 1, characterized in that: The rear mold cavity is provided with a plurality of pre-arranged holes.
3. A mold roughing method according to claim 2, characterized in that: The pre-arranged holes are divided into two categories: ejector holes and sleeve holes.
4. A mold roughing method according to claim 3, characterized in that: The ejector pin holes are evenly distributed on the rear mold cavity.
5. A mold roughing method according to claim 3, characterized in that: The structure of the pre-arranged holes includes a matching section and an avoidance section. The matching section is arranged in the rear model cavity and passes through the top and bottom of the rear model cavity. The matching section extends to the bottom of the rear model cavity and the end is nested in the avoidance section. The outer diameter of the matching section is consistent with the inner diameter of the avoidance section.
6. A mold roughing method according to claim 5, characterized in that: Before making the rear model cavity, preset the position of the ejector hole. When the ejector hole is at a steep slope position at the top of the rear model cavity, make a rough mark on this position.
7. A mold roughing method according to claim 6, characterized in that: When making the rear model cavity, reserve a roughing platform at all roughing mark positions, use a drill at the preset position of the ejector hole, drill out the avoidance section and the matching section from the bottom to the top of the rear model cavity, and perform fine milling to remove the roughing platform.
8. A mold roughing method according to claim 5, characterized in that: Before making the rear model cavity, mark the sleeve hole according to the position of the BOSS column and make a rough mark on the location of the sleeve hole.
9. A mold roughing method according to claim 8, characterized in that: When making the rear model cavity, reserve roughing platforms at all roughing mark positions. At the sleeve hole, use a drill to drill the matching section from the top to the bottom of the rear model cavity, and use a drill to drill the avoidance section from the bottom to the top of the rear model cavity, and perform fine milling to remove the roughing platform.
10. A mold roughing method according to claim 1, characterized in that: After removing the front mold cavity, insert the ejector pin into the ejector pin hole, and the ejector pin extends along the ejector pin hole to eject the product and complete demoulding.