Packaging structure and packaging method of silicon carbide power module
By using semi-insulated silicon carbide single-crystal double-sided copper plating substrate and vacuum reflow soldering technology in the silicon carbide power module, the thermal resistance problem at high temperature is solved, the heat dissipation efficiency and reliability of the module are improved, and the working temperature is improved.
Patent Information
- Application Number
- CN202411545463.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-01
- Publication Date
- 2024-12-06
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Silicon carbide power modules have high thermal resistance in high temperature environments, which affects their reliability, service life and working temperature, especially the stress problems caused by the difference in thermal expansion coefficient of ceramic copper clad plates.
Using semi-insulated silicon carbide single crystal double-sided copper plating substrate and vacuum reflow soldering technology, the thermal resistance of the welding layer is reduced by using aluminum bonding wires in the silicon carbide power module and optimizing welding conditions, and the oxide layer is removed through plasma cleaning. , improve heat dissipation efficiency and mechanical strength of the module.
It effectively reduces the maximum internal temperature of the silicon carbide power module, improves the heat dissipation efficiency and service life, reduces the thermal stress of the chip, and improves the reliability and working temperature of the module.
Smart Images

Figure CN119092512A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor technology, and in particular to a packaging structure and a packaging method of a silicon carbide power module. Background Art
[0002] In power electronics applications, in order to improve the current carrying capacity of power modules, a multi-chip configuration is usually adopted. As a multi-chip packaged power module, it is not only necessary to have excellent electrothermal performance, but also to maintain good thermomechanical reliability, which directly affects the service life of the module. With the reduction in the size of silicon carbide devices and the increase in power density, module packaging is moving towards miniaturization and lightweight. Compared with silicon-based power modules, the devices in silicon carbide modules have higher junction temperatures when working, so a high temperature environment becomes a basic requirement for their normal operation.
[0003] When SiC power modules operate under high temperature conditions, their rated power will decrease when the temperature exceeds a certain value. For example, the output power decreases by 30% for every 20°C increase in temperature. In actual applications, the ambient temperature fluctuates with changes in climate and system operating conditions. Normally, the module will not operate at the highest ambient temperature for a long time. If the temperature is properly controlled, the module only needs to limit its capacity in an extremely high temperature environment, thereby maximizing power under most operating conditions.
[0004] High temperature is a key factor affecting the thermomechanical reliability of power modules. For wide-bandgap SiC devices, their high-voltage, high-temperature, and high-frequency operating characteristics pose new challenges to package heat dissipation. As electric vehicles increase their power demand for SiC modules, the reliability of ceramic copper-clad laminates at high temperatures becomes particularly important. However, due to the difference in thermal expansion coefficients between ceramic and copper, large stresses are generated at the interface between the two during thermal cycling, which may cause ceramic cracking or copper layer peeling, thereby causing module failure and reducing its reliability.
[0005] At present, the heat generated in high-power density electronic packaging is mainly dissipated by conducting the heat from the ceramic copper-clad laminate to the outer shell. Since oxygen-free copper has a high thermal conductivity, the thermal conductivity of the ceramic copper-clad laminate is determined by the performance of the ceramic substrate material. However, the ceramic layer and its welding layer of this type of substrate have a large thermal resistance, which has become the main bottleneck for reducing the thermal resistance of the power module, affecting the reliability, service life and operating temperature of the power device. Summary of the invention
[0006] In order to solve the problem that the current power module has a large thermal resistance, thereby affecting the reliability, service life and operating temperature of the power device, the purpose of the present invention is to provide a packaging structure and packaging method for a silicon carbide power module.
[0007] To achieve the above objectives, the technical solution of the present invention is as follows.
[0008] A first aspect of the present invention provides a packaging structure of a silicon carbide power module, comprising: a base plate; four semi-insulating silicon carbide double-sided copper-plated substrates, which are connected to the base plate by vacuum reflow soldering; a silicon carbide power module, comprising two half-bridge circuit structures, each of which comprises six first silicon carbide chips and six second silicon carbide chips; wherein the three first silicon carbide chips and the three second silicon carbide chips correspond one to one and are connected to one of the semi-insulating silicon carbide double-sided copper-plated substrates by vacuum reflow soldering; the adjacent first silicon carbide chips and the second silicon carbide chips are connected by bonding wires; and the two semi-insulating silicon carbide double-sided copper-plated substrates located on the same half-bridge circuit structure are connected by bonding wires.
[0009] The present invention is mainly based on a semi-insulating silicon carbide single crystal double-sided copper-plated substrate and a silicon carbide power module. On the basis of reducing thermal resistance, the present invention improves the heat dissipation efficiency and service life of the silicon carbide power module, increases the operating temperature of the silicon carbide power module, and solves the problem that the current power module has a large thermal resistance, thereby affecting the reliability, service life and operating temperature of the power device.
[0010] Preferably, the bottom plate is a heat dissipation bottom plate. The heat dissipation bottom plate of the present invention can improve the heat dissipation efficiency.
[0011] Preferably, the solder used in vacuum reflow soldering is Sn5Pb 92.5 Ag 2.5 Solder. The present invention uses silicon carbide chips, Sn5Pb 92.5 Ag 2.5 After the solder paste is printed on the steel screen, it is sent to the reflow oven for reflow. The maximum temperature of vacuum reflow is set to 340℃ and maintained for 120s to reduce the void rate of the solder layer.
[0012] Preferably, the conditions for vacuum reflow soldering are: the temperature of vacuum reflow soldering is 290°C to 340°C, and the time of peak temperature reflow is 80s to 120s. The present invention mainly reduces the oxidation of components that may occur during the welding process by adopting a vacuum reflow soldering process. Vacuum reflow soldering is a soldering method that heats the paste-shaped solder pre-applied to the pad to melt it, and the vacuum value atmospheric pressure can be reduced to below 500pa and maintained for a certain period of time, thereby establishing a mechanical and electrical connection between the surface mounted components and the pad.
[0013] Preferably, the first silicon carbide chip is a SiC SBD; the second silicon carbide chip is a SiC MOSFET. In the present invention, in each half-bridge circuit structure, the number of SiC MOSFETs is 6 and the number of SiC SBDs is 6.
[0014] Preferably, the bonding wire is an aluminum bonding wire. The bonding wire of the present invention is connected by an ultrasonic bonding process. In order to reduce costs, the bonding wire is usually made of aluminum wire. Since the power loop current is large, the prepared silicon carbide power module is interconnected by 5 aluminum bonding wires with a wire diameter of 380μm. Since the drive loop current is small, the prepared silicon carbide power module is interconnected by a single aluminum bonding wire 8 with a wire diameter of 125μm as the drive loop electrical connection.
[0015] Preferably, the semi-insulating silicon carbide double-sided copper-plated substrate includes: a semi-insulating silicon carbide single crystal substrate; a first copper layer, arranged on one side of the semi-insulating silicon carbide single crystal substrate; a second copper layer, arranged on the other side of the semi-insulating silicon carbide single crystal substrate; the ratio of the thickness of the semi-insulating silicon carbide single crystal substrate, the first copper layer and the second copper layer is 100μm~1 mm: 100μm~300μm: 100μm~300μm.
[0016] Preferably, the silicon carbide single crystal in the semi-insulating silicon carbide single crystal substrate is grown in a 0-degree forward direction.
[0017] A second aspect of the present invention provides a packaging method for a silicon carbide power module, comprising the following steps: According to the packaging structure of the silicon carbide power module described in the first aspect, three first silicon carbide chips and three second silicon carbide chips are connected to a semi-insulating silicon carbide double-sided copper-plated substrate by vacuum reflow soldering; four welded semi-insulating silicon carbide double-sided copper-plated substrates are connected to a base plate by vacuum reflow soldering; the adjacent first silicon carbide chips and second silicon carbide chips on the semi-insulating silicon carbide double-sided copper-plated substrates are connected by bonding wires, and at the same time, the two semi-insulating silicon carbide double-sided copper-plated substrates located on the same half-bridge circuit structure are connected by bonding wires to form a silicon carbide power module.
[0018] Preferably, before connecting the three first silicon carbide chips and the three second silicon carbide chips to the semi-insulating silicon carbide double-sided copper-plated substrate by vacuum reflow soldering, it also includes: plasma cleaning the semi-insulating silicon carbide double-sided copper-plated substrate, the first silicon carbide chip and the second silicon carbide chip.
[0019] Preferably, the specific operation of the plasma cleaning is: self-cleaning the plasma chamber, and then oxygen cleaning and argon cleaning are performed on the semi-insulating silicon carbide double-sided copper-plated substrate, the first silicon carbide chip and the second silicon carbide chip in sequence. In the present invention, the function of oxygen cleaning is to remove organic matter attached to the surface; the function of argon cleaning is to remove possible oxide layers.
[0020] Preferably, the oxygen cleaning time is 1 min to 2 min; the argon cleaning time is 1 min to 2 min.
[0021] Beneficial effects of the present invention: 1. The present invention is mainly based on a semi-insulating silicon carbide single crystal double-sided copper-plated substrate and a silicon carbide power module. On the basis of reducing thermal resistance, the heat dissipation efficiency and service life of the silicon carbide power module are improved, and the operating temperature of the silicon carbide power module is increased, thereby solving the problem that the current power module has a large thermal resistance, thereby affecting the reliability, service life and operating temperature of the power device.
[0022] 2. The present invention can effectively reduce the maximum internal temperature of the packaging structure of the silicon carbide power module to below 70 degrees Celsius by introducing a semi-insulating silicon carbide single crystal double-sided copper-plated substrate and a silicon carbide power module.
[0023] 3. The present invention utilizes a silicon carbide power module based on a semi-insulating silicon carbide substrate, which can reduce chip thermal stress and junction temperature and improve reliability. BRIEF DESCRIPTION OF THE DRAWINGS
[0024] Figure 1 It is a schematic structural diagram of a semi-insulating silicon carbide double-sided copper-plated substrate provided by one embodiment of the present invention.
[0025] Figure 2 It is a schematic structural diagram of a packaging structure of a silicon carbide power module provided in one embodiment of the present invention.
[0026] Reference numerals: 1. First copper layer; 2. Semi-insulating silicon carbide single crystal substrate; 3. Second copper layer; 4. First silicon carbide chip; 5. Second silicon carbide chip; 6. Bottom plate; 7. Semi-insulating silicon carbide double-sided copper-plated substrate; 8. Bonding wire. DETAILED DESCRIPTION
[0027] In order to make the purpose, technical solution and advantages of the present invention more clearly understood, the present invention is further described in detail below in conjunction with the embodiments. It should be understood that the specific embodiments described herein are only used to explain the present invention and are not used to limit the present invention.
[0028] Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of the present invention.
[0029] At present, the substrates used in electronic devices and various modules include: resin substrates, ceramic substrates and metal base substrates. Resin substrates have low thermal conductivity of 1 W / (m·K), which leads to poor heat dissipation, heat resistance and reliability, and are usually used for control boards. The thermal conductivity of metal base substrates is about 2 to 6 W / (m·K), and they are mainly used for power modules rated below 600V / 50A systems. The thermal conductivity of ceramic substrates is 20 to 170 W / (m·K), and they are often used in high-power and high-current silicon carbide modules. The heat generated in high-power density electronic packaging is mainly dissipated by conducting the ceramic copper clad laminate to the outer shell. Since oxygen-free copper has a high thermal conductivity, the determining factor of the thermal conductivity of the ceramic copper clad laminate is the performance of the ceramic substrate material. However, the ceramic layer and its welding layer of this type of substrate have a large thermal resistance, which has become the main bottleneck for reducing the thermal resistance of the power module and affects the reliability of the power device. It affects the environmental reliability of the silicon carbide power module and restricts the service life of the power module.
[0030] In order to improve the heat dissipation performance of the module, an insulating substrate with high thermal conductivity must be placed between the chip and the base plate. The main method of building circuit interconnections on insulating substrates is direct bonding copper, in which a ceramic insulating layer with very good electrical insulation and dielectric strength is directly bonded between two layers of copper. These substrates are usually selected based on the application and their thermal, mechanical and electrical insulation properties. Common insulating substrate materials include aluminum oxide, aluminum nitride, silicon nitride, etc.
[0031] Among them, aluminum oxide has low cost and relatively high mechanical strength. However, compared with other materials, aluminum oxide has relatively weak thermal conductivity, which is not in line with the development requirements of subsequent power devices. Aluminum nitride has higher thermal conductivity, and its thermal expansion coefficient is almost the same as silicon, which effectively reduces problems such as delamination and solder fatigue, but its mechanical strength is not enough in larger thermal cycles. The thermal expansion coefficient of Si3N4 is also very close to that of semiconductor chips, and it provides good mechanical strength and thermal fatigue resistance, but the cost is relatively high.
[0032] Based on this, the present invention provides a packaging structure and packaging method for a silicon carbide power module to shorten the thermal resistance from the power device to the packaging substrate, improve the heat dissipation efficiency of the packaging structure, achieve the purpose of quickly reducing the junction temperature of the power device, and at the same time increase the operating temperature of the packaging structure.
[0033] The present invention is mainly based on a semi-insulating silicon carbide single crystal double-sided copper-plated substrate and a silicon carbide power module. On the basis of reducing thermal resistance, the present invention improves the heat dissipation efficiency and service life of the silicon carbide power module, increases the operating temperature of the silicon carbide power module, and solves the problem that the current power module has a large thermal resistance, thereby affecting the reliability, service life and operating temperature of the power device.
[0034] The technical solution of the present invention is further described below by means of specific examples. In the following examples, the methods described are conventional methods unless otherwise specified; the reagents and materials described are commercially available unless otherwise specified.
[0035] In the following embodiments, SiC SBD, whose full English name is Silicon Carbide Schottky Diode, is called Silicon Carbide Schottky Diode in Chinese.
[0036] SiC MOSFET, the full English name is Silicon Carbide Metal Oxide Semiconductor Field Effect Transistor, and the Chinese name is Silicon Carbide Metal Oxide Semiconductor Field Effect Transistor.
[0037] See also Figure 2 A packaging structure of a silicon carbide power module includes a base plate 6, a semi-insulating silicon carbide double-sided copper-plated substrate 7, and a silicon carbide power module. The base plate 6 is a heat dissipation base plate. The semi-insulating silicon carbide double-sided copper-plated substrate 7 has four and is connected to the base plate 6 by vacuum reflow soldering. Figure 2 , four semi-insulating silicon carbide double-sided copper-plated substrates 7 are symmetrically arranged around the bottom plate 6. The silicon carbide power module includes two half-bridge circuit structures, each of which includes six first silicon carbide chips 4 and six second silicon carbide chips 5; wherein, three first silicon carbide chips 4 and three second silicon carbide chips 5 correspond to each other one by one, and are connected to a semi-insulating silicon carbide double-sided copper-plated substrate 7 by vacuum reflow soldering; adjacent first silicon carbide chips 4 and second silicon carbide chips 5 are connected by bonding wires 8; two semi-insulating silicon carbide double-sided copper-plated substrates 7 located on the same half-bridge circuit structure are connected by bonding wires 8.
[0038] Specifically, based on the semi-insulating silicon carbide single crystal double-sided copper-plated substrate and silicon carbide power module, the heat dissipation efficiency and service life of the silicon carbide power module are improved on the basis of reducing thermal resistance, and the operating temperature of the silicon carbide power module is increased, so as to solve the problem that the current power module has a large thermal resistance, thereby affecting the reliability, service life and operating temperature of the power device.
[0039] Based on the above embodiment, as a more preferred embodiment, the solder used in vacuum reflow soldering is Sn5Pb 92.5 Ag 2.5 solder.
[0040] Based on the above embodiment, as a more preferred embodiment, the vacuum reflow soldering conditions are: the vacuum reflow soldering temperature is 290° C. to 340° C., and the reflow time at the peak temperature is 80 s to 120 s.
[0041] Specifically, in order to obtain high-quality chip interconnection, a vacuum reflow process is usually used to reduce the oxidation of components that may occur during the welding process. Vacuum reflow is a soldering method that heats the paste-shaped solder pre-applied on the pad to melt it, and the vacuum value atmospheric pressure can be reduced to below 500pa and maintained for a certain period of time, thereby establishing mechanical and electrical connections between the surface mounted components and the pad. Vacuum reflow is generally divided into four working areas: heating zone, insulation zone, reflow zone, and cooling zone. A prepared customized fixture is used to achieve the alignment of the first silicon carbide chip 4, the second silicon carbide chip 5, the semi-insulating silicon carbide double-sided copper-plated substrate 7 and the base plate 6. The thickness of the welding fixture of the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7 is 5mm, and the depth of the slot window is 1mm. In addition, in order to reduce the void rate of the welding layer, the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7 are welded with high quality in a vacuum environment. 92.5 Ag 2.5 After the solder paste is printed on the steel screen, it is sent to the reflow oven for reflow. The maximum temperature of vacuum reflow is set to 340℃ and maintained for 120s. After the vacuum reflow is completed, the bonding wire 8 is interconnected.
[0042] On the basis of the above embodiment, as a more preferred embodiment, the first silicon carbide chip 4 is a SiC SBD; and the second silicon carbide chip 5 is a SiC MOSFET.
[0043] Specifically, the embodiment of the present invention selects a half-bridge circuit structure, and in each half-bridge circuit structure, six 1200V 68A SiC MOSFETs and six 1200V 20A SiC SBDs are used to form a 1200V 300A silicon carbide power module.
[0044] On the basis of the above embodiment, as a more preferred embodiment, the bonding wire 8 is an aluminum bonding wire. The bonding wire 8 adopts an ultrasonic bonding process. In order to reduce costs, the bonding wire 8 usually adopts an aluminum wire. Since the power loop current is large, the prepared silicon carbide power module uses 5 aluminum bonding wires with a wire diameter of 380μm to interconnect. Since the drive loop current is small, the prepared silicon carbide power module uses a single aluminum bonding wire 8 with a wire diameter of 125μm to interconnect as the drive loop electrical connection.
[0045] On the basis of the above-mentioned embodiment, as a more preferred embodiment, Figure 1The semi-insulating silicon carbide double-sided copper-plated substrate 7 includes: a first copper layer 1, a semi-insulating silicon carbide single crystal substrate 2, and a second copper layer 3. The silicon carbide single crystal in the semi-insulating silicon carbide single crystal substrate 2 adopts 0-degree forward growth. The first copper layer 1 is arranged on one side of the semi-insulating silicon carbide single crystal substrate 2; the second copper layer 3 is arranged on the other side of the semi-insulating silicon carbide single crystal substrate 2; the ratio of the thickness of the semi-insulating silicon carbide single crystal substrate 2, the first copper layer 1 and the second copper layer 3 is 100μm~1mm: 100μm~300μm: 100μm~300μm.
[0046] Specifically, if Figure 1 The single crystal in the semi-insulating silicon carbide single crystal substrate 2 is grown forward at 0 degrees, with a thickness of 100μm to 1mm; and in order to achieve the purpose of insulation, the resistivity is greater than 1e5. The lower surface of the semi-insulating silicon carbide single crystal substrate 2 is a second copper layer 3, which is attached to the lower surface of the semi-insulating silicon carbide single crystal substrate 2 and has a thickness of 100 to 300μm. The upper surface of the semi-insulating silicon carbide single crystal substrate 2 is a first copper layer 1, which is attached to the upper surface of the semi-insulating silicon carbide single crystal substrate 2 and has a thickness of 100 to 300μm.
[0047] Based on the above embodiments, a packaging method for a silicon carbide power module is provided, comprising the following steps: according to Figure 2 The packaging structure of the silicon carbide power module is as follows: three first silicon carbide chips 4 and three second silicon carbide chips 5 are connected to a semi-insulating silicon carbide double-sided copper-plated substrate 7 by vacuum reflow soldering; then the four welded semi-insulating silicon carbide double-sided copper-plated substrates 7 are connected to a bottom plate 6 by vacuum reflow soldering; thereafter, the adjacent first silicon carbide chips 4 and second silicon carbide chips 5 on the semi-insulating silicon carbide double-sided copper-plated substrate 7 are connected by bonding wires, and at the same time, the two semi-insulating silicon carbide double-sided copper-plated substrates 7 located on the same half-bridge circuit structure are connected by bonding wires 8 to form a silicon carbide power module, such as Figure 2 shown.
[0048] On the basis of the above embodiment, as a more preferred embodiment, before the three first silicon carbide chips 4 and the three second silicon carbide chips 5 are connected to the semi-insulating silicon carbide double-sided copper-plated substrate 7 by vacuum reflow soldering, it also includes: The semi-insulating silicon carbide double-sided copper-plated substrate 7, the first silicon carbide chip 4 and the second silicon carbide chip 5 are plasma cleaned.
[0049] On the basis of the above embodiment, as a more preferred embodiment, the specific operation of the plasma cleaning is: self-cleaning the plasma chamber, and then oxygen cleaning and argon cleaning are performed on the semi-insulating silicon carbide double-sided copper-plated substrate, the first silicon carbide chip and the second silicon carbide chip in sequence. Preferably, the oxygen cleaning time is 1min to 2min; the argon cleaning time is 1min to 2min. Specifically, the role of oxygen cleaning is to remove organic matter attached to the surface; the role of argon cleaning is to remove possible oxide layers.
[0050] Specifically, in order to avoid the introduction of pollutants in the previous process, before the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7 are welded, the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7 to be welded need to be cleaned again with a plasma cleaning machine. Before cleaning the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7, the plasma chamber needs to be self-cleaned. Then, oxygen cleaning is performed for 2 minutes to remove organic matter attached to the surface, and then argon cleaning is performed for 2 minutes to remove possible oxide layers, and then the first silicon carbide chip 4, the second silicon carbide chip 5 and the semi-insulating silicon carbide double-sided copper-plated substrate 7 are welded.
[0051] Based on the above implementation, Figure 2 The packaging structure of the silicon carbide power module is studied on the ceramic materials in the semi-insulating silicon carbide double-sided copper-plated substrate 7, and the ceramic materials include Al2O3, AlN, Si3N4 and SiC; the packaging structure of the silicon carbide power module packaged with the semi-insulating silicon carbide double-sided copper-plated substrate 7 prepared by these four ceramic materials is compared and analyzed, and simulation is carried out under the same conditions. The results are shown in Table 1.
[0052] Table 1 Simulation results of packaging structures of SiC power modules packaged with different ceramic materials
[0053] From the comparative analysis results in Table 1, it can be seen that the maximum internal temperature of the packaging structure of the silicon carbide power module encapsulated by introducing silicon carbide as a ceramic material is relatively low. This shows that the packaging structure of the silicon carbide power module provided by the embodiment of the present invention can reduce the thermal stress and junction temperature of the chip without the need for surface metallization. Since the thermal conductivity of semi-insulating silicon carbide as a ceramic material is better than that of traditional materials, it will not cause the junction temperature of the chip to rise too much, thereby preventing the chip from being damaged by excessive thermal stress and causing reliability problems.
[0054] The vacuum reflow soldering simulation was performed on the semi-insulating silicon carbide double-sided copper-plated substrate 7 made of four ceramic materials: Al2O3, AlN, Si3N4 and SiC. The results are shown in Table 2.
[0055] Table 2 Vacuum reflow soldering simulation results
[0056] From the results in Table 2, it can be seen that the maximum z-direction warpage of the semi-insulating silicon carbide double-sided copper-plated substrate 7 prepared with silicon carbide as the ceramic material provided by the embodiment of the present invention is reduced by about 81%, 70%, and 68% respectively compared with Al2O3, AlN, and Si3N4. This shows that the embodiment of the present invention can solve the DBC warpage problem in the preparation process of the silicon carbide module, reduce the thermal resistance of the semi-insulating silicon carbide double-sided copper-plated substrate, thereby improving the heat dissipation efficiency of the silicon carbide module and increasing the operating temperature of the silicon carbide power module.
[0057] The above are only preferred embodiments of the present invention and are not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A packaging structure of a silicon carbide power module, It is characterized in that include: Bottom plate (6); A semi-insulating silicon carbide double-sided copper-plated substrate (7), having four substrates and connected to the base plate (6) by vacuum reflow soldering; A silicon carbide power module, comprising two half-bridge circuit structures, each of the half-bridge circuit structures comprising six first silicon carbide chips (4) and six second silicon carbide chips (5); The three first silicon carbide chips (4) and the three second silicon carbide chips (5) correspond to each other one by one and are connected to a semi-insulating silicon carbide double-sided copper-plated substrate (7) by vacuum reflow soldering; The adjacent first silicon carbide chip (4) and the second silicon carbide chip (5) are connected via bonding wires; and the two semi-insulating silicon carbide double-sided copper-plated substrates (7) located on the same half-bridge circuit structure are connected via bonding wires.
2. The packaging structure of the silicon carbide power module according to claim 1, It is characterized in that The solder used in vacuum reflow soldering is Sn 5 Pb 92.5 Ag 2.5 solder.
3. The packaging structure of the silicon carbide power module according to claim 1, It is characterized in that The conditions for vacuum reflow soldering are: the temperature of vacuum reflow soldering is 290℃~340℃, and the time of peak temperature reflow is 80s~120s.
4. The packaging structure of the silicon carbide power module according to claim 1, It is characterized in that The first silicon carbide chip (4) is a SiC SBD; and the second silicon carbide chip (5) is a SiC MOSFET.
5. The packaging structure of the silicon carbide power module according to claim 1, It is characterized in that The bonding wire is an aluminum bonding wire.
6. The packaging structure of the silicon carbide power module according to claim 1, It is characterized in that The semi-insulating silicon carbide double-sided copper-plated substrate (7) comprises: Semi-insulating silicon carbide single crystal substrate (2); A first copper layer (1) is arranged on one side of the semi-insulating silicon carbide single crystal substrate (2); A second copper layer (3) is arranged on the other side of the semi-insulating silicon carbide single crystal substrate (2); The thickness ratio of the semi-insulating silicon carbide single crystal substrate (2), the first copper layer (1) and the second copper layer (3) is 100 μm to 1 mm: 100 μm to 300 μm: 100 μm to 300 μm.
7. The packaging structure of the silicon carbide power module according to claim 6, It is characterized in that The silicon carbide single crystal in the semi-insulating silicon carbide single crystal substrate (2) is grown in a 0-degree forward direction.
8. A packaging method for a silicon carbide power module, It is characterized in that The following steps are involved: According to the packaging structure of the silicon carbide power module of claim 1, three first silicon carbide chips (4) and three second silicon carbide chips (5) are connected to a semi-insulating silicon carbide double-sided copper-plated substrate (7) by vacuum reflow soldering; Connecting four welded semi-insulating silicon carbide double-sided copper-plated substrates (7) to the base plate (6) by vacuum reflow soldering; A first silicon carbide chip (4) and a second silicon carbide chip (5) adjacent to each other on a semi-insulating silicon carbide double-sided copper-plated substrate (7) are connected via bonding wires, and at the same time, two of the semi-insulating silicon carbide double-sided copper-plated substrates (7) located on the same half-bridge circuit structure are connected via bonding wires to form a silicon carbide power module.
9. The method for packaging a silicon carbide power module according to claim 8, It is characterized in that Before the three first silicon carbide chips (4) and the three second silicon carbide chips (5) are connected to the semi-insulating silicon carbide double-sided copper-plated substrate (7) by vacuum reflow soldering, the method further comprises: The semi-insulating silicon carbide double-sided copper-plated substrate (7), the first silicon carbide chip (4) and the second silicon carbide chip (5) are plasma cleaned.
Citation Information
Patent Citations
Module with multiple silicon carbide chips connected in parallel
CN113764358A
Multi-chip parallel half-bridge module based on SiC MOSFET
CN114695290A
Silicon carbide single crystal AMB copper-clad substrate and power device thereof
CN117779029A
Silicon carbide single crystal copper-clad circuit board for power module and preparation method
CN117979541A
Packaging structure of IGBT (Insulated Gate Bipolar Translator) module
CN217641329U