Log skin flowerpot and manufacturing method thereof
By peeling the outer skin from the log and using waterproof materials and fillers, the problems of extended time and low durability during the manufacturing process of log pots are solved, and efficient production and durability are achieved.
Patent Information
- Application Number
- CN202380042035.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-07-15
- Filing Date
- 2023-06-23
- Publication Date
- 2025-01-10
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing log flower pots have problems such as extended time, low production capacity and reduced durability during the manufacturing process, especially oak wood, which is prone to rot, resulting in the inability to produce in large quantities.
By peeling the outer skin from the xylem of the log, a longitudinally cut peripheral portion is formed and a waterproof material and filler are used to improve sealing and moisture resistance, combined with underfills and support members to enhance bottom thickness and waterproof performance.
The rapid separation and mass production of log-skin flower pots is achieved, which improves durability, prevents rot and mold, enhances waterproofing, and enables the flower pot to be semi-permanently used.
Smart Images

Figure CN119300707A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a flower pot. Background Art
[0002] Usually, flowerpot is the vessel that is used to plant and cultivate plants such as flowers or trees. Known this flowerpot has plastic injection molding, i.e. plastic flowerpot and ceramic flowerpot baked with soil etc.
[0003] Such plastic or ceramic flower pots have a cold and hard feeling due to the characteristics of their materials, and therefore have limitations in giving a natural and spontaneous feeling.
[0004] As an existing technology to improve this problem, a log flower pot disclosed in Korean Authorized Utility Model Gazette No. 20-0427153 is manufactured in the following manner: a log with a thick outer layer is prepared as a material and the prepared log is cut horizontally, leaving only 5 to 10 mm on the outside of the log, and the wooden part inside is dug out.
[0005] However, the existing log flower pots provide a technical structure that involves a method of digging out the wood with a machine, so there is a problem of extended manufacturing time due to the time required for digging. In particular, for oak trees with hard wood, there is a problem of extremely low production capacity. For example, the processing blade is damaged before a few are produced. Due to the characteristics of flower pots, they are often in contact with water, so there is a problem of reduced durability such as the wood being easily rotten, so they cannot be mass-produced, and there is a problem that they cannot be developed and circulated as a commodity in reality. Summary of the invention
[0006] Problem that the invention aims to solve
[0007] The technical problem of the present invention is to provide a log outer skin flower pot and a manufacturing method thereof, which can faithfully convey the natural feeling and improve the processability so that it can be mass-produced.
[0008] Another technical problem of the present invention is to provide a log rind flower pot with improved durability and a method for manufacturing the same.
[0009] Means used to solve problems
[0010] In order to achieve the above-mentioned purpose, the log bark flower pot of an embodiment of the present invention includes: a bark, which is peeled off from the wood part of the log and has a longitudinal cut portion; a peripheral forming portion, which forms the peripheral part in a manner that includes the bark and has a shape that penetrates from top to bottom; and a bottom surface forming portion, which seals the lower open portion of the peripheral forming portion and forms the bottom.
[0011] The bark may be stripped from the wood of the log by boiling or pre-treatment with a stripping agent.
[0012] As an example, the outer peripheral forming part may include: an outer peripheral forming member, which is made of the outer skin and has the longitudinal cut portion bonded; an outer peripheral waterproof member, which is tubular and located inside the outer peripheral forming member; an outer peripheral fixing part, which fixes the outer peripheral forming member and the outer peripheral waterproof member on the bottom surface forming part so that the interval between the inner surface of the outer peripheral forming member and the outer surface of the outer peripheral waterproof member is maintained at a set interval; and an outer peripheral filler of waterproof material, which is filled between the inner surface of the outer peripheral forming member and the outer surface of the outer peripheral waterproof member. Among them, PET or PVC hose can be used as the outer peripheral waterproof member, silicone can be used as the outer peripheral fixing part to improve the sealing force between the outer peripheral forming member and the outer peripheral waterproof member and the bottom surface forming member, and transparent epoxy resin can be used as the outer peripheral filler.
[0013] As another example, the outer peripheral forming part may include: an outer peripheral forming member, which is made of the outer skin and whose perimeter is cut based on the longitudinal cut portion; an outer peripheral waterproof member, which is tubular, is wrapped by the outer peripheral forming member, and has an outer diameter corresponding to the inner diameter of the cut perimeter; an adhesive, which bonds the inner surface of the outer peripheral forming member to the outer surface of the outer peripheral waterproof member; and an outer peripheral fixing part, which fixes the bonded outer peripheral forming member and the outer peripheral waterproof member to the bottom surface forming part. Silicone can be used as the outer peripheral fixing part to improve the sealing force between the outer peripheral waterproof member and the bottom surface forming member.
[0014] As another example, the outer peripheral forming part may include: an outer peripheral forming member, which is made of the outer skin and has the longitudinal cut portion bonded; an outer peripheral fixing portion, which fixes the outer peripheral forming member to the bottom surface forming portion; and an outer peripheral waterproofing agent made of a waterproof material, which is applied to the inner surface of the outer peripheral forming member. The outer peripheral waterproofing agent may be applied to the inner surface of the outer peripheral forming member more than once. A transparent epoxy resin may be used as the outer peripheral waterproofing agent.
[0015] The bottom surface forming part may include a plate-shaped bottom surface forming member that blocks the lower opening of the peripheral forming part. The bottom surface forming member may be plate-shaped and may be made of a waterproof material such as plastic. For example, PET (polyethylene terephthalate) material may be used as the plastic.
[0016] The bottom surface forming part may further include a bottom surface filler filled on the bottom surface forming part. A transparent epoxy resin may be used as the bottom surface filler. The transparent epoxy resin used as the bottom surface filler may further contain a toner.
[0017] The log husk flower pot of the above-mentioned embodiment of the present invention may further include a drainage hole formed by penetrating the bottom surface forming component and the bottom surface filler.
[0018] The log husk flowerpot of the above-mentioned embodiment of the present invention may further include a bottom surface supporting member, which is disposed on the lower surface of the bottom surface forming member and supports the bottom surface forming member in a state of being separated from the ground.
[0019] The bottom support component may be made of a rubber material or coated with a rubber material.
[0020] On the other hand, the method for manufacturing the log bark flower pot of an embodiment of the present invention includes: a cutting step of cutting the log into a set length; a pretreatment step of pretreatment the bark of the cut log so that the bark can be smoothly peeled off from the wood part; a separation step of separating the bark from the wood part by longitudinally cutting the pretreated log bark; a drying step of drying the separated bark; and a periphery and bottom surface forming step of forming the periphery and the bottom surface using the periphery forming part including the dried bark and the bottom surface forming part including the bottom surface forming part.
[0021] As an example, the pretreatment step may include the following steps: preparing a container filled with water; placing the cut logs in the prepared container; and heating the water for a set time, wherein the set time may be about 1 hour.
[0022] As another example, the pretreatment step may include the following steps: preparing a container filled with water; adding a stripping agent to the prepared container; and soaking the cut logs in the container with the stripping agent for a set time, wherein the set time may be about 2 days.
[0023] As an example, the periphery and bottom surface forming step may include the following steps: completing the periphery forming component by gluing the cut portion of the dried outer skin; placing a tubular periphery waterproof component inside the periphery forming component in order to block water from penetrating into the inner surface of the periphery forming component; fixing the periphery forming component and the periphery waterproof component to the bottom surface forming component so that the interval between the inner surface of the periphery forming component and the outer surface of the periphery waterproof component is maintained at a set interval; and filling a periphery filler of a waterproof material between the inner surface of the periphery forming component and the outer surface of the periphery waterproof component. The set interval may be about 3 mm to 5 mm. The cut portion of the outer skin may be glued with a wood adhesive. In order to fix the periphery forming component and the periphery waterproof component to the bottom surface forming component, silicone may be used. At the same time, the periphery and bottom surface forming step may also include the following steps: filling a bottom surface filler on the bottom surface forming component after the step of filling with the periphery filler. The bottom surface filler may be filled to a thickness of about 15 mm to 20 mm.
[0024] As another example, the periphery and bottom surface forming step may include the following steps: preparing a tubular periphery waterproof component; cutting the circumference of the dried outer skin in a manner suitable for the outer diameter of the periphery waterproof component, and manufacturing the cut outer skin into a periphery forming component; wrapping and bonding the periphery waterproof component using the cut periphery forming component; and fixing the periphery forming component and the periphery waterproof component to the bottom surface forming component. In order to fix the periphery forming component and the periphery waterproof component to the bottom surface forming component, silicone may be used. At the same time, the periphery and bottom surface forming step may also include the following steps: after the step of fixing the bottom surface forming component, filling the bottom surface filling agent on the bottom surface forming component. In which, the bottom surface filling agent may be filled to a thickness of about 15 mm to 20 mm.
[0025] As another example, the periphery and bottom surface forming step may include the following steps: completing the periphery forming component by gluing the cut portion of the dried outer skin; fixing the bottom surface forming component on the lower end surface of the periphery forming component; and coating the inner surface of the periphery forming component with a periphery waterproofing agent made of a waterproof material in order to block water from penetrating into the inner surface of the periphery forming component. In order to fix the bottom surface forming component on the lower end surface of the periphery forming component, silicone may be used. The periphery waterproofing agent may be coated 2 to 3 times. At the same time, the step of forming the periphery and bottom surface may also include the following steps: before or after the step of coating the periphery waterproofing agent, filling the bottom surface forming component with a bottom surface filler. In order to prevent water from penetrating into the inner ...
[0026] The manufacturing method of the log outer skin flower pot of the above-mentioned embodiment of the present invention may further include: a drainage hole forming step, after the step of forming the outer periphery and the bottom surface, forming a drainage hole by penetrating the bottom surface forming component and the bottom surface filler.
[0027] The manufacturing method of the log bark flower pot of the above-mentioned embodiment of the present invention may also include: a supporting step, after the step of forming the outer periphery and the bottom surface, a bottom surface supporting component is arranged on the lower surface of the bottom surface forming component, and the bottom surface forming component is supported in a state separated from the ground.
[0028] Effects of the Invention
[0029] As described above, the log husk flowerpot and the manufacturing method thereof according to the embodiments of the present invention can have the following effects.
[0030] According to an embodiment of the present invention, a log bark flower pot is provided, wherein the log bark flower pot comprises a bark, a peripheral forming portion and a bottom forming portion, wherein the bark is peeled off from the wood portion of the log and has a longitudinal cut portion, and the peripheral forming portion comprises the bark and forms a peripheral portion, presenting a shape that is through-through from top to bottom, therefore, the log bark flower pot of the present invention can form a natural original appearance through the bark of the log, thereby can faithfully express a natural and natural feeling, and is different from the prior art of manufacturing a flower pot by laboriously digging out the hard wood portion of the log, the log bark can be easily separated by peeling the log bark from the wood portion, thereby significantly improving production capacity, and thus the log bark flower pot of the present invention can be mass-produced.
[0031] In addition, according to an embodiment of the present invention, a technical solution is provided for peeling the bark from the wood part of a log by pretreatment (by boiling or using a stripping agent). Therefore, even without using a separate physical tool (a saw or a knife, etc.), the bark of the log can be more easily peeled from the wood part through this pretreatment, ultimately contributing to the mass production of the log bark flower pots of the present invention.
[0032] In addition, according to an embodiment of the present invention, a technical solution is provided in which a peripheral forming part includes a peripheral forming component made of the outer bark and a peripheral waterproof component or a peripheral waterproof agent for waterproofing. Therefore, the peripheral forming component made of the outer bark of the log can be prevented from rotting or moldy due to watering the log outer bark flower pot of the present invention. Ultimately, the moisture resistance is improved, so that the log outer bark flower pot of the present invention can be used semi-permanently.
[0033] In addition, according to an embodiment of the present invention, a technical solution is provided which also includes a bottom filler, so that the thickness of the bottom of the log bark flower pot of the present invention can be strengthened together with the bottom forming component and the waterproof performance can be improved.
[0034] In addition, according to an embodiment of the present invention, a technical solution including a bottom support component is provided, so that the bottom forming component can be supported in a state separated from the ground, so that the drainage hole is not blocked by the table, so that the discharged water can be smoothly discharged to the outside, and the air permeability is good. In the log bark flower pot of the present invention, mold can be prevented, and deformation of the peripheral forming component made of the log bark can be prevented.
[0035] On the other hand, according to an embodiment of the present invention, there is provided a method for manufacturing a log bark flower pot, the method comprising: a cutting step of cutting a log into a set length, a pretreatment step of pretreatment the bark of the cut log so that the bark can be smoothly peeled off from the wood part, a separation step of separating the bark from the wood part by longitudinally cutting the bark of the pretreated log, a drying step of drying the separated bark, and a periphery and bottom surface forming step of forming the periphery and the bottom surface using a periphery forming portion including the dried bark and a bottom surface forming portion including a bottom surface forming component; therefore, the log bark flower pot of the present invention can form a natural original appearance through the bark of the log, thereby faithfully expressing a natural and natural feeling, and in the manufacturing method, unlike the prior art of manufacturing a flower pot by laboriously digging out the hard wood part of the log, the bark of the log can be easily separated by peeling it from the wood part through the pretreatment process, thereby significantly improving the production capacity, so that the log bark flower pot of the present invention can be mass-produced. BRIEF DESCRIPTION OF THE DRAWINGS
[0036] Figure 1 It is a cross-sectional view schematically showing a log-bark flowerpot according to a first embodiment of the present invention.
[0037] Figure 2 It is schematically shown Figure 1 Illustration of the process of making log bark flower pots.
[0038] Figure 3 It is shown in pictures Figure 1 Picture of a log bark flower pot.
[0039] Figure 4 It is schematically shown Figure 3 Illustration of the state of growing plants in log bark pots.
[0040] Figure 5 It is schematically shown Figure 1 Flow chart of the manufacturing method of the log outer skin flower pot.
[0041] Figure 6 It is a cross-sectional view schematically showing a log-bark flowerpot according to a second embodiment of the present invention.
[0042] Figure 7 It is shown in pictures Figure 6 Picture of a log bark flower pot.
[0043] Figure 8 It is schematically shown Figure 7 Illustration of the state of growing plants in log bark pots.
[0044] Fig. 9 It is schematically shown Figure 6 Flow chart of the manufacturing method of the log outer skin flower pot.
[0045] Fig.10 It is a cross-sectional view schematically showing a log-bark flowerpot according to a third embodiment of the present invention.
[0046] Fig.11 It is schematically shown Fig.10 Flow chart of the manufacturing method of the log outer skin flower pot. DETAILED DESCRIPTION
[0047] Hereinafter, embodiments of the present invention will be described in detail with reference to the accompanying drawings so that those skilled in the art can easily implement the present invention. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein.
[0048] Figure 1 is a cross-sectional view schematically showing a log outer skin flower pot according to a first embodiment of the present invention, Figure 2 It is schematically shown Figure 1 Illustration of the process of making log bark flower pots. Figure 3 Yes Yes Show Figure 1 A three-dimensional picture of a log-bark flower pot. Figure 4 It is schematically shown Figure 3 Illustration of the state of growing plants in log bark pots.
[0049] like Figures 1 to 4 As shown, the log skin flower pot 100 of the first embodiment of the present invention comprises: a skin L12, a peripheral forming portion 110 and a bottom surface forming portion 120. Figures 1 to 4 , each component is described in detail.
[0050] like Figure 1 and Figure 2 As shown, the outer skin L12 is one of the components used to form the outer peripheral forming portion 110. Figure 2 As shown, the outer skin L12 can be peeled off from the wood part L11 of the log L10 and has a longitudinal cut portion S11. For example, in order to obtain the outer skin L12, the log L10 is cut into a set length ( Figure 2 a portion), which can be cut longitudinally ( Figure 2The outer bark L12 of the cut log L10 is peeled off from the wood part L11. Then, the outer bark L12 can be provided after being dried.
[0051] like Figure 1 and Figure 2 As shown, the outer periphery forming portion 110 is a component for forming the outer periphery of the log outer skin flower pot 100 of the present invention. Figure 2 As shown, the outer peripheral forming portion 110 may include the outer skin L12 peeled off from the wood portion L11 of the log L10, and may be in a vertically penetrating shape (see Figure 2 b) of the
[0052] like Figure 1 As shown, the bottom surface forming part 120 is a component for forming the bottom of the log outer skin flower pot 100 of the present invention. Such a bottom surface forming part 120 can be set in a manner to block the lower opening of the peripheral forming part 110. For example, the bottom surface forming part 120 may include a plate-shaped bottom surface forming part 121 that blocks the lower opening of the peripheral forming part 110. Furthermore, the bottom surface forming part 121 can be made of a waterproof material such as plastic. For reference, when the log outer skin flower pot 100 of the present invention is placed on a table, etc., the bottom surface forming part 121 is a component facing the upper surface of the table, so compared with the outer skin L12 of the peripheral forming part 110, its external exposure is quite small, and it may be more advantageous to use plastic with good waterproof properties instead of logs. Furthermore, the bottom surface forming part 121 can be made of a transparent material, and can be made of PET (polyethylene terephthalate) material, which is a kind of plastic.
[0053] Therefore, since the constituent elements as described above are provided, the log bark flower pot 100 of the present invention can form a natural original appearance through the bark L12 of the log L10, thereby can faithfully express the natural feeling. Unlike the prior art that manufactures flower pots by laboriously digging out the hard wood of the log, the bark L12 of the log L10 can be easily separated by peeling it from the wood L11, thereby significantly improving production capacity, so that the log bark flower pot 100 of the present invention can be mass-produced.
[0054] Furthermore, the outer skin L12 forming the outer covering of the outer peripheral forming portion 110 can be peeled off from the wood portion L11 of the log L10 by pretreatment, i.e., by boiling or using a peeling agent (containing sodium hydroxide). Therefore, even without using a separate physical tool (a saw or a knife, etc.) for peeling, the outer skin L12 of the log L10 can be peeled off from the wood portion L11 more easily by such pretreatment, and ultimately, it is more conducive to the mass production of the log outer skin flower pot 100 of the present invention.
[0055] Below, continue to refer to Figures 1 to 4 , the outer peripheral forming portion 110 is described in more detail.
[0056] The outer peripheral forming portion 110 may have a structure that blocks water from penetrating into the outer peripheral forming member 111 made of the outer skin L12. Figure 1 and Figure 2 As shown, the outer peripheral forming part 110 may include: an outer peripheral forming member 111, an outer peripheral waterproof member 112, an outer peripheral fixing member 113 and an outer peripheral filler 114. The outer peripheral forming member 111 may be made of an outer skin L12, and may have a state in which a longitudinal cut portion S11 of the outer skin L12 is bonded with a wood adhesive. The outer peripheral waterproof member 112 may be in a pipe shape and may be located inside the outer peripheral forming member 111. The outer peripheral fixing member 113 may fix the outer peripheral forming member 111 and the outer peripheral waterproof member 112 to the bottom surface forming member 121 so that a set interval is maintained between the inner surface of the outer peripheral forming member 111 and the outer surface of the outer peripheral waterproof member 112. The outer peripheral filler 114 may be made of a waterproof material and may be filled between the inner surface of the outer peripheral forming member 111 and the outer surface of the outer peripheral waterproof member 112. Among them, PET or the like can be used as the outer waterproof component 112, silicone or the like can be used as the outer fixing part 113, which is used to improve the sealing force between the outer forming component 111 and the outer waterproof component 112 and the bottom surface forming component 121, and transparent epoxy resin can be used as the outer filler 114.
[0057] Therefore, even if water is poured on the plants in the log bark flower pot 100 of the present invention, the water flowing to the peripheral forming part 111 can be blocked by the peripheral waterproof part 112 and the peripheral filler 114, thereby preventing the peripheral forming part 111 made of the bark L12 of the log L10 from rotting or mold, and ultimately improving the moisture resistance, so that the log bark flower pot 100 of the present invention can be used semi-permanently.
[0058] At the same time, Figure 1 and Figure 2 As shown, the log skin flower pot 100 of the first embodiment of the present invention may further include a bottom filler 122. The bottom filler 122 may be filled on the bottom forming member 121. The bottom filler 122 may be filled to a thickness of about 15 mm to 20 mm. Therefore, together with the bottom forming member 121, the thickness of the bottom of the log skin flower pot 100 of the present invention may be strengthened and the waterproof performance may be improved.
[0059] In addition, a transparent epoxy resin may be used as the bottom surface filler 122. Furthermore, the transparent epoxy resin used as the bottom surface filler 122 may further contain a toner (not shown) for forming a bottom surface pattern.
[0060] At the same time, Figure 1 and Figure 2As shown, the log outer skin flower pot 100 of the first embodiment of the present invention may further include a drainage hole 130. The drainage hole 130 may be in a shape that penetrates the bottom surface forming member 121 and the bottom surface filler 122.
[0061] At the same time, Figure 1 and Figure 2 As shown, the log skin flower pot 100 of the first embodiment of the present invention may further include a bottom surface support member 140. The bottom surface support member 140 may be disposed on the lower surface (i.e., the bottom surface) of the bottom surface forming member 121, and may support the bottom surface forming member 121 in a state separated from the ground. Therefore, the drainage hole 130 is not blocked by the table, so that the drained water can be smoothly drained to the outside. For example, the bottom surface support member 140 may be made of a rubber material or coated with a rubber material.
[0062] Below, refer to Figures 1 to 5 , a method for manufacturing the log outer skin flower pot 100 according to the first embodiment of the present invention is described.
[0063] Figure 5 It is schematically shown Figure 1 Flow chart of the manufacturing method of the log outer skin flower pot.
[0064] First, the method for manufacturing the log skin flower pot 100 according to the first embodiment of the present invention is to cut the log L10 into a set length ( Figure 2 Part A and Figure 5 For reference, the set length may be the height of the log bark flower pot 100 of the present invention.
[0065] Next, the bark L12 of the cut log is pretreated so that the bark is smoothly peeled off from the wood part L11 (step S120). As an example, the pretreatment process (step S120) is not shown in the figure, but can be carried out through the following series of processes: prepare a container filled with water (not shown), place the cut log in the prepared container, and heat the water for a set time. Among them, the set heating (boiling) time can be about 1 hour. As another example, the pretreatment process is not shown in the figure, but can be carried out through the following series of processes: prepare a container filled with water, add a stripping agent containing sodium hydroxide to the prepared container, and soak the cut log in the container with the stripping agent for a set time. Among them, the set soaking time can be about 2 days.
[0066] Then, the bark L12 of the pretreated log can be separated from the wood part L11 by cutting the bark L12 longitudinally. Figure 2 Part b and c of Figure 5Next, the separated outer skin L12 is dried in a cool place (step S140). Then, the outer skin forming part 110 including the dried outer skin L12 and the bottom surface forming part 120 including the bottom surface forming part 121 are used to form the outer skin and bottom surface of the log outer skin flower pot 100 of the present invention (step S130). Figure 2 Parts d, e, f and g of Figure 5 Specifically, the process of forming the periphery and the bottom surface ( Figure 5 Step S150) is as follows.
[0067] First, the outer peripheral forming member 111 ( Figure 2 The d part, Figure 5 Then, in order to block water from penetrating into the inner surface of the peripheral forming member 111, a tubular peripheral waterproof member 112 ( Figure 5 Next, the combination of the outer peripheral forming member 111 and the outer peripheral waterproof member 112 can be fixed to the bottom surface forming member 121 by the outer peripheral fixing portion 113, so that the interval between the inner surface of the outer peripheral forming member 111 and the outer surface of the outer peripheral waterproof member 112 is maintained at a set interval ( Figure 5 Finally, a peripheral filler 114 made of a waterproof material may be filled between the inner surface of the peripheral forming member 111 and the outer surface of the peripheral waterproof member 112 ( Figure 5 Step S154).
[0068] In the process of completing the peripheral forming part 111 ( Figure 5 In step S151), the cut portion S11 of the outer skin L12 can be bonded with a wood adhesive. And, the process of fixing the bottom surface forming member 121 using the peripheral fixing portion 113 ( Figure 5 In step S153), the bottom surface forming member 121 may be plate-shaped and may be made of waterproof materials such as plastics. PET (polyethylene terephthalate) material may be used as plastics, and silicone may be used as the peripheral fixing portion 113 to improve the sealing force between the peripheral forming member 111 and the peripheral waterproof member 112 and the bottom surface forming member 121. The set interval between the peripheral forming member 111 and the peripheral waterproof member 112 may be about 3 mm to 5 mm, PET may be used as the peripheral waterproof member 112, and transparent epoxy resin may be used as the peripheral filler 114.
[0069] At the same time, in the process of filling the peripheral filler as described above ( Figure 5 After the step S154 is completed, the process of forming the periphery and the bottom surface ( Figure 5The step S150 may further include a process of filling the bottom surface filler 122 on the bottom surface forming member 121 ( Figure 5 Step S155). The bottom filler 122 may be filled to a thickness of 15 mm to 20 mm.
[0070] Then, after filling the bottom filler 122, the drainage hole 130 can be formed by penetrating the bottom forming member 121 and the bottom filler 122 (step S160). Finally, the bottom support member 140 is provided on the lower surface of the bottom forming member 121 to support the bottom forming member 121 in a state separated from the ground (step S170).
[0071] Below, refer to Figures 6 to 8 , the log bark flower pot 200 according to the second embodiment of the present invention is described.
[0072] Figure 6 is a cross-sectional view schematically showing a log outer skin flower pot according to a second embodiment of the present invention, Figure 7 It is shown Figure 6 A three-dimensional picture of a log-bark flower pot. Figure 8 It is schematically shown Figure 7 Illustration of the state of growing plants in log bark pots.
[0073] like Figure 6 As shown, except for the outer peripheral forming portion 210, the log bark flower pot 200 of the second embodiment of the present invention is the same as the first embodiment of the present invention described above, so the following description will mainly focus on this.
[0074] like Figure 6 As shown, the outer periphery forming part 210 may include: an outer periphery forming member 211, an outer periphery waterproof member 212, an adhesive 213 and an outer periphery fixing member 214. The outer periphery forming member 211 may be made of an outer skin L12, and its circumference may be measured by a longitudinal cut portion (refer to Figure 2 The outer peripheral waterproof member 212 may be provided in a directly split state without bonding the wood with an adhesive. The outer peripheral waterproof member 212 may be in a pipe shape and may be wrapped by the outer peripheral forming member 211 in a split state. The adhesive 213 may bond the inner surface of the outer peripheral forming member 211 to the outer surface of the outer peripheral waterproof member 212. The outer peripheral fixing portion 214 may fix the combination of the outer peripheral forming member 211 and the outer peripheral waterproof member 212 bonded to each other to the bottom surface forming member 121.
[0075] The perimeter of the outer surface forming part 211 can be cut to have an inner diameter corresponding to the outer diameter of the outer surface waterproof part 212. A PVC hose that is harder than PET can be used as the outer surface waterproof part 212, and silicone or the like can be used as the outer surface fixing part 214 to improve the sealing force between the outer surface waterproof part 212 and the bottom surface forming part 121.
[0076] Below, refer to Figures 6 to 9 , a method for manufacturing the log bark flower pot 200 according to the second embodiment of the present invention is described.
[0077] Fig. 9 It is schematically shown Figure 6 Flow chart of the manufacturing method of the log outer skin flower pot.
[0078] like Fig. 9 As shown, except for the process of forming the periphery and the bottom surface (step S250), the manufacturing method of the log bark flower pot 200 of the second embodiment of the present invention is the same as the manufacturing method mentioned in the first embodiment of the present invention mentioned above, so it will be mainly described below.
[0079] like Fig. 9 As shown, first, a tubular outer waterproof member 212 is prepared (step S251). Next, the dried outer skin is cut in a manner suitable for the outer diameter of the outer waterproof member 212 (see Figure 2 The perimeter of the outer skin L12 is measured, and the cut outer skin L12 is manufactured into the outer peripheral forming part 211 (step S252). Then, the cut outer peripheral forming part 211 is used to wrap and bond the outer peripheral waterproof part 212 (step S253). Finally, the combination of the outer peripheral forming part 211 and the outer peripheral waterproof part 212 bonded to each other with the adhesive 213 is fixed to the bottom surface forming part 121 with the outer peripheral fixing part 214 (step S254).
[0080] In the process of fixing with the peripheral fixing part 214 (step S254), silicone or the like can be used as the peripheral fixing part 214, in order to fix the combination of the peripheral forming part 211 and the peripheral waterproof part 21 that are bonded to each other on the bottom surface forming part 121 to make it sealed. The bottom surface forming part 121 can be plate-shaped and can be made of a plastic waterproof material, and PET (polyethylene terephthalate) material can be used as the plastic.
[0081] At the same time, in the process of fixing with the peripheral fixing portion 214 as described above ( Fig. 9 After step S254 is completed, the process of forming the periphery and the bottom surface ( Fig. 9 The step S250 may further include a process of filling the bottom surface filler 122 on the bottom surface forming member 121 ( Fig. 9Step S255). The bottom filler 122 may be filled to a thickness of 15 mm to 20 mm.
[0082] Below, refer to Fig.10 , the log bark flower pot 300 according to the third embodiment of the present invention is described.
[0083] Fig.10 It is a cross-sectional view schematically showing a log-bark flowerpot according to a third embodiment of the present invention.
[0084] like Fig.10 As shown, except for the outer peripheral forming portion 310, the log bark flower pot 300 of the third embodiment of the present invention is the same as the first embodiment of the present invention described above, so it will be mainly described below.
[0085] like Fig.10 As shown, the outer peripheral forming part 310 may include: an outer peripheral forming member 311, an outer peripheral fixing part 312 and an outer peripheral waterproofing agent 313. The outer peripheral forming member 311 may be made of the outer skin L12, and the longitudinal cut portion of the outer skin L12 (refer to Figure 2 The outer peripheral fixing part 312 can fix the outer peripheral forming part 311 on the bottom surface forming part 121. The outer peripheral waterproofing agent 313 can be made of a waterproof material and can be coated on the inner surface of the outer peripheral forming part 311.
[0086] Silicone or the like may be used as the peripheral fixing portion 312 to improve the sealing force between the peripheral forming member 311 and the bottom surface forming member 121. The peripheral waterproofing agent 313 may be applied more than once to the inner surface of the peripheral forming member 311. Transparent epoxy resin may be used as the peripheral waterproofing agent 313.
[0087] Below, refer to Fig.10 and Fig.11 , a method for manufacturing the log bark flower pot 300 according to the third embodiment of the present invention is described.
[0088] Fig.11 It is schematically shown Fig.10 Flow chart of the manufacturing method of the log outer skin flower pot.
[0089] like Fig.11 As shown, except for the process of forming the periphery and the bottom surface (step S350), the manufacturing method of the log bark flower pot 300 of the third embodiment of the present invention can be the same as the manufacturing method mentioned in the first embodiment of the present invention mentioned above, so the following description will mainly focus on this.
[0090] like Fig.11 As shown, first, the cut portion of the dried outer skin L12 can be bonded (see Figure 2The outer periphery forming part 311 is completed by the outer periphery fixing part 312 (step S351). Next, the outer periphery forming part 311 is fixed to the bottom surface forming part 121 by the outer periphery fixing part 312 (step S352). Finally, in order to prevent water from penetrating into the inner surface of the outer periphery forming part 311, an outer periphery waterproofing agent 313 made of a waterproof material can be applied to the inner surface of the outer periphery forming part 311 (step S353).
[0091] The bottom surface forming member 121 may be plate-shaped and may be made of waterproof materials such as plastic, and PET (polyethylene terephthalate) material may be used as the plastic. Silicone or the like may be used as the peripheral fixing portion 312 to improve the sealing force between the peripheral forming member 311 and the bottom surface forming member 121. The peripheral waterproofing agent 313 may be applied 2 to 3 times.
[0092] At the same time, in the process of coating with the peripheral waterproofing agent 313 as described above ( Fig.11 After the step S353 is completed, the process of forming the periphery and the bottom surface ( Fig.11 The step S350 may further include a process of filling the bottom surface filler 122 on the bottom surface forming member 121 ( Fig.11 Step S354). The bottom filler 122 may be filled to a thickness of 15 mm to 20 mm.
[0093] The preferred embodiments of the present invention are described in detail above, but the scope of the present invention is not limited thereto, and various modifications and improvements made by those skilled in the art using the basic concepts of the present invention defined in the claims also fall within the scope of the present invention.
[0094] Industrial Applicability
[0095] The invention relates to a flower pot and thus has industrial applicability.
Claims
1. A log skin flower pot, in, include: The outer bark, peeled from the wood of the log and having longitudinal cuts; a peripheral forming portion that forms a peripheral portion so as to include the outer skin and has a shape that penetrates vertically; and The bottom surface forming portion closes the lower opening of the outer peripheral forming portion and forms a bottom.
2. The log outer skin flower pot according to claim 1, wherein: The log skin flower pot has a waterproof structure, which blocks water from penetrating into the peripheral forming part.
3. A method for manufacturing the log skin flower pot according to claim 1, in, include: A cutting step, cutting the log into a set length; A pretreatment step of pretreating the outer bark of the cut logs so that the outer bark can be smoothly peeled off from the wood part; a separation step of separating the bark from the wood by longitudinally cutting the pretreated log; a drying step of drying the separated husk; and The outer periphery and bottom forming step forms an outer periphery and a bottom surface using an outer periphery forming portion including the dried outer skin and a bottom surface forming portion including a bottom surface forming member.
Citation Information
Patent Citations
Method for girdling in Broussonetia papyrifera (L.) Vent.
CN101733803A
Novel environment-friendly flowerpot
CN204191236U
Wooden container, its manufacture and use
JP1998291206A
ornamental flowerpot
JP3063760U
Veneer production
US4108226A