Crystal growth multi-layer composite crucible convenient for quartz crucible separation and capable of preventing leakage

By designing a multi-layer composite crucible structure, using a multi-segment or multi-petal spliced ​​sandwich crucible to match the quartz crucible, combined with a spliced ​​or integral bottom crucible, the difficulty in separation and leakage of the quartz crucible is solved, and rapid separation and safety are achieved. High temperature melt processing.

CN221918328UActive Publication Date: 2024-10-29SICHUAN YINGTAN TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420366208.4
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-02-27
Publication Date
2024-10-29
Estimated Expiration
2034-02-27

AI Technical Summary

Technical Problem

In the existing technology, it is difficult to separate the quartz crucible from the open crucible or the integral crucible, resulting in damage to the crucible and leakage of high-temperature melt, which increases production costs and safety risks.

Method used

Design a multi-layer composite crucible structure, including a quartz crucible, a sandwich crucible and a bottom crucible. The sandwich crucible adopts a multi-segment or multi-petal splicing structure to match the quartz crucible. The bottom crucible has a spliced ​​or overall structure to form a multi-layer composite structure to achieve quick separation and prevent leakage.

Benefits of technology

It achieves rapid separation of the quartz crucible, reduces the service life cost of the crucible, eliminates leakage of high-temperature melt, and improves production safety.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221918328U_ABST
    Figure CN221918328U_ABST
Patent Text Reader

Abstract

The utility model discloses a multilayer composite crucible for crystal growth, which is convenient for quartz crucible separation and prevents leakage. The multilayer composite crucible at least comprises but not limited to a quartz crucible, an interlayer crucible and a bottom layer crucible, the interlayer crucible is arranged between the quartz crucible and the bottom-layer crucible, and the interlayer crucible at least comprises two sections or two sections of spliced structures; according to the scheme, the interlayer crucible is arranged to be of a multi-section structure, compared with an open crucible manufactured in the prior art, the interlayer crucible can be rapidly separated from a quartz crucible on the upper layer of the interlayer crucible, the separation time is shortened, meanwhile, the quartz crucible does not need to be crushed or cut into a plurality of fragments by adopting an alloy hammer or a mechanical cutting mode, and the production efficiency is improved. The service life of the open crucible or the whole crucible is prolonged, and the single-time use cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the field of growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride or solar photovoltaic single crystals, and in particular to a multi-layer composite crucible for crystal growth which is convenient for separating quartz crucibles and preventing leakage. Background Art

[0002] Existing semiconductor crystal growth technologies such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride, and solar photovoltaic crystal growth technologies require the raw materials used for semiconductor crystal growth such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride, and solar photovoltaic crystal growth to be placed in a thermal field (such as Figure 1 ) is melted under high temperature conditions, and in order to hold the high temperature melt of raw materials used for the growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride and the growth of solar photovoltaic crystals, a quartz crucible (1) made of high-purity quartz and an open crucible (2) made of high-purity graphite materials, solid insulation felt materials, carbon fiber composite materials, silicon carbide materials, silicon carbide composite materials, silicon nitride materials and the like are used (such as Figure 2 ), a quartz crucible (1) made of high-purity quartz and an integral crucible (3) made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material, etc. can also be used (such as Figure 3 ).

[0003] During the crystal growth process, the outer surface of the quartz crucible (1) is in direct contact with the inner surface of the open crucible (2) (e.g. Figure 2 ), or directly contacting the inner surface of the integral crucible (3) (e.g. Figure 3 ), the current process mainly uses a quartz crucible (1) and an open crucible (2) combination (such as Figure 2 ).

[0004] After the raw materials used for the growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride and the growth of solar photovoltaic crystals are melted at high temperature and during the crystal growth process, the quartz crucible (1) softens at 1200°C-1800°C. After the softening, the quartz crucible (1) is deformed by the pressure of the high-temperature melt of the semiconductor raw materials, and argon, nitrogen and other gases in the gap between the outer surface of the quartz crucible (1) and the open crucible (2), or the inner surface of the integral crucible (3) are discharged. The quartz crucible (1) is closely matched with the open crucible (2) or the integral crucible (3), thereby enhancing the friction force between the outer surface of the quartz crucible (1) and the open crucible (2), or the inner surface of the integral crucible (3);

[0005] After the semiconductor crystal growth and solar photovoltaic crystal growth cycle process is completed, in order to reduce costs, it is necessary to separate the quartz crucible (1) from the open crucible (2) and the integral crucible (3), and to recycle the open crucible (2) or the integral crucible (3) for multiple reuse. Due to the deformation of the quartz crucible (1) and the friction between the outer surface and the open crucible (2) or the inner surface of the integral crucible (3), the separation of the quartz crucible (1) from the open crucible (2) or the integral crucible (3) is hindered. In the actual production process under the current process conditions, the quartz crucible (1) is separated by an alloy hammer or mechanical cutting method. The quartz crucible (1) is broken or cut into a plurality of pieces, thereby realizing the separation of the quartz crucible (1) from the open crucible (2) or from the integral crucible (3). In the process of breaking or cutting the quartz crucible (1) into a plurality of pieces by an alloy hammer or mechanical cutting, the impact force of the alloy hammer breaking the quartz crucible (1) destroys the graphite microstructure of the open crucible (2) or the integral crucible (3) or breaks the carbon fiber filaments, causing damage to the open crucible (2) or the integral crucible (3) and metal contamination, thereby reducing the service life of the open crucible (2) or the integral crucible (3) and increasing the use cost;

[0006] In order to reduce the manufacturing difficulty and cost of the open crucible (2) and facilitate separation of the quartz crucible (1), an opening structure (21) is reserved when designing the open crucible (2). The opening structure (21) is assembled with the crucible bottom (22). During the growth of semiconductor crystals and solar photovoltaic crystals, the opening structure (2-1) easily causes the quartz crucible (1) to deform and break, or the quartz crucible (1) to break due to reasons such as semiconductor crystal growth and solar photovoltaic crystal falling, or the quartz crucible (1) to break due to other reasons, causing the semiconductor raw material high-temperature melt to leak. The semiconductor raw material high-temperature melt leaking from the quartz crucible (1) continues to leak along the assembly gap between the opening structure (21) and the crucible bottom (22), causing a major production accident. Utility Model Content

[0007] The purpose of the utility model is to provide a multi-layer composite crucible for crystal growth that is convenient for separating quartz crucibles and prevents leakage, in view of the above-mentioned shortcomings, and solves the problem that the quartz crucible (1), the open crucible (2) or the integral crucible (3) in the prior art is not easy to separate, and at the same time solves the problem that the open crucible (2) or the integral crucible (3) is easily damaged during the separation process of the quartz crucible (1), the open crucible (2) or the integral crucible (3).

[0008] The utility model is realized by the following scheme:

[0009] A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, at least including but not limited to a quartz crucible, an interlayer crucible and a bottom crucible; the interlayer crucible is arranged between the quartz crucible and the bottom crucible, and the interlayer crucible comprises at least a 2-section or 2-petal splicing structure.

[0010] Based on the above structure of a crystal growth multilayer composite crucible that facilitates separation of the quartz crucible and prevents leakage, the splicing structure is spliced ​​along the warp or weft direction of the quartz crucible to form a structure that matches the quartz crucible.

[0011] Based on the structure of the multi-layer composite crucible for crystal growth which facilitates separation of quartz crucibles and prevents leakage, the bottom crucible is a splicing structure, an integral structure or a supporting structure with an opening structure.

[0012] Based on the above structure of the multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, when the bottom crucible is a spliced ​​structure, the bottom crucible includes at least two spliced ​​structures.

[0013] Based on the above-mentioned structure of a multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, the bottom crucible may specifically include a straight support member, a bottom support member and a transition connection member; the transition connection member is arranged between a vertical support member and a bottom support member, the vertical support member is arranged on the upper part of the transition connection member, and the end of the bottom support member is connected to the transition connection member; the vertical support member, the bottom support member and the transition connection member are spliced ​​to form an open cavity that can accommodate a sandwich crucible.

[0014] Based on the above structure of a multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, when the bottom crucible is an integral structure, the bottom crucible is an integral open structure that matches the shape of the sandwich crucible, and the bottom support is a full-surface structure with no opening structure thereon.

[0015] Based on the above structure of a crystal growth multilayer composite crucible that facilitates separation of quartz crucibles and prevents leakage, the sandwich crucible is prepared by combining one or more materials selected from high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

[0016] Based on the above structure of a multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, the bottom crucible is prepared by a combination of one or more materials selected from high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

[0017] Based on the structure of the multilayer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, the thickness of the sandwich crucible is 1 to 30 mm; after splicing, there is no opening structure at the bottom, and the overall structure of the sandwich crucible is a hemispherical structure.

[0018] Based on the structure of the multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, the thickness of the bottom crucible is 5 to 50 mm, and the bottom crucible after assembly is a hemispherical structure.

[0019] In summary, due to the adoption of the above technical solution, the beneficial effects of the utility model are:

[0020] 1. In the present solution, the sandwich crucible is arranged as a multi-stage or multi-petal splicing structure. Compared with the open crucible made in the prior art, it can be quickly separated from the quartz crucible on the upper layer, reducing the separation time. At the same time, there is no need to use an alloy hammer or mechanical cutting method to break or cut the quartz crucible made of high-purity quartz into several pieces, thereby increasing the service life of the open crucible (3) made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and the like, or the integral crucible (3) made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and the like, and reducing the cost per use.

[0021] 2. In this scheme, a quartz crucible is placed in a sandwich crucible spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in a bottom crucible with an opening structure to form a first multi-layer composite structure crucible; a quartz crucible is placed in a sandwich crucible spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in the bottom crucible of the overall structure to form a second multi-layer composite structure crucible; a quartz crucible is placed in a sandwich crucible spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in the bottom crucible of the spliced ​​structure to form a third multi-layer composite structure crucible; each multi-layer composite structure crucible can realize rapid separation of the quartz crucible and prevent or eliminate leakage. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 Thermal fields used for semiconductor crystal growth and solar photovoltaic crystal growth;

[0023] Figure 2-3 It is a schematic diagram of the prior art;

[0024] Figure 4 This is a schematic diagram of the first multi-layer composite structure crucible;

[0025] Figure 5 This is a schematic diagram of a second type of multi-layer composite structure crucible;

[0026] Figure 6 This is a schematic diagram of the third type of multi-layer composite structure crucible;

[0027] Description of the drawings: 1. Quartz crucible; 2. Open crucible; 3. Integral crucible; 4. Interlayer crucible; 5. Bottom crucible; 21. Open structure; 22. Crucible bottom; 51. Vertical support member; 52. Bottom support member; 53. Transition connector. DETAILED DESCRIPTION

[0028] All features disclosed in this specification, or steps in all methods or processes disclosed, except mutually exclusive features and / or steps, can be combined in any manner.

[0029] Any feature disclosed in this specification (including any additional claims and abstract), unless otherwise stated, may be replaced by other equivalent or alternative features having similar purposes. That is, unless otherwise stated, each feature is only an example of a series of equivalent or similar features.

[0030] In the description of the present invention, it should be understood that the terms "up", "down", "left", "right", etc., indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0031] In addition, the terms "first", "second", etc. are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Thus, a feature defined as "first", "second", etc. may explicitly or implicitly include one or more of the features.

[0032] Example 1

[0033] like Figure 4 and 6 As shown, the utility model provides a technical solution:

[0034] A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, which at least includes but is not limited to a quartz crucible 1, an interlayer crucible 4 and a bottom crucible 5; the interlayer crucible 4 is arranged between the quartz crucible 1 and the bottom crucible 5, and the interlayer crucible 4 includes at least 2 sections or 2 petals of spliced ​​structure.

[0035] Based on the above structure, in the present scheme, the sandwich crucible 4 is set as a multi-stage or multi-petal splicing structure. Compared with the open crucible 2 made in the prior art, it can be quickly separated from the quartz crucible 1 on the upper layer, reducing the separation time. At the same time, there is no need to use an alloy hammer or mechanical cutting method to break or cut the quartz crucible 1 made of high-purity quartz into several fragments, thereby improving the service life of the open crucible 2 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and the like, or the integral crucible 3 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and the like, and reducing the cost of single use.

[0036] As an example, the spliced ​​structure is spliced ​​along the longitude or latitude direction of the quartz crucible 1 to form an opening structure 21 matching the quartz crucible 1 .

[0037] Based on the above structure, the form of the splicing structure can include any structure, as long as it can be spliced ​​into a structure matching the quartz crucible 1 through multiple sections or multiple petals, which is convenient for placing the quartz crucible 1. At the same time, the quartz crucible 1 is placed in the sandwich crucible 4 under the action of its own gravity.

[0038] As an example, the bottom crucible 5 is a spliced ​​structure, an integral structure or a supporting structure with an opening structure 21 .

[0039] When the bottom crucible 5 is formed by splicing multiple sections of splicing structures, the bottom crucible 5 includes at least two sections of splicing structures, and the bottom crucible 5 may specifically include a vertical support member 51, a bottom support member 52 and a transition connection member 53; the transition connection member 53 is arranged between the vertical support member 51 and the bottom support member, the vertical support member 51 is arranged on the upper part of the transition connection member 53, and the end of the bottom support member is connected to the transition connection member 53; the vertical support member 51, the bottom support member 52 and the transition connection member 53 are spliced ​​to form an open cavity capable of accommodating the sandwich crucible 4;

[0040] When the bottom crucible 5 is an integral structure, the bottom crucible 5 is an integral opening structure 21 matching the shape of the sandwich crucible 4, and the bottom support member 52 is a full-surface structure without the opening structure 21 thereon.

[0041] When the bottom crucible 5 is a support structure with an opening structure 21 , it is the same as the prior art and will not be described in detail herein.

[0042] Based on the above structure, by setting the bottom crucible 5 as a multi-section splicing structure, on the one hand, the sandwich crucible 4 and the quartz crucible 1 inside it can be supported, and on the other hand, the splicing structure can also be quickly disassembled, and there is no opening structure 21 in the bottom crucible 5, which can prevent major production safety accidents caused by leakage of high-temperature melts of semiconductor raw materials such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, and gallium nitride.

[0043] As an example, the sandwich crucible 4 is made of a combination of one or more materials selected from the group consisting of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

[0044] The bottom crucible 5 is made of one or more materials selected from the group consisting of high-purity graphite material, solid thermal insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

[0045] Through this solution, the quartz crucible 1 can be placed in a sandwich crucible 4 spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in the bottom crucible 5 with the opening structure 21 to form a first multi-layer composite structure crucible; the quartz crucible 1 is placed in a sandwich crucible 4 spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in the bottom crucible 5 of the overall structure to form a second multi-layer composite structure crucible; the quartz crucible 1 is placed in a sandwich crucible 4 spliced ​​with multiple sections or multiple petals, and then the overall structure is placed in the bottom crucible 5 of the spliced ​​structure to form a third multi-layer composite structure crucible; each multi-layer composite structure crucible can realize the rapid separation of the quartz crucible 1 and prevent or eliminate leakage.

[0046] With the advancement of existing semiconductor crystal growth technologies such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride, and solar photovoltaic crystal growth technologies, the quartz crucible 1 made of high-purity quartz and the open crucible 2 made of high-purity graphite materials, solid insulation felt materials, carbon fiber composite materials, silicon carbide materials, silicon carbide composite materials, silicon nitride materials, etc., or the overall crucible 3 made of high-purity graphite materials, solid insulation felt materials, carbon fiber composite materials, silicon carbide materials, silicon carbide composite materials, silicon nitride materials, etc. are getting bigger and bigger in size, which can hold the growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride, and solar photovoltaic crystals. The amount of raw materials or high-temperature melt used reaches 600kg-1500kg. If the raw materials or high-temperature melts used in the growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride and solar photovoltaic crystals leak rapidly and in large quantities, it will lead to very serious production safety accidents, ranging from economic losses to casualties. Therefore, the growth technology of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride and solar photovoltaic crystal growth processes pay more and more attention to the rapid and large-scale leakage of raw materials or high-temperature melts used in the growth of semiconductor crystals such as silicon, germanium, gallium arsenide, indium phosphide, silicon carbide, gallium nitride and solar photovoltaic crystals.

[0047] As an example, the thickness of the sandwich crucible 4 is 1-30 mm; after the splicing is completed, there is no opening structure 21 at the bottom, and the overall structure of the sandwich crucible 4 is a hemispherical structure.

[0048] The bottom crucible 5 has a thickness of 5 to 50 mm, and after assembly, the bottom crucible 5 has a hemispherical structure.

[0049] In this solution, a multi-petal (≥2 petals) or multi-segment (≥2 segments) sandwich crucible 4 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon nitride material and other materials in a multi-layer composite structure crucible structure can be quickly separated from a quartz crucible 1 made of high-purity quartz; or a quartz crucible 1 made of high-purity quartz and a bottom crucible 5 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and other materials can be quickly separated.

[0050] At the same time, this scheme introduces the structure of the prior art:

[0051] The quartz crucible 1 made of high-purity quartz has no significant difference from the existing process, and all existing processes use this structural product, such as the structure shown in the figures:

[0052] 1. Made of high-purity silicon dioxide quartz sand melted at high temperature;

[0053] 2Thickness is between 5mm and 25mm;

[0054] 3. Thickness range ≤5mm;

[0055] 4 The overall structure of the quartz crucible 1 is hemispherical;

[0056] Open crucible 2 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and other materials. All existing processes use this structural product:

[0057] 1. Made of high-purity graphite materials, solid insulation felt materials, carbon fiber composite materials, silicon carbide materials, silicon carbide composite materials, silicon nitride materials, etc.

[0058] 2Thickness is between 5mm and 50mm;

[0059] 3 The bottom has an opening structure 21, and the opening structure 21 is partially assembled with the bottom 22 of the crucible;

[0060] 4 After assembly, the overall structure presents hemispherical characteristics;

[0061] The integral crucible 3 made of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, silicon carbide composite material, silicon nitride material and the like, some of the existing processes are using this structural product:

[0062] 1. Made of high-purity graphite materials, solid insulation felt materials, carbon fiber composite materials, silicon carbide materials, silicon carbide composite materials, silicon nitride materials, etc.

[0063] 2Thickness is between 5mm and 50mm;

[0064] 3 bottom opening structure 21;

[0065] 4 The overall structure is hemispherical.

[0066] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage, characterized in that: At least including but not limited to a quartz crucible, an interlayer crucible and a bottom crucible; the interlayer crucible is arranged between the quartz crucible and the bottom crucible, and the interlayer crucible comprises at least 2 sections or 2 petals spliced ​​structure.

2. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 1, characterized in that: The spliced ​​structure is spliced ​​along the warp or weft direction of the quartz crucible to form a structure matching the quartz crucible.

3. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 2, characterized in that: The bottom crucible is a spliced ​​structure, an integral structure or a supporting structure with an opening structure.

4. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 3, characterized in that: When the bottom crucible is a spliced ​​structure, the bottom crucible includes at least two spliced ​​structures.

5. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 4, characterized in that: The bottom crucible specifically includes a straight support member, a bottom support member and a transition connection member; the transition connection member is arranged between the vertical support member and the bottom support member, the vertical support member is arranged on the upper part of the transition connection member, and the end of the bottom support member is connected to the transition connection member; the vertical support member, the bottom support member and the transition connection member are spliced ​​to form an open cavity capable of accommodating the sandwich crucible.

6. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 3, characterized in that: When the bottom crucible is an integral structure, the bottom crucible is an integral open structure matching the shape of the sandwich crucible, and the bottom of the bottom crucible is a whole surface structure without an opening structure thereon.

7. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in any one of claims 1 to 6, characterized in that: The sandwich crucible is prepared by combining one or more materials selected from the group consisting of high-purity graphite material, solid insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

8. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in any one of claims 1 to 6, characterized in that: The bottom crucible is prepared by combining one or more materials selected from the group consisting of high-purity graphite material, solid thermal insulation felt material, carbon fiber composite material, silicon carbide material, and silicon nitride material.

9. A multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in any one of claims 1 to 6, characterized in that: The thickness of the sandwich crucible is 1 to 30 mm; after the splicing is completed, there is no opening structure at the bottom, and the overall structure of the sandwich crucible is a hemispherical structure.

10. The multi-layer composite crucible for crystal growth that facilitates separation of quartz crucibles and prevents leakage as claimed in claim 6, characterized in that: The bottom crucible has a thickness of 5 to 50 mm, and the bottom crucible after assembly is in a hemispherical structure.