Amorphous silicon drying and pressure stabilizing system for polycrystalline silicon tail gas recovery

By using high-efficiency silicon powder filters and backblowing packs in the polycrystalline silicon exhaust gas recovery system, the amorphous silicon is dried inside the system and sent to the regeneration condensation system, which solves the unstable exhaust gas recovery and poor drying effect of amorphous silicon. The problem has achieved more efficient energy utilization and pollution reduction.

CN221950787UActive Publication Date: 2024-11-05NINGXIA CRYSTAL NEW ENERGY MATERIALS CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420226718.1
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-01-30
Publication Date
2024-11-05
Estimated Expiration
2034-01-30

AI Technical Summary

Technical Problem

In the existing polycrystalline silicon exhaust gas recovery system, the exhaust gas recovery is unstable due to the low intake pressure of the regenerating compressor, and the drying effect of amorphous silicon is poor, resulting in high energy consumption and pollution problems in the equipment.

Method used

Design a polycrystalline silicon exhaust gas recovery amorphous silicon drying and pressure stabilization system, using high-efficiency silicon powder filter, backblowing pack, venting filter and silicon powder receiving tank, and make amorphous silicon in the system through hydrogen backblowing and nitrogen replacement. Dry the internally and the dried silicon powder is sent into the regeneration condensation system to balance the pressure of the adsorption column regeneration system to avoid stopping the regeneration compressor.

Benefits of technology

It effectively reduces the pollution of solid waste treatment to the environment, improves the operation cycle of the regeneration device, reduces energy consumption, enhances the controllability of the process, and avoids compressor stoppage caused by the automatic control logic of the adsorption column.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221950787U_ABST
    Figure CN221950787U_ABST
Patent Text Reader

Abstract

The utility model discloses an amorphous silicon drying and pressure stabilizing system for polycrystalline silicon tail gas recovery, which is characterized in that a blowback gas bag releases high-pressure gas by using hydrogen, so that amorphous silicon on the surface of a metal sintered filter element falls off, a silicon powder receiving tank collects the amorphous silicon and heats and dries the amorphous silicon by using reduced tail gas and high-temperature gas at an outlet of a compressor; the emptying filter is used for collecting amorphous silicon mixed in a gas phase in the silicon powder receiving tank during nitrogen displacement and pressure relief, and the amorphous silicon collected by the nitrogen pressurizing emptying filter is selectively conveyed to the silicon powder receiving tank for drying or conveyed to the silicon powder collecting tank for collecting according to the sold drying condition of the amorphous silicon. Amorphous silicon is filtered by a high-efficiency silicon powder filter, dried by a silicon powder receiving tank and subjected to gas-phase heat exchange by the silicon powder receiving tank and then is conveyed to a regeneration condensation system, so that silicon powder is dried in the system, the pollution of solid waste to the environment in the treatment process can be effectively reduced, the jump stop of a regeneration gas compressor indirectly caused by the restriction of self-control logic of an adsorption column is avoided, and the service life of the regeneration gas compressor is prolonged. The regeneration device operation period is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of polysilicon production, and in particular to a polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system. Background Art

[0002] In the reduction process of polysilicon, the trichlorosilane (TCS) liquid from distillation is vaporized and mixed with hydrogen. After the mixed gas is heated by a heat exchanger, it is sent to the reduction furnace to participate in the reduction reaction. On the surface of the hot silicon core at 1080°C, trichlorosilane decomposes to form crystalline silicon, which is deposited on the surface of the hot silicon core, forming polycrystalline silicon rods over time. Due to the temperature fluctuation on the surface of the reduced silicon core, trichlorosilane decomposes to form dichlorodihydrosilane (DCS). The amorphous silicon formed after heating will be sent to the exhaust gas recovery system with the reduced exhaust gas flow due to the fast deposition rate. It will be efficiently filtered and removed in the exhaust gas recovery system. In order to avoid the liquefaction of the silane gas inside the amorphous silicon, high-temperature gas phase filtration (temperature 120°C-170°C) is carried out, which can improve the cleanliness of the exhaust gas recovery system and the operation cycle of the exhaust gas recovery condensate pump.

[0003] In the prior art, when the pressure of the adsorption column is relieved by the modified Siemens process package, the time is set to 140 minutes, and the cascade control logic is used to relieve the pressure in the adsorption column from 1.3MPa to 0.05MPa within 40 minutes. Due to the low intake pressure of the regeneration gas compressor and the large periodic loss of the gas source in the compressor return pipe, the intake pressure is underreported, causing the exhaust gas recovery regeneration gas compressor to trip due to the intake pressure chain, affecting the stable operation of the exhaust gas recovery compression device. At the same time, the amorphous silicon filtration device uses 2 kg of steam (saturated steam is about 120°C) or electric auxiliary heating for heating. The use of steam has poor controllability due to fluctuations in the operating process in winter and high energy consumption; the use of electric auxiliary heating has high energy consumption, and because auxiliary heating is performed on the outside of the equipment, it will also cause the problem of poor drying effect of amorphous silicon. Utility Model Content

[0004] The purpose of this application is to provide a polysilicon tail gas recovery amorphous silicon drying and pressure stabilization system in order to overcome the existing technical defects. The reduced tail gas is dried through a high-efficiency silicon powder filter and a silicon powder receiving tank and then connected to the regeneration condensation system, so as to balance the pressure of the adsorption column regeneration system, avoid the process fluctuations caused by the suction pressure stop of the regeneration gas compressor, and allow the silicon powder to be dried inside the system. The system has strong controllability and can effectively reduce the pollution of the environment to the solid waste during the treatment process.

[0005] The purpose of this application is achieved through the following technical solutions:

[0006] In the first aspect, the present application proposes a polysilicon tail gas recovery amorphous silicon drying and stabilizing system, characterized in that it is used for tail gas recovery, and the system includes a high-efficiency silicon powder filter, a back-blowing air bag, a venting filter, a silicon powder receiving tank and a silicon powder collecting tank;

[0007] The back-blowing air bag is connected to the high-efficiency silicon powder filter and is used to release the high-pressure gas inside the back-blowing air bag with hydrogen, increase the backwashing pressure of the metal sintered filter element, so that the amorphous silicon on the surface of the metal sintered filter element falls off and is sent to the silicon powder receiving tank through the pipeline;

[0008] The high-efficiency silicon powder filter is connected to the silicon powder receiving tank, and is used to filter and reduce the amorphous silicon in the tail gas through the metal sintered filter element, and send the filtered amorphous silicon to the silicon powder receiving tank;

[0009] The silicon powder receiving tank is connected to the silicon powder collecting tank and the venting filter respectively, and is used to collect the amorphous silicon filtered out by the high-efficiency silicon powder filter and the venting filter, and heat and dry the amorphous silicon;

[0010] The vent filter is used to filter and collect amorphous silicon mixed in the silane gas when the silicon powder receiving tank is depressurized by nitrogen replacement and amorphous silicon in the nitrogen when the high-efficiency silicon powder filter is replaced by a filter element;

[0011] The silicon powder collecting tank is used to collect the amorphous silicon heated and dried in the silicon powder receiving tank and the vent filter to collect the amorphous silicon mixed in the silane gas when the silicon powder receiving tank is depressurized by nitrogen replacement;

[0012] In a possible implementation, the silicon powder receiving tank, the adsorption column backblower condensation skid, the regeneration gas compressor suction tank, the regeneration gas compressor, the regeneration gas compressor post-air cooler, and the regeneration gas compressor exhaust tank are connected in sequence;

[0013] The silicon powder receiving tank receives the reduction tail gas sent from the outlet of the high-efficiency silicon powder filter, mixes the reduction tail gas with the high-temperature back-blowing hydrogen gas of the adsorption column and the depressurized hydrogen gas to obtain a mixed gas, and sends the mixed gas to the back-blowing gas condensation skid of the adsorption column for condensation;

[0014] The adsorption column backblower condensation skid discharges the uncondensed mixed gas through the regeneration gas compressor suction tank, the regeneration gas compressor, the regeneration gas compressor post-air cooler, and the regeneration gas compressor exhaust tank.

[0015] In one possible implementation, the silicon powder receiving tank is connected to the regeneration gas compressor suction tank through a pressure regulating valve. The regeneration gas compressor suction tank is provided with a pressure transmitter. When the pressure of the regeneration gas compressor suction tank is low, the pressure regulating valve sends gas into the regeneration gas compressor suction tank to balance the compressor suction pressure.

[0016] In a possible implementation, the back-blowing air bag acts on the high-efficiency silicon powder filter to perform pressure replacement through nitrogen when the filter element is replaced.

[0017] In a possible implementation, the silicon powder receiving tank is also connected to a regeneration condensing system to receive high-temperature exhaust gas from a hydrogen compressor, perform heat exchange in the silicon powder receiving tank, and send the exhaust gas to the regeneration condensing system.

[0018] In a possible implementation, the high-efficiency silicon powder filter includes multiple groups of metal sintered filter elements.

[0019] In a possible implementation manner, the silicon powder receiving tank is heated by an inner coil and / or an outer coil.

[0020] In a possible implementation, the vent filter is also used to send the volatilized chlorosilane gas into the exhaust gas system for recovery.

[0021] In a possible implementation, the high-efficiency silicon powder filter is also used to send the filtered reduction tail gas to a condensation system for tail gas condensation.

[0022] In a possible implementation, there is at least one valve at each connection in the system.

[0023] The above-mentioned main scheme of the present application and its further options can be freely combined to form multiple schemes, all of which are schemes that can be adopted and claimed for protection in the present application; and in the present application, (non-conflicting options) options and other options can also be freely combined. After understanding the scheme of the present application, those skilled in the art can understand that there are multiple combinations based on the prior art and common knowledge, all of which are technical schemes to be protected by the present application, and they are not exhaustively listed here.

[0024] The present application discloses a system for drying and stabilizing amorphous silicon from polysilicon tail gas. The back-blowing gas bag uses hydrogen to release high-pressure gas, causing the amorphous silicon on the surface of the metal sintering filter element to fall off. The silicon powder receiving tank collects amorphous silicon and uses the reducing tail gas and the high-temperature gas at the outlet of the compressor to heat and dry the amorphous silicon. The venting filter collects the amorphous silicon mixed in the gas phase in the silicon powder receiving tank when the silicon powder receiving tank is depressurized by nitrogen replacement. The amorphous silicon collected by the nitrogen pressurized venting filter is sent to the silicon powder receiving tank for drying or to the silicon powder collecting tank for collection according to the drying conditions of the amorphous silicon for sale. The amorphous silicon is filtered through a high-efficiency silicon powder filter, dried in the silicon powder receiving tank, and sent to the regeneration condensation system after gas-phase heat exchange in the silicon powder receiving tank, so that the silicon powder is dried inside the system, which can effectively reduce the pollution of the environment to the solid waste during the treatment process, avoid the tripping and stopping of the regeneration gas compressor indirectly caused by the restriction of the adsorption column automatic control logic, and improve the operation cycle of the regeneration device. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 A schematic structural diagram of a polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system proposed in an embodiment of the present application is shown.

[0026] Icons: 1-backblowing air bag; 2-high-efficiency silicon powder filter; 3-silicon powder receiving tank; 4-silicon powder collection tank; 5-venting filter; 6-adsorption column backblowing device condensation skid; 7-regeneration gas compressor suction tank; 8-regeneration gas compressor; 9-regeneration gas compressor after-air cooler; 10-regeneration gas compressor exhaust tank. DETAILED DESCRIPTION

[0027] The following describes the embodiments of the present application through specific examples, and those skilled in the art can easily understand other advantages and effects of the present application from the contents disclosed in this specification. The present application can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present application. It should be noted that the following embodiments and features in the embodiments can be combined with each other without conflict.

[0028] Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of this application.

[0029] In the prior art, when the pressure of the adsorption column is relieved by the modified Siemens process package, the time is set to 140 minutes, and the cascade control logic is used to relieve the pressure in the adsorption column from 1.3MPa to 0.05MPa within 40 minutes. Due to the low intake pressure of the regeneration gas compressor and the large periodic loss of the gas source in the compressor return pipe, the intake pressure is underreported, causing the exhaust gas recovery regeneration gas compressor to trip due to the intake pressure chain, affecting the stable operation of the exhaust gas recovery compression device. At the same time, the amorphous silicon filtration device uses 2 kg of steam (saturated steam is about 120°C) or electric auxiliary heating for heating. The use of steam has poor controllability due to fluctuations in the operating process in winter and high energy consumption; the use of electric auxiliary heating has high energy consumption, and because auxiliary heating is performed on the outside of the equipment, it will also cause the problem of poor drying effect of amorphous silicon.

[0030] Therefore, in order to solve the above-mentioned problems, the embodiment of the present application proposes a polysilicon tail gas recovery amorphous silicon drying and pressure stabilization system, which sends the gas in the amorphous silicon receiving tank into the regeneration gas condensation system. Since the high-temperature gas source at the reduction tail gas end and the exhaust outlet end of the hydrogen compressor is continuous and stable, it is possible to balance the cooling load of the regeneration system and the suction pressure of the regeneration gas compressor, and avoid the process fluctuation caused by the intermittent nature of the pressure relief gas from the adsorption column indirectly leading to the compressor tripping due to low intake pressure. It is described in detail below.

[0031] Please refer to Figure 1 , Figure 1The schematic diagram of the structure of a polysilicon tail gas recovery amorphous silicon drying and stabilizing system proposed in an embodiment of the present application is shown, the system is used for tail gas recovery, and includes a high-efficiency silicon powder filter 2, a back-blowing air bag 1, a venting filter 5, a silicon powder receiving tank 3 and a silicon powder collecting tank 4;

[0032] The back-blowing air bag 1 is connected to the high-efficiency silicon powder filter 2, and is used to use hydrogen to release the high-pressure gas inside the back-blowing air bag 1, increase the backwashing pressure of the metal sintered filter element, so that the amorphous silicon on the surface of the metal sintered filter element falls off and is sent to the silicon powder receiving tank 3 through the pipeline;

[0033] The high-efficiency silicon powder filter 2 is connected to the silicon powder receiving tank 3, and is used to filter and reduce the amorphous silicon in the tail gas through the metal sintered filter element, and send the filtered amorphous silicon to the silicon powder receiving tank 3;

[0034] The silicon powder receiving tank 3 is connected to the silicon powder collecting tank 4 and the venting filter 5 respectively, and is used to collect the amorphous silicon filtered out by the high-efficiency silicon powder filter 2 and the venting filter 5, and heat and dry the amorphous silicon;

[0035] The vent filter 5 is used to filter and collect the amorphous silicon mixed in the silane gas when the silicon powder receiving tank 3 is depressurized by nitrogen replacement and the amorphous silicon in the nitrogen when the high-efficiency silicon powder filter 2 is replaced by the filter element;

[0036] The silicon powder collecting tank 4 is used to collect the amorphous silicon heated and dried in the silicon powder receiving tank 3 and the venting filter 5 is used to collect the amorphous silicon mixed in the silane gas in the silicon powder receiving tank 3 when the nitrogen replacement pressure is released;

[0037] The back-blowing air bag 1 releases the high-pressure gas in the air bag when using high-pressure hydrogen (purging hydrogen), which can increase the back-flushing pressure of the metal sintered filter element in the high-efficiency silicon powder filter 2, causing the amorphous silicon filter cake enriched on the surface of the metal sintered filter element to fall off. At this time, the amorphous silicon is dried along the pipeline through the silicon powder receiving tank 3 and then sent to the silicon powder collecting tank 4 for collection.

[0038] In a possible implementation, the backflush air bag 1 is pressure-replaced by nitrogen when the filter element is replaced.

[0039] When the filter element needs to be replaced, use nitrogen to effectively replace the pressure.

[0040] The high-efficiency silicon powder filter 2 filters the amorphous silicon in the reduction tail gas through a high-efficiency metal sintered filter element, which can greatly reduce the solid dust in the reduction tail gas and condensate of the condensation system.

[0041] The silicon powder receiving tank 3 collects amorphous silicon filtered by the high-efficiency silicon powder filter 2 and the vent filter 5, and dries it by reducing the high-temperature gas and exhausting the hydrogen compressor.

[0042] The silicon powder collecting tank 4 receives the dried amorphous silicon from the silicon powder receiving tank 3 and the venting filter 5 filters the amorphous silicon mixed in the depressurized gas phase.

[0043] The vent filter 5 collects the silane gas vented in the silicon powder receiving tank 3, the amorphous silicon mixed in the gas phase, and the amorphous silicon mixed in the nitrogen when the filter element of the high-efficiency silicon powder filter 2 is replaced.

[0044] In a possible implementation, the silicon powder receiving tank 3, the adsorption column backblower condensation skid 6, the regeneration gas compressor suction tank 7, the regeneration gas compressor 8, the regeneration gas compressor post-air cooler 9, and the regeneration gas compressor exhaust tank 10 are connected in sequence;

[0045] The silicon powder receiving tank 3 receives the reduction tail gas sent from the high-efficiency silicon powder filter 2, mixes the reduction tail gas with the high-temperature back-blowing hydrogen gas of the adsorption column and the depressurized hydrogen gas to obtain a mixed gas, and sends the mixed gas to the adsorption column back-blowing device condensation skid 6 for condensation;

[0046] The adsorption column backblower condensation skid 6 discharges the uncondensed mixed gas through the regeneration gas compressor suction tank 7, the regeneration gas compressor 8, the regeneration gas compressor post-air cooler 9, and the regeneration gas compressor exhaust tank 10.

[0047] The silicon powder receiving tank 3 mixes the reduction tail gas or compressor hydrogen after heat exchange with the high-temperature back-blowing hydrogen (about 120°C) and depressurized hydrogen (about 20 degrees) of the adsorption column, and then enters the adsorption column backblowing device condensation skid 6. After the high-temperature gas is condensed by the condensation skid, the silane liquid is pumped to the downstream process through the delivery pump. The uncondensed gas enters the regeneration gas compressor suction tank 7, the regeneration gas compressor 8, the regeneration gas compressor post-air cooler 9, and the regeneration gas compressor exhaust tank 10 in turn, and the hydrogen is sent to the cold hydrogenation process for use.

[0048] In a possible implementation, the silicon powder receiving tank 3 is connected to the regeneration gas compressor suction tank 7 through a pressure regulating valve. The regeneration gas compressor suction tank 7 is provided with a pressure transmitter. When the pressure of the regeneration gas compressor suction tank 7 is low, the pressure regulating valve sends gas into the regeneration gas compressor suction tank 7 to balance the compressor suction pressure.

[0049] The regeneration gas compressor suction tank 7 is equipped with a pressure transmitter, and a pressure regulating valve is set on the outlet pipeline of the silicon powder receiving tank with a pressure interlock. When the pressure of the regeneration gas compressor suction tank 7 is low, the regulating valve will be activated to add gas to the regeneration gas compressor suction tank 7 to balance the compressor suction pressure.

[0050] In a possible implementation, the high-efficiency silicon powder filter 2 includes a plurality of groups of metal sintered filter elements, and the metal sintered filter elements may be high-precision metal sintered filter elements.

[0051] The inner coil and the outer coil are arranged inside the silicon powder receiving tank 3 so that the heat exchange area of ​​the equipment cylinder can be increased and the drying rate of the indeterminate silicon can be improved.

[0052] When collecting the silicon powder filtered by the high-efficiency silicon powder filter 2, at least one set of inner coil heat exchange sleeves or jackets are added to the silicon powder receiving tank 3. Since the existing reduction tail gas needs to avoid the large amount of silane gas enrichment inside the amorphous silicon, it needs to be filtered at high temperature. At this time, the temperature of the reduction tail gas is between 120°C and 170°C. Then, the filtered amorphous silicon is dried by using the heat of the reduction tail gas itself through at least one set of inner coil heat exchange sleeves or jackets. Due to the heat loss, the consumption of refrigerant energy of the regeneration gas condensation system can be reduced.

[0053] In a possible implementation, the silicon powder receiving tank 3 is also connected to the regeneration condensation system to receive the exhaust gas from the hydrogen compressor and cool it before sending it to the regeneration condensation system.

[0054] The exhaust end of the hydrogen recovery compressor is between 110℃-120℃, the reduction tail gas enters the low-pressure condensation system, and the exhaust end of the hydrogen recovery compressor enters the high-pressure condensation system. Part of the reduction tail gas or hydrogen compressor exhaust filtered by the high-efficiency silicon powder filter 2 is connected to the silicon powder receiving tank 3.

[0055] The dried amorphous silicon can be further processed according to its physical properties, and the gas after passing through the silicon powder receiving tank 3 is sent to the regeneration gas condensation system. Since the high-temperature gas source at the reduction tail gas end and the exhaust outlet of the hydrogen compressor is continuous and stable, it can balance the cooling load of the regeneration system and the suction pressure of the regeneration gas compressor, and avoid the process fluctuation caused by the regeneration gas compressor indirectly tripping due to low intake pressure due to the intermittent nature of the pressure relief gas from the adsorption column.

[0056] In a possible implementation, the vent filter 5 is also used to send the volatilized chlorosilane gas into the exhaust gas system for recovery.

[0057] The volatilized chlorosilane gas can be sent to the three-waste condensation system through the amorphous silicon vent filter 5 gas phase material to further recover the chlorosilane in the gas phase.

[0058] In a possible implementation manner, the high-efficiency silicon powder filter 2 is also used to send the filtered reduced tail gas to the condensation system for tail gas condensation.

[0059] In a possible implementation, there is at least one valve at each connection in the system.

[0060] The valve at the connection point can be selected according to actual conditions, such as disc valve, ball valve, etc.

[0061] Connecting part of the reduced tail gas to the regeneration system, connecting part of the compressor exhaust section to the regeneration system; canceling the input of electric auxiliary heating energy for the silicon powder collection tank 4 or the input of steam for the steam jacket can reduce the device investment and operation cost.

[0062] The present application performs drying inside amorphous silicon, has strong controllability, and can effectively reduce the pollution of the environment caused by solid waste during treatment. It can also avoid the tripping of the regeneration gas compressor indirectly caused by the restriction of the adsorption column automatic control logic, and improve the operation cycle of the regeneration device.

[0063] Compared with the prior art, the embodiments of the present application have the following beneficial effects:

[0064] The temperature difference between process materials is used for mutual heat exchange to achieve mutual utilization of energy, reduce energy consumption, optimize the process of tail gas recovery regeneration gas unit, balance the energy consumption load of the regeneration system, and avoid process fluctuations caused by the tripping of the regeneration gas compressor.

[0065] In summary, the polysilicon tail gas recovery amorphous silicon drying and stabilizing pressure system disclosed in the present application uses hydrogen to release high-pressure gas in the back-blowing gas bag 1, so that the amorphous silicon on the surface of the metal sintering filter element falls off and is collected in the silicon powder receiving tank 3 through the pipeline. The silicon powder receiving tank 3 collects the amorphous silicon filtered out by the high-efficiency silicon powder filter 2 and the venting filter 5, and uses the reducing tail gas and the high-temperature gas at the outlet of the compressor to heat and dry the amorphous silicon. The venting filter 5 collects the amorphous silicon mixed in the gas phase in the silicon powder receiving tank 3 when the nitrogen is replaced and depressurized, and the amorphous silicon collected by the venting filter 5 is pressurized by nitrogen, and is sent to the silicon powder receiving tank 3 for drying or sent to the silicon powder collecting tank 4 for collection according to the drying situation of the amorphous silicon for sale. The amorphous silicon is filtered by the high-efficiency silicon powder filter 2 and dried in the silicon powder receiving tank 3, and the silicon powder receiving tank 3 is sent to the regeneration condensation system after gas phase heat exchange, so that the silicon powder is dried inside the system, which can effectively reduce the pollution of the environment to the solid waste during the treatment process.

[0066] The above description is only a preferred embodiment of the present application and is not intended to limit the present application. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present application should be included in the protection scope of the present application.

Claims

1. A polysilicon tail gas recovery amorphous silicon drying and voltage stabilization system, characterized in that: Used for tail gas recovery, the system includes a high-efficiency silicon powder filter, a back-blowing air bag, a vent filter, a silicon powder receiving tank and a silicon powder collecting tank; The back-blowing air bag is connected to the high-efficiency silicon powder filter and is used to release the high-pressure gas inside the back-blowing air bag with hydrogen, increase the backwashing pressure of the metal sintered filter element, so that the amorphous silicon on the surface of the metal sintered filter element falls off and is sent to the silicon powder receiving tank through the pipeline; The high-efficiency silicon powder filter is connected to the silicon powder receiving tank, and is used to filter the amorphous silicon in the reduction tail gas through the metal sintered filter element, and send the filtered amorphous silicon to the silicon powder receiving tank; The silicon powder receiving tank is connected to the silicon powder collecting tank and the venting filter respectively, and is used to collect the amorphous silicon filtered out by the high-efficiency silicon powder filter and the venting filter, and heat and dry the amorphous silicon; The vent filter is used to filter and collect amorphous silicon mixed in the silane gas when the silicon powder receiving tank is depressurized by nitrogen replacement and amorphous silicon in the nitrogen when the high-efficiency silicon powder filter is replaced by a filter element; The silicon powder collecting tank is used to collect the amorphous silicon heated and dried in the silicon powder receiving tank and the venting filter to collect the amorphous silicon mixed in the silane gas when the silicon powder receiving tank is depressurized by nitrogen replacement.

2. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The silicon powder receiving tank, the adsorption column backblower condensation skid, the regeneration gas compressor suction tank, the regeneration gas compressor, the regeneration gas compressor post-air cooler, and the regeneration gas compressor exhaust tank are connected in sequence; The silicon powder receiving tank receives the reduction tail gas sent from the outlet of the high-efficiency silicon powder filter, mixes the reduction tail gas with the high-temperature back-blowing hydrogen gas of the adsorption column and the depressurized hydrogen gas to obtain a mixed gas, and sends the mixed gas to the back-blowing gas condensation skid of the adsorption column for condensation; The adsorption column backblower condensation skid discharges the uncondensed mixed gas through the regeneration gas compressor suction tank, the regeneration gas compressor, the regeneration gas compressor post-air cooler, and the regeneration gas compressor exhaust tank.

3. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 2, characterized in that: The silicon powder receiving tank is connected to the regeneration gas compressor suction tank through a pressure regulating valve. The regeneration gas compressor suction tank is equipped with a pressure transmitter. When the pressure of the regeneration gas compressor suction tank is low, the pressure regulating valve sends gas into the regeneration gas compressor suction tank to balance the compressor suction pressure.

4. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The back-blowing air bag acts on the high-efficiency silicon powder filter to perform pressure replacement through nitrogen when the filter element is replaced.

5. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The silicon powder receiving tank is also connected to the regeneration condensation system to receive the high-temperature exhaust gas from the hydrogen compressor, perform heat exchange in the silicon powder receiving tank, and send it to the regeneration condensation system.

6. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The high-efficiency silica powder filter includes multiple groups of metal sintered filter elements.

7. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The silicon powder receiving tank is heated by an inner coil and / or an outer coil.

8. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The vent filter is also used to send the volatilized chlorosilane gas into the exhaust gas system for recovery.

9. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: The high-efficiency silicon powder filter is also used to send the filtered reduction tail gas to the condensation system for tail gas condensation.

10. The polysilicon tail gas recovery and amorphous silicon drying and voltage stabilization system according to claim 1, characterized in that: There is at least one valve at each connection in the system.