Solder ball

By designing a hot ball structure with soldering layer and grooves, the problem of pre-coating flux during welding of existing hot balls is solved, and the hot balls are automatically wrapped during the welding process, preventing oxidation and reducing surface tension and improving welding Effect, simplify operation.

CN221952573UActive Publication Date: 2024-11-05DONGGUAN YONGCHENG SOLDER PROD CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202323670978.2
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2023-12-31
Publication Date
2024-11-05
Estimated Expiration
2033-12-31

AI Technical Summary

Technical Problem

The existing hot balls need to be pre-applied and heated when soldering, which is cumbersome and inconvenient to prevent tin oxidation.

Method used

A tin ball is designed, including an inner tin layer, an outer tin layer and a soldering layer. The soldering layer is a rosin layer. The outer tin layer has a hollow spherical shape and a plurality of circular grooves. The inner tin layer is spherical. The soldering is made by heating. The layer is wrapped with tin to prevent oxidation and reduce surface tension and avoid external flux coating.

Benefits of technology

During the welding process, the solder layer wraps the hot balls to prevent oxidation and reduce surface tension, improves the welding effect, and makes operation more convenient, without external flux coating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221952573U_ABST
    Figure CN221952573U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of solder balls, in particular to a solder ball, which comprises an inner tin layer and an outer tin layer, a soldering-aid layer is arranged between the inner tin layer and the outer tin layer, the inner tin layer is spherical, and the outer tin layer and the soldering-aid layer are hollow spherical. The welding device has the effect of facilitating welding.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of solder balls, in particular to a solder ball. Background Art

[0002] Tin is a chemical element with the chemical symbol Sn and atomic number 50. It is a metal element in the periodic table and exists in nature in the form of various ores. Tin has a low melting point, good ductility and toughness, and is relatively corrosion-resistant. These characteristics make tin widely used in various fields, including manufacturing, electronics, food packaging, iron plating, welding metals or making alloys. Common white tin is silvery white, has strong ductility, and is not easy to change in the air. At present, tin is made into tin balls on the market to facilitate the welding of contacts on components, but the current tin balls need to be coated with flux on the components in advance when welding, and the flux is heated and melted before placing the tin balls, which is more troublesome. Utility Model Content

[0003] In order to facilitate welding, the utility model provides a solder ball to solve the problems of the prior art. The utility model provides a solder ball, which adopts the following technical solution:

[0004] A tin ball comprises an inner tin layer and an outer tin layer, a soldering layer is arranged between the inner tin layer and the outer tin layer, the inner tin layer is arranged in a spherical shape, and the outer tin layer and the soldering layer are both arranged in a hollow spherical shape.

[0005] Preferably, the soldering layer is a rosin layer.

[0006] Preferably, the outer surface of the outer tin layer is provided with a plurality of grooves.

[0007] Preferably, the groove is arranged in a circular shape.

[0008] Preferably, the diameter of the outer tin layer is in the range of 0.8-1.0 mm, the diameter of the soldering layer is in the range of 0.6-0.7 mm, and the diameter of the inner solder layer is in the range of 0.4-0.5 mm.

[0009] In summary, the present invention includes at least one of the following beneficial technical effects:

[0010] When soldering, place the tin ball and then heat it. After the tin ball melts, the flux layer inside the outer tin layer can wrap the tin, thereby preventing the tin from oxidizing and reducing the surface tension of the tin, which allows for better soldering and does not require external flux application, making it more convenient. BRIEF DESCRIPTION OF THE DRAWINGS

[0011] Figure 1 It is a schematic diagram of the overall structure of the utility model.

[0012] Figure 2It is a cross-sectional schematic diagram of the utility model.

[0013] Figure 3 It is a cross-sectional schematic diagram of the utility model.

[0014] In the figure: 1, inner tin layer; 2, outer tin layer; 21, groove; 3, soldering layer; DETAILED DESCRIPTION

[0015] The following will be combined with the drawings in the embodiments of the utility model to clearly and completely describe the technical solutions in the embodiments of the utility model. Obviously, the described embodiments are only part of the embodiments of the utility model, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.

[0016] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc. indicate positions or positional relationships based on the positions or positional relationships shown in the accompanying drawings, or the positions or positional relationships in which the product of the application is usually placed when in use. They are only for the convenience of describing the present application and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as a limitation on the present application. In addition, the terms "first", "second", "third", etc. are only used to distinguish the description, and cannot be understood as indicating or implying relative importance.

[0017] The utility model embodiment discloses a solder ball, such as Figure 1-3 As shown, it includes an inner tin layer 1 and an outer tin layer 2, a soldering layer 3 is arranged between the inner tin layer 1 and the outer tin layer 2, the inner surface of the soldering layer 3 is in contact with the inner tin layer 1, the outer surface of the soldering layer 3 is in contact with the inner surface of the outer tin layer 2, the inner tin layer 1 is arranged in a spherical shape, and the outer tin layer 2 and the soldering layer 3 are both arranged in a hollow spherical shape. During welding, the tin balls are arranged and then heated. After the tin balls are melted, the soldering layer 3 in the outer tin layer 2 can wrap the tin, thereby preventing the tin from being oxidized and reducing the surface tension of the tin, so as to achieve better welding without the need for external soldering flux. In addition, the soldering layer 3 is a rosin layer, the melting point of rosin is low, and it can remove oxides and reduce the surface tension of the material being welded during welding, so as to achieve better welding.

[0018] At the same time, the outer surface of the outer tin layer 2 is provided with a plurality of grooves 21, and the grooves 21 are arranged in a circular shape. The grooves 21 can better cover the tin in the solder ball during the melting process during welding, thereby improving the welding effect. At the same time, the diameter range of the outer tin layer 2 is 0.8-1.0mm, the diameter range of the solder layer 3 is 0.6-0.7mm, and the diameter range of the inner solder layer is 0.4-0.5mm. In this embodiment, the diameter of the outer tin layer 2 is preferably 0.8mm, the diameter of the solder layer 3 is preferably 0.7mm, and the diameter of the inner solder layer is preferably 0.4mm. The solder ball within this diameter range has a better welding effect.

[0019] The implementation principle of a solder ball in an embodiment of the utility model is as follows: during soldering, the solder ball is placed and then heated. After the solder ball melts, the solder layer 3 in the outer tin layer 2 can wrap the tin, thereby preventing the tin from being oxidized and reducing the surface tension of the tin, which makes soldering better and more convenient without the need to apply solder flux externally.

[0020] The above is only a preferred embodiment of the utility model, and does not limit the utility model in any form. Although the utility model is disclosed as a preferred embodiment as above, it is not used to limit the utility model. Any technician familiar with this profession can make some changes or modifications to equivalent embodiments of equivalent changes by using the technical content disclosed above without departing from the scope of the technical solution of the utility model. However, any simple modification, equivalent change and modification made to the above embodiments according to the technology of the utility model, which does not depart from the content of the technical solution of the utility model, belongs to the scope of the technical solution of the utility model.

Claims

1. A solder ball, characterized in that: The invention comprises an inner tin layer (1) and an outer tin layer (2), wherein a soldering layer (3) is arranged between the inner tin layer (1) and the outer tin layer (2), the inner tin layer (1) is arranged in a spherical shape, and the outer tin layer (2) and the soldering layer (3) are both arranged in a hollow spherical shape.

2. A solder ball according to claim 1, characterized in that: The soldering layer (3) is a rosin layer.

3. The solder ball according to claim 1, characterized in that: The outer surface of the outer tin layer (2) is provided with a plurality of grooves (21).

4. A solder ball according to claim 3, characterized in that: The groove (21) is arranged in a circular shape.

5. The solder ball according to claim 1, characterized in that: The diameter of the outer tin layer (2) is in the range of 0.8-1.0 mm, the diameter of the soldering layer (3) is in the range of 0.6-0.7 mm, and the diameter of the inner tin layer (1) is in the range of 0.4-0.5 mm.