By using press-fit plates and metal connecting plates with moderate thermal conductivity in wafer bonding equipment, the uneven expansion force problem caused by deformation of metal upper press-fit plates in high temperature environments is solved, the risk of wafer rupture is reduced, and the bonding success rate is improved and yield rate.

CN222015355UActive Publication Date: 2024-11-15YIXIN (XIAMEN) TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420419289.X
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-05
Publication Date
2024-11-15
Estimated Expiration
2034-03-05

AI Technical Summary

Technical Problem

The existing metal upper pressure plates made of metal have high thermal conductivity in high temperature environments, resulting in rapid temperature changes, rapid deformation speed, uneven expansion force, and increased the risk of wafer rupture.

Method used

Use a press-fit plate with a thermal conductivity of 0.05W/(m·K) to 20W/(m·K), combined with a metal connecting plate, locked by bolts and fixed by adhesive, and use Teflon, PEEK or rubber materials as press-fit plate to reduce Deformation and buffering effect reduce the risk of wafer rupture.

Benefits of technology

It effectively reduces the risk of wafer breakage during bonding, improves yield and yield. By controlling the deformation of the pressed-plate, a more uniform pressure is ensured and the wafer is protected.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN222015355U_ABST
    Figure CN222015355U_ABST
Patent Text Reader

Abstract

The utility model relates to a pressing plate of wafer bonding equipment, which comprises a connecting plate and a pressing plate compounded with the connecting plate, and the heat conductivity coefficient of the pressing plate is 0.05 W / (m.K) to 20W / (m.K). After the technical scheme of the utility model is adopted, the heat conductivity coefficient of the pressing plate is reduced, the overall temperature change speed of the pressing plate is slower than that of metal, the deformation quantity of the pressing plate in a short time is reduced, a wafer can be better protected, and the risk that the wafer is broken during bonding is reduced; the pressing plate can be protected, and meanwhile the weight of the whole pressing plate can be increased. Preferably, a Teflon material is selected as the material of the pressing plate, and the material is softer than the metal pins, so that a certain buffering effect can be achieved, the temperature cannot be changed very quickly, and the risk of wafer breakage can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model embodiment relates to the field of semiconductor manufacturing technology, in particular to a pressing plate of a wafer bonding device. Background Art

[0002] Wafer bonding technology refers to the process of tightly bonding two mirror-polished homogeneous or heterogeneous wafers together through chemical and physical effects. After the wafers are bonded, the atoms on the interface react under the action of external forces to form covalent bonds that combine them into one, and the bonding interface reaches a specific bonding strength.

[0003] Existing thermal compression bonding equipment generally uses an oil cylinder to control an upper heating extrusion block and a lower heating extrusion plate to perform thermal compression bonding on semiconductor chips.

[0004] Chinese patent application No. 202211076324.4 discloses a semiconductor package thermal compression bonding device, including a base, a box body is fixedly arranged on the upper end of the base, a support plate is fixedly arranged on the inner wall of the box body, the support plate is used to set a workbench, an oil cylinder is fixedly arranged on the upper end of the box body, and a U-shaped cover is arranged inside the box body. In the embodiment of the utility model, the upper pressing plate is driven by the oil cylinder and the motor to drive the threaded rod to slide downward and cooperate with the lower pressing plate for bonding.

[0005] The upper and lower plates of existing wafer bonding equipment are mostly made of metal. When the upper plate made of metal enters the high temperature environment of the bonding chamber from room temperature, the temperature of the entire upper plate changes rapidly due to its high thermal conductivity, and the deformation speed is fast due to thermal expansion and contraction. The deformation force acts on the wafer, causing the wafer to be subjected to uneven expansion force and crack.

[0006] Based on the above issues, the applicant conducted research on the above issues and resulted in this case. Utility Model Content

[0007] The utility model aims to provide a pressing plate of a wafer bonding device which can better protect the wafer.

[0008] In order to achieve the above purpose, the utility model adopts the following technical solutions:

[0009] A pressing plate of a wafer bonding device comprises a connecting plate and a pressing plate combined with the connecting plate, wherein the thermal conductivity of the pressing plate is 0.05W / (m·K) to 20W / (m·K).

[0010] As a preferred embodiment of the present invention, the pressing plate is a Teflon plate, a PEEK plate, or a rubber plate.

[0011] As a preferred embodiment of the present invention, the connecting plate and the pressing plate are locked together by a plurality of first bolts.

[0012] As a preferred embodiment of the present invention, the pressing plate and the connecting plate are respectively provided with a first through hole and a first threaded hole, and the first bolt is passed through the first through hole and the first threaded hole.

[0013] As a preferred embodiment of the present invention, a countersunk hole is provided on the pressing plate, and the first bolt is received in the countersunk hole.

[0014] As a preferred embodiment of the present invention, a pressing portion extending axially is provided at the center of the pressing plate.

[0015] As a preferred embodiment of the present invention, the radius of the pressing plate is not greater than 30CM.

[0016] As a preferred embodiment of the present invention, the connecting plate is a metal plate.

[0017] As a preferred embodiment of the present invention, the weight of the connecting plate is no more than 10KG.

[0018] As a preferred embodiment of the present invention, the connecting plate and the pressing plate are fixed together by an adhesive.

[0019] After adopting the technical solution of the utility model, the thermal conductivity of the press plate is 0.05W / (m·K) to 20W / (m·K). When entering a high temperature environment from room temperature, the press plate is not easy to produce a large deformation in a short time, which can better protect the wafer and reduce the risk of wafer cracking during bonding. The connecting plate, as a connecting carrier between the entire press plate and other components, can protect the press plate and also increase the weight of the entire press plate. Furthermore, the utility model selects Teflon material as the material of the press plate, which is softer than metal, can play a certain buffering role, and will not change temperature very quickly, which can reduce the risk of wafer cracking. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a structural schematic diagram of a pressing plate of a wafer bonding device according to the first embodiment of the utility model.

[0021] Figure 2 yes Figure 1 Center A view.

[0022] Figure 3 It is a structural schematic diagram of the upper pressing plate of the second embodiment of the utility model. DETAILED DESCRIPTION

[0023] The utility model is now further described in conjunction with the accompanying drawings and specific embodiments. Embodiment 1

[0024] refer to Figure 1 The embodiment of the utility model discloses a pressing plate of a wafer bonding device, including a pressing plate 8, and the thermal conductivity of the pressing plate is 0.05W / (m·K) to 20W / (m·K).

[0025] In order to keep the lower end surface of the pressing plate flat when pressing the wafer, a connecting plate 9 is also included, and the pressing plate 8 is attached to the lower end surface of the connecting plate 9 .

[0026] In the embodiment of the present invention, the pressing plate 8 is made of Teflon. Based on this embodiment, the pressing plate 8 can also be made of PEEK, rubber, etc.

[0027] A connecting portion 12 is provided at the upper end of the connecting plate 9, and a connecting ring 14 is detachably provided on the circumferential side of the connecting portion 12 through a second bolt 13. The connecting ring 14 can be used to connect to one end of an iron chain, and the other end of the iron chain can be connected to an external upper cover body, thereby realizing that the pressure plate of the wafer bonding equipment is set on the external upper cover body, and the pressure plate of the wafer bonding equipment is detachably connected to the iron chain, thereby achieving the effect of replacing the pressure plates of different wafer bonding equipment according to different bonding pressures or bonding areas.

[0028] Furthermore, in order to conveniently set the pressing plate 8 on the lower end surface of the connecting plate 9, the pressing plate 8 and the connecting plate 9 are respectively provided with a first through hole and a first threaded hole for the first bolt 10 to pass through. In order to ensure the bonding effect, the lower end surface of the pressing plate 8 is provided with a countersunk hole 11. By setting the countersunk hole 11, when the first bolt 10 connects the pressing plate 8 and the connecting plate 9 together, the lower end surface of the threaded head of the first bolt 10 can be flush with the lower end surface of the pressing plate 8 or retracted into the countersunk hole 11.

[0029] The thermal conductivity acting on the pressing plate 8 is 0.05W / (m·K) to 20W / (m·K), which is close to the wafer. After entering the high-temperature environment, the degree of deformation generated instantly is relatively controllable, avoiding the traditional use of metal as a pressure structure to enter the high-temperature environment, which causes a large and uncontrollable short-term deformation, resulting in uneven force on the wafer and damage to the wafer during bonding. That is, the deformation force of the traditional metal pressure structure acting on the wafer will cause the wafer to be subjected to uneven expansion force and crack.

[0030] Furthermore, the pressing plate 8 has a certain elasticity, and can play a buffering role when in contact with the wafer, and will not cause temperature changes at the moment of contact with the wafer.

[0031] Based on the above characteristics, using the pressing plate 8 as the contact surface during bonding can greatly reduce the probability of wafer breakage during bonding and improve the yield and good product rate.

[0032] refer to Figure 2 In order to improve the success rate and yield rate of bonding, the first bolts 10 are divided into arrays, thereby further reducing the deformation of the contact surface of the pressing plate 8 caused by high temperature deformation. Embodiment 2

[0033] refer to Figure 3 In order to adapt to different bonding areas of wafers, a pressing portion 15 is provided on the lower end surface of the pressing plate 8. The material properties of the pressing portion 15 are the same as those of the pressing plate 8. The projected area of ​​the pressing portion 15 can be set to different specifications as needed.

[0034] In this embodiment, the pressing part 15 and the pressing plate 8 are integrally manufactured, and the pressing part 15 may be in the shape of a disk. In this way, a height difference is formed between the pressing part 15 and the periphery of the pressing plate 8, that is, a buffer zone is formed on the periphery of the pressing part 15. When bonding a wafer with a smaller area, the wafer can be bonded only through the pressing part 15, so as to avoid damage to the periphery of the wafer caused by the pressing plate 8 being too large, and at the same time, the pressing plate 8 and the connecting plate 9 can provide sufficient weight to ensure the bonding pressure.

[0035] Based on the above-mentioned embodiments 1 and 2, the pressing plate of the wafer bonding equipment is no greater than 30CM.

[0036] The connecting plate 9 is made of metal and weighs no more than 10KG.

[0037] The radius of the pressing plate 8 is not greater than 30CM, and the thickness is not greater than 30CM.

[0038] The pressing plate 8 and the connecting plate 9 may also be connected together by adhesive.

[0039] The pressing part 15 can also be manufactured separately and connected with the pressing plate 8 through the first bolt 10 .

[0040] The modifications and changes made using this creation are all within the patent scope claimed by this creation, and are not limited to those disclosed in the embodiments.

Claims

1. A pressure plate for a wafer bonding device, characterized in that: The invention comprises a connecting plate and a pressing plate combined with the connecting plate, wherein the thermal conductivity of the pressing plate is 0.05W / (m·K) to 20W / (m·K).

2. The pressing plate of the wafer bonding equipment according to claim 1, characterized in that: The pressing plate is a Teflon plate, a PEEK plate or a rubber plate.

3. The pressing plate of the wafer bonding equipment according to claim 1, characterized in that: The connecting plate and the pressing plate are locked together by a plurality of first bolts.

4. The pressing plate of the wafer bonding equipment according to claim 3, characterized in that: The pressing plate and the connecting plate are respectively provided with a first through hole and a first threaded hole, and the first bolt is passed through the first through hole and the first threaded hole.

5. The pressing plate of the wafer bonding equipment according to claim 4, characterized in that: The pressing plate is provided with a countersunk hole, and the first bolt is received in the countersunk hole.

6. The pressing plate of the wafer bonding equipment according to claim 5, characterized in that: A pressing portion extending axially is provided at the center of the pressing plate.

7. The pressing plate of the wafer bonding equipment according to claim 1, characterized in that: The radius of the pressing plate is not greater than 30CM.

8. The pressing plate of the wafer bonding equipment according to claim 1, characterized in that: The connecting plate is a metal plate.

9. The pressing plate of the wafer bonding equipment according to claim 8, characterized in that: The weight of the connecting plate is not more than 10KG.

10. The pressing plate of the wafer bonding equipment according to claim 1, characterized in that: The connecting plate and the pressing plate are fixed together by adhesive.