Scratch-proof thermochromic colored crystal glass
By adopting a multi-layer structure in color crystal glass, including heat absorption layer, thermal chromatomorphism layer, explosion-proof layer, waterproof and oil-proof layer and fire-proof layer, combined with a protective film, the scratch-proof, high-temperature and explosion-proof of color crystal glass is improved. , waterproof and oil-proof and fire-proof performance solve the problem of single function of existing colored crystal glass.
Patent Information
- Application Number
- CN202420561619.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-22
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-03-22
AI Technical Summary
The existing colored crystal glass has relatively single scratch-resistant, high temperature resistance, waterproof, oil-resistant and flame-retardant fire-resistant properties, which is difficult to meet the market's demand for functional improvement.
It adopts tempered glass substrate, combined with heat absorption layer made of iron oxide, thermal chromatographic layer made of cyanobiphenyl, explosion-proof layer made of polyvinylidene diethylene, waterproof and oil-proof layer made of polytetrafluoroethylene resin, The fire-resistant layer made of aluminum hydroxide and the protective film made of linear low-density polyethylene form a multi-layer structure of anti-scratch thermally chromatinous color crystal glass.
It enhances the wear resistance and high temperature resistance of glass, improves explosion-proof, waterproof and oil-proof and fire-proof performance, making the glass less likely to scratch during handling, can be kept clean for a long time, and has the safety functions of flame retardant and fire-proof.
Smart Images

Figure CN222039879U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of glass, in particular to a scratch-resistant thermochromic colored crystal glass. Background Art
[0002] Colored crystal glass is an ideal new decorative material. A layer of colored coating with ink or a colored transparent coating with ink is printed on the surface of ordinary flat glass or tempered glass, and then a layer of resin with a cross-linked molecular structure is applied. Plastic colored crystal particles (or glitter paper, gold powder, silver powder, laser powder) are pasted on the adhesive layer. After drying or air-drying, a layer of epoxy resin protective layer is applied to make colored crystal glass. If a layer of epoxy resin is applied on the epoxy resin protective layer and a piece of flat glass is pasted, it will form a sandwich (double-layer) colored crystal glass.
[0003] In order to adapt to the development of the market, the industry's requirements for colored crystal glass are constantly increasing. The colored crystal glass on the market is generally mainly for decorative performance, with relatively simple functions. The scratch resistance, high temperature resistance, waterproof and oil resistance, and flame retardant and fireproof properties of colored crystal glass need to be improved. Utility Model Content
[0004] The utility model aims to solve the shortcomings of the prior art and proposes a scratch-resistant thermochromic colored crystal glass.
[0005] In order to achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a scratch-resistant thermochromic colored crystal glass, comprising a glass substrate, a heat-absorbing layer is arranged on one side of the glass substrate, a thermochromic layer is bonded to the surface of the heat-absorbing layer, an explosion-proof layer is bonded to the surface of the thermochromic layer, a waterproof and oil-proof layer is arranged on the other side of the glass substrate, a fire-proof layer is arranged around the glass substrate, and a protective film is arranged on the outside of the explosion-proof layer, the waterproof and oil-proof layer and the fire-proof layer.
[0006] As a further description of the above technical solution:
[0007] The glass substrate is made of tempered glass.
[0008] As a further description of the above technical solution:
[0009] The heat absorption layer is made of iron oxide material.
[0010] As a further description of the above technical solution:
[0011] The thermochromic layer is made of cyanobiphenyl material.
[0012] As a further description of the above technical solution:
[0013] The explosion-proof layer is made of polyvinylidene material.
[0014] As a further description of the above technical solution:
[0015] The waterproof and oil-proof layer is made of polytetrafluoroethylene resin material.
[0016] As a further description of the above technical solution:
[0017] The fireproof layer is made of aluminum hydroxide.
[0018] As a further description of the above technical solution:
[0019] The protective film is made of linear low-density polyethylene material.
[0020] The utility model has the following beneficial effects:
[0021] 1. Compared with the prior art, the anti-scratch thermochromic colored crystal glass, through the provision of a protective film, a heat absorption layer and a thermochromic layer, has generally better scratch resistance and high temperature resistance than the prior colored crystal glass. The protective film can enhance the wear resistance of the glass to prevent scratches or damage to the glass during transportation. The heat absorption layer can increase the infrared transmittance and reflectivity of the thermochromic layer when absorbing heat, thereby reducing the internal temperature and improving the high temperature resistance.
[0022] 2. Compared with the prior art, the scratch-resistant thermochromic colored crystal glass has an explosion-proof layer, a waterproof and oil-proof layer and a fire-proof layer. Compared with the conventional colored crystal glass, which has general explosion-proof, waterproof and oil-proof and fire-proof properties, the device increases the explosion-proof property by setting the explosion-proof layer. The waterproof and oil-proof layer enables the glass to have a good function of preventing dust or oil from adhering, so that the glass can remain clean for a long time. The fire-proof layer enables each side edge of the glass to have flame-retardant and fire-proof safety functions. BRIEF DESCRIPTION OF THE DRAWINGS
[0023] Figure 1 This is a schematic diagram of the overall structure of a scratch-resistant thermochromic colored crystal glass proposed by the utility model;
[0024] Figure 2 This is a cross-sectional view of the overall structure of the scratch-resistant thermochromic colored crystal glass proposed by the utility model.
[0025] Legend:
[0026] 100, glass substrate; 200, heat absorption layer; 300, thermochromic layer; 400, explosion-proof layer; 500, waterproof and oil-proof layer; 600, fireproof layer; 700, protective film. DETAILED DESCRIPTION
[0027] Reference Figure 1-2The utility model provides a scratch-resistant thermochromic colored crystal glass, which includes a glass substrate 100, a heat absorption layer 200, a thermochromic layer 300, an explosion-proof layer 400, a waterproof and oil-proof layer 500, a fireproof layer 600 and a protective film 700.
[0028] The glass substrate 100 is used for support. Specifically, the glass substrate 100 is made of tempered glass and has good bending strength and impact resistance.
[0029] The heat absorption layer 200 is used to absorb heat, thereby changing the infrared transmittance and reflectivity of the thermochromic layer 300 . Specifically, the heat absorption layer 200 is disposed on one side of the glass substrate 100 , and the heat absorption layer 200 is made of iron oxide.
[0030] The thermochromic layer 300 is used to reduce the temperature of the glass substrate 100. Specifically, the thermochromic layer 300 is attached to the surface of the heat absorption layer 200. The thermochromic layer 300 is made of cyanobiphenyl material. When used, when the heat absorption layer 200 absorbs heat and the temperature rises, the infrared transmittance and reflectivity of the thermochromic layer 300 are increased, thereby reducing the internal temperature.
[0031] The explosion-proof layer 400 is used to increase the explosion-proof property. Specifically, the surface of the thermochromic layer 300 is bonded with the explosion-proof layer 400, and the explosion-proof layer 400 is made of polyvinylidene material.
[0032] The waterproof and oil-proof layer 500 is used to make the glass have good dust or oil-proof adhesion function, so that the glass can remain clean for a long time. Specifically, the other side of the glass substrate 100 is provided with a waterproof and oil-proof layer 500, and the waterproof and oil-proof layer 500 is made of polytetrafluoroethylene resin.
[0033] The fireproof layer 600 is used to make each side edge of the glass substrate 100 have the safety functions of flame retardancy and fire prevention. Specifically, the fireproof layer 600 is arranged around the glass substrate 100, and the fireproof layer 600 is made of aluminum hydroxide.
[0034] The protective film 700 is used to enhance the wear resistance of the glass and prevent the glass from being scratched or damaged during transportation. Specifically, the explosion-proof layer 400, the waterproof and oil-proof layer 500 and the fireproof layer 600 are provided with the protective film 700 outside, and the protective film 700 is made of linear low-density polyethylene.
[0035] Working principle: In specific use, the glass substrate 100 is made of tempered glass and has good bending strength and impact strength. The upper surface of the glass substrate 100 is bonded with a heat absorption layer 200 by adhesive, and the upper surface of the heat absorption layer 200 is bonded with a thermochromic layer 300 by adhesive. The heat absorption layer 200 is used to absorb heat, thereby changing the infrared transmittance and reflectivity of the thermochromic layer 300. When the heat absorption layer 200 absorbs heat and the temperature rises, the infrared transmittance and reflectivity of the thermochromic layer 300 are increased, thereby reducing the internal temperature. The upper surface of the thermochromic layer 300 is bonded with an explosion-proof layer 400 by adhesive, and the explosion-proof layer 400 is used to increase the explosion-proof property. A waterproof and oil-proof layer 500 is adhered to the lower surface of the glass substrate 100 by adhesive. The waterproof and oil-proof layer 500 is used to make the glass have a good function of preventing dust or oil from adhering, so that the glass can be kept clean for a long time. A fireproof layer 600 is adhered to the four sides of the glass substrate 100 by adhesive. The fireproof layer 600 is used to make the side edges of the glass substrate 100 have flame retardant and fireproof safety functions. The outside of the explosion-proof layer 400, the waterproof and oil-proof layer 500 and the fireproof layer 600 is coated with a protective film 700. The protective film 700 is made of linear low-density polyethylene material, has a certain viscosity, and can enhance the wear resistance of the glass to prevent scratches or damage to the glass during transportation.
[0036] Finally, it should be noted that the above is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or make equivalent substitutions for some of the technical features therein. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
Claims
1. A scratch-resistant thermochromic colored crystal glass, comprising a glass substrate (100), Features: A heat absorption layer (200) is provided on one side of the glass substrate (100), a thermochromic layer (300) is laminated on the surface of the heat absorption layer (200), an explosion-proof layer (400) is laminated on the surface of the thermochromic layer (300), a waterproof and oil-proof layer (500) is provided on the other side of the glass substrate (100), a fire-proof layer (600) is provided around the glass substrate (100), and a protective film (700) is provided on the outside of the explosion-proof layer (400), the waterproof and oil-proof layer (500), and the fire-proof layer (600).
2. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The glass substrate (100) is made of tempered glass.
3. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The heat absorption layer (200) is made of iron oxide material.
4. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The thermochromic layer (300) is made of cyanobiphenyl material.
5. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The explosion-proof layer (400) is made of polyvinylidene material.
6. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The waterproof and oil-proof layer (500) is made of polytetrafluoroethylene resin material.
7. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The fireproof layer (600) is made of aluminum hydroxide material.
8. The scratch-resistant thermochromic colored crystal glass according to claim 1, Features: The protective film (700) is made of linear low-density polyethylene material.