A kind of effect and leather technology, which is applied in the field of preparation of abrasive effect leather products, can solve the problems of large differences in dye penetration, large color differences, and widely varying abrasive effects, and achieve the effect of stable appearance quality and small differences between them
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A kind of preparation method of grain effect leather product, comprises the following steps:
[0014] 1) Conduct a permeability test on the skin. The permeability test is based on the observation of the water drop experiment. During the test, a few drops of water are dropped on the skin. The water drops will not soak the leather surface or penetrate into the skin for 15-30 seconds. After 1-2 minutes, the surface of the skin is slightly wetted, and the contact angle between the water drop and the surface of the skin is measured to obtain a permeability detection value of 30, and the total amount of penetrant used for the two spray dyeings is determined to be 30g / sf.
[0015] 2) Carry out a spray dyeing to the leather base:
[0016] The spray formulation is
[0017] Dye water 40g / L
[0018] Penetrant 700g / L
[0019] Water 600g / L
[0020] The spraying machine has a large amount of spraying, 8 guns, 8-12 grids, spraying 3 times, drying at low temperature,
[0021] 3) G...
Embodiment 2
[0035] A kind of preparation method of grain effect leather product, comprises the following steps:
[0036] 1) Conduct a permeability test on the skin. The permeability test is based on the observation of the water drop experiment. During the test, a few drops of water are dropped on the skin. The water drops will not soak the leather surface or penetrate into the skin for 15-30 seconds. After 1-2 minutes, the surface of the skin is slightly soaked, and the contact angle between the water drop and the surface of the skin is measured, and the permeability detection value is 60, and the total amount of penetrant used for the two spray dyeings is determined to be 12g / sf.
[0037] 2) Carry out a spray dyeing to the leather base:
[0038] The spray formulation is
[0039] Dye water 40g / L
[0040] Penetrant 600g / L
[0041] Water 600g / L
[0042] The spraying machine has a large amount of spraying, 8 guns, 8-12 grids, spraying 3 times, drying at low temperature,
[0043] 3) Grin...
Embodiment 3
[0057] A kind of preparation method of grain effect leather product, comprises the following steps:
[0058] 1) Conduct a permeability test on the skin. The permeability test is based on the observation of the water drop experiment. During the test, a few drops of water are dropped on the skin. The water drops will not soak the leather surface or penetrate into the skin for 15-30 seconds. After 1-2 minutes, the surface of the skin is slightly wetted, and the contact angle between the water drop and the surface of the skin is measured to obtain a permeability detection value of 70, and the total amount of penetrant used for the two spray dyeings is determined to be 6g / sf.
[0059] 2) Carry out a spray dyeing to the leather base:
[0060] The spray formulation is
[0061] Dye water 40g / L
[0062] Penetrant 400g / L
[0063] Water 600g / L
[0064] The spraying machine has a large amount of spraying, 8 guns, 8-12 grids, spraying 3 times, drying at low temperature,
[0065] 3) Gr...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com