Circulating cooling water slow-release scale inhibitor and preparation method thereof
By using sustained release scale inhibitors with components such as hyperbranched polymers and modified chitosan in the circulating cooling water system, the problem of low efficiency of scale inhibitors in the prior art in a high-salt environment is solved, and high efficiency is achieved Scale-resistance effect and environmentally friendly performance extend the service life of the equipment.
Patent Information
- Application Number
- CN202411158783.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-22
- Publication Date
- 2024-11-29
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The scale inhibitor used in existing circulating cooling water systems is not effective in high-salt environments, and its environmental protection and temperature resistance are insufficient, which limits its application promotion.
Using a sustained release scale inhibitor containing hyperbranched polymer, modified chitosan, anionic polyacrylamide, melamine and dispersant, nanoscale voids are formed by chelating with metal ions by hydroxyl, carboxy and phosphonic acid groups. The cavity and double electron layer inhibit the formation of scale layer and disperse scale particles, improving scale resistance effect.
It significantly improves the scale resistance effect of the circulating cooling water system, enhances the service life and operation efficiency of the equipment, and has good environmental protection, temperature and salt resistance.
Smart Images

Figure BDA0005005841960000041 
Figure BDA0005005841960000071 
Figure BDA0005005841960000081
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of scale inhibitors, and in particular relates to a circulating cooling water slow-release scale inhibitor and a preparation method thereof. Background Art
[0002] As the tension of water environment resources continues to intensify, all walks of life have begun to widely adopt circulating cooling water systems to improve the utilization efficiency of water resources. In this system, due to the repeated recycling of cooling water, the content of mineral ions such as calcium and magnesium in the water gradually accumulates, causing the ion concentration to increase and exceed its solubility limit, thereby forming insoluble salts and depositing on the inner wall of the equipment pipeline to form a scale layer, which will not only accelerate the corrosion process of metal equipment, but also reduce the heat exchange efficiency of the system due to the adsorption of calcium scale, which may shorten the service life of the equipment.
[0003] To meet this challenge, the commonly used method is to add chemical antiscalants to the circulating cooling water system, which is both economical and effective. However, existing antiscalants have some problems, such as poor environmental performance, low antiscaling efficiency, and high cost, which limit their promotion in practical applications.
[0004] Chinese patent CN 109942101A relates to a composite slow-release scale inhibitor, comprising the following raw materials: calcium tartrate, benzotriazole, polyaspartic acid, polyacrylamide, diethanol monoisopropanolamine, water, starch matrix, hydroxyethylene diphosphonic acid, modified chitosan and polyphosphate. The composite slow-release scale inhibitor of this invention has a simple preparation process, energy saving and environmental protection, low cost and strong practicality; however, for some high-salt circulating cooling water, the scale inhibition efficiency of the scale inhibitor is poor.
[0005] Therefore, there is an urgent need for a circulating cooling water slow-release scale inhibitor and a preparation method thereof, so that the scale inhibitor has good scale inhibition effect and is temperature-resistant and salt-resistant. Summary of the invention
[0006] In view of the existing technical problems, the purpose of the present invention is to provide a circulating cooling water slow-release scale inhibitor and a preparation method thereof. The scale inhibitor of the present invention not only has excellent scale inhibition effect, but also has the advantages of environmental protection, temperature resistance, salt resistance and corrosion resistance, can effectively improve the operating efficiency of the circulating cooling water system and the service life of the equipment, and has good application value.
[0007] In order to achieve the above object, the technical solution adopted by the present invention is as follows:
[0008] On the one hand, the present invention provides a circulating cooling water slow-release scale inhibitor, which comprises the following raw materials in parts by weight: 20-30 parts of polyacrylamide, 10-20 parts of polyepoxysuccinic acid, 10-15 parts of sodium gluconate, 5-15 parts of hyperbranched polymer, 5-15 parts of isophorone diamine, 4-8 parts of modified chitosan, 2-6 parts of melamine, 1-5 parts of benzotriazole, 1-2 parts of tartaric acid, 1-2 parts of dispersant and 30-50 parts of deionized water.
[0009] The reaction mechanism and effects of the present invention are as follows:
[0010] 1. Organic phosphonates and their derivatives are still one of the main ingredients of scale inhibitors due to their high scale inhibition performance, temperature resistance, stability and easy transportation. However, organic phosphonate scale inhibitors may hydrolyze under strong acid and strong alkali conditions, affecting their stability and scale inhibition effect, and high-phosphorus scale inhibitors may pollute the water body during use. Hyperbranched polymer molecules have the characteristics of low viscosity, high solubility, high reactivity and environmental friendliness, which makes them more advantageous in scale inhibition. The combination of the two can make the scale inhibitor have a wide pH adaptability range and stable scale inhibition performance. In a strong alkaline environment, the more branched structures, the more conducive to scale inhibition.
[0011] The invention synthesizes a novel hyperbranched polymer as a scale inhibitor, and the branched structure can provide more terminal functional groups to enhance the scale inhibition effect. The applicant uses citric acid and 1,2,4-butanetriol to react to form a branched structure compound intermediate, and then uses the hydroxyl group on it to undergo a substitution reaction with a halogen element to introduce it into 6-chloro-2,4-difluoroaniline, and finally introduces hydroxyethylidene diphosphonic acid to synthesize a low-phosphorus hyperbranched scale inhibitor.
[0012] The hydroxyl, carboxyl and phosphonic acid groups in the hyperbranched polymer structure can chelate with metal ions in water, thereby inhibiting the formation of scale; at the same time, the oxygen atoms in these functional groups will combine with the calcium atoms on the crystal surface in the form of chemical bonds, occupying the active sites on the crystal surface, causing the crystal surface to distort, resulting in lattice distortion, and hindering the normal growth of the crystal. This not only prevents the formation of scale layers, but may also cause the existing scale layers to gradually loosen or even fall off, thereby maintaining the cleanliness of the system and the efficient operation of the equipment, and significantly improving the stability and maintenance efficiency of the circulating cooling water treatment system.
[0013] In addition, the active amino groups and metal ions in the nanometer-scale cavities formed by the hyperbranched scale inhibitor of the present invention repel each other to form a double electron layer, which plays a role in dispersing and inhibiting scale.
[0014] 2. Chitosan has good biocompatibility, biodegradability and antibacterial properties. However, in a high-salt environment, high concentrations of salt may reduce the solubility of chitosan through the "salting out" effect, affecting its function. This is because salt reduces the availability of water molecules, thereby reducing the hydration between chitosan molecules and causing the precipitation of chitosan.
[0015] The present invention utilizes the amino group of chitosan and the carboxyl group of sodium 5-sulfoisophthalic acid to condense and prepare modified chitosan. The introduction of sulfonic acid groups makes the modified chitosan have good temperature and salt resistance, and improves its salt resistance in high-salt circulating cooling water. In addition, the sulfonic acid group has strong acidity, which is helpful for the dispersion and dissolution of scale; at the same time, the sulfonic acid group can synergistically act with the hydroxyl group on the chitosan, effectively chelate with the metal ions in the water, and form a stable complex, thereby inhibiting these metal ions from combining with anions in the water to form insoluble precipitates.
[0016] 3. The anionic polymer polyacrylamide is added in the present invention, which can ionize electronegative groups in the solution, collide with the microcrystalline particles and adsorb on the surface of the microcrystalline, so that the surface of the microcrystalline carries a large amount of negative charge. Since the same charges repel each other, the electrostatic repulsion can prevent the effective collision, growth and deposition between the microcrystalline particles, and further disperse the microcrystalline particles in the water body to achieve the scale inhibition effect. The applicant achieves a more sufficient effect by adjusting the molecular weight of the anionic polyacrylamide to avoid the possible pipeline blockage problem.
[0017] 4. The dispersant (sodium alkylbenzene sulfonate and / or polyethylene glycol) added in the present invention plays a key role in dispersing scale particles and raw materials. Sodium alkylbenzene sulfonate, as an anionic surfactant, has good solubility and hard water resistance; polyethylene glycol, as a non-ionic surfactant, has good water solubility and biocompatibility. Both effectively prevent the formation and deposition of scale through multiple mechanisms such as electrostatic repulsion, dispersion, chelation and crystal distortion, improve heat exchange efficiency, reduce energy consumption, and extend the service life of equipment.
[0018] 5. In the present invention, melamine can form a dense protective film on the surface of the pipe material through the polar adsorption group, and the hydrophobic group in isophorone diamine can prevent water and dissolved oxygen from diffusing to the metal surface. The two can synergistically inhibit the occurrence of corrosion reactions.
[0019] In some embodiments, the polyacrylamide is anionic polyacrylamide.
[0020] In some embodiments, the number average molecular weight of the anionic polyacrylamide is 8-20 million.
[0021] Preferably, the number average molecular weight of the anionic polyacrylamide is 10-18 million.
[0022] In some embodiments, the method for preparing the hyperbranched polymer comprises the following preparation steps:
[0023] S1. Add citric acid and 1,2,4-butanetriol to a reaction kettle, stir, then add p-toluenesulfonic acid, heat to 115-125°C, control the vacuum degree to 0.20-0.75MPa, stir and react for 8-12h to obtain intermediate 1;
[0024] S2. The intermediate 1 obtained in step S1, dimethyl sulfoxide, and 6-chloro-2,4-difluoroaniline are added to a reaction kettle, stirred, and sodium carbonate is added under an inert gas atmosphere, heated to 70-100° C., stirred for 10-12 hours, washed, and dried to obtain intermediate 2;
[0025] S3. Add hydroxyethylidene diphosphonic acid and deionized water into a reaction kettle, stir, then add 4-dimethylaminopyridine and stir, dropwise add intermediate 2 obtained in step S2, heat to 65-75°C, react for 10-14h, wash, and dry to obtain a hyperbranched polymer.
[0026] In some embodiments, the molar ratio of citric acid to 1,2,4-butanetriol in step S1 is (3-3.6):1.
[0027] Preferably, the molar ratio of citric acid to 1,2,4-butanetriol in step S1 is 3.2:1.
[0028] In some embodiments, the molar ratio of the intermediate 1 to 6-chloro-2,4-difluoroaniline in step S2 is 1:(3.2-3.8).
[0029] Preferably, the molar ratio of the intermediate 1 to 6-chloro-2,4-difluoroaniline in step S2 is 1:3.5.
[0030] In some embodiments, the molar ratio of the intermediate 2 to hydroxyethylidene diphosphonic acid in step S3 is 1:(3.2-3.8).
[0031] Preferably, in step S3, the molar ratio of intermediate 2 to hydroxyethylidene diphosphonic acid is 1:3.5.
[0032] In some embodiments, the structural formula of the hyperbranched polymer is as follows:
[0033]
[0034] In some embodiments, the method for preparing the modified chitosan comprises the following preparation steps:
[0035] (1) adding chitosan and deionized water into a reaction kettle, adjusting the pH to 2.5-3, and stirring to obtain a chitosan solution;
[0036] (2) adding sodium 5-sulfoisophthalic acid and deionized water into a reaction kettle, stirring, and then adding 1-ethyloctyl-(3-dimethylaminopropyl)carbodiimide hydrochloride to obtain a sodium 5-sulfoisophthalic acid solution;
[0037] (3) Mixing the chitosan solution obtained in step (1) with the sodium 5-sulfonate solution obtained in step (2), adjusting the pH to 6-7, stirring at room temperature for 4-5 hours, and filtering to obtain modified chitosan.
[0038] In some embodiments, the mass ratio of chitosan to sodium 5-sulfoisophthalate is 1:(1.5-3).
[0039] In some embodiments, the dispersant is sodium alkyl sulfonate and / or polyethylene glycol.
[0040] Preferably, the dispersant is sodium alkyl sulfonate and polyethylene glycol, and the mass ratio of the two is 1:(1-3).
[0041] More preferably, the sodium alkyl sulfonate is sodium dodecyl sulfonate; and the polyethylene glycol is polyethylene glycol 200.
[0042] Another aspect of the present invention is to provide a method for preparing a slow-release antiscalant for circulating cooling water, comprising the following steps:
[0043] Add polyacrylamide, polyepoxysuccinic acid, sodium gluconate, hyperbranched polymer, isophorone diamine, modified chitosan, melamine, benzotriazole, tartaric acid, dispersant and deionized water into a reactor, stir for 20-60 minutes, heat to 50-70°C, and stir for 2-4 hours at an ultrasonic power of 100-350W to obtain a slow-release scale inhibitor.
[0044] Compared with the prior art, the present invention has the following beneficial effects:
[0045] 1. The scale inhibitor of the present invention not only has excellent scale inhibition effect, but also has the advantages of environmental protection, temperature resistance, salt resistance and corrosion resistance. It can effectively improve the operating efficiency of the circulating cooling water system and the service life of the equipment, and has good application value.
[0046] 2. The hyperbranched polymer of the present invention can provide more terminal functional groups to enhance the scale inhibition effect. The hydroxyl, carboxyl and phosphonic acid groups in the structure can chelate with metal ions in water, thereby inhibiting the formation of scale; at the same time, the oxygen atoms in these functional groups will combine with the calcium atoms on the surface of the crystal in the form of chemical bonds, occupying the active sites on the surface of the crystal, causing lattice distortion, preventing the formation of scale layers, and may also cause the existing scale layers to gradually loosen or even fall off, maintaining the cleanliness of the system and the efficient operation of the equipment.
[0047] 3. The modified chitosan of the present invention has good temperature and salt resistance; the introduced sulfonic acid group has strong acidity, which is helpful for the dispersion and dissolution of scale; at the same time, the sulfonic acid group can synergistically act with the hydroxyl groups on the chitosan, effectively chelate with the metal ions in the water to form a stable complex, thereby inhibiting scale formation.
[0048] 4. The anionic polymer polyacrylamide added in the present invention can prevent the effective collision, growth and deposition between microcrystalline particles, and then disperse the microcrystalline particles in the water body to achieve the scale inhibition effect.
[0049] 5. In the present invention, melamine and isophorone can synergistically inhibit the occurrence of corrosion reactions. DETAILED DESCRIPTION
[0050] The present invention will be described below in conjunction with specific embodiments. It should be noted that the following embodiments are examples of the present invention and are only used to illustrate the present invention, rather than to limit the present invention. Other combinations and various modifications within the concept of the present invention may be performed without departing from the spirit or scope of the present invention.
[0051] According to the ratios of the raw materials and the preparation methods specified in the following examples and comparative examples, various slow-release scale inhibitors were prepared.
[0052] In order to facilitate those skilled in the art to implement the present invention, some raw material manufacturers of the embodiments and comparative examples are described as follows:
[0053] Anionic polyacrylamide: purchased from Gongyi Hongyuan Environmental Protection Technology Co., Ltd., with a number average molecular weight of 14 million;
[0054] Cationic polyacrylamide: purchased from Guangdong Shouxin Environmental Protection Materials Technology Co., Ltd., with a number average molecular weight of 14 million;
[0055] Polyepoxysuccinic acid: purchased from Guangzhou Yuanchang Trading Co., Ltd.
[0056] Melamine: purchased from Suzhou Yichen Chemical Technology Co., Ltd.;
[0057] Polyethylene glycol 200: purchased from Wuhan Jixinyibang Biotechnology Co., Ltd.;
[0058] Chitosan: purchased from Guangdong Hongyou Biotechnology Co., Ltd.;
[0059] Other raw materials are not specially specified and can be purchased from the market.
[0060] Preparation Example 1
[0061] The preparation method of hyperbranched polymer A comprises the following steps:
[0062] S1. 32 mmol of citric acid and 10 mmol of 1,2,4-butanetriol were added to the reactor, stirred for 1 h, and then 0.84 mmol of p-toluenesulfonic acid was added, heated to 120 ° C, the vacuum degree was controlled to 0.5 MPa by a vacuum pump, and stirred for 10 h to obtain intermediate 1;
[0063] S2. Take 30 mmol of intermediate 1 obtained in step S1, 105 mmol of 6-chloro-2,4-difluoroaniline, and 100 ml of dimethyl sulfoxide and add them to a reaction kettle, stir for 1 hour, add 6 mmol of sodium carbonate under a nitrogen atmosphere, heat to 80 ° C, stir and react for 10 hours, wash with deionized water 3 times, and dry at 105 ° C for 6 hours to obtain intermediate 2;
[0064] S3. Add 210 mmol of hydroxyethylidene diphosphonic acid and 250 ml of deionized water into a reactor, stir until the hydroxyethylidene diphosphonic acid is completely dissolved, add 3.5 mmol of 4-dimethylaminopyridine, stir for 1 hour, and add 60 mmol of intermediate 2 obtained in step S2 dropwise within 2 hours. After the addition is completed, heat to 70°C, react for 12 hours, vacuum dry for 2 hours, wash with ethanol 3 times, and then dry at 75°C for 24 hours to obtain a hyperbranched polymer A.
[0065] The structural formula of the hyperbranched polymer A is as follows:
[0066]
[0067] Preparation Example 2
[0068] The preparation method of hyperbranched polymer B comprises the following steps:
[0069] S1. 32 mmol of citric acid and 10 mmol of 1,2,4-butanetriol were added to the reactor, stirred for 1 h, and then 0.84 mmol of p-toluenesulfonic acid was added, heated to 120 ° C, the vacuum degree was controlled to 0.5 MPa by a vacuum pump, and stirred for 10 h to obtain intermediate 1;
[0070] S2. Take 30 mmol of intermediate 1 obtained in step S1, 105 mmol of 6-chloro-2,4-difluoroaniline and 100 ml of dimethyl sulfoxide and add them into a reactor, stir for 1 hour, add 6 mmol of sodium carbonate under a nitrogen atmosphere, heat to 80°C, stir and react for 10 hours, wash with deionized water 3 times, and dry at 105°C for 6 hours to obtain a branched polymer B.
[0071] The structural formula of the hyperbranched polymer B is as follows:
[0072]
[0073] Preparation Example 3
[0074] The preparation method of hyperbranched polymer C is the same as that of Preparation Example 1, except that the amount of citric acid added is 22 mmol.
[0075] Preparation Example 4
[0076] The preparation method of hyperbranched polymer D is the same as that of Preparation Example 1, except that the amount of 6-chloro-2,4-difluoroaniline added is 66 mmol.
[0077] Preparation Example 5
[0078] The preparation method of modified chitosan A comprises the following steps:
[0079] (1) 9 g of chitosan and 300 ml of deionized water were added to a reaction kettle, 1 mol / L hydrochloric acid was added to adjust the pH to 3, and stirred for 2 h to obtain a chitosan solution;
[0080] (2) 18.5 g of sodium 5-sulfoisophthalic acid and 600 ml of deionized water were added to a reaction kettle, stirred for 30 min, and then 0.825 g of 1-ethyloctane-(3-dimethylaminopropyl)carbodiimide hydrochloride was added to obtain a sodium 5-sulfoisophthalic acid solution;
[0081] (3) The chitosan solution obtained in step (1) was mixed with the sodium 5-sulfonate solution obtained in step (2), 0.1 mol / L sodium hydroxide was added to adjust the pH to 7, and the mixture was stirred at room temperature for 5 h to obtain modified chitosan A.
[0082] Preparation Example 6
[0083] The preparation method of modified chitosan B is the same as that of Preparation Example 5, except that in step (2), 9 g of sodium 5-sulfonate isophthalic acid and 300 ml of deionized water are added to a reaction kettle, stirred for 30 min, and then 0.54 g of 1-ethyloctane-(3-dimethylaminopropyl)carbodiimide hydrochloride is added to obtain a sodium 5-sulfonate solution of isophthalic acid.
[0084] Example 1
[0085] A circulating cooling water slow-release scale inhibitor comprises the following raw materials in parts by weight: 25 parts of polyacrylamide, 15 parts of polyepoxysuccinic acid, 12.5 parts of sodium gluconate, 10 parts of hyperbranched polymer A, 10 parts of isophorone diamine, 6 parts of modified chitosan A, 4 parts of melamine, 3 parts of benzotriazole, 1.5 parts of tartaric acid, 0.5 parts of sodium dodecyl sulfonate, 1 part of polyethylene glycol 200, and 40 parts of deionized water.
[0086] The preparation method of the slow-release scale inhibitor of this embodiment comprises the following steps:
[0087] Polyacrylamide, polyepoxysuccinic acid, sodium gluconate, hyperbranched polymer A, isophorone diamine, modified chitosan A, melamine, benzotriazole, tartaric acid, sodium dodecyl sulfate, polyethylene glycol 200 and deionized water were added to a reactor, stirred for 40 minutes, heated to 60°C, and stirred at 250 W ultrasonic power for 3 hours to obtain a slow-release scale inhibitor.
[0088] Example 2
[0089] A circulating cooling water slow-release scale inhibitor comprises the following raw materials in parts by weight: 20 parts of polyacrylamide, 10 parts of polyepoxysuccinic acid, 10 parts of sodium gluconate, 5 parts of hyperbranched polymer A, 5 parts of isophorone diamine, 4 parts of modified chitosan A, 2 parts of melamine, 1 part of benzotriazole, 1 part of tartaric acid, 0.5 parts of sodium dodecyl sulfonate, 0.5 parts of polyethylene glycol 2000 and 30 parts of deionized water.
[0090] The preparation method of the slow-release scale inhibitor of this embodiment comprises the following steps:
[0091] Polyacrylamide, polyepoxysuccinic acid, sodium gluconate, hyperbranched polymer A, isophorone diamine, modified chitosan A, melamine, benzotriazole, tartaric acid, sodium dodecyl sulfate, polyethylene glycol 200 and deionized water were added to a reactor, stirred for 20 minutes, heated to 70°C, and stirred at an ultrasonic power of 100 W for 4 hours to obtain a slow-release scale inhibitor.
[0092] Example 3
[0093] A circulating cooling water slow-release scale inhibitor comprises the following raw materials in parts by weight: 30 parts of polyacrylamide, 20 parts of polyepoxysuccinic acid, 15 parts of sodium gluconate, 15 parts of hyperbranched polymer A, 15 parts of isophorone diamine, 8 parts of modified chitosan A, 6 parts of melamine, 5 parts of benzotriazole, 2 parts of tartaric acid, 0.5 parts of sodium dodecyl sulfonate, 1.5 parts of polyethylene glycol 200, and 50 parts of deionized water.
[0094] The preparation method of the slow-release scale inhibitor of this embodiment comprises the following steps:
[0095] Polyacrylamide, polyepoxysuccinic acid, sodium gluconate, hyperbranched polymer A, isophorone diamine, modified chitosan A, melamine, benzotriazole, tartaric acid, sodium dodecyl sulfate, polyethylene glycol 200 and deionized water were added to a reactor, stirred for 60 minutes, heated to 50°C, and stirred at 350W ultrasonic power for 2 hours to obtain a slow-release scale inhibitor.
[0096] Example 4
[0097] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of hyperbranched polymer B is used to replace hyperbranched polymer A.
[0098] Example 5
[0099] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of hyperbranched polymer C is used to replace hyperbranched polymer A.
[0100] Example 6
[0101] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of hyperbranched polymer D is used to replace hyperbranched polymer A.
[0102] Example 7
[0103] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of modified chitosan B is used to replace modified chitosan A.
[0104] Example 8
[0105] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation method is the same as that of Example 1, except that anionic polyacrylamide is replaced by an equal amount of cationic polyacrylamide.
[0106] Comparative Example 1
[0107] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of commercially available chitosan is used to replace modified chitosan A.
[0108] Comparative Example 2
[0109] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that the hyperbranched polymer A is not added.
[0110] Comparative Example 3
[0111] A circulating cooling water slow-release scale inhibitor and a preparation method thereof, wherein the specific implementation manner is the same as that of Example 1, except that an equal amount of aminotrimethylenephosphonic acid is used to replace the hyperbranched polymer A.
[0112] Effect evaluation:
[0113] The scale inhibitors prepared in the above Examples 1-8 and Comparative Examples 1-3 were tested and analyzed, and the specific results are shown in Table 1.
[0114] Performance Test:
[0115] The extracted high-mineralization water was placed in a tray and evaporated to dryness. The obtained solid was ground and stored in a dryer. 5g and 45g of the solid were dissolved in 1L of distilled water to obtain water with a mineralization of 5g / L and 45g / L. At a temperature of 60°C, the scale inhibitors in the embodiments and comparative examples were added. The dosage standard of the scale inhibitor was 40mg of the scale inhibitor per liter of water. The scale inhibition rate of the slow-release scale inhibitor was determined by the constant temperature concentration method.
[0116] Table 1
[0117] Serial number Descaling rate at mineralization 5g / L / % Descaling rate at mineralization 45g / L / % Example 1 99.7 99.0 Example 2 99.4 98.1 Example 3 99.5 98.6 Example 4 94.6 92.7 Example 5 89.4 81.6 Example 6 91.3 83.9 Example 7 92.9 84.2 Example 8 93.2 91.8 Comparative Example 1 88.3 74.1 Comparative Example 2 74.7 62.4 Comparative Example 3 80.8 69.6
[0118] From the results in Table 1, it can be seen that the slow-release scale inhibitor prepared in Examples 1-3 has a high scale inhibition efficiency, and can still maintain a high scale inhibition rate in a water environment with high salt mineralization, and has good application value.
[0119] Compared with Example 1, in Example 4, hydroxyethylidene diphosphonic acid is not introduced when preparing the hyperbranched polymer. The lack of phosphonic acid groups weakens the chelating effect with metal ions in water, reduces the lattice distortion effect, and thus reduces the scale inhibition rate.
[0120] Compared with Example 1, in Example 5, the molar ratio of citric acid and 1,2,4-butanetriol was changed when preparing the hyperbranched polymer, so that the branched structure was weakened, thereby resulting in a decrease in the scale inhibition rate.
[0121] Compared with Example 1, Example 6 changes the molar ratio of intermediate 1 and 6-chloro-2,4-difluoroaniline when preparing the hyperbranched polymer, which reduces the amount of hydroxyethylidene diphosphonic acid added in step S3 and reduces the scale inhibition rate.
[0122] Compared with Example 1, Example 7 changes the mass ratio of chitosan to sodium 5-sulfoisophthalate when preparing modified chitosan, which will reduce the salt resistance and thus reduce the scale inhibition rate.
[0123] Compared with Example 1, Example 8 uses an equal amount of cationic polyacrylamide to replace anionic polyacrylamide, which cannot produce the effect of mutual repulsion between charges of the same kind, and the scale inhibition effect is reduced.
[0124] Compared with Example 1, Comparative Example 1 uses an equal amount of commercially available chitosan to replace modified chitosan. Chitosan may be partially ineffective in high-mineralization water, and lacks the introduction of sulfonic acid groups, resulting in reduced salt resistance and temperature resistance.
[0125] Compared with Example 1, Comparative Example 2 does not add hyperbranched polymer A, and Comparative Example 3 replaces hyperbranched polymer A with an equal amount of aminotrimethylenephosphonic acid, both of which make the temperature resistance worse and the scale inhibition efficiency significantly reduced.
[0126] The above is only a preferred embodiment of the present invention and does not constitute any form of limitation to the present application. Although the present application is disclosed as above in the preferred embodiment, it is not intended to limit the present application. Any technician familiar with the profession, without departing from the scope of the technical solution of the present application, using the technical content disclosed above to make slight changes or modifications are equivalent to equivalent implementation cases. However, any simple modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution.
Claims
1. A slow-release antiscalant for circulating cooling water, It is characterized in that The scale inhibitor comprises the following raw materials by weight: 20-30 parts of polyacrylamide, 10-20 parts of polyepoxysuccinic acid, 10-15 parts of sodium gluconate, 5-15 parts of hyperbranched polymer, 5-15 parts of isophorone diamine, 4-8 parts of modified chitosan, 2-6 parts of melamine, 1-5 parts of benzotriazole, 1-2 parts of tartaric acid, 1-2 parts of dispersant and 30-50 parts of deionized water.
2. A circulating cooling water slow-release antiscalant according to claim 1, It is characterized in that The polyacrylamide is anionic polyacrylamide.
3. A circulating cooling water slow-release antiscalant according to claim 2, It is characterized in that The number average molecular weight of the anionic polyacrylamide is 8-20 million.
4. A circulating cooling water slow-release antiscalant according to claim 1, It is characterized in that The preparation method of the hyperbranched polymer comprises the following preparation steps: S1. Add citric acid and 1,2,4-butanetriol to a reaction kettle, stir, then add p-toluenesulfonic acid, heat to 115-125°C, control the vacuum degree to 0.20-0.75MPa, stir and react for 8-12h to obtain intermediate 1; S2. The intermediate 1 obtained in step S1, dimethyl sulfoxide, and 6-chloro-2,4-difluoroaniline are added to a reaction kettle, stirred, and sodium carbonate is added under an inert gas atmosphere, heated to 70-100° C., stirred for 10-12 hours, washed, and dried to obtain intermediate 2; S3. Add hydroxyethylidene diphosphonic acid and deionized water into a reaction kettle, stir, then add 4-dimethylaminopyridine and stir, dropwise add intermediate 2 obtained in step S2, heat to 65-75°C, react for 10-14h, wash, and dry to obtain a hyperbranched polymer.
5. A circulating cooling water slow-release antiscalant according to claim 4, It is characterized in that The molar ratio of citric acid to 1,2,4-butanetriol in step S1 is (3-3.6):
1.
6. A circulating cooling water slow-release antiscalant according to claim 4, It is characterized in that The molar ratio of the intermediate 1 to 6-chloro-2,4-difluoroaniline in step S2 is 1:(3.2-3.8).
7. A circulating cooling water slow-release antiscalant according to claim 1, It is characterized in that The preparation method of the modified chitosan comprises the following preparation steps: (1) adding chitosan and deionized water into a reaction kettle, adjusting the pH to 2.5-3, and stirring to obtain a chitosan solution; (2) adding sodium 5-sulfoisophthalic acid and deionized water into a reaction kettle, stirring, and then adding 1-ethyl-(3-dimethylaminopropyl)carbodiimide hydrochloride to obtain a sodium 5-sulfoisophthalic acid solution; (3) Mixing the chitosan solution obtained in step (1) with the sodium 5-sulfonate solution obtained in step (2), adjusting the pH to 6-7, stirring at room temperature for 4-5 hours, and filtering to obtain modified chitosan.
8. A circulating cooling water slow-release antiscalant according to claim 7, It is characterized in that The mass ratio of chitosan to sodium 5-sulfoisophthalate is 1:(1.5-3).
9. A circulating cooling water slow-release antiscalant according to claim 1, It is characterized in that The dispersant is sodium alkyl sulfonate and / or polyethylene glycol.
10. A method for preparing the circulating cooling water slow-release antiscalant according to any one of claims 1 to 9, It is characterized in that The preparation steps include: Add polyacrylamide, polyepoxysuccinic acid, sodium gluconate, hyperbranched polymer, isophorone diamine, modified chitosan, melamine, benzotriazole, tartaric acid, dispersant and deionized water into a reactor, stir for 20-60 minutes, heat to 50-70°C, and stir for 2-4 hours at an ultrasonic power of 100-350W to obtain a slow-release scale inhibitor.
Citation Information
Cited By
A method for preparing a highly effective scale inhibitor
CN119750801A